Recovery method and manufacturing method for power storage device
A novel recovery method using a reduced aromatic hydrocarbon compound and metal ions addresses the complexity of existing third electrode methods, effectively restoring olivine-type positive electrode capacity by maintaining a high reaction driving force and minimizing negative electrode impact.
Patent Information
- Application Number
- JP2022033400
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-03-04
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-03-04
AI Technical Summary
Existing methods for restoring capacity in olivine-type positive electrode active materials in electricity storage devices, such as non-aqueous electrolyte secondary batteries, often complicate the battery structure by incorporating a third electrode, and there is a need for a novel recovery method that does not require one.
A recovery method involving a solution containing a reduced aromatic hydrocarbon compound and metal ions of the same type as the carrier ions is injected into the battery at a temperature higher than room temperature, with a maintained voltage lower than the full charge voltage, to restore capacity by supplying electrons and metal ions to the positive electrode.
This method effectively recovers the capacity of olivine-type positive electrode active materials by maintaining a high driving force for the recovery reaction, reducing the impact on the negative electrode, and suppressing gelation and precipitation of recovery agent components, resulting in improved battery performance.
Smart Images

Figure 0007586116000007 
Figure 0007586116000008 
Figure 0007586116000009
Abstract
Description
[Technical field]
[0001] Disclosed herein are methods of recovery and manufacturing of power storage devices. [Background technology]
[0002] Conventionally, as a method for restoring the capacity of an electricity storage device such as a nonaqueous electrolyte secondary battery whose capacity has deteriorated due to long-term storage or charge / discharge cycles, a method has been proposed in which a third electrode is provided in addition to a positive electrode and a negative electrode, the third electrode and the positive electrode are externally short-circuited, and carrier ions are supplied from the third electrode to the positive electrode (see, for example, Patent Document 1). Also proposed as an electricity storage device is one that uses olivine-type lithium iron phosphate as the positive electrode active material (see, for example, Patent Document 2). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2016-076358 A [Patent Document 2] JP 2009-104794 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in Patent Document 1, there was a problem that the structure of the battery became complicated by incorporating a third electrode. For this reason, there was a demand for a method for recovering the capacity without using a third electrode. In addition, a new recovery method capable of recovering the deteriorated capacity of an olivine type positive electrode active material such as that in Patent Document 2 was desired.
[0005] The present disclosure has been made to solve such problems, and has as its main object to provide a novel recovery method for performing capacity recovery on an electricity storage device including an olivine type active material, and a method for manufacturing the electricity storage device. [Means for solving the problem]
[0006] As a result of extensive research to achieve the above-mentioned object, the inventors discovered that when a solution of a restoring agent containing a reduced aromatic hydrocarbon compound and the same type of metal ion as the carrier ion of the electricity storage device is introduced into the electricity storage device at a specified temperature range and a specified voltage range, the deteriorated capacity can be restored, and have completed the present disclosure.
[0007] That is, the method for recovering an electricity storage device disclosed in the present specification includes the steps of: A method for recovering the capacity of an electricity storage device that uses metal ions as carrier ions, comprising the steps of: a recovery step of injecting a recovery agent, which is a solution containing an aromatic hydrocarbon compound in a reduced state and the same type of metal ions as the carrier ions, into the electricity storage device containing an olivine type compound as a positive electrode active material at a predetermined temperature range higher than room temperature, and maintaining a predetermined voltage lower than the full charge voltage by applying a constant voltage, thereby recovering the capacity of the electricity storage device; It includes.
