Microspectral chip based on different shaped units and method for producing micro-nanostructure arrays on the microspectral chip

The microspectral chip with randomly shaped micro-nanostructure units addresses the limitations of conventional spectrometers by enhancing spectral recovery accuracy and miniaturization, suitable for applications in small platforms.

JP7578795B2Active Publication Date: 2024-11-06TSINGHUA UNIVERSITY
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023504407
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-08-14
Filing Date
2021-08-03
Publication Date
2024-11-06
Estimated Expiration
2041-08-03

AI Technical Summary

Technical Problem

Conventional spectrometers face limitations in miniaturization due to the need for precise spectroscopic elements and regular-shaped micro-nanostructure units, which restrict broadband modulation capabilities and spectral recovery accuracy.

Method used

A microspectral chip utilizing randomly shaped micro-nanostructure units with a two-dimensional lattice structure, integrated with a CMOS image sensor, to achieve high precision and miniaturization by varying the shape and arrangement of internal units for enhanced spectral modulation.

Benefits of technology

The chip achieves high-precision spectral recovery with rich broadband modulation characteristics, enabling miniaturization and reducing device size while improving stability and reducing costs, suitable for applications in small platforms like satellites and drones.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578795000001
    Figure 0007578795000001
  • Figure 0007578795000002
    Figure 0007578795000002
  • Figure 0007578795000003
    Figure 0007578795000003
Patent Text Reader

Abstract

According to an embodiment of the present invention, a micro-spectral chip based on units of different shapes includes a CIS wafer and a light modulation layer. The light modulation layer includes a plurality of micro-nanostructure units disposed on the surface of the photosensitive region of the CIS wafer, each of which includes a plurality of micro-nanostructure arrays. Within each micro-nanostructure unit, different micro-nanostructure arrays are two-dimensional lattices composed of internal units of different shapes. The present invention also provides a method for producing a micro-nanostructure array on a spectral chip. In each micro-nanostructure unit, the internal units in different micro-nanostructure arrays have different shapes, and each set of micro-nanostructure arrays has different modulation effects on light of different wavelengths. By fully utilizing the flexibility of the "shape," various modulation effects can be obtained for the incident light, improving the accuracy of spectral recovery and reducing the size of the unit. The two-dimensional lattice structure based on internal units of different shapes provides rich, broadband modulation characteristics for the incident light, enabling high-precision measurement of the incident light spectrum.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims priority to Chinese patent application filed on August 14, 2020, bearing application number 202010821286.5 and entitled "Micro-spectral chip based on units of different shapes", Chinese patent application filed on August 14, 2020, bearing application number 202010820381.3 and entitled "Micro-spectral chip based on units of random shapes", and Chinese patent application filed on August 14, 2020, bearing application number 202010820373.9 and entitled "Method for generating micro-nanostructure arrays in spectral chips", each of which is incorporated by reference in its entirety.

[0002] The present invention relates to the technical field of spectral imaging, in particular to a micro-spectral chip based on units of different shapes and a method for producing a micro-nanostructure array on the spectral chip. [Background technology]

[0003] In conventional spectrometers, the different wavelength components of the incident light must be spatially separated by a spectroscopic element before detection, and the precise spectroscopic element usually has a large volume, which limits the miniaturization of the spectrometer. In addition, the incident light is modulated by a micro-nanostructure array of units with a regular repeating shape, and the spectral information of the incident light can be restored from the detector response by an algorithm. However, this technical solution adopts regular-shaped units, and the broadband modulation function that can be realized by changing parameters such as period and duty is limited, which limits the accuracy of the spectrum recovery and makes it difficult to further reduce the size of the device. Therefore, it is very important to realize high precision and miniaturization of the spectral chip.

[0004] Traditional spectrometers require precise spectroscopic elements, are complicated in equipment, and are large in volume, while current micro-spectrometers modulate the incident light by a micro-nanostructure array of regular-shaped units, and then use an algorithm to restore the spectral information of the incident light from the detector response. For example, as shown in Figure 30, each unit of the light modulation layer is provided with several modulation holes drilled in the substrate, and the cross-sectional shapes of the modulation holes include circle, ellipse, cross, regular polygon, star or rectangle. This method adopts regular-shaped units, and the spectral modulation function that can be realized by changing the structural parameters such as period, duty, angle, etc. is limited, so the accuracy of the spectrum recovery is limited, and it is difficult to further reduce the size of the device. Summary of the Invention [Problem to be solved by the invention]

[0005] In order to solve the problems that the wideband modulation function that can be realized by conventional technology spectral chips is limited, which limits the accuracy of spectral recovery and makes it difficult to further reduce the size of the device, an embodiment of the present invention provides a micro-spectral chip based on a unit of a different shape, which can achieve high accuracy and miniaturization of the spectral chip.

[0006] In order to solve the problem that the wideband modulation functions that can be realized by prior art spectral chips are limited, which limits the accuracy of spectral recovery and makes it difficult to further reduce the size of the device, an embodiment of the present invention provides a micro-spectral chip based on random-shaped units, which can realize a spectral chip with higher accuracy and smaller size.

[0007] In response to problems existing in the prior art, embodiments of the present invention provide a method for producing micro-nanostructure arrays on a spectral chip. [Means for solving the problem]

[0008] An embodiment of the present invention provides a micro-spectral chip that includes a CIS (CMOS (Complementary Metal Oxide Semiconductor) Image Sensor) wafer and a light modulation layer, the light modulation layer including a plurality of micro-nanostructure units provided on a surface of a photosensitive region of the CIS wafer, each micro-nanostructure unit including a plurality of micro-nanostructure arrays, and in each micro-nanostructure unit, different micro-nanostructure arrays are based on different shaped units that are two-dimensional lattices composed of internal units of different shapes.

[0009] In the micro-spectral chip based on different shaped units according to an embodiment of the present invention, the micro-nanostructure units are identical repeating units, and the micro-nanostructure arrays located at corresponding positions in the different micro-nanostructure units are the same, and / or there is no micro-nanostructure array at at least one corresponding position in the different micro-nanostructure units, and / or the size of each of the micro-nanostructure units is less than 0.5 μm. 2 ~40,000μm 2 and / or the period of each of said micro-nanostructure arrays is between 20 nm and 50 μm.

[0010] In a micro-spectral chip based on different shaped units according to one embodiment of the present invention, the number of micro-nanostructure arrays contained in each of the micro-nanostructure units is dynamically adjustable and / or the multiple micro-nanostructure units have C4 symmetry.

[0011] In the micro-spectral chip based on different shaped units according to one embodiment of the present invention, each micro-nanostructure array corresponds to one or more pixels in the CIS wafer.

[0012] In the micro-spectral chip based on different shaped units according to one embodiment of the present invention, the chip further includes a signal processing circuit connected to the CIS wafer via electrical contacts.

[0013] In a micro-spectral chip based on different shaped units according to one embodiment of the present invention, the CIS wafer includes a light detection layer and a metal wiring layer, the light detection layer is disposed below the metal wiring layer and the light modulation layer is integrated on the metal wiring layer, or the light detection layer is disposed above the metal wiring layer and the light modulation layer is integrated on the light detection layer.

[0014] In the microspectral chip based on different-shaped units according to one embodiment of the present invention, when the photodetection layer is above the metal wiring layer, the photomodulation layer is fabricated by etching on the photodetection layer of the CIS wafer, and the etching depth is 50 nm-2 μm.

[0015] In the microspectral chip based on different shaped units according to one embodiment of the present invention, the light modulation layer is a single layer, double layer or multi-layer structure, and the thickness of each layer is 50 nm to 2 μm; the material of the light modulation layer is at least one of silicon, germanium, silicon germanium material, silicon compound, germanium compound, metal or III-V material, among which the silicon compound includes at least one of silicon nitride, silicon dioxide, and silicon carbide; and / or when the light modulation layer is double layer or multi-layer, at least one layer is not perforated.

[0016] In one embodiment of the present invention, in the microspectroscopic chip based on different shaped units, a light transmission medium layer is provided between the light modulation layer and the CIS wafer, the thickness of the light transmission medium layer is 50nm-2μm, the material of the light transmission medium layer is silicon dioxide, and the light transmission medium layer is manufactured on the CIS wafer by chemical vapor deposition, sputtering or spin coating, and then the light modulation layer is deposited and etched above the light transmission medium layer, or the light modulation layer is manufactured on the light transmission medium layer, and then the light transmission medium layer and the light modulation layer are transferred to the CIS wafer.

[0017] In a microspectral chip based on different shaped units according to one embodiment of the present invention, the microspectral chip is integrated with microlenses and / or filters, which are installed above or below the light modulation layer.

[0018] According to one embodiment of the present invention, a micro-spectral chip based on different shaped units includes a CIS wafer and a light modulation layer, the light modulation layer including a plurality of micro-nanostructure units provided on the surface of a photosensitive region of the CIS wafer, each micro-nanostructure unit including a plurality of micro-nanostructure arrays, and in at least one micro-nanostructure unit, the different micro-nanostructure arrays are two-dimensional lattices composed of randomly shaped internal units.

[0019] According to the micro-spectral chip based on units of different shapes according to one embodiment of the present invention, the random-shaped internal units have at least two kinds of curvature.

[0020] An embodiment of the present invention provides a method for producing a micro-nanostructure array on a spectral chip, the spectral chip comprising: The present invention includes a wafer-level image sensor, and a light modulating layer is fabricated on the upper surface of the photosensitive region of the wafer-level image sensor, the light modulating layer includes a unit array consisting of a plurality of micro-nano units, each micro-nano unit corresponds to one or more pixel points on the wafer-level image sensor, the micro-nano units include a plurality of sets of micro-nano structure arrays, each set of micro-nano structure arrays is formed in a two-dimensional lattice structure, the two-dimensional lattice structure in the plurality of sets of micro-nano structure arrays of each micro-nano unit is for modulating incident light and encoding spectral information of the incident light into different pixel points of the wafer-level image sensor, to obtain an image including the spectral information of the incident light; The method for generating a micro-nano structure array on the spectral chip includes generating the two-dimensional grating structure, wherein the two-dimensional grating structure is formed by a periodic arrangement of randomly shaped structures; The step of generating the two-dimensional lattice structure described above specifically includes the steps of: determining an arrangement period of the random shape structures in the two-dimensional lattice structure; generating each randomly shaped structure in the two-dimensional lattice structure according to the following processing steps: The processing procedure includes dividing an area within the array period into meshes to obtain a plurality of mesh areas; performing a random assignment of pixel values ​​for the plurality of mesh regions to obtain an initial pattern corresponding to the randomly shaped structure, where different pixel values ​​indicate that corresponding mesh regions have different refractive indices; and performing a binarization process on the initial pattern to obtain a first binarized pattern, the first binarized pattern corresponding to one randomly shaped structure, and 0 and 1 in the first binarized pattern representing air and medium, respectively.

