Optoelectronic semiconductor device and method for manufacturing the same

The etching process for creating faceted surfaces in optoelectronic semiconductor devices addresses manufacturing reliability and complexity issues, enabling reliable, efficient production of semiconductor laser diodes with improved optical properties and design flexibility.

JP7583899B2Active Publication Date: 2024-11-14AMS OSRAM INT GMBH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023197301
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-05-11
Filing Date
2023-11-21
Publication Date
2024-11-14
Estimated Expiration
2039-05-10

AI Technical Summary

Technical Problem

Existing optoelectronic semiconductor devices face challenges in manufacturing reliability and complexity due to the limitations of the scribe-break process, which results in high surface roughness, premature component failure, and limited design flexibility.

Method used

The use of an etching process to create faceted surfaces in the semiconductor device, allowing for low surface roughness, improved plane parallelism, and the ability to produce devices with smaller dimensions, along with the integration of DBR and DFB mirrors directly into the semiconductor body.

Benefits of technology

This approach enhances device reliability, reduces manufacturing complexity, and enables the production of semiconductor laser diodes with narrow band emission spectra and improved optical reflectivity, while allowing for more design flexibility and efficient processing of wafer composites.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007583899000003
    Figure 0007583899000003
  • Figure 0007583899000004
    Figure 0007583899000004
  • Figure 0007583899000005
    Figure 0007583899000005
Patent Text Reader

Abstract

To provide an optoelectronic semiconductor device with improved reliability.SOLUTION: A first region (101), an active region (103) and a second region (102) are arranged along a stacking direction (Y). The active region (103) extends from a rear surface (30) opposite to a coupling-out surface (20) to the coupling-out surface (20) along a longitudinal direction (X) transverse to or perpendicular to the stacking direction (Y). The coupling-out surface (20) is arranged plane-parallel to the rear surface (30). The coupling-out surface (20) and the rear surface (30) of the semiconductor body (10) are produced by an etching process.SELECTED DRAWING: Figure 7A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Optoelectronic semiconductor devices and methods for manufacturing optoelectronic semiconductor devices are disclosed. The optoelectronic semiconductor devices may be radiation-emitting optoelectronic semiconductor devices that emit electromagnetic radiation (such as light) during operation. Summary of the Invention [Problem to be solved by the invention]

[0002] One problem to be solved is to disclose optoelectronic semiconductor devices having improved reliability.

[0003] A further problem to be solved is to disclose a method for producing an optoelectronic semiconductor device, which allows for simplified manufacturing. [Means for solving the problem]

[0004] According to at least one embodiment of the optoelectronic semiconductor device, the optoelectronic semiconductor device comprises a semiconductor body with a first region of a first conductivity type, an active region designed to generate electromagnetic radiation and a second region of a second conductivity type along the deposition direction. Furthermore, the semiconductor body has an extraction surface intended to extract the electromagnetic radiation generated during operation. This extraction surface extends, for example, transversely or perpendicularly to the longitudinal direction.

[0005] The active region extends from a back surface opposite the extraction surface along a longitudinal direction transverse to or perpendicular to the deposition direction to the extraction surface, and preferably comprises a pn junction, a double heterostructure, a single quantum well (SQW) or, particularly preferably, a multiple quantum well (MQW) for generating radiation.

[0006] These regions of the semiconductor body are preferably epitaxially grown. The first and second regions of the semiconductor body each have a different conductivity type. The conductivity types are preferably formed by doping the semiconductor material. The p-type conductivity is preferably formed, for example, by doping with an acceptor material. The n-type conductivity is preferably formed, for example, by doping with a donor material.

[0007] The extraction surface is in particular arranged plane-parallel to the rear surface.

[0008] According to at least one embodiment of the optoelectronic semiconductor device, both the extraction side and the back side of the semiconductor body are produced by an etching process.

[0009] The shape that the extraction surface and the back surface of the semiconductor body follow when produced by the etching process is not a pure shape due to the method, but is visible in the finished component and therefore also the target shape. Surface features produced by the etching process are in particular unevenness on the surface of the extraction surface and / or the back surface depending on the material composition, due to slightly different etching rates in different materials, and / or steps on the surface of the back surface and the extraction surface. A further feature of the etching process is a distance of less than 300 μm between the extraction surface and the back surface. Such a small distance between the extraction surface and the back surface can hardly be produced by a scribing and breaking process at present.

[0010] These features are produced by at least one etching of the semiconductor body and are visible in the finished semiconductor device, for example by electron microscope imaging or under an optical microscope.

[0011] According to at least one embodiment of the optoelectronic semiconductor device, the optoelectronic semiconductor device comprises a semiconductor body with a first region of a first conductivity type, an active region designed to generate electromagnetic radiation, and a second region of a second conductivity type, and the optoelectronic semiconductor device has an extraction surface provided for extracting the electromagnetic radiation, the first region, the active region, and the second region are arranged along a deposition direction; the active area extends from a back surface opposite the extraction surface along a longitudinal direction extending transversely or perpendicularly to the deposition direction to the extraction surface, - The ejection surface is arranged parallel to the back surface, The extraction side and the rear side of the semiconductor body are produced by an etching process.