[0008] Further, a method for producing an electricity storage device disclosed in the present specification includes the steps of: a recovery step of recovering the capacity of the electricity storage device having metal ions as carrier ions and having a deteriorated capacity by the above-mentioned recovery method; It includes. Effect of the Invention
[0009] This recovery method and manufacturing method for an electric storage device can provide a novel one that performs capacity recovery of an electric storage device containing an olivine type compound positive electrode active material. The reason why such an effect is obtained is presumed to be as follows. For example, a recovery agent containing an aromatic hydrocarbon compound in a reduced state and a metal ion acts directly on the positive electrode by simply injecting it into an electric storage device, and a recovery reaction occurs in which electrons and metal ions are supplied to the positive electrode. The driving force of this recovery reaction is considered to be the potential difference between the positive electrode and the recovery agent. When the recovery agent is only injected and a constant voltage is not applied, the potential of the positive electrode decreases as electrons and metal ions are supplied to the positive electrode, and the potential difference between the positive electrode and the recovery agent becomes smaller. On the other hand, when the recovery agent is injected and a constant voltage is applied to maintain a predetermined voltage, the potential of the positive electrode is kept high even if electrons and metal ions are supplied to the positive electrode, and the potential difference between the positive electrode and the recovery agent is kept high. As a result, the driving force of the recovery reaction is kept high, so that more metal ions can be supplied to the battery. In addition, in this recovery treatment, the temperature of the recovery agent is increased and the recovery treatment is performed at a higher voltage, so that it is possible to sufficiently recover the capacity of the positive electrode active material, which is an olivine type compound, and it is presumed that the impact on the negative electrode, etc. is reduced. [Brief description of the drawings]
[0010] [Figure 1] FIG. 2 is a schematic diagram showing an example of an electricity storage device 20. [Diagram 2] FIG. 2 is an explanatory diagram showing an example of a recovery reaction scheme. [Diagram 3] FIG. 13 is an explanatory diagram conceptually showing a change in the potential difference ΔErec between the positive electrode and the recovery agent after injection of the recovery agent. [Figure 4] Charging and discharging curves before and after recovery treatment in Experimental Examples 1 to 7. [Diagram 5] 1 shows the measurement results of the capacitance change after the recovery process in Experimental Examples 1 to 7. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The recovery method disclosed in this specification is a recovery method for recovering the capacity of an electricity storage device, and includes a recovery step of recovering the capacity of the electricity storage device using a recovery agent. The electricity storage device is not particularly limited as long as it uses metal ions as carrier ions, and may use, for example, Group 1 ions such as lithium, sodium, and potassium, or Group 2 ions such as magnesium, calcium, and strontium as carrier ions. The electricity storage device may be a nonaqueous electrolyte secondary battery, an ion secondary battery such as a lithium ion secondary battery, or a metal secondary battery such as a lithium metal secondary battery. In the following, as an example, a case where the electricity storage device is a lithium ion secondary battery will be mainly described.
[0012] (Electricity storage device) The power storage device includes a positive electrode, a negative electrode, and a non-aqueous electrolyte. The positive electrode may have a positive electrode active material capable of absorbing and releasing lithium ions. The negative electrode may have a negative electrode active material capable of absorbing and releasing lithium ions. The non-aqueous electrolyte may be interposed between the positive electrode and the negative electrode and conduct the lithium ions.
[0013] The positive electrode may be formed by, for example, mixing a positive electrode active material, a conductive material, and a binder, adding an appropriate solvent to form a paste-like positive electrode mixture, applying it to the surface of a current collector, drying it, and compressing it to increase the electrode density as necessary. The positive electrode active material may be an olivine type compound, such as lithium iron phosphate. The lithium iron phosphate may be one to which an additive element such as manganese is added. The positive electrode active material may have an oxidation-reduction potential of 3.5 V or more, or 4.0 V or more, based on Li metal.
