Reducing material for gas pressure welding, tools for processing same, and gas pressure welding method

The cap body with deformable features for gas pressure welding addresses the issue of lightweight ring body holding members being blown away, ensuring secure and efficient attachment to steel materials, simplifying the installation process and reducing oxide film formation.

JP7578321B1Active Publication Date: 2024-11-06MURAYOSHI GAS PRESSURE WELDING IND CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023195679
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-11-17
Publication Date
2024-11-06
Estimated Expiration
2043-11-17

AI Technical Summary

Technical Problem

Conventional ring body holding members used in gas pressure welding are lightweight and prone to being blown away by strong winds or accidentally detached, causing time-consuming and troublesome reattachment processes when the gap between steel materials is narrow.

Method used

A cap body with an opening/closing part and deformable side plates or legs that can be fitted onto the tip of the steel material, allowing easy attachment and fixation even in narrow gaps, and includes features like deformable side plates, trunk legs, and a line of weakness for flexible fitting and fixing.

Benefits of technology

Enables secure and efficient attachment of the reducing material to the tip of pressure-welded materials, reducing the complexity and time required for installation, and preventing detachment due to wind or accidental contact, while also suppressing oxide film formation during welding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578321000001_ABST
    Figure 0007578321000001_ABST
Patent Text Reader

Abstract

To provide a reducing material for gas pressure welding, which can be attached to the tip of a pressure-welded material such as a fixed-side steel material while the gap between the tip faces of the pressure-welded materials is narrow. [Solution] The reducing material D1 for gas pressure welding is made of a thermoplastic resin and has a cap body 1a that can be fitted onto the tip portion of the pressure welding side of the material to be pressure welded. A cutting edge 120 is provided on the body 10 of the cap body 1a with a predetermined thickness along the top plate 11 of the cap body 1a and with a width that allows the cap body to be fitted circumferentially into the material to be pressure welded. Continuing from the cutting edge 120, cutting edges 122 and 123 are provided in the remaining thickness portion of the body 10, approximately perpendicular to the top plate 11, to the bottom end, to form an insertion opening 12.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a reducing material for gas pressure welding, a tool for processing the same, and a gas pressure welding method, and more particularly to a reducing material for gas pressure welding that enables the material to be attached to the tip end of the material to be pressure welded even when the gap between the tip faces of the material to be pressure welded is narrow. [Background technology]

[0002] The process of pressure welding of steel materials such as rebar involves bringing two pieces of steel materials arranged vertically or horizontally into contact with each other, with their tip surfaces aligned along a common central axis, and then applying a prescribed pressure to the moving steel material. When the upper limit of pressure is reached, the area around the contact point is heated with a flame fueled by combustible gas. When the temperature of the heated area reaches a point at which plastic deformation occurs, the pressure welding area becomes thicker and a so-called nodule is formed, completing the process.

[0003] In addition, in the pressure welding of steel materials, a reducing agent for gas pressure welding is often used to achieve stronger pressure welding. The reducing agent for gas pressure welding is used by sandwiching it between the end faces to be joined or by placing it near the end faces when two steel materials are opposed to each other and gas pressure welding is performed. For example, there is a "ring holding member with a built-in ring for gas pressure welding" as shown in Patent Document 1.

[0004] This ring holding member comprises a ring having approximately the same shape as the end face, made of approximately the same material as the steel, and having a gas vent portion; a holding container made of synthetic resin having a protrusion on the bottom side having a ring installation space in which the ring is stored and a convex portion connected to the protrusion and for attachment by contacting the outer shape of the steel; and a synthetic resin lid that fits over the ring installation space of the holding container and stops the rotation of the ring.

[0005] Conventional ring body holding members have this configuration, and by stopping the rotation of the ring body with a lid inside the holding container, the position of the gas vent section can be reliably set at a predetermined position, making it extremely easy and safe to set the ring body on the end of the steel material. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2011-177780 A Summary of the Invention [Problem to be solved by the invention]

[0007] However, because the holding container of this ring-shaped holding member is made of a thin sheet of synthetic resin and is lightweight overall, it may come off the tip of the steel material and be blown away by a sudden strong wind when working outdoors, etc. Or, when a worker works around the contact part of the steel material, he or she may accidentally get his or her gloves caught on the ring-shaped holding member and remove it.

[0008] Specifically, in the past, when using a ring-shaped holding member to press steel materials, the gap between the tip faces of the fixed steel material and the movable steel material was first set to a gap approximately equal to the height of the holding container of the ring-shaped holding member so that it could pass through. When setting the ring-shaped holding member, the ring-shaped holding member was inserted through the gap between the tip faces of the steel materials and attached to the tip of the fixed steel material, and the tip face of the movable steel material was brought close to the tip face of the fixed steel material by the hydraulic cylinder of the press machine in order to sandwich the circular top part of the ring-shaped holding member.

[0009] However, if the wind blows strongly at this timing, or if a worker touches it, the ring-holding member may come off the tip of the steel material and pass through a gap that is not yet narrow enough, causing it to fall or fly away. In this case, even after the ring-holding member passes through the gap, the movable steel material continues to move toward the fixed steel material, so even if an operation is performed to stop the steel material, in many cases its tip surface will come into contact with the tip surface of the fixed steel material, leaving no gap between the tip surfaces.

[0010] In order to reattach the ring-holding member to the tip of the fixed steel material, the movable steel material must be returned from the position where it abuts the tip face of the fixed steel material to its original position again, so that the ring-holding member can pass through the gap between the tip faces of the steel materials, and the steel material must be temporarily stopped in that position. This task of ensuring the gaps between the tip faces of the steel materials is a very time-consuming and troublesome task, especially when the gaps are large and the workload is heavy.

[0011] The present invention has been devised in consideration of the above points, and has as its object to provide a reducing material for gas pressure welding (corresponding to a ring-shaped holding member) that can be attached to the tip of a material to be pressure welded (corresponding to a steel material) when the gap between the tip faces of the materials to be pressure welded is narrow, a processing tool for the reducing material, and a gas pressure welding method. [Means for solving the problem]

[0012] [1] In order to achieve the above object, the present invention provides a reducing material for gas pressure welding, which has a cap body that can be fitted onto the tip of the material to be pressure welded, and the body of the cap body has an opening and closing portion that can be fitted into the material to be pressure welded from the side.

[0013] The reducing agent for gas pressure welding of the present invention includes a cap body, which can be fitted onto the tip of a material to be pressure welded such as a steel material. An opening and closing part is formed in the body of the cap body for fitting the reducing agent for gas pressure welding into the material to be pressure welded from the side.

[0014] The gas pressure welding reducing material has an opening and closing part, and when the opening and closing part is opened, an insertion opening part can be provided for fitting the cap body from the side into the pressure welded material, and when the gap between the tip faces of the pressure welded materials is narrow, the insertion opening part can be matched with the tip end of the pressure welded material to easily insert the cap body into the pressure welded material. Also, when the opening and closing part is closed after insertion, the cap body can be fixed to the pressure welded material.

[0015] [2] In the reducing material for gas pressure welding of the present invention, the body portion has a required number of side plates arranged in the circumferential direction of the top portion to form the body portion, and a predetermined one of the side plates can be deformed independently of the other side plates.

[0016] In this case, among the required number of side plates forming the body, a predetermined independently deformable side plate can be deformed forward or sideways to open it, and an insertion opening for fitting the pressure welded material from the side can be provided on the cap body. This allows the insertion opening to be aligned with the tip end of the pressure welded material and fitted laterally, with the gap between the tip ends of the pressure welded materials being narrow.

[0017] In addition, by pressing a certain side plate against the material to be pressure welded and deforming it toward the back, the fitting opening can be aligned with the tip of the material to be pressure welded and horizontal fitting can be performed. Furthermore, when the side plate is closed after fitting, it can be fixed to the material to be pressure welded.

[0018] [3] The reducing material for gas pressure welding of the present invention may be configured such that the body has four body legs formed in a cross shape from a sheet on the same plane and bent in the same direction at approximately the same length, and certain of the body legs formed in the circumferential direction of the top part are deformable.

[0019] In this case, of the four legs of the body formed in a cross shape from a sheet on the same plane, a predetermined deformable leg can be deformed forward or sideways to open it, and an inlet can be provided on the cap body for fitting the pressure welded material from the side. This allows the inlet to be aligned with the tip of the pressure welded material and fitted laterally when the gap between the tip faces of the pressure welded materials is narrow.

[0020] In addition, by pressing a certain leg part against the material to be pressure welded and deforming it toward the back, the fitting opening part can be aligned with the tip of the material to be pressure welded and horizontal fitting can be performed. Furthermore, if the leg part is closed after fitting, it can be fixed to the material to be pressure welded.

[0021] [4] In the reducing material for gas pressure welding of the present invention, the body portion has a required number of body leg portions that are divided by cut portions in the circumferential direction of the top portion and form the body portion, and the body leg portions can be configured to be deformable.

[0022] In this case, the cap body can be provided with a fitting opening for fitting the pressure welded material from the side by opening a required number of body legs that are divided by cuts in the circumferential direction of the top part and deforming them forward or backward to open them up. This allows the fitting opening to be aligned with the tip of the pressure welded material and fitted laterally when the gap between the tip faces of the pressure welded materials is narrow.

[0023] In addition, by pressing a certain leg part against the material to be pressure welded and deforming it toward the back, the fitting opening part can be aligned with the tip of the material to be pressure welded and horizontal fitting can be performed. Furthermore, if the leg part is closed after fitting, it can be fixed to the material to be pressure welded.

[0024] [5] In order to achieve the above object, the present invention provides a reducing material for gas pressure welding, which comprises a cap body that can be fitted onto the tip of the material to be pressure welded, the cap body having a top portion and a required number of leg portions arranged circumferentially around the top portion, and the spacing between at least one pair of adjacent leg portions is formed to be approximately the same as the diameter of the material to be pressure welded or larger than the diameter of the material to be pressure welded.

[0025] The reducing material for gas pressure welding of the present invention includes a cap body, which can be fitted onto the tip of the material to be pressure welded. The top part of the cap body and a required number of legs provided in the circumferential direction of the top part are formed so that the interval between at least one pair of adjacent legs is approximately the same as the diameter of the material to be pressure welded or is larger than the diameter of the material to be pressure welded, and the space between the legs forms an insertion opening for fitting into the material to be pressure welded from the side.