[0021] Furthermore, before the initial image is subjected to binarization processing, a filter smoothing process is performed in advance on the initial image.

[0022] Furthermore, after obtaining the first binarized pattern, the method further comprises: The method further includes the step of sequentially performing a blurring process and a binarization process on the first binary pattern to obtain a second binary pattern, whereby the second binary pattern corresponds to a random shape structure.

[0023] Further, randomly allocating pixel values ​​to the plurality of mesh regions to obtain an initial pattern corresponding to the random shape structure includes: Grouping a plurality of mesh regions to obtain a plurality of sets of meshes, in which when grouping the plurality of mesh regions, one or more mesh regions are grouped as one set; Randomly assigning pixel values ​​to each set of meshes according to a standard normal distribution to obtain an initial pattern corresponding to the random geometric structure, where the pixel values ​​of each mesh region in the set are the same.

[0024] Furthermore, when generating each random shape structure in the two-dimensional lattice structure, one or more of a mesh division parameter corresponding to a mesh division operation, a random assignment parameter corresponding to a pixel value random assignment operation, a filter smoothing parameter corresponding to a filter smoothing processing operation, and a blurring parameter corresponding to a blurring processing operation are controlled so that the minimum size of the random shape structure is larger than a predetermined threshold value and the ratio of medium to air in the random shape structure satisfies a predetermined constraint condition.

[0025] Furthermore, after obtaining the first binary pattern or the second binary pattern, the method further includes: performing a symmetry process on the first binary pattern or the second binary pattern to obtain a pattern with symmetry, and correspondingly, the pattern with symmetry corresponds to a random shape structure; The symmetry processing includes one or more of the following: a two-fold rotational symmetry processing, a mirror symmetry processing about the Y axis, a mirror symmetry processing about the X axis, a simultaneous mirror symmetry processing about the Y axis and the X axis, a four-fold rotational symmetry processing, and a simultaneous mirror symmetry and four-fold rotational symmetry processing about the Y axis and the X axis; Correspondingly, the pattern with the acquired symmetry is The pattern may include one or more of the following: a pattern with two-fold rotational symmetry, a pattern with mirror symmetry about the Y axis, a pattern with mirror symmetry about the X axis, a pattern with simultaneous mirror symmetry about the Y and X axes, a pattern with four-fold rotational symmetry, and a pattern with simultaneous mirror symmetry and four-fold rotational symmetry about the Y and X axes.

[0026] Furthermore, after obtaining the first binary pattern or the second binary pattern, the method further includes performing a dilation or erosion operation on the first binary pattern or the second binary pattern to simulate an under-etching or over-etching situation during process manufacturing.

[0027] Further, the spectrum chip further includes a signal processing circuit coupled to the wafer-level image sensor; The signal processing circuit is for processing an image including spectral information of the incident light to obtain the spectral information of the incident light.

[0028] Additionally, a light transmissive medium layer is provided between the light modulation layer and the wafer-level image sensor.

[0029] Furthermore, the wafer-level image sensor is a front-illuminated type, and includes a metal line layer and a light detection layer arranged from top to bottom, and the light modulation layer is integrated on a surface of the metal line layer away from the light detection layer; or The wafer-level image sensor is back-illuminated and includes a photodetection layer and a metal line layer disposed from top to bottom, and the photomodulation layer is integrated on a surface of the photodetection layer away from the metal line layer.

[0030] Furthermore, the spectral chip further comprises a microlens and / or a filter; the microlens is disposed on a surface of the light modulating layer away from a wafer-level image sensor, or the microlens is disposed on a surface of the light modulating layer closer to a wafer-level image sensor; The filter may be located on a side of the light modulating layer away from a wafer-level image sensor, or the filter may be located on a side of the light modulating layer closer to a wafer-level image sensor. Effect of the Invention

[0031] As can be seen from the above technical solution, the method for generating a micro-nanostructure array in a spectral chip according to an embodiment of the present invention involves dividing an area within an array period into meshes to obtain a plurality of mesh areas, randomly allocating pixel values ​​to the plurality of meshes to obtain an initial pattern, and then performing a smoothing filter and binarization processing on the initial image to further obtain a random shape structure. Each set of micro-nanostructure arrays, i.e., each two-dimensional lattice structure, is composed of a random shape structure generated randomly in this way, so that the light modulation layer including multiple sets of micro-nanostructure arrays contains a variety of random shape structures, thereby giving the light modulation layer rich broadband modulation characteristics for incident light, which is advantageous in overcoming the limitations in the accuracy of spectral recovery, realizing high-precision measurement of the incident light spectrum, and improving the accuracy of spectral recovery.

[0032] In the micro-spectral chip based on units of different shapes according to the embodiment of the present invention, in each micro-nanostructure unit, the shapes of the internal units in different micro-nanostructure arrays are different, and each set of micro-nanostructure arrays has different modulation effects on light of different wavelengths. By making full use of the freedom of "shape", various modulation effects can be obtained on the incident light, improving the accuracy of spectral recovery while reducing the size of the unit. The two-dimensional lattice structure based on internal units of different shapes provides rich broadband modulation characteristics for the incident light, and realizes high-precision measurement of the incident light spectrum. In order to more clearly describe the embodiments of the present invention or the technical solutions in the prior art, the drawings necessary for describing the embodiments or the prior art are briefly described below. Of course, the drawings described below are multiple embodiments of the present invention, and those skilled in the art can further obtain other drawings based on these drawings without requiring creative efforts. [Brief description of the drawings]

[0033] [Figure 1] 1A-1D are schematic diagrams of the lateral structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Diagram 2] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Diagram 3] 1A-1D are schematic diagrams of the lateral structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 4] 1A-1D are schematic diagrams of the lateral structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Diagram 5] 1A-1D are schematic diagrams of the lateral structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 6] 1A-1D are schematic diagrams of vertical structures of a front-illuminated CIS wafer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 7] 1A-1D are schematic diagrams of vertical structures of a back-illuminated CIS wafer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 8] 1 is a schematic diagram of a vertical structure in which the light modulation layer is a single-layer grating in a microspectral chip based on units of different shapes according to an embodiment of the present invention; [Figure 9] 1 is a schematic diagram of a vertical structure in which the light modulation layer is a single-layer grating in a microspectral chip based on units of different shapes according to an embodiment of the present invention; [Figure 10] 1 is a schematic diagram of a vertical structure in which the light modulation layer is a multi-layer grating in a microspectral chip based on different shaped units according to an embodiment of the present invention; FIG. [Figure 11] 1 is a schematic diagram of a vertical structure in which the light modulation layer in a microspectral chip based on different shaped units according to an embodiment of the present invention is a multi-layer grating, one of which is not perforated. [Figure 12]1A-1D are schematic diagrams of the vertical structure of the etching of the light modulation layer and back-illuminated CIS wafer in the microspectral chip based on different shaped units according to an embodiment of the present invention. [Figure 13] 1A-1D are schematic diagrams of the lateral structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 14] 1A-1D are schematic diagrams of the lateral structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 15] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 16] 2 is a flowchart of multispectral image acquisition according to an embodiment of the present invention. [Figure 17] 1A-1D are schematic diagrams of the lateral structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Figure 18] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 19] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 20] 1 is a schematic diagram of the vertical structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention; [Figure 21] 1 is a schematic diagram of the vertical structure of the light modulation layer in a microspectral chip based on units of different shapes according to an embodiment of the present invention; [Figure 22] 1A-1D are schematic diagrams of vertical structures of a CIS wafer in a microspectral chip based on units of different shapes according to an embodiment of the present invention. [Diagram 23] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 24]1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Diagram 25] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 26] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 27] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 28] 1 is a schematic diagram of the vertical structure of a microspectral chip based on units of different shapes according to an embodiment of the present invention; FIG. [Figure 29] FIG. 2 is a schematic diagram of randomly generated irregular shapes in a microspectral chip based on randomly shaped units according to an embodiment of the present invention. [Diagram 30] FIG. 2 is a schematic diagram of the structure of a spectrum chip according to the prior art of the present invention; [Diagram 31] 1 is a schematic diagram of a structure of a spectral chip according to one embodiment of the present invention; [Diagram 32] 1 is a cross-sectional view of a spectral chip according to one embodiment of the present invention. [Diagram 33] 1 is a flowchart for generating a two-dimensional lattice structure according to an embodiment of the present invention. [Diagram 34] FIG. 1 is a schematic diagram of generating a two-dimensional lattice structure according to an embodiment of the present invention. [Diagram 35] FIG. 13 is a schematic diagram of generating a two-dimensional lattice structure according to another embodiment of the present invention. [Diagram 36] FIG. 13 is a schematic diagram of generating a two-dimensional lattice structure according to another embodiment of the present invention. [Figure 37] FIG. 2 is a schematic diagram of a pattern with double rotational symmetry according to an embodiment of the present invention. [Figure 38] FIG. 2 is a schematic diagram of a pattern with Y-axis mirror symmetry according to an embodiment of the present invention. [Figure 39]FIG. 2 is a schematic diagram of a pattern with mirror symmetry about the X-axis according to an embodiment of the present invention. [Diagram 40] FIG. 2 is a schematic diagram of a pattern with Y-axis and X-axis mirror symmetry according to an embodiment of the present invention. [Diagram 41] FIG. 2 is a schematic diagram of a pattern with four-fold rotational symmetry according to an embodiment of the present invention. [Diagram 42] FIG. 2 is a schematic diagram of a pattern with Y- and X-axis mirror symmetry and four-fold rotational symmetry according to an embodiment of the present invention. [Diagram 43] FIG. 2 is a schematic diagram of a random shaped structure according to one embodiment of the present invention. [Diagram 44] 4 is a schematic diagram of a random shaped structure after performing an erosion operation on a media region in accordance with an embodiment of the present invention. FIG. [Diagram 45] 13A-13C are schematic diagrams of randomly shaped structures after performing a dilation operation on a media region in accordance with an embodiment of the present invention; [Diagram 46] 2 is a schematic diagram of an operation procedure of a spectral chip according to an embodiment of the present invention; FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0034] In order to make the objectives, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be described below clearly and completely with reference to the drawings of the embodiments of the present invention. Of course, the described embodiments are not all the embodiments, but only some of the embodiments of the present invention. All other embodiments obtained by those skilled in the art without creative efforts based on the embodiments of the present invention are included in the protection scope of this application.