[0014] In the positive electrode, the conductive material may be, for example, one or more of graphite such as natural graphite (scale graphite, flake graphite) or artificial graphite, acetylene black, carbon black, Ketjen black, carbon whisker, needle coke, carbon fiber, metal (copper, nickel, aluminum, silver, gold, etc.), etc. Among these, from the viewpoint of electronic conductivity and coating property, carbon black and acetylene black are preferable as the conductive material. The binder plays a role of binding the active material particles and the conductive material particles, and may be, for example, fluorine-containing resin such as polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVdF), fluorine rubber, etc., or thermoplastic resin such as polypropylene and polyethylene, ethylene propylene diene monomer (EPDM) rubber, sulfonated EPDM rubber, natural butyl rubber (NBR), etc., used alone or as a mixture of two or more kinds. In addition, aqueous binders such as cellulose-based carboxymethylcellulose (CMC), styrene butadiene copolymer (SBR), and aqueous dispersions of polyvinyl alcohol can also be used. As a solvent for dispersing the positive electrode active material, conductive material, and binder, for example, organic solvents such as N-methylpyrrolidone, dimethylformamide, dimethylacetamide, methyl ethyl ketone, cyclohexanone, methyl acetate, methyl acrylate, diethylenetriamine, N,N-dimethylaminopropylamine, ethylene oxide, and tetrahydrofuran can be used. In addition, a dispersant, a thickener, and the like can be added to water, and the active material can be slurried with latex such as SBR. As a thickener, for example, polysaccharides such as carboxymethylcellulose and methylcellulose can be used alone or as a mixture of two or more kinds. Examples of application methods include roller coating such as an applicator roll, screen coating, doctor blade method, spin coating, and bar coater, and any thickness and shape can be obtained by using any of these. The basis weight of the positive electrode mixture is not particularly limited, but for example, 5 mg / cm 2 May exceed 6mg / cm 2 or more, 7 mg / cm 2The weight of the positive electrode mixture may be, for example, 20 mg / cm 2 The following may be used. As the current collector, in addition to aluminum, titanium, stainless steel, nickel, iron, baked carbon, conductive polymer, conductive glass, etc., aluminum or copper whose surface is treated with carbon, nickel, titanium, silver, etc. for the purpose of improving adhesion, conductivity, and oxidation resistance can be used. The surface of these can also be subjected to oxidation treatment. The shape of the current collector can be a foil, film, sheet, net, punched or expanded one, lath, porous body, foam, fiber group formation, etc. The thickness of the current collector used is, for example, 1 to 500 μm.
[0015] The negative electrode may be formed by bonding a negative electrode active material and a current collector, or may be formed by mixing a negative electrode active material, a conductive material, and a binder, adding an appropriate solvent to form a paste-like negative electrode composite, applying it to the surface of a current collector, drying it, and compressing it to increase the electrode density as necessary. Examples of the negative electrode active material include inorganic compounds such as lithium, lithium alloys, and tin compounds, carbonaceous materials capable of absorbing and releasing lithium ions, composite oxides containing multiple elements, and conductive polymers. Examples of the carbonaceous material include cokes, glassy carbons, graphites, non-graphitizable carbons, pyrolytic carbons, and carbon fibers. Among these, graphites such as artificial graphite and natural graphite are preferred because they have an operating potential close to that of metallic lithium, can be charged and discharged at a high operating voltage, and can suppress self-discharge when a lithium salt is used as a supporting salt, and can reduce irreversible capacity during charging. Examples of the composite oxide include lithium titanium composite oxide and lithium vanadium composite oxide. Of these, carbonaceous materials are preferred as the negative electrode active material from the viewpoint of safety. The conductive material, binder, solvent, etc. used in the negative electrode can be the same as those exemplified for the positive electrode. The negative electrode active material may have an oxidation-reduction potential of 1.0 V or less, 0.5 V or less, or 0.3 V or less, based on Li metal. The weight of the negative electrode composite material is, for example, 3 mg / cm. 2 May exceed 4mg / cm 2The weight of the negative electrode mixture may be, for example, 15 mg / cm. 2 The negative electrode current collector may be made of copper, nickel, stainless steel, titanium, aluminum, baked carbon, conductive polymer, conductive glass, Al-Cd alloy, etc., or may be made of copper or the like whose surface has been treated with carbon, nickel, titanium, silver, etc., for the purpose of improving adhesion, conductivity, and reduction resistance. The surface of these materials may also be oxidized. The shape of the current collector may be the same as that of the positive electrode.
