Thin tube welding method
The method addresses gaps and positioning issues in thin tube welding by using a washer with a matching hole and inward caulking, resulting in a compact, interference-free welded joint.
Patent Information
- Application Number
- JP2020157020
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-18
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2040-09-18
AI Technical Summary
Conventional thin tube welding methods result in gaps due to large dimensional tolerances, leading to potential penetration into the inner diameter and difficulty in precise positioning, affecting the shape of connected pressure equipment.
A method involving a washer with a through hole matching the thin tube's outer diameter, where the washer is caulked inward to ensure close contact, followed by laser welding to form a compact welded joint without protrusion.
The method ensures a gap-free, compact welded joint, improving mechanical strength, assembly efficiency, and preventing interference with connected equipment.
Smart Images

Figure 0007582824000001 
Figure 0007582824000002 
Figure 0007582824000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a welded structure and method for a thin tube, in which a thin tube is passed through a through hole and welded to the wall of the through hole. [Background technology]
[0002] A technique for passing a thin tube through a through hole and welding it to the wall of the through hole is described in, for example, Patent Document 1. Patent Document 1 discloses an apparatus for connecting two pressure vessels with a thin tube and transmitting pressure from one pressure vessel to the other pressure vessel through the thin tube. The thin tube is connected to the pressure vessel via a connecting part (hereinafter, this part is simply referred to as a "washer"). The thin tube and washer are explained with reference to Figs. 10(A) and (B). Fig. 10(A) is a cross-sectional view of the thin tube and washer during welding, and Fig. 10(B) is a cross-sectional view of the thin tube and washer after welding. As shown in Fig. 10(A), the thin tube 1 is passed through the through hole 3 of the washer 2 and is welded to the tip of the washer 2 by laser welding. In Fig. 10(A), the two-dot chain line L indicates the laser light during welding.
[0003] The thin tube 1 has a large dimensional tolerance with respect to the diameter. For example, a thin tube designated as 30G in the standard designation of the thin tube 1 has a tolerance of φ0.31±0.02. Therefore, when welding the thin tube 1 to the washer 2, a gap of the tolerance may occur between the thin tube 1 and the wall surface of the through hole 3. This gap varies between a maximum of −0.02 mm and +0.02 mm. In other words, the maximum width of the gap is 0.04 mm. The thin tube 1 has been welded so as to fill this gap. For this reason, as shown in FIG. 10(B), a welding method has been adopted in which the amount of melting of the base material (washer 2) is increased to fill the gap. In FIG. 10(B), the welded portion 4 is formed so as to extend over substantially the entire area of the small diameter portion 2a of the washer 2. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 6559584 Summary of the Invention [Problem to be solved by the invention]
[0005] In the conventional welding structure and welding method described above, a large amount of melt is produced during welding, and there is a risk that the melt may penetrate to the inner diameter side of the thin tube 1. When the thickness of the thin tube 1 becomes thin, this problem becomes more noticeable. Another problem is that it is not possible to precisely determine the relative positions of the thin tube 1 and the washer 2. The reason for this is that a large amount of melt is produced during welding, so welding must be performed with the thin tube 1 protruding significantly from the washer 2. If the thin tube 1 protrudes significantly from the washer 2, this will affect the shape of the pressure equipment to which it is connected. In other words, a large hole must be drilled in the pressure equipment to avoid interference with the protruding part of the thin tube 1. For this reason, there is a demand to form the welded part compactly so that the thin tube 1 does not protrude.
[0006] An object of the present invention is to provide a welded structure for a thin tube and a welding method for a thin tube in which no gap occurs between the thin tube and a washer and the welded part is compact. [Means for solving the problem]
[0007] In order to achieve this objective, the welding structure for a thin tube of the present invention is a welding structure in which a metal thin tube is inserted into a through hole of a washer having a through hole with a hole diameter corresponding to the outer diameter of the thin tube, and the thin tube is welded to the washer, and with the thin tube inserted into the through hole of the washer, the thin tube is pressed toward the inside of the washer by a crimping process from the outer surface of one end of the washer, bringing the outer circumference of the thin tube and the inner circumference of the through hole into a tight contact state, and then the thin tube is welded and fixed by laser welding around the abutment area between the thin tube and the opening of the through hole on the one end of the washer.
[0008] In the present invention, in the welded structure of the thin tube, the washer may be a columnar member extending along the through hole, and the columnar member may have an outer diameter of an outer surface pressed by the crimping process that is smaller than the outer diameter of the other outer surfaces.