[0035] Hereinafter, referring to Fig. 1, a microspectral chip based on units of different shapes according to an embodiment of the present invention will be described, the microspectral chip based on units of different shapes includes a CIS wafer 2 and a light modulation layer 1, the light modulation layer 1 includes a plurality of micro-nano structure units arranged on the surface of the photosensitive region of the CIS wafer 2, each micro-nano structure unit includes a plurality of micro-nano structure arrays, and in each micro-nano structure unit, different micro-nano structure arrays are two-dimensional lattices composed of internal units of different shapes. Further, the present invention describes the internal units of different shapes, and the internal units of different shapes in the present invention refer to non-matching shapes and / or non-matching dimensions, that is, in principle, the spectral signals output by the microspectral chip after being modulated by the internal units of different shapes for the same light during use will not be consistent.

[0036] The high-precision micro-spectral chip based on different-shaped units according to the present invention, the structural schematic diagram of which is shown in Figure 1, includes a light modulation layer 1, a CIS wafer 2, and a signal processing circuit 3. After passing through the light modulation layer 1, the incident light is converted into an electrical signal in the CIS wafer 2, and then processed and output by the signal processing circuit 3. The light modulation layer 1 includes a plurality of repeated micro-nano structure units, each of which is composed of a plurality of sets of micro-nano structure arrays, and the number of array sets included in each micro-nano structure unit may be 8 or more, and its overall size is 0.5 μm 2 ~40000μm 2In each micro-nano structure unit, different micro-nano structure arrays have internal units of different shapes, the period of each micro-nano structure array is 20 nm to 50 μm, the internal units of different shapes have different modulation effects on light of different wavelengths, and each set of micro-nano structure arrays corresponds to one or more photosensitive pixels of the CIS wafer in the vertical direction. After passing through the light modulation layer 1, the incident light is modulated by each set of micro-nano structure arrays in the unit, and the intensity of the modulated optical signal is detected by the CIS wafer 2 and converted into an electrical signal, which is further processed by the signal processing circuit 3, and the spectral information of the incident light is restored and obtained by an algorithm. The light modulation layer 1 is provided on the CIS wafer by monolithic integration. The present invention makes use of the freedom of "shape" by a two-dimensional lattice structure based on units of different shapes, thereby obtaining various modulation effects on the incident light, improving the accuracy of spectrum recovery, and reducing the size of the unit. The two-dimensional lattice structure based on internal units of different shapes provides rich wideband modulation characteristics for the incident light, and realizes high-precision measurement of the incident light spectrum. The light modulation layer and image sensor based on different shaped units are monolithically integrated, and there is no separate element, which helps to improve the stability of the device, greatly promotes the miniaturization and weight reduction of imaging spectrometers, and has broad prospects for application in small platforms such as small satellites and drones (UAVs). By realizing monolithic integration at the wafer level, the distance between the sensor and the light modulation layer can be minimized, which helps to reduce the size of the unit, achieve higher spectral resolution, and reduce packaging costs.

[0037] In an alternative embodiment, the light modulating layer can be defined as only one micro-nanostructure unit, and the micro-nanostructure unit is composed of multiple sets of micro-nanostructure arrays, where the micro-nanostructure array shapes in different regions may be the same or different, for example, the light modulating layer can be obtained by arranging multiple different internal units, which are designed or randomly generated as described above, according to a certain rule, for example, by duplicating and arranging multiple different internal units.

[0038] In another variant embodiment, at least two micro-nanostructure units are not the same, and as can be understood, the difference in the micro-nanostructure units may be the number of micro-nanostructure arrays contained therein, the arrangement manner and / or shape of the internal units in the micro-nanostructure array may be different, and of course both may be different. This embodiment can generate more spectral signals in the entire spectrum, further improving the accuracy. Furthermore, all the micro-nanostructure units may be different. It should be noted that in this variant embodiment, in many cases, each individual micro-nanostructure unit is individually designed and / or selected, since it needs to realize multiple specific requirements, such as obtaining better spectral information, improving processing, obtaining image information, etc. Therefore, in this variant embodiment, the structure and modulation effect of at least two of the micro-nanostructure units are different, for example, at least one of the micro-nanostructure units is not through-etched or processed to obtain image information, so that the light passes through the light modulation layer without being modulated, and thus the CIS can directly receive the iconographic information, while some of the micro-nanostructure units are modulated to obtain the spectral information.

[0039] Furthermore, in order to improve the effect of the present invention, the present invention needs to ensure that the micro-nano structure unit includes at least four kinds of internal units, that is, the micro-spectral chip generates at least four different spectral signals when the same light is input. That is, the present invention ensures that the modulation action of different shaped internal units on different wavelengths of light is different, and can generate more spectral signals, and by detecting the spectral signals generated after the light passes through each unit, the spectral information of the light to be measured can be recovered by the algorithm, and the spectral signals of the present invention are relatively rich, so that the recovered spectral information is more accurate. Preferably, the light modulation layer includes at least nine different kinds of the internal units, so that the information after the light is modulated is rich, and the calculated spectrum can be more accurate. It is preferable that the micro-nano structure unit of the light modulation layer includes a square number (for example, 4, 9, 16, etc.) of micro-nano structure arrays, which makes it easier to design and process, and the design can reduce the difficulty of spectrum calculation.

[0040] Viewed from the vertical direction, as shown in FIG. 2, each set of micro-nanostructure arrays in the light modulation layer 1 is a two-dimensional lattice based on different shaped internal units 11, which can be fabricated by directly growing one or more layers of medium or metal material on the CIS wafer 2 and then etching. By changing the geometric shape of 11, each set of micro-nanostructure arrays can have different modulation effects on different wavelengths of light in the target range. The thickness of the light modulation layer 1 is 50 nm to 2 μm, and each set of micro-nanostructure arrays in the light modulation layer 1 corresponds to one or more pixels on the CIS wafer 2. The light modulation layer 1 is fabricated directly on the CIS wafer 2, and the CIS wafer 2 and the signal processing circuit 3 are connected through electrical contacts. The present invention can directly monolithically integrate the light modulation layer 1 on the CIS wafer 2 at the wafer level and complete the fabrication of the spectrum chip in one tape-out using the CMOS process. Compared with the traditional spectral imaging device, the present invention monolithically integrates the light modulation layer 1 and the CIS wafer 2 based on different shaped units, and has no separate elements, which helps to improve the stability of the device and reduce the volume and cost of the device.

[0041] It can be understood that in microspectral chips based on internal units of different shapes mentioned in the above embodiments, the internal units can be designed by the inventors as needed, or can be randomly generated, for example, by an algorithm, or can be randomly generated by an algorithm and then adjusted as needed, and further, the internal units of the light modulation layer can be artificially designed and / or randomly generated.

[0042] In one preferred embodiment of the present invention, the high-precision micro-spectral chip is composed of a random-shaped internal unit, the structural schematic diagram of which is shown in Figure 1, and includes a light modulation layer 1, a CIS wafer 2 and a signal processing circuit 3. After passing through the light modulation layer 1, the incident light is converted into an electrical signal by the CIS wafer 2, and then processed and output by the signal processing circuit 3. The light modulation layer 1 includes a plurality of repeated micro-nano structure units, each of which is composed of a plurality of sets of micro-nano structure arrays, and the number of array sets included in each micro-nano structure unit may be 8 or more, and its overall dimension is 0.5 μm 2 ~40000μm 2In each micro-nano structure unit, the shapes of the internal units of different micro-nano structure arrays may be partially the same or different from each other, and the shapes of the internal units are randomly formed and irregular, preferably the shapes of the internal units of different micro-nano structure arrays are different, and the period of each micro-nano structure array is 20 nm to 50 μm, and the internal units of different shapes have different modulation effects on light of different wavelengths, and the spectrum information of the light to be measured can be recovered by an algorithm by detecting the response after the light passes through the unit, and each set of micro-nano structure arrays corresponds to one or more CIS wafer photosensitive pixels in the vertical direction. After the incident light passes through the light modulation layer 1, it is modulated by each set of micro-nano structure arrays in the unit, and the modulated optical signal intensity is detected and converted into an electrical signal by the CIS wafer 2, and further processed by the signal processing circuit 3, and the spectrum information of the incident light is recovered and obtained by an algorithm. The light modulation layer 1 is provided on the CIS wafer in a monolithic integration manner. The present invention makes full use of the freedom of "shape" by using a two-dimensional lattice structure based on random-shaped units, thereby obtaining various modulation effects on the incident light, improving the accuracy of spectrum recovery, and reducing the size of the units. The random-shaped internal units are a large number of different irregular shapes randomly generated based on preset conditions, so that various modulation effects can be generated on the incident light, which helps to improve the accuracy of spectrum recovery. The two-dimensional lattice structure based on the random-shaped internal units provides rich broadband modulation characteristics for the incident light and realizes high-precision measurement of the incident light spectrum. The light modulation layer based on the random-shaped units and the image sensor are monolithically integrated, and there are no individual elements, which helps to improve the stability of the device, greatly promoting the miniaturization and weight reduction of the imaging spectrometer, and has broad prospects for application to small platforms such as small satellites and drones.By achieving monolithic integration at the wafer level, the distance between the sensor and the light modulation layer can be minimized, which helps to reduce the unit size, achieve higher spectral resolution, and reduce packaging costs.

