Electronic Components
By employing a substrate with strategic thickness variations and aligned sealing layer expansion coefficients, the design mitigates peeling issues, ensuring robust sealing in electronic components under thermal stress.
Patent Information
- Application Number
- JP2020216631
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-12-25
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2040-12-25
AI Technical Summary
The peeling of the sealing layer from the substrate due to thermal stress is a common issue in electronic components, leading to deteriorated sealing properties.
The design incorporates a substrate with specific thickness variations and stepped regions, where the sealing layer has a higher coefficient of linear expansion than the substrate, and a sealing member with an even higher expansion coefficient, ensuring the side surface of the sealing layer aligns with the step between these regions, thereby reducing stress and preventing peeling.
This configuration effectively suppresses the peeling of the sealing layer from the substrate, maintaining the integrity of the sealing properties under thermal stress.
Smart Images

Figure 0007577535000003 
Figure 0007577535000004 
Figure 0007577535000005
Abstract
Description
[Technical field]
[0001] The present invention relates to electronic components. [Background technology]
[0002] There is known an electronic component in which a device chip having an element is mounted on a substrate, and the element is sealed by a sealing layer provided on the substrate surrounding the device chip and a sealing member provided on the sealing layer (for example, Patent Document 1). It is also known to provide a recess or protrusion on the substrate, and to provide a sealing layer on the recess or protrusion (for example, Patent Documents 2 and 3). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2006-203149 A [Patent Document 2] JP 2016-201780 A [Patent Document 3] JP 2019-36784 A Summary of the Invention [Problem to be solved by the invention]
[0004] When stress such as thermal stress is applied between the sealing layer and the substrate, the sealing layer may peel off from the substrate, which deteriorates the sealing performance of the element.
[0005] The present invention has been made in consideration of the above problems, and has an object to suppress peeling of a sealing layer from a substrate. [Means for solving the problem]
[0006] The present invention is, in plan view, Rectangular Periphery and the periphery In line with Frame-shaped A first region; a third region surrounded by the first region; In the first region On the opposite side to the periphery Next to each other and a second insulating layer is disposed between at least one of the four sides of the first region and the third region and along the at least one side.a second region, the thickness of the second region being smaller than the thickness of the first region by a step provided between the second region and the first region; The thickness of the third region is greater than the thickness of the second region due to a step between the third region and the second region. A substrate and a In the third region a device chip mounted on the substrate and having an element; a sealing layer provided in the first region to surround the device chip and having a linear expansion coefficient larger than that of the substrate; and a sealing layer provided on the sealing layer and supporting the element together with the sealing layer. In the gap between the device chip and the substrate and a sealing member having a linear expansion coefficient greater than that of the sealing layer. The side surface of the sealing layer coincides with the side surface of the step between the first region and the second region. It is an electronic component.
[0008] In the above configuration, the second region is provided along four sides of the first region, The third region may be surrounded in a plan view of the substrate.
[0009] The present invention relates to a method for manufacturing a semiconductor device, comprising: a peripheral edge having a rectangular shape in a plan view; a frame-shaped first region along the peripheral edge; and a second region adjacent to the first region on the opposite side to the peripheral edge, In plan view, the first region is surrounded by the first region and is located inside the first region. a second region occupying 90% or more of an area and having a thickness smaller than that of the first region due to a step provided between the second region and the first region; The second region is provided with the first region and the second region, and a sealing member having a linear expansion coefficient greater than that of the sealing layer, the sealing member being disposed on the sealing layer and sealing the element in a gap between the device chip and the substrate, the sealing member having a linear expansion coefficient greater than that of the sealing layer, the side surface of the sealing layer coinciding with a side surface of a step between the first region and the second region.
[0013] In the above configuration, the substrate may be a ceramic substrate, and the sealing member may be solder.