[0009] In the present invention, in the welded structure, one end of the welded thin tube does not need to protrude from an end face on one end side of the washer.
[0010] The method for welding a thin tube according to the present invention is a method for welding a thin tube made of metal to a washer while the thin tube is inserted into a through hole of the washer having a through hole with a hole diameter corresponding to the outer diameter of the thin tube, the method comprising: a first step of inserting the thin tube into the through hole of the washer; a second step of pressing the outer surface of one end of the washer toward the inside of the washer with a crimping tool to bring the outer circumference of the thin tube into tight contact with the inner circumference of the through hole; and a third step of welding and fixing the periphery of the contact portion between the thin tube and the opening of the through hole on the one end of the washer by laser welding after the second step.
[0011] The present invention may be directed to a method for welding a thin tube, in which in the first step or the second step, the thin tube is positioned so that one end of the thin tube does not protrude from an end face on one end side of the washer. Effect of the Invention
[0012] According to the present invention, it is possible to provide a welded structure for a thin tube and a welding method for a thin tube in which no gap occurs between the thin tube and the washer and the welded part is compact. [Brief description of the drawings]
[0013] [Figure 1] FIG. 1 is a cross-sectional view of a thin tube and a washer used in a welded structure of a thin tube according to the present invention. [Diagram 2] FIG. 2 is an enlarged cross-sectional view showing a main part of the welded structure of a thin tube according to the present invention. [Diagram 3] FIG. 3 is a schematic diagram showing the configuration of a crimping tool. [Figure 4] FIG. 4 is a plan view showing the configuration of the crimping deformation member. [Diagram 5] FIG. 5 is a plan view showing a specific example of a crimping tool. [Figure 6] FIG. 6 is a cross-sectional view taken along line VI-VI in FIG. [Figure 7] FIG. 7 is a flow chart showing a method for welding thin tubes according to the present invention. [Figure 8] FIG. 8 is an enlarged cross-sectional view of a part of the crimping tool. [Figure 9] FIG. 9 is an enlarged cross-sectional view of a part of the crimping tool. [Figure 10] FIG. 10 is a cross-sectional view showing a conventional welding structure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] BEST MODE FOR CARRYING OUT THE DISCLOSURE Hereinafter, an embodiment of a welded structure and a welded method for a thin tube according to the present invention will be described in detail with reference to Figs. The thin tube 11 shown in Fig. 1 is for conducting pressure to a pressure sensor (not shown), and is used by being welded to a washer 13 by a welding structure 12 (see Fig. 2) according to the present invention. The material forming the thin tube 11 and the washer 13 is metal. The washer 13 is a columnar member having a through hole 14 through which the thin tube 11 is inserted. The diameter of the through hole 14 corresponds to the outer diameter of the thin tube 11.
[0015] Since there is a tolerance in the outer diameter of the thin tube 11, a gap indicated by the symbol d in Fig. 1 may occur between the thin tube 11 and the washer 13. Fig. 1 is drawn in a state where the maximum gap d occurs between the thin tube 11 and the through hole 14. The washer 13 according to this embodiment is formed in a thin cylindrical shape with the through hole 14 located at the axial center, and has a large diameter portion 13a from which the thin tube 11 protrudes, and a small diameter portion 13c connected to the large diameter portion 13a via a tapered portion 13b. The tapered portion 13b is formed so that the outer diameter gradually decreases from the large diameter portion 13a toward the small diameter portion 13c, and is welded, for example by resistance welding, to the opening edge of a connection port formed in a pressure vessel (not shown) so that the opening shape is circular.
[0016] As shown in Fig. 2, the welded structure 12 for welding the thin tube 11 to the washer 13 is composed of a crimped portion 12a formed by crimping the small diameter portion 13c of the washer 13, and a welded portion 12b for welding the tip of the thin tube 11 to the tip of the washer 13. The crimping is performed by pressing the outer surface (small diameter portion 13c) of one end side of the washer 13 toward the inside of the washer 13 with the thin tube 11 inserted into the through hole 14 of the washer 13. This crimping is performed using a crimping tool 15 (see Fig. 3) described later, and is performed so that the outer periphery of the thin tube 11 and the inner periphery of the through hole 14 are in close contact with each other.
[0017] The welded portion 12b is formed by laser welding and fixing the periphery of the contact portion between the thin tube 11 and the opening of the through hole 14 on one end side (the small diameter portion 13c side) of the washer 13. As shown in Fig. 2, one end of the thin tube 11 welded to the washer 13 by the welding structure 12 according to this embodiment does not protrude from the end face on the one end side of the washer 13.