[0012] The optoelectronic semiconductor device described herein is based, inter alia, on the following considerations: In the manufacture of edge-emitting semiconductor laser diodes, it is particularly necessary that the extraction face and the back face (facet) are as plane-parallel as possible to each other, smooth and produced by a suitable method. High surface roughness reduces the reflectivity and may even lead to premature failure of the component. Surface defects may cause optical damage (COD) of the facet, resulting in complete failure of the component.

[0013] To produce suitable facets, a scribe-and-break process can be used. The break axis is selected along the crystal plane of the semiconductor. This results in a smooth break line along the selected crystal axis, which ensures surface parallelism and reduces the surface roughness to only a few nanometers. However, the disadvantage of the scribe-and-break process is the high rate of defective parts due to facets that were not broken smoothly and are immediately separated into individual semiconductor laser diodes. As a result, it is no longer possible to carry out further processes on the facets of the parts produced in the composite (especially the wafer composite). Instead, each semiconductor device must be processed individually or several parts must be combined into a group by additional processes, processed together, and then separated from each other again.

[0014] In addition, when separated by a scribe-and-break process, the minimum length of the semiconductor laser diode is limited to a relatively large value because the force required for the breaking process increases sharply as the length decreases.

[0015] Furthermore, the use of scribe-and-break processes is limited to the use of breakable substrates, which further restricts the freedom in the design of optoelectronic semiconductor devices.

[0016] The optoelectronic semiconductor devices described herein specifically utilize the concept of using an etching process instead of a scribe-and-break process to create facet surfaces. This allows the facets to be created in a wafer composite. A chemical polishing process is used to ensure low surface roughness and high surface parallelism of the facets.

[0017] According to at least one embodiment of the optoelectronic semiconductor device, the optoelectronic semiconductor device is designed to generate coherent radiation. In other words, the optoelectronic semiconductor device can be an edge-emitting semiconductor laser diode that emits laser radiation during operation. The extraction surface and the back surface of the semiconductor body serve as laser facets and correspond to the resonator mirrors of the semiconductor laser diode.

[0018] According to at least one embodiment of the optoelectronic semiconductor device, the semiconductor body has an extension in the longitudinal direction of less than 300 μm, preferably less than 100 μm, particularly preferably less than 50 μm. The minimum length of the semiconductor body in the longitudinal direction is limited by the minimum length in the scribe-and-break process. By using an etching process, this limitation no longer applies. Semiconductor laser diodes with an extension of less than 300 μm can advantageously have a low gain.

[0019] According to at least one embodiment of the optoelectronic semiconductor device, at least one region of the semiconductor body (in particular the entire semiconductor body) is in a nitride compound semiconductor material system. In this context, "in a nitride compound semiconductor material system" means that the semiconductor body, or at least a part of it, is made of Al n Ga m In 1-n-m N (0≦n≦1, 0≦m≦1, n+m≦1). The material does not necessarily have to have a mathematically exact composition according to the above chemical formula. Rather, the material may include, for example, one or more dopants and additional components. However, for simplicity of explanation, the above formula includes only the essential components of the crystal lattice (Al, Ga, In, N), some of which may be replaced and / or supplemented by small amounts of other substances.

[0020] A p-type conductivity in the first region of the semiconductor body is achieved by doping with a material such as magnesium, while an n-type conductivity in the second region of the semiconductor body is achieved by doping with a material such as silicon.

[0021] According to at least one embodiment of the optoelectronic semiconductor device, the extraction surface and the back surface run parallel to an m-plane of the crystal of the semiconductor body. The m-plane is a plane of a crystal having a hexagonal basic structure of the wurtzite type.

number

[0022] According to at least one embodiment of the optoelectronic semiconductor device, the optoelectronic semiconductor device comprises a growth substrate on which the semiconductor body is deposited, the growth substrate being made of one of the following materials: sapphire, gallium nitride, silicon carbide, silicon. Gallium nitride and silicon carbide can also be used in a scribe-and-break process and have a lower defect density than sapphire. Sapphire and silicon are difficult or impossible to process in a scribe-and-break process. The use of an etching process therefore advantageously allows greater freedom in the design of the optoelectronic semiconductor device.

[0023] According to at least one embodiment of the optoelectronic semiconductor device, the extraction face and the back face have an average roughness in the range of 0.1 nm to 10 nm, preferably in the range of 0.1 nm to 1 nm. The average roughness is defined as the average distance from a measurement point on the surface to the imaginary center line of the surface contour. For a high reflectivity of the extraction face and the back face, a low average roughness is advantageous. A high optical reflectivity is particularly advantageous for forming laser facets. With a view to achieving low values ​​of average roughness, chemical polishing of the extraction face and the back face is advantageous. In particular, the use of TMAH (tetramethylammonium hydroxide) as an etchant in the chemical polishing step results in advantageously low roughness values.

[0024] According to at least one embodiment of the optoelectronic semiconductor device, a mirror is arranged downstream of the back surface and / or the extraction surface, facing away from the semiconductor body. This mirror can be designed, for example, as a DBR mirror (distributed Bragg reflector). This mirror comprises a periodic sequence of several layers with varying refractive index. DBR mirrors are characterized in particular by a high reflectivity in a spectrally very small wavelength range. This makes it possible to produce semiconductor laser diodes with very narrow emission spectra. The DBR mirror can be in direct contact with the semiconductor body and is generated in the semiconductor body. In other words, the DBR mirror is produced by structuring the semiconductor body. A number of groove-shaped recesses arranged one behind the other form a periodic sequence of varying refractive index in a cross section at the transition between the material of the semiconductor body and the recesses.