[0014] In the above configuration, the device chip is The above The element may be an acoustic wave element on a surface facing the substrate via a gap. Effect of the Invention
[0015] According to the present invention, peeling of the sealing layer from the substrate can be suppressed. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1(a) is a cross-sectional view of the electronic component according to the first embodiment, FIG. 1(b) is an enlarged cross-sectional view of the vicinity of a sealing layer, and FIG. 1(c) is a plan view of a substrate. [Diagram 2]2(a) and 2(b) are a plan view and a cross-sectional view illustrating an example of an acoustic wave device according to a first embodiment. [Diagram 3] 3(a) and 3(b) are cross-sectional views (part 1) illustrating the method for manufacturing the electronic component according to the first embodiment. [Figure 4] 4(a) and 4(b) are cross-sectional views (part 2) illustrating the method for manufacturing the electronic component according to the first embodiment. [Diagram 5] FIG. 5(a) is a plan view of a substrate in a first modified example of the first embodiment, and FIG. 5(b) is a plan view of a substrate in a second modified example of the first embodiment. [Figure 6] FIG. 6(a) is a cross-sectional view of the electronic component according to the second embodiment, FIG. 6(b) is an enlarged cross-sectional view of the sealing layer and its vicinity, and FIG. 6(c) is a plan view of the substrate. [Figure 7] 7(a) and 7(b) are cross-sectional views (part 1) illustrating a method for manufacturing an electronic component according to the second embodiment. [Figure 8] 8(a) and 8(b) are cross-sectional views (part 2) illustrating the method for manufacturing an electronic component according to the second embodiment. [Figure 9] FIG. 9(a) is a cross-sectional view of an electronic component according to a modified example of the second embodiment, FIG. 9(b) is an enlarged cross-sectional view of the vicinity of the sealing layer, and FIG. 9(c) is a plan view of the substrate. [Figure 10] FIG. 10 is a cross-sectional view of an electronic component according to a comparative example. [Figure 11] FIG. 11 is a cross-sectional view showing a problem that occurs in an electronic component according to a comparative example. [Figure 12] FIG. 12 is a plan view of the model used in the simulation. [Figure 13] 13(a) and 13(b) are cross-sectional views of models A and B taken along line AA in FIG. [Figure 14] 14(a) to 14(c) are cross-sectional views of models C to E taken along line AA in FIG. [Figure 15] FIG. 15 is a graph showing the simulation results. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, embodiments of the present invention will be described with reference to the drawings. EXAMPLES
[0018] Fig. 1(a) is a cross-sectional view of an electronic component according to a first embodiment, Fig. 1(b) is an enlarged cross-sectional view of the vicinity of a sealing layer, and Fig. 1(c) is a plan view of a substrate. As shown in Figs. 1(a) to 1(c), an electronic component 100 according to a first embodiment has one or more device chips 30 mounted on a substrate 10. The substrate 10 includes a plurality of insulating layers 11a to 11c. The insulating layers 11a to 11c are, for example, ceramic layers such as LTCC (Low Temperature Co-fired Ceramics) or HTCC (High Temperature Co-fired Ceramics) or resin layers such as glass epoxy resin.
[0019] Terminals 14 are provided on the lower surface of the substrate 10. Metal layers 12a are provided between insulating layers 11a and 11b and between insulating layers 11b and 11c. Metal layers 12b are provided on insulating layer 11c. Via wiring 13 is provided between insulating layers 11a to 11c. Metal layers 12a and 12b, via wiring 13, and terminals 14 are metal layers such as, for example, a copper layer, an aluminum layer, a gold layer, or a tungsten layer.
[0020] The device chip 30 mounted on the substrate 10 includes a substrate 31, and an acoustic wave element 32 and wiring 33 provided on the lower surface of the substrate 31. The wiring 33 is a metal layer such as a copper layer, an aluminum layer, or a gold layer. The device chip 30 is flip-chip mounted (face-down mounted) on the substrate 10 via bumps 34. The bumps 34 bond the metal layer 12b and the wiring 33. The bumps 34 are, for example, gold bumps, solder bumps, or copper bumps.
[0021] The substrate 10 is substantially rectangular in plan view. The substantially rectangular shape includes cases where the corners are rounded and cases where each side is curved. The substrate 10 has a region 20 along the four sides in plan view, a region 21 located inside the region 20 and adjacent to the region 20, and having a thickness smaller than the region 20 due to a step 25 provided between the region 20 and the region 21, and a region 22 adjacent to the region 21 on the opposite side to the region 20, and having a thickness larger than the region 21 due to a step 26 provided between the region 21 and the region 21. That is, a groove 23 recessed with respect to the upper surfaces of the regions 20 and 22 is provided on the upper surface of the region 21. The step may be an angle of about 70° to 140° between the side of the step and the surface of the substrate when the surface (plane) of the substrate is set at 0° when the cross section of the electronic component is observed. The thickness of the substrate 10 in the region 20 is substantially the same as the thickness of the substrate 10 in the region 22, and the upper surface of the region 20 and the upper surface of the region 22 are substantially flush with each other. Region 22 is surrounded by regions 20 and 21 in plan view. Region 21 is surrounded by region 20 in plan view.
