Semiconductor package manufacturing method
The method efficiently forms functional layers on semiconductor packages by arranging them on a support carrier with a 0.1 mm interval and using sputtering or vapor deposition, addressing signal interference and enhancing performance.
Patent Information
- Application Number
- JP2022509221
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-03-27
- Filing Date
- 2020-07-28
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2040-07-28
AI Technical Summary
The miniaturization and increased integration of semiconductor packages lead to impaired performance due to increased impedance and signal interference between signal lines, necessitating an efficient method to form functional layers like electromagnetic shielding layers on their surfaces.
A method involving forming a temporary fixing material layer on a panel member, applying an adhesive film, dividing into individual packages, arranging them on a support carrier with a 0.1 mm interval, and forming a functional layer like an electromagnetic shielding layer through sputtering or vapor deposition, ensuring the layer wraps around the circuit surface.
This method allows for stable formation of a functional layer on the semiconductor package, even with thin rewiring layers, reducing signal interference and enhancing performance.
Smart Images

Figure 0007582295000001 
Figure 0007582295000002 
Figure 0007582295000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a semiconductor package, and more specifically, to a method for manufacturing a semiconductor package having a functional layer (for example, an electromagnetic wave shielding layer) on at least a portion of its surface. [Background technology]
[0002] In recent years, semiconductor packages have become smaller, more functional, and more integrated, leading to an increase in the number of pins on semiconductor chips, higher density, and narrower wiring pitches. As a result, the inherent performance of semiconductor packages tends to be impaired due to increased impedance or signal interference between signal lines. Patent Document 1 discloses an adhesive film for semiconductor devices having an adhesive layer and an electromagnetic wave shielding layer. This adhesive film for semiconductor devices is produced through a process of forming an electromagnetic wave shielding layer on the surface of the adhesive layer by sputtering or vapor deposition. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-124466 A Summary of the Invention [Problem to be solved by the invention]
[0004] The present inventors have investigated the possibility of imparting such a function to a semiconductor package by directly forming a functional layer such as an electromagnetic wave shielding layer on the surface of the semiconductor package. The present disclosure provides a method for efficiently manufacturing a semiconductor package having at least a portion of its surface covered with a functional layer. [Means for solving the problem]
[0005] The method for manufacturing a semiconductor package according to the present disclosure includes the following steps. (A) A step of forming a temporary fixing material layer on a first surface of a panel member having a plurality of semiconductor packages, the first surface on which circuit surfaces or rewiring layers of the plurality of semiconductor packages are exposed. (B) applying a first adhesive film to a second surface of the panel member. (C) A step of singulating the panel member and the temporary fixing material layer on the first adhesive film into a plurality of semiconductor packages with temporary fixing material pieces. (D) A process of arranging a plurality of semiconductor packages with temporary fixing material pieces on a support carrier so that the temporary fixing material pieces of the semiconductor packages with temporary fixing material pieces are in contact with the support carrier and the spacing between adjacent semiconductor packages with temporary fixing material pieces is 0.1 mm or more. (E) A step of peeling off the first adhesive film from the support carrier and the semiconductor package with the plurality of temporary fixing material pieces. (F) A step of forming a functional layer on the surface of the semiconductor package with the multiple temporary fixing material pieces exposed by peeling off the first adhesive film. After the step (A), a step of curing the temporary fixing material layer by ultraviolet irradiation or heat treatment may be carried out.
[0006] According to the above manufacturing method, in step (D), a plurality of semiconductor packages with temporary fixing material pieces are arranged on a support carrier so that the interval between two adjacent semiconductor packages with temporary fixing material pieces is 0.1 mm or more, so that in step (F), a functional layer of a desired thickness can be formed on the side surface of the semiconductor package, for example, by sputtering or vapor deposition. In addition, in step (F), a functional layer is formed on a semiconductor package whose circuit surface is covered with temporary fixing material pieces, so that the material constituting the functional layer can be prevented from flowing around to the circuit surface of the semiconductor package. The functional layer is, for example, an electromagnetic wave shielding layer (metal layer).