[0043] The irregular shape above may be a random shape generated by an algorithm, and the process of the algorithm is as follows. First, the area within one period is uniformly divided into meshes, and the size of the mesh can be flexibly set. Then, a refractive index is assigned to each lattice point in the mesh according to a certain distribution law, and the assignment is usually performed by adopting a standard normal distribution. However, the assigned refractive index here is just a numerical value and does not represent the refractive index of the actual material. Next, the image filter smoothing process and binarization process are performed on the refractive index distribution, and the refractive index distribution obtained at this time has only two values, 0 and 1, which represent air and medium, respectively. In order to facilitate the process manufacturing, blurring and binarization processes are also required to eliminate the parts in the structure that are too small in size. In the final generated image, the values ​​0 and 1 represent the regions of air and medium, respectively, and structures that are too small in size are not included, which is convenient for process processing. In addition, certain constraints can be added to the generated random structure. For example, if a certain symmetry is required for the structure, the algorithm can perform a symmetrization process on the refractive index distribution. Furthermore, by changing the parameters in the algorithm, the characteristics such as the minimum feature size of the generated random shape can be adjusted.

[0044] Figure 29 shows some of the random shapes generated by the algorithm, where the numbers 0 and 1 represent the air and medium regions, respectively. As can be seen, the algorithm can generate many different irregular shapes, which can generate rich modulation effects on the incident light and help improve the accuracy of the spectrum recovery.

[0045] Viewed from the vertical direction, as shown in FIG. 2, each set of micro-nanostructure arrays in the light modulation layer 1 is a two-dimensional lattice based on random-shaped internal units 11, which can be fabricated by directly growing one or more layers of medium or metal material on the CIS wafer 2 and then etching. By changing the geometric shape of 11, each set of micro-nanostructure arrays can have different modulation effects on different wavelengths of light in the target range. The thickness of the light modulation layer 1 is 50 nm to 2 μm, and each set of micro-nanostructure arrays in the light modulation layer 1 corresponds to one or more pixels on the CIS wafer 2. The light modulation layer 1 is fabricated directly on the CIS wafer 2, and the CIS wafer 2 and the signal processing circuit 3 are connected through electrical contacts. The present invention can directly monolithically integrate the light modulation layer 1 on the CIS wafer 2 at the wafer level and complete the fabrication of the spectrum chip in one tape-out using the CMOS process. Compared with the conventional spectral imaging device, the present invention is characterized in that the light modulation layer 1 based on random-shaped units and the CIS wafer 2 are monolithically integrated, and there are no discrete elements, which helps to improve the stability of the device and reduce the volume and cost of the device.

[0046] The light modulation layer 1 is engraved with various micro-nano structure arrays composed of two-dimensional lattices with different shaped structures as internal units, which modulate the received light, and different structures have different modulation effects. Viewed from the lateral direction, the light modulation layer 1 can have the following three forms:

[0047] Form 1: As shown in FIG. 3, there are multiple repeating micro-nanostructure units, such as 11, 22, 33, 44, 55, 66, on a plate, and each unit is composed of multiple sets of micro-nanostructure arrays, and the micro-nanostructure arrays at the same position in different units are the same, for example, the micro-nanostructure array included in the micro-nanostructure unit 11 includes a first set of two-dimensional lattices 110 having a first shape, a second set of two-dimensional lattices 111 having a second shape, a third set of two-dimensional lattices 112 having a third shape, and a fourth set of two-dimensional lattices 113 having a fourth shape, and further, for example, the micro-nanostructure array included in the micro-nanostructure unit 44 includes a first set of two-dimensional lattices 440 having a first shape, a second set of two-dimensional lattices 443 having a second shape, a third set of two-dimensional lattices 442 having a third shape, and a fourth set of two-dimensional lattices 444 having a fourth shape. As can be seen, the shapes of the internal units of different micro-nanostructure arrays are different, and the shapes of the internal units constituting the two-dimensional lattice of the same micro-nanostructure array are the same, and the internal units are actually internal lattice units constituting the two-dimensional lattice. Each set of micro-nanostructure arrays in the micro-nanostructure unit has a different modulation effect on light of different wavelengths, and each set of micro-nanostructures has a different modulation effect on the input light, and the specific modulation methods include, but are not limited to, scattering, absorption, interference, surface plasmon, resonance enhancement, etc. By changing the shape of the unit, the corresponding transmission spectrum is different after the light passes through different sets of micro-nanostructures. There is a corresponding sensor below each set of micro-nanostructure arrays, and after the light is modulated by the micro-nanostructure array, the intensity of the light is detected by the optical sensor below. Each unit and its optical sensor below constitute a pixel point, and the spectral information at each pixel point, that is, the intensity distribution of each wavelength, can be obtained through the restoration algorithm of the prior art, and the multiple pixel points constitute an image containing spectral information.

[0048] Form 2: As shown in Fig. 4, there are multiple repeating micro-nanostructure units, such as 11, 22, 33, 44, 55, 66, on a plate, each unit includes multiple sets of different micro-nanostructure arrays, the micro-nanostructure arrays at the same position in different units are the same, and there is a corresponding sensor under each set of micro-nanostructure arrays. For example, the micro-nanostructure array included in the micro-nanostructure unit 11 includes a first set of gratings 110 having a first shape, a second set of gratings 111 having a second shape, and a third set of gratings 112 having a third shape, and the fourth set 113 is empty, and further, for example, the micro-nanostructure array included in the micro-nanostructure unit 44 includes a first set of gratings 440 having a first shape, a second set of gratings 443 having a second shape, and a third set of gratings 442 having a third shape, and the fourth set 444 is empty. As can be seen, the micro-nanostructure array adopted in this embodiment is the same as that of embodiment 1, except for the following difference, the difference being that there is no micro-nanostructure at one of the sets. This allows the incident light to travel straight ahead and can be used for calibration and / or imaging of the unit's straight ahead light intensity. It should be understood that Fig. 4 of the present invention is merely an example for ease of understanding, and that there may be two or more sets of positions where the micro-nanostructure is absent in each embodiment.

[0049] Form 3: As shown in FIG. 5, there are multiple micro-nanostructure units, such as 11, 22, 33, 44, 55, 66, 77, 88, etc., on the plate, each micro-nanostructure unit includes multiple sets of different micro-nanostructure arrays, and there is a corresponding sensor under each set of micro-nanostructure arrays. The difference between this form and form 1 is that the number of micro-nanostructure arrays included in each micro-nanostructure unit can be dynamically adjusted, for example, the left side of FIG. 5 shows that each unit includes 9 sets of micro-nanostructure arrays, and the right side shows that each micro-nanostructure unit includes 4 sets of micro-nanostructure arrays. The more arrays included in each micro-nanostructure unit, the higher the accuracy of spectrum recovery and the better the noise resistance performance, but the lower the density of spectrum pixels. This dynamic combination form can achieve a balance between the accuracy of spectrum recovery and the density of spectrum pixels. It should be understood that the same micro-nanostructure arrays may be present in the micro-nanostructure units.

[0050] According to different needs, the specific structure of the CIS wafer 2 can have two selectable forms.

[0051] Form 1: As shown in FIG. 6, the CIS wafer 2 is of a front-illuminated type, the light detection layer 21 is located below the metal wiring layer 22, no microlenses and filters are integrated on the CIS wafer, and the light modulation layer 1 is directly integrated on the metal wiring layer 22.

[0052] Form 2: As shown in FIG. 7, the CIS wafer 2 is a back-illuminated type, the light detection layer 21 is located above the metal wiring layer 22, no microlenses or filters are integrated on the CIS wafer, and the light modulation layer 1 is directly integrated on the light detection layer 21.

[0053] In the vertical direction, the light modulating layer 1 may be composed of one or more layers of material, which helps to enhance the spectral modulation and sampling ability of the light modulating layer 1 for the incident light, and improve the accuracy of the spectrum recovery. The light modulating layer 1 may have the following four forms in the vertical direction:

[0054] Form 1: 8, the light modulation layer 1 is a single-layer lattice structure of a single material, and the lattice units are structures with different shapes, with a thickness of 50 nm to 2 μm. Specific materials may include silicon, germanium, silicon germanium materials, silicon compounds, germanium compounds, metals, III-V materials, etc., among which silicon compounds include, but are not limited to, silicon nitride, silicon dioxide, and silicon carbide.

[0055] Form 2: 9 and 10, the light modulating layer 1 may be composed of two or more layers of materials, of which 11, 12, and 13 are all different materials, and the thickness of each layer is 50 nm to 2 μm. Specific materials may include silicon, germanium, silicon germanium materials, silicon compounds, germanium compounds, metals, III-V materials, etc., of which silicon compounds include, but are not limited to, silicon nitride, silicon dioxide, and silicon carbide.

[0056] Form 3: As shown in Fig. 11, the light modulating layer 1 may be composed of multiple layers or mixed materials, of which 11 and 12 are different materials and one or more layers may be solid, in Fig. 11, 12 is solid and each layer has a thickness of 50nm~2μm. Specific materials include silicon, germanium, silicon germanium material, silicon compound, germanium compound, metal, III-V group material, mixed sputtering material of silicon and SiN, etc., of which silicon compound includes but is not limited to silicon nitride, silicon dioxide, silicon carbide, etc.

[0057] Form 4: As shown in FIG. 12, the light modulation layer 1 is manufactured by directly etching its structure onto the light detection layer 21 of a back-illuminated CIS wafer, and the etching depth is 50 nm to 2 μm.

[0058] The microspectral chip based on different shape units of the present invention will be further described below with reference to specific embodiments.

[0059] Embodiment 1: As shown in FIG. 13, the spectrum chip includes a light modulation layer 1, a CIS wafer 2, and a signal processing circuit 3. The light modulation layer 1 is directly fabricated on the CIS wafer, and its lateral structure adopts the above-mentioned form 1, and the specific structure is shown in FIG. 14 and FIG. 15. The light modulation layer 1 includes a plurality of repeated micro-nano structure units, and the inside of each micro-nano structure unit is divided into 9 sets of different micro-nano structure arrays 110-118, and each set of micro-nano structure arrays is a lattice based on units of different shapes, and the shape of the lattice can be a regular shape such as a circle, a ring, a polygon, a cross, or other preset irregular shape, and the period of each set of micro-nano structure arrays is 20 nm-50 μm respectively, and each set of micro-nano structure arrays has a different broadband modulation effect on the incident light, and the micro-nano structure arrays at the corresponding positions in different micro-nano structure units are the same, and the overall size of each unit is 0.5 μm. 2 ~40,000μm 2 The medium material in the light modulation layer 1 is polycrystalline silicon, and the thickness is 50 nm to 2 μm.