[0022] The width W1 of the region 20 is, for example, 50 μm to 150 μm. The width W2 of the region 21 is, for example, 10 μm to 100 μm. The height H of the step 25 between the regions 20 and 21 and the step 26 between the regions 21 and 22 (i.e., the depth of the groove portion 23) is, for example, 1 μm to 50 μm.
[0023] The device chip 30 is mounted in the region 22 of the substrate 10. The sealing layer 15 is provided in the region 20 of the substrate 10 so as to surround the device chip 30. The sealing layer 15 is provided over the entire region 20 in a ring shape so as to completely surround the device chip 30. The sealing layer 15 is not limited to completely surrounding the device chip 30, and may be interrupted in part. The sealing layer 15 is not provided in the region 21. The side surface 17 of the sealing layer 15 on the device chip 30 side is substantially flush with the side surface (step side surface) 35a of the step 25 between the regions 20 and 21. The sealing layer 15 is formed of a material having a linear expansion coefficient larger than that of the substrate 10, and is formed of, for example, a metal mainly composed of copper.
[0024] A sealing member 36 is provided on the sealing layer 15 so as to surround the device chip 30. The sealing member 36 is provided, for example, so as to completely surround the device chip 30. The sealing member 36 is formed of a member having a linear expansion coefficient larger than that of the sealing layer 15, for example, formed of solder containing tin. The sealing member 36 is bonded, for example, to the upper surface of the sealing layer 15. A flat lid 37 is provided on the upper surface of the device chip 30 and the upper surface of the sealing member 36. The lid 37 is, for example, a metal plate such as a Kovar plate or an insulating plate. A protective film 38 is provided so as to cover the lid 37, the sealing member 36, and the sealing layer 15. The protective film 38 is, for example, a metal film such as nickel or an insulating film.
[0025] The acoustic wave element 32 faces the substrate 10 via a gap 16. The acoustic wave element 32 is sealed in the gap 16 by a sealing layer 15, a sealing member 36, a lid 37, and the substrate 10. The bumps 34 are surrounded by the gap 16. The terminals 14 are electrically connected to the acoustic wave element 32 via the via wiring 13, the metal layers 12a and 12b, the bumps 34, and the wiring 33.
[0026] 2(a) and 2(b) are a plan view and a cross-sectional view showing an example of an acoustic wave element in the first embodiment. As shown in FIG. 2(a), an acoustic wave element 32 may be a surface acoustic wave resonator. A substrate 31 is a piezoelectric substrate, and an IDT (Interdigital Transducer) 40 and a reflector 41 are provided on the substrate 31. The IDT 40 has a pair of opposing comb electrodes 42. The comb electrode 42 has a plurality of electrode fingers 43 and a bus bar 44 connecting the plurality of electrode fingers 43. The reflectors 41 are provided on both sides of the IDT 40. The IDT 40 excites a surface acoustic wave in the substrate 31, which is a piezoelectric substrate. The reflector 41 reflects the surface acoustic wave.
[0027] The IDT 40 and the reflector 41 are formed of, for example, an aluminum film or a copper film. A protective film or a temperature compensation film covering the IDT 40 and the reflector 41 may be provided on the substrate 31. The substrate 31 may be directly or indirectly bonded to a supporting substrate such as a sapphire substrate, an alumina substrate, a spinel substrate, a quartz substrate, or a silicon substrate.
[0028] 2(b), acoustic wave element 32 may be a piezoelectric thin film resonator. A piezoelectric film 46 is provided on substrate 31. A lower electrode 45 and an upper electrode 47 are provided to sandwich piezoelectric film 46. A gap 48 is formed between lower electrode 45 and substrate 31. A region where lower electrode 45 and upper electrode 47 face each other, sandwiching at least a portion of piezoelectric film 46, is resonance region 49. In resonance region 49, lower electrode 45 and upper electrode 47 excite acoustic waves in thickness longitudinal vibration mode in piezoelectric film 46.
[0029] The substrate 31 is, for example, a sapphire substrate, a spinel substrate, an alumina substrate, a glass substrate, a quartz substrate, or a silicon substrate. The lower electrode 45 and the upper electrode 47 are, for example, metal films such as ruthenium films. The piezoelectric film 46 is, for example, an aluminum nitride film. Note that an acoustic reflection film that reflects elastic waves may be provided instead of the gap 48.
[0030] 2(a) and 2(b), acoustic wave element 32 includes electrodes that excite acoustic waves. For this reason, acoustic wave element 32 is covered with gap 16 so as not to impede the excitation of acoustic waves, as shown in FIG.