[0007] The first adhesive film may be a film having extensibility (hereinafter referred to as "extensible film"). In this case, the step (D) may include the following steps: (d1) Enlarging the distance between two adjacent semiconductor packages with temporary fixing material pieces by applying tension to the first adhesive film. (d2) transferring the semiconductor packages with the plurality of temporary fixing material pieces on the first adhesive film to a support carrier while tension is being applied to the first adhesive film; By carrying out these steps in the process (D), it is possible to collectively arrange a plurality of semiconductor packages with temporary fixing material pieces on the first adhesive film on the support carrier.
[0008] After the step (F), the following steps may be appropriately carried out so that the semiconductor packages can be picked up efficiently. (G) A process of attaching a second adhesive film so as to cover the functional layer formed on the surface of the semiconductor package with the plurality of temporary fixing material pieces. (H) A step of peeling off the temporary fixing material pieces together with the support carrier from the plurality of semiconductor packages on the second adhesive film.
[0009] When the functional layer is an electromagnetic shielding layer, the semiconductor package may have a redistribution layer less than 50 μm thick and a ground contact point provided on a side of the redistribution layer. Even if the redistribution layer of the semiconductor package is as thin as less than 50 μm, the electromagnetic shielding layer can be stably formed on the side of the redistribution layer in step (F). Therefore, the ground contact point on the side of the redistribution layer can be electrically connected to the electromagnetic shielding layer (see FIG. 1). Effect of the Invention
[0010] According to the present disclosure, there is provided a method for efficiently manufacturing a semiconductor package having at least a portion of a surface covered with a functional layer. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a cross-sectional view that illustrates a schematic example of a semiconductor package (fan-out wafer-level package) manufactured by the manufacturing method of the present disclosure. [Diagram 2]FIG. 2 is a plan view showing a schematic example of a panel member for a fan-out wafer-level package. [Diagram 3] Figure 3(a) is a cross-sectional view showing a schematic state in which a temporary fixing material layer has been formed on a first surface of a panel member, Figure 3(b) is a cross-sectional view showing a schematic state in which a first adhesive film has been attached to a second surface of the panel member, and Figure 3(c) is a cross-sectional view showing a schematic state in which the panel member and the temporary fixing material layer have been diced into semiconductor packages with multiple temporary fixing material pieces. [Figure 4] Figure 4(a) is a cross-sectional view showing, as a schematic, a state in which the distance between two adjacent semiconductor packages with temporary fixing material pieces is expanded by applying tension to a first adhesive film; Figure 4(b) is a cross-sectional view showing, as a schematic, a state in which a support carrier is attached to multiple semiconductor packages with temporary fixing material pieces on a first adhesive film with tension applied to the first adhesive film; and Figure 4(c) is a cross-sectional view showing, as a schematic, a state in which the first adhesive film has been peeled off from the state shown in Figure 4(b). [Diagram 5] FIG. 5 is a cross-sectional view that illustrates a state in which an electromagnetic wave shielding layer (functional layer) is formed on the surface of a semiconductor package with a plurality of temporary fixing material pieces attached thereto. [Figure 6] 6(a) to 6(c) are cross-sectional views that typically show the process up to picking up a semiconductor package. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, an embodiment of the present disclosure will be described in detail with reference to the drawings. In the following description, the same or equivalent parts are given the same reference numerals, and duplicated descriptions will be omitted. Furthermore, unless otherwise specified, the positional relationships such as up, down, left, and right are based on the positional relationships shown in the drawings. Furthermore, the dimensional ratios of the drawings are not limited to the illustrated ratios.
[0013] When terms such as "left", "right", "front", "back", "top", "bottom", "upper", and "lower" are used in the description and claims of this specification, they are intended to be explanatory and do not necessarily mean that the relative positions are permanently in this order. Furthermore, the term "layer" encompasses a structure having a shape formed on the entire surface as well as a structure having a shape formed on a part of the surface when observed in a plan view.
[0014] (Semiconductor Package) FIG. 1 is a cross-sectional view showing a semiconductor package manufactured by the manufacturing method according to the present embodiment. The semiconductor package 10 shown in this figure is called a fan-out wafer-level package (Fan-out WLP, FO-WLP). The semiconductor package 10 includes a semiconductor chip 1, a sealing layer 3, a rewiring layer 4, and an electromagnetic shielding layer 5 (functional layer). The package form is not limited to the FO-WLP, and may be a wafer-level package (WLP), a flip-chip chip-scale package (FC-CSP), a flip-chip ball grid array (FC-BGA), a memory package, or the like.