[0018] The crimping tool 15 is configured as shown in Figures 3 to 6. Figures 3 and 4 show the configuration of the main parts of the crimping tool 15, and Figures 5 and 6 show a specific example of the crimping tool 15. As shown in Figure 3, the crimping tool 15 can be configured using a fixed guide member 21 depicted at the bottom in Figure 3, a crimping deformation member 22 superimposed on the fixed guide member 21, and a movable pressing member 23 superimposed on the crimping deformation member 22.
[0019] The fixed guide member 21 has a recess 24 capable of accommodating a crimping deformation member 22 described later, and is fixed onto a support surface 25a of a support table 25 (see Figs. 5 and 6) as shown in Figs. 5 and 6. The support table 25 is formed in a plate shape and fixed to a base (not shown), and supports a washer 13 as a workpiece from one direction (from below in Fig. 6) in cooperation with the fixed guide member 21 and the crimping deformation member 22.
[0020] The recess 24 of the fixed guide member 21 has a first inclined surface 24a and a second inclined surface 24b that are inclined so as to gradually approach each other as they proceed downward in Fig. 3, and opens toward the movable pressing member 23. The first inclined surface 24a and the second inclined surface 24b support the crimped deformation member 22 and restrict movement in the left-right direction and downward in Fig. 3. That is, the fixed guide member 21 restricts movement of the crimped deformation member 22 in directions other than one direction (upward in Fig. 3) on the support surface 25a of the support table 25 by abutting its own inner wall surface (first and second inclined surfaces 24a, 24b) against the crimped deformation member 22.
[0021] The crimping deformation member 22 is formed in a disk shape, and is in contact with a first inclined surface 24a and a second inclined surface 24b of the fixed guide member 21 and a movable pressing member 23 described below when placed on a support surface 25a of a support table 25. The crimping deformation member 22 has a space 31 in its center, as well as one open groove 32 and two closed grooves 33, 34 extending radially from the space 31, as shown in Fig. 4.
[0022] The space 31 has a circular opening so as to accommodate the small diameter portion 13c of the washer 13. The space 31 opens to the bottom of a circular recess 35 (see Figs. 5 and 6) formed in the center of the crimping deformation member 22 on the opposite side to the support table 25. The large diameter portion 13a and tapered portion 13b of the washer 13 are accommodated in the circular recess 35. The inner diameter of the largest diameter portion of the circular recess 35 is larger than the outer diameter of the large diameter portion 13a of the washer 13.
[0023] The open groove 32 extends from a space 31 in the center of the crimped deformation member 22 to the outer circumferential end. The open groove 32 in this embodiment is composed of a narrow portion 32a extending from the space 31 to the outside in the radial direction of the crimped deformation member 22, and a wide portion 32b extending from the outer circumferential end of the crimped deformation member 22 to the inside in the radial direction. When the crimped deformation member 22 is assembled to the fixed guide member 21, the crimped deformation member 22 is positioned so that the open end of the open groove 32 does not come into contact with the fixed guide member 21 and the movable pressing member 23, as shown in FIG. The two closed grooves 33, 34 are formed so as to extend from the space 31 in the center of the crimp deformation member 22 toward the outer circumferential end but not to the outer circumferential end. That is, the two closed grooves 33, 34 are composed of narrow width portions 33a, 34a extending from the space 31 to the outside in the radial direction of the crimp deformation member 22 and circular holes 33b, 34b provided in the outer circumferential portion of the crimp deformation member 22, radially inward from the outer circumferential end.
[0024] The three grooves consisting of the one open groove 32 and the two closed grooves 33, 34 are provided at positions that divide the crimp deformation member 22 into thirds in the circumferential direction. In this embodiment, the positions of the three grooves are set so that the open end of the open groove 32 does not come into contact with the first and second inclined surfaces 24a, 24b of the fixed guide member 21 and the movable pressing member 23 described below. By forming the three grooves in the crimp deformation member 22 in this manner, first to third claws 36-38 are formed in the crimp deformation member 22, surrounding the space portion 31 from three directions, as shown in FIG.
[0025] Therefore, the shape of the crimping deformation member 22 is a shape that imitates the shape of a so-called three-jaw chuck. In this case, the first to third jaws 36-38 are not completely separated but are connected by a thin-walled portion 39. The thin-walled portion 39 is provided at two locations between the two closing grooves 33, 34 of the crimping deformation member 22 and the outer circumferential end of the crimping deformation member 22. The crimping tool 15 according to this embodiment, which will be described in detail later, is configured to perform pressing by elastically deforming the thin-walled portion 39 to operate the first to third jaws 36-38 as if they were separated.