[0031] [Manufacturing method] 3(a) to 4(b) are cross-sectional views showing a manufacturing method of an electronic component according to Example 1. As shown in Fig. 3(a), a substrate 10 is prepared. The substrate 10 includes laminated insulating layers 11a to 11c, a metal layer 12a provided between insulating layers 11a and 11b and between insulating layers 11b and 11c, a metal layer 12b and a sealing layer 15 provided on the upper surface of insulating layer 11c, via wiring 13 provided between insulating layers 11a to 11c, and a terminal 14 provided on the lower surface of insulating layer 11a.
[0032] As shown in FIG. 3(b), the groove 23 is formed in the substrate 10. The groove 23 is formed, for example, by forming a mask layer that covers areas other than the area where the groove 23 is to be formed, and etching the substrate 10 using the mask layer as a mask. The depth of the groove 23 may be smaller or larger than the thickness of the insulating layer 11c. As a result, the substrate 10 has a region 20 in which the sealing layer 15 is provided, a region 21 adjacent to the region 20 and having a smaller thickness than the region 20 due to a step, and a region 22 on the opposite side to the region 20 and adjacent to the region 21 and having a larger thickness than the region 21 due to a step. The groove 23 may be formed by dicing the substrate 10, or the groove 23 may be formed by forming the substrate 10 by firing the insulating layers 11a to 11c using the insulating layer 11c in which the groove 23 is formed.
[0033] 4(a), the device chip 30 is flip-chip mounted on the substrate 10 via bumps 34. As a result, the substrate 10 and the acoustic wave element 32 face each other with a gap 16 therebetween.
[0034] 4(b), a lid 37 having a solder plate made of, for example, tin-silver formed on its underside is placed on the substrate 31. The solder is heated and melted, and the lid 37 is pressed toward the substrate 31. Since the upper surface of the sealing layer 15 has good wettability with the solder, the molten solder wets and spreads over the upper surface of the sealing layer 15 to be bonded to the sealing layer 15. As a result, a sealing member 36 is formed that surrounds the device chip 30 and is bonded to the sealing layer 15.
[0035] After cutting the lid 37, the sealing member 36, the sealing layer 15, and the substrate 10 to separate the electronic components, a protective film 38 is formed to cover the sealing layer 15, the sealing member 36, and the lid 37. In this way, the electronic component 100 shown in Figures 1(a) to 1(c) is formed.
[0036] [Modification of Example 1] 5(a) is a plan view of a substrate in Modification 1 of Example 1, and FIG. 5(b) is a plan view of a substrate in Modification 2 of Example 1. As shown in FIG. 5(a), in electronic component 110 in Modification 1 of Example 1, region 21 having a smaller thickness than region 20 due to a step is provided along two of four sides (e.g., two opposing sides) when substrate 10 is viewed in plan. As shown in FIG. 5(b), in electronic component 120 in Modification 2 of Example 1, region 21 having a smaller thickness than region 20 due to a step is provided along one of four sides when substrate 10 is viewed in plan. Other configurations of Modification 1 and Modification 2 of Example 1 are the same as those of Example 1, and therefore illustration and description are omitted. EXAMPLES
[0037] FIG. 6(a) is a cross-sectional view of an electronic component according to Example 2, FIG. 6(b) is a cross-sectional view enlarging the vicinity of the sealing layer, and FIG. 6(c) is a plan view of the substrate. As shown in FIG. 6(a) to FIG. 6(c), in the electronic component 200 of Example 2, the substrate 10 has a region 20 along the four sides when viewed in a plan view, and a region 21a adjacent to the region 20, surrounded by the region 20, which is substantially the entire region inside the region 20, and has a thickness smaller than that of the region 20 due to a step 27 provided between the region 20 and the region 21a. The device chip 30 is mounted in the region 21a of the substrate 10. The side surface 17 of the sealing layer 15 provided in the region 20 on the device chip 30 side is substantially flush with the step side surface 35b between the regions 20 and 21a. The width W of the region 20 is, for example, 50 μm to 150 μm. The height H of the step between the regions 20 and 21a is, for example, 1 μm to 50 μm. The other configurations are the same as those in the first embodiment, so the explanation will be omitted.
[0038] [Manufacturing method] 7(a) to 8(b) are cross-sectional views showing a manufacturing method of an electronic component according to Example 2. As shown in Fig. 7(a), a substrate 10 is prepared. The substrate 10 includes laminated insulating layers 11a to 11c, a metal layer 12a provided between insulating layers 11a and 11b and between insulating layers 11b and 11c, a metal layer 12b provided on the upper surface of insulating layer 11c, via wiring 13 provided between insulating layers 11a to 11c, and a terminal 14 provided on the lower surface of insulating layer 11a.
