Multi-layered soluble solid article containing solid particles for making same - Patents.com
A coating composition with a non-aqueous liquid carrier and thickener enhances the stability and sealing of multilayer dissolvable sheets, addressing sealing issues and ensuring effective delivery of solid particles like bleach, thereby improving product performance and consumer safety.
Patent Information
- Application Number
- JP2022534392
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-09
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2040-10-09
AI Technical Summary
Existing multilayer dissolvable sheets face challenges in incorporating solid particles, such as bleach, due to issues with sealing and potential powder leakage, which affect product integrity and consumer experience.
A coating composition comprising a non-aqueous liquid carrier, a thickener, and solid particles is applied to the contact surfaces of multilayer flexible dissolvable porous sheets to improve stability and sealing, using non-ionic surfactants and specific thickening agents like silica and polyacrylate to enhance performance.
The solution significantly improves the stability and leakage resistance of multilayer dissolvable sheets, allowing for effective delivery of active ingredients like bleaching agents while maintaining structural integrity and preventing premature reactions with moisture.
Smart Images

Figure 0007578693000024 
Figure 0007578693000025 
Figure 0007578693000026
Abstract
Description
[Technical field]
[0001] The present invention relates to a multi-layered dissolvable solid article containing solid particles and a process for making the same. [Background technology]
[0002] Flexible dissolving sheets containing surfactants and / or other active ingredients in a water-soluble polymer carrier or matrix are well known. Such sheets are particularly useful for delivering surfactants and / or other active ingredients upon dissolution in water. Compared with traditional granules or liquid forms in the same product category, such sheets have better structural integrity, are more concentrated, and are easier to store, transport / ship, carry, and handle. Compared with solid tablet forms in the same product category, such sheets are more flexible, less brittle, and have better sensory appeal to consumers.
[0003] To improve the dissolution profile of such sheets, some studies have developed porous sheets with open-celled foam (OCF) structure characterized by an open cell content percentage of about 80% to 100%. In particular, WO2010077627 discloses a batch process for forming such porous sheets with OCF structure, which includes vigorously aerating a premix of raw materials and then thermally drying the aerated premix in a batch (e.g., in a convection oven or microwave oven) to form a porous sheet with the desired OCF structure. WO2012138820 discloses a process similar to that of WO2010077627, except that continuous drying of the aerated wet premix is achieved by, for example, using an impingement oven (instead of a convection oven or microwave oven).
[0004] On the other hand, it is desirable to use multiple layers of such flexible and dissolvable sheets to deliver sufficient amounts of surfactants and / or other active ingredients to achieve the desired product function, and it is even more desirable to assemble such multiple layers into a monolithic dissolvable solid article, which can then be sold as a monolithic finished product. Furthermore, some active ingredients that are not suitable for processing into sheets due to thermal stability or inactivation when contacted with water can be applied as a coating composition between the layers of a multilayer article. Such coating compositions containing active ingredients that are applied between layers in a multilayer article can be in liquid or particulate form. However, various challenges can be encountered when trying to apply such coating compositions between sheets. In particular, some active ingredients (e.g., bleach, foaming systems, etc.) exist only in the form of solid particles, but incorporating these particles between the layers of a foam involves significant challenges. For example, sealing particles between layers of foam sheets can be technically difficult (i.e., the presence of solid particles may result in insufficient contact area between adjacent layers to allow for a good seal, or particles at the edges may prevent sealing in that area leaving the sides of the product open) and can cause powder leakage during use, which is undesirable for the consumer. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] International Publication No. 2010077627 [Patent Document 2] International Publication No. 2012138820 Summary of the Invention [Problem to be solved by the invention]
[0006] Thus, there is a continuing need for multi-layer articles containing solid particle compositions that have improved performance. [Means for solving the problem]
[0007] The present invention provides multi-layer articles with improved performance using a coating composition comprising solid particles dispersed in a non-aqueous liquid carrier applied to the contact surface of one or both of the adjacent layers of a multi-layer flexible dissolvable porous sheet.
[0008] The inventors of the present invention have found that solid particles are often incompatible with non-aqueous liquid carriers. The solid particles tend to aggregate and / or settle. In some worse cases, phase separation occurs. To solve this problem, the inventors have developed a coating composition comprising a non-aqueous liquid carrier, a thickener, and solid particles. In particular, the coating composition according to the present invention comprises a non-ionic surfactant as the non-aqueous liquid carrier, a thickener, and solid particles. In some preferred embodiments, the thickener may be selected from the group consisting of silica, clay, polyacrylate thickener, polyacrylamide thickener, xanthan thickener, guar gum, alginic acid ethoxylated cellulose, hydroxypropyl cellulose, hydroxyethyl cellulose, and any combination thereof.
[0009] The inventors of the present invention have surprisingly found that the coating composition according to the present invention can significantly improve the stability of the coating composition. Moreover, the coating composition according to the present invention can bring about additional effects, including but not limited to improved stability of active ingredients, improved leakage, improved loading capacity, and improved process feasibility. In particular, the inventors of the present invention have surprisingly found that the stability of the bleaching agent added as solid particles in the coating composition is significantly improved. Such an improvement is completely unexpected, considering that air or moisture can enter the porous structure of the multi-layered dissolvable solid article, in other words, the bleaching agent between the layers can still come into contact with environmental materials.
[0010] In one aspect, the invention relates to a dissolvable solid article comprising two or more flexible porous dissolvable sheets, each of the two or more sheets comprising a water soluble polymer and a surfactant and characterized by a percent open cell content of 80% to 100% and an overall average pore size of 100 μm to 2000 μm, and a coating composition comprising a non-aqueous liquid carrier, solid particles, and a thickener is present on at least one surface of at least one of the two or more sheets, with the proviso that the coating composition is not present on any exterior surface of the dissolvable solid article. Preferably, the solid particles include a first group of particles and a second group of particles, the first group of particles includes an available oxygen source, preferably selected from the group consisting of percarbonates, perborates, persulfates, and any combination thereof, and the second group of particles includes a bleach activator selected from the group consisting of tetraacetylethylenediamine (TAED), oxybenzenesulfonate, caprolactam; pentaacetate glucose (PAG), nitrile quaternary ammonium, imide bleach activators, and any combination thereof.
[0011] In another aspect, the present invention provides a dissolvable solid article comprising three or more flexible porous dissolvable sheets, each of the three or more sheets comprising a water soluble polymer and a surfactant and characterized by a percent open cell content of 80% to 100% and an overall average pore size of 100 μm to 2000 μm, a first coating composition is present on at least one surface of at least one of the three or more sheets, the first coating composition comprising a first non-aqueous liquid carrier, a thickener, and a first population of solid particles comprising a source of available oxygen, and a second .... and a second coating composition comprising a second non-aqueous liquid carrier, a thickener, and a second population of solid particles comprising a bleach activator, the first non-aqueous liquid carrier and the second non-aqueous liquid carrier being independently selected from the group consisting of polyethylene glycols, polypropylene glycols, silicones, fatty acids, perfume oils, non-ionic surfactants, and any combination thereof, with the proviso that the first and second coating compositions are not on the same surface and are not present on any exterior surface of the dissolvable solid article. Preferably, the first coating composition is a C6-C alkoxylated polyol having a weight average degree of alkoxylation in the range of 5 to 15. 20 The second coating composition may comprise 20% to 50% of a first non-aqueous liquid carrier which is a linear or branched alkyl alkoxylated alcohol (AA), 30% to 70% of a first solid particle population comprising a percarbonate or perborate, and 0.1% to 1.5% of a thickener, and the second coating composition may comprise a C6-C alkoxylated alcohol having a weight average degree of alkoxylation in the range of 5 to 15. 20 It may include 20% to 50% of a second non-aqueous liquid carrier which is a linear or branched alkyl alkoxylated alcohol (AA), 30% to 70% of a second solid particle population comprising tetraacetylethylenediamine (TAED), and 0.1% to 1.5% of a thickener.
[0012] In a further aspect, the invention relates to a process for preparing a dissolvable solid article comprising the steps of: 1) providing two or more flexible porous dissolvable sheets and a coating composition, each of the two or more sheets comprising a water soluble polymer and a surfactant and characterized by a percent open cell content of 80% to 100% and an overall average pore size of 100 μm to 2000 μm, the coating composition comprising a non-aqueous liquid carrier, solid particles, and a thickener; 2) applying the coating composition onto at least one surface of at least one of the two or more sheets; and 3) arranging the two or more sheets in a stack to form a dissolvable solid article such that the coating composition is not present on any outer surface of the stack. Preferably, the two or more flexible porous dissolving sheets can be provided by using the following steps: a) preparing a wet premix comprising the water-soluble polymer and the surfactant; b) aerating the wet premix to form an aerated wet premix; c) forming the aerated wet premix into a sheet having first and second opposing sides; and d) drying the formed sheet to produce the two or more flexible porous dissolving sheets. More preferably, step d) can be performed along a heating direction forming a decreasing temperature gradient from the first side to the second side of the formed sheet at a temperature of 70°C to 200°C, preferably 90°C to 140°C, for a period of 5 minutes to 300 minutes, preferably 10 minutes to 120 minutes, the heating direction being substantially opposite to the direction of gravity for more than half the drying time, preferably more than 75% of the drying time. In particular, the wet premix can be dried at 40°C and 1s. -1 and / or the aerated wet premix may have a density of 0.05 to 0.7 g / mL, preferably 0.15 g / mL to 0.6 g / mL, more preferably 0.2 g / mL to 0.5 g / mL, and most preferably 0.25 g / mL to 0.45 g / mL.
[0013] In a further aspect, the present invention relates to the use of a dissolvable solid article according to the present disclosure in eliminating bacteria and / or preventing or reducing malodours.
[0014] One advantage of the dissolvable solid articles according to the present disclosure is that coating compositions that include a thickener exhibit significantly improved stability compared to coating compositions that do not include a thickener.
[0015] One advantage of the dissolving solid article according to the present disclosure is that it can contain sufficient amount of active ingredient as solid particles to produce effect.In other words, the dissolving solid article according to the present disclosure provides a carrier with enhanced capacity for loading solid particles.In particular, the dissolving solid article containing the coating composition with thickener can produce less leakage when loading the same amount of solid particles compared with the dissolving solid article containing the coating composition without thickener, that is, it balances between dissolution profile and leakage.
[0016] One advantage of the dissolvable solid article according to the present disclosure is that the moisture-sensitive active ingredient (e.g., bleach) contained in the dissolvable solid article exhibits significantly improved stability compared to the moisture-sensitive active ingredient alone stored under the same conditions. In other words, the dissolvable solid article according to the present disclosure provides a better environment for the storage of the moisture-sensitive active ingredient.
[0017] One advantage of the dissolvable solid article according to the present disclosure is that it can provide a satisfactory carrier for bleaching agents (e.g., available oxygen source and bleach activator). In particular, the available oxygen source and bleach activator in the dissolvable solid article can be present in a physically separate manner to prevent premature reaction between them when accidentally contacting with water or moisture. More specifically, the dissolvable solid article can be formed into a multi-layer structure with improved dissolution rate, and the available oxygen source and bleach activator can be separately coated between two adjacent layers (i.e., the available oxygen source is coated between two adjacent layers, and the bleach activator is coated between another two adjacent layers).
[0018] One advantage of the dissolvable solid article according to the present disclosure is that it can achieve excellent antimicrobial effect. In particular, the dissolvable solid article according to the present disclosure can significantly remove microorganisms from fabrics or hard surfaces (e.g., glass, wood, metal, ceramic, etc.). In the context of the present disclosure, removing microorganisms includes, but is not limited to, killing, inactivating, eliminating, and / or cleaning microorganisms.
[0019] One advantage of the dissolvable solid articles according to the present disclosure is that excellent malodor prevention or reduction may be achieved.
[0020] These and other aspects of the invention will become further apparent from a reading of the following detailed description. [Brief description of the drawings]
[0021] [Figure 1] 1 shows a convection heating / drying configuration for making flexible porous dissolvable solid sheet articles in a batch process. [Diagram 2] 1 shows a microwave heating / drying configuration for making flexible porous dissolvable solid sheet articles in a batch process. [Diagram 3] 1 shows an impingement oven heating / drying configuration for making flexible porous dissolvable solid sheet articles in a continuous process. [Figure 4] 1 illustrates a bottom conduction heating / drying configuration for making flexible porous dissolvable sheets in a batch process according to one embodiment of the present invention. [Diagram 5] 13 shows a rotating drum heating / drying configuration for making another flexible porous dissolvable sheet in a continuous process according to another embodiment of the present invention. [Figure 6A] FIG. 1 shows a Scanning Electron Microscopic (SEM) image of the top surface of a flexible porous dissolvable sheet containing fabric care actives made by a process employing a rotating drum heating / drying configuration. [Figure 6B]FIG. 6B shows an SEM image of the top surface of an alternative flexible porous dissolvable sheet containing the same fabric care actives as the sheet shown in FIG. 6A, but made by a process employing an impingement oven type heating / drying configuration. [Figure 7A] 1 shows an exemplary diagram of an embodiment of a dissolvable solid article having multiple flexible porous sheets according to the present disclosure, where a coating composition comprising a bleaching agent is applied between two adjacent sheets. [Figure 7B] FIG. 1 shows an exemplary diagram of another embodiment of a dissolvable solid article having a plurality of flexible porous sheets according to the present disclosure, where a first coating composition comprising an available oxygen source is applied between two adjacent sheets and a second coating composition comprising a bleach activator is applied between another two adjacent sheets. [Figure 7C] FIG. 1 shows an exemplary diagram of another embodiment of a dissolvable solid article having a plurality of flexible porous sheets according to the present disclosure, wherein the solid article comprises a first group of sheets, a second group of sheets, and a coating composition comprising an available oxygen source applied between two adjacent sheets in the first group of sheets. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] I. Definition As used herein, the term "flexible" refers to the ability of an article to withstand stress when bent 90° along a centerline perpendicular to its length without breaking or significant disruption. Preferably, such articles are capable of undergoing significant elastic deformation and are characterized by a Young's modulus of 5 GPa or less, preferably 1 GPa or less, more preferably 0.5 GPa or less, and most preferably 0.2 GPa or less.
[0023] As used herein, the term "solubility" refers to the ability of an article to completely or substantially dissolve in a sufficient amount of deionized water at 20° C. and atmospheric pressure within 8 hours without any agitation, with less than 5% by weight remaining as an insoluble residue.
[0024] As used herein, the term "solid" refers to the ability of an article to substantially retain its shape (i.e., without any visible change in its shape) at 20° C. and atmospheric pressure when the article is unconstrained and no external forces are applied to the article.
[0025] As used herein, the term "sheet" refers to a non-fibrous structure having a three-dimensional shape, i.e., thickness, length, and width, while the aspect ratios of length to thickness and width to thickness are both at least about 5:1, and the length to width ratio is at least about 1:1. Preferably, the aspect ratios of length to thickness and width to thickness are both at least about 10:1, more preferably at least about 15:1, and most preferably at least about 20:1, and the aspect ratio of length to width is preferably at least about 1.2:1, more preferably at least about 1.5:1, and most preferably at least about 1.618:1.
[0026] As used herein, the term "contact surface" of adjacent sheets refers to two surfaces, each originating from two adjacent sheets, that contact each other when the adjacent sheets are arranged in a stack. For example, the contact surface can be the lower surface of the top sheet and the upper surface of the bottom sheet when two adjacent sheets are arranged in a vertical stack.
[0027] As used herein, the term "bottom surface" refers to the surface of the flexible porous dissolvable solid sheet of the present invention that is in direct contact with the support surface on which the sheet of aerated wet premix is placed during the drying process, while the term "top surface" refers to the surface of said sheet opposite the bottom surface. Furthermore, such a solid sheet can be divided along its thickness into three regions, including a top region adjacent its top surface, a bottom region adjacent its bottom surface, and a middle region located between the top and bottom regions. The top, middle, and bottom regions are equal in thickness, i.e., each has a thickness of about 1 / 3 of the total thickness of the sheet.
[0028] As used herein, the term "outermost sheet" refers to a sheet that is adjacent to only one sheet in the multi-layer dissolvable solid article of the present invention.
[0029] As used herein, the term "open cell foam" or "open cell pore structure" refers to a solid interconnected polymer-containing matrix that contains a gas, typically a gas (such as air), and defines a network of voids or cells that do not collapse the foamed structure during the drying process, thereby maintaining physical strength and solid coherence. The interconnectedness of the structure may be described by the percent open cell content, as measured by Test 3 disclosed below.
[0030] As used herein, the term "water solubility" refers to the ability of a sample material to completely dissolve or disperse in water without leaving any visible solids or forming any visible separate phases, when at least about 25 grams, preferably at least about 50 grams, more preferably at least about 100 grams, and most preferably at least about 200 grams of such material are placed in one liter (1 L) of deionized water at 20° C. and atmospheric pressure with sufficient agitation.
[0031] As used herein, the terms "aerate", "aerating" or "aeration" refer to the process of introducing gas into a liquid or pasty composition by mechanical and / or chemical means.
[0032] As used herein, the term "heating direction" refers to a direction in which a heat source applies thermal energy to an article, resulting in a temperature gradient in such an article that decreases from one side to the other side of such an article. For example, if a heat source located on one side of an article applies thermal energy to the article to generate a temperature gradient that decreases from one side to the other side, the heating direction is then considered to extend from one side to the other side. If both sides of such an article or different portions of such an article are heated simultaneously without an observable temperature gradient across such an article, then the heating occurs in a non-directional manner and there is no heating direction.
[0033] As used herein, the terms "substantially opposite" or "substantially offset" refer to two directions or two lines that have an offset angle between them of 90° or more.
[0034] As used herein, the terms "substantially aligned" or "substantial alignment" refer to two directions or two lines that have an offset angle between them of less than 90°.
[0035] As used herein, the term "primary heat source" refers to a heat source that provides more than 50%, preferably more than 60%, more preferably more than 70%, and most preferably more than 80% of the total heat energy absorbed by an object (e.g., a sheet of aerated wet premix according to the present invention).
[0036] As used herein, the term "controlled surface temperature" refers to a surface temperature that is relatively stable, i.e., having less than + / - 20% variation, preferably less than + / - 10% variation, and more preferably less than + / - 5% variation.
[0037] The terms "essentially free of" or "essentially free from" mean that the indicated substance is present in such small amounts that it has not been intentionally added to a composition or product, or preferably is not present in such composition or product at concentrations detectable by analysis. Compositions or products may be included in which the indicated substance is present only as an impurity of one or more substances intentionally added to such composition or product.