[0026] The moving pressing member 23 is supported on the support surface 25a of the support table 25 via a guide member (not shown) so as to be movable in parallel, and is connected to a pressing device (not shown). The direction in which the moving pressing member 23 moves in parallel with the support table 25 is the direction in which it approaches and separates from the fixed guide member 21 and the crimping deformation member 22 (the vertical direction in FIG. 3). The pressing device presses the moving pressing member 23 with a predetermined load in a direction approaching the fixed guide member 21 and the crimping deformation member 22 when performing the crimping process, and moves the moving pressing member 23 in the opposite direction after the crimping process. That is, the moving pressing member 23 abuts against and presses the crimping deformation member 22 with its own inner wall surface 23a from one direction on the support surface 25a of the support table 25 (from above in FIG. 3).
[0027] The inner wall surface 23a and the first and second inclined surfaces 24a, 24b are configured to form an angle of 60 degrees with each other. That is, as shown in Fig. 3, the angles θ1, θ2 between the bottom surface 24c of the recess 24, which is parallel to the inner wall surface 23a of the moving pressing member 23, and the first and second inclined surfaces 24a, 24b are each 60 degrees. In this way, by fixing two of the three walls (the first and second inclined surfaces 24a, 24b) and moving the other one (the inner wall surface 23a of the moving pressing member 23), it is possible to generate uniform forces in the first to third claws 36-38 of the crimping deformation member 22.
[0028] 6, the crimping tool 15 according to this embodiment includes a guide cover member 41 that cooperates with the crimping deformation member 22 to clamp the washer 13. The guide cover member 41 abuts against the fixed guide member 21 and the washer 13 from the side opposite to the support surface 25a of the support table 25 to hold the washer 13. The guide cover member 41 is also formed with a guide hole 41a that guides the thin tube 11 extending from the washer 13 to the side opposite to the support table 25.
[0029] Next, a description will be given of a welding method for realizing the above-mentioned welded structure 12. This welding method is performed by first to third steps S1 to S3, as shown in the flow chart of Fig. 7. In the first step S1, the thin tube 11 is inserted into the through hole 14 of the washer 13, as shown in Fig. 1. In the second step S2, the capillary tube 11 and the washer 13 are loaded into the crimping tool 15 and crimped. That is, the capillary tube 11 and the washer 13 are inserted into the space 31 of the crimping deformation member 22, and the tips of the capillary tube 11 and the washer 13 are abutted against the support table 25 as shown in FIG. 6. By abutting the capillary tube 11 and the washer 13 against the support table 25 in this manner, the capillary tube 11 is positioned so that one end of the capillary tube 11 does not protrude from the end face on one end side of the washer 13. This positioning can also be performed in the first step S1 described above. By inserting the washer 13 into the space 31, the washer 13 comes into contact with the first to third claws 36 to 38 as shown in FIG. 8.
[0030] Next, the movable pressing member 23 presses the crimped deformation member 22 against the first and second inclined surfaces 24a, 24b with a predetermined load. That is, the crimped deformation member 22 is pressed toward the inside of the washer 13 from the outer surface of one end side of the washer 13 by the crimping tool 15. This pressing elastically deforms the two closed grooves 33, 34 of the crimped deformation member 22 and the two thin-walled portions 39 between the outer peripheral end of the crimped deformation member 22, and the first to third claws 36-38 formed by the three grooves are displaced toward the center of the crimped deformation member 22 from the initial position shown in FIG. 8 to the crimped position shown in FIG. 9. In this way, the crimped deformation member 22 is subjected to an external force, and the space 31 is variably narrowed.
[0031] As a result, as shown in FIG. 9, the small diameter portion 13c of the washer 13 is plastically deformed, and the outer circumference of the thin tube 11 and the inner circumference of the through hole 14 are brought into close contact with each other. After performing the second step S2 in which the crimping process is performed in this manner, the assembly consisting of the thin tube 11 and the washer 13 is removed from the crimping tool 15 and attached to a welding device (not shown) to perform the third step S3. In the third step S3, the periphery of the abutment portion between the thin tube 11 and the opening of the through hole 14 on one end side of the washer 13 is welded and fixed by laser welding. The laser welding can be performed by irradiating a laser beam toward the end faces of the washer 13 and the thin tube 11. After welding, a welded portion 12b is formed at the abutment portion between the thin tube 11 and the opening of the through hole 14 as shown in FIG. 2. This welded portion 12b does not protrude from the end face of the washer 13. Therefore, according to this embodiment, it is possible to provide a welded structure and a welding method for a thin tube in which no gap occurs between the thin tube 11 and the washer 13 and the welded portion 12b is compact.