[0026] This allows the fitting opening to be aligned with the tip of the material to be pressure-welded and horizontal fitting to be performed while the gap between the tip faces of the materials to be pressure-welded is narrow. In addition, since the fitting opening does not need to be opened or closed when or after the gas pressure welding reducing material is attached, the troublesome part of the work is reduced and the work can be performed easily.

[0027] [6] In order to achieve the above object, the present invention provides a reducing material for gas pressure welding, which has a cap body that can be fitted onto the tip of the material to be pressure welded, and the body of the cap body is formed so that it can be fitted into the material to be pressure welded from the side by deforming its shape.

[0028] The reducing material for gas pressure welding of the present invention includes a cap body, and the cap body can be fitted onto the front end of the material to be pressure welded. In other words, since the shape of the body of the cap body is deformed, the top part of the cap body can be inserted into a gap in the front end surface of the material to be pressure welded while deforming the body, thereby allowing the cap body to be fitted into the material to be pressure welded from the side.

[0029] The part of the body that has been deformed during fitting can be returned to its original shape after fitting and fixed so that the tip surface is surrounded by the body, or it can be folded into the gap while still deformed. In this case, the folded part can be used as a reducing material, which is preferable.

[0030] [7] In order to achieve the above object, the present invention provides a reducing material for gas pressure welding, which has a cap body that can be fitted onto the tip of the material to be pressure welded, and the body of the cap body has an insertion port portion that can be fitted into the material to be pressure welded from the side.

[0031] The cap body can be fitted onto the tip of the material to be pressure welded. By appropriately setting the dimensions of the cap body, it is possible to maintain the state of being fitted even after the cap body is attached.

[0032] In addition, the body of the cap body is formed with an insertion opening that can be inserted into the material to be pressure welded from the side, so that even if the gap at the tip of the material to be pressure welded is narrow, the reducing material for gas pressure welding can be attached by being inserted into the material from the side. Even if the gap at the tip of the material to be pressure welded is wide, the reducing material can be attached to the tip of the material to be pressure welded and used as a reducing material.

[0033] The reducing material for gas pressure welding may be configured such that the fitting opening has a cut edge along the top of the cap body at a predetermined thickness and with a width that allows the material to be fitted from the side in the circumferential direction, and a cut edge is provided in the remaining thickness of the body, continuing from the cut edge, at a predetermined angle to the top or in a predetermined shape, all the way to the bottom end.

[0034] In this case, if the leading end surface (pressure welding surface) of each pressure-welded material is open at least as wide as the thickness of the top part of the cap body, the gas pressure welding reducing material can be attached to the leading end of the pressure-welded material by inserting the thickness of the top part into the gap in the leading end surface of each pressure-welded material and fitting the fitting opening formed by the cutting edge and continuing from the part along the top part to the bottom end into the side of the leading end of the pressure-welded material. In this case, the gas pressure welding reducing material can be attached by simply expanding the gap to a width equal to the thickness of the top part of the cap body, which is significantly thinner than the thickness of the entire cap body.

[0035] [8] In order to achieve the above object, the present invention provides a reducing material for gas pressure welding, which comprises a cap body that can be fitted onto the tip of the material to be pressure welded, and a detachable weakened line is provided in the body of the cap body so as to form an insertion port that can be fitted into the material to be pressure welded from the side.

[0036] The cap body can be fitted onto the tip of the pressure-welded side of the material to be pressure-welded. If the dimensions of the cap body are set appropriately, the cap body can be kept in that state even after it is attached.

[0037] In addition, the body of the cap body has a breakable weakened line that can be cut away to form an inlet that can be fitted into the side of the material to be welded, so that the inlet can be formed by cutting along the breakable line and removing the unnecessary part. As a result, the reducing material for gas pressure welding has an inlet in the body, unlike the original form, and can achieve the same effect as the reducing material for gas pressure welding described above in [7].

[0038] The reducing material for gas pressure welding may be configured so that the weakened line extends along the top of the cap body to a predetermined thickness and is of a width that enables the cap body to be fitted circumferentially from the side into the material to be pressure welded, and continues from there to the bottom end in the remaining thickness of the body, at a predetermined angle to the top or in a predetermined shape.

[0039] In this case, the weakened line is provided along the top of the cap body, with a width that allows it to be fitted circumferentially into the material to be welded at a specified thickness, and is continuous with the remaining thickness of the body so that an insertion opening can be formed that is cut out to the bottom end at a specified angle or in a specified shape relative to the top.

[0040] In this way, by cutting off the portion of a specified thickness along the top of the weakened line from the remaining thickness of the body and removing the unnecessary portion, an inlet can be formed from the portion along the top to the bottom end of the body. As a result, the reducing material for gas pressure welding has an inlet in the body, unlike the original form, and can achieve the same effects as the reducing material for gas pressure welding described above in [7].

[0041] The reducing material for gas pressure welding can also be configured so that the weakened line is approximately parallel to the top of the cap body, has a width that allows it to be fitted circumferentially from the side of the material to be pressure welded with a predetermined thickness, and is connected to the middle part and cut off to the bottom end to form an opening and closing portion that can open and close the body part, in an approximately T-shape.

[0042] In this case, the weakened line is arranged approximately parallel to the top of the cap body, with a width that allows it to be fitted circumferentially into the material to be welded at a predetermined thickness, and is connected to the middle part and cut off to the bottom end to form an opening and closing portion that can open and close the body part, in an approximately T-shape.

[0043] As a result, the reducing material for gas pressure welding is separated into a portion of a predetermined thickness parallel to the top of the weakened line and a portion that is connected to the middle part and can be separated down to the bottom end, and by opening the two opening and closing pieces formed outward or inward, an opening and closing portion can be formed from the portion along the top to the bottom end of the body, which differs from the original shape.

[0044] In the gas pressure welding method using this reducing material for gas pressure welding, the opening and closing piece is opened to form an opening and closing part in the cap body. Then, the thick part of the top part is inserted into the gap on the tip surface of the material to be pressure welded. As a result, the opening and closing part that continues from the part along the top part to the bottom end can be fitted into the side surface of the tip of the material to be pressure welded on the fixed side, so that the top part can be dropped into the tip of the material to be pressure welded to attach it.

[0045] The reducing material for gas pressure welding may be provided with a second cap body that can be fitted onto the tip of the material to be pressure welded, and the second cap body may be configured to be overlapped on the cap body in a state in which the body of the second cap body blocks at least a portion of the fitting opening portion.

[0046] In this case, the reducing material for gas pressure welding is provided with a second cap body that can be externally fitted onto the tip of the material to be pressure welded, and the second cap body is structured so as to be overlapped on the cap body in a state in which its body blocks at least a portion of the fitting opening portion.

[0047] First, the gas pressure welding reducing material is not used in a double structure when the end faces of the pressure-welded materials are narrower than the height of the cap body. When the gas pressure welding reducing material is placed on the end of the pressure-welded materials before the top part of the cap body of the gas pressure welding reducing material is sandwiched between the end faces of the pressure-welded materials, that is, when there is a wide gap between them, the gas pressure welding reducing material can be placed in a double structure. This makes it difficult for the gas pressure welding reducing material to come off the end of the pressure-welded materials due to the deep body of the second cap body, even if some wind blows before the top part of the cap body is sandwiched.

[0048] If the gas pressure welding reducing material does not come off before the top of the cap body of the gas pressure welding reducing material is sandwiched between the front end faces of the materials to be pressure welded, the sandwiched double-layered gas pressure welding reducing material can be used as a reducing material. In addition, since the top of the cap body of the gas pressure welding reducing material is also double-layered, a favorable effect as a reducing material can be expected.

[0049] In addition, if the gas pressure welding reducing material comes off before the top of the cap body of the gas pressure welding reducing material is sandwiched between the front end surface of each workpiece, the gas pressure welding reducing material having the fitting opening part in the cap body is removed from the second cap body of the removed gas pressure welding reducing material, and only this gas pressure welding reducing material is used as the reducing material. The action in this case is the same as that of the gas pressure welding reducing material described in [7] above, so that will be used here and the explanation will be omitted.

[0050] Furthermore, the second cap body can be used as a single gas pressure welding reducing material even after the gas pressure welding reducing material having an insertion opening in the cap body is removed, and can therefore be reused, for example, as a normal bottomed cylindrical (topped cylindrical in terms of posture) gas pressure welding reducing material or as a part of this double-structure gas pressure welding reducing material.

[0051] The gas pressure welding reducing material may be provided on the top portion of the cap body and may include a ring body made of resin, metal, or graphite that melts at a higher temperature than the material constituting the top portion.

[0052] In this case, a ring body made of resin, metal, or graphite is provided on the top of the cap body and melts at a higher temperature than the material that makes up the top, so that during the crimping operation, the top of the cap body first melts and burns when heated by the gas flame.

[0053] Then, in the small gap between the tip of the material to be welded and the inside of the ring, which has not yet melted, the top melts in a very short time, burns, and then vaporizes.Then, due to the sudden increase in volume, the air in the gap inside the ring is pushed out under high pressure, and the oxygen in the air combines with the carbon in the polymer to become carbon dioxide gas, suppressing the oxidation of the welded surface.

[0054] In addition, before the ring body melts, air is prevented from entering the gap inside the ring body, which in turn suppresses oxidation within the gap and prevents an oxide coating from forming on the tip surface of the pressure-welded side of the material to be pressure-welded.

[0055] In this way, when using natural gas, propane gas, hydrogen gas, or the like, which have a lower heating power than acetylene gas, to perform gas pressure welding of the materials to be pressure-welded, the reducing material for gas pressure welding can suppress the formation of residues such as oxide coatings and metal residues on the pressure welding portion, even if heating is performed with a standard flame from the initial heating stage so as to obtain sufficient heating power, making it possible to perform pressure welding with sufficient strength.

[0056] [9] The reducing material for gas pressure welding of the present invention may be configured so that a hole penetrating from the front to the back is formed at a predetermined position of the body portion.

[0057] In this case, by forming a hole penetrating from the front to the back at a specified location on the body, it is possible to reduce the amount of dripping when the cap body is heated and the occurrence of stains caused by the dripping and burning, making it easier to perform post-processing such as finishing (cleaning) the pressure-welded part.

[0058]

[10] The reducing material for gas pressure welding of the present invention may be configured so that a hook protruding inward is formed at a predetermined position of the body portion.

[0059] In this case, a hook portion that protrudes inward is formed at a specified location on the body, so that when the gas pressure welding reducing material is attached to the material to be pressure welded, the fixing force of the gas pressure welding reducing material to the material to be pressure welded is stronger, making it less likely to shift, and reducing the inconvenience of the material being blown away or displaced by the wind after attachment.