[0015] The shape of the semiconductor package 10 in plan view is, for example, a square or a rectangle. The area of the semiconductor package 10 in plan view is, for example, 1 to 900 mm. 2 9 to 625 mm 2 Or 25~400mm 2 The length of one side of the semiconductor package 10 in a plan view may be, for example, 1 to 30 mm, 3 to 25 mm, or 5 to 20 mm. The thickness of the semiconductor package 10 (excluding the height of the bumps 4c) may be, for example, 100 to 1500 μm, or 200 to 1000 μm.
[0016] The semiconductor chip 1 has a circuit surface 1a and a plurality of bumps 1b (protruding electrodes) formed on the circuit surface 1a. The circuit surface 1a may have relatively flat metal pads such as Ni / Au plated pads. The bumps 1b are, for example, copper bumps and solder bumps. The shape of the semiconductor chip 1 in plan view is, for example, a square or a rectangle. The area of the semiconductor chip 1 in plan view is, for example, 1 to 400 mm 2 9 to 225 mm 2 Or 25~100mm 2 The length of one side of the semiconductor chip 1 in a plan view may be, for example, 1 to 20 mm, 3 to 15 mm, or 5 to 10 mm. The thickness of the semiconductor chip 1 (excluding the height of the bumps 1b) may be, for example, 50 to 775 μm, or 100 to 500 μm.
[0017] The encapsulation layer 3 is made of a thermosetting resin composition. The encapsulation layer 3 protects the semiconductor chip 1 from light, heat, moisture, dust, physical impact, and the like. The encapsulation layer 3 is formed by, for example, compression molding, transfer molding, or lamination of a film-like encapsulant. The thickness of the encapsulation layer 3 is, for example, 50 μm or more, and may be 100 μm or more.
[0018] The rewiring layer 4 is electrically connected to the bump 1b of the semiconductor chip 1. The rewiring layer 4 is composed of a conductor portion 4a, an insulating portion 4b, and bumps 4c and 4d. The conductor portion 4a electrically connects the bump 1b of the semiconductor chip 1 to the bump 4c. The bump 4d shown at the left end of FIG. 1 is electrically connected to the electromagnetic shielding layer 5. The side surface 4f of the rewiring layer 4 has a ground contact point 4g. The ground contact point 4g is in contact with the electromagnetic shielding layer 5. This allows the electromagnetic shielding layer 5 to be grounded. Although one ground contact point 4g is illustrated in FIG. 1, the semiconductor package 10 may have multiple ground contact points on the side surface 4f of the rewiring layer 4.
[0019] The electromagnetic shielding layer 5 covers the surface 3a and the side surface 3b of the sealing layer 3, and also covers at least a part of the side surface 4f of the rewiring layer 4. The electromagnetic shielding layer 5 is a metal layer formed by, for example, sputtering or vapor deposition. The electromagnetic shielding layer 5 contains, for example, a metal element such as copper, chromium, or nickel. The metal element constituting the electromagnetic shielding layer 5 may be one type or two or more types. The thickness of the electromagnetic shielding layer 5 is, for example, 0.01 to 100 μm, and may be 0.05 to 50 μm. The method for forming the electromagnetic shielding layer 5 is not limited to sputtering or vapor deposition, and may be a screen printing method, a spray printing method, an electroless plating method, an electrolytic plating method, or the like.
[0020] (Method of manufacturing semiconductor packages) Next, a description will be given of a method for manufacturing the semiconductor package 10. The semiconductor package 10 can be manufactured, for example, through the following steps. (a) A step of forming a temporary fixing material layer 15 on a first surface 30a of a panel member 30 having a plurality of semiconductor packages 10A (see FIG. 3(a)). (b) A step of attaching an adhesive film 21 (first adhesive film) to the second surface 30b of the panel member 30 (see FIG. 3(b)). (c) A step of singulating the panel member 30 and the temporary fixing material layer 15 on the adhesive film 21 into a plurality of semiconductor packages 25P with temporary fixing material pieces (see FIG. 3(c)). (d) A process of arranging multiple semiconductor packages 25P with temporary fixing material pieces on a support carrier 35 so that the temporary fixing material pieces 15P of the semiconductor packages 25P with temporary fixing material pieces are in contact with the support carrier 35 and the spacing between adjacent semiconductor packages 25P with temporary fixing material pieces is 0.1 mm or more (see Figure 4(b)). (e) A step of peeling off the adhesive film 21 from the support carrier 35 and the semiconductor packages 25P with the plurality of temporary fixing material pieces (see FIG. 4(c)). (f) A process of forming an electromagnetic wave shielding layer 5 by sputtering or vapor deposition on the surface of the semiconductor package 25P with the plurality of temporary fixing material pieces attached, which is exposed by peeling off the adhesive film 21 (see FIG. 5).