[0025] Furthermore, the semiconductor body may include a DFB mirror (distributed feedback), which comprises a periodic arrangement of refractive index variations along an imaginary bond line between the extraction surface and the back surface. The DBR mirror is arranged on the side of the extraction surface facing away from the semiconductor body and / or on the side of the back surface facing away from the semiconductor body, whereas the DFB mirror is arranged between the back surface and the extraction surface.

[0026] According to at least one embodiment of the optoelectronic semiconductor device, the mirror is made of the material of the semiconductor body. By introducing recesses into the semiconductor body, regions with different refractive indices are created. For example, the recesses can be filled with a transparent material, such as air or a plastic material or a dielectric, which has a refractive index different from that of the semiconductor body. The recesses have a defined periodic distance along the longitudinal direction, resulting in a periodic variation of the refractive index. By producing the mirror with the material of the semiconductor body, the step of forming multiple dielectric layers can be advantageously omitted.

[0027] According to at least one embodiment of the optoelectronic semiconductor device, the first region of the extraction surface has at least one step in the longitudinal direction, which is a protrusion or overhang transverse to the deposition direction of the material of the first region beyond the imaginary plane of the extraction surface. The optoelectronic semiconductor device may in particular also have several steps.

[0028] According to at least one embodiment of the optoelectronic semiconductor device, the step is structured in such a way that the electromagnetic radiation emitted by the semiconductor body is not incident on the step. In other words, the step width and the step height are selected in such a way that the radiation emitted by the optoelectronic semiconductor device can propagate particularly unhindered. The structuring of the at least one step can be carried out, for example, by an etching process.

[0029] According to at least one embodiment of the optoelectronic semiconductor device, the width b of at least one step of the first region in the longitudinal direction n is expressed as follows: n <[(h n -aw) / tan(α / 2)]-(b n-1 -b n-2 -...-b2-b1) with a tolerance of + / - 10%, preferably with a tolerance of + / - 5%, nwhere b is defined as the width of the step of the first region across the extraction surface, a is the distance of the active region from the surface of the second region opposite the active region, and h n is the extent of the extraction surface in a direction parallel to the deposition direction of the semiconductor body, w is the thickness of the waveguide on the side of the first region adjacent to the active region and α is the vertical far field angle. The subscript n denotes the number of steps. Such structured steps in the first region of the semiconductor body particularly efficiently prevent the emitted light from being blocked by the first region.

[0030] A method for manufacturing an optoelectronic semiconductor device is also disclosed. In particular, any semiconductor device described herein may be manufactured using this method. That is, all features disclosed with respect to the semiconductor device are also disclosed with respect to the method, and vice versa.

[0031] According to at least one embodiment of a method for manufacturing an optoelectronic semiconductor device, the method includes the following steps.

[0032] Providing a semiconductor body comprising, along a deposition direction, a first region of a first conductivity type, an active region designed to generate electromagnetic radiation, and a second region of a second conductivity type, the active region extending between the first and second regions along a longitudinal direction transverse to or perpendicular to the deposition direction.

[0033] According to at least one embodiment of the method, a first groove is inserted at least partially along the deposition direction and perpendicular to the longitudinal direction by a first etching step, the first groove passing completely through the second region and the active region, so that an extraction surface for extracting electromagnetic radiation is provided on the side of the first groove facing the semiconductor body. This first etching step produces in particular a step in the extraction surface, which can be seen in the finished semiconductor device.

[0034] According to at least one embodiment of the method, a second trench is inserted at least partially along the deposition direction of the semiconductor body and perpendicular to the longitudinal direction by a first etching step on the side of the semiconductor body opposite the first trench. The second trench passes completely through the second region and the active region. A back surface is thereby formed on the side of the second trench facing the semiconductor body. This first etching step produces in particular a step on the back surface, which can be seen in the finished semiconductor device.

[0035] The first etching step preferably comprises a plasma etching step using chlorine ions and argon ions, a laser ablation step, or a photochemical wet etching step. The etching areas of the first and second grooves can be limited, for example, by a mask layer that protects the active area from the effects of the etching solution.

[0036] According to at least one embodiment of the method, the smoothing of the extraction surface and the back surface is carried out by a second etching step, which serves in particular to prepare the m-planes of the semiconductor crystal. The m-planes are the planes of a crystal having a hexagonal basic structure of the wurtzite type.

number

[0037] According to at least one embodiment of the method, the second etchant comprises one of the following etchants: KOH, NaOH, NH4OH, LiOH, TMAH, NMP. These wet chemical etching steps reduce the surface roughness of the facets, thus improving the surface quality.

[0038] According to at least one embodiment of the method, the extraction surface and the back surface are cleaned by ion cleaning, for example by low energy ions such as nitrogen ions, argon ions, hydrogen plasma, oxygen plasma, xenon ions, etc. The ion cleaned facet surface preferably no longer exhibits foreign impurities.