[0038] II. Overview of the Process for Making Solid Sheets WO2010077627 discloses a batch process for forming a porous sheet having an open cell foam (OCF) structure characterized by an open cell content percentage of about 80%-100% that functions to improve dissolution. Specifically, a premix of raw materials is first formed, which is vigorously aerated and then thermally dried in batch (e.g., in a convection oven or microwave oven) to form a porous sheet having the desired OCF structure. Although such an OCF structure significantly improves the dissolution rate of the resulting porous sheet, there are still visually denser, less porous bottom regions within such sheets, with thicker cell walls. Such dense bottom regions can adversely affect the flow of water through the sheet, thereby adversely affecting the overall dissolution rate of the sheet. When multiple such sheets are laminated together to form a multi-layer structure, the "barrier" effect of the multiple dense bottom regions is particularly enhanced.
[0039] WO2012138820 discloses a process similar to that of WO2010077627, except that continuous drying of the aerated wet premix is achieved by using, for example, an impingement oven (instead of a convection oven or microwave oven). The OCF sheet formed by such a continuous drying process is characterized by improved uniformity / consistency in the pore structure across its different regions. Unfortunately, such OCF sheets still have rate-limiting factors, such as a top surface with relatively small pore openings and an upper region with relatively small pores (i.e., a crusty upper region), which can adversely affect the flow of water passing therethrough and slow down its dissolution.
[0040] During the drying step in the above process, the OCF structure is formed under the simultaneous mechanisms of water evaporation, bubble collapse, interstitial liquid drainage from the thin film bubble surfaces into the plateau boundaries between the bubbles (creating openings between the bubbles to form open cells), and premix solidification. Various processing conditions can affect these mechanisms, such as, for example, solids content in the wet premix, viscosity of the wet premix, gravity, and drying temperature, as well as the need to balance such processing conditions to achieve controlled drainage to form the desired OCF structure.
[0041] In addition to the processing conditions described above, it was a surprising and unexpected discovery by the present inventors that the direction of the thermal energy used during the drying step (i.e., heating direction) can also have a significant effect on the resulting OCF structure.
[0042] For example, when thermal energy is applied to a non-directional material (i.e., there is no clear heating direction) during the drying process, or when the heating direction is substantially aligned with the gravity direction (i.e., the offset angle between them is less than 90°) throughout the majority of the drying process, the resulting flexible porous dissolvable solid sheet tends to have a top surface with smaller pore openings and greater pore size variation in different regions along the direction through its thickness. In contrast, when the heating direction is offset from the gravity direction (i.e., with an offset angle of 90° or more between them) throughout the majority of the drying process, the resulting solid sheet may have a top surface with larger pore openings and reduced pore size variation in different regions along the direction through the thickness of such sheet. Correspondingly, the latter sheet is more receptive to water flowing therethrough, and therefore more soluble, than the former sheet.
[0043] Without wishing to be bound by any theory, it is believed that the alignment or misalignment between the heating direction and the gravity direction during the drying process, and its duration, can significantly affect the interstitial liquid evacuation between the gas bubbles, which in turn can affect the pore expansion and pore opening in the solidified premix, resulting in solid sheets with very different OCF structures. Such differences are more clearly shown in Figures 1-4 below.
[0044] FIG. 1 shows a convection heating / drying configuration. During the drying process, a mold 10 (which may be made of any suitable material, such as metal, ceramic, or Teflon®) is filled with the aerated wet premix, which forms a sheet 12 having a first surface 12A (i.e., the top surface) and an opposing second surface 12B (i.e., the bottom surface since it is in direct contact with the support surface of the mold 10). Such mold 10 is placed in a convection oven at 130° C. for about 45-46 minutes during the drying process. The convection oven heats the sheet 12 from above, i.e., along a downward heating direction (as indicated by the cross-hatched arrows), which creates a decreasing temperature gradient within the sheet 12 from the first surface 12A to the opposing second surface 12B. The downward heating direction is aligned with the gravity direction (as indicated by the white arrow), and such aligned position is maintained throughout the drying time. During drying, gravity drains the liquid premix downwards towards the bottom region, while the downward heating direction causes the top region to dry first and the bottom region to dry last. As a result, a porous solid sheet is formed with a top surface that contains many pores with small openings formed by bubbles that have not had the chance to fully expand. Such a top surface with smaller pore openings is not optimal for water penetration into the sheet, which may limit the dissolution rate of the sheet. Meanwhile, the bottom region of such a sheet is denser and less porous, with a very small number of larger pores formed by fully expanded bubbles, and the bubble walls between the pores in such a bottom region are thicker due to the downward liquid drainage caused by gravity. Such a dense bottom region with fewer pores and thick bubble walls is an additional rate limiting factor for the overall dissolution rate of the sheet.
[0045] FIG. 2 shows a microwave heating / drying configuration. During the drying process, a mold 30 is filled with aerated wet premix, which forms a sheet 32 having a first surface 32A (top surface) and an opposing second surface 32B (bottom surface). Such mold 30 is then placed in a low energy density microwave applicator (not shown) provided by Industrial Microwave Systems Inc. (North Carolina) and operated at a power of 2.0 kW, a belt speed of 1 ft / min, and an ambient air temperature of 54.4° C. The mold 30 is left under such microwave application for about 12 minutes during the drying process. Such microwave applicator heats the sheet 32 from the inside without any clear or consistent heating direction. Correspondingly, no temperature gradient is formed in the sheet 32. During drying, the entire sheet 32 is heated simultaneously or nearly simultaneously, but gravity (as indicated by the white arrows) still drains the liquid premix downward toward the bottom region. As a result, the solidified sheet so formed has more evenly distributed and more uniformly sized pores compared to sheets formed by convection heating / drying configurations. However, liquid drainage under gravity during the microwave drying process may still result in a dense bottom region with thick cell walls. Furthermore, simultaneous heating of the entire sheet 32 may still limit pore expansion and pore opening at the top surface during the drying process, and the resulting sheet may still have a top surface with relatively small pore openings. Furthermore, microwave energy may heat water within the sheet 32, causing such water to boil, generating irregularly sized bubbles and forming unintended dense regions with thick cell walls.
[0046] FIG. 3 shows an impingement oven heating / drying configuration. During the drying process, a mold 40 is filled with aerated wet premix, which forms a sheet 42 having a first surface 42A (top surface) and an opposing second surface 42B (bottom surface). Such mold 40 is then placed in a continuous impingement oven (not shown) under conditions similar to those described in Example 1, Table 2 of WO2012138820. Such a continuous impingement oven heats the sheet 42 from both the top and bottom with opposing and offset heating directions (as indicated by the two cross-hatched arrows). Correspondingly, no significant temperature gradient is formed within the sheet 42 during drying, and the entire sheet 42 is heated from both its top and bottom surfaces at approximately the same time. Similar to the microwave heating / drying configuration described in FIG. 3, gravity (as indicated by the white arrow) continues to drain the liquid premix downwards toward the bottom region in such an impingement oven heating / drying configuration of FIG. 4. As a result, the solidified sheet so formed has more evenly distributed and more uniformly sized pores compared to sheets formed by convection heating / drying configurations. However, liquid drainage under gravity during the drying process may still result in a dense bottom region with thick cell walls. Furthermore, the nearly simultaneous heating of the sheet 42 from both directions may still limit pore expansion and pore opening at the top surface during the drying process, and the resulting sheet may still have a top surface with relatively small pore openings.
[0047] In contrast to the heating / drying configurations mentioned above (convection, microwave or impingement oven), the present invention provides a heating / drying configuration for drying an aerated wet pre-mix in which the direction of heating is purposefully configured to impede / reduce gravity-driven liquid drainage towards the bottom region (thereby reducing density and improving pore structure in the bottom region) and to allow more time for gas bubbles near the top surface to expand during drying (thereby creating significantly larger pore openings at the top surface of the resulting sheet). Both of these features function to improve the overall dissolution rate of the sheet and are therefore desirable.
[0048] FIG. 4 illustrates a bottom conduction heating / drying configuration for making a flexible porous dissolvable sheet according to one embodiment of the present invention. Specifically, a mold 50 is filled with an aerated wet premix, which forms a sheet 52 having a first side 52A (i.e., bottom side) and an opposing second side 52B (i.e., top side). Such mold 50 is placed on a heated surface (not shown), for example a preheated Peltier plate having a controlled surface temperature of about 125-130° C., for about 30 minutes during the drying process. Heat is conducted from the heated surface at the bottom of mold 50 through the mold, heating sheet 52 from below, i.e., along an upward heating direction (as indicated by the cross-hatched arrows), which creates a decreasing temperature gradient within sheet 52 from first side 52A (bottom side) to opposing second side 52B (top side). Such upward heating direction is opposite to the direction of gravity (as indicated by the white arrow) and is maintained as such throughout the entire drying time (i.e., the heating direction is opposite to the direction of gravity for nearly 100% of the drying time). During drying, gravity still drains the liquid premix downward toward the bottom region. However, the upward heating direction dries the sheet from bottom to top, and since the heat-generated water vapor in the bottom region rises upward to escape the solidified matrix, downward liquid drainage toward the bottom region is significantly restricted and "impeded" / reduced by the solidified matrix and the rising water vapor. Correspondingly, the bottom region of the resulting dried sheet is less dense and contains a large number of pores with relatively thin cell walls. Furthermore, since the top region is the last region to be dried during the process, the air bubbles in the top region have enough time to expand to form sizable open pores on the top surface of the resulting sheet, which is particularly effective in promoting water ingress into the sheet. Additionally, the resulting sheet has a more even distribution of overall pore sizes throughout its different regions (eg, top, middle, bottom).
[0049] FIG. 5 illustrates a rotating drum heating / drying configuration for making flexible porous dissolvable sheets according to another embodiment of the present invention. Specifically, a feed trough 60 is filled with an aerated wet premix 61. A heated rotatable cylinder 70 (also referred to as a drum dryer) is positioned above the feed trough 60. The heated drum dryer 70 has a cylindrical heated outer surface characterized by a controlled surface temperature of about 130° C., which rotates along a clockwise direction (as indicated by the thin curve with an arrow) to pick up the aerated wet premix 61 from the feed trough 60. The aerated wet premix 61 forms a thin sheet 62 on the cylindrical heated outer surface of the drum dryer 70, and such sheet 62 of aerated wet premix is rotated and dried for about 10-15 minutes. To ensure a consistent thickness of the sheet 62 thus formed, the thickness of the sheet 62 can be controlled by simply adjusting the viscosity of the aerated wet premix 61 and the rotational speed and surface temperature of the drum dryer 70, although a leveling blade (not shown) may be positioned near the slurry pick-off location. Once dried, the sheet 62 can be picked off manually or by a scraper 72 at the end of the drum rotation.
[0050] As shown in FIG. 5, the sheet 62 formed by the aerated wet premix 61 includes a first surface 62A (i.e., bottom surface) that is in direct contact with the heated exterior surface of the heated drum dryer 70, and an opposing second surface 62B (i.e., top surface). Correspondingly, heat from the drum dryer 70 is conducted to the sheet 62 along an outward heating direction, first heating the first surface 62A (bottom surface) of the sheet 62, and then heating the opposing second surface 62B (top surface). Such an outward heating direction creates a temperature gradient within the sheet 62 that decreases from the first surface 62A (bottom surface) to the opposing second surface 62B (top surface). The outward heating direction slowly and constantly changes as the drum dryer 70 rotates, along a very distinct and predictable path (as shown by the multiple outwardly extending cross-hatched arrows in FIG. 5). The relative positions of the outward heating direction and the gravity direction (as indicated by the white arrows) also decelerate and constantly change in a similarly distinct and predictable manner. For less than half of the drying time (i.e., when the heating direction is below the horizontal dashed line), the outward heating direction is substantially aligned with the gravity direction with an offset angle of less than 90° between them. For the majority of the drying time (i.e., when the heating direction is at or above the horizontal dashed line), the outward heating direction is opposite or substantially opposite the gravity direction with an offset angle of 90° or more between them. Depending on the initial "start" coating location of the sheet 62, the heating direction can be opposite or substantially opposite the gravity direction for more than 55% of the drying time (if coating begins just at the bottom of the drum dryer 70) and preferably for more than 60% of the drying time (if coating begins higher up on the drum dryer 70 as shown in FIG. 5). As a result, during most of the drying process, this slow rotation and change in heating direction in the rotating drum heating / drying configuration can still function to limit and "block" / reduce gravity-induced liquid drainage within the sheet 62, resulting in improved OCF structure in the sheet so formed.The resulting sheet after drying with the heated drum dryer 70 is also characterized by a less dense bottom region having a greater number of more uniformly sized pores and a top surface having relatively larger pore openings. Additionally, the resulting sheet has a more uniform distribution of overall pore size throughout its different regions (e.g., top, middle, bottom).
[0051] In addition to employing a desired heating direction (i.e., a substantially offset relationship to the direction of gravity) as described above, it may also be desirable and even important to carefully adjust the viscosity and / or solids content of the wet pre-mix, the amount and rate of aeration (air supply pump speed, mixing head speed, air flow rate, density of the aerated pre-mix, etc., which can affect the air bubble size and amount in the aerated pre-mix and correspondingly affect the pore size / distribution / amount / characteristics of the solidified sheet), drying temperature and drying time to achieve optimal OCF structure in the resulting sheet according to the present invention.
[0052] A more detailed description of the process for making flexible porous dissolvable sheets according to the present invention, as well as the physical and chemical properties of such sheets, are provided in the reserved sections.
[0053] III. Fabrication process of solid sheets The present invention relates to a process for the preparation of a liquid composition comprising: (a) a liquid composition containing raw materials (e.g., a water-soluble polymer, an active ingredient such as a surfactant, and optionally a plasticizer) dissolved or dispersed in water or a suitable solvent, the raw materials being heated to about 40° C. and 1 s -1(b) forming a premix characterized by a viscosity of about 1,000 cps to about 25,000 cps as measured by NMR; (b) aerating the premix (e.g., by introducing a gas into the wet slurry) to form an aerated wet premix; (c) forming the aerated wet premix into a sheet having opposed first and second sides; and (d) drying the formed sheet at a temperature of 70° C. to 200° C. for a drying time of 1 minute to 60 minutes along a heating direction that forms a decreasing temperature gradient from the first side to the second side of the formed sheet, wherein the heating direction is substantially offset from the gravity direction for more than half of the drying time, i.e., heating is performed primarily along an "anti-gravity" heating direction. Such a primarily "anti-gravity" heating orientation can be achieved by a variety of means, including but not limited to bottom conduction heating / drying configurations and rotating drum heating / drying configurations, as shown in Figures 4 and 5, respectively.
[0054] Step (A): Preparation of Wet Premix The wet premix of the present invention is generally prepared by mixing the solids of interest, including water-soluble polymers, surfactants and / or other benefit agents, optional plasticizers, and other optional ingredients, with a sufficient amount of water or another solvent in a premix tank. The wet premix can be formed using a mechanical mixer. Mechanical mixers useful herein include, but are not limited to, turbines with pitched blades, or MAXBLEND mixers (Sumitomo Heavy Industries).
[0055] In the present invention, 40° C. and 1s -1It is particularly important to control the viscosity of the wet premix so that it is within a predetermined range of about 1,000 cps to about 25,000 cps when measured at 40°C. The viscosity of the wet premix can significantly affect the pore expansion and pore opening of the aerated premix during the subsequent drying step, and wet premixes with different viscosities can form flexible porous dissolvable solid sheets of very different foam structures. On the other hand, if the wet premix is too thick / too viscous (e.g., at 40°C and 1s), the viscosity of the wet premix can be significantly affected. -1 Aeration of such wet premixes may become more difficult if the wet premix is too thin / stretchy (e.g., having a viscosity of more than about 25,000 cps as measured at 40° C. and 1 s). More importantly, interstitial liquid drainage from the thin film cellular surface into the plateau boundaries of the three-dimensional foam during the subsequent drying step may be adversely affected or significantly restricted. It is believed that interstitial liquid drainage during drying is important to allow pore expansion and pore opening in the aerated wet premix during the subsequent drying step. As a result, the flexible porous dissolvable solid sheet so formed may have significantly smaller pores and lower interconnectivity between the pores (i.e., more "closed" pores than open pores), which makes it difficult for water to enter and exit such sheets. On the other hand, if the wet premix is too thin / stretchy (e.g., having a viscosity of more than about 25,000 cps as measured at 40° C. and 1 s), it may become more difficult to aerate the wet premix. -1 If the aerated wet premix has a viscosity of less than about 1,000 cps as measured by aerobic dynamics (e.g., 1000 psi), the aerated wet premix may not be stable enough, i.e., air bubbles may quickly burst, collapse, or coalesce in the wet premix after aeration and before drying. As a result, the resulting solid sheet may be much less porous and denser than desired.
[0056] In one embodiment, the viscosity of the wet premix is 40° C. and 1 s -1The viscosity value of the premix is measured using a Malvern Kinexus Lab+ rheometer (CP1 / 50 SR3468 SS) with a cone and plate geometry at a gap width of 0.054 mm, a temperature of 40° C., and a shear rate of 1.0 reciprocal seconds for 360 seconds.
[0057] Step (B): Aeration of the Wet Premix Aeration of the wet premix is performed to introduce a sufficient amount of air bubbles into the wet premix to subsequently form an OCF structure therein upon drying. After being fully aerated, the wet premix is characterized by a density significantly lower than that of a non-aerated wet premix (which may contain a few inadvertently trapped air bubbles) or a poorly aerated wet premix (which may contain some air bubbles, but at a very low volumetric percentage and with significantly larger air bubble sizes). Preferably, the aerated wet premix has a density in the range of about 0.05 g / mL to about 0.8 g / mL, preferably about 0.1 g / mL to about 0.75 g / mL, more preferably about 0.15 g / mL to about 0.7 g / mL, even more preferably about 0.2 g / mL to about 0.6 g / mL, and most preferably about 0.25 g / mL to about 0.5 g / mL.
[0058] Aeration can be achieved by either physical or chemical means in the present invention. In one embodiment, it can be achieved by introducing gas into the wet premix through mechanical agitation, for example, by using any suitable mechanical processing means, including, but not limited to, rotor-stator mixers, planetary mixers, pressurized mixers, non-pressurized mixers, batch mixers, continuous mixers, semi-continuous mixers, high shear mixers, low shear mixers, submerged scourers, or any combination thereof. In another embodiment, it can be achieved through chemical means, for example, using chemical blowing agents to provide gas formation in situ via chemical reaction of one or more components, including the formation of carbon dioxide (CO2 gas) by the foaming system.