[0021] The above-described manufacturing method provides the following effects. In step (d), a plurality of semiconductor packages 25P with temporary fixing material pieces are arranged on the support carrier 35 with the space between two adjacent semiconductor packages 25P with temporary fixing material pieces being expanded, so that in step (f), an electromagnetic wave shielding layer 5 of a desired thickness can be formed on the side surface of the semiconductor package 10P by sputtering or deposition. Note that the semiconductor package 25P with temporary fixing material pieces is composed of the semiconductor package 10P (before the electromagnetic wave shielding layer 5 is formed) and the temporary fixing material pieces 15P. In process (f), an electromagnetic wave shielding layer 5 is formed on the semiconductor package 10P in which the rewiring layer 4 is covered with the temporary fixing material piece 15P, thereby preventing the material constituting the electromagnetic wave shielding layer 5 from flowing around to the surface of the semiconductor package 10 on the rewiring layer 4 side. The first surface 30a of the panel member 30 is the surface on which the rewiring layer 4 is exposed. It can be said that the rewiring layer 4 belongs to the semiconductor package 10A or the panel member 30, or it can be said that the rewiring layer 4 belongs to the semiconductor package 10P or the semiconductor package 10 after they are formed. It can be noted that a part of the circuit surface 1a of the semiconductor chip 1 may be exposed on the first surface 30a of the panel member 30.
[0022] [(a) Process] Step (a) is a step of forming a temporary fixing material layer 15 on a first surface 30a of a panel member 30 including a plurality of semiconductor chips 1 and an encapsulant 13 encapsulating the plurality of semiconductor chips 1. In this embodiment, a case where a fan-out wafer level package (Fan-out WLP, FO-WLP) is used as the panel member 30 is taken as an example. FIG. 2 is a plan view that shows a schematic view of the panel member 30 that is an FO-WLP. The panel member 30 is substantially circular in plan view, and has a diameter of, for example, 100 to 300 mm. The panel member 30 is composed of a plurality of semiconductor chips 1 and an encapsulant 13 that encapsulates the semiconductor chips 1. Although FIG. 2 shows 21 semiconductor chips 1 for convenience, the number of semiconductor chips 1 included in the FO-WLP is, for example, 100 or more, and may be 400 to 6000 or 1600 to 24000.
[0023] FIG. 3(a) is a cross-sectional view showing a schematic state in which the temporary fixing material layer 15 is formed on the first surface 30a of the panel member 30. The temporary fixing material layer 15 is made of a resin composition having adhesion to the panel member 30. The temporary fixing material layer 15 may be formed using a paste of the resin composition, or the resin composition may be formed in advance into a film and attached to the first surface 30a. As shown in FIG. 3(a), it is preferable that the temporary fixing material layer 15 contacts the circuit surface 1a of the panel member 30 and the bumps 1b are embedded in the temporary fixing material layer 15. Since the temporary fixing material layer 15 is in close contact with the circuit surface 1a, it is possible to highly prevent the material constituting the electromagnetic wave shielding layer 5 from getting around to the circuit surface 1a even after the formation of the electromagnetic wave shielding layer 5 in the (F) step.
[0024] [(b) Process] Step (b) is a step of attaching an adhesive film 21 (first adhesive film) to the second surface 30b of the panel member 30 (see FIG. 3(b)). The adhesive film 21 includes a base film 21a and an adhesive layer 21b. The adhesive film 21 is preferably a stretchable film. For example, an expandable film used in stealth dicing or the like can be used as the stretchable film. The adhesive film 21 is used to separate the panel member 30 in step (c) and to expand the interval between adjacent semiconductor packages 25P with temporary fixing material pieces in step (d). The interval after expansion need not necessarily be uniform over the entirety as long as the electromagnetic wave shielding layer 5 is appropriately formed on the side surface of the semiconductor package 10P in step (f). Therefore, instead of an expandable film, an adhesive film having a certain degree of stretchability (for example, a dicing film) may be used as the adhesive film 21.