[0039] According to at least one embodiment of the method, the extraction and back surfaces are covered with a semi-crystalline material. As semi-crystalline material, aluminum nitride, silicon nitride, aluminum oxynitride, silicon oxynitride, silicon, aluminum oxide, gallium nitride, zinc selenide, gallium arsenide, gallium phosphide, ternary compounds and / or quaternary compounds can be used. The semi-crystalline material is primarily used to passivate the extraction and back surfaces. The semi-crystalline material can be deposited on the extraction and back surfaces, in particular, by a sputtering or ALD (Atomic Layer Deposition) process. In an ALD process, a monolayer of atoms can be deposited. The deposition of the monolayer can be performed by the deposition of several submonolayers, for example by organometallic precursors such as trimethylaluminum. The methyl groups prevent a complete monolayer by sterically hindering the individual ligands, thus forming a submonolayer. This cycle can be repeated several times until several submonolayers to a monolayer are formed. Thus, instead of atomic layers stacked one on top of the other, only a monolayer is deposited on one surface. The advantage of such a monolayer is that the surface is very well covered and that even the smallest particles and inhomogeneities are covered on the outside. This results in a very dense layer, which can advantageously provide a good diffusion barrier.

[0040] According to at least one embodiment of the method, the extraction surface and the back surface are coated with a dielectric material or metal. The coating of the extraction surface and the back surface with a dielectric material or metal serves to adjust the desired reflectivity and thus to determine the optical parameters of the optoelectronic semiconductor device. The layer of the dielectric material or metal can be deposited by sputtering, evaporation, CVD (chemical vapor deposition) or as an ALD layer. Materials such as silicon nitride, aluminum oxide, aluminum oxynitride, silicon oxynitride, tantalum oxide, silicon dioxide, or silicon can be used.

[0041] According to at least one embodiment of the method, the step of the first region is structured in the longitudinal direction beyond the extraction surface by an etching process. This structuring can serve to prevent the divergent electromagnetic radiation emitted by the active region from being blocked at the extraction surface and at the same time to separate the individual optoelectronic semiconductor devices. For the structuring, for example, a plasma etching process is used. This method step can also be carried out before cleaning the extraction surface and the back surface, in particular by using ion cleaning.

[0042] According to at least one embodiment of the method for manufacturing an optoelectronic semiconductor device, the process steps described herein are performed on a plurality of optoelectronic semiconductor devices in a wafer composite. In other words, the method steps described herein are performed before the optoelectronic semiconductor devices are separated from the wafer composite. The wafer composite is characterized by a plurality of optoelectronic semiconductor devices monolithically formed on a common growth substrate. All process steps described herein are performed before the individual optoelectronic semiconductor devices are separated. This leads to significant manufacturing advantages, in particular due to the compatibility of these method steps with processes already established from the manufacture of light-emitting diodes. The procedure of accurately combining the individual optoelectronic semiconductor devices by merging, mirror coating and then singulating can be advantageously omitted.

[0043] Further advantages, advantageous embodiments and further designs of the optoelectronic semiconductor device will become apparent from the following exemplary embodiments in conjunction with the drawings. [Brief description of the drawings]

[0044] [Figure 1A] 1 is a schematic representation of a top view of a wafer composite having a plurality of optoelectronic semiconductor devices at a step of fabrication according to an exemplary embodiment of a method described herein. [Figure 1B] 1A-1D are schematic cross-sectional views of an optoelectronic semiconductor device according to a first exemplary embodiment at steps of fabrication according to exemplary embodiments of the method described herein. [Figure 2A] 1 is a schematic representation of a top view of a wafer composite having a plurality of optoelectronic semiconductor devices at a step of fabrication according to an exemplary embodiment of a method described herein. [Figure 2B] 1A-1D are schematic cross-sectional views of an optoelectronic semiconductor device according to a first exemplary embodiment at steps of fabrication according to exemplary embodiments of the method described herein. [Figure 3A] 1 is a schematic representation of a top view of a wafer composite having a plurality of optoelectronic semiconductor devices at a step of fabrication according to an exemplary embodiment of a method described herein. [Figure 3B] 1A-1D are schematic cross-sectional views of an optoelectronic semiconductor device according to a first exemplary embodiment at steps of fabrication according to exemplary embodiments of the method described herein. [Figure 4A] 1 is a schematic representation of a top view of a wafer composite having a plurality of optoelectronic semiconductor devices at a step of fabrication according to an exemplary embodiment of a method described herein. [Figure 4B] 1A-1D are schematic cross-sectional views of an optoelectronic semiconductor device according to a first exemplary embodiment at steps of fabrication according to exemplary embodiments of the method described herein. [Figure 5A] 1 is a schematic representation of a top view of a wafer composite having a plurality of optoelectronic semiconductor devices at a step of fabrication according to an exemplary embodiment of a method described herein. [Figure 5B] 1A-1D are schematic cross-sectional views of an optoelectronic semiconductor device according to a first exemplary embodiment at steps of fabrication according to exemplary embodiments of the method described herein. [Figure 6A]1 is a schematic representation of a top view of a wafer composite having a plurality of optoelectronic semiconductor devices at a step of fabrication according to an exemplary embodiment of a method described herein. [Figure 6B] 1A-1D are schematic cross-sectional views of an optoelectronic semiconductor device according to a first exemplary embodiment at steps of fabrication according to exemplary embodiments of the method described herein. [Figure 7A] 1 is a schematic cross-sectional view of an optoelectronic semiconductor device according to a first exemplary embodiment; [Figure 8A] 1 is an optoelectronic semiconductor device according to a first exemplary embodiment in a schematic side view. [Figure 8B] 1 is an optoelectronic semiconductor device according to a first exemplary embodiment in a schematic top view. [Figure 8C] 1 is an optoelectronic semiconductor device according to a first exemplary embodiment in a schematic front view; [Figure 9A] 2 is an optoelectronic semiconductor device according to a second exemplary embodiment in a side view. [Figure 9B] 2 is an optoelectronic semiconductor device according to a second exemplary embodiment in a top view. [Figure 10] 4 is a schematic cross-sectional view of an optoelectronic semiconductor device according to a third exemplary embodiment. [Figure 11] FIG. 11 is a schematic cross-sectional view of an optoelectronic semiconductor device according to a fourth exemplary embodiment. [Figure 12] FIG. 2 is a top view of a plurality of optoelectronic semiconductor devices as described herein in a bar configuration. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0045] Identical, similar or equivalent elements are provided with the same reference numerals in the figures. The figures and the proportions of the elements depicted therein should not be considered to be to scale. Rather, individual elements may be exaggerated and larger in size for the purpose of making the figures easier to read and / or to facilitate a better understanding of the invention.