[0060]

[11] In order to achieve the above object, the present invention is a machining tool for processing the body of a cap body that can be fitted onto the tip of a material to be pressure-welded, and forming an opening / closing portion or an insertion port portion on the cap body that can be fitted onto the side of the material to be pressure-welded, the machining tool comprising: a base member having a receiving device; a seesaw member having one end that is spring-loaded to swing relative to the base member so as to close toward the base member; a cutting blade of a predetermined shape that is provided on the seesaw member and forms the opening / closing portion or the insertion port portion by making a slit or cutting into the cap body; and a blade groove provided on the receiving device into which the cutting blade fits.

[0061] The processing tool of the present invention opens one end of the seesaw member on which the cutting blade is provided, and closes the body of the cap body by using the biasing force of a spring between the receiver of the base member inserted inside the cap body and the one end of the seesaw member outside the body. As a result, the cutting blade makes a slit or cuts the body of the cap body to form an opening / closing part or an insertion opening part, and the cutting blade fits into the cutting groove.

[0062] In addition, if the cutting of the body is not sufficient, pressing the receiving tool of the base member and one end of the seesaw member in a direction in which they approach each other will allow the cutting blade to more reliably make a slit or cut the body and fit into the blade groove. This makes it possible to produce a reducing material for gas pressure welding in which the body of the cap body has a predetermined slit or fitting opening.

[0063]

[12] In order to achieve the above object, the present invention is a gas pressure welding method comprising the steps of: attaching a cap body having a height greater than the gap to a tip end face of one pressure welded material, the tip end face of which is arranged opposite to and separated by a predetermined gap, by fitting the cap body, having a height greater than the gap, from the side of the one pressure welded material so as to fit the cap body onto the tip end of the one pressure welded material; and, with the cap body attached, butting the tip ends of the one pressure welded material and the other pressure welded material together and heating them.

[0064] According to the gas pressure welding method of the present invention, a cap body having a height greater than the gap is fitted from the side of one of the pressure-welded materials, which is arranged facing the tip face of the other pressure-welded material with a specified gap between them.Therefore, even if the gap is narrower than the height of the cap body, it can be attached by externally fitting it onto the tip end of one of the pressure-welded materials.

[0065] As a result, for example, when re-attaching (re-attaching) the reducing material for gas pressure welding in the gaps on the tip faces of each pressure-welded material, there is no need to significantly widen the gaps on the tip faces of each pressure-welded material and make complicated adjustments.It is possible to attach the reducing material for gas pressure welding from the side of the pressure-welded material when the gap is narrow, which greatly reduces the complexity of the work and ultimately makes it easier to perform the gas pressure welding work.

[0066] By butting the leading edge of one material to be pressure-welded against the leading edge of the other material and heating them, it is possible to perform strong pressure welding while preventing the formation of an oxide film on the leading edge. That is, the top part of the cap body melts and burns in a very short time in the small gap between the leading edge of each material to be pressure-welded, and then vaporizes and its volume increases rapidly, pushing the air out with high pressure and the oxygen in the air combines with the carbon in the polymer to become carbon dioxide gas, thereby preventing the oxidation of the pressure-welded surface.

[0067] The gas pressure welding method may include a step of forming an insertion port in the body of the cap body prior to the attachment step so that the cap body can be inserted from a side surface of one of the materials to be pressure welded.

[0068] In this case, an insertion port is formed in the body of the cap body prior to the attachment process so that the cap body can be fitted from the side of one of the materials to be pressure-welded. Therefore, when the pressure welding operation is performed, it is possible to prepare a reducing material for gas pressure welding having a cap body which is equipped with an insertion port that is already adapted to the shape of the material to be pressure-welded, so that the pressure welding operation can be performed efficiently. Effect of the Invention

[0069] The present invention can provide a reducing material for gas pressure welding that can be attached to the tip portion of a material to be pressure welded when the gap between the tip surfaces of the materials to be pressure welded is narrow, a processing tool for the reducing material, and a gas pressure welding method. [Brief description of the drawings]

[0070] [Figure 1] FIG. 2 is an explanatory diagram showing an embodiment of Type A of the reducing material for gas pressure welding according to the present invention. [Diagram 2] FIG. 2 is an explanatory diagram showing an embodiment of Type B of the reducing material for gas pressure welding according to the present invention. [Diagram 3] FIG. 2 is an explanatory diagram showing an embodiment of Type C of the reducing material for gas pressure welding according to the present invention. [Figure 4] FIG. 2 is an explanatory diagram showing one method of mounting the reducing material for gas pressure welding according to an embodiment of Type A. [Diagram 5] FIG. 11 is an explanatory diagram showing one method of mounting the reducing material for gas pressure welding according to an embodiment of Type B. [Figure 6] FIG. 11 is an explanatory diagram showing one method of mounting the reducing material for gas pressure welding according to an embodiment of Type C. [Figure 7] FIG. 4 is an explanatory view showing another embodiment of the A-type reducing material for gas pressure welding. [Figure 8] FIG. 4 is an explanatory view showing still another embodiment of the A-type reducing material for gas pressure welding. [Figure 9] FIG. 4 is an explanatory view showing still another embodiment of the A-type reducing material for gas pressure welding. [Figure 10] FIG. 4 is an explanatory view showing another embodiment of the B type of the reducing material for gas pressure welding. [Figure 11] FIG. 2 is an explanatory diagram showing an embodiment of Type D of the reducing material for gas pressure welding according to the present invention. [Figure 12] FIG. 2 is an explanatory diagram showing an embodiment of an E-type reducing material for gas pressure welding according to the present invention. [Figure 13] FIG. 2 is an explanatory diagram showing an embodiment of an F-type reducing material for gas pressure welding according to the present invention. [Figure 14] FIG. 13 is an explanatory diagram showing one method of mounting the reducing material for gas pressure welding according to an embodiment of Type D. [Figure 15] FIG. 2 is an explanatory diagram showing one method of mounting an embodiment of the E-type reducing material for gas pressure welding. [Figure 16] FIG. 1 is an explanatory diagram showing a method of mounting an embodiment of an F-type reducing material for gas pressure welding. [Figure 17] FIG. 2 is an explanatory diagram showing a modified example of a reducing material for gas pressure welding, where (a) is a perspective view of the reducing material for gas pressure welding, and (b) is a sectional view of the reducing material for gas pressure welding taken along line AA. [Figure 18] 1A and 1B show an embodiment of a machining tool of the present invention, in which FIG. [Figure 19] 5A and 5B show a method of using the processing tool, where (a) is a cross-sectional explanatory view, and (b) is an explanatory view showing a cutting line in the cap body. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0071] First, an embodiment of the present invention will be described in detail with reference to Figures 1 to 10. In the following description of the reducing material for gas pressure welding, the reducing material will be divided into three types (A, B, and C). Type A is a substantially box-shaped material with a bottom, type B is a cylindrical material with a bottom and a body portion cut in the circumferential direction by slits, and type C is a material with multiple body legs provided in the circumferential direction of the top portion.

[0072] (Type A) The gas pressure welding reducing material A1 shown in Fig. 1(a) has a cap body 4a. The cap body 4a is made of a sheet of polystyrene resin, which is a thermoplastic resin. The cap body 4a has a square top plate 41 on the top part, and rectangular side plates of the same size that constitute the body part 40 are connected to the four sides of the top plate 41.

[0073] Of the side plates, the side plates 42 attached to three sides of the top plate 41 are connected to each other at their edges and integrated in the circumferential direction. Side plate 42a attached to the other side of the top plate 41 can deform and swing around the attachment edge (reference number omitted). The bottom end of each side plate 42, 42a is bent at a substantially right angle with a predetermined width to form a flange portion 420.

[0074] The reducing material A1 for gas pressure welding can open and close a portion of the body 40 by swinging the side plate 42a, and whether the side plate 42a extends outward or moves inward, an insertion opening portion (symbol omitted) can be formed for inserting the material to be pressure welded from the side.

[0075] The gas pressure welding reducing material A2 shown in Fig. 1(b) has a cap body 4b. The cap body 4b is made of a sheet made of polystyrene resin, which is a thermoplastic resin. The cap body 4b is formed by stacking two rectangular sheets of the same size at the center in the length direction, integrating them into a cross shape on the same plane, and bending them at a right angle at the same length in the same direction to form a body 45 consisting of four body legs 44 provided in the circumferential direction of a square top plate 43.

[0076] Each of the trunk legs 44 forming the trunk 45 can be deformed and swung. Each of the trunk legs 44 can be swung outward or inward to provide fitting openings for fitting the pressure-welded material from the side on all four sides in the circumferential direction of the cap body 4b. The bottom end of each of the trunk legs 44 is bent at a substantially right angle by a predetermined width to form a flange 440.

[0077] (action) Here, with reference to FIG. 1(b) and FIG. 4, a gas pressure welding method using the above-mentioned reducing material A2 for gas pressure welding, which is one of the A types, and its action will be described.

[0078] The cap body 4b of the reducing material A2 for gas pressure welding can be fitted onto the tip of the pressure welding side (pressure welding surface 910 side) of the material to be pressure welded 91 such as a steel material. The cap body 4b is made of a thermoplastic resin and has a predetermined shape retention and deformability (flexibility, etc.), so that it can be easily fitted onto the tip of the material to be pressure welded 91 and can maintain that state even after it is fitted.

[0079] The cap body can also be formed from other materials such as graphite (the same applies to the following gas pressure welding reducing materials A2, A3, A4, A5, gas pressure welding reducing materials B1, B2, B3, gas pressure welding reducing materials C1, C2, gas pressure welding reducing materials D1, D2, gas pressure welding reducing materials E1, E2, and gas pressure welding reducing material F).

[0080] In addition, the material to be welded 91 (and 92 described below) is made of steel such as deformed reinforcing bars, round bars, etc., and in addition to deformed reinforcing bars (SD295A, SD295B, SD345, SD390, SD490) specified in the steel bars for reinforced concrete (JIS G3112), round bars (SR235, SR295), or high-strength reinforcing bars (USD385A, USD385B, USD980) it is also possible to use stainless steel reinforcing bars (SUS316, SUS304, etc.) with improved durability and corrosion resistance.