[0016] The non-aqueous electrolyte may contain a supporting salt and an organic solvent. Examples of the supporting salt include inorganic salts such as LiPF6, LiClO4, LiAsF6, and LiBF4, and organic salts such as LiN(FSO2)2, LiN(CF3SO2)2, and LiN(C2F5SO2)2. These supporting salts may be used alone or in combination. The concentration of the supporting salt is preferably 0.1 to 2.0 M, and more preferably 0.8 to 1.2 M. Examples of the organic solvent that can be used include aprotic organic solvents. Examples of such organic solvents include cyclic carbonates, chain carbonates, cyclic esters, cyclic ethers, and chain ethers. Examples of the cyclic carbonates include ethylene carbonate, propylene carbonate, butylene carbonate, and vinylene carbonate. Examples of the chain carbonates include dimethyl carbonate, diethyl carbonate, and methyl ethyl carbonate. Examples of cyclic esters include gamma butyrolactone and gamma valerolactone. Examples of cyclic ethers include tetrahydrofuran and 2-methyltetrahydrofuran. Examples of chain ethers include dimethoxyethane and ethylene glycol dimethyl ether. These may be used alone or in combination. In addition, the non-aqueous electrolyte may include nitrile solvents such as acetonitrile and propylnitrile, ionic liquids, gel electrolytes, etc. The non-aqueous electrolyte may contain additives such as a film-forming agent and a flame retardant.
[0017] The electric storage device may have a separator between the positive electrode and the negative electrode. The separator is not particularly limited as long as it has a composition that can withstand the range of use of the electric storage device, and examples thereof include polymer nonwoven fabrics such as polypropylene nonwoven fabrics and polyphenylene sulfide nonwoven fabrics, and thin microporous films of olefin resins such as polyethylene and polypropylene. These may be used alone or in combination.
[0018] The shape of the electricity storage device is not particularly limited, and examples thereof include coin type, button type, sheet type, laminated type, cylindrical type, flat type, and square type. The electricity storage device may also be applied to large devices used in electric vehicles and the like. FIG. 1 is a schematic diagram showing an example of an electricity storage device 20. The electricity storage device 20 includes a cup-shaped battery case 21, a positive electrode 22 having a positive electrode active material and provided at the bottom of the battery case 21, a negative electrode 23 having a negative electrode active material and provided at a position opposite the positive electrode 22 via a separator 24, a gasket 25 formed of an insulating material, and a sealing plate 26 disposed at an opening of the battery case 21 and sealing the battery case 21 via the gasket 25. In the electricity storage device 20, a nonaqueous electrolyte 27 is filled in the space between the positive electrode 22 and the negative electrode 23.
[0019] (Recovery Agent) The recovery agent is a solution containing an aromatic hydrocarbon compound in a reduced state and metal ions of the same type as the carrier ions of the electricity storage device. The recovery agent may be a recovery agent prepared in advance, or may be prepared in a preparation step for preparing the recovery agent. In the recovery agent, the aromatic hydrocarbon compound in a reduced state and the metal ions may be dissociated or associated. The recovery agent may contain an electrolyte in addition to an allenide solution containing an aromatic hydrocarbon compound in a reduced state and metal ions of the same type as the carrier ions of the electricity storage device. The recovery agent may be an allenide solution without containing an electrolyte. The allenide solution may further contain an organic solvent.