[0059] In a particularly preferred embodiment, it has been found that aeration of the wet premix can be cost-effectively achieved by using a continuous pressurized aerator or mixer that is conventionally utilized in the food industry in the manufacture of marshmallows. The continuous pressurized mixer serves to homogenize or aerate the wet premix, resulting in a highly uniform and stable foam structure with uniform cell size. The unique design of the high shear rotor / stator mixing head can result in uniform cell size in the layer of open cell foam. Suitable continuous pressurized aerators or mixers include Morton whisks (Morton Machine Co., Motherwell, Scotland), Oakes continuous automatic mixers (ETOakes Corporation, Hauppauge, New York), Fedco continuous mixers (Peerless Group, Sidney, Ohio), Mondo (Haas-Mondomix BV, Netherlands), Aeros (Aeros Industrial Equipment Co., Ltd., Guangdong Province, China), and Preswhip (Hosokawa Micron Group, Osaka, Japan). For example, an Aeros A20 continuous aerator can be operated at a feed pump speed setting of about 300-800 (preferably about 500-700) with a mix head speed setting of about 300-800 (preferably about 400-600), with an air flow rate of about 50-150 (preferably 60-130, more preferably 80-120), respectively. In another example, an Oakes continuous automated mixer can be operated at a mix head speed setting of about 10-30 rpm (preferably about 15-25 rpm, more preferably about 20 rpm), with an air flow rate of about 10-30 liters / hour (preferably about 15-25 L / hour, more preferably about 19-20 L / hour).
[0060] In another particular embodiment, aeration of the wet premix can be achieved by using a rotary bar that is part of the rotary drum dryer, more specifically, a component of the feed trough in which the wet premix is stored before being coated and dried on the heated exterior surface of the drum dryer. The rotary bar is typically used to agitate the wet premix during the waiting time before being coated on the heated rotary drum of the drum dryer to prevent phase separation or settling in the feed trough. In the present invention, such a rotary bar can be operated at a rotation speed ranging from about 150 to about 500 rpm, preferably from about 200 to about 400 rpm, more preferably from about 250 to about 350 rpm to provide sufficient mechanical agitation necessary to mix the wet premix at the air interface and achieve the desired aeration of the wet premix.
[0061] As mentioned above, the wet premix can be maintained at an elevated temperature during the aeration process to tailor the viscosity of the wet premix for optimized aeration and controlled drainage during drying. For example, when aeration is accomplished by using a rotating bar on a rotating drum, the aerated wet premix in the feed trough is typically maintained at about 60° C. during the initial aeration by the rotating bar (while the rotating drum is stationary), and then heated to about 70° C. when the rotating drum is heated and begins to rotate.
[0062] The bubble size of the aerated wet premix helps achieve uniform layers within the OCF structure of the resulting solid sheet. In one embodiment, the bubble size of the aerated wet premix is from about 5 to about 100 micrometers, and in another embodiment, the bubble size is from about 20 micrometers to about 80 micrometers. The uniformity of the bubble size allows the resulting solid sheet to have a consistent density.
[0063] Step (C): Sheet formation After sufficient aeration, the aerated wet premix forms one or more sheets having opposing first and second surfaces. The sheet forming process can be carried out in any suitable manner, for example, by extrusion, casting, molding, vacuum forming, pressing, printing, coating, etc. More specifically, the aerated wet premix can be formed into a sheet by (i) casting it into a shallow cavity or tray or a specially designed sheet mold, (ii) extruding it onto a continuous belt or screen of a dryer, and (iii) coating it onto the exterior surface of a rotary drum dryer. Preferably, the support surface on which the sheet is formed is formed of or coated with a corrosion-resistant, non-interacting and / or non-stick material, such as metal (e.g., steel, chrome, etc.), TEFLON®, polycarbonate, NEOPRENE®, HDPE, LDPE, rubber, glass, etc.
[0064] Preferably, the formed sheet of aerated wet premix has a thickness in the range of 0.5 mm to 4 mm, preferably 0.6 mm to 3.5 mm, more preferably 0.7 mm to 3 mm, even more preferably 0.8 mm to 2 mm, and most preferably 0.9 mm to 1.5 mm. Controlling the thickness of such a formed sheet of aerated wet premix can be important to ensure that the resulting solid sheet has the desired OCF structure. If the formed sheet is too thin (e.g., less than 0.5 mm thick), many of the trapped air bubbles in the aerated wet premix will expand during the subsequent drying step to form through-holes that extend through the entire thickness of the resulting solid sheet. Such through-holes, if too numerous, can significantly impair both the overall structural integrity and aesthetic appearance of the sheet. If the formed sheet is too thick, it will not only take longer to dry, but will also result in a solid sheet with a larger pore size variation between different regions (e.g., top, middle, and bottom regions) along its thickness. This is because the longer the drying time, the more unbalanced forces may be created by bubble bursting / collapse / coalescence, liquid drainage, pore expansion, pore opening, water evaporation, etc. Additionally, multiple layers of relatively thin sheets can be assembled into three-dimensional structures of greater thickness to provide a desired cleaning or other effect, while providing sufficient pore structure for rapid dissolution and ensuring efficient drying within a relatively short drying time.
[0065] Step (D): Drying under antigravity heat An important feature of the present invention is the use of an anti-gravity heating direction during the drying process, either throughout the entire drying time or at least for more than half of the drying time. Without being bound by any theory, it is believed that such an anti-gravity heating direction can reduce or prevent excessive interstitial liquid drainage toward the bottom region of the formed sheet during the drying process. Furthermore, since the top surface dries last, it allows more time for air bubbles near the top surface of the formed sheet to expand and form pore openings on the top surface (because once the wet matrix is dried, the air bubbles can no longer expand or form surface openings). As a result, the solid sheet formed by drying with such anti-gravity heating is characterized by an improved OCF structure, which allows for faster dissolution and other surprising and unexpected effects.
[0066] In certain embodiments, the anti-gravity heating direction is provided by a conduction heating / drying configuration the same or similar to that shown in FIG. 4. For example, the aerated wet premix can be cast into a mold to form a sheet with two opposing faces. The mold can then be placed on a hot plate or a heated moving belt or any other suitable heating device having a planar heated surface characterized by a controlled surface temperature of about 80°C to about 170°C, preferably about 90°C to about 150°C, more preferably about 100°C to about 140°C. By transferring heat energy by conduction from the planar heated surface to the bottom surface of the sheet of aerated wet premix, the solidification of the sheet starts from the bottom region and gradually moves upward to finally reach the top region. To ensure that the heating direction is primarily anti-gravity (i.e., substantially offset from the gravity direction) during this process, the heated surface is preferably the primary heat source of the sheet being dried. If any other heating source is present, the overall heating direction may be changed accordingly. More preferably, the heated surface is the only heat source for the sheet during drying.
[0067] In another particular embodiment, the anti-gravity heating direction is provided by a rotating drum heating / drying configuration, also referred to as drum drying or roller drying, similar to that shown in FIG. 5. Drum drying is a type of contact drying method used to dry liquid from a viscous premix of raw materials on the exterior surface of a heated rotatable drum (also referred to as a roller or cylinder) at relatively low temperatures to form a sheet-like article. It is a continuous drying process that is particularly suitable for drying large quantities. Because drying is performed at relatively low temperatures via contact heating / drying, it is typically energy efficient and does not adversely affect the compositional integrity of the raw materials.
[0068] The heated rotatable cylinder used in drum drying is internally heated, for example by steam or electricity, and rotated by an electric drive attached to a base bracket at a predetermined rotational speed. The heated rotatable cylinder or drum preferably has an outer diameter in the range of about 0.5 meters to about 10 meters, preferably about 1 meter to about 5 meters, more preferably about 1.5 meters to about 2 meters. It may have a controlled surface temperature of about 80°C to about 170°C, preferably about 90°C to about 150°C, more preferably about 100°C to about 140°C. Furthermore, such a heated rotatable cylinder rotates at a speed of about 0.005 rpm to about 0.25 rpm, preferably about 0.05 rpm to about 0.2 rpm, more preferably about 0.1 rpm to about 0.18 rpm.
[0069] The total drying time in the present invention depends on the amount of ingredients and solids content in the wet premix, the drying temperature, the heat energy flow rate, and the thickness of the sheet material being dried. Preferably, the drying time is from about 1 minute to about 60 minutes, preferably from about 2 minutes to about 30 minutes, more preferably from about 2 minutes to about 15 minutes, even more preferably from about 2 minutes to about 10 minutes, and most preferably from about 2 minutes to about 5 minutes.
[0070] During such drying time, the heating direction is arranged to be substantially opposite the direction of gravity for more than half of the drying time, preferably more than 55% or 60% of the drying time (e.g., as in the rotary drum heating / drying configuration described above), more preferably more than 75% or even 100% of the drying time (e.g., as in the bottom conduction heating / drying configuration described above). Furthermore, the sheet of aerated wet premix can be dried for a first duration under a first heating direction and then dried for a second duration under a second, opposing heating direction, the first heating direction being substantially opposite the direction of gravity, the first duration being anywhere between 51% and 99% (e.g., 55%, 60%, 65%, 70% to 80%, 85%, 90%, or 95%) of the total drying time. Such a change in heating direction can be easily achieved by various other configurations not shown herein, for example, by a serpentine-shaped elongated heating belt that can rotate along its longitudinal center axis.
[0071] IV. Physical Properties of Solid Sheets The flexible porous soluble solid sheets formed by the above-mentioned processing steps are characterized by an improved pore structure that allows easier water ingress into the sheet and faster dissolution of the sheet in water. Such improved pore structure is achieved primarily by adjusting the various processing conditions as described above, which are relatively independent or unaffected by the chemical formulation or specific ingredients used in making such sheets.
[0072] In general, such solid sheets may be characterized by (i) a percent open cell content of about 80%-100%, preferably about 85%-100%, more preferably about 90%-100%, as measured by Test 3 below, and (ii) an overall average pore size of about 100 μm to about 2000 μm, preferably about 150 μm to about 1000 μm, more preferably about 200 μm to about 600 μm, as measured by the Micro-CT method described in Test 2 below. The overall average pore size defines the porosity of the OCF structure of the present invention. The percent open cell content defines the interconnectivity between the pores in the OCF structure of the present invention. The interconnectivity of the OCF structure may also be described by the star volume or Structure Model Index (SMI) as disclosed in WO2010077627 and WO2012138820.
[0073] Such solid sheets of the present invention have opposing top and bottom surfaces, and the top surface may be characterized by a surface average pore diameter of greater than about 100 μm, preferably greater than about 110 μm, preferably greater than about 120 μm, more preferably greater than about 130 μm, and most preferably greater than about 150 μm, as measured by the SEM method described in Test 1 below. Compared to solid sheets formed by conventional heating / drying configurations (e.g., convection, microwave, or impingement oven configurations), solid sheets formed by the improved heating / drying configurations of the present invention have significantly larger surface average pore diameters at their top surface (as shown in Figures 6A-6B, which are described in detail in Example 1 below). This is because, under the specifically prepared directional heating of the present invention, the top surface of the formed sheet of aerated wet premix dries / solidifies last, and the air bubbles near the top surface have the longest time to expand and form larger pore openings at the top surface.
[0074] Furthermore, the solid sheet formed by the improved heating / drying (e.g., rotary drum heating / drying) configuration of the present invention is characterized by a more uniform pore size distribution between different regions along its thickness direction compared to sheets formed by other heating / drying configurations (e.g., impingement oven). Specifically, the solid sheet of the present invention includes a top region adjacent to the top surface, a bottom region adjacent to the bottom surface, and a middle region therebetween, the top region, middle region, and bottom region all having the same thickness. Each of the top region, middle region, and bottom region of such a solid sheet is characterized by an average pore size, with the ratio of the average pore size in the bottom region to the average pore size in the top region (i.e., bottom to top average pore size ratio) being about 0.6 to about 1.5, preferably about 0.7 to about 1.4, preferably about 0.8 to about 1.3, more preferably about 1 to about 1.2. In comparison, solid sheets formed by impingement oven heating / drying configurations may have bottom to top average pore size ratios of greater than 1.5, typically about 1.7 to 2.2 (as shown in Example 1 below). The solid sheets of the present invention may also be characterized by bottom to middle average pore size ratios of about 0.5 to about 1.5, preferably about 0.6 to about 1.3, more preferably about 0.8 to about 1.2, and most preferably about 0.9 to about 1.1, as well as middle to top average pore size ratios of about 1 to about 1.5, preferably about 1 to about 1.4, and more preferably about 1 to about 1.2.
[0075] Furthermore, the relative standard deviation (RSTD) between the average pore sizes in the top, middle, and bottom regions of the solid sheets of the present invention is 20% or less, preferably 15% or less, more preferably 10% or less, and most preferably 5% or less. In contrast, solid sheets formed by the impingement oven heating / drying configuration may have an RSTD between the top / middle / bottom average pore sizes of more than 20%, perhaps more than 25%, or even more than 35% (as shown in Example 1 below).
[0076] Preferably, the solid sheets of the present invention are further characterized by an average cell wall thickness of from about 5 μm to about 200 μm, preferably from about 10 μm to about 100 μm, and more preferably from about 10 μm to about 80 μm, as measured by Test 2 below.
[0077] The solid sheet of the present invention may contain a small amount of water. Preferably, it is characterized by a final moisture content of 0.5% to 25%, preferably 1% to 20%, more preferably 3% to 10% by weight of the solid sheet, measured by Test 4 below. A suitable final moisture content in the resulting solid sheet can ensure the desired flexibility / deformability of the sheet as well as provide a soft / smooth feel to the consumer. If the final moisture content is too low, the sheet may be too brittle or too stiff. If the final moisture content is too high, the sheet may be too sticky and its overall structural integrity may be compromised.
[0078] The solid sheets of the present invention may have a thickness ranging from about 0.6 mm to about 3.5 mm, preferably from about 0.7 mm to about 3 mm, more preferably from about 0.8 mm to about 2 mm, and most preferably from about 1 mm to about 2 mm. The thickness of the solid sheet can be measured using Test 6 described below. The solid sheet after drying may be slightly thicker than a sheet of aerated wet premix due to pore expansion resulting in an overall volume expansion.
[0079] The solid sheet of the present invention has a hardness of about 50 grams / m2, as measured by Test 6 described below. 2 ~ approx. 500g / m 2 , preferably about 150 g / m 2 ~ approx. 450g / m 2 , more preferably about 250 grams / m 2 ~ approx. 400g / m 2 The sheet may be further characterized by its basis weight.
[0080] Furthermore, the solid sheets of the present invention have a compressibility of about 0.05 grams / cm as measured by Test 7 below.3 ~ approx. 0.5g / cm 3 , preferably about 0.06 g / cm 3 ~ approx. 0.4g / cm 3 , more preferably about 0.07 grams / cm 3 ~ approx. 0.2g / cm 3 , and most preferably about 0.08 grams / cm 3 ~ approx. 0.15g / cm 3 The density of the solid sheets of the present invention is lower than that of a sheet of aerated wet premix due in part to pore expansion which leads to an overall volume expansion.
[0081] In some embodiments, the solid sheets of the present invention have a density of about 0.06 grams / cm 3 ~ approx. 0.16g / cm 3 , preferably about 0.07 g / cm 3 ~ approx. 0.15g / cm 3 , more preferably about 0.08 grams / cm 3 ~ approx. 0.145 g / cm 3 Solid articles containing such relatively low density sheets may achieve even more improved leakage performance.
[0082] Furthermore, the solid sheets of the present invention have a thickness of about 0.03 m, as measured by Test 8 described below. 2 / g~approx.0.25m 2 / g, preferably about 0.04m 2 / g~approx.0.22m 2 / g, more preferably 0.05m 2 / g~0.2m 2 / g, most preferably 0.1m 2 / g~0.18m 2 The specific surface area of the solid sheet of the present invention may be indicative of its porosity and may affect its dissolution rate, e.g., the higher the specific surface area, the more porous the sheet is and the faster its dissolution rate.
[0083] In a preferred embodiment, the solid sheet according to the present disclosure and / or the dissolvable solid article according to the present disclosure comprises: an open cell content of 85% to 100%, preferably 90% to 100%, and / or an overall average pore size of 150 μm to 1000 μm, preferably 200 μm to 600 μm, and / or an average cell wall thickness of 5 μm to 200 μm, preferably 10 μm to 100 μm, more preferably 10 μm to 80 μm, and / or a final moisture content of 0.5% to 25% by weight of the solid sheet article, preferably 1% to 20% by weight, more preferably 3% to 10% by weight, and / or a thickness of 0.6 mm to 3.5 mm, preferably 0.7 mm to 3 mm, more preferably 0.8 mm to 2 mm, and most preferably 1 mm to 2 mm; and / or Approximately 50g / m 2 ~ approx. 500g / m 2 , preferably about 150 g / m 2 ~ approx. 450g / m 2 , more preferably about 250 grams / m 2 ~ approx. 400g / m 2 and / or 0.05g / cm 3 ~0.5g / cm 3 , preferably 0.06 g / cm 3 ~0.4g / cm 3 , more preferably 0.07 g / cm 3 ~0.2g / cm 3 , most preferably 0.08 g / cm 3 ~0.15g / cm 3 and / or 0.03m 2 / g~0.25m 2 / g, preferably 0.04m 2 / g~0.22m 2 / g, more preferably 0.05m 2 / g~0.2m 2 / g, most preferably 0.1m 2 / g~0.18m 2It is characterized by its specific surface area in g / g.
[0084] V. Solid Sheet Formulations 1. Water-soluble polymers As mentioned above, the flexible porous dissolvable solid sheets of the present invention can be formed by a wet premix comprising a water-soluble polymer and a first surfactant. Such water-soluble polymer can function as a film former, structuring agent, and carrier for other active ingredients (e.g., surfactants, emulsifiers, builders, chelating agents, fragrances, colorants, etc.) in the resulting solid sheet.
[0085] Preferably, the wet premix may comprise from about 3% to about 20% water soluble polymer, by weight of the premix, and in one embodiment from about 5% to about 15% water soluble polymer, and in one embodiment from about 7% to about 10% water soluble polymer, by weight of the premix.
[0086] After drying, the water-soluble polymer is preferably present in the flexible porous dissolvable solid sheet of the invention in an amount ranging from about 5% to about 60% by weight, preferably from about 7% to about 50% by weight, more preferably from about 9% to about 40% by weight, and most preferably from about 10% to about 30% by weight, such as 10%, 12%, 15%, 18%, 20%, 25%, 30% by weight, or any range therebetween, based on the total weight of the solid sheet. In a particularly preferred embodiment of the invention, the total amount of water-soluble polymer present in the flexible porous dissolvable solid sheet of the invention is 25% by weight or less based on the total weight of such sheet.
[0087] Water-soluble polymers suitable for the practice of the present invention may be selected to have a weight average molecular weight ranging from about 5,000 to about 400,000 Daltons, preferably from about 10,000 to about 300,000 Daltons, more preferably from about 15,000 to about 200,000 Daltons, and most preferably from about 20,000 to about 150,000 Daltons. The weight average molecular weight is calculated by adding the average molecular weight of each polymer raw material multiplied by its relative weight percentage by weight of the total weight of polymer present in the porous solid sheet. The weight average molecular weight of the water-soluble polymer used herein may affect the viscosity of the wet premix, which in turn may affect the number and size of bubbles during the aeration step, and the pore expansion / opening results during the drying step. Additionally, the weight average molecular weight of the water-soluble polymer may affect the overall film-forming properties of the wet premix, and its compatibility / incompatibility with certain surfactants.