[0081] When gas pressure welding of the pressure-welded materials 91, 92 is performed, first, the fixed pressure-welded material 91 is held vertically at a specified height by a fixed clamp (not shown). The movable pressure-welded material 92 is held vertically by a movable clamp (not shown). The pressure-welded materials 91, 92 are adjusted so that their center lines are on the same straight line, and the pressure-welded surfaces 910, 920 of the pressure-welded materials 91, 92 are set at an appropriate distance. Note that the pressure-welded materials 91, 92 may be held horizontally during the pressure welding operation.

[0082] When the cap body 4b of the reducing material A2 for gas pressure welding is attached, the body leg portion 44 close to the material to be pressure welded 91 is moved inward (or outward in some cases) to open the fitting opening. If the pressure contact surfaces 910, 920 of the materials to be pressure welded 91, 92 are opened at least to the same extent as the thickness of the top plate 43 of the cap body 4b, the cap body 4b can be attached to the tip of the material to be pressure welded 91 on the fixed side.

[0083] That is, first, the thickness portion of the top plate 43 is inserted horizontally into the gap 900 between the pressure-welded surfaces 910, 920 of the materials to be pressure-welded 91, 92. Note that the top plate 43 may be inserted at an angle rather than horizontally. Accordingly, the fitting opening is fitted into the side surface of the tip of the material to be pressure-welded 91 on the fixed side, so that by aligning the top plate 43 with the pressure-welded surface 910, it can be attached to the tip of the material to be pressure-welded 91 (see FIG. 4).

[0084] With the reducing material A2 for gas pressure welding attached as described above, the material to be pressure-welded 92 is lowered and the top plate 43 of the cap body 4b is sandwiched between the pressure-welded surfaces 910, 920. Then, by heating the materials to be pressure-welded 92 together with the materials to be pressure-welded 91, 92 by the gas flame, it is possible to perform strong pressure welding while preventing the formation of an oxide film on the pressure-welded surfaces 910, 920.

[0085] In other words, the top plate 43 of the cap body 4b, which is made of a thermoplastic resin, melts, burns, and vaporizes in a very short time in the small gap between the pressure contact surfaces 910, 920 of each of the materials to be pressure-welded 91, 92, causing a sudden increase in volume. As a result, the air is pushed outward at high pressure, and the oxygen in the air combines with the carbon in the polymer to become carbon dioxide gas, thereby suppressing oxidation of the pressure contact surfaces.

[0086] Furthermore, when the reducing material A2 for gas pressure welding comes off before closing the pressure welding surfaces 910, 920 of the materials to be pressure welded, for example, it is necessary to reinstall the reducing material A2 for gas pressure welding. However, even in this case, there is no need to make complicated adjustments by significantly widening the gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 (see FIG. 4).

[0087] If the reducing material for gas pressure welding does not have an inlet portion on the cap body, in order to insert the reducing material for gas pressure welding into the gap, it must be adjusted to be higher than the pressure welding surface 910 shown in Fig. 4 by h (see Fig. 14(b) described later). The task of ensuring a gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 is a very time-consuming and tedious task, and particularly involves a large workload.

[0088] In contrast, the gas pressure welding reducing material A2 can be attached as described above simply by spreading it into a gap of the same width as the thickness of the top plate 43 of the cap body 4b, which is significantly thinner than the entire thickness of the cap body 4b.

[0089] This greatly reduces the complexity of the work, and as a result, the gas pressure welding work can be easily performed. When the reducing material A2 for gas pressure welding is attached to the material to be pressure welded 91, the material to be pressure welded 91 is sandwiched between the side plates 42 on both sides, so that the reducing material A2 for gas pressure welding has excellent holding power to prevent it from coming off.

[0090] In the case of the gas pressure welding reducing material A1, the side plate 42a is opened toward the front or rear to form an insertion opening for lateral insertion, or the side plate 42a is pressed against the reinforcing bar to push the side plate 42a toward the rear, forming an insertion opening for lateral insertion.

[0091] (Type B) The reducing material for gas pressure welding B1 shown in Fig. 2(a) has a cap body 5a. The cap body 5a is made of a sheet made of polystyrene resin, which is a thermoplastic resin. The cap body 5a has a circular top plate 51, and a substantially cylindrical body part 50 is provided at the same height around the entire periphery of the top plate 51.

[0092] The trunk 50 is provided with a predetermined width around its entire circumference, and cuts 500 are made in the vertical direction, leaving a portion of the original end, to form the required number of trunk legs 52. A flange 520 is provided at the tip of each trunk leg 52. This allows each trunk leg 52 to be deformed independently.

[0093] (action) Here, with reference to FIG. 2(a) and FIG. 5, a gas pressure welding method using the above-mentioned reducing material for gas pressure welding B1, which is one of the B types, and its action will be described.

[0094] The cap body 5a of the reducing material for gas pressure welding B1 can be fitted onto the tip of the pressure welding side (pressure welding surface 910 side) of the material to be pressure welded 91 such as a steel material. The cap body 5a is made of a thermoplastic resin and has a predetermined shape retention and deformability, so that it can be easily fitted onto the tip of the material to be pressure welded 91 and can maintain that state even after it is fitted.

[0095] When mounting the cap body 5a of the reducing material for gas pressure welding B1, the trunk leg portion 52 close to the material to be pressure welded 91 is pressed against the material to be pressure welded to deform it inwardly and open the fitting opening (note that the trunk leg portion 52 may be manually adjusted). If the pressure contact surfaces 910, 920 of the materials to be pressure welded 91, 92 open to an extent at least slightly larger than the thickness of the top plate 51 of the cap body 5a, mounting is possible on the tip of the material to be pressure welded 91 on the fixed side.

[0096] Then, the thick portion of the top plate 51 is inserted horizontally into the gap 900 between the pressure-welded surfaces 910, 920 of the materials to be pressure-welded 91, 92. Accordingly, the fitting opening portion fits into the side surface of the tip of the material to be pressure-welded 91 on the fixed side, so that by aligning the top plate 51 with the pressure-welded surface 910, it can be attached to the tip of the material to be pressure-welded 91 (see FIG. 5).

[0097] With the reducing material B1 for gas pressure welding attached as described above, the material to be pressure-welded 92 is lowered and the top plate 51 of the cap body 5a is sandwiched between the pressure-welded surfaces 910, 920. Then, by being heated by the gas flame together with the materials to be pressure-welded 91, 92, the formation of an oxide film on the pressure-welded surfaces 910, 920 is prevented, and the materials to be pressure-welded 91, 92 can be firmly pressure-welded in the same manner as when the reducing material A2 for gas pressure welding is used.

[0098] Furthermore, when the reducing material B1 for gas pressure welding comes off before the pressure welding surfaces 910, 920 of the materials to be pressure welded are closed, it is necessary to reattach the reducing material B1 for gas pressure welding, but even in this case, there is no need to make complicated adjustments by greatly widening the gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 (see FIG. 5). This reduces the workload in such cases, and as a result, the gas pressure welding work can be performed easily.

[0099] The gas pressure welding reducing material B2 shown in Fig. 2(b) has a cap body 5b. The cap body 5b is made of a sheet of polystyrene resin, which is a thermoplastic resin. The cap body 5b has a circular top plate 51, and a substantially cylindrical body part 53 is provided at the same height around the entire periphery of the top plate 51.

[0100] Furthermore, a slit 500 is made in the body 53 in the vertical direction at one location in the circumferential direction, leaving a portion of the original end, and the body leg portion 54 is divided into two. A flange portion 540 is provided at the tip of the body leg portion 54, which extends over substantially the entire circumference. This allows the portions of each body leg portion 54 that sandwich the slit 500 to deform independently.

[0101] When the gas pressure welding reducing material B2 is attached to the material to be pressure welded 91, unlike the gas pressure welding reducing material B1, the body leg portion 52 is not deformed inward, but rather both sides of the cut 500 in the body leg portion 54 are opened and deformed outward so that the top plate 51 can be inserted into the gap 900.

[0102] As another method, the reducing agent B2 forcibly fits in from the slit 500 (for example, the two faces on either side of the slit 500 are deformed in the front-to-rear direction, and the reducing agent B2 is forced into the reinforcing bar through the gap (the gap created by the front-to-rear deformation) between them). Other than this, the reducing agent B2 for gas pressure welding can be used in substantially the same way as the reducing agent B1 for gas pressure welding, and therefore a description of the operation thereof will be omitted here.

[0103] (C type) The gas pressure welding reducing material C1 shown in Fig. 3(a) has a cap body 6a. The cap body 6a is made of a sheet of polystyrene resin, which is a thermoplastic resin. The cap body 6a has a circular top plate 61. A skirt portion 62 is provided on the outer periphery of the top plate 61, with the same width, over the entire circumference. The skirt portion 62 has three body legs 64 provided in the circumferential direction.

[0104] Of the body legs 64, a pair of adjacent opposing body legs 64 are provided approximately on the diameter line of the top plate 61 and at a right angle to the top plate 61. The remaining body leg 64 is provided parallel to the circumferential middle portion of the other opposing body leg 64. The tip of each body leg 64 forms a flange portion 640.

[0105] The distance between the opposing legs 64, 64 is set to be approximately the same as the diameter of the material 91 to be pressure welded or larger than the diameter of the material 91 to be pressure welded. As a result, an insertion opening 65 is formed on the front side between the legs 64, 64.

[0106] (action) Here, with reference to FIG. 3(a) and FIG. 6, a gas pressure welding method using the above-mentioned reducing material for gas pressure welding C1, which is one of the C types, and its action will be described.

[0107] The cap body 6a of the reducing material for gas pressure welding C1 can be fitted onto the tip of the pressure welding side (pressure welding surface 910 side) of the material to be pressure welded 91 such as a steel material. The cap body 6a is made of a thermoplastic resin and has a predetermined shape retention and deformability, so that it can be easily fitted onto the tip of the material to be pressure welded 91 and can maintain that state even after it is fitted.

[0108] If the pressure-welded surfaces 910, 920 of the materials to be pressure-welded 91, 92 are open to an extent at least slightly larger than the thickness of the top plate 51 of the cap body 5a, the cap body 6a of the reducing agent for gas pressure welding C1 can be attached to the tip of the material to be pressure-welded on the fixed side 91. When the cap body 6a is attached, the fitting opening 65 between the opposing body legs 64, 64 is aligned with the tip of the material to be pressure-welded 91, and the thickness portion of the top plate 61 is inserted horizontally into the gap 900 between the pressure-welded surfaces 910, 920 of the materials to be pressure-welded 91, 92.