[0039] As shown in FIG. 7(b), the mask layer 60 covers the area other than the area where the sealing layer 15 is to be formed. The mask layer 60 is, for example, a photoresist film. Using the mask layer 60 as a mask, the same material as the insulating layers 11a to 11c is deposited or screen printed to form the protrusions 61 in the area where the sealing layer 15 is to be formed. Then, using the mask layer 60 as a mask, the material for forming the sealing layer 15 is plated or screen printed to form the sealing layer 15 on the protrusions 61. As a result, the substrate 10 has a region 20 where the sealing layer 15 is provided and a region 21a adjacent to the region 20 and having a smaller thickness due to a step than the region 20. In FIG. 7(a), the substrate 10 having a frame-shaped insulating layer corresponding to the protrusions 61 provided on the insulating layer 11c may be formed by firing, and then the sealing layer 15 may be formed using a mask layer as in FIG. 7(b).
[0040] 8(a), after removing the mask layer 60, the device chip 30 is flip-chip mounted on the substrate 10 via the bumps 34. As a result, the substrate 10 and the acoustic wave element 32 face each other with a gap 16 therebetween.
[0041] 8(b), a lid 37 having a solder plate made of, for example, tin-silver formed on its underside is placed on the substrate 31. The solder is heated and melted, and the lid 37 is pressed toward the substrate 31. Since the upper surface of the sealing layer 15 has good wettability with the solder, the molten solder wets and spreads over the upper surface of the sealing layer 15 to be bonded to the sealing layer 15. As a result, a sealing member 36 is formed that surrounds the device chip 30 and is bonded to the sealing layer 15.
[0042] After cutting the lid 37, the sealing member 36, the sealing layer 15, and the substrate 10 to separate the electronic components, a protective film 38 is formed to cover the sealing layer 15, the sealing member 36, and the lid 37. This forms the electronic component 200 shown in Figures 6(a) to 6(c).
[0043] [Modification of Example 2] Fig. 9(a) is a cross-sectional view of an electronic component according to a modification of Example 2, Fig. 9(b) is an enlarged cross-sectional view of the vicinity of the sealing layer, and Fig. 9(c) is a plan view of the substrate. As shown in Figs. 9(a) to 9(c), in an electronic component 210 according to a modification of Example 2, the side surface 17 of the sealing layer 15 on the device chip 30 side is located inside the region 20 with respect to the step side surface 35b between the region 20 and the region 21a. The other configurations are the same as those of Example 2, and therefore will not be described.
[0044] [Comparative Example] Fig. 10 is a cross-sectional view of an electronic component according to a comparative example. As shown in Fig. 10, in electronic component 500 of the comparative example, the upper surface of substrate 10 is flat. The other configurations are the same as those in Example 1, and therefore description thereof will be omitted.
[0045] FIG. 11 is a cross-sectional view showing a problem that occurs in an electronic component according to a comparative example. As shown in FIG. 11, in the electronic component according to the comparative example, after a temperature cycle test, the sealing layer 15 may peel off from the substrate 10 starting from the end portion on the device chip 30 side. This is considered to be because a difference between the linear expansion coefficients of the sealing layer 15 and the sealing member 36 and the linear expansion coefficient of the substrate 10 causes distortion and stress near the interface of the sealing layer 15 with the substrate 10. If the sealing layer 15 peels off from the substrate 10, a gap 50 is formed between the sealing layer 15 and the substrate 10, and the sealing property of the acoustic wave element 32 deteriorates. As an example, the linear expansion coefficient is 10.4 ppm / °C when the substrate 10 is an LTCC substrate, 17.7 ppm / °C when the sealing layer 15 is a copper (Cu) layer, and 30 ppm / °C when the sealing member 36 is a tin-silver (SnAg) solder.
[0046] [simulation] The strain applied to the sealing layer 15 was simulated. FIG. 12 is a plan view of a model used in the simulation. FIGS. 13(a) and 13(b) are cross-sectional views of models A and B between AA in FIG. 12. FIGS. 14(a) to 14(c) are cross-sectional views of models C to E between AA in FIG. 12. Model A in FIG. 13(a) corresponds to a comparative example, model B in FIG. 13(b) corresponds to Example 1, model C in FIG. 14(a) corresponds to Example 2, and models D and E in FIG. 14(b) and FIG. 14(c) correspond to modified examples of Example 2. FIG. 12 illustrates model A in FIG. 13(a) as an example, but models B to E in FIG. 13(b) to FIG. 14(c) are the same except that a step is formed on the upper surface of the substrate 10. In model B in FIG. 13(b), a groove portion 23 is provided in an L-shape along the sealing layer 15. The normal direction of the substrate 10 is the Z direction, and the side directions of the substrate 10 are the X direction and the Y direction.