[0088] Water soluble polymers of the present invention may include, but are not limited to, synthetic polymers including polyvinyl alcohol, polyvinylpyrrolidone, polyalkylene oxides, polyacrylates, caprolactams, polymethacrylates, polymethylmethacrylates, polyacrylamides, polymethylacrylamides, polydimethylacrylamides, polyethylene glycol monomethacrylates, copolymers of acrylic acid and methyl acrylate, polyurethanes, polycarboxylic acids, polyvinyl acetates, polyesters, polyamides, polyamines, polyethyleneimines, maleic acid / (acrylate or methacrylate) copolymers, copolymers of methyl vinyl ether and maleic anhydride, copolymers of vinyl acetate and crotonic acid, copolymers of vinylpyrrolidone and vinyl acetate, copolymers of vinylpyrrolidone and caprolactam, copolymers of vinylpyrrolidone / vinyl acetate, copolymers of anionic, cationic and amphoteric monomers, and combinations thereof.
[0089] The water soluble polymers of the present invention may also be selected from polymers of natural origin including those of vegetable origin with examples such as karaya gum, tragacanth gum, gum arabic, acemannan, konjac mannan, acacia gum, ghatti gum, whey protein isolate, and soy protein isolate, seed extracts including guar gum, locust bean gum, quince seed, and psyllium seed, seaweed extracts such as carrageenan, alginic acid, and agar, fruit extracts (pectins), those of microbial origin including xanthan gum, gellan gum, pullulan, hyaluronic acid, chondroitin sulfate, and dextran; and those of animal origin including casein, gelatin, keratin, keratin hydrolysate, keratin sulfonate, albumin, collagen, glutelin, glucagon, gluten, zein, and shellac.
[0090] Modified natural polymers may also be used as water-soluble polymers in the present invention.Suitable modified natural polymers include, but are not limited to, cellulose derivatives such as hydroxypropyl methylcellulose, hydroxymethylcellulose, hydroxyethylcellulose, methylcellulose, hydroxypropylcellulose, ethylcellulose, carboxymethylcellulose, cellulose acetate phthalate, nitrocellulose and other cellulose ethers / esters, and guar derivatives such as hydroxypropyl.
[0091] The water-soluble polymer of the present invention may comprise starch. As used herein, the term "starch" includes both naturally occurring starch and modified starch. Typical natural sources of starch can include cereals, tubers, roots, legumes and fruits. More specific natural sources can include corn, beans, potatoes, bananas, barley, wheat, rice, sago, amaranth, tapioca, arrowroot, canna, sorghum, and their waxy or higher amylase species. Native starch can be modified by any modification method known in the art to form modified starches, including physically modified starches such as sheared or thermally inhibited starches, chemically modified starches such as crosslinked, acetylated, and organic esterification, hydroxyethylated, and hydroxypropylated, phosphorylation, and inorganic esterification, cationic, anionic, nonionic, amphoteric and zwitterionic, and their succinate and substituted succinate derivatives, conversion products derived from starch including fluid or thin boiled starches prepared by oxidation, enzymatic conversion, acid hydrolysis, heat or acid dextrinization, heat and / or sheared products, heat and / or sheared products that may be useful herein, and pregelatinized starches known in the art.
[0092] Preferred water-soluble polymers of the present invention include polyvinyl alcohol, polyvinylpyrrolide, polyalkylene oxide, starch and starch derivatives, pullulan, gelatin, hydroxypropylmethylcellulose, methylcellulose, and carboxymethylcellulose. More preferred water-soluble polymers of the present invention include polyvinyl alcohol and hydroxypropylmethylcellulose.
[0093] The most preferred water-soluble polymers of the present invention are polyvinyl alcohols characterized by a degree of hydrolysis ranging from about 40% to about 100%, preferably from about 50% to about 95%, more preferably from about 65% to about 92%, and most preferably from about 70% to about 90%. Commercially available polyvinyl alcohols include those available under the tradename CELVOL from Celanese Corporation (Texas, USA), including but not limited to those available under the tradenames CELVOL 523, CELVOL 530, CELVOL 540, CELVOL 518, CELVOL 513, CELVOL 508, CELVOL 504, those available under the tradenames Mowiol® and POVAL® from Kuraray Europe GmbH (Frankfurt, Germany), PVA 1788 (also referred to as PVA BP17) available from a variety of sources including Lubon Vinylon Co. (Nanjing, China), and combinations thereof. In a particularly preferred embodiment of the present invention, the flexible porous dissolvable solid sheet comprises from about 10% to about 25% by weight, more preferably from about 15% to about 23% by weight, based on the total weight of such sheet, of polyvinyl alcohol having a weight average molecular weight in the range of 80,000 to about 150,000 Daltons and a degree of hydrolysis in the range of about 80% to about 90%.
[0094] In addition to polyvinyl alcohol as described above, a single starch or combination of starches may be used as a filler material in an amount that reduces the overall concentration of water-soluble polymer required, as long as it helps provide a solid sheet with the requisite structure and physical / chemical properties as described herein. However, too much starch may affect the solubility and structural integrity of the sheet. Thus, in a preferred embodiment of the present invention, the solid sheet article desirably contains no more than 20% by weight of starch, preferably 0% to 10% by weight, more preferably 0% to 5% by weight, and most preferably 0% to 1% by weight of the solid sheet.
[0095] 2. Surfactants In addition to the water-soluble polymers described above, the solid sheets of the present invention include a surfactant, which can act as an emulsifier during the aeration process to generate a sufficient amount of stable air bubbles to form the desired OCF structure of the present invention. Additionally, the surfactant can act as an active ingredient to achieve the desired cleaning effect.
[0096] In a preferred embodiment of the present invention, the solid sheet comprises a surfactant selected from the group consisting of anionic surfactants, nonionic surfactants, cationic surfactants, zwitterionic surfactants, amphoteric surfactants, polymeric surfactants and combinations thereof.Different surfactants can be selected depending on the desired use of such solid sheet and the desired consumer benefits to be achieved.One advantage of the present invention is that the OCF structure of the solid sheet allows high surfactant content to be incorporated while still providing fast dissolution.As a result, high concentration of cleaning composition can be incorporated into the solid sheet of the present invention to provide consumers with a new and excellent cleaning experience.
[0097] Surfactants as used herein may include surfactants in both the conventional sense (i.e., surfactants that provide a consumer-perceived lathering effect) and emulsifiers (i.e., those that do not provide any lathering performance, but are intended primarily as a process aid in creating a stable foam structure). Examples of emulsifiers used as surfactant components herein include mono- and di-glycerides, fatty alcohols, polyglycerol esters, propylene glycol esters, sorbitan esters, and other emulsifiers commonly used to stabilize the air interface by known or otherwise methods.
[0098] The total amount of surfactant present in the solid sheet of the present invention may range from about 5% to about 95% by weight, preferably about 30% to about 90% by weight, preferably about 40% to about 80% by weight, more preferably about 50% to about 70% by weight, for example, 20%, 30%, 40%, 50%, 60%, 70%, 80% by weight, or any range therebetween, based on the total weight of the solid sheet. As a result, the wet premix may contain from about 1% to about 50% by weight of the wet premix surfactant, in one embodiment from about 2% to about 40% by weight of the wet premix surfactant, in one embodiment from about 10% to about 35% by weight of the wet premix surfactant, in one embodiment from about 15% to about 30% by weight of the wet premix surfactant.
[0099] Non-limiting examples of anionic surfactants suitable for use herein include alkyl and alkyl ether sulfates, sulfated monoglycerides, sulfonated olefins, alkylaryl sulfonates, primary or secondary alkane sulfonates, alkyl sulfosuccinates, acyltaurates, acyl isethionates, alkyl glyceryl ether sulfonates, sulfonated methyl esters, sulfonated fatty acids, alkyl phosphates, acyl glutamates, acyl sarcosinates, alkyl sulfoacetates, acylated peptides, alkyl ether carboxylates, acyl lactylates, anionic fluorosurfactants, sodium lauroyl glutamate, and combinations thereof.
[0100] One category of anionic surfactants that are particularly suitable for the practice of the present invention is C6-C 20 Examples of suitable surfactants that can be used in the present invention include linear alkylbenzene sulphonate (LAS) surfactants. LAS surfactants are well known in the art and can be readily obtained by sulfonating commercially available linear alkylbenzenes. 10 ~C 20 As linear alkylbenzene sulfonates, C 10~C 20 Alkali metal salts, alkaline earth metal salts, or ammonium salts of linear alkylbenzene sulfonic acid, preferably C 11 ~C 18 Or C 11 ~C 14 Examples of the salts include sodium, potassium, magnesium, and / or ammonium salts of linear alkylbenzene sulfonic acid. More preferred are 12 and / or C. 14 The sodium or potassium salt of linear alkylbenzene sulfonic acid is preferably C 12 and / or C. 14 The sodium salts of linear alkylbenzene sulfonates, i.e., sodium dodecylbenzene sulfonate or sodium tetradecylbenzene sulfonate.
[0101] LAS provides excellent cleaning effects and is particularly suitable for use in laundry detergent applications. It was a surprising and unexpected discovery of the present invention that when polyvinyl alcohol having a higher weight average molecular weight (e.g., about 50,000 to about 400,000 Daltons, preferably about 60,000 to about 300,000 Daltons, more preferably about 70,000 to about 200,000 Daltons, most preferably about 80,000 to about 150,000 Daltons) is used as the film former and carrier, LAS can be used as the primary surfactant, i.e., can be present in an amount of more than 50% by weight of the total surfactant content in the solid sheet without adversely affecting the film forming performance and stability of the overall composition. Correspondingly, in certain embodiments of the present invention, LAS is used as the primary surfactant in the solid sheet. When LAS is present in the solid sheet of the present invention, the amount thereof may range from about 10% to about 70% by weight, preferably from about 20% to about 65% by weight, and more preferably from about 40% to about 60% by weight, based on the total weight of the solid sheet.
[0102] Another category of anionic surfactants suitable for the practice of the present invention includes sodium trideceth sulfates (STS) having a weight average degree of alkoxylation ranging from about 0.5 to about 5, preferably from about 0.8 to about 4, more preferably from about 1 to about 3, and most preferably from about 1.5 to about 2.5. Trideceth, in one embodiment, is a 13-carbon branched alkoxylated hydrocarbon containing an average of at least one methyl branch per molecule. STS used in the present invention can include ST(EOxPOy)S, where EOx represents a repeating ethylene oxide unit having a repeat number x ranging from 0 to 5, preferably from 1 to 4, more preferably from 1 to 3, and POy represents a repeating propylene oxide unit having a repeat number y ranging from 0 to 5, preferably from 0 to 4, more preferably from 0 to 2. For example, it is understood that a material such as ST2S having a weight average degree of ethoxylation of about 2 may contain significant amounts of molecules with no ethoxylates, 1 mole of ethoxylate, 3 moles of ethoxylate, etc., and the distribution of ethoxylation can be broad, narrow, or truncated and still result in a total weight average degree of ethoxylation of about 2. It was a surprising and unexpected discovery of the present invention that STS is particularly suitable for personal cleansing applications, and that when polyvinyl alcohol having a higher weight average molecular weight (e.g., about 50,000 to about 400,000 daltons, preferably about 60,000 to about 300,000 daltons, more preferably about 70,000 to about 200,000 daltons, most preferably about 80,000 to about 150,000 daltons) is used as the film former and carrier, STS can be used as the primary surfactant, i.e., can be present in an amount of more than 50% by weight of the total surfactant content in the solid sheet without adversely affecting the film forming performance and stability of the overall composition. Correspondingly, in certain embodiments of the present invention, STS is used as the primary surfactant in the solid sheet. When STS is present in the solid sheet of the present invention, the amount may range from about 10% by weight to about 70% by weight, preferably about 20% by weight to about 65% by weight, more preferably about 40% by weight to about 60% by weight, based on the total weight of the solid sheet.
[0103] Another category of anionic surfactants suitable for the practice of the present invention includes the alkyl sulfates. These materials have the corresponding formula: ROSO3M, where R is an alkyl or alkenyl of about 6 to about 20 carbon atoms, x is 1 to 10, and M is a water soluble cation such as ammonium, sodium, potassium, and triethanolamine. Preferably, R has about 6 to about 18, preferably about 8 to about 16, and more preferably about 10 to about 14 carbon atoms. As previously mentioned, the non-alkoxylated C6-C 20 Linear or branched alkyl sulfates (AS) are considered to be preferred surfactants in soluble solid sheets, especially as the main surfactant therein, due to their compatibility with low molecular weight polyvinyl alcohols (e.g., those having a weight average molecular weight of 50,000 Daltons or less) in film forming performance and stability. However, it was a surprising and unexpected discovery of the present invention that when polyvinyl alcohols having a higher weight average molecular weight (e.g., about 50,000 to about 400,000 Daltons, preferably about 60,000 to about 300,000 Daltons, more preferably about 70,000 to about 200,000 Daltons, most preferably about 80,000 to about 150,000 Daltons) are used as film formers and carriers, other surfactants (e.g., LAS and / or STS) can be used as the main surfactant in the solid sheet without adversely affecting the film forming performance and stability of the overall composition. Therefore, in particularly preferred embodiments of the present invention, it is desirable to provide a solid sheet having no more than about 20% by weight of the solid sheet AS, preferably 0% to about 10% by weight, more preferably 0% to about 5% by weight, and most preferably 0% to about 1% by weight.
[0104] Another category of anionic surfactants suitable for the practice of the present invention includes C6-C 20 Linear or branched chain alkylalkoxy sulfates (AAS) are also included. Within this category, the corresponding formula RO(C2H4O) xParticularly preferred are linear or branched alkylethoxy sulfates (AES) having the formula SO3M, where R is an alkyl or alkenyl of about 6 to about 20 carbon atoms, x is 1 to 10, and M is a water soluble cation such as ammonium, sodium, potassium, and triethanolamine. Preferably, R has about 6 to about 18, preferably about 8 to about 16, and more preferably about 10 to about 14 carbon atoms.
[0105] The nonionic surfactants that may be included in the solid sheets of the present invention may be any conventional nonionic surfactant, including, but not limited to, alkyl alkoxylated alcohols, alkyl alkoxylated phenols, alkyl polysaccharides (particularly alkyl glucosides and alkyl polyglucosides), polyhydroxy fatty acid amides, alkoxylated fatty acid esters, sucrose esters, sorbitan esters and alkoxylated derivatives of sorbitan esters, amine oxides, etc. Preferred nonionic surfactants are represented by the formula R 1 (OC2H4) n OH (in the formula, R 1 is C8~C 18 and n is an alkyl or alkylphenyl group, and n is from about 1 to about 80. Particularly preferred are C8-C10 nonionic surfactants having a weight average degree of ethoxylation of from about 1 to about 20, preferably from about 5 to about 15, and more preferably from about 7 to about 10, such as the NEODOL® nonionic surfactants available from Shell. 18 Other non-limiting examples of nonionic surfactants useful herein include C6-C alkoxylated alcohols, where the alkoxylate units can be ethyleneoxy units, propyleneoxy units, or mixtures thereof. 12 Alkylphenol alkoxylate; C 12 ~C 18 C6-C with alcohol and ethylene oxide / propylene oxide block polymer 12 Alkylphenol condensates (such as Pluronic® (BASF)); C 14 ~C 22Medium-chain branched alcohol (BA); C 14 ~C 22 Medium Branched Chain Alkyl Alkoxylate, BAE x (wherein x is 1 to 30); alkyl polysaccharides, particularly alkyl polyglycosides; polyhydroxy fatty acid amides; and ether-terminated poly(oxyalkylated) alcohol surfactants. Suitable nonionic surfactants also include those sold by BASF under the trade name Lutensol®.
[0106] The most preferred nonionic surfactants for the practice of the present invention are C6-C alkoxylated surfactants having a weight average degree of alkoxylation in the range of 5 to 15. 20 Linear or branched alkylalkoxylated alcohols (AA), more preferably C 10 having a weight average degree of alkoxylation in the range of 7 to 9 12 ~C 14 Linear ethoxylated alcohols are included. When the AA type nonionic surfactant is present in the solid sheet of the present invention, the amount thereof may be in the range of about 2% by weight to about 40% by weight, preferably about 5% by weight to about 30% by weight, more preferably about 8% by weight to about 12% by weight, based on the total weight of the solid sheet.
[0107] Amphoteric surfactants suitable for use in the solid sheets of the present invention include those broadly described as derivatives of aliphatic secondary and tertiary amines, where the aliphatic radical may be straight or branched, one of the aliphatic substituents containing from about 8 to about 18 carbon atoms and one containing an anionic water-soluble group, such as carboxy, sulfonate, sulfate, phosphate, or phosphonate. Examples of compounds falling within this definition are sodium 3-dodecylaminopropionate, sodium 3-dodecylaminopropanesulfonate, sodium lauryl sarcosinate, N-alkyltaurines such as those prepared by reacting dodecylamine with sodium isethionate, and N-higher alkyl aspartic acids.
[0108] Suitable zwitterionic surfactants include those broadly described as derivatives of aliphatic quaternary ammonium, phosphonium and sulfonium compounds, in which the aliphatic radicals can be straight or branched chain, one of the aliphatic substituents containing from about 8 to about 18 carbon atoms and one containing an anionic group, such as a carboxy, sulfonate, sulfate, phosphate or phosphonate. Such suitable zwitterionic surfactants can be represented by the formula:
[0109] [ka] (In the formula, R 2 contains an alkyl, alkenyl, or hydroxyalkyl radical of about 8 to about 18 carbon atoms, 0 to about 10 ethylene oxide moieties, and 0 to about 1 glyceryl moiety; Y is selected from the group consisting of nitrogen, phosphorus, and sulfur atoms; R 3 is an alkyl or monohydroxyalkyl group containing from about 1 to about 3 carbon atoms, X is 1 when Y is a sulfur atom and is 2 when Y is a nitrogen or phosphorus atom, R 4 is an alkylene or hydroxyalkylene of about 1 to about 4 carbon atoms, and Z is a radical selected from the group consisting of carboxylate, sulfonate, sulfate, phosphonate, and phosphate groups.
[0110] Cationic surfactants can also be utilized in the present invention, particularly in fabric softener and hair conditioner products. When used in making products containing cationic surfactants as the primary surfactant, such cationic surfactants are preferably present in an amount ranging from about 2% to about 30%, preferably from about 3% to about 20%, more preferably from about 5% to about 15%, based on the total weight of the solid sheet.