[0109] As a result, the fitting opening 65 fits into the side of the tip of the fixed side pressure-welded material 91, so that by aligning the top plate 61 with the pressure-welding surface 910, it can be attached to the tip of the pressure-welded material 91 (see Figure 6).Furthermore, with the gas pressure welding reducing material C1 attached as described above, the pressure-welded material 92 is lowered and the top plate 61 of the cap body 6a is sandwiched between the pressure-welding surfaces 910, 920.

[0110] By heating each of the pressure-welded materials 91, 92 with a gas flame, the formation of an oxide film on the pressure-welded surfaces 910, 920 is prevented, while the pressure-welded materials 91, 92 can be firmly pressure-welded, as in the case where the above-mentioned gas pressure welding reducing material A2 is used.

[0111] Furthermore, when the reducing material C1 for gas pressure welding comes off before the pressure welding surfaces 910, 920 of the pressure-welded materials are closed, the reducing material C1 for gas pressure welding must be reattached, but even in this case, there is no need to make complicated adjustments by greatly widening the gap between the pressure welding surfaces 910, 920 of the pressure-welded materials 91, 92 (see FIG. 6). This reduces the workload in such cases, and as a result, the gas pressure welding work can be performed easily.

[0112] The gas pressure welding reducing material C2 shown in FIG. 3(b) has a cap body 6b. The cap body 6b is made of a sheet of polystyrene resin, which is a thermoplastic resin. The cap body 6b has a circular top plate 61. A bottom portion 62 is provided on the outer periphery of the top plate 61, with the same width, over the entire circumference. The bottom portion 62 has three legs 63 provided at equal intervals in the circumferential direction of the top plate 61. Each of the legs 63 is provided at a right angle to the top plate 61. The tip of each of the legs 63 forms a flange portion 630.

[0113] Since the circumferential distance between each of the legs 63 is slightly narrower than the diameter of the material to be welded 91, it is necessary to deform one of the legs 63 when attaching it to the tip of the material to be welded 91. In more detail, the left and right legs 63 may be bent backwards and placed between the pressure contact surfaces 910, 920, or may be simply expanded horizontally to about the insertion opening 65.

[0114] Also, the worker may open the body leg parts 63 toward the front or rear to form an insertion opening, or may push them apart horizontally to form an insertion opening and then fit them laterally, or the worker may press the gaps between the body leg parts 63 against the reinforcing bar and push the body leg parts 63 apart horizontally to fit them laterally. Except for this, the reducing material for gas pressure welding C2 can be used in substantially the same way as the reducing material for gas pressure welding C1, so a description of its operation will be omitted here.

[0115] (Another example of Type A) The gas pressure welding reducing material A3 shown in Fig. 7 has a cap body 4c. The cap body 4c is made of a sheet of polystyrene resin, which is a thermoplastic resin. The cap body 4c has a square top plate 46 on the top part, and rectangular side plates of the same size that constitute the body part 40 are connected to the four sides of the top plate 46.

[0116] Of the side plates, the side plates 47 attached to three sides of the top plate 46 are connected to each other at their edges and integrated in the circumferential direction. The side plate 47a attached to the other side of the top plate 46 can deform and swing around the attachment edge (reference number omitted). The bottom end of each side plate 47, 47a is bent at a substantially right angle with a predetermined width to form a flange portion 470.

[0117] 7, the side plate 47a of the two left and right side plates 47 has three hooks 471 at equal intervals, which are formed by cutting two right-angled sides of a right triangle and adding creases connecting the tips of the two sides. As a result, the hooks 471 are bent inward to protrude, so that when the plate is attached, they hook onto the surface of the material to be welded 91 inside and can be fixed in place to prevent it from slipping.

[0118] A pressing plate 472 is provided over the entire length of the end portion of the side plate 47a of the two left and right side plates 47. Furthermore, a circular hole 48 is provided in the center of the side plate 47a, penetrating from the front to the back.

[0119] The reducing material A3 for gas pressure welding can open and close a portion of the body 40 by swinging the side plate 47a, and the side plate 47a can be inserted inward to form an insertion opening portion (symbol omitted) for fitting the material to be pressure welded from the side.

[0120] The side plate 47a is prevented from moving outward by pressing plates 472 on both sides. The function of the reducing material A3 for gas pressure welding after it is attached to the material to be pressure welded 91 is the same as that of the reducing material A1 for gas pressure welding described above, and therefore a description thereof will be omitted here.

[0121] 8 is similar to the reducing material A3 for gas pressure welding in that it has a cap body 4d, which has a top plate 46 and side plates 47, 47a and is formed into a box shape with a bottom. In the reducing material A4 for gas pressure welding, each of the three side plates 47 is provided with a substantially triangular hook portion 473 that is connected in a circular direction and has four substantially circular folds.

[0122] The side plate 47a is prevented from moving outward by pressing plates 472 on both sides. The function of the reducing material A4 for gas pressure welding after it is attached to the material to be pressure welded 91 is the same as that of the reducing material A1 for gas pressure welding described above, and therefore a description thereof will be omitted here.

[0123] 9 is similar to the reducing material A3 for gas pressure welding in that it has a cap body 4e, which has a top plate 46 and side plates 47, 47a and is formed into a box shape with a bottom. In the reducing material A5 for gas pressure welding, the two left and right side plates 47 are each provided with a substantially triangular hook portion 49 that is connected in a circular direction and has a substantially circular fold at one location in the center.

[0124] The side plates 47a are provided at two locations, front and rear, and each side plate 47a is provided with a through hole 48 at the center. Each side plate 47a is prevented from moving outward by pressing plates 472 on both sides. The function of the gas pressure welding reducing material A5 after it is attached to the pressure welded material 91 is the same as that of the gas pressure welding reducing material A1 described above, and therefore a description thereof will be omitted here.

[0125] (Another example of Type B) The reducing material for gas pressure welding B3 shown in Fig. 10 has a cap body 5c. The cap body 5c is made of a sheet made of polystyrene resin, which is a plastic resin. The cap body 5c has a circular top plate 51, and a substantially cylindrical body part 57 is provided at the same height around the entire periphery of the top plate 51.

[0126] The trunk 57 has a predetermined width around its entire circumference, and cuts 500 are made in the vertical direction, leaving a portion of the original end, to form four trunk legs 55. A roughly triangular hook 56 is provided in the center of each trunk leg 55, with a roughly circular fold at one location, and the hooks are connected in the circular direction. A flange 550 is provided at the tip of each trunk leg 55. This allows each trunk leg 55 to be deformed independently.

[0127] The body legs 55 are provided at four locations in the circumferential direction, and two locations are deformed to fit and attach to the pressure welded material 91. Furthermore, when the gas pressure welding reducing material B3 is attached to the pressure welded material 91, by having the engaging portions 56 protrude inward, it is possible to prevent the gas pressure welding reducing material B3 from shifting, similarly to the above-mentioned gas pressure welding reducing materials A3, A4, and A5. Furthermore, the action of the gas pressure welding reducing material B3 after attachment to the pressure welded material 91 is similar to that of the above-mentioned gas pressure welding reducing material B1, and therefore a description thereof will be omitted here.

[0128] In addition, although not shown in the figures, the reducing material for gas pressure welding of the present invention is provided with a cap body that can be fitted onto the tip of the material to be pressure welded 91, and a structure can also be adopted in which the body of the cap body is formed so that it can be fitted into the material to be pressure welded from the side by deforming its shape.

[0129] This reducing material for gas pressure welding has a body of a cap body which is formed, for example, from a material which is extremely soft and has sufficient strength and which is easily deformed. Therefore, by deforming the body and inserting and fitting the top part into the gap 900 between the tip surfaces 910, 920 of the pressure welding materials 91, 92, it is possible to fit the top part into the pressure welding materials 91, 92 from the side.

[0130] The deformed portion of the body during fitting can be returned to its original shape after fitting and fixed so that the tip end face is surrounded by the body, or it can be folded into the gap while still deformed. In this case, the folded portion can be used as a reducing material, which is preferable.

[0131] Next, an embodiment of the present invention will be described in detail with reference to Figures 11 to 19. In the following description of the reducing material for gas pressure welding, the reducing material will be further divided into three types (D, E, and F). Type D is a material with a pre-installed fitting portion, type E is a material with a weakened line so that the fitting portion and the opening and closing portion can be formed, and type F is a material with a pre-installed fitting portion and a cylindrical cap body with a bottom layered on top of it.

[0132] (D type) The reducing material for gas pressure welding D1 shown in Fig. 11(a) has a cap body 1a. The cap body 1a is made of a sheet made of polystyrene resin, which is a thermoplastic resin. The body 10 (tubular part) of the cap body 1a is processed based on a cylindrical shape that is slightly flared at the bottom, and the upper end in Fig. 11(a) is closed by a circular top plate 11.

[0133] Furthermore, a cutting edge 120 is provided in the body 10 in the circumferential direction along the top plate 11 to a predetermined thickness, with a width that allows it to be fitted into a material to be welded 91 (see Figures 14 to 16) described below. The thickened portion formed by the cutting edge 120 and the top plate 11 has a partially cylindrical shape, and this portion also serves as a fitting portion 121 that prevents the material to be welded 91 from falling off when it is fitted onto the tip of the material to be welded.

[0134] Continuing from both ends of the cut edge 120, cut edges 122, 123 are provided in the remaining thickness (height) portion of the body 10 in a direction approximately perpendicular to the top plate 11, forming a U-shaped fitting opening 12. A flange 13 with a slightly larger diameter is provided along the entire length of the bottom of the cap body 1a.

[0135] In the present embodiment, the central angle between the cutting edges 122 and 123 of the reducing material for gas pressure welding D1 in a plan view (the opening angle of the fitting opening 12) is 150°, but is not limited to this. The central angle is sufficient if at least the cutting edge portion of the fitting opening 12 can be fitted into the material to be pressure welded 91, and is preferably an angle smaller than 180° so that the fitted state can be maintained after fitting (see FIG. 11(b)).

[0136] The gas pressure welding reducing material D2 shown in Fig. 11(c) has a cap body 1c. The cap body 1c is made of a sheet made of polystyrene resin, which is a thermoplastic resin. The body 10c of the cap body 1c is processed based on a cylindrical shape that is slightly flared at the bottom, and the upper end is closed by a circular top plate 11 in Fig. 11(c).