[0025] [(c) Process] Step (c) is a step of dividing the panel member 30 and the temporary fixing material layer 15 on the adhesive film 21 into a plurality of semiconductor packages 25P with temporary fixing material pieces (see FIG. 3(c)). The separation distance between two adjacent semiconductor packages 25P with temporary fixing material pieces is approximately the same as the blade width used for cutting, for example, about 50 μm.
[0026] [(d) Process] Step (d) is a step of arranging a plurality of semiconductor packages 25P with temporary fixing material pieces on the support carrier 35 so that the temporary fixing material pieces 15P of the semiconductor packages 25P with temporary fixing material pieces are in contact with the support carrier 35 and the interval between adjacent semiconductor packages 25P with temporary fixing material pieces is 0.1 mm or more. In step (d), for example, by carrying out the following steps, it is possible to collectively arrange a plurality of semiconductor packages 25P with temporary fixing material pieces on the adhesive film 21 on the support carrier 35. (d1) By applying tension to the adhesive film 21, the distance between two adjacent semiconductor packages 25P with temporary fixing material pieces is increased (see FIG. 4(a)). (d2) While tension is being applied to the adhesive film 21, the semiconductor packages 25P with the temporary fixing material pieces on the adhesive film 21 are transferred to a support carrier 35.
[0027] The support carrier 35 is made of a material having sufficient heat resistance because it is exposed to sputtering or vapor deposition in the (f) step. The support carrier 35 has a laminated structure including, for example, a heat-resistant base film 35a and an adhesive layer 35b having high adhesion to the temporary fixing material piece 15P. As described above, the base film 35a may be any material having heat resistance, such as a polyimide film, a PET film (stretched), or polyvinylidene chloride. The base film 35a may be a single-layer film, or a multilayer film obtained by combining two or more of the above plastic films or two or more of the same type of plastic films. The adhesive layer 35b may be made of, for example, an adhesive composition, and may exhibit strong adhesion to the temporary fixing material piece 15P when heated.
[0028] The separation distance between two adjacent semiconductor packages 25P with temporary fixing material pieces after expansion is preferably 100 to 2000 μm, and more preferably 200 to 800 μm. When this distance is 2000 μm or less, breakage of the temporary fixing material layer 15 tends to be suppressed. The ratio (D / T) of this distance D to the thickness T of the semiconductor package is preferably 1 or more. When the ratio D / T is 1 or more, an electromagnetic wave shielding layer 5 of a desired thickness can be stably formed on the side surface of the semiconductor package 10P by sputtering or vapor deposition in the (E) step.
[0029] [(e) Process] Step (e) is a step of peeling off the adhesive film 21 from the support carrier 35 and the semiconductor package 25P with the plurality of temporary fixing material pieces. Fig. 4(c) is a cross-sectional view that shows a schematic state in which the adhesive film 21 has been peeled off from the state shown in Fig. 4(b). Note that Fig. 4(c) shows a state in which the state of Fig. 4(b) has been turned upside down. Prior to carrying out step (e), the adhesive strength of the adhesive film 21 may be reduced, for example, by irradiating the adhesive film 21 with ultraviolet light.
[0030] [(f) Process] Step (f) is a step of forming an electromagnetic wave shielding layer 5 by sputtering or vapor deposition on the surface of the semiconductor package 25P with multiple temporary fixing material pieces exposed by peeling off the adhesive film 21. Sputtering can be performed using, for example, CCS-2110 (product name) manufactured by Shibaura Mechatronics Co., Ltd. Vapor deposition can be performed using, for example, AIP-G series (product name, "AIP" is a registered trademark) manufactured by Kobe Steel, Ltd. FIG. 5 is a cross-sectional view that shows a schematic state in which the electromagnetic wave shielding layer 5 is formed on the surface of the semiconductor package 25P with multiple temporary fixing material pieces.