[0046] 1A shows a schematic representation of a top view of a wafer 90 with a plurality of optoelectronic semiconductor devices 1 in a first step of manufacture. The wafer 90 comprises a growth substrate 900, in particular sapphire. The wafer 90 further comprises a plurality of first contact structures 810 and a plurality of second regions 102. The first contact structures 810 are formed, for example, by a metal or a metal alloy and serve as electrical contacts for the optoelectronic semiconductor devices 1. The second regions 102 have a second conductivity type and are preferably epitaxially grown.

[0047] 1B shows a schematic cross-sectional view of an optoelectronic semiconductor device 1 according to a first exemplary embodiment. The cross-sectional view of the optoelectronic semiconductor device 1 shown here corresponds to a cut along the cut line A of the wafer 90 shown in FIG. 1A. The optoelectronic semiconductor device 1 comprises a first contact structure 810, a second region 102, an active region 103 and a first region 101, which are collectively associated with a semiconductor body 10. These regions of the semiconductor body 10 are preferably epitaxially grown on a growth substrate 900. The first region 101 has a first conductivity type, the second region 102 has a second conductivity type and the active region 103 is designed to generate electromagnetic radiation.

[0048] 2A shows a mask layer 50 formed on the side of the second region 102 and the first contact structure 810 facing away from the active region 103. For structuring purposes, a number of recesses 52 are formed in the mask layer.

[0049] Figure 2B shows a schematic cross-sectional view of an optoelectronic semiconductor device 1 according to a first exemplary embodiment. The cross-sectional view of the optoelectronic semiconductor device 1 shown here corresponds to a cut along the cut line A of the wafer 90 shown in Figure 2A. In this further method step, a mask 50 is formed on top of the optoelectronic semiconductor device 1. The mask 50 comprises a number of recesses 52 in a mask layer defining areas where the optoelectronic semiconductor device 1 will be further processed and protecting areas that will not be processed.

[0050] 3A shows the location of trench-shaped recesses 40 created by a plasma etching process which creates etching of the semiconductor body 10 at the location of the recesses 52 in the mask layer.

[0051] FIG. 3B shows a schematic cross-sectional view of an optoelectronic semiconductor device 1 according to a first exemplary embodiment. The cross-sectional view of the optoelectronic semiconductor device 1 shown here corresponds to a cut along the cutting line A of the wafer 90 shown in FIG. 3A. A number of recesses 40 are introduced into the optoelectronic semiconductor device 1. This can be done, for example, by a plasma etching step or another dry chemical etching step. The recesses 40 penetrate completely through the second region 102 and the active region 103. As a result of the etching, irregularities and damaged areas 200 appear on the surface of the sidewalls of the recesses 40. To remove the damaged areas 200, a further etching step is then performed in the recesses 40. One of the following wet chemical etchants can be used: KOH, NaOH, NH4OH, LiOH, TMAH, NMP. The mask layer 50 is then removed.

[0052] FIG. 4A shows a schematic of an ion cleaning step on the sidewalls of recess 40, which removes etch residues and other contaminants.

[0053] 4B shows a schematic cross-sectional view of an optoelectronic semiconductor device 1 according to a first exemplary embodiment. The cross-sectional view of the optoelectronic semiconductor device 1 shown here corresponds to a cut surface of the wafer 90 shown in FIG. 4A along the cut line A. Ion cleaning is carried out, for example, by nitrogen ions, argon ions, hydrogen plasma, oxygen plasma or xenon ions with low kinetic energy, which makes it possible to remove etching residues or other foreign matter from the side surfaces of the recess 40 in order to obtain a facet surface that is as clean as possible.

[0054] FIG. 5A shows the passivation 60 formed on the sides of the recess 40 by a coating process.