[0137] Furthermore, in the trunk portion 10c, a cutting edge 124 is provided in the circumferential direction along the top plate 11 to a predetermined thickness, with a width that allows it to be fitted into the pressure-welded material 91 described below. The thickened portion formed by the cutting edge 124 and the top plate 11 has a partially cylindrical shape, and this portion also serves as a fitting portion 125 that prevents the pressure-welded material 91 from falling off when it is fitted onto the tip of the pressure-welded material 91.

[0138] Then, continuing from both ends of the cut edge 124, approximately S-shaped cut edges 126, 127 are provided in the remaining thickness (height) portion of the body portion 10c, which are symmetrical with respect to the top plate 11, to form the fitting opening portion 12c. A flange portion 13 with a slightly larger diameter is provided along the entire length at the bottom of the cap body 1c. The approximately S-shaped cut edges 126, 127 are each structured so that the side closer to the bottom protrudes in a direction narrowing the fitting opening portion 12c, forming holding portions 128, 129.

[0139] (action) Here, with reference to FIG. 11(a) and FIG. 14, a gas pressure welding method using the above-mentioned reducing material D1 for gas pressure welding, which is one of the D types, and its operation will be described.

[0140] The cap body 1a of the reducing material for gas pressure welding D1 can be fitted onto the tip of the pressure welding side (pressure welding surface 910 side) of the material to be pressure welded 91. The cap body 1a is made of a thermoplastic resin and has a predetermined shape retention and deformability, so that it can be easily attached by fitting onto the tip of the material to be pressure welded 91 and can maintain that state even after attachment.

[0141] When gas pressure welding the pressure-welded materials 91, 92, first, the fixed pressure-welded material 91 is held vertically at a specified height by a fixed clamp (not shown). The movable pressure-welded material 92 is held vertically by a movable clamp (not shown). The pressure-welded materials 91, 92 are adjusted so that their center lines are on the same line, and the pressure-welded surfaces 910, 920 of the pressure-welded materials 91, 92 are set at an appropriate distance. The pressure-welded materials 91, 92 may be held horizontally during the pressure welding operation.

[0142] The cap body 1a of the reducing material D1 for gas pressure welding has an insertion opening 12 formed at the cut edge of the body 10 from the portion along the top plate 11 to the bottom end, so that as long as the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 are open at least to the same extent as the thickness of the top of the cap body 1a, it can be attached to the tip of the fixed side material to be pressure welded 91.

[0143] That is, first, the thickness of the top part is inserted horizontally into the gap between the pressure contact surfaces 910, 920 of the pressure-welded materials 91, 92. The top part may be inserted at an angle or in an inclined direction instead of horizontally. Accordingly, the fitting mouth part 12 continuing from the part along the top part to the bottom end is fitted into the side surface of the tip part of the pressure-welded material 91 on the fixed side, so that the top part can be attached to the tip part of the pressure-welded material 91 by dropping it into the pressure contact surface 910 (see FIG. 14(a)). Note that this fitting by dropping may be performed not only when the pressure contact surface 910 is located above the fitting mouth part 12 (closer to the top part than the fitting mouth part 12 or at the top part), but also when it is located below the fitting mouth part 12.

[0144] With the reducing material D1 for gas pressure welding attached as described above, the material to be pressure-welded 92 is lowered and the top plate 11 of the cap body 1a is sandwiched between the pressure-welded surfaces 910, 920. Then, by heating the materials to be pressure-welded 92 together with the materials to be pressure-welded 91, 92 by the gas flame, it is possible to perform strong pressure welding while preventing the formation of an oxide film on the pressure-welded surfaces 910, 920.

[0145] In other words, the top of the thermoplastic resin cap body melts and burns in a very short time in the small gap between the tip faces of the materials to be pressed, and then vaporizes, causing a sudden increase in volume. As a result, the air is pushed outward at high pressure, and the oxygen in the air combines with the carbon in the polymer to become carbon dioxide, suppressing oxidation of the pressing surfaces.

[0146] Furthermore, with the reducing material D1 for gas pressure welding, if the reducing material D1 for gas pressure welding comes off before closing the pressure welding surfaces 910, 920 of the materials to be pressure welded, for example, it is necessary to reinstall the reducing material D1 for gas pressure welding. However, even in this case, there is no need to make complicated adjustments by greatly widening the gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 (see Figure 14(a)).

[0147] If the cap body does not have an inlet portion, as in the case of the reducing material D for gas pressure welding shown in Fig. 14(b), in order to insert the reducing material D for gas pressure welding into the gap, it must be adjusted to be at least a height h higher than the pressure welding surface 910 shown in Fig. 14(a). The task of ensuring a gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 is a very time-consuming and tedious task, and the workload is particularly heavy when the gap is large.

[0148] In contrast, the reducing material D1 for gas pressure welding can be attached as described above by simply spreading it over a gap as wide as the thickness of the top part of the cap body 1a, which is significantly thinner than the overall thickness of the cap body 1a. This significantly reduces the complexity of the work, and as a result, the gas pressure welding work can be easily performed.

[0149] When the reducing material for gas pressure welding D2 is attached to the material to be pressure welded 91, the holding parts 128, 129 grip the material to be pressure welded 91 in a slightly wraparound manner, providing excellent holding power to prevent the reducing material for gas pressure welding D2 from coming off. Other than that, the action of the reducing material for gas pressure welding D2 is the same as that of the reducing material for gas pressure welding D1 described above, and therefore a description thereof will be omitted here.

[0150] (E type) The gas pressure welding reducing material E1 shown in Fig. 12(a) has a cap body 2a. The cap body 2a is made of a sheet made of polystyrene resin, which is a thermoplastic resin. The body 20a of the cap body 2a has a cylindrical shape that is slightly flared at the bottom, and the upper end in Fig. 12(a) is closed by a circular top plate 21.

[0151] The body 20a is provided with a weakened line 22a that can be torn off. The weakened line 22a has perforations 220 of a width that allows the pressure-welded material 91 to be fitted into the pressure-welded material in the circumferential direction to a predetermined thickness along the top plate 21. The thick portion formed by the perforations 220 and the top plate 21 has a partially cylindrical shape, and this portion also becomes a fitting portion 221 that prevents the pressure-welded material 91 from falling off when it is fitted onto the tip of the pressure-welded material 91 after the separation piece 200 described later is separated.

[0152] Then, continuing from both ends of the perforation 220, perforations 222, 223 are formed in a U-shape in the remaining thickness (height) portion of the body portion 20a in a direction approximately perpendicular to the top plate 21 to the bottom end. Circular holes 229 are provided at both corners of the perforation 220 to prevent excessive cutting when separating. The holes 229 may be of other shapes, such as a rectangle.

[0153] In addition, a flange portion 23a having a slightly larger diameter is provided around the entire circumference of the bottom of the cap body 2a. By cutting along the perforations 220, 222, and 223, the separation piece 200 can be separated to form an insertion port similar to the insertion port 12 of the gas pressure welding reducing material D1.

[0154] The gas pressure welding reducing material E2 shown in Fig. 12(b) has a cap body 2b. The cap body 2b is made of a sheet made of polystyrene resin, which is a thermoplastic resin. The body 20b of the cap body 2b has a cylindrical shape that is slightly flared at the bottom, and the upper end in Fig. 12(b) is closed by a circular top plate 21.

[0155] The body 20b is provided with a weakened line 22b that can be torn off. The weakened line 22b has a perforation 224 in the circumferential direction along the top plate 21 to a predetermined thickness, with a width that allows the pressure-welded material 91 to be fitted therein. A perforation 225 is provided in the remaining thickness (height) of the body 20b, continuing from the middle of the perforation 224, in a direction approximately perpendicular to the top plate 21 to the bottom end, forming an approximately T-shape.

[0156] Then, when it is cut apart at the perforations 224, 225, opening and closing pieces 226, 227 can be formed, and the thick portion formed by the perforations 224 and the top plate 21 has a partially cylindrical shape. This portion becomes a fitting portion 228 that prevents the pressure-welded material 91 from falling off when it is fitted onto the tip of the pressure-welded material 91.

[0157] In addition, a flange portion 23b having a slightly larger diameter is provided around the entire periphery of the bottom of the cap body 2b. By cutting along perforations 224 and 225, opening / closing pieces 226 and 227 can be made openable and closable, and an opening / closing portion (not shown) can be formed by opening the opening / closing pieces 226 and 227.

[0158] In this embodiment, perforations are used as the lines of weakness, but this is not limited to this and any other structure that can be easily torn by hand, such as a structure with short intermittent linear slits or a structure with a very thin sheet arranged in a linear pattern, will do.

[0159] (action) Here, with reference to FIG. 12(a) and FIG. 15, a gas pressure welding method using the above-mentioned reducing material for gas pressure welding E1, which is one of the E types, and its operation will be described.

[0160] The cap body 2a of the reducing material E1 for gas pressure welding can be fitted onto the tip of the pressure welding side (pressure welding surface 910 side) of the material to be pressure welded 91. The cap body 2a is made of a thermoplastic resin and has a predetermined shape retention and deformability, so that it can be easily fitted onto the tip of the material to be pressure welded 91 and can maintain that state even after it is fitted.

[0161] When gas pressure welding of the materials to be pressure-welded 91, 92 is performed, the fixed material to be pressure-welded 91 and the movable material to be pressure-welded 92 are set in the same manner as in the case of the pressure welding work using the reducing material for gas pressure welding D1. Then, for example, when it becomes necessary to attach the reducing material for gas pressure welding E1 again, the cap body 2a is cut along the perforations 220, 222, 223 to separate the cut-off piece 200, which is the unnecessary part, and the reducing material for gas pressure welding E11 having the fitting opening portion 24 (see FIG. 15) can be produced.

[0162] The method of use and action of the reducing material E11 for gas pressure welding after the fitting opening 24 is formed in the cap body 2a are the same as those of the reducing material D1 for gas pressure welding. Note that if the reducing material E1 for gas pressure welding comes off before closing the pressure welding surfaces 910, 920 of the pressure-welded materials, it is necessary to reattach the reducing material E1 for gas pressure welding.

[0163] In this case, there is no need to adjust the gap between the pressure-welded surfaces 910, 920 of the materials to be pressure-welded 91, 92 by widening it significantly. Just by widening the gap to a width equivalent to the thickness of the top part of the cap body 2a, which is significantly thinner than the overall thickness of the cap body 2a, the reducing material E1 for gas pressure welding can be attached, just like the reducing material D1 for gas pressure welding described above.