[0031] After step (f), in order to efficiently pick up the semiconductor package 10, the semiconductor package 25P with the temporary fixing material pieces may be transferred from the support carrier 35 to an adhesive film 22 (second adhesive film), and the semiconductor package 10 may be picked up from the adhesive film 22. That is, after step (f), the following steps may be appropriately performed. Note that, as the adhesive film 22, for example, one whose adhesive strength decreases when irradiated with ultraviolet light or heated may be used. (g) and (f) are steps of adhering an adhesive film 22 so as to cover the electromagnetic shielding layer 5 of the semiconductor packages 25P with the temporary fixing material pieces thereon after the steps (see FIG. 6(a)). (h) A step of peeling off the temporary fixing material pieces 15P together with the support carrier 35 from the multiple semiconductor packages 10 on the adhesive film 22 (see FIG. 6(b)). (i) a step of reducing the adhesive strength of the adhesive film 22 to the semiconductor package 10. (j) a step of picking up the semiconductor package 10 from the adhesive film 22.
[0032] Fig. 6(c) is a cross-sectional view that shows a schematic diagram of a state in which the semiconductor package 10 is picked up from the adhesive film 22. As shown in Fig. 6(c), the semiconductor package 10 is pushed up from the lower surface side of the adhesive film 22 by a push-up jig 51, and the semiconductor package 10 is picked up by suction with a collet 52.
[0033] Although the embodiments of the present disclosure have been described in detail above, the present invention is not limited to the above embodiments. For example, in the above embodiments, the case where the electromagnetic shield layer 5 is formed as the functional layer is exemplified, but instead of the electromagnetic shield layer 5, a heat dissipation layer and / or a protective layer may be formed on the surface of the semiconductor package 10P. In addition, in the above embodiments, the case where the adhesive film 21 having extensibility is used in the step (c) and the semiconductor packages 25P with the temporary fixing material pieces are transferred to the support carrier 35 at once in the step (d) is exemplified, but in the step (c), a dicing film with no extensibility or low extensibility may be used and the semiconductor packages 25P with the temporary fixing material pieces after dicing may be picked up one by one and placed on the support carrier 35.
[0034] According to this embodiment, even if the rewiring layer 4 of the semiconductor package 10 is as thin as less than 50 μm, the effect of being able to stably establish a ground connection for the electromagnetic shielding layer 5 is achieved. That is, in the step (f), the electromagnetic shielding layer 5 is also stably formed on the side surface of the rewiring layer 41, and the ground contact point 42 can be provided on the side surface 41f of the rewiring layer 41. The thickness of the rewiring layer 41 may be less than 50 μm, or may be less than 30 μm. The lower limit of the thickness of the rewiring layer 41 is, for example, about 10 μm. EXAMPLES
[0035] The present disclosure will be described in more detail with reference to the following examples, but the present invention is not limited to these examples.
[0036] A panel member for WLP (diameter: 24 mm, thickness: 0.3 mm, number of semiconductor chips: 16, bumps on circuit surface: solder) was prepared. A temporary fixing film having an adhesive layer was attached to the first surface (circuit surface) of the panel member for WLP (step (A)). A stretchable film (a dicing film having stretchability, a first adhesive film) was attached to the second surface (the surface opposite to the circuit surface) of the panel member for WLP (step (B)). By carrying out blade dicing under the following conditions, a semiconductor package with multiple pieces of temporary fixing material (size 6 mm × 6 mm in plan view) was formed on the stretchable film (step (C)). Dicer: DFD3361 (Disco Corporation) Blade: ZH05-SD3000-N1-70 (Disco Corporation) Blade width: 28μm Blade rotation speed: 30000 rpm Dicing speed: 10mm / sec
[0037] A ring having an inner diameter larger than the diameter of the WLP panel member was pressed against the stretchable film from below, thereby applying tension to the stretchable film (step (d1)). This expanded the distance between two adjacent semiconductor packages with temporary fixing material pieces to approximately 320 μm. With tension applied to the stretchable film, a support carrier was attached using a vacuum laminator so as to cover the multiple temporary fixing material pieces, and the semiconductor packages with the multiple temporary fixing material pieces were transferred to the support carrier (step (d1)). A polyimide film having an ultraviolet-curing adhesive layer on its surface was used as the support carrier. The stretchable film was then peeled off from the semiconductor packages with the multiple temporary fixing material pieces (step (E)).