[0055] FIG. 5B shows a schematic cross-sectional view of the optoelectronic semiconductor device 1 according to a first exemplary embodiment. The cross-sectional view of the optoelectronic semiconductor device 1 shown here corresponds to a cut surface of the wafer 90 shown in FIG. 5A along the cut line A. To form the passivation 60, the side of the recess 40 is covered with a semi-crystalline material such as aluminum nitride, silicon, aluminum oxynitride, silicon oxynitride, aluminum oxide, gallium nitride, zinc selenide, gallium arsenide, gallium phosphide, silicon nitride, or another ternary or quaternary compound. The passivation 60 prevents damage to the active region 103 or the first region 101 or the second region 102 from external environmental influences such as moisture.

[0056] FIG. 6A shows a mirror layer 70 formed on the side of the recess 40 by a further coating step.

[0057] FIG. 6B shows a schematic cross-sectional view of the optoelectronic semiconductor device 1 according to a first exemplary embodiment. The cross-sectional view of the optoelectronic semiconductor device 1 shown here corresponds to a cut along the cut line A of the wafer 90 shown in FIG. 6A. A mirror layer 70 is formed on the passivation layer 60 inside the recess 40. The mirror layer 70 comprises, for example, a metal layer or one or more layers of one or more dielectric materials. The mirror layer 70 can include or be made of silicon nitride, aluminum oxide, aluminum oxynitride, tantalum oxide, silicon dioxide or silicon. The mirror layer 70 is formed, for example, by a sputtering, evaporation, CVD or ALD process. By forming the mirror layer 70, a defined reflectivity of the extraction surface 20 and the back surface 30 of the optoelectronic semiconductor device 1 can be achieved.

[0058] 1A, 2A, 3A, 4A, 5A and 6A each show a top view of a wafer 90 at different steps of a method for manufacturing a number of optoelectronic semiconductor devices 1. In particular, all the method steps shown therein can be advantageously carried out in a wafer composite. The structuring of the wafer is carried out by inserting a number of recesses 40 in the form of grooves. Further processing (including grinding of the groove flanks and passivation and subsequent coating of the groove flanks) can also be carried out in the wafer composite. This simplifies the production and reduces the costs per manufactured device.

[0059] FIG. 7 shows a schematic cross-section of an optoelectronic semiconductor device 1 according to a first exemplary embodiment. The optoelectronic semiconductor device 1 comprises a semiconductor body 10 with a second region 102, an active region 103 and a first region 101. A first contact structure 810 is arranged on a side of the second region 102 facing away from the active region 103. A second contact structure 820 is arranged on a side of the first region 101 facing away from the active region 103. The first contact structure 810 and the second contact structure 820 are formed, for example, from a metal, such as gold, and are intended to electrically connect the semiconductor body 10. An extraction face 20 and a back face 30 are coupled to the edge of the semiconductor body 10. The extraction face 20 is arranged plane-parallel to the back face 30 and serves to extract the electromagnetic radiation E generated in the active region 103. A layer sequence of a passivation 60 and a mirror layer 70 is formed on the extraction face 20 and on the back face 30.

[0060] The first region 101 is represented by the formula b n <[(h n -aw) / tan(α / 2)]-(b n-1 -b n-2-...-b2-b1). In this concrete example with two steps 1011, the width b1 of the first step 1011 is according to this formula b1<(h1-aw) / tan(α / 2) and the width b2 of the second step 1011 is according to this formula b2<[(h2-aw) / tan(α / 2)]-b1. The variable a represents the distance of the active area 103 from the face of the second area 102 opposite to the active area 103. The variable h1 represents the first etching depth of the recess 40, measured from the face of the second area 102 opposite to the active area 103. The variable h2 represents the second etching depth of another recess, measured from the face of the second area 102 opposite to the active area 103. The variable w represents the thickness of the waveguide area in the first area 101 adjacent to the active area 103. The waveguide region is used to optically guide the electromagnetic radiation generated in the active region 103. The variable α represents the vertical far-field angle of the electromagnetic radiation E emitted from the extraction surface 20. If the two steps 1011 are structured according to the above formula, blocking of the emitted electromagnetic radiation E by the material of the first region 101 is avoided and the electromagnetic radiation E can be emitted from the optoelectronic semiconductor device 1 particularly unhindered.

[0061] 8A shows a schematic side view of an optoelectronic semiconductor device 1 according to a first exemplary embodiment. Unlike the exemplary embodiment shown in FIG. 7, the exemplary embodiment shown in this figure has only one step 1011.

[0062] 8B shows a schematic top view of the optoelectronic semiconductor device 1 according to the first exemplary embodiment. In this plan view, the small extent of the second region 102 is evident (the second region 102 does not cover the entire width of the semiconductor body 10). This serves in particular to define the active region 103 located below the second region 102. This limits the spread of the emitted electromagnetic radiation in the active region 103, which advantageously improves the beam quality.

[0063] Fig. 8C shows a schematic front view of the optoelectronic semiconductor device 1 according to a first exemplary embodiment. The front view shown in Fig. 8C shows the extraction surface 20 of the optoelectronic semiconductor device 1. Electrical contact is made via a first contact structure 810 and a second contact structure 820 arranged on the opposite side of the first contact structure 810. Electromagnetic radiation E is extracted in a narrowly defined area.