[0111] Cationic surfactants can include DEQA compounds that include diamide active ingredients and active ingredients with a mixture of amide and ester bonds.Preferred DEQA compounds are typically made by reacting alkanolamines such as MDEA (methyldiethanolamine) and TEA (triethanolamine) with fatty acid.Some materials that typically obtain from such reactions include N,N-di(acyl-oxyethyl)-N,N-dimethylammonium chloride or N,N-di(acyl-oxyethyl)-N,N-methylhydroxyethylammonium methyl sulfate, where acyl groups are derived from animal fat, unsaturated and polyunsaturated fatty acids.
[0112] Polymeric surfactants suitable for use in the personal care compositions of the present invention include, but are not limited to, block copolymers of ethylene oxide and fatty alkyl residues, block copolymers of ethylene oxide and propylene oxide, hydrophobically modified polyacrylates, hydrophobically modified celluloses, silicone polyethers, silicone copolyol esters, diquaternary polydimethylsiloxanes, and co-modified amino / polyether silicones.
[0113] In a preferred embodiment, the surfactant is a C 20 Linear alkylbenzene sulfonates (LAS), C6-C with weight average degree of alkoxylation ranging from 0.5 to 10 20 Linear or branched chain alkyl alkoxy sulfates (AAS), C6-C with a weight average degree of alkoxylation ranging from 5 to 15 20 Linear or branched chain alkyl alkoxylated alcohols (AA), C6-C 20 It may be selected from the group consisting of linear or branched chain alkyl sulfates (AS) and any combination thereof.
[0114] 3. Plasticizers In a preferred embodiment of the present invention, the flexible porous dissolvable solid sheet of the present invention may further comprise a plasticizer, preferably in an amount ranging from about 0.1% to about 25% by weight, preferably about 0.5% to about 20% by weight, more preferably about 1% to about 15% by weight, and most preferably 2% to 12% by weight, based on the total weight of the solid sheet. Correspondingly, the wet premix used to form such a solid sheet may comprise from about 0.02% to about 20% by weight of the wet premix of plasticizer, in one embodiment from about 0.1% to about 10% by weight of the wet premix of plasticizer, in one embodiment from about 0.5% to about 5% by weight of the wet premix of plasticizer.
[0115] Plasticizers suitable for use in the present invention include, for example, polyols, copolyols, polycarboxylic acids, polyesters, dimethicone copolyols, and the like.
[0116] Examples of useful polyols include, but are not limited to, glycerin, diglycerin, ethylene glycol, polyethylene glycol (especially 200-600), propylene glycol, butylene glycol, pentylene glycol, glycerol derivatives (such as propoxylated glycerol), glycidol, cyclohexanedimethanol, hexanediol, 2,2,4-trimethylpentane-1,3-diol, pentaerythritol, urea, sugar alcohols (such as sorbitol, mannitol, lactitol, xylitol, maltitol, and other mono- and polyhydric alcohols), mono-, di-, and oligo-saccharides (such as fructose, glucose, sucrose, maltose, lactose, high fructose corn syrup solids, and dextrins), ascorbic acid, sorbates, ethylene bisformamide, amino acids, and the like.
[0117] Examples of polycarboxylic acids include, but are not limited to, citric acid, maleic acid, succinic acid, polyacrylic acid, and polymaleic acid.
[0118] Examples of suitable polyesters include, but are not limited to, glycerol triacetate, acetylated monoglyceride, diethyl phthalate, triethyl citrate, tributyl citrate, acetyl triethyl citrate, acetyl tributyl citrate.
[0119] Examples of suitable dimethicone copolyols include, but are not limited to, PEG-12 dimethicone, PEG / PPG-18 / 18 dimethicone, and PPG-12 dimethicone.
[0120] Particularly preferred examples of plasticizers include glycerin, ethylene glycol, polyethylene glycol, propylene glycol, and mixtures thereof. The most preferred plasticizer is glycerin.
[0121] 4. Additional Ingredients In addition to the above-mentioned components, such as water-soluble polymers, surfactants, and plasticizers, the solid sheet of the present invention may contain one or more additional components depending on its intended use. Such one or more additional components may be selected from the group consisting of fabric care actives, dishwashing actives, hard surface cleaning actives, beauty and / or skin care actives, personal cleansing actives, hair care actives, oral care actives, feminine care actives, baby care actives, bittering agents, and any combination thereof. In a preferred embodiment, the solid sheet of the present invention may contain bittering agents.
[0122] The solid sheets of the present invention may further comprise other optional ingredients as are known or useful for use in compositions, provided that such optional materials are compatible with the selected essential materials described herein or do not unduly impair product performance.
[0123] Non-limiting examples of product type embodiments that may be formed with the solid sheets of the present invention include laundry detergent products, fabric softener products, hand washing products, hair shampoos or other hair treatment products, body cleansing products, shaving preparation products, dishwashing products, personal care substrates containing pharmaceutical or other skin care actives, moisturizing products, sunscreen products, beauty or skin care products, deodorant products, oral care products, feminine cleaning products, baby care products, fragrance-containing products, and the like.
[0124] VI. Coating Composition Formulations The coating composition according to the present disclosure may include a non-aqueous liquid carrier, a thickener, and solid particles. In some embodiments, the coating composition is at 20° C. and 1 s -1 The viscosity may be from about 1 cps to about 25,000 cps, preferably from about 2 cps to about 10,000 cps, more preferably from about 3 cps to about 5,000 cps, and most preferably from about 1,000 cps to about 5,000 cps, as measured by . Viscosity values are measured using a Malvern Kinexus Lab+ rheometer (CP1 / 50 SR3468 SS) with cone and plate geometry at a gap width of 0.054 mm, a temperature of 20° C., and a shear rate of 1.0 reciprocal seconds over 360 seconds.
[0125] 1. Non-aqueous liquid carrier The coating composition may comprise from 1 wt% to 99 wt%, preferably from 5 wt% to 70 wt%, more preferably from 20 wt% to 50 wt%, for example, 1 wt%, 2 wt%, 3 wt%, 4 wt%, 5 wt%, 6 wt%, 7 wt%, 8 wt%, 9 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 95 wt%, or any range therebetween of the non-aqueous liquid carrier, based on the total weight of the coating composition.
[0126] The non-aqueous liquid carrier may be selected from the group consisting of polyethylene glycol, polypropylene glycol, silicone, fatty acid, perfume oil, non-ionic surfactant, organic solvent, and any combination thereof. Preferably, the non-aqueous liquid carrier may include a non-ionic surfactant. The non-ionic surfactant may be any suitable non-ionic surfactant listed above. In a more preferred embodiment, the non-ionic surfactant is a C6-C alkoxylation ester having a weight average degree of alkoxylation in the range of 5 to 15. 20 Linear or branched alkyl alkoxylated alcohols (AA), preferably C having a weight average degree of alkoxylation in the range of 7 to 9. 12 ~C 14 In another embodiment, the non-aqueous liquid carrier may comprise a polyethylene glycol having a weight average molecular weight of less than 1000, less than 800, or less than 600.
[0127] 2. Thickener The coating composition may comprise from 0.01 wt% to 30 wt%, preferably from 0.05 wt% to 20 wt%, more preferably from 0.1 wt% to 10 wt%, for example, 0.1 wt%, 0.2 wt%, 0.3 wt%, 0.4 wt%, 0.5 wt%, 0.6 wt%, 0.7 wt%, 0.8 wt%, 0.9 wt%, 1.0 wt%, 1.5 wt%, 2.0 wt%, 2.5 wt%, 3.0 wt%, 3.5 wt%, 4.0 wt%, 4.5 wt%, 5.0 wt%, 6.0 wt%, 7.0 wt%, 8.0 wt%, 9.0 wt%, or any range therebetween of thickening silica based on the total weight of the coating composition.
[0128] In particular, the thickener may be selected from the group consisting of silica, clay, polyacrylate thickener, polyacrylamide thickener, xanthan thickener, guar gum, alginate ethoxylated cellulose, hydroxypropyl cellulose, hydroxyethyl cellulose, and any combination thereof. Preferably, the thickener may comprise silica, preferably fumed silica, more preferably hydrophilic fumed silica (e.g., Aerosil A200). The hydrophilic fumed silica may contain less than 10% residual salts based on the total weight of the silica, and upon hydration may form swollen silica particles having a particle size distribution Dv50 of 1 μm to 100 μm. In particular, the fumed silica used in the present invention has a particle size distribution Dv50 of about 30 to about 1000 m. 2 / g, preferably about 50 to about 500m 2 / g, e.g., 50, 100, 150, 200, 250, 300, 350, 400, 450m 2 / g, or any range therebetween.
[0129] 3.Solid particles The solid particles contained in the coating composition according to the present invention may include oxidative dye compounds, pH adjusters and / or buffers, radical scavengers, chelating agents, warming actives, color indicators, anionic surfactants, enzymes, bleaching agents, effervescent systems, and any combination thereof. In some embodiments, the solid particles have a preferred average particle size of 80 μm to 2000 μm. In particular, the particles may have an average particle size of 90 μm to 1000 μm, preferably 100 μm to 700 μm, more preferably 110 μm to 500 μm, and most preferably 120 μm to 400 μm, such as 100 μm, 200 μm, 300 μm, 400 μm, 500 μm, 600 μm, 700 μm, 800 μm, 900 μm, 1000 μm, 1100 μm, 1200 μm, or any range therebetween.
[0130] The coating composition may comprise 1 wt% to 99 wt%, preferably 5 wt% to 90 wt%, more preferably 30 wt% to 70 wt%, for example 1 wt%, 2 wt%, 3 wt%, 4 wt%, 5 wt%, 6 wt%, 7 wt%, 8 wt%, 9 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 95 wt%, or any range therebetween of solid particles based on the total weight of the coating composition.
[0131] a) Oxidation dye compounds The solid particles contained in the coating compositions according to the present invention may include oxidative dye compounds in the form of primary intermediates or couplers.
[0132] These compounds are well known in the art and include aromatic diamines, aminophenols, aromatic diols, and their derivatives (a representative but non-exhaustive list of oxidative dye precursors can be found in Sagarin, Cosmetic Science and Technology, Interscience, Special Edition, Vol. 2, pp. 308-310). It should be understood that the precursors detailed below are merely examples and are not intended to limit the compositions and processes herein. These are: 1,7-dihydroxynaphthalene (1,7-naphthalenediol), 1,3-diaminobenzene (m-phenylenediamine), 1-methyl-2,5-diaminobenzene (toluene-2,5-diamine), 1,4-diaminobenzene (p-phenylenediamine), 1,3-dihydroxybenzene (resorcinol), 1,3-dihydroxy-4-chlorobenzene, (4-chlororesorcinol), 1-hydroxy-2-aminobenzene, (o-aminophenol), 1-hydroxy-3-aminobenzene (m-aminophenol), 1-hydroxy-4-amino-benzene (p-aminophenol), 1-hydroxynaphthalene (1-naphthol), 1,5-dihydroxynaphthalene (1,5-naphthalenediol), 2,7-dihydroxynaphthalene (2,7-naphthalenediamine). ol), 1-hydroxy-2,4-diaminobenzene (4-diaminophenol), 1,4-dihydroxybenzene (hydroquinone), 1-hydroxy-4-methylaminobenzene (p-methylaminophenol), 6-hydroxybenzo-morpholine (hydroxybenzomorpholine), 1-methyl-2-hydroxy-4-aminobenzene (4-amino-2-hydroxy-toluene), 3,4-diaminobenzoic acid (3,4-diaminobenzoic acid), 1-methyl-2-hydroxy-4-(2'-hydroxyethyl)aminobenzene (2-methyl-5-hydroxy-ethylamino-phenol), 1,2,4-trihydroxybenzene (1,2,4-trihydroxybenzene), 1-phenol-3-methylpyrazol-5-one (phenylmethylpyrazolone), 1-(2'-hydroxyethyloxy)-2,4-Diaminobenzene (2,4-diaminophenoxy-ethanol HCL), 1-hydroxy-3-amino-2,4-dichlorobenzene (3-amino-2,4-dichloro-phenol), 1,3-dihydroxy-2-methylbenzene (2-methylresorcinol), 1-amino-4-bis-(2'-hydroxyethyl)aminobenzene (N,N-bis(2-hydroxy-ethyl)-p-phenylene-diamine), 2,4,5,6-tetraaminopyrimidine (HC Red 16), 1-hydroxamyl-2-methylbenzene (2-methyl-2-methyl-3-phenyl-4-phenyl-2-phenyl-1 ...2-phenyl-1-phenyl-2-phenyl-2-phenyl-1-phenyl-2-phenyl-2-phenyl-1-phenyl-2-phenyl-2-phenyl-1-phenyl-2-phenyl-2-phenyl-1-phenyl-2-phenyl-2-phenyl-2-phenyl-1-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2-phenyl-2- 1-hydroxy-3-methyl-4-aminobenzene (4-amino-m-cresol), 1-hydroxy-2-amino-5-methylbenzene (6-amino-m-cresol), 1,3-bis-(2,4-diaminophenoxy)propane (1,3-bis-(2,4-diamino-phenoxy)-propane), 1-(2'-hydroxyethyl)-2,5-diaminobenzene (hydroxyethyl-p-phenylenediamine sulfate), 1-methoxy-2-amino-4-(2'-hydroxyethylamino)benzene , (2-amino-4-hydroxyethylaminoanisole), 1-hydroxy-2-methyl-5-amino-6-chlorobenzene (5-amino-6-chloro-o-cresol), 1-hydroxy-2-amino-6-methylbenzene (6-amino-o-cresol), 1-(2'-hydroxyethyl)-amino-3,4-methylenedioxybenzene (hydroxyethyl-3,4-methylenedioxy-aniline HCl), 2,6-dihydroxy-3,4-dimethylpyridine (2,6-dihydroxy -3,4-dimethylpyridine), 3,5-diamino-2,6-dimethoxypyridine (2,6-dimethoxy-3,5-pyridinediamine), 5,6-dihydroxyindole (dihydroxy-indole), 4-amino-2-aminomethylphenol (2-aminoethyl-p-amino-phenol HCl), 2,4-diamino-5-methylphenetole (2,4-diamino-5-methyl-phenetole HCl), 2,4-diamino-5-(2'-hydroxyethyloxy)toluene (2,4-Diamino-5-methylphenoxyethanol HCl), 5-amino-4-chloro-2-methylphenol (5-amino-4-chloro-o-cresol), 4-amino-1-hydroxy-2-(2'-hydroxyethylaminomethyl)benzene hydroxyethylaminomethyl-p-aminophenol HCl), 4-amino-1-hydroxy-2-methoxymethylbenzene (2-methoxymethyl-p-aminophenol HCl), 1,3-bis(N(2-hydroxyethyl)N(4-amino-phenyl)amino)-2-propanol (hydroxypropyl-bis-(N-hydroxy-ethyl-p-phenylenediamine) HCL), 6-hydroxyindole (6-hydroxy-indole), 2,3-indolidinedione (isatin), 3-amino-2-methylamino-6-methoxypyridine (HC Blue No. 7), 1-phenyl-3-methyl-5-pyrazolone-2,4-dihydro-5,2-phenyl-3H-pyrazol-3-one, 2-amino- 3-Hydroxypyridine (2-amino-3-hydroxypyridine), 5-amino-salicylic acid, 1-methyl-2,6-bis(2-hydroxy-ethylamino)benzene (2,6-hydroxyethylamino-toluene), 4-hydroxy-2,5,6-triaminopyrimidine (2,5,6-triamino-4-pyrimidinol sulfate), 2,2'-[1,2-ethanediyl-bis-(oxy-2,1-ethanediyloxy)]-bis-benzene-1,4-diamine (PEG-3 ,2',2'-di-p-phenylenediamine), 5,6-dihydroxyindoline (dihydroxyindoline), N,N-dimethyl-3-ureidoaniline (m-dimethyl-amino-phenylurea), 2,4-diamino-5-fluortoluene sulfate hydrate (4-fluoro-6-methyl-m-phenylenediamine sulfate), and 1-acetoxy-2-methylnaphthalene (1-hydroxyethyl-4,5-diaminopyrazole sulfate). These can be used in molecular form or in the form of peroxide-compatible salts.
[0133] b) pH adjusters and buffers The solid particles contained in the coating composition according to the present invention may include a pH adjusting and / or buffering agent in an amount effective enough to adjust the pH of the composition to within the range of about 3 to about 13, in some embodiments, about 8 to about 12, and even about 8 to about 11. Suitable pH adjusting and / or buffering agents for use herein include, but are not limited to, ammonia, alkanolamines such as monoethanolamine, diethanolamine, triethanolamine, monopropanolamine, dipropanolamine, tripropanolamine, tripropanolamine, 2-amino-2-methyl-1-propanol, and 2-amino-2-hydroxymethyl-1,3,-propanediol, and guanidinium salts, hydroxides and carbonates of alkali metals and ammonium, preferably sodium hydroxide and ammonium carbonate, and inorganic acids and acidulants such as inorganic acids, for example, phosphoric acid, acetic acid, ascorbic acid, citric acid or tartaric acid, hydrochloric acid, and mixtures thereof.
[0134] c) Radical scavenger system The solid particles contained in the coating composition according to the present invention may contain a radical scavenger in an amount sufficient to reduce damage to hair during the oxidative bleaching or coloring process. The radical scavenger is preferably selected so that it is not of the same species as the alkalizing agent. Preferred radical scavengers may be selected from the classes of alkanolamines, amino sugars, amino acids, and mixtures thereof, and may include, but are not limited to, monoethanolamine, 3-amino-1-propanol, 4-amino-1-butanol, 5-amino-1-pentanol, 1-amino-2-propanol, 1-amino-2-butanol, 1-amino-2-pentanol, 1-amino-3-pentanol, 1-amino-4-pentanol, 3-amino-2-methylpropan-1-ol, 1-amino-2-methylpropan-2-ol, 3-aminopropane-1,2-diol, glucosamine, N-acetylglucosamine, glycine, arginine, lysine, proline, glutamine, histidine, serine, tryptophan, and the potassium, sodium, and ammonium salts of the above, and mixtures thereof. Other preferred radical scavenger compounds include benzylamine, glutamic acid, imidazole, di-tert-butylhydroxytoluene, hydroquinone, catechol, and mixtures thereof.
[0135] d) Chelating Agents The solid particles contained in the coating composition according to the present invention may contain a sufficient amount of chelating agent to reduce the amount of metal available for interaction with the formulation components. Suitable chelating agents for use herein include, but are not limited to, diamine-N,N'-dipolyacids, monoamine monoamide-N,N'-dipolyacids, and N,N'-bis(2-hydroxybenzyl)ethylenediamine-N,N'-diacetic acid chelating agents (preferably EDDS (ethylenediamine disuccinic acid)), carboxylic acids (preferably amino carboxylic acids), phosphonic acids (preferably amino phosphonic acids), and polyphosphoric acids (especially linear polyphosphoric acids), their salts and derivatives.