[0020] In the recovery agent, the aromatic hydrocarbon compound is preferably polyacene or polyphenyl. Polyacene is a compound having a structure in which a plurality of benzene rings are condensed, and examples thereof include naphthalene, anthracene, tetracene, and pentacene. Polyphenyl is a compound having a structure in which a plurality of phenyl groups are linked by single bonds, and examples thereof include biphenyl, ortho-terphenyl, meta-terphenyl, para-terphenyl, para-quaterphenyl, and para-quinquiphenyl. Polyacene and polyphenyl may have a substituent on the aromatic ring, or may contain a heteroatom in the aromatic ring. Examples of the substituent include a halogen atom, an alkyl group, an aryl group, an alkenyl group, an alkoxy group, an aryloxy group, a sulfonyl group, an amino group, a cyano group, a carbonyl group, an acyl group, an amide group, and a hydroxyl group. Examples of the heteroatom include nitrogen, oxygen, and sulfur. Examples of polyacene containing a heteroatom in an aromatic ring include quinoline, chromene, and acridine. Examples of polyphenyl containing a heteroatom in an aromatic ring include bipyridine. The aromatic hydrocarbon compound is preferably one or more of naphthalene, biphenyl, anthracene, ortho-terphenyl, and para-terphenyl among the above-mentioned compounds, and more preferably one or more of naphthalene and biphenyl. The aromatic hydrocarbon compound may be, for example, one or more of formula (1) and formula (2). The aromatic hydrocarbon compound in a reduced state is, for example, the above-mentioned aromatic hydrocarbon compound in a reduced state (also called a reduced form), for example, a radical anion. The aromatic hydrocarbon compound in a reduced state may be, for example, one or more of the reduced form of the compound of formula (1) and the reduced form of the compound of formula (2).
[0021] [ka]
[0022] In the recovery agent, the metal ions may be of the same type as the carrier ions in the electricity storage device, but are preferably one or more of alkali metal ions such as lithium ions, sodium ions, and potassium ions.
[0023] The restoring agent may include one or more compounds of formula (3) and formula (4). In the compounds of formula (3) and formula (4), the radical anion portion is the above-mentioned aromatic hydrocarbon compound in a reduced state, and the metal cation portion is the above-mentioned metal ion.
[0024] [ka]
[0025] The recovery agent may contain an organic solvent. The organic solvent is preferably a solvent having an ether skeleton, and may be a cyclic ether or a chain ether. The recovery agent may contain one or more solvents selected from tetrahydrofuran (THF), dimethoxyethane (DME), diethoxyethane (DEE), dioxolane (DOL), and dioxane (DOX). The recovery agent preferably contains one or more solvents selected from tetrahydrofuran and dimethoxyethane, and dimethoxyethane is more preferable from the viewpoint of suppressing the deterioration of the charge / discharge characteristics after the recovery process.
[0026] The recovery agent may be obtained by adding an aromatic hydrocarbon compound and a metal in a metallic state, not an ion state, to a solvent. For example, the recovery agent may be obtained by one or more of formulas (5) and (6). More specifically, the recovery agent may be obtained by reacting naphthalene, diphenyl, or terphenyl with Li metal in a THF solvent, as shown in formulas (7) to (9). Also, the recovery agent may be obtained by reacting naphthalene, diphenyl, or terphenyl with Li metal in a DME solvent, according to formulas (7) to (9). In this way, a recovery agent containing an aromatic hydrocarbon compound in a reduced state and a metal ion can be easily prepared. The recovery agent may be prepared by adding a metal to a precursor obtained by adding an aromatic hydrocarbon compound to a solvent. The recovery agent may be prepared under an inert atmosphere such as an argon atmosphere. The recovery agent may be prepared under a low dew point environment, such as a dew point of -20°C or less, -40°C or less, or -60°C or less. The recovery agent may be prepared by stirring a solvent, an aromatic hydrocarbon compound, and a metal, and a stirrer or the like may be used in this case.
[0027] [ka]
[0028] [ka]
[0029] The solution containing the aromatic hydrocarbon compound in a reduced state, metal ions, and an organic solvent described above is also called an allenide solution. This allenide solution may be used as a recovery agent as is, or may be used as a recovery agent after mixing with an electrolyte solution to adjust its reducing power. In the allenide solution, the concentrations of the aromatic hydrocarbon compound in a reduced state and the metal ions may be 0.05 mol / L or more and 1.1 mol / L or less, 0.1 mol / L or more and 1.1 mol / L or less, or 0.5 mol / L or more and 1.0 mol / L or less, respectively. Furthermore, these concentrations may be less than the solubility. Furthermore, the number of moles M of the aromatic hydrocarbon compound in a reduced state contained in the recovery agent is A (mol) and the number of moles of metal ion M B (mol) M A / M B is preferably 1 / 1, but may be 1.1 / 1.0 to 1.0 / 1.1, or may be 1.2 / 1.0 to 1.0 / 1.2.