[0047] As shown in Fig. 12 to Fig. 14(c), the simulation was performed using a 1 / 4 symmetric model of the substrate 10. That is, the sealing layer 15, the sealing member 36, and the protective film 38 are not provided on the +X side surface and the -Y side surface of the substrate 10, and the boundary conditions of these surfaces are mirror conditions. The lengths of the substrate 10 in the Y direction and the X direction are D1 and D2. The lengths of the device chip 30 in the X direction and the Y direction are D4 and D5. The width of the sealing layer 15 is D3. The diameter of the bump 34 is D6. The thickness of the substrate 10 is T1. The thickness of the sealing layer 15 and the bump 34 is T2. The thickness of the device chip 30 is T3. The thickness of the lid 37 is T4. The thickness of the protective film 38 is T5. In the model B of Fig. 13(b), the height of the step between the region 20 and the region 21 is H1, and the width of the region 21 is W. The side surface of sealing layer 15 and the side surface of the step between regions 20 and 21 are flush with each other. In models C to E of Fig. 14(a) to Fig. 14(c), the height of the step between region 20 and region 21a is H2. In model C of Fig. 14(a), the side surface of sealing layer 15 and the side surface of the step between regions 20 and 21a are flush with each other. In models D and E of Fig. 14(b) and Fig. 14(c), the distance between the side surface of sealing layer 15 and the side surface of the step between regions 20 and 21a is L.
[0048] The simulation conditions are as follows. Substrate 10: LTCC substrate Metal layers 12a, 12b: Copper (Cu) Sealing layer 15: Copper (Cu) Bump 34: Gold (Au) Device Chip 30: Sapphire Sealing member 36: Tin silver (SnAg) Lid 37: Kovar Protective film 38: Nickel (Ni)
[0049] D1=1.25mm, D2=1.0mm, D3=0.1mm, D4=0.8mm, D5=1.05mm, D6=75μm T1=330μm, T2=15μm, T3=350μm, T4=25μm, T5=10μm
[0050] In model B in FIG. 13(b), H1=30 μm, W=50 μm In model C in Fig. 14(a), H2 = 30 μm In model D in Fig. 14(b), H2 = 30 μm, L = 10 μm In model E in Fig. 14(c), H2 = 30 μm, L = 20 μm
[0051] Table 1 shows the Young's modulus, linear expansion coefficient, and Poisson's ratio of each material used in the simulation. [Table 1]
[0052] As the strain applied to the sealing layer 15, the sealing member 36 was assembled at 221°C, and 5.5 cycles were performed from +25°C, which takes into account the temperature of the completed product, to -40°C to +125°C, which takes into account the temperature cycle test, to simulate the accumulated strain at the final temperature of +125°C. In the simulation, the accumulated strain was measured near the interface of the sealing layer 15 with the substrate 10 and near the end on the device chip 30 side (the dashed line part in FIG. 12).
[0053] The simulation results are shown in Table 2 and Fig. 15. As shown in Table 2 and Fig. 15, model B corresponding to Example 1, model C corresponding to Example 2, and models D and E corresponding to the modified example of Example 2 all had smaller maximum values of cumulative strain than model A corresponding to the comparative example. [Table 2]
[0054] In model A corresponding to the comparative example, the strain applied to the sealing layer 15 is large. As a result, when the adhesion between the sealing layer 15 and the substrate 10 is poor, the sealing layer 15 may peel off from the substrate 10 as shown in FIG. 11. On the other hand, in model B corresponding to Example 1, model C corresponding to Example 2, and models D and E corresponding to the modified example of Example 2, the strain applied to the sealing layer 15 is reduced. This is considered to be due to the following reason. That is, in models B to E, the regions 21 and 21a are provided adjacent to the region 20 in which the sealing layer 15 and the sealing member 36 are provided and have a smaller thickness than the region 20 due to a step. In this structure, when the sealing layer 15 and the sealing member 36 expand and contract due to a temperature change, the region 20 becomes a behavior region that is easily deformed following the expansion and contraction of the sealing layer 15 and the sealing member 36. In this way, it is considered that the strain applied to the sealing layer 15 is reduced by forming a behavior region in the substrate 10 that deforms together with the sealing layer 15 and the sealing member 36.