[0164] In the case of the reducing material E2 for gas pressure welding, for example, when it becomes necessary to attach the reducing material E2 for gas pressure welding again after the materials to be pressure welded 91, 92 are set, the cap body 2b can be cut at the perforations 224, 225 to deform the opening / closing pieces 226, 227 inward and outward to make it openable and closable. This makes it possible to produce a reducing material for gas pressure welding (not shown) that can form an opening / closing portion (not shown) by opening the opening / closing pieces 226, 227.

[0165] In the gas pressure welding method using the reducing material E2 for gas pressure welding, the opening and closing pieces 226, 227 are opened to form an opening and closing portion in the cap body 2b. Then, the thick portion of the top portion is inserted into the gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92. Accordingly, the opening and closing portion continuing from the portion along the top portion to the bottom end is fitted into the side surface of the tip of the material to be pressure welded 91 on the fixed side, so that the top portion can be attached to the tip of the material to be pressure welded 91 by dropping it into the pressure welding surface 910.

[0166] In addition, if the reducing material E2 for gas pressure welding comes off before closing the pressure welding surfaces 910, 920 of the pressure-welded materials, it is necessary to reattach the reducing material E2 for gas pressure welding. In this case, there is no need to adjust the gap between the pressure welding surfaces 910, 920 of the pressure-welded materials 91, 92 by significantly widening it, and the reducing material E2 for gas pressure welding can be attached just by widening the gap to a width equivalent to the thickness of the top part of the cap body 2b, which is significantly thinner than the thickness of the entire cap body 2b, in the same manner as the reducing material D1 for gas pressure welding described above.

[0167] (F type) The reducing material F for gas pressure welding shown in Fig. 13 is configured by combining a reducing material F11 for gas pressure welding having a structure similar to that of the reducing material D1 for gas pressure welding (the cap body has an inlet portion) and a reducing material F12 for gas pressure welding having a second cap body having a bottomed cylindrical shape and a structure substantially similar to that of the reducing material E1 for gas pressure welding and no weakened line 22a. Note that explanations of the respective structures of the reducing material F11 for gas pressure welding and the reducing material F12 for gas pressure welding are omitted here.

[0168] In this embodiment, the reducing material for gas pressure welding F has a double structure in which a reducing material for gas pressure welding F12 is covered with a reducing material for gas pressure welding F11. The reducing material for gas pressure welding F11 is processed from a material having the same shape as the reducing material for gas pressure welding F12, and is covered somewhat tightly with a flexible polystyrene resin sheet.

[0169] In addition, in the double-structure gas pressure welding reducing material F, the gas pressure welding reducing material F12 can be combined with the gas pressure welding reducing material F11 by covering it therewith, in the opposite manner to the above. When the gas pressure welding reducing material F12 is covered with the gas pressure welding reducing material F11, the gas pressure welding reducing material F11 is built into the gas pressure welding reducing material F12, which has the advantage that the gas pressure welding reducing material F11 is less likely to fall off due to unintended contact or the like.

[0170] (action) Here, a gas pressure welding method using the above-mentioned gas pressure welding reducing material F of type F and its action will be described with reference to Figs.

[0171] The reducing material for gas pressure welding F has a structure in which a reducing material for gas pressure welding F11 having an inlet portion is layered on the outside of a reducing material for gas pressure welding F12 which is a bottomed cylindrical body.

[0172] First, before the top part of the cap body of the reducing material F for gas pressure welding is sandwiched between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92, that is, when the gap is wide, the reducing material F for gas pressure welding is placed over the tip part of the fixed-side material to be pressure welded 91 while keeping the double structure. As a result, even if some wind blows before the top part of the cap body is sandwiched, the reducing material F for gas pressure welding is unlikely to come off the tip part of the material to be pressure welded 91 due to the action of the deep body of the bottomed cylindrical reducing material F12 for gas pressure welding.

[0173] If the gas pressure welding reducing material F does not come off before the top of the cap body of the gas pressure welding reducing material F is sandwiched between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92, the sandwiched double-layered gas pressure welding reducing material F is used as a reducing material. Note that since the top of the cap body of the gas pressure welding reducing material F is also double-layered, a favorable effect as a reducing material can be expected.

[0174] Furthermore, if the reducing material F for gas pressure welding comes off before the top part of the cap body of the reducing material F for gas pressure welding is clamped between the pressure welding surfaces 910, 920 of each of the materials to be pressure welded 91, 92, the reducing material F11 for gas pressure welding having the fitting opening part 24 on the cap body is removed from the reducing material F12 for gas pressure welding in the detached state, and only this reducing material F11 for gas pressure welding is used as the reducing material.

[0175] The action of the reducing material F11 for gas pressure welding when used is the same as that of the reducing material D1 for gas pressure welding, and when re-attaching the reducing material F11 for gas pressure welding, there is no need to adjust the gap between the pressure welding surfaces 910, 920 of the materials to be pressure-welded 91, 92 by significantly widening it. The reducing material F11 for gas pressure welding can be attached simply by widening the gap to a width equal to the thickness of the top part of the cap body, which is significantly thinner than the thickness of the entire cap body.

[0176] The reducing material F11 for gas pressure welding can be combined with an air blocking ring and a reducing sheet in order to more reliably prevent the formation of an oxide film on the pressure welding surfaces 910, 920 when pressure welding the materials 91, 92. The reducing material E3 for gas pressure welding shown in Fig. 17 is one embodiment of the E type.

[0177] The gas pressure welding reducing material E3 has a cap body 3. The cap body 3 is made of a sheet of polystyrene resin, which is a thermoplastic resin. The body 30 of the cap body 3 has a cylindrical shape that is slightly flared at the bottom, and the upper end is closed by a circular top plate 31.

[0178] The body 30 is provided with vertical reinforcing parts 32 that bulge outward at a predetermined interval in the circumferential direction. The body 30 is also provided with weakened lines 35 that can be torn apart to separate it. The weakened lines 35 are provided in the circumferential direction along the top plate 31 to a predetermined thickness, and have perforations 350 of a width that allows them to be fitted into the material 91 to be pressure welded.

[0179] The thick portion formed by the perforations 350 and the top plate 31 has a partially cylindrical shape, and this portion also becomes a fitting portion 351 that prevents the pressure welding material 91 from falling off when it is fitted onto the tip of the pressure welding material 91 after the separation piece 300 is cut off. The reducing material E3 for gas pressure welding has strength due to the vertical reinforcing portion 32, and has a good grip on the pressure welding material 91.

[0180] Then, continuing from both ends of the perforation 350, perforations 352, 353 are formed in a U-shape in the remaining thickness (height) portion of the body portion 30 in a direction approximately perpendicular to the top plate 31 to the bottom end. Also, a flange portion 36 having a slightly larger diameter is provided around the entire circumference of the bottom portion of the cap body 3. By cutting along the perforations 352, 353, the separation piece 300 can be separated to form an insertion port similar to the insertion port portion 12 of the gas pressure welding reducing material D1 described above.

[0181] An air blocking ring 33 made of polyimide resin, which is a thermosetting resin, is disposed on the inner surface (lower surface) of the top plate 31, and a circular reduction sheet 34 made of polystyrene resin and slightly larger in diameter than the air blocking ring 33 is welded to the top plate 31 at its center, sandwiching the air blocking ring 33 between the inner surface of the top plate 31 and the reduction sheet 34. The reduction sheet 34 is thermally deformed so as to conform to the outer shape of the air blocking ring 33, and cooperates with the inner surface to enclose the air blocking ring 33 (see the enlarged view of FIG. 17).

[0182] When gas pressure welding of the pressure-welded materials 91, 92 is performed using the reducing material E3 for gas pressure welding, the fixed side pressure-welded material 91 and the movable side pressure-welded material 92 are set in the same manner as in the case of pressure welding work using the reducing material D1 for gas pressure welding. Then, for example, when it becomes necessary to attach the reducing material E3 for gas pressure welding again, the cap body 3 can be cut along the perforations 350, 352, 353 to separate the cut-off piece 300, which is the unnecessary part, and a reducing material for gas pressure welding (not shown) having an insertion opening portion (not shown) can be produced.

[0183] The method of use and action of the reducing material for gas pressure welding after the fitting opening is formed in the cap body 3 is the same as that of the reducing material for gas pressure welding D1 described above, except that the addition of the air blocking ring 33 and the reducing sheet 34 produces an action due to these.

[0184] In this case, in the pressure welding operation, the reducing material E3 for gas pressure welding is heated by the gas flame together with the materials to be pressure welded 91, 92, so that first the reducing sheet 34 and the top plate 31 melt and burn. Then, in a very short time, the reducing sheet 34 melts and burns in the small gap between the pressure welding surfaces 910, 920 of the materials to be pressure welded 91, 92 inside the air blocking ring 33, which is made of thermosetting resin and has not yet melted.

[0185] Furthermore, as a result of the combustion causing vaporization and a sudden increase in volume, the air in the gap inside the air shutoff ring 33 is pushed outward under high pressure, and the oxygen in the air combines with the polymeric carbon to become carbon dioxide gas, thereby suppressing oxidation of the pressure contact surface.

[0186] Furthermore, before the air blocking ring 33 melts, air is prevented from entering the gap inside the air blocking ring 33, which in turn suppresses oxidation within the gap and prevents an oxide coating from forming on the tip surface on the pressure-welded side.

[0187] In this way, when using natural gas, propane gas, hydrogen gas, or the like, which have a lower heating power than acetylene gas, when performing gas pressure welding, the reducing material E3 can suppress the generation of residues such as oxide coatings and metal residues on the pressure welding surfaces 910, 920 even if heating is performed with a standard flame from the initial heating stage so as to obtain sufficient heating power, making it possible to perform pressure welding with sufficient strength.

[0188] In addition, if the reducing material E3 for gas pressure welding comes off before closing the pressure welding surfaces 910, 920 of the pressure-welded materials, it is necessary to reattach the reducing material E3 for gas pressure welding. At that time, there is no need to adjust the gap between the pressure welding surfaces 910, 920 of the pressure-welded materials 91, 92 by significantly widening it, and the reducing material E3 for gas pressure welding can be attached simply by widening the gap to a width equivalent to the thickness of the top part of the cap body 3, which is significantly thinner than the thickness of the entire cap body 3.

[0189] In addition, the configuration in which the gas pressure welding reducing material is provided with an air blocking ring and a reducing sheet as shown in FIG. 17 can be similarly applied to the above-mentioned gas pressure welding reducing materials A1, A2, A3, A4, A5, gas pressure welding reducing materials B1, B2, B3, gas pressure welding reducing materials C1, C2, gas pressure welding reducing materials D1, D2, gas pressure welding reducing materials E1, E2, and gas pressure welding reducing material F.