[0064] 9A shows a schematic side view of an optoelectronic semiconductor device 1 according to a second exemplary embodiment. The second exemplary embodiment essentially corresponds to the first exemplary embodiment, differing only in the type of electrical contacts: a second contact structure 820 is arranged at another height, next to the first contact structure 810. The optoelectronic semiconductor device 1 shown here is therefore suitable for mounting on an electrically non-conductive substrate.

[0065] 9B shows a schematic top view of an optoelectronic semiconductor device 1 according to a second exemplary embodiment. Electrical contact is achieved by a first contact structure 810 and a second contact structure 820 arranged laterally therebetween.

[0066] FIG. 10 shows an optoelectronic semiconductor device 1 according to a third exemplary embodiment. The optoelectronic semiconductor device 1 shown here comprises a number of recesses 40 arranged on the back surface 30 opposite the extraction surface 20 and forming a mirror 701. Each recess 40 is provided with a passivation 60 and a mirror layer 70. The mirrors 701 comprise a so-called DBR structure, which is characterized in particular by a spectrally selective reflectivity and a very high reflectivity. The recesses 40 generate a periodic sequence of refractive index variations through the transition between the material of the semiconductor body 10 and the recesses 40. The DBR mirror is integrated directly into the semiconductor body 10. In particular for high mechanical stability and / or to adjust the refractive index, the recesses 40 can be filled with BCB or another transparent polymer or dielectric. The first region 101 has a step 1011 at the extraction surface 20 in the longitudinal direction X.

[0067] FIG. 11 shows an optoelectronic semiconductor device 1 according to a fourth exemplary embodiment. The fourth exemplary embodiment essentially corresponds to the third exemplary embodiment and additionally comprises a further mirror 702 at the extraction surface 20 of the optoelectronic semiconductor device 1. This further mirror 702 is also designed as a DBR structure and comprises several recesses 40, each with a passivation 60 and a mirror layer 70. The second mirror 702 is inserted directly into the semiconductor body 10. The different refractive indices of the semiconductor material of the semiconductor body 10 and of the material in the recesses 40 allow a periodic variation of the refractive index and thus the construction of a DBR mirror. This also applies to recesses 40 that are filled only with air. The first region 101 has a step 1011 at the extraction surface 20 in the longitudinal direction X.

[0068] 12 shows a number of optoelectronic semiconductor devices 1 combined in a monolithic structure to form a bar. By monolithic, it is meant that the optoelectronic semiconductor devices 1 shown here are grown on a common growth substrate 900 and are bonded to one another by the growth substrate 900 and / or by epitaxially produced semiconductor layers. A bar with a number of optoelectronic semiconductor devices 1 can advantageously be directly manufactured, advantageously avoiding the assembly of several previously independent optoelectronic semiconductor devices 1.

[0069] The invention is not limited by the description of the exemplary embodiments, but rather includes any novel feature and any combination of features, including in particular any combination of features in the claims, which feature or combination of features is included in the invention even if it is not itself explicitly disclosed in the claims or in the exemplary embodiments.

[0070] [Related Applications] This patent application claims priority from German patent application No. 102018111319.6, the disclosure content of which is incorporated herein by reference. [Explanation of symbols]

[0071] 1 Optoelectronic semiconductor devices 10 Semiconductor body 101 First Area 1011 Multilayered section 102 Second Area 103 Active region 20 Extraction surface 30 Back side 40 Recess 50 Mask Layers 52 Recess in mask layer 60 Passivation 70 Mirror Layer 701 Mirror 702 Mirror 200 Damage area 810 First contact structure 820 Second Contact Structure 90 Wafers 900 Growth substrate A cutting line Α Vertical far viewing angle E Electromagnetic radiation X Longitudinal direction Y deposition direction

Claims

1. A method for manufacturing an optoelectronic semiconductor device (1), comprising the steps of: Providing a semiconductor body (10) with a first region (101) of a first conductivity type, an active region (103) designed to generate electromagnetic radiation and a second region (102) of a second conductivity type along a deposition direction (Y), the active region (103) extending between the first region (101) and the second region (102) along a longitudinal direction (X) transverse to or perpendicular to the deposition direction (Y), inserting, at least partially by a first etching process, a first trench completely passing through said second region (102) and said active region (103) along said deposition direction (Y) and perpendicular to said longitudinal direction (X), the side of said first trench facing said semiconductor body (10) being provided with an extraction surface (20) for extracting electromagnetic radiation (E); inserting, by means of the first etching process, a second trench, which passes completely through the second region (102) and the active region (103), at least partially along the deposition direction (Y) of the semiconductor body (10) and perpendicular to the longitudinal direction (X), on a side of the semiconductor body opposite the first trench, whereby a back surface (30) is formed on a side of the second trench facing the semiconductor body (10); smoothing the extraction surface (20) and the back surface (30) by a second etching step; the extraction surface (20) and the back surface (30) extend parallel to a crystallographic m-plane of the semiconductor body (10); the steps of providing the semiconductor body (10), forming the first groove, forming the second groove and smoothing the extraction surface (20) and the back surface (30) are performed on an optoelectronic semiconductor device (1) in the wafer composite before the wafer composite is separated, a plurality of recesses (40) are arranged on the extraction surface (20) and on the back surface (30) which are inserted directly into the semiconductor body (10) and form a mirror (701) and an additional mirror (702); A method for manufacturing an optoelectronic semiconductor device (1), wherein each of said recesses (40) is provided with a passivation layer (60) and a mirror layer (70).