[0060] The irregular shape may be a random shape generated by an algorithm, but this does not limit the present invention. It can be understood that the random shape of the present invention can be obtained by at least one algorithm, or by combining artificial adjustment and an algorithm. Here, the present invention provides an algorithm, the process of which is as follows. First, the area in one period is uniformly divided into meshes, and the size of the mesh can be flexibly set. Then, a refractive index is assigned to each lattice point in the mesh according to a certain distribution law, and the assignment is usually performed by adopting a standard normal distribution. However, the refractive index assigned here is just a numerical value and does not represent the refractive index of the actual material. Next, the refractive index distribution is subjected to image filter smoothing and binarization processing, and the refractive index distribution obtained at this time has only two values, 0 and 1, which respectively represent air and medium. Blurring and binarization are also required to eliminate the parts in the structure that are too small in size, so as to facilitate the process manufacturing. In the final generated image, the values ​​0 and 1 represent the air and medium regions, respectively, and do not include structures that are too small in size, which is convenient for processing. In addition, certain constraints can be imposed on the generated random structure. For example, if a particular symmetry is desired for the structure, the algorithm can symmetrize the refractive index distribution.Furthermore, by changing parameters in the algorithm, properties such as the minimum feature size of the generated random shapes can be tuned.

[0061] Figure 29 shows some of the random shapes generated by the algorithm, where the numbers 0 and 1 represent the air and medium regions, respectively. As can be seen, the algorithm can generate many different irregular shapes, which will generate different modulation effects on the incident light and help improve the accuracy of the spectrum recovery.

[0062] As shown in Figure 6, the specific structure of the CIS wafer 2 is as follows: 21 is a silicon detector layer, 22 is a metal wiring layer, the response range is from the visible to near infrared band, the CIS wafer is bare, and no Bayer filter array or microlens array is fabricated thereon. Each set of micro-nano structures corresponds to one or more optical sensor units in the CIS wafer 2.

[0063] The complete process of multispectral image acquisition is as shown in Fig. 16, broadband light source 100 illuminates object 200, and then reflected light is collected by spectrum chip 300 or light directly emitted by object is collected by spectrum chip 300. Each micro-nanostructure array and the light sensor below it constitute a pixel point, and the spectral information at each pixel point can be obtained by the restoration algorithm, and multiple pixel points constitute an image containing spectral information. Both the light modulation layer 1 and the CIS wafer 2 can be manufactured by semiconductor CMOS integration process, and the monolithic integration at wafer level can be realized to shorten the distance between the sensor and the light modulation layer, which helps to reduce the volume of the device, realize higher spectral resolution, and reduce the packaging cost.

[0064] Embodiment 2: In embodiment 2, as shown in FIG. 17, the main difference from embodiment 1 lies in the lateral structure, specifically, the multiple micro-nano structure units constituting the light modulation layer 1 have C4 symmetry, that is, after being rotated by 90°, 180°, or 270°, they overlap with the original structure without rotation, thus giving the structure polarization-independent properties.

[0065] Embodiment 3: In the third embodiment, as shown in FIG. 18, the main difference with the first embodiment is in the vertical structure of the micro-spectral chip, specifically, a light transmission medium layer 4 is added between the light modulation layer 1 and the CIS wafer 2, the thickness of the light transmission medium layer 4 is 50 nm-2 μm, and the material can be silicon dioxide. When the direct deposition growth process scheme is adopted, the light transmission medium layer can be manufactured on the CIS wafer by chemical vapor deposition, sputtering, spin coating and other methods, and then the light modulation layer structure can be deposited and etched on it. When the transfer process scheme is adopted, the micro-nano structure can be manufactured on the silicon dioxide first, and then the two parts can be transferred onto the CIS wafer as a whole. The manufacture of the spectrum chip can be completed in one tape-out by the CMOS process, which is helpful to reduce the failure rate of the device, improve the device yield and reduce the cost.

[0066] Embodiment 4: In embodiment 4, as shown in Fig. 19, the difference from embodiment 1 is that the lattice in the light modulation layer 1 is partially etched, and the holes do not completely penetrate the plate but have a certain depth. The thickness of the micro-nano structure is 50nm-2μm, the thickness of the whole plate is 100nm-4μm, and this structure may add a transparent medium layer between 1 and 2.

[0067] Embodiment 5: In embodiment 5, as shown in FIG. 20, the difference from embodiment 1 is that the light modulation layer 1 has a two-layer structure, 11 is a silicon layer, and 12 is a silicon nitride layer, and the thickness of each of the two-layer structure is 50 nm to 2 μm, and the lower layer material of this structure can also adopt a partially etched structure that is not penetrated, as shown in FIG. 21.

[0068] Embodiment 6: As shown in FIG. 22, the sixth embodiment is different from the first embodiment in that the CIS wafer is a back-illuminated type and the light detection layer 21 is located above the metal wiring layer 22, thereby reducing the effect of the metal wiring layer on the incident light and improving the quantum efficiency of the device.

[0069] Embodiment 7: In the seventh embodiment, the difference from the first embodiment is that a microlens or a filter or both are integrated in the spectrum chip. As shown in Figures 23 and 24, a microlens 4 is integrated in the spectrum chip, and the microlens can be above (Figure 23) or below (Figure 24) the light modulation layer; as shown in Figures 25 and 26, a filter 5 is integrated in the spectrum chip, and the filter can be above (Figure 25) or below (Figure 26) the light modulation layer; as shown in Figures 27 and 28, a microlens 4 and a filter 5 are integrated in the spectrum chip, and the positions can be above (Figure 27) or below (Figure 28) the light modulation layer.

[0070] Furthermore, the present invention provides a method for generating a micro-nano structure array in a spectrum chip, and the research objective of this embodiment of the present invention is to generate a random shape structure in a random manner, and make the two-dimensional lattice structure based on the random shape structure have rich broadband modulation characteristics for incident light, which helps to improve the accuracy of spectrum recovery. It can be understood that the random shape structure generated in the present invention in a random manner can be obtained by an algorithm, or a combination of artificial adjustment and algorithm, for example, generated by an algorithm and then artificially adjusted. Furthermore, the present invention takes the example of random generation by an algorithm.

[0071] 31 is a schematic diagram of the structure of a spectral chip according to an embodiment of the present invention. As shown in FIG. 31, the spectral chip includes a wafer-level image sensor 2, and a light modulation layer 1 is fabricated on the upper surface of the photosensitive region of the wafer-level image sensor 2, and the light modulation layer 1 includes a unit array consisting of a plurality of micro-nano units 4, each of which corresponds to one or more pixel points on the wafer-level image sensor 2, and the micro-nano units 4 include a plurality of sets of micro-nano structure arrays, each set of micro-nano structure arrays is formed in a two-dimensional lattice structure, and the two-dimensional lattice structure in the plurality of sets of micro-nano structure arrays of each micro-nano unit 4 is for modulating incident light and encoding the spectral information of the incident light into different pixel points of the wafer-level image sensor 2 to obtain an image including the spectral information of the incident light. The method for generating a micro-nanostructure array in the spectral chip includes the step of generating the two-dimensional grating structure, wherein the two-dimensional grating structure is formed by a periodic arrangement of random-shaped structures, wherein the random-shaped structures in the same set of micro-nanostructure arrays may be the same or different, and the random-shaped structures in different sets of micro-nanostructure arrays may be the same or different; The step of generating the two-dimensional lattice structure described above specifically includes the steps of: determining an arrangement period of the random shape structures in the two-dimensional lattice structure; generating each randomly shaped structure 5 in the two-dimensional lattice structure according to the following procedure: The processing procedure includes dividing an area within the array period into meshes to obtain a plurality of mesh areas; performing a random assignment of pixel values ​​for the plurality of mesh regions to obtain an initial pattern corresponding to the randomly shaped structure, where different pixel values ​​indicate that corresponding mesh regions have different refractive indices; and performing a binarization process on the initial pattern to obtain a first binarized pattern, the first binarized pattern corresponding to one random shape structure 5, and 0 and 1 in the first binarized pattern representing air and medium, respectively. In order to make the final random shape contour smoother, the initial pattern can be subjected to a filter smoothing process before the binarization process.

[0072] The following describes the method for generating the micro-nano structure array in the spectrum chip of this embodiment. The research objective of the present invention is to generate random shape structures in a random manner, and make the two-dimensional lattice structure based on the random shape structures have rich broadband modulation characteristics for the incident light, which helps to improve the accuracy of spectrum recovery.

[0073] In this embodiment, the structural schematic diagram of the spectral chip is shown in FIG. 31, where the spectral chip includes a wafer-level image sensor 2, and a light modulation layer 1 is fabricated on the upper surface of the photosensitive area of ​​the wafer-level image sensor 2, for example, by directly growing one or more layers of a medium or metal material on the photosensitive area of ​​the wafer-level image sensor 2, and then performing etching and manufacturing processes to obtain the light modulation layer 1.

[0074] In this embodiment, the wafer-level image sensor 2 can be realized by employing a CIS wafer.

[0075] The light modulating layer 1 includes a unit array consisting of a plurality of micro-nano units 4, each of which vertically corresponds to one or more pixel points on a wafer-level image sensor, and the micro-nano units 4 include a plurality of sets of micro-nano structure arrays, each set of micro-nano structure arrays being formed in a two-dimensional lattice structure. After passing through the light modulating layer 1, the incident light is modulated by the two-dimensional lattice structure in the plurality of sets of micro-nano structure arrays of each micro-nano unit 4, and the intensity of the modulated optical signal is detected by the wafer-level image sensor 2 and converted into an electrical signal.

[0076] It should be noted that in this embodiment, after the incident light passes through the light modulation layer 1, the two-dimensional lattice structure in the light modulation layer 1 modulates the incident light and encodes the spectral information of the incident light into different pixel points of the wafer-level image sensor to obtain an image containing the spectral information of the incident light. That is, after the incident light passes through the light modulation layer 1, it is converted into an electrical signal by the wafer-level image sensor 2 to form an image containing the spectral information of the incident light, and finally, the image containing the spectral information of the incident light is processed by a signal processing circuit connected to the wafer-level image sensor 2 to obtain the spectral information of the incident light.