[0136] e) Warming active substances The solid particles contained in the coating composition according to the present invention may include a warming active. The warming active may include a heat generating agent or a heat generating powder that releases heat through an exothermic reaction (heat generation) when mixed with water during application. Heat generating agents include, but are not limited to, inorganic salts, glycols, finely divided solid sorbent materials, and iron redox systems. In one embodiment, the warming active is selected from the group consisting of anhydrous inorganic salts, including, but not limited to, calcium chloride, magnesium chloride, calcium oxide, magnesium sulfate, aluminum sulfate, and combinations thereof. In yet another embodiment, the warming active of the present invention is selected from the group consisting of anhydrous calcium chloride, anhydrous magnesium chloride, anhydrous magnesium sulfate, and combinations thereof.
[0137] f) Color indicators The solid particles contained in the coating composition according to the present invention may include a color indicator. Such color indicators may be present in an amount sufficient to cause a visual color change when the indicator is in contact with water. The term "visual color change" refers to a color change that can be detected by the human eye alone or with the aid of an energy source such as black light. The color indicators of the present invention may include, but are not limited to, those selected from the group consisting of pH indicators, photoactive pigments, thermochromatic pigments, and combinations thereof.
[0138] In one embodiment, the color change is a pH sensitive color changing component. The color indicator may be selected from the group consisting of bromocresol green, phenolphthalein, σ-cresolphthalein, thymolphthalein, coumarin, 2,3-dioxyxanthone, coumaric acid, 6,8-dinitro-2,4(1H)quinazolinedione, ethyl-bis(2,4-dimethylphenyl)ethanoate, and combinations thereof.
[0139] g) Enzymes The solid particles contained in the coating composition according to the present invention may contain an enzyme. Any enzyme known in the art may be used in the coating composition. Preferred enzymes are selected from the group consisting of proteases, amylases, cellulases, lipases, xyloglucanases, pectate lyases, mannases, cutinases, and any combination thereof.
[0140] h) Bleach The solid particles contained in the coating composition according to the present invention may include a bleaching agent. The bleaching agent may be selected from the group consisting of an available oxygen source, a bleaching activator, a preformed peracid, a bleaching catalyst, a reduced bleaching agent, and any combination thereof. In particular, the bleaching agent may be in the form of particles having an average particle size preferably between 80 μm and 2000 μm, preferably between 100 μm and 1500 μm, such as 100 μm, 200 μm, 300 μm, 400 μm, 500 μm, 600 μm, 700 μm, 800 μm, 900 μm, 1000 μm, 1100 μm, 1200 μm, or any range therebetween. The preferred range of particle size may result in an improved dissolution profile and / or improved leakage performance.
[0141] The available oxygen source (AvOx) may be a hydrogen peroxide source, preferably selected from the group consisting of percarbonates, perborates, persulfates, and any combination thereof. The available oxygen source may be at least partially coated, or even completely coated, with a coating component such as carbonates, sulfates, silicates, borosilicates, or any mixture thereof, including mixed salts thereof. Suitable percarbonates may be prepared by a fluidized bed process or by a crystallization process. Suitable perborates include sodium perborate monohydrate (PB1), sodium perborate tetrahydrate (PB4), and anhydrous sodium perborate, also known as effervescent sodium perborate. Other suitable AvOx sources include persulfates, such as Oxone. Another suitable AvOx source is hydrogen peroxide.
[0142] The bleach activator may be selected from the group consisting of tetraacetylethylenediamine (TAED); oxybenzenesulfonates such as nonanoyloxybenzenesulfonate (NOBS), caprylamidononanoyloxybenzenesulfonate (NACA-OBS), 3,5,5-trimethylhexanoyloxybenzenesulfonate (Iso-NOBS), dodecyloxybenzenesulfonate (LOBS), and any mixtures thereof; caprolactam; glucose pentaacetate (PAG); nitrile quaternary ammonium; imide bleach activators such as N-nonanoyl-N-methylacetamide; and any mixtures thereof.
[0143] The preformed peracid can be N,N-phthaloylaminoperoxycaproic acid (PAP).
[0144] The bleach catalyst may be selected from the group consisting of oxaziridinium bleach catalysts, transition metal bleach catalysts, and any combination thereof.
[0145] Suitable oxaziridinium bleach catalysts have the formula:
[0146] [ka] (In the formula, R 1 is selected from the group consisting of H, branched chain alkyl groups containing 3 to 24 carbons, and straight chain alkyl groups containing 1 to 24 carbons; R 1 may be a branched alkyl group containing 6 to 18 carbons or a linear alkyl group containing 5 to 18 carbons; R 1 may be selected from the group consisting of 2-propylheptyl, 2-butyloctyl, 2-pentylnonyl, 2-hexyldecyl, n-hexyl, n-octyl, n-decyl, n-dodecyl, n-tetradecyl, n-hexadecyl, n-octadecyl, iso-nonyl, iso-decyl, iso-tridecyl, and iso-pentadecyl; R 2 is independently selected from the group consisting of H, a branched chain alkyl group containing 3 to 12 carbons, and a straight chain alkyl group containing 1 to 12 carbons; optionally, R2 are independently selected from H and a methyl group; and n is an integer from 0 to 1.
[0147] The transition metal bleach catalyst may comprise cations of copper, iron, titanium, ruthenium, tungsten, molybdenum, and / or manganese. Suitable transition metal bleach catalysts are manganese-based transition metal bleach catalysts.
[0148] The reducing bleaching agent may be sodium sulfite and / or thiourea dioxide (TDO).
[0149] In particular, the coating composition may comprise from 1 wt% to 99 wt%, preferably from 10 wt% to 80 wt%, more preferably from 30 wt% to 70 wt%, for example 1 wt%, 2 wt%, 3 wt%, 4 wt%, 5 wt%, 6 wt%, 7 wt%, 8 wt%, 9 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 95 wt%, or any range therebetween of bleaching agent based on the total weight of the coating composition. More specifically, the coating composition may comprise an available oxygen source in an amount of 1% to 99% by weight, preferably 10% to 80% by weight, more preferably 30% to 70% by weight, based on the total weight of the coating composition, for example, 1% by weight, 2% by weight, 3% by weight, 4% by weight, 5% by weight, 6% by weight, 7% by weight, 8% by weight, 9% by weight, 10% by weight, 15% by weight, 20% by weight, 25% by weight, 30% by weight, 35% by weight, 40% by weight, 45% by weight, 50% by weight, 55% by weight, 60% by weight, 65% by weight, 70% by weight, 75% by weight, 80% by weight, 85% by weight, 90% by weight, 95% by weight, or any range therebetween. , and / or the coating composition may comprise from 1 wt% to 99 wt%, preferably from 10 wt% to 80 wt%, more preferably from 30 wt% to 70 wt%, for example, 1 wt%, 2 wt%, 3 wt%, 4 wt%, 5 wt%, 6 wt%, 7 wt%, 8 wt%, 9 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 95 wt%, or any range therebetween of bleach activator based on the total weight of the coating composition.
[0150] i) Foaming system The solid particles contained in the coating composition according to the present invention can include an effervescent system.Any effervescent system known in the art can be used in the coating composition.A preferred effervescent system includes an acid source and an alkali source that can react with each other in the presence of water to produce gas.
[0151] The acid source component can be any organic, mineral, or inorganic acid, or derivatives thereof, or combinations thereof. Preferably, the acid source component comprises an organic acid. The acid compound is preferably substantially anhydrous or non-hygroscopic, and the acid is preferably water-soluble. It may be preferred that the acid source is overdried.
[0152] Suitable acid source components include citric acid, malic acid, tartaric acid, fumaric acid, adipic acid, maleic acid, aspartic acid, glutaric acid, malonic acid, succinic acid, boric acid, benzoic acid, oleic acid, citramalic acid, 3-ketoglutaric acid, or any combination thereof. Citric acid, maleic acid, or tartaric acid are particularly preferred. The acid source may be further coated with a coating such as a salt. In one embodiment, citric acid as the acid source may be coated with sodium citrate.
[0153] Any alkalinity source capable of reacting with an acid source to produce a gas may be present in the particles, which may be any gas known in the art, including nitrogen, oxygen, and carbon dioxide gas. Preferred may be an alkalinity source selected from the group consisting of carbonates, bicarbonates, sesquicarbonates, and any combination thereof. The alkalinity source is preferably substantially anhydrous or non-hygroscopic. It may be preferred that the alkalinity source is overdried.
[0154] Preferably, the gas is carbon dioxide, and thus the alkali source is preferably a carbonate source, which may be any carbonate source known in the art. In a preferred embodiment, the carbonate source is a carbonate salt. Examples of preferred carbonate salts are alkaline earth and alkali metal carbonates, including sodium or potassium carbonate, bicarbonate, and sesquicarbonate, and any combination thereof, as well as ultrafine calcium carbonate or sodium carbonate. Alkali metal percarbonates are also suitable sources of carbonate species, which may be present in combination with one or more other carbonate sources.
[0155] 4. Additional Ingredients In addition to the above components, the coating composition of the present invention may contain one or more additional components depending on its intended use. Such one or more additional components may be selected from the group consisting of fabric care actives, dishwashing actives, hard surface cleaning actives, cosmetic and / or skin care actives, personal cleansing actives, hair care actives, oral care actives, feminine care actives, baby care actives, bittering agents, and any combination thereof.
[0156] In particular, the coating composition may further comprise additional components selected from the group consisting of softeners, silicones, emulsifiers, enzymes, colorants, brighteners, dye transfer inhibitors, deposition aids, antimicrobial agents, chelating agents, non-film forming polymers, antifoam agents, defoamers, and any combination thereof.
[0157] The coating composition may comprise from 0.0001 wt% to 99 wt%, preferably from 1 wt% to 95 wt%, more preferably from 10 wt% to 80 wt%, for example, 0.001 wt%, 0.01 wt%, 0.1 wt%, 1 wt%, 2 wt%, 3 wt%, 4 wt%, 5 wt%, 8 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 95 wt%, or any range therebetween of additional components based on the total weight of the coating composition.
[0158] VII. Conversion of the Multiple Solid Sheets and Coating Compositions into a Multi-Layer Dissolvable Solid Article Containing the Coating Composition Once the flexible dissolvable porous solid sheet articles of the present invention are formed, as described above, two or more of such sheets can be treated by applying a coating composition containing a bleaching agent and then combined to form a dissolvable solid article of any desired three-dimensional shape, including but not limited to, a sphere, a cube, a rectangle, an oval, a cylinder, a rod, a sheet, a flower, a sector, a star, a disk, etc. The sheets may be combined and / or treated by any means known in the art, including but not limited to, chemical means, mechanical means, and combinations thereof. Such combining and / or treating steps are collectively referred to herein as a "conversion" process, i.e., which serves to convert two or more flexible dissolvable porous sheets of the present invention into a dissolvable solid article containing a coating composition.
[0159] It was a surprising and unexpected discovery of the present invention that the bleaching agent contained in the multi-layer solid article exhibits significantly improved stability compared to the bleaching agent alone stored under the same conditions.It was another surprising and unexpected discovery of the present invention that the bleaching agent contained in the multi-layer solid article exhibits significantly improved antimicrobial efficacy.
[0160] Further, the multi-layered dissolvable solid article of the present invention may be characterized by a maximum dimension D and a minimum dimension z (perpendicular to the maximum dimension), with the D / z ratio (hereinafter also referred to as "aspect ratio") ranging from 1 to about 10, preferably from about 1.4 to about 9, preferably from about 1.5 to about 8, more preferably from about 2 to about 7. It is noted that when the aspect ratio is 1, the dissolvable solid article has a spherical shape. When the aspect ratio is about 1.4, the dissolvable solid article has a cubic shape. The multi-layered dissolvable solid article of the present invention may have a minimum dimension z greater than about 3 mm but less than about 20 cm, preferably from about 4 mm to about 10 cm, more preferably from about 5 mm to about 30 mm.
[0161] The multi-layered dissolvable solid article described above may include two or more of such flexible dissolvable porous sheets. For example, it may include about 3 to about 50, preferably about 4 to about 40, more preferably about 5 to about 30, such as 6, 7, 8, 9, 10, 15, 20, 25, 30, or any range therebetween, flexible dissolvable porous sheets. The improved OCF structure within the flexible dissolvable porous sheets made according to the present invention allows many sheets (e.g., 15 to 40) to be stacked together while still providing a sufficient overall dissolution rate for the stack.
[0162] In a particularly preferred embodiment of the present invention, the multi-layer dissolvable solid article comprises 15-40 layers of the flexible dissolvable porous sheet described above and has an aspect ratio in the range of about 2 to about 7.
[0163] In particular, the coating composition containing the bleaching agent can be applied between the individual sheets of the multi-layer soluble solid article by any suitable means, such as spraying, sprinkling, dusting, coating, spreading, dipping, pouring, rolling, or even vapor deposition. More specifically, the coating composition can be applied to one or both of the contact surfaces of adjacent sheets in the stack. In a preferred embodiment, in order to avoid interference of the coating composition with the cut seal or edge seal near the periphery of the individual sheets, the coating composition can be applied to the central region of each of the application surfaces of each sheet, which is preferably defined as an area spaced apart from the periphery of such adjacent sheets by a distance of at least 5%, preferably at least 10%, more preferably at least 15%, and most preferably at least 20% of the maximum dimension D. In an alternative preferred embodiment, the coating composition is applied to the entire application surface of each sheet, preferably such that the application area occupies at least 90%, preferably 95%, more preferably 98%, and most preferably 99% of the total area of the application surface.
[0164] In a preferred embodiment, the coating composition may be applied to the contact surface of one or both of any adjacent sheets in the solid article. In another preferred embodiment, the coating composition may be applied to the contact surface of one or both of the middle two sheets in a stack. In yet another preferred embodiment, the coating composition may be applied to the contact surface of one or both of any two adjacent sheets in a stack, except for the two outermost sheets.
[0165] In a preferred embodiment, the dissolvable solid article comprises a first group of one or more sheets and a second group of one or more sheets, the coating composition is present on at least one surface of at least one of the first group of one or more sheets, but not on any one surface of the second group of one or more sheets, the coating composition comprises an available oxygen source, preferably an available oxygen source selected from the group consisting of percarbonates, perborates, persulfates, and any combination thereof, and each sheet of the second group of one or more sheets comprises a bleach activator, preferably a bleach activator selected from the group consisting of tetraacetylethylenediamine (TAED), oxybenzenesulfonate, caprolactam; pentaacetate glucose (PAG), nitrile quaternary ammonium, imide bleach activator, and any combination thereof. In this case, the available oxygen source is separated from the bleach activator so that the stability of the available oxygen source can be further improved. In particular, the first group of one or more sheets may include at least two sheets, preferably at least four sheets, stacked together, with the coating composition present on the contact surfaces of one or both of the middle two sheets in the first group of one or more sheets. Further, the second group of one or more sheets may be located on the bottom or top, or both, of the first group of one or more sheets.
[0166] As used herein, the term "middle two sheets" refers to two adjacent sheets located in the middle of an arrangement of sheets stacked together. In particular, if the total number of sheets is an odd number (e.g., 7), the middle two sheets include the centrally located sheet and any of its two adjacent sheets (e.g., the third and fourth sheets or the fourth and fifth sheets), and if the total number of sheets is an even number (e.g., 6), the middle two sheets include the two centrally located sheets (e.g., the third and fourth sheets).
[0167] In particular, the weight ratio of coating composition to solid sheet in the multi-layer dissolvable solid article can be from 0.1 to 10, preferably from 0.1 to 7, more preferably from 0.5 to 5, and most preferably from 1 to 3, such as 0.5, 0.6, 0.7, 0.8, 0.9, 1, 1.2, 1.5, 2, 2.5, 3, 3.5, 4, 4.5, 5, or any range therebetween.
[0168] FIG. 7A shows an exemplary multi-layer dissolvable solid article according to the present disclosure in which a coating composition 82 including a bleaching agent (eg, percarbonate) is applied between two middle sheets 81.
[0169] FIG. 7B shows another exemplary multi-layer dissolvable solid article according to the present disclosure in which a first coating composition 84 including an available oxygen source (e.g., percarbonate) is applied between sheets 83 and 85, and a second coating composition 86 including a bleach activator (e.g., TAED) is applied between sheets 85 and 87.
[0170] 7C shows another exemplary multi-layer dissolvable solid article according to the present disclosure, where the article includes a first set of sheets 89 (four solid sheets), a second set of sheets 90 (two solid sheets total), and a coating composition 88 including an available oxygen source (e.g., percarbonate). The coating composition 88 is applied between the middle two sheets in the first set of sheets 89, which preferably do not include a bleach activator. The second set of sheets 90 includes a bleach activator (e.g., TAED) and is located on the top and bottom of the first set of sheets 89.
[0171] Test Method Test 1: Scanning Electron Microscopy (SEM) Method for Determining Surface Average Pore Size of Sheet Articles SEM micrographs of the samples are obtained using a Hitachi TM3000 Tabletop Microscope (S / N: 123104-04). Samples of the solid sheet articles of the present invention are approximately 1 cm x 1 cm in area and are cut from larger sheets. Images are collected at 50X magnification and the unit is operated at 15 kV. A minimum of five microscopic images are collected from randomly selected locations across each sample, resulting in an estimated average pore size of approximately 43.0 mm. 2 Obtain the total analyzed area.
[0172] The SEM micrographs are then first processed using an image analysis toolbox in Matlab®. Images are converted to grayscale if necessary. For a given image, a histogram of intensity values for every single pixel is generated using the Matlab® “imhist” function. Typically, such a histogram reveals two separate distributions, corresponding to the lighter sheet surface pixels and the darker area pixels within the pores. A threshold is selected that corresponds to an intensity value between the peak values of these two distributions. All pixels with intensity values lower than this threshold are then set to an intensity value of 0, and pixels with intensity values higher than it are set to 1, thereby generating a binary black and white image. The binary image is then analyzed using ImageJ (https: / / imagej.nih.gov, version 1.52a) to examine both the pore area ratio and the pore size distribution. The scale bar of each image is used to provide a pixel / mm scaling factor. For analysis, the autothresholding and analyze particles functions are used to isolate each pore. Output from the analysis function includes area ratios for the whole image and pore area, and pore perimeter for each detected pore.
[0173] The average pore size is D A 50, i.e., 50% of the total pore area is D AIt is composed of pores having a hydraulic diameter of 50 or less average diameter. Hydraulic diameter='4 * Pore area (m 2 ) / pore circumference (m)'
[0174] This is an equivalent diameter calculated to take into account pores that are not all circular.
[0175] Test 2: Micro-Computed Tomographic (μCT) Method for Determining Whole or Regional Average Pore Size and Average Cell Wall Thickness of Open Cell Foams (OCF) Porosity is the ratio of void space to the total space occupied by the OCF. Porosity can be calculated from a μCT scan by segmenting the void space by thresholding and determining the ratio of void voxels to total voxels. Similarly, solid volume fraction (SVF) is the ratio of solid space to total space, and SVF can be calculated as the ratio of occupied voxels to total voxels. Both porosity and SVF are average scalar values that do not provide structural information such as the pore size distribution across the height of the OCF or the average cell wall thickness of the OCF struts.