[0032] The washer 13 according to this embodiment is a columnar member extending along the through hole 14. The outer diameter of the outer surface (small diameter portion 13c) of this columnar member that is pressed by the crimping process is smaller than the outer diameter of the other outer surface (large diameter portion 13a). Therefore, the load when performing the crimping process can be reduced, and the crimping tool 15 can be made smaller. In addition, in this embodiment, the one end of the welded thin tube 11 does not protrude from the end face on one end side of the washer 13. Therefore, a further compact welded portion 12b is obtained.
[0033] The method for welding thin tube 11 according to this embodiment includes a first step S1 of inserting thin tube 11 into through hole 14 of washer 13, a second step S2 of using a crimping tool 15 to bring the outer periphery of thin tube 11 into intimate contact with the inner periphery of through hole 14, and a third step S3 of laser welding and fixing the periphery of the contact portion between thin tube 11 and the opening of through hole 14. Therefore, welding can be performed in a state in which thin tube 11 is fixed to washer 13 by crimping, making welding easy and reliable.
[0034] According to the method for welding the thin tube 11 according to this embodiment, the thin tube 11 is positioned in the first step S1 or the second step S2 so that the thin tube 11 does not protrude from the end face of the washer 13. Therefore, the position of the thin tube 11 can be adjusted before the crimping process is performed, so that the crimping process can be performed accurately.
[0035] As shown in this embodiment, by carrying out welding after the crimping process, temporary fixing can be achieved at the crimped portion, which has the following advantages. (1) The thin tube 11 and the washer 13 are in close contact with each other, so that melting and separation are unlikely to occur. (2) Ease of assembly can be improved. That is, when the thin tube 11 is inserted into the through hole 14 of the washer 13, if it is not fixed properly, it will shift during welding work, so some kind of fixation with a jig or tool is necessary. By crimping, it can be fixed by frictional force, so fixing with a jig or tool is not necessary, improving workability. (3) Improved mechanical strength. In other words, if there is no crimped portion, when an external force is applied to the thin tube after welding, only the welded portion must bear the external force. On the other hand, when crimping is performed, frictional force acts on the crimped portion, which enhances the mechanical strength of the welded portion, resulting in a sturdy and durable structure.
[0036] In the above-described embodiment, an example has been shown in which the crimping tool 15 having the crimping deformation member 22 is used to crimp the washer 13. However, the present invention is not limited to such a limitation, and the crimping process can also be performed using a device such as a collet chuck that applies pressure from the outside to narrow the outer diameter. [Explanation of symbols]
[0037] 1...thin tube, 12...welded structure, 13...washer, 13a...large diameter portion (other outer surface), 13c...small diameter portion (outer surface pressed by crimping process), 14...through hole, S1...first step, S2...second step, 15...crimping tool, S3...third step.
Claims
1. A method for welding a metal thin tube to a washer having a through hole with a hole diameter corresponding to an outer diameter of the thin tube, the method comprising the steps of: a first step of inserting the thin tube into the through hole of the washer; a second step of pressing the outer surface of the washer toward the inside of the washer with a crimping tool to bring the outer periphery of the capillary tube and the inner periphery of the through hole into tight contact with each other; a third step of welding and fixing the periphery of a contact portion between the thin tube and an opening of the through hole on one end side of the washer by laser welding after the second step, The second step is performed by using a disk-shaped crimping deformation member having a circular space in which the washer is housed, the space being open at the center, and having three claws separated by three grooves extending radially from the space, and by pressing the crimping deformation member radially inward with the washer inserted into the space, A method for welding thin tubes, characterized in that the crimping deformation member is pressed radially inward, causing a thin-walled portion between the groove and the outer peripheral end of the crimping deformation member to elastically deform, and the three claws to be displaced toward the center of the crimping deformation member.
2. The method for welding thin tubes according to claim 1, A method for welding thin tubes, characterized in that in the first step or the second step, the thin tube is positioned so that one end of the thin tube does not protrude from an end face on one end side of the washer.
Citation Information
Patent Citations
Caulking device
JP1983107230U
Join of joint and thin-thickness fine pipe
JP1990236083A
Nonaqueous solvent battery
JP1993006769A
Method for joining metal pipe