[0077] FIG. 33 is a flowchart for generating a two-dimensional lattice structure according to one embodiment of the present invention. As shown in FIG. 33, generating a two-dimensional lattice structure according to an embodiment of the present invention includes the following steps 101 to 104.

[0078] Step 101: The arrangement period of the random shape structures in the two-dimensional lattice structure is determined.

[0079] In this step, the purpose of determining the arrangement period of the random shape structure in the two-dimensional lattice structure is to guide the area within one period to be divided into meshes in step 102. For example, if the arrangement period is assumed to be 300 nm, the area within 300 nm is divided into meshes.

[0080] According to the processing procedure of steps 102 to 104, each random shape structure in the two-dimensional lattice structure is generated.

[0081] Step 102: Divide the region within the array period into meshes to obtain a plurality of mesh regions.

[0082] In this step, referring to (1) of Fig. 5, the region within the array period is divided into meshes, for example, into 100*100 meshes within one period. Note that the size of the meshes can be flexibly set, and the smaller the mesh, the smoother the edges of the obtained random shape will be.

[0083] Step 103: For the multiple mesh regions, randomly assign pixel values ​​to obtain an initial pattern corresponding to the random shape structure, where different pixel values ​​indicate that corresponding mesh regions have different refractive indices.

[0084] In this step, pixel values ​​are randomly assigned to a plurality of mesh regions to obtain an initial pattern corresponding to the random shape structure (as shown in FIG. 34(2)), and referring to FIG. 34(2), the degree of color shading in different mesh regions corresponds to different pixel values, and corresponding refractive indices are assigned according to the pixel values, so that mesh regions with different pixel values ​​also have different refractive indices, and since pixel values ​​are randomly assigned to a plurality of mesh regions, there is also randomness in the assignment of refractive indices. However, the assigned refractive indices in this step are simply numerical values ​​and do not represent the refractive indices of the actual material.

[0085] Step 104: Perform a binarization process on the initial pattern to obtain a first binarized pattern, where the first binarized pattern corresponds to one random shape structure, and 0 and 1 in the first binarized pattern represent air and medium, respectively. In order to make the final random shape contour more smooth, the initial pattern can be subjected to a filter smoothing process before performing the binarization process.

[0086] For example, in this step, a filter smoothing process is performed on an initial pattern (as shown in FIG. 34(2)) to obtain a pattern (as shown in FIG. 34(3)), and a binarization process is performed to obtain a first binarized pattern (as shown in FIG. 34(4)). In this step, the binarization process can be performed, for example, by a method in which "all regions where the refractive index is greater than a certain threshold are set to 1, and all regions where the refractive index is less than this threshold are set to 0", and the refractive index distribution obtained at this time has only two values, 0 and 1, which represent air and medium, respectively. In this step, the initial pattern is obtained by randomly allocating pixel values ​​to multiple mesh regions, so that a random shape structure can be generated.

[0087] It can be understood that after obtaining a first binarized pattern, according to the distribution situation of air and medium on the first binarized pattern, a corresponding medium can be used to etch according to the first binarized image to obtain a corresponding random shape structure.

[0088] In this embodiment, it can be understood by referring to the cross-sectional view of the spectral chip shown in Figure 32, where each set of micro-nanostructure arrays in the spectral modulation layer is formed based on a two-dimensional lattice structure, and by changing the random shape structure 5 of the two-dimensional lattice structure, the micro-nanostructure arrays have different modulation effects on the incident light in the target wavelength band.

[0089] As can be seen from the above technical solution, the method for generating a micro-nanostructure array in a spectral chip according to an embodiment of the present invention involves dividing an area within an array period into meshes to obtain a plurality of mesh areas, randomly allocating pixel values ​​to the plurality of meshes to obtain an initial pattern, and then performing a smoothing filter and binarization processing on the initial image to further obtain a random shape structure. Each set of micro-nanostructure arrays, i.e., each two-dimensional lattice structure, is composed of a random shape structure generated randomly in this way, so that the light modulation layer including multiple sets of micro-nanostructure arrays contains a variety of random shape structures, thereby giving the light modulation layer rich broadband modulation characteristics for incident light, which is advantageous in overcoming the limitations in the accuracy of spectral recovery, realizing high-precision measurement of the incident light spectrum, and improving the accuracy of spectral recovery.

[0090] In addition to the above embodiments, in this embodiment, after obtaining the first binarized pattern, the method further comprises: The method further includes the step of sequentially performing a blurring process and a binarization process on the first binary pattern to obtain a second binary pattern, whereby the second binary pattern corresponds to a random shape structure.

[0091] In this embodiment, referring to FIG. 35 , after obtaining a first binary pattern, in order to remove the parts in the random shape structure that are too small in size and facilitate processing, blurring and binary processing are sequentially performed on the first binary pattern to generate a second binary pattern, which corresponds to one random shape structure, and the random shape structure corresponding to the second binary pattern does not include any structures that are too small in size, which is convenient for processing.

[0092] In addition, the undersized and / or oversized portions of the randomly shaped structures can be directly selected and removed by means of an algorithm or the like, which is convenient for processing.

[0093] In addition to the above embodiment, in this embodiment, the step of randomly allocating pixel values ​​to the plurality of mesh regions to obtain an initial pattern corresponding to the random shape structure further comprises: Grouping a plurality of mesh regions to obtain a plurality of sets of meshes, in which when grouping the plurality of mesh regions, one or more mesh regions are grouped as one set; Randomly assigning pixel values ​​to each set of meshes according to a standard normal distribution to obtain an initial pattern corresponding to the random geometric structure, where the pixel values ​​of each mesh region in the set are the same.

[0094] In this embodiment, referring to FIG. 36, for example, the arrangement period of the random-shaped structure in the two-dimensional lattice structure is determined to be 300 nm, and one period is divided into 100*100 meshes and grouped (for example, grouped into 10*10 large meshes, i.e., 10 lattice points are divided into one large mesh), and pixel values ​​are randomly assigned to each set of meshes according to the standard normal distribution to obtain an initial pattern corresponding to the random-shaped structure (as shown by the dashed frame in FIG. 36).

[0095] As can be seen from the above technical solution, the method for generating a micro-nanostructure array in a spectral chip according to an embodiment of the present invention randomly assigns pixel values ​​to each set of meshes according to a standard normal distribution, and makes the pixel values ​​of each mesh area in the set the same to obtain the same random shape structure.

[0096] In addition to the above embodiment, in this embodiment, when generating each random shape structure in the two-dimensional lattice structure, one or more of a mesh division parameter corresponding to a mesh division operation, a random allocation parameter corresponding to a pixel value random allocation operation, a filter smoothing parameter corresponding to a filter smoothing operation, and a blurring parameter corresponding to a blurring operation are controlled so that the minimum size of the random shape structure is greater than a preset threshold and the ratio of the medium to air in the random shape structure satisfies a preset constraint condition. Furthermore, in a separate embodiment, this method also needs to control the maximum size of the random shape structure to be smaller than a preset threshold and the ratio of the medium to air in the random shape structure to satisfy a preset constraint condition.

[0097] In this embodiment, it can be understood that by adjusting the algorithm parameters (e.g., one or more of mesh division parameters, random allocation parameters, filter smoothing parameters, and blurring parameters), a random shaped structure having a minimum feature size larger than a preset threshold value can be generated, for example, the minimum feature size of the generated random shaped structure can be controlled to be larger than 30 nm, and by adjusting the algorithm parameters, the ratio of medium to air in the random shaped structure can be controlled to be within a specific range, for example, the proportion of medium area is 20% to 80%, so as to satisfy constraints.

[0098] As can be seen from the above technical solution, the method for generating a micro-nano structure array in a spectrum chip according to the embodiment of the present invention can set a certain restriction on the generated random shape structure by adjusting algorithm parameters, such as mesh division parameters, random allocation parameters, filter smoothing parameters, blurring parameters, etc., and control the minimum characteristic size of the generated random shape according to the requirements of process manufacturing, so as to meet the requirements of processing precision of process manufacturing, thereby reducing the difficulty. At the same time, it can be seen that by controlling the relevant processing parameters in the process of generating the random shape structure, the size of the random shape structure can be easily controlled to be reduced, so that the volume and cost of the spectrum chip can be easily reduced.

[0099] Furthermore, in some embodiments, the random shape generated by the algorithm has a richer curvature change than regular shapes such as circles, squares, and crosses, and preferably the shape that can be generated has two or more different curvatures, so that the light modulation effect is better. For example, different curvatures are specified, for example, a circle containing one type of curvature has its curvature specified, while a sector contains three types of curvatures: 0 (straight line), infinity (vertex), and a specific value (arc). It can be understood that the richer the curvature of the structure, the more significant the effects of scattering, refraction, etc. on the incident light, and the better the light modulation effect, so in the present invention, preferably, the internal unit of the random shape can contain two, three, four, five or more curvatures.

[0100] In addition to the above embodiment, in this embodiment, after obtaining the first binarized pattern or the second binarized pattern, the method further includes: performing a symmetry process on the first binarized pattern or the second binarized pattern to obtain a pattern with symmetry, and correspondingly, the pattern with symmetry corresponds to a random shape structure; Wherein, the symmetry processing includes one or more of the following: a two-fold rotational symmetry processing, a mirror symmetry processing about the Y axis, a mirror symmetry processing about the X axis, a simultaneous mirror symmetry processing about the Y axis and the X axis, a four-fold rotational symmetry processing, and a simultaneous mirror symmetry and four-fold rotational symmetry processing about the Y axis and the X axis; Correspondingly, the pattern with the acquired symmetry is The pattern may include one or more of the following: a pattern with two-fold rotational symmetry, a pattern with mirror symmetry about the Y axis, a pattern with mirror symmetry about the X axis, a pattern with simultaneous mirror symmetry about the Y and X axes, a pattern with four-fold rotational symmetry, and a pattern with simultaneous mirror symmetry and four-fold rotational symmetry about the Y and X axes.