[0038] An electromagnetic wave shielding layer (thickness: 4380 nm) was formed by sputtering on the surface of the semiconductor package with multiple temporary fixing material pieces on the polyimide film (step (F)). Chromium and copper were used as targets.
[0039] When the circuit surface of the semiconductor package was observed under magnification, no leakage of the material constituting the electromagnetic shielding layer onto the circuit surface was observed. [Industrial Applicability]
[0040] According to the present disclosure, there is provided a method for efficiently manufacturing a semiconductor package having at least a portion of a surface covered with a functional layer. [Explanation of symbols]
[0041] 1...semiconductor chip, 1a...circuit surface, 1b...bump, 3...sealing layer, 3a...surface, 3b...side, 4...rewiring layer, 4a...conductor portion, 4b...insulating portion, 4c, 4d...bump, 4f...side, 4g...ground contact point, 5...electromagnetic wave shielding layer (functional layer), 10...semiconductor package, 10A...semiconductor package (before individualization), 10P...semiconductor package (before functional layer formation), 13...sealing material, 15...temporary fixing material layer, 15P...temporary fixing material piece, 21...adhesive film (first adhesive film), 21a...base film, 21b...adhesive layer, 22...adhesive film (second adhesive film), 25P...semiconductor package, 30...panel member, 30a...first surface, 30b...second surface, 35...support carrier, 35a...base film, 35b...adhesive layer, 51...jig, 52...collet
Claims
1. (A) forming a temporary fixing material layer on a first surface of a panel member having a plurality of semiconductor packages, the first surface being an exposed surface of the circuit surfaces or rewiring layers of the plurality of semiconductor packages; (B) attaching a first adhesive film to a second surface of the panel member; (C) dividing the panel member and the temporary fixing material layer on the first adhesive film into a plurality of semiconductor packages with temporary fixing material pieces; (D) arranging a plurality of the semiconductor packages with the temporary fixing material pieces on the support carrier such that the temporary fixing material pieces of the semiconductor packages with the temporary fixing material pieces are in contact with the support carrier and the interval between adjacent semiconductor packages with the temporary fixing material pieces is 0.1 mm or more; (E) peeling the first adhesive film from the support carrier and the semiconductor packages with the temporary fixing material pieces; (F) forming a functional layer on the surfaces of the semiconductor packages with the temporary fixing material pieces exposed by peeling off the first adhesive film; (G) attaching a second adhesive film to cover the functional layer formed on the surface of the semiconductor package with the plurality of temporary fixing material pieces; (H) peeling off the temporary fixing material pieces from the plurality of semiconductor packages on the second adhesive film together with the support carrier; A method for manufacturing a semiconductor package, comprising:
2. The first adhesive film has extensibility, 2. The method for manufacturing a semiconductor package according to claim 1, wherein the step (D) includes: (d1) applying tension to the first adhesive film to expand the distance between two adjacent semiconductor packages with the temporary fixing material pieces; and (d2) transferring the semiconductor packages with the temporary fixing material pieces on the first adhesive film to the support carrier while applying tension to the first adhesive film.
3. The method for manufacturing a semiconductor package according to claim 1 , wherein the functional layer is a metal layer formed by sputtering or vapor deposition.
4. The circuit surface or the rewiring layer has a plurality of bumps provided on a surface of the circuit surface or the rewiring layer, 4. The method for manufacturing a semiconductor package according to claim 1, wherein in step (A), the plurality of bumps are embedded in the temporary fixing material layer.
5. The method for manufacturing a semiconductor package according to any one of claims 1 to 4, wherein the functional layer is an electromagnetic wave shielding layer.
6. The method of claim 5 , wherein the semiconductor package has a redistribution layer less than 50 μm thick and a ground contact point provided on a side of the redistribution layer.
Citation Information
Patent Citations
Method for taking out semiconductor chip
JP2000164682A
Adhesive film for semiconductor device and semiconductor device
JP2012124466A
Electronic component module and manufacturing method for the same
JP2015195398A
Semiconductor package manufacturing method
JP2017208529A
Semiconductor package and forming method thereof
JP2019009371A