[0055] According to the first and second embodiments and their modifications, the substrate 10 has a region 20 along the periphery in plan view, and regions 21 and 21a adjacent to the region 20 and having a thickness smaller than that of the region 20 due to steps 25 and 27 provided between the region 20 and the region 21 and 21a. The region 20 is provided with a sealing layer 15 that surrounds the device chip 30 mounted on the substrate 10 and has a linear expansion coefficient larger than that of the substrate 10. The sealing layer 15 is provided with a sealing member 36 that has a linear expansion coefficient larger than that of the sealing layer 15 and seals the acoustic wave element 32 together with the sealing layer 15. As a result, the region 20 of the substrate 10 becomes a behavior region that deforms together with the sealing layer 15 and the sealing member 36, so that the stress applied to the sealing layer 15 is reduced, and the sealing layer 15 can be prevented from peeling off from the substrate 10.
[0056] In the first embodiment and its modified example, in addition to the regions 20 and 21, the substrate 10 has a region 22 which is surrounded by the region 20 in a plan view and has the region 21 interposed between the region 20 and at least a part of the region 22. The thickness of the region 22 is made larger than the thickness of the region 21 by a step 26 provided between the region 22 and the region 21. The device chip 30 is mounted in the region 22. This allows a large thickness to be secured over most of the substrate 10, thereby suppressing a decrease in the strength of the substrate 10.
[0057] The depth of the groove 23 formed in the region 21 is preferably 0.1 times or more, more preferably 0.2 times or more, and even more preferably 0.3 times or more, the width of the sealing layer 15, from the viewpoint of reducing the strain applied to the sealing layer 15 and suppressing peeling of the sealing layer 15. If the depth of the groove 23 is too deep, the strength of the substrate 10 decreases or it becomes difficult to thin the substrate 10, so the depth of the groove 23 is preferably 1 time or less, more preferably 0.8 times or less, and even more preferably 0.6 times or less, the width of the sealing layer 15, from the viewpoint of reducing the strain applied to the sealing layer 15, the width of the groove 23 is preferably 0.1 times or more, more preferably 0.3 times or more, and even more preferably 0.5 times or more, the width of the sealing layer 15. If the width of the groove 23 becomes too large, the substrate 10 becomes large, so the width of the groove 23 is preferably 1 time or less, more preferably 0.8 times or less, and even more preferably 0.6 times or less, the width of the sealing layer 15. Groove 23 is preferably provided along at least half of each side of substrate 10, more preferably along at least 2 / 3, and even more preferably along at least 3 / 4. In order to reduce stress applied to sealing layer 15, groove 23 is preferably provided along at least two opposing sides of four sides of substrate 10 in plan view, and preferably extends along the long sides when substrate 10 is rectangular in plan view.
[0058] In the first embodiment, the region 21 of the substrate 10 surrounds the region 22 in a plan view. This effectively prevents peeling of the sealing layer 15. Note that, although Fig. 1(c) shows a case where the region 21 completely surrounds the region 22 from four directions, the region 21 may surround the region 22 from three directions.
[0059] In the second embodiment and its modified example, the region 21a of the substrate 10 is surrounded by the region 20 in a plan view and is substantially the entire region inside the region 20. The device chip 30 is mounted in the region 21a. This allows the substrate 10 to be easily manufactured. "Substantially the entire region" is not limited to the entire region inside the region 20, but includes 90% or more of the region inside the region 20.
[0060] In Examples 1 and 2, the side surface 17 of the sealing layer 15 on the device chip 30 side is approximately aligned with the step side surfaces 35a and 35b between the region 20 and the regions 21 and 21a in the plan view direction of the substrate 10. This makes it possible to effectively reduce the distortion applied to the sealing layer 15 and effectively suppress peeling of the sealing layer 15, as shown in Table 2 and Fig. 15. "Approximately aligned" does not necessarily mean a perfect match, but also includes a deviation to the extent of a manufacturing error.
[0061] In the modified example of Example 2, the step side 35b between the regions 20 and 21a is located closer to the device chip 30 than the side 17 of the sealing layer 15 on the device chip 30 side. This eases the positional accuracy of the sealing layer 15, making it easier to manufacture. As shown in Table 2 and FIG. 15, as the distance between the side 17 of the sealing layer 15 and the step side 35b between the regions 20 and 21a becomes wider, the strain applied to the sealing layer 15 becomes larger. Therefore, the distance between the side 17 of the sealing layer 15 and the step side 35b between the regions 20 and 21a is preferably smaller than the height of the step between the regions 20 and 21a, and is more preferably 0.9 times or less, even more preferably 0.7 times or less, and even more preferably 0.5 times or less. Note that in Example 1 as well, the step side 35a between the regions 20 and 21 may be located closer to the device chip 30 than the side 17 of the sealing layer 15 on the device chip 30 side.