[0101] In this embodiment, after acquiring the first binary pattern or the second binary pattern, a symmetry processing is performed on the first binary pattern or the second binary pattern using a corresponding symmetry processing function, thereby obtaining a pattern having symmetry. It can be understood that different symmetry processing functions need to be adopted for different symmetry processing. For example, a double rotation symmetry processing needs to be realized by adopting a double rotation symmetry processing function, that is, a pattern having double rotation symmetry can be obtained by processing the obtained first binary pattern or the second binary pattern using the double rotation symmetry processing function. In addition, in order to simplify the processing procedure, the above processing can be directly performed in MATLAB (registered trademark). For example, a symmetry processing for the first binary pattern or the second binary pattern can be realized by calling the corresponding symmetry processing function based on the MATLAB (registered trademark) software. For example, assuming that a four-fold rotation symmetry processing needs to be performed on the first binary pattern or the second binary pattern, a pattern having four-fold rotation symmetry is obtained by calling the four-fold rotation symmetry processing function. Similarly, for example, assuming that it is necessary to perform mirror symmetry processing about the Y axis on the first binary pattern or the second binary pattern, a pattern having mirror symmetry about the Y axis is obtained by calling a mirror symmetry processing function about the Y axis.

[0102] In this embodiment, symmetry restrictions are imposed on the first binarized pattern or the second binarized pattern with reference to Fig. 37 to Fig. 42. For example, in Fig. 37, a double rotational symmetry process is performed to obtain a pattern having double rotational symmetry, in Fig. 38, a mirror symmetry process about the Y axis is performed to obtain a pattern having mirror symmetry about the Y axis, in Fig. 39, a mirror symmetry process about the X axis is performed to obtain a pattern having mirror symmetry about the X axis, in Fig. 40, a mirror symmetry process about the Y axis and the X axis is simultaneously performed to obtain a pattern having mirror symmetry about the Y axis and the X axis simultaneously, in Fig. 41, a fourfold rotational symmetry process is performed to obtain a pattern having fourfold rotational symmetry, and in Fig. 42, a mirror symmetry process about the Y axis and the X axis and a fourfold rotational symmetry process are simultaneously performed to obtain a pattern having mirror symmetry about the Y axis and the X axis simultaneously and a fourfold rotational symmetry process are simultaneously performed.

[0103] Here, in order to make the two-dimensional lattice structure in the micro-nano structure array a lattice structure having polarization-independent characteristics, in one implementation form, a pattern having four-fold rotational symmetry can be obtained by performing four-fold rotational symmetry processing on the first binary pattern or the second binary pattern. Note that since the two-dimensional lattice structure in the micro-nano structure array satisfies four-fold rotational symmetry, the light modulation layer is not sensitive to the polarization of the incident light. In addition, in the present embodiment, in a conventional spectrometer, it is necessary to separate different wavelength components of the incident light by a spectroscopic element before detection, but the spectroscopic element often has different responses to incident light of different angles and different polarizations. In practical use, since the incident angle and polarization characteristics of the light to be measured cannot be known in advance, the conventional spectrometer usually needs to add a collimating element and a polarizing plate, which not only increases the volume and cost of the device, but also reduces the operation stability of the device. Therefore, it is important in practical use to realize a spectral device that is not sensitive to either the incident angle or the polarization. For this reason, the embodiment of the present invention provides a spectral chip, and performs a four-fold rotational symmetry process on the first binarized pattern or the second binarized pattern obtained in the process of generating a micro-nano structure array in the spectral chip to obtain a random shape structure with four-fold rotational symmetry. As a result, the spectral chip can measure the spectral information of incident light without being affected by the incident angle or the polarization characteristics of the incident light within a certain range, that is, the spectral chip is not sensitive to the incident angle or polarization, so the spectral measurement results are not affected by the incident angle and polarization characteristics of the light to be measured, and the stability of the spectral measurement performance can be ensured. In addition, the spectral chip of the embodiment of the present invention monolithically integrates an optical modulation layer that is not sensitive to the incident angle and polarization with a wafer-level image sensor, and there is no separate element and no need to add complex optical devices such as collimating elements, polarizing plates, etc., which helps to improve the stability of the device and reduce the volume and cost of the device.

[0104] As can be seen from the above technical solution, the method for generating a micro-nanostructure array in a spectral chip according to an embodiment of the present invention can impose symmetry constraints on the binary pattern, so that the generated random-shaped structures can meet different symmetry requirements.

[0105] In addition to the above embodiments, in this embodiment, after obtaining the first binary pattern or the second binary pattern, the method further includes performing an expansion or erosion operation on the first binary pattern or the second binary pattern, so as to simulate an under-etching or over-etching situation during process manufacturing.

[0106] In this embodiment, referring to Figures 43 to 45, an expansion or corrosion operation is performed on a first binary pattern or a second binary pattern, with Figure 43 being a random-shaped binary pattern, Figure 44 being a corrosion operation on a binary pattern, for example, a random-shaped binary pattern after the medium area has been corroded by 10 nm, and Figure 45 being a random-shaped binary pattern after an expansion operation is performed on a binary pattern, for example, a random-shaped binary pattern after the medium area has been expanded by 10 nm.

[0107] As can be seen from the above technical solution, the method for generating a micro-nanostructure array in a spectral chip according to an embodiment of the present invention can simulate the situation of under-etching or over-etching during process manufacturing, and through subsequent electromagnetic simulation, can analyze the impact of under-etching or over-etching on the spectral characteristics of the structure, thereby facilitating the analysis of the process error resistance characteristics of the structure, and thereby selecting a random-shaped structure with relatively good process error resistance characteristics.

[0108] In addition to the above embodiment, in this embodiment, the spectrum chip further includes a signal processing circuit 3 connected to the wafer-level image sensor 2, The signal processing circuit 3 is for processing an image containing spectral information of the incident light to obtain the spectral information of the incident light.

[0109] In this embodiment, the light modulation layer includes multiple repeat units, and a signal processing circuit corresponding to each unit can recover the spectral information of the unit. The input of the signal processing circuit is the light intensity signal detected by each photosensitive pixel of the CIS wafer, and these light intensity values ​​can be used to combine the transmission spectrum of each set of micro-nano structure arrays measured in advance in an experiment, and the spectral information of the input light can be recovered through a corresponding algorithm. In practical application, different algorithms can be used to process the image containing the spectral information of the incident light as needed to obtain the spectral information of the incident light.

[0110] In this embodiment, the complete flow of collecting multi-spectral images is as shown in Fig. 46, after a broadband light source 100 from visible light to near infrared illuminates a target object 200, the reflected light is collected by the spectrum chip 300, or the light directly emitted from the target object is collected by the spectrum chip 300. Each unit forms a pixel point together with the light sensor below it, and the spectral information on each pixel point can be obtained through a recovery algorithm, and multiple pixel points form an image containing spectral information. Both the light modulation layer 1 and the wafer-level image sensor 2 can be manufactured by semiconductor CMOS integration process, which can realize monolithic integration at the wafer level, which is helpful in shortening the distance between the sensor and the light modulation layer, reducing the volume of the device, achieving higher spectral resolution, and reducing packaging costs.

[0111] In this embodiment, referring to FIG. 31 , the spectral chip further includes a signal processing circuit 3 connected to the wafer-level image sensor 2, and the signal processing circuit 3 processes an image including spectral information of the incident light to recover and acquire the spectral information of the incident light.

[0112] In addition to the above embodiments, in this embodiment, a light transmission medium layer is provided between the light modulation layer 1 and the wafer-level image sensor 2 .

[0113] In this embodiment, by providing a light-transmitting medium layer between the light modulation layer and the wafer-level image sensor, the light modulation layer and the wafer-level image sensor can be effectively separated to avoid mutual interference between the two.

[0114] Here, the thickness of the light transmission medium layer can be 50nm-1μm, and the material can be silica. In the case of a direct deposition growth process, the light transmission medium layer can be fabricated on the wafer-level image sensor by chemical vapor deposition, sputtering, or spin coating, and then the light modulation layer structure can be deposited and etched on top of it. In the case of a transfer process, the micro-nano structure can be fabricated on the silica, and then the two parts can be transferred to the wafer-level image sensor as a whole.

[0115] In addition to the above embodiments, in this embodiment, the wafer-level image sensor 2 is a front-illuminated type, and includes a metal line layer and a light detection layer arranged from top to bottom, and the light modulation layer 1 is integrated on the side of the metal line layer away from the light detection layer, or The wafer-level image sensor 2 is back-illuminated and includes a photodetection layer and a metal line layer arranged from top to bottom, and the photomodulation layer 1 is integrated on the side of the photodetection layer away from the metal line layer.

[0116] In addition, in a back-illuminated wafer-level image sensor, the light detection layer is above the metal line layer, which can reduce the influence of the metal line layer on the incident light and increase the quantum efficiency of the device.

[0117] In addition to the above embodiments, in this embodiment, the spectral chip further includes a microlens and / or a filter; the microlens is provided on a surface of the light modulating layer 1 that is remote from the wafer-level image sensor 2, or the microlens is provided on a surface of the light modulating layer 1 that is close to the wafer-level image sensor 2, The filter is provided on a side of the light modulating layer 1 away from the wafer-level image sensor 2 or the filter is provided on a side of the light modulating layer 1 closer to the wafer-level image sensor 2 .

[0118] Moreover, in the present invention, the terms "first", "second", etc. are merely for descriptive purposes and are not to be understood as indicating or implying a relative importance or implicitly indicating the number of technical features indicated. Thus, a feature that is qualified by "first" or "second" may expressly or imply that it includes at least one of the feature. In the description of the present invention, unless there is a clear and specific limitation, "plurality" means at least two, e.g., two, three, etc.

[0119] In the present invention, the use of relational terms such as "first" and "second" is merely intended to distinguish one entity or operation from another entity or operation, and does not necessarily require or imply that there is any actual relationship or sequence between these entities or operations. And, "comprises," "includes," or any other variation thereof is intended to cover a non-exclusive inclusion, so that a process, method, article, or device that includes a set of elements includes not only those elements, but also other elements not expressly stated or elements inherent to the process, method, article, or device. In the absence of further limitations, an element defined by the phrase "including a ..." does not exclude the presence of other identical elements in the process, method, article, or device that includes the element.