2. The etching solution in the second etching step is the following etching solution: KOH, NaOH, NH 4 2. The method of claim 1, wherein the reactant comprises one of the following: OH, LiOH, TMAH, NMP.

3. The method for manufacturing an optoelectronic semiconductor device (1) according to claim 1 or 2, wherein the extraction surface (20) and the back surface (30) are cleaned by ion cleaning.

4. 4. The method for manufacturing an optoelectronic semiconductor device (1) according to claim 3, wherein the extraction face (20) and the back face (30) are coated with a semi-crystalline material.

5. 5. The method for manufacturing an optoelectronic semiconductor device (1) according to claim 4, wherein the extraction surface (20) and the back surface (30) are covered with a dielectric material or a metal.

6. 6. A method for manufacturing an optoelectronic semiconductor device (1) according to any one of claims 1 to 5, wherein a step (1011) of the first region (101) is structured in the longitudinal direction (X) via the extraction surface (20) by an etching process.

7. The method for manufacturing an optoelectronic semiconductor device (1) according to any one of the preceding claims, wherein the second etching step is a wet-chemical etching step.

8. 8. The method for manufacturing an optoelectronic semiconductor device (1) according to claim 7, wherein the optoelectronic semiconductor device (1) is designed to generate coherent radiation.

9. Method for manufacturing an optoelectronic semiconductor device (1) according to any one of the preceding claims, wherein the semiconductor body (10) has an extension in the longitudinal direction (X) of less than 300 μm.

10. 10. Method for manufacturing an optoelectronic semiconductor device (1) according to any one of the preceding claims, wherein at least a part of the semiconductor body (10) is in a nitride compound semiconductor material system.

11. 11. A method for manufacturing an optoelectronic semiconductor device (1) according to any one of claims 1 to 10, wherein the semiconductor body (10) is deposited on a growth substrate (900), the growth substrate (900) being made of one of the following materials: sapphire, gallium nitride, silicon carbide, silicon.

12. The method for manufacturing an optoelectronic semiconductor device (1) according to any one of the preceding claims, wherein the extraction surface (20) and the back surface (30) have an average roughness in the range of 0.1 nm to 10 nm.

13. 13. A method for manufacturing an optoelectronic semiconductor device (1) according to any one of claims 1 to 12, wherein the first region (101) of the extraction surface (20) has at least one step (1011) in the longitudinal direction (X).

14. 14. The method for manufacturing an optoelectronic semiconductor device (1) according to claim 13, wherein the step (1011) is structured such that electromagnetic radiation (E) emitted from the semiconductor body (10) is not incident on the step (1011).

15. The width b of the at least one step (1011) of the first region (101) in the longitudinal direction (X) n is expressed as follows: n <[(h n -aw) / tan(α / 2)]-(b n-1 -b n-2 -. . . -b 2 -b 1 ) to an error of + / - 10% n a is the distance of the active area (103) from the face of the second area (102) opposite the active area (103), and h n 14. The method for manufacturing an optoelectronic semiconductor device (1) according to claim 13, wherein x is the extent of the extraction surface (20) in a direction parallel to the deposition direction (Y) of the semiconductor body (10), w is the thickness of the waveguide on the side of the first region (101) adjacent to the active region (103), α is defined as the vertical far field angle, and the index n denotes the number of steps (1011).

16. A method for manufacturing an optoelectronic semiconductor device (1), comprising the steps of: depositing a first region (101) of a first conductivity type, an active region (103) for generating electromagnetic radiation, and a second region (102) of a second conductivity type to form a semiconductor body (10); providing a first trench and a second trench completely through said second region (102) and said active region (103) by a first etching process; forming an extraction surface (20) on a side surface of the first groove for extracting electromagnetic radiation (E); forming a back surface (30) on a side surface of the second groove, the back surface (30) being plane-parallel to the extraction surface (20); smoothing the extraction surface (20) and the back surface (30) by a second etching process; the extraction surface (20) and the back surface (30) extend parallel to a crystallographic m-plane of the semiconductor body (10); the steps of providing the semiconductor body (10), forming the first groove, forming the second groove and smoothing the extraction surface (20) and the back surface (30) are performed on an optoelectronic semiconductor device (1) in the wafer composite before the wafer composite is separated, a plurality of recesses (40) are arranged on the extraction surface (20) and on the back surface (30) which are inserted directly into the semiconductor body (10) and form a mirror (701) and an additional mirror (702); A method for manufacturing an optoelectronic semiconductor device (1), wherein each of said recesses (40) is provided with a passivation layer (60) and a mirror layer (70).

Citation Information

Patent Citations

  • Manufacture of group iii nitride semiconductor laser diode

    JP1998041584A

  • Nitride-based semiconductor element

    JP2004260058A

  • Low-cost ingaaln-based lasers

    JP2009506550A

  • Semiconductor laser element and method of manufacturing the same

    JP2011181604A

  • Single longitudinal mode laser diode