[0062] When the substrate 10 is a ceramic substrate and the sealing member 36 is solder, as shown in Table 1, solder (particularly solder containing tin) has a large linear expansion coefficient, so that a large strain is applied to the sealing layer 15, making it easy to peel off from the substrate 10. Therefore, in such a case, it is preferable to provide the substrate 10 with regions 21, 21a adjacent to the region 20 and having a thickness smaller than that of the region 20 due to the steps 25, 27 between the region 20.
[0063] In the first and second embodiments and their modified examples, the acoustic wave element 32 (surface acoustic wave resonator or piezoelectric thin film resonator) is used as an element of the device chip 30, but other elements such as passive elements such as inductors or capacitors, active elements including transistors, or MEMS (Micro Electro Mechanical System) elements may be used. The sealing member 36 may be a resin layer. In this case, the sealing layer 15 may be a metal layer or a resin layer.
[0064] In the first and second embodiments and their modified examples, the acoustic wave element 32 may form an acoustic wave filter, or may form a multiplexer such as a duplexer, a triplexer, or a quadplexer.
[0065] Although the embodiment of the present invention has been described in detail above, the present invention is not limited to such specific embodiment, and various modifications and variations are possible within the scope of the gist of the present invention described in the claims. [Explanation of symbols]
[0066] 10 Substrate 11a to 11c Insulating layer 12a, 12b metal layer 13 Via wiring 14 Terminals 15 Sealing layer 16 void 17 Side 20, 21, 21a, 22 areas 23 Groove 25, 26, 27 steps 30 Device Chips 31 Substrate 32 Acoustic Wave Devices 33 Wiring 34 Bump 35a, 35b Step side 36 Sealing member 37 Lid 38 Protective film 40 IDT 41 Reflector 42 Comb-shaped electrode 43 Electrode finger 44 Busbar 45 Lower electrode 46 Piezoelectric Film 47 Upper electrode 48 void 49 Resonance region 50 Gap 100, 110, 120, 200, 210, 500 Electronic Components
Claims
1. a substrate having a rectangular peripheral edge in a plan view, a frame-shaped first region along the peripheral edge, a third region surrounded by the first region, and a second region adjacent to the first region on the opposite side to the peripheral edge, located between at least one of four sides of the first region and the third region and along the at least one side, wherein the thickness of the second region is smaller than the thickness of the first region due to a step provided between the second region and the third region, and the thickness of the third region is larger than the thickness of the second region due to a step provided between the second region and the third region; a device chip mounted on the substrate in the third region and having an element; a sealing layer provided in the first region to surround the device chip, the sealing layer having a linear expansion coefficient larger than that of the substrate; a sealing member provided on the sealing layer, which seals the element in the gap between the device chip and the substrate together with the sealing layer and has a linear expansion coefficient greater than that of the sealing layer; An electronic component, wherein a side surface of the sealing layer coincides with a step side surface between the first region and the second region.
2. The electronic component according to claim 1 , wherein the second region is provided along four sides of the first region and surrounds the third region when the substrate is viewed in plan.
3. A substrate having a rectangular periphery in a planar view, a frame-shaped first region along the periphery, and a second region adjacent to the first region on the opposite side to the periphery, surrounded by the first region in the planar view and occupying 90% or more of the region inside the first region, the second region having a thickness smaller than that of the first region due to a step provided between the first region and the second region; a device chip mounted on the substrate in the second region and having an element; a sealing layer provided in the first region to surround the device chip, the sealing layer having a linear expansion coefficient larger than that of the substrate; a sealing member provided on the sealing layer, which seals the element in the gap between the device chip and the substrate together with the sealing layer and has a linear expansion coefficient greater than that of the sealing layer; An electronic component, wherein a side surface of the sealing layer coincides with a step side surface between the first region and the second region.
4. the substrate is a ceramic substrate; The electronic component according to claim 1 , wherein the sealing member is a solder.
5. The electronic component according to claim 1 , wherein the device chip has an acoustic wave element as the element on a surface facing the substrate with the gap therebetween.
Citation Information
Patent Citations
Composite semiconductor device
JP1999260968A
Printed wiring board
JP2005057090A
Electronic component and its manufacturing method
JP2006203149A
Elastic wave device
JP2016201780A
Acoustic wave device
JP2018101955A