[0120] Also, in the description of this specification, a description referring to terms such as "one embodiment", "multiple embodiments", "example", "specific example" or "multiple examples" means that the specific feature, structure, material, or characteristic described with reference to the embodiment or example is included in at least one embodiment or example of the present invention. In this specification, general expressions of the above terms are not necessarily directed to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described can be combined in any suitable manner in any one or more embodiments or examples. It is noted that a person skilled in the art can combine and combine different embodiments or examples described in this specification and features of different embodiments or examples without mutual contradiction.

[0121] The above description is a preferred embodiment of the present application, and merely describes the technical principles applied. Those skilled in the art should understand that the scope of the disclosure of the present application is not limited to the technical solution formed by a specific combination of the above technical features, and at the same time, covers other technical solutions composed of any combination of the above technical features or their equivalents without departing from the above disclosed ideas. For example, technical solutions formed by replacing the above features with technical features having similar functions to the technical features disclosed in the present application (but not limited to them).

[0122] The above-mentioned embodiment is merely for illustrative purposes of the principles and effects of the present invention, and is not intended to limit the present invention. Those skilled in the art may make improvements or modifications to the above-mentioned embodiment without departing from the spirit and scope of the present invention. Therefore, all equivalent improvements or modifications made by a person having ordinary knowledge in the art without departing from the spirit and technical ideas disclosed in the present invention are still included in the scope of the claims of the present invention.

Claims

1. A CIS wafer, a light modulation layer, and a signal processing circuit, The light modulation layer includes a plurality of micro-nanostructure units provided on the surface of the photosensitive region of the CIS wafer, each micro-nanostructure unit includes one or more micro-nanostructure arrays, the micro-nanostructure array in at least one micro-nanostructure unit is a two-dimensional lattice composed of internal units of different shapes, and the micro-nanostructure array in at least one micro-nanostructure unit is a two-dimensional lattice composed of internal units of random shapes, and the random-shaped internal units have at least two types of curvature, characterized in that the micro-spectral chip is based on units of different shapes.

2. The micro-spectral chip based on units of different shapes as described in claim 1, characterized in that each of the one or more micro-nanostructure arrays is a two-dimensional lattice composed of internal units of different shapes.

3. The plurality of micro-nanostructure units are identical repeating units, and the micro-nanostructure arrays located at corresponding positions in different micro-nanostructure units are the same, and / or there is no micro-nanostructure array at at least one corresponding position in different micro-nanostructure units, and / or the size of each of the plurality of micro-nanostructure units is less than 0.5 μm. 2 ~40,000μm 2 and / or the period of each of the plurality of micro-nanostructure arrays is 20 nm to 50 μm. The micro-spectral chip based on different shaped units of claim 1 .

4. The micro-spectral chip based on different shaped units as described in claim 1, characterized in that the number of micro-nanostructure arrays contained in each of the plurality of micro-nanostructure units is dynamically adjustable and / or the plurality of micro-nanostructure units have C4 symmetry.

5. The micro-spectral chip based on different shaped units as claimed in claim 1 , wherein each micro-nanostructure array corresponds to one or more pixels in the CIS wafer.

6. The microspectral chip based on different shape units according to claim 1 , characterized in that the signal processing circuitry is connected to the CIS wafer via electrical contacts.

7. The micro-spectral chip based on different shaped units as described in claim 1, characterized in that the CIS wafer includes a light detection layer and a metal wiring layer, and the light detection layer is located below the metal wiring layer and the light modulation layer is integrated on the metal wiring layer, or the light detection layer is located above the metal wiring layer and the light modulation layer is integrated on the light detection layer.

8. The micro-spectral chip based on different-shaped units as claimed in claim 1, characterized in that the light modulation layer is a single-layer, double-layer or multi-layer structure, and the thickness of each layer is 50 nm to 2 μm; the material of the light modulation layer is at least one of silicon, germanium, silicon germanium material, silicon compound, germanium compound, metal or III-V material, among which the silicon compound includes at least one of silicon nitride, silicon dioxide, and silicon carbide; and / or when the light modulation layer is double-layer or multi-layer, at least one layer is not penetrated.

9. The microspectral chip based on different shaped units as described in claim 1, characterized in that a light-transmitting medium layer is provided between the light modulation layer and the CIS wafer, the thickness of the light-transmitting medium layer is 50 nm to 2 μm, and the material of the light-transmitting medium layer is silicon dioxide.

10. The microspectral chip based on different shaped units as described in claim 1, characterized in that the microspectral chip is integrated with microlenses and / or filters, and the microlenses and / or filters are installed above or below the light modulation layer.

11. A method for producing a micro-nanostructure array on a spectral chip, comprising: The spectral chip includes a wafer-level image sensor, and a light modulating layer is fabricated on the upper surface of the photosensitive region of the wafer-level image sensor, and the light modulating layer includes a unit array consisting of a plurality of micro-nano units, each of which corresponds to one or more pixel points on the wafer-level image sensor, and the micro-nano units include a plurality of sets of micro-nano structure arrays, each set of micro-nano structure arrays being formed in a two-dimensional lattice structure, and the two-dimensional lattice structure in the plurality of sets of micro-nano structure arrays of each micro-nano unit is for modulating incident light and encoding spectral information of the incident light into different pixel points of the wafer-level image sensor, to obtain an image including the spectral information of the incident light; The method for generating a micro-nano structure array on the spectral chip includes generating the two-dimensional grating structure, the two-dimensional grating structure being formed by a periodic arrangement of randomly shaped structures; The step of generating the two-dimensional lattice structure comprises: determining an arrangement period of the random shape structures in the two-dimensional lattice structure; generating each randomly shaped structure in the two-dimensional lattice structure according to the following procedure: The processing procedure includes: Dividing an area within the array period into meshes to obtain a plurality of mesh areas; performing a random assignment of pixel values ​​for the plurality of mesh regions to obtain an initial pattern corresponding to the randomly shaped structure, where different pixel values ​​indicate that corresponding mesh regions have different refractive indices; A method for generating a micro-nanostructure array on a spectral chip, comprising: performing a binarization process on the initial pattern to obtain a first binarized pattern, the first binarized pattern corresponding to one randomly shaped structure, and 0 and 1 in the first binarized pattern representing air and medium, respectively.

12. The method for generating a micro-nano structure array in a spectral chip according to claim 11, characterized in that a filter smoothing process is performed on the initial pattern before a binarization process is performed on the initial pattern.

13. After obtaining the first binarized pattern, The method for generating a micro-nanostructure array on a spectral chip as described in claim 12, further comprising the step of sequentially performing a blurring process and a binarization process on the first binarized pattern to obtain a second binarized pattern, whereby the second binarized pattern corresponds to a randomly shaped structure.

14. Randomly assigning pixel values ​​to the plurality of mesh regions to obtain an initial pattern corresponding to the random shape structure, Grouping a plurality of mesh regions to obtain a plurality of sets of meshes, in which when grouping the plurality of mesh regions, one or more mesh regions are grouped as one set; The method for generating a micro-nanostructure array in a spectral chip as described in claim 12, characterized in that it includes randomly assigning pixel values ​​to each set of meshes according to a standard normal distribution to obtain an initial pattern corresponding to the randomly shaped structure, wherein the pixel values ​​of each mesh region in the set are the same.

15. and performing a symmetry process on the first binarized pattern or the second binarized pattern after obtaining the first binarized pattern or the second binarized pattern to obtain a pattern having symmetry, whereby the pattern having symmetry corresponds to a random shape structure; The symmetry processing includes one or more of the following: a two-fold rotational symmetry processing, a mirror symmetry processing about the Y axis, a mirror symmetry processing about the X axis, a simultaneous mirror symmetry processing about the Y axis and the X axis, a four-fold rotational symmetry processing, and a simultaneous mirror symmetry and four-fold rotational symmetry processing about the Y axis and the X axis; The method for generating a micro-nanostructure array in a spectral chip as described in claim 13, characterized in that the pattern with the acquired symmetry includes one or more of the following: a pattern with two-fold rotational symmetry, a pattern with mirror symmetry about the Y axis, a pattern with mirror symmetry about the X axis, a pattern with mirror symmetry simultaneously about the Y axis and the X axis, a pattern with four-fold rotational symmetry, and a pattern with mirror symmetry and four-fold rotational symmetry simultaneously about the Y axis and the X axis.

16. The method for generating a micro-nanostructure array in a spectral chip as described in claim 13, characterized in that after obtaining the first binarized pattern or the second binarized pattern, the method further includes performing an expansion or corrosion operation on the first binarized pattern or the second binarized pattern so as to simulate a situation of insufficient etching or over-etching during process manufacturing.

17. the spectral chip further includes a signal processing circuit coupled to the wafer-level image sensor; the signal processing circuit is for processing an image including spectral information of the incident light to obtain the spectral information of the incident light; a light transmission medium layer is provided between the light modulation layer and the wafer-level image sensor; The wafer-level image sensor is a front-illuminated type, and includes a metal line layer and a light detection layer arranged from top to bottom, and the light modulation layer is integrated on a surface of the metal line layer away from the light detection layer; or The method for generating a micro-nanostructure array in a spectral chip, as described in claim 12, characterized in that the wafer-level image sensor is back-illuminated and includes a photodetection layer and a metal line layer arranged from top to bottom, and the photomodulation layer is integrated on a surface of the photodetection layer away from the metal line layer.

18. The spectral chip further comprises a microlens and / or a filter; the microlens is disposed on a surface of the light modulating layer away from a wafer-level image sensor, or the microlens is disposed on a surface of the light modulating layer closer to a wafer-level image sensor; The method for generating a micro-nanostructure array on a spectral chip as described in claim 12, characterized in that the filter is provided on a surface of the light modulation layer away from a wafer-level image sensor, or the filter is provided on a surface of the light modulation layer closer to a wafer-level image sensor.

Citation Information

Patent Citations

  • Light modulation micro-nano structure, micro-integrated spectrometer and spectral modulation method

    CN110346313A

  • Spectral imaging chip and spectral recognition equipment

    CN111490060A

  • Monolithic integrated image sensing chip and spectrum recognition equipment

    CN111505820A

  • Spectrometer structure and electronic equipment

    CN211122509U

  • Electromagnetic wave detector

    JP2015121417A