[0176] To characterize the 3D structure of the OCF, the sample is imaged using a μCT X-ray scanning instrument capable of acquiring a data set with high isotropic spatial resolution. An example of a suitable instrument is a SCANCO System model 50 μCT scanner (Scanco Medical AG, Bruttisellen, Switzerland) operating with the following settings: energy level: 45 kVp at 133 μA; projection: 3000; field of view: 15 mm; integration time: 750 ms; average: 5 times; and voxel size: 3 μm per pixel. After the scan and subsequent data reconstruction are completed, the scanner system creates a 16-bit data set, referred to as an ISQ file, in which the gray levels reflect the changes in X-ray attenuation and thus relate to the material density. The ISQ file is then converted to 8-bit using a scaling factor.
[0177] Scanned OCF samples are typically prepared by punching a core approximately 14 mm in diameter. The OCF punch is placed flat on a low damping foam and then mounted into a 15 mm diameter plastic cylindrical tube for scanning. A scan of the sample is acquired such that the entire volume of all mounted cut samples is included in the data set. From this larger data set, smaller sub-volumes of the sample data set are extracted from the total cross-section of the scanned OCF to create a 3D data slab, where the pores can be qualitatively evaluated without edge / boundary effects.
[0178] To characterize the pore size distribution in the height direction, a strut size, local thickness map algorithm, or LTM, is implemented on the subvolume dataset. The LTM method starts with Euclidean Distance Mapping (EDM), assigning each void voxel a gray level value equal to its distance from its nearest boundary. Based on the EDM data, the 3D void space representing the pores (or the 3D solid space representing the struts) is tessellated with spheres sized to match the EDM values. Voxels enclosed by the spheres are assigned the radial value of the largest sphere. In other words, each void voxel (or solid voxel of a strut) is assigned the radial value of the largest sphere that both fits within the void space boundary (or solid space boundary of a strut) and contains the assigned voxel.
[0179] The 3D labeled sphere distribution output from the LTM data scan is processed as a stack of two-dimensional images in the height direction (or Z direction) and can be used to estimate the change in sphere diameter from slice to slice as a function of OCF depth. Strut thickness is processed as a 3D data set and average values can be evaluated for all or part of the subvolume. Calculations and measurements were performed using Thermo Fisher Scientific's AVIZO Lite (9.2.0) and Mathworks' MATLAB (R2017a).
[0180] Test 3: Percentage of Open Cells in Sheet Articles The percent open cell content is measured through gas pycnometry. Gas pycnometry is a common analytical technique that uses gas displacement to accurately measure volume. An inert gas such as helium or nitrogen is used as the displacement medium. A sample of the solid sheet article of the present invention is sealed in an instrument compartment of known volume, charged with the appropriate inert gas, and then expanded to another precise internal volume. The pressure before and after expansion is measured and used to calculate the volume of the sample article.
[0181] ASTM Standard Test Method D2856 provides a procedure for determining the open cell percentage using an older model of an air comparison pycnometer. This device is no longer manufactured. However, tests using a Micromeritics AccuPyc pycnometer can be performed to conveniently and precisely determine the open cell percentage. ASTM Procedure D2856 describes five methods (A, B, C, D, and E) for determining the open cell ratio of foamed materials. For these experiments, nitrogen gas can be used to analyze samples using an Accupyc 1340 with ASTM foampyc software. ASTM Procedure Method C should be used to calculate the open cell percentage. This method simply compares the geometric volume determined using calipers and standard volume calculations to the open cell volume measured by the Accupyc according to the following equation: Percent open cell = open cell volume of sample / geometric volume of sample * 100
[0182] It is recommended that these measurements be performed by Micromeretics Analytical Services, Inc., One Micromeritics Dr, Suite 200, Norcross, GA 30093. More information on this technique is available on the Micromeretics Analytical Services website (www.particletesting.com or www.micromeritics.com) or published in "Analytical Methods in Fine Particle Technology" by Clyde Orr and Paul Webb.
[0183] Test 4: Final Moisture Content of Sheet Articles The final moisture content of the solid sheet product of the present invention is obtained by using a Mettler Toledo HX204 Moisture Analyzer (S / N B706673091). A minimum of 1 g of the dried sheet product is placed on the measurement tray. A standard program is then run with additional program settings of 10 minutes analysis time and 110°C temperature.
[0184] Test 5: Thickness of Sheet Article The thickness of the flexible porous solid sheet articles of the present invention is obtained using a micrometer or feeler gauge, such as a Mitutoyo Corporation Digital Disk Stand Micrometer Model Number IDS-1012E (Mitutoyo Corporation, 965 Corporate Blvd, Aurora, IL, USA 60504), which has a platen with a diameter of 1 inch, weighs about 32 grams, and has a pressure of about 0.09 psi (6.32 gm / cm 2 ) the thickness is measured at an applied pressure of 1000 psi.
[0185] The thickness of a flexible porous solid sheet article is measured by raising the platen, placing a portion of the sheet article on a stand directly beneath the platen, carefully lowering the platen to touch the sheet article, releasing the platen, and measuring the thickness of the sheet article in millimeters on a numeric display. Except for uneven, more rigid substrates, the sheet article should be fully extended over all edges of the platen to ensure that the thickness is measured at the least possible surface pressure.
[0186] Test 6: Basis Weight of Sheet Articles The basis weight of the flexible porous dissolvable solid sheet article of the present invention is determined by the weight of the sheet article per area (grams / m 2 The area is calculated as the projected area on a flat surface perpendicular to the outer edges of the sheet article. The solid sheet article of the present invention is cut into 10 cm x 10 cm square samples so that its area is known. Each such square sample is then weighed and the resulting weight is then multiplied by 100 cm. 2 Divide by the known area to determine the corresponding basis weight.
[0187] For irregularly shaped articles, if it is a flat object, the area is calculated based on the area enclosed within the perimeter of such object. Thus, for a spherical object, the area is calculated based on the average diameter, 3.14 x (diameter / 2) 2 The area is calculated as: diameter x length. Thus, for cylindrical objects, the area is calculated based on the average diameter and average length. For irregularly shaped three-dimensional objects, the area is calculated based on the side with the largest outer dimension projected onto a flat surface oriented perpendicular to this side. This can be accomplished by carefully tracing the outer dimensions of the object with a pencil on a piece of graph paper and then calculating the area by approximately counting the squares and multiplying by the known area of the squares, or by taking a photograph of the traced area (shaded for contrast) including a scale and using image analysis techniques.
[0188] Test 7: Density of Sheet Articles The density of the flexible porous solid sheet articles of the present invention is determined by the following equation: Calculated density = basis weight of porous solid / (thickness of porous solid x 1,000). The basis weight and thickness of the flexible porous solid are determined according to the methods described herein.
[0189] Test 8: Specific surface area of sheet article The specific surface area of flexible porous soluble solid sheet articles is measured via a gas adsorption technique. Surface area is a measurement of the exposed surface of a solid sample on a molecular scale. BET (Brunauer, Emmet, and Teller) theory is the most well-known model used to determine surface area and is based on gas adsorption isotherms. Gas adsorption uses physical adsorption and capillary condensation to measure gas adsorption isotherms. This technique is summarized by the following steps: The sample is placed in a sample tube and heated under vacuum or gas flow to remove contaminants on the surface of the sample. The sample weight is obtained by subtracting the empty sample tube weight from the combined weight of the degassed sample and sample tube. The sample tube is then placed on the analysis port and the analysis begins. The first step in this analysis process is to evacuate the sample tube and then measure the free space volume in the sample tube using helium gas at liquid nitrogen temperature. The sample is then evacuated again and the helium gas is removed. The instrument then begins to collect the adsorption isotherm by dosing krypton gas at user-specified intervals until the required pressure measurement is achieved. The samples may then be analyzed using an ASAP2420 with krypton gas adsorption. It is recommended that these measurements be performed by Micromeretics Analytical Services, Inc., One Micromeritics Dr, Suite 200, Norcross, GA 30093. More information on this technique is available on the Micromeretics Analytical Services website (www.particletesting.com or www.micromeritics.com) or published in the book "Analytical Methods in Fine particle Technology" by Clyde Orr and Paul Webb.
[0190] Test 9: Dissolution Rate of Sheet Articles The dissolution rate of the dissolving sheet or solid article of the present invention is measured as follows. 1. Add 400 mL of room temperature (25° C.) deionized water to a 1 L beaker and then place the beaker on a magnetic stir plate. 2. A magnetic stirring bar having a length of 23 mm and a thickness of 10 mm is placed in the water and set to rotate at 300 rpm. 3. Calibrate a Mettler Toledo S230 conductivity meter to 1413 μS / cm and place the probe into a beaker of water. 4. In each experiment, the number of samples is selected so that a minimum of 0.2 g of sample is dissolved in water. 5. Start the data recording function on the conductivity meter and allow the samples to drop into the beaker. For 5 seconds, use a flat steel plate with a diameter similar to that of the glass beaker to immerse the samples below the surface of the water, ensuring that they do not float to the surface. 6. Conductivity is recorded for at least 10 minutes until a steady state value is reached. To calculate the time required to reach 7.95% dissolution, a 10 second running average is first calculated from the conductivity data, and the time at which this running average exceeds 95% of the final steady state conductivity value is then extrapolated to obtain the time required to achieve 95% dissolution.
[0191] Test 10: Stability of the coating composition The coating compositions are prepared by adding all ingredients together in a 250 mL plastic beaker and mixing for 1 minute at 1000 RPM using an overhead stirrer. Each formulation is then poured into a 30 mL glass vial until the vial is completely filled to determine the stability of the coating compositions. The vials are sealed and then stored upright at room temperature for 24 hours. After 24 hours, each vial is visually inspected for liquid-solid separation. The mixture is considered unstable if a liquid layer with a vertical length of at least 5 mm is measured.
[0192] Test 11: Leakage of coating composition The leakage of the coating composition between adjacent solid sheet layers after the coating composition is added is evaluated by using a drop test. The solid sheets used in this test, prepared according to the method of Section III: Solid Sheet Preparation Process, are first conditioned by placing them in a temperature and humidity controlled room for a minimum of 1 hour, where the temperature and humidity are controlled in the range of 23-24.5°C and 41-45% relative humidity, respectively. The sheets are placed individually and are not laminated to each other.
[0193] A 10x10 cm square sample of foam sheet is then cut from the larger sheet by utilizing a paper cutter. All four edges of the 10x10 cm square are cut by utilizing a paper cutter. None of the existing edges of the larger sheet stack are used as edges of the smaller 10x10 cm square.
[0194] The coating composition is then applied to the center of one of the 10x10 cm square samples, and then a second 10x10 cm sample is placed on top of the first sample, so that the two sheet layers are oriented in a face-to-face configuration. No excessive pressure is applied to the sheet stack during testing, and excessive pressure is defined as any pressure that results in a change in thickness of the sheet of 0.05 mm or more. The 10x10 cm sample is further cut into smaller 5x5 cm samples by using a paper cutter, leaving the coating composition in the center of the 5x5 cm sample.
[0195] The drop test is performed as follows: Utilizing plastic thumb forceps, 1.0 meter of the test sample (i.e., a 5×5 cm sample) is placed on a solid surface such as a floor or tabletop. The sample is oriented such that one of the edges exposed by the cut is parallel to the solid surface. The sample is then released and allowed to drop. After dropping onto the solid surface, the edges of the two sheet layers may separate due to the presence of the coating composition, resulting in leakage of the coating composition. Thus, the percentage of adhesion can be used as a "leakage score" to characterize the leakage degree of the coating composition. A "leakage score" ranging from 0 to 5 is assigned to each sample according to the following criteria: 0 - Less than 5% of the edges of the two sheets are in contact with each other 1- Just 5% or 5-25% of the edges of two sheet layers are bonded together 2- Exactly 25% or 25%-50% of the edges of the two sheet layers are bonded together 3- Exactly 50% or 50%-75% of the edges of the two sheet layers are bonded together 4- Exactly 75% or 75%-95% of the edges of the two sheet layers are bonded together 5- Exactly 95% or more than 95% of the edges of the two sheet layers are bonded together
[0196] For each sample edge, the apparent separation between adjacent sheet layers is identified by visual observation and the length of the apparent edge separation is measured by using a ruler. The percentage of adhesion is then calculated as follows: apparent edge separation length summed over four edges (in centimeters) / sum of four edge lengths (in centimeters). A minimum of three replicate measurements of the drop test are performed for each formulation.
[0197] Test 12: Bleaching agent stability The stability of bleach in solid articles is determined as the level of available oxygen (AvO) in the solid article after a storage period. In particular, the level of AvO is determined by iodometric analysis. The sample is acidified with glacial acetic acid, after which an excess of potassium iodide is added. Peroxide (H2O2) in the reaction [1] is converted to iodide (I - ) to iodine (I2). Iodine [2] can complex with excess iodide to give a water-soluble triiodide species (I3 - The concentration of triiodide is determined by titration with sodium thiosulfate[3] and is proportional to the amount of available oxygen in the sample.
[0198] [ka]
[0199] operation: 1. Weigh the entire contents of the sample into a 1 L volumetric flask to the nearest 0.001 g. Record the weight as W g. 2. Carefully dilute with 10% acetic acid. 3. Adjust the volume with 10% acetic acid. Stir well for about 2 hours. 4. While maintaining stirring, pipette 10 mL into the titration vessel. Then add 40 mL of 10% acetic acid to the vessel. 5.Add 10 mL of 40% potassium iodide solution to the titration vessel and add 1 mL of molybdate reagent to facilitate the reaction. 6. Begin titration with 0.1N sodium thiosulfate solution. Titrate rapidly. 7. Slowly titrate until the solution becomes colorless and remains colorless for at least 10 seconds, presumably indicating the end point has been reached. 8. Record the volume reached at the endpoint as TmL. Calculation:
[0200]
number
[0201] Test 13: Viscosity The viscosity values of the liquid compositions are measured using a Malvern Kinexus Lab+ rheometer with cone and plate geometry (CP1 / 50 SR3468 SS) at a gap width of 0.054 mm, a temperature of 20° C. and a shear rate of 1.0 per second for 360 seconds.
[0202] Test 14: Antimicrobial Efficacy The antimicrobial effect of the solid sheet according to the present disclosure is measured according to the simulation method of Chinese Light Industry Standard QB / T2738-2012 (Test Method for Evaluating Daily Chemical Products in Antibacterial and Bacteriostatic Effects). In summary, under simulated washing conditions, a set of fabric swatches inoculated with microorganisms is placed in a diluted product solution and stirred. After a certain contact time, the wash water and test fabric are quantitatively cultured and determined separately. In particular, Staphylococcus aureus and Escherichia coli are used as test strains. The killing effect is calculated as follows: Kill %=(I-II) / I×100 where I is the average number of colonies in the control sample, II is the average number of colonies in the test samples). EXAMPLES
[0203] Example 1: Different OCF structures in solid sheets produced by different heating / drying configurations Wet premixes having the following surfactant / polymer compositions as set forth in Tables 1 and 2 below were prepared for laundry care sheets and hair care sheets, respectively.
[0204] [Table 1]
[0205] The viscosity of the wet premix composition set forth in Table 1 was about 14309.8 cps. After aeration, the average density of such aerated wet premix was about 0.25 g / cm 3 It was.
[0206] [Table 2]
[0207] The viscosity of the wet premix composition set forth in Table 2 was about 19254.6 cps. After aeration, the average density of such aerated wet premix was about 0.225 g / cm 3 It was.
[0208] Flexible porous dissolvable solid sheets A and B were prepared from the above wet premixes described in Tables 1 and 2 using a continuous aerator (Aeros) and a rotary drum dryer with the following settings and conditions set out in Table 3 below.
[0209] [Table 3]
[0210] A flexible porous dissolvable solid sheet C was also prepared from the above wet premix described in Table 2 using a continuous aerator (Oakes) and a mold placed on a hot plate (providing bottom conduction heating) using the following settings and conditions described in Table 4 below.
[0211] [Table 4]
[0212] Additionally, flexible porous dissolvable solid sheets I and II were prepared from the above wet premixes described in Tables 1 and 2 using a mold placed over a continuous aerator (Oakes) and impingement oven using the following settings and conditions set forth in Table 5 below.
[0213] [Table 5]
[0214] Tables 6-9 below summarize various physical parameters and pore structures measured for Solid Sheets A-C and Solid Sheets I-II made from the wet premix and drying process described above.
[0215] [Table 6]
[0216] [Table 7]
[0217] [Table 8]
[0218] [Table 9]
[0219] The above data show that the solid sheets of the present invention are predominantly open-celled, with the solid sheets made by the rotary drum drying process having a top surface average pore size of greater than 100 μm, and the solid sheets made by the impingement oven process not. Specifically, Figure 6A shows a scanning electron microscope (SEM) image of the top surface of Sheet A, and Figure 6B shows an SEM image of the top surface of Solid Sheet I.
[0220] Furthermore, the above data shows that the solid sheets produced by the rotary drum drying process have significantly less local variation in average pore size, and in particular a significantly smaller ratio of bottom average pore size to top average pore size, than the solid sheets produced by the impingement oven drying process.
[0221] Example 2: Stable coating composition obtained by adding thickeners Coating compositions containing a liquid carrier, solid particles, and a thickener, and coating compositions containing only a liquid carrier and solid particles were prepared and then tested according to Test 10: Stability of Coating Compositions. The results are shown in the table below. The addition of a thickener to a liquid carrier containing a non-ionic surfactant successfully achieves a stable coating composition.
[0222] [Table 10] 1 Sodium percarbonate (SPC) available from Jinke. 2 C12-C14 ethoxylated alcohols (AE7). 3 Aerosil A200 available from Evonik Industries. 4 TAED (96% active) available from Jinke. 5 Linear Alkylbenzene Sulfonate (LAS), 80% active 6 Sodium Laureth-3 Sulfate (AES) with Amine Oxide (75.2% AES and 18.8% AO)
[0223] Example 3: Improved leakage of coating compositions containing thickeners compared to coating compositions without thickeners A dissolvable solid article containing the coating composition was prepared as follows.
[0224] First, a large solid sheet (with a minimum area of 1.0×1.0 m) was prepared according to the method in Section III: Fabrication Process of Solid Sheets.