[0190] Please refer to Figures 18(a) and 18(b). The processing tool 8 is a tool for forming a fitting opening in a cap body G that does not have a fitting opening. The processing tool 8 has a base member 80. Support members 81 are provided on both sides in the width direction of one surface (the upper surface in FIG. 18) of the base member 80. A receiving leg 82 is provided at the tip of the base member 80, and a receiving tool 83 is provided extending from the support member 81 to the receiving leg 82, slanting slightly downward toward the tip.

[0191] A seesaw member 84 is placed on the support member 81 so as to be able to swing in the direction of the arrow via a fulcrum part 840. A tip member 841 (left side in FIG. 18(b)) of the seesaw member 84 has a shape curved in the width direction toward the base member 80 side. A cutting blade 843 that is U-shaped in plan view is attached to a concave surface 842 on the base member 80 side of the tip member 841 along the curved shape. Also, as shown in FIG. 18, the seesaw member 84 is formed in a shape that is curved slightly upwards with the fulcrum part 840 as a boundary, and a pressing piece 844 is provided at the tip and an operating part 845 is formed on the base side.

[0192] The seesaw member 84 is biased by a C-shaped leaf spring 85 in a direction in which the tip of the seesaw member 84 and the receiver 83 of the base member 80 are sandwiched at both ends and come into close contact with each other. In a normal state, the seesaw member 84 is closed and the cutting blade 843 is housed in a blade groove 830 provided in the receiver 83. The cutting blade is not limited to being U-shaped, and can be formed, for example, in a U-shape with the fitting opening also being U-shaped.

[0193] The seesaw member 84 can be swung in the direction of the arrow by pushing back the operation part 845. The distance between the tip of the base 83 and the cutting blade 843 when the seesaw member 84 is closed is set to the same as the height of the fitting part 121 in the thickness direction.

[0194] A method of using the machining tool 8 will be described with reference to FIGS. 19(a) and 19(b). The cap body G to be processed here is a type that does not have a flange portion around the opening 100.

[0195] First, the operating portion 845 is pressed to open the tip member 841 of the seesaw member 84 having the cutting blade 843, and the tip portion of the base member 80 is inserted from the opening 100 of the cap body G. At this time, the body portion 101 of the cap body G is inserted between the tip portion of the base member 80 and the tip member 841 of the seesaw member 84.

[0196] Then, when the tip of the base member 80 is brought into contact with the top plate 102, the operating portion 845 is loosened, and the leaf spring 85 is returned to its normal state, the tip member 841 closes. As a result, the pressing piece 844 comes into contact with the top plate 102 of the cap body G and pinches the top plate 102, determining the position of the cutting blade 843, and at the same time, the cutting blade 843 cuts the body part 101 of the cap body G into a U-shape and fits into the blade groove 830 (see the shapes shown by dotted lines in Figures 18(b), 19(a), and 19(b)).

[0197] One end of the seesaw member 84 has a shape that is curved roughly like a gutter toward the base member 80, the receiving device 83 on the base member 80 side is curved to roughly follow the curved surface of the seesaw member 84, and the cutting blade 843 provided on the seesaw member 84 has a curved cutting edge that roughly follows the curved surface of the body 101 of the cap body G to be processed.

[0198] As a result, the cutting edge of the cutting blade 843 is close to the curved surface of the body 101 of the cap body G over almost the entire length before it moves in the cutting direction, so the movement of the cutting blade 843 until cutting is completed is reduced. Accordingly, deformation of the cap body G caused by the cutting blade 843 during cutting is kept small, so that the cap body G can be prevented from being cut in a distorted manner.

[0199] In addition, if the biasing force of the leaf spring 85 alone is not enough to allow the cutting blade 843 to sufficiently cut the body 101, the body 101 of the cap body G can be reliably pushed through by pinching the tip of the base member 80 and the tip member 841 of the seesaw member 84 with the hands from inside and outside the cap body G.

[0200] The processing tool 8 can also process a cap body having a flange portion. In this case, if the cap body is cut in a state where it is appropriately deformed so that the flange portion does not get in the way, a reducing material for gas pressure welding that is substantially the same as the reducing material for gas pressure welding D1 described above can be formed.

[0201] The terms and expressions used in the present specification and claims are merely for explanatory purposes and are not limiting in any way, and are not intended to exclude terms and expressions equivalent to the features described in the present specification and claims and parts thereof. In addition, it goes without saying that various modifications are possible within the scope of the technical idea of ​​the present invention. [Explanation of symbols]

[0202] A1 Reducing agent for gas pressure welding 4a Cap body 40 Torso 41 Tabletop 42 Side Panel 42a side plate 420 Flange part 91, 92 Pressure welded material 910, 920 tip surface 900 Gap A2 Reducing agent for gas pressure welding 4b Cap body 43 Tabletop 44 Torso and legs 440 Flange 45 Torso A3 Reducing agent for gas pressure welding 4c Cap body 40 Torso 46 Tabletop 47 Side Panel 47a side plate 470 Flange 471 Hanging part 472 Retaining plate 48 Hole A4 Reducing agent for gas pressure welding 4d Cap body 473 Hanging part A5 Reducing agent for gas pressure welding 4e Cap body 47 Side Panel 48 Hole 49 Hook B1 Reducing agent for gas pressure welding 5a Cap body 50 Torso 51 Tabletop 500 cuts 52 Torso and legs 520 Flange part B2 Reducing agent for gas pressure welding 5b Cap body 51 Tabletop 53 Torso 500 cuts 54 Torso and legs 540 Flange B3 Reducing agent for gas pressure welding 5c Cap body 51 Tabletop 55 Torso and legs 550 Flange 56 Hook 57 Torso C1 Reducing agent for gas pressure welding 6a Cap body 61 Tabletop 62 Hem 64 Torso and legs 640 Flange part 65 Insertion mouth C2 Reducing agent for gas pressure welding 6b Cap body 61 Tabletop 62 Hem 63 Torso and legs 630 Flange part D1 Reducing agent for gas pressure welding 1a Cap body 10. Torso 11 Tabletop 12. Insertion port 120 Cutting Edge 121 Fitting part 122, 123 Cutting edge 13 Flange D2 Reducing agent for gas pressure welding 1c Cap body 10c Torso 12c Insertion opening 124 Cutting Edge 125 Fitting part 126, 127 Cutting edge 128, 129 Holding part E1 Reducing agent for gas pressure welding 2a Cap body 20a Torso 21 Tabletop 22a Line of weakness 220 Perforation 221 Fitting part 222, 223 Perforation 229 holes 200 section 23a Flange E2 Reducing agent for gas pressure welding 2b Cap body 20b Torso 22b Line of weakness 224, 225 Perforation 226, 227 Opening / closing piece 228 Fitting part 23b Flange part F Reducing agent for gas pressure welding F11 Reducing agent for gas pressure welding F12 Reducing agent for gas pressure welding G Reducing agent for gas pressure welding 3 Cap body 30 Torso 31 Tabletop 32 Vertical reinforcement 33 Air cutoff ring 34 Rebate Sheet 35 Weakened Lines 350 perforations 351 Fitting part 352, 353 Perforation 300 section 36 Flange section 8 Processing tools 80 Base material 81 Support member 82 Socket 83 Receiver 830 Cutting groove 84 Seesaw member 840 Support part 841 Tip material 842 Concave 843 Cutting blade 844 Clamp 845 Operation section 85 Leaf Spring

Claims

1. A cap body is provided which can be fitted onto the tip of the material to be pressure-welded, and an opening and closing part is formed on the body of the cap body which can be fitted onto the material to be pressure-welded from the side so that the top part of the cap body comes into contact with the tip surface of the material to be pressure-welded. A reducing material for gas pressure welding.

2. The body portion has a required number of side plates that are provided in the circumferential direction of the top portion and form the body portion, and a predetermined side plate among the side plates is deformable independently of the other side plates. The reducing material for gas pressure welding according to claim 1.

3. The torso section has four legs formed in a cross shape on the same plane with a sheet and bent in the same direction with approximately the same length, and a predetermined one of the legs formed in the circumferential direction of the top section is deformable. The reducing material for gas pressure welding according to claim 1.

4. The body portion is provided with a required number of body legs that are divided by cut portions in the circumferential direction of the top portion and form the body portion, and the body legs are deformable. The reducing material for gas pressure welding according to claim 1.

5. A cap body that can be fitted onto the tip of the material to be pressure-welded is provided, and the cap body has a top part that contacts the tip surface of the material to be pressure-welded and a required number of legs provided in the circumferential direction of the top part, and the interval between at least one pair of adjacent legs is formed to be approximately the same as the diameter of the material to be pressure-welded or larger than the diameter of the material to be pressure-welded. A reducing material for gas pressure welding.

6. A cap body is provided which can be fitted onto the tip of the material to be pressure-welded, and the body of the cap body is formed so that it can be fitted from the side into the material to be pressure-welded so that the top part of the cap body comes into contact with the tip surface of the material to be pressure-welded by changing its shape. A reducing material for gas pressure welding.

7. A cap body is provided which can be fitted onto the tip of the material to be pressure-welded, and a fitting opening is formed in the body of the cap body so that the top of the cap body can be fitted into the material to be pressure-welded from the side so that the top of the cap body comes into contact with the tip surface of the material to be pressure-welded. A reducing material for gas pressure welding.

8. A cap body is provided that can be fitted onto the tip of the material to be pressure-welded, and a breakable weakened line is provided on the body of the cap body, By cutting away the weakened line, a fitting opening portion that can be fitted from the side into the material to be pressure-welded can be formed so that the top portion of the cap body comes into contact with the tip surface of the material to be pressure-welded. A reducing material for gas pressure welding.

9. A hole is formed at a predetermined location of the body, penetrating from the front to the back. The reducing material for gas pressure welding according to claim 1, 2, 3, 4, 5, 6, 7, or 8.

10. A hook protruding inward is formed at a predetermined location on the body. The reducing material for gas pressure welding according to claim 1, 2, 3, 4, 5, 6, 7, or 8.

Citation Information

Patent Citations

  • Annular body holding member with annular body for gas pressure welding built therein

    JP2011177780A

  • Holding member for annular body incorporated with annular body for gas-pressure welding

    JP2012110936A

  • Gas pressure contact cover, and gas pressure contact method using said cover

    JP2017094349A