[0225] Specifically, a wet premix containing the solid sheet ingredients and additional water was first prepared to obtain a total solids content of about 35% by weight (i.e., the total water content in the slurry is about 65% by weight). The slurry preparation method was as follows: 1. First, the water and glycerin were added together to a glass beaker and stirred at 200 rpm using an overhead stirrer. 2. With continued stirring, the polyvinyl alcohol was then slowly added to the beaker containing the water and glycerin, without causing the solution to foam or the polyvinyl alcohol to clump. 3. The beaker was then placed in a water bath and heated to 80° C. with continued stirring. The beaker was covered with cling film or tin foil to reduce water evaporation and mixing was continued for at least 1.0 hour. 4. The remaining ingredients were weighed and added together in a separate glass beaker. The remainder of the water needed to achieve a total water content of 65% in the slurry was also added to this beaker. 5. The beaker was placed in an 80° C. water bath and the contents were stirred with an overhead stirrer at 500 rpm for at least 30 minutes. 6. After the pre-specified mixing time had been reached in both beakers, both contents were added together into a single glass beaker, followed by continuous stirring at 500 rpm and maintaining the temperature at 80° C. for at least an additional 30 minutes.
[0226] The wet premix was then aerated as follows. 1. An Aeros A20 continuous aerator consisting of a jacketed hopper (Model JCABT10) and an A20 mixhead was preheated to 80° C. using a water bath and pump. 2. The previously prepared slurry was then added to the hopper. The aerator device was then turned on and the mix head speed, feed pump speed, and air flow rate were set to 600, 500, and 100 respectively. 3. The aerated slurry was collected from the aerator outlet and its density was measured by filling a density cup of known volume and weighing the mass of the aerated slurry. With the above aerator settings, it was approximately 0.225 g / cm 3 An aerated slurry density of 0.01 was achieved.
[0227] Flexible and porous solid sheets with thicknesses of approximately 0.8-1.5 mm were produced using a rotary drum dryer process as follows. 1. Preheat a rotary drum dryer (having a drum diameter of about 1.5 m) to about 100°C. 2. The aerated slurry collected from the outlet of the Aeros A20 is fed into the feed trough of a drum dryer. 3. Once loaded, the drum dryer is started and the rotation speed is set to provide a residence time of the slurry on the heated drum of approximately 15 minutes. 4. After drying, the flexible and porous sheet so formed is peeled off from the drum surface and placed in a plastic bag.
[0228] The solid sheets were then stored at an ambient relative humidity of 41-45% and a temperature of 23-24.5°C for a minimum of 1 hour.
[0229] A 10x10 cm square sample of the solid sheet was then cut from the larger sheet by utilizing a paper cutter. All four edges of the 10x10 cm square were cut by utilizing a paper cutter. None of the existing edges of the larger sheet stack were used as edges of the smaller 10x10 cm square.
[0230] The coating composition was then applied to the center of one of the 10×10 cm square samples according to the coating method described below, and then a second 10×10 cm sample was placed on top of the first sample, so that the two sheet layers were oriented in a face-to-face configuration. No excessive pressure was applied to the sheet stack during testing, and excessive pressure is defined as any pressure that results in a change in thickness of the sheet of 0.05 mm or more. The 10×10 cm sample was further cut into smaller 5×5 cm samples by using a paper cutter, leaving the coating composition in the center of the 5×5 cm sample. The 5×5 cm sample was then used in the leak test.
[0231] The coating method consists of the following steps: In particular, the coating composition was obtained by mixing the components. Then, using a pipette or spoon, a drop of the coating composition was distributed to a single location on the surface of the solid sheet, a pipette was used when the coating composition was a mixture of liquid and solid particles and had good flowability. This location was always the most central point of the total foam mass. The solid sheet was placed on a mass balance and, with the mass tared to zero, drops were added continuously until the required mass of the coating composition was reached.
[0232] In particular, the solid sheet and coating composition used in this example comprise the components shown in Tables 11 and 12, respectively. Samples 11-17 comprise the same solid sheet but different coating compositions. More specifically, Sample 14 comprises a coating composition in the form of solid particles to which only 1.8 grams of percarbonate powder has been added, which is equal to the total mass of percarbonate powder added to Sample 13. Sample 17 was a solid sheet that did not comprise a coating composition.
[0233] [Table 11] 1 Polyvinyl alcohol with a hydrolysis level of 88% and a degree of polymerization of approximately 1700, available from Sigma Aldrich.
[0234] [Table 12] 1 Sodium percarbonate (SPC) available from Jinke. 2 C12-C14 ethoxylated alcohols (AE7). 3 Aerosil A200 available from Evonik Industries. 4 Solid particles only (no liquid carriers or thickeners) 5Linear Alkylbenzene Sulfonate (LAS), 80% active 6 Sodium Laureth-3 Sulfate (AES) and Amine Oxide (75.2% AES and 18.8% AO) 7 Only the foam sheet without any coating composition.
[0235] The foam sheets containing the coating composition therebetween were tested for leakage according to Test 11: Leakage of Coating Composition. The results are shown in the table above and show that the addition of thickener significantly improves the leakage of the coating composition (5 vs. 2 or 0).
[0236] Example 4: Antimicrobial Efficacy of Solid Articles Containing Bleaching Agent A bleach-containing dissolvable solid article was prepared similarly to Example 3, with the solid sheets and coating composition each having the formulations shown in the table below. Additionally, half of the solid sheets were first stacked in a head-to-tow configuration, then the coating composition was dispensed onto the center-most point of the top sheet, and the remaining sheets were stacked on top of it. The solid sheets were placed on a mass balance, and with the mass tared to zero, drops were added continuously until the required mass of coating composition was reached. In particular, the total number of solid sheets was 10, with the first through third sheets and the ninth through tenth sheets from bottom to top being the outer solid sheets, the formulations of which are shown in Table 13a, and the fourth through eighth sheets being the inner solid sheets, the formulations of which are shown in Table 13b, and the coating composition being applied between the fifth and sixth sheets from bottom to top. Samples 18 and 19 contain the same solid sheets, but different coating compositions.
[0237] [Table 13] 1 Polyvinyl alcohol with a hydrolysis level of 88% and a degree of polymerization of approximately 1700, available from Sigma Aldrich.
[0238] [Table 14] 1 Polyvinyl alcohol with a hydrolysis level of 88% and a degree of polymerization of approximately 1700, available from Sigma Aldrich.
[0239] [Table 15] 1 Sodium percarbonate (SPC) available from Jinke. 2 C12-C14 ethoxylated alcohols (AE7). 3 Aerosil A200 available from Evonik Industries.
[0240] The antimicrobial effect of the solid article according to the present disclosure is tested. In particular, the solid article is first completely dissolved in water, and then diluted according to a specific dilution factor. Then, the antimicrobial effect is determined according to test 14 (i.e., the simulation method in QBT2738-2012) using a dilution factor of 33. The results shown in Table 15 below show that the solid article according to the present disclosure achieves excellent antimicrobial effect.
[0241] [Table 16]
[0242] Example 5: Improved stability of bleach in a coating composition contained on a dissolvable solid article compared to bleach alone stored under the same conditions The dissolvable solid articles containing the coating composition were prepared similarly to Example 3, where the coating composition included a bleaching agent. Furthermore, half of the sheets were first stacked in a head-to-toe configuration, then the coating composition was dispensed onto the most central point of the top sheet, and the remaining sheets were stacked on top of it. When more than one coating composition was applied, some sheets were first stacked in a head-to-toe configuration, then the first coating composition was dispensed onto the most central point of the top sheet. Then, one or more sheets were stacked on top, then the second coating composition was dispensed onto the most central point of the top sheet. Finally, the remaining sheets were stacked on top of it. The sheets were always oriented so that the coating composition was distributed on the bottom surface of the sheet. The solid sheet was placed on a mass balance, and with the mass tared to zero, drops were added continuously until the required mass of coating composition was reached.
[0243] The solid sheet and coating compositions each have the formulations shown in the table below, with Comparative Example i being a simple mixture of percarbonate particles and TAED particles. Furthermore, the total number of solid sheet layers in Examples I and II is 15, with the first coating composition applied between the 5th and 6th sheets from bottom to top, and the second coating composition applied between the 10th and 11th sheets from bottom to top.
[0244] [Table 17] 1 Polyvinyl alcohol with a hydrolysis level of 88% and a degree of polymerization of approximately 1700, available from Sigma Aldrich. 2 Rewoquat Ci-Deedmac (cationic surfactant) from Evonik 3 Sodium percarbonate (SPC) available from Jinke. 4 Aerosil A200 available from Evonik Industries. 5TAED (96% active) available from Jinke. 6 Aerosil A200 available from Evonik Industries.
[0245] The stability of the bleaching agent contained in the solid article according to the present disclosure was tested according to Test 12. The results, shown in Table 17 below, indicate that the stability of the bleaching agent contained in the solid article is significantly improved compared to the bleaching agent alone.
[0246] [Table 18] 1 It was sealed in a 45 micron thick PP pouch and then stored at 45° C. and 75% RH for 3 weeks.
[0247] Prior to the present invention, it was expected that the porous structure of the solid sheet according to the present disclosure would impair the stability of the bleaching agent outside the solid sheet according to the present disclosure, or at best maintain a similar stability, since the porous structure would absorb a lot of moisture in the environment, which would react with the bleaching agent. On the contrary, it has surprisingly been discovered by the inventors of the present disclosure that the stability of the bleaching agent loaded into the dissolvable solid article is significantly improved compared to the bleaching agent alone.
[0248] The moisture in the inside (i.e., the sample was taken at the very center of the layer in contact with the first coating composition) and edge (i.e., the sample was taken at the edge of the solid sheet) of Example I was tested according to Test 4 after 24 hours of storage (sealed in a 45 micron thick PP pouch and then stored at 45°C and 75% RH). The results shown in Table 18 below show that the moisture in the inside and edge of the solid sheet is substantially the same after 24 hours of the solid sheet being placed in a humid environment. Therefore, the improved stability achieved in the present disclosure is completely unexpected because the bleaching agent in the solid sheet can still come into contact with moisture.
[0249] [Table 19]
[0250] Dimensions and values disclosed herein should not be understood as being strictly limited to the exact numerical values recited. Instead, unless otherwise indicated, each such dimension is intended to mean both the recited value and a functionally equivalent range surrounding that value. For example, a dimension disclosed as "40 mm" is intended to mean "about 40 mm."
[0251] All documents cited herein, including any cross-referenced or related patents or patent applications, and any patent applications or patents to which this application claims priority or the benefit thereof, are incorporated herein by reference in their entirety, unless expressly stated to the contrary. The citation of any document shall not be deemed to be prior art to any invention disclosed or claimed herein, or to teach, suggest or disclose such invention, either alone or in combination with any other reference(s). Furthermore, to the extent that any meaning or definition of a term in this document conflicts with any meaning or definition of the same term in a document incorporated by reference, the meaning or definition assigned to that term in this document shall govern.
[0252] While particular embodiments of the present invention have been illustrated and described, it would be obvious to those skilled in the art that various other changes and modifications can be made without departing from the spirit and scope of the invention. It is therefore intended to cover in the appended claims all such changes and modifications that are within the scope of this invention.
Claims
1. A dissolvable solid article comprising two or more flexible porous dissolvable sheets, each of said two or more sheets comprising 5% to 40% by weight of a water-soluble polymer based on the total weight of said sheets and 20% to 90% by weight of a surfactant based on the total weight of said sheets, characterized by a percent open cell content of 80% to 100% and an overall average pore size of 100 μm to 2000 μm; a coating composition comprising a non-aqueous liquid carrier, solid particles, and a thickener is present on at least one surface of at least one of the two or more sheets; the non-aqueous liquid carrier is selected from the group consisting of polyethylene glycol, polypropylene glycol, silicone, fatty acid, perfume oil, non-ionic surfactant, and any combination thereof; the thickening agent is selected from the group consisting of silica, clay, polyacrylate thickeners, polyacrylamide thickeners, ethoxylated cellulose alginate, hydroxypropyl cellulose, hydroxyethyl cellulose, and any combination thereof; the solid particles comprise an anionic surfactant, an enzyme, a bleaching agent, a foaming system, or any combination thereof; A dissolvable solid article, provided that said coating composition is not present on any exterior surface of said dissolvable solid article.
2. 10. The dissolvable solid article of claim 1, wherein the non-aqueous liquid carrier is a non-ionic surfactant and / or the thickening agent is silica.
3. The non-aqueous liquid carrier is a C alkoxylation carrier having a weight average degree of alkoxylation in the range of 5 to 15. 6 ~C 20 3. The dissolvable solid article of claim 2, comprising a nonionic surfactant selected from the group consisting of straight or branched chain alkyl alkoxylated alcohols (AA), and wherein the thickener comprises silica.
4. the anionic surfactant is selected from the group consisting of alkyl and alkyl ether sulfates, sulfated monoglycerides, sulfonated olefins, alkylaryl sulfonates, primary or secondary alkane sulfonates, alkyl sulfosuccinates, acyltaurates, acyl isethionates, alkyl glyceryl ether sulfonates, sulfonated methyl esters, sulfonated fatty acids, alkyl phosphates, acyl glutamates, acyl sarcosinates, alkyl sulfoacetates, acylated peptides, alkyl ether carboxylates, acyl lactylates, anionic fluorosurfactants, sodium lauroyl glutamate, and any combination thereof; the enzyme is selected from the group consisting of protease, amylase, cellulase, lipase, xyloglucanase, pectate lyase, mannase, cutinase, and any combination thereof; the bleaching agent is selected from the group consisting of an available oxygen source, a bleach activator, a pre-formed peracid, a bleach catalyst, a reducing bleach, and any combination thereof; 10. The dissolvable solid article of claim 1, wherein the effervescent system is an acid source selected from the group consisting of citric acid, malic acid, tartaric acid, fumaric acid, adipic acid, maleic acid, aspartic acid, glutaric acid, malonic acid, succinic acid, boric acid, benzoic acid, oleic acid, citramalic acid, 3-ketoglutaric acid, or any combination thereof, and an alkalinity source selected from the group consisting of carbonates, bicarbonates, sesquicarbonates, and any combination thereof.
5. 10. The dissolvable solid article of claim 1, wherein the solid particles comprise a C6-C20 linear alkyl benzene sulfonate (LAS) surfactant.
6. 10. The dissolvable solid article of claim 1, wherein said solid particles comprise a source of available oxygen selected from the group consisting of percarbonates, perborates, persulfates, and any combination thereof.
7. 10. The dissolvable solid article of claim 1, wherein the solid particles comprise a bleach activator selected from the group consisting of tetraacetylethylenediamine (TAED), oxybenzenesulfonate, caprolactam; pentaacetic acid glucose (PAG), nitrile quaternary ammonium, imide bleach activators, and any combination thereof.
8. The coating composition comprises: 1) 5% to 70% by weight of the non-aqueous liquid carrier, based on the total weight of the coating composition; and / or 2) 10% to 80% by weight of the solid particles, based on the total weight of the coating composition; and / or 3) The dissolvable solid article of any one of claims 1 to 7, comprising 0.05 wt% to 5 wt% of said thickener, based on the total weight of said coating composition.
9. The dissolvable solid article of any one of claims 1 to 8, wherein at least one of said sheets comprises from 7% to 30% by weight of said water-soluble polymer, based on the total weight of said sheet.
10. 10. The dissolvable solid article of any one of claims 1 to 9, wherein at least one of said sheets comprises 30% to 80% by weight of said surfactant, based on the total weight of said sheet.
11. the two or more sheets include a first set of sheets and a second set of sheets, and the coating composition is present on at least one surface of at least one of the first set of sheets but not on any surface of the second set of sheets; the coating composition comprises a source of available oxygen selected from the group consisting of percarbonates, perborates, persulfates, and any combination thereof; 11. The dissolvable solid article of any one of claims 1 to 10, wherein each sheet in the second set of sheets comprises a bleach activator selected from the group consisting of tetraacetylethylenediamine (TAED), oxybenzenesulfonate, caprolactam; pentaacetate glucose (PAG), nitrile quaternary ammonium, imide bleach activators, and any combination thereof.
12. Each of the sheets is an open cell content of 85% to 100%, and / or an overall average pore size of 150 μm to 1000 μm, and / or an average cell wall thickness of 5 μm to 200 μm, and / or a final moisture content of between 0.5% and 25% by weight of the sheet, and / or a thickness between 0.6 mm and 3.5 mm, and / or 50 grams / m 2 ~500g / m 2 and / or 0.05 grams / cm 3 ~0.5 grams / cm 3 density of, and / or ・0.03m 2 / g to 0.25m 2 12. The dissolvable solid article according to any one of claims 1 to 11, characterized by a specific surface area of 1 / g.
13. Use of a dissolvable solid article according to any one of claims 1 to 12 in removing microorganisms from fabrics or hard surfaces and / or in preventing or reducing malodours.
14. 1. A process for preparing a dissolvable solid article, comprising: 1) providing two or more flexible porous dissolvable sheets and a coating composition, each of the two or more sheets comprising 5% to 40% by weight of a water-soluble polymer based on the total weight of the sheet and 20% to 90% by weight of a surfactant based on the total weight of the sheet, characterized by a percent open cell content of 80% to 100% and an overall average pore size of 100 μm to 2000 μm, the coating composition comprising a non-aqueous liquid carrier, a thickener, and solid particles, the thickener being selected from the group consisting of silica, clay, polyacrylate thickeners, polyacrylamide thickeners, ethoxylated cellulose alginate, hydroxypropyl cellulose, hydroxyethyl cellulose, and any combination thereof, the non-aqueous liquid carrier being selected from the group consisting of polyethylene glycol, polypropylene glycol, silicone, fatty acid, perfume oil, non-ionic surfactant, and any combination thereof, the solid particles comprising anionic surfactants, enzymes, bleaching agents, effervescent systems, or any combination thereof; 2) applying the coating composition onto at least one surface of at least one sheet from the two or more sheets; and 3) arranging the two or more sheets in a stack to form the dissolvable solid article such that the coating composition is not present on any outer surface of the stack.
15. The two or more flexible porous dissolvable sheets are formed by the following steps: a) preparing a wet premix comprising the water-soluble polymer and the surfactant; b) aerating the wet premix to form an aerated wet premix; c) forming the aerated wet premix into a sheet having opposed first and second surfaces; d) drying the formed sheet to create the two or more flexible porous dissolvable sheets.
16. 16. The process of claim 15, wherein step d) is conducted at a temperature of 70°C to 200°C for a period of 5 minutes to 300 minutes along a heating direction that creates a decreasing temperature gradient from the first side to the second side of the formed sheet, the heating direction being substantially opposite to the direction of gravity for more than half of the drying time of step d) of claim 15. [Request 17] The wet premix is heated at 40° C. and -1 17. The process of claim 15 or 16, wherein the aerated wet premix has a viscosity of from 1,000 cps to 25,000 cps as measured by HPLC and / or the aerated wet premix has a density of from 0.05 to 0.8 g / mL.
Citation Information
Patent Citations
Laundry additive product
JP1984074198A
Sheetlike detergent
JP1998204499A
Laundry stain and dirt pre-treatment sheets
JP2012501372A
Process of making an article for dissolution upon use to deliver surfactants
WO2010077627A2
Continuous process of making an article of dissolution upon use to deliver surfactants
WO2012138820A1