[0030] When the recovery agent contains an electrolyte in addition to the arenide solution, the electrolyte may be, for example, a non-aqueous electrolyte exemplified as a non-aqueous electrolyte for a power storage device, or may contain a battery solvent exemplified as a non-aqueous electrolyte and a supporting salt exemplified as a non-aqueous electrolyte. The battery solvent contained in the electrolyte may be different from the organic solvent of the arenide solution, and is preferably one or more of a cyclic carbonate, a chain carbonate, and a cyclic ester, and more preferably one or more of a cyclic carbonate and a chain carbonate. The battery solvent may be one or more of ethylene carbonate, dimethyl carbonate, and ethyl methyl carbonate. The supporting salt of the electrolyte may be different from the solute of the areneide solution, and may be an inorganic salt such as LiPF6, or may include an imide-based anion such as lithium bis(fluorosulfonyl)imide (LiFSI), lithium bis(fluorosulfonyl)imide (LiFSI), or lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), and is more preferably an imide-based anion. The electrolyte may include additives such as a film-forming agent or a flame retardant. The composition of the electrolyte may be the same as or different from the non-aqueous electrolyte of the power storage device to be restored. When the recovery agent includes an electrolyte, the content of the electrolyte may be 30% by volume or more and 70% by volume or less, 30% by volume or more and 60% by volume or less, or 30% by volume or more and 50% by volume or less. When preparing a recovery agent including an electrolyte, the areneide solution and the electrolyte may be mixed, and it is more preferable to use the mixture immediately for the recovery process after mixing. Immediately after the arenide solution and the electrolyte are mixed, the solution temperature rises to, for example, a range of 36° C. or more and 45° C. or less, which is favorable for the capacity recovery of the electricity storage device.
[0031] The redox potential of the recovery agent may be higher than that of the negative electrode and lower than that of the positive electrode. The redox potential of the recovery agent may be, for example, 0.5 V to 2.5 V, 1.0 V to 2.0 V, or 1.2 V to 1.9 V, based on Li metal.
[0032] (Recovery process) In this process, a recovery agent is injected into the electricity storage device at a predetermined temperature range where the solution temperature of the recovery agent is higher than room temperature, and a predetermined voltage lower than the full charge voltage is maintained by applying a constant voltage, thereby recovering the capacity of the electricity storage device. The electricity storage device to be recovered is a battery in a capacity-degraded state (also called a degraded battery), and may be, for example, a battery in a capacity-degraded state relative to the rated capacity of the electricity storage device. The electricity storage device to be recovered may be either an unused product or a used product. Even unused products may experience capacity degradation due to long-term storage, etc.
[0033] The solution temperature when the recovery agent is added is a predetermined temperature range higher than room temperature (such as 20°C), and for example, a temperature range of 36°C to 45°C is preferable. When the solution temperature is 36°C or higher, precipitation or gelation of the substances contained in the recovery agent can be further suppressed, and when it is 45°C or lower, the deterioration of the recovery agent can be further suppressed, which is preferable. In addition, when the recovery agent is a mixed solution of an allenide solution and an electrolyte, it is preferable to add the recovery agent to the electricity storage device immediately after mixing the allenide solution and the electrolyte. This is because when these solutions are mixed, the temperature rises and reaches the vapor temperature range. Immediately after mixing may be before the solution temperature drops to room temperature, and examples of the like include within 5 minutes, within 3 minutes, and within 2 minutes after mixing.
[0034] In the recovery process, the predetermined voltage for holding the constant voltage may be a voltage lower than the full charge voltage, but is preferably a voltage that makes the potential of the positive electrode higher than the potential of the recovery agent. The full charge voltage may be the upper limit charging voltage set for the power storage device (pre-degraded battery). The predetermined voltage may be appropriately determined according to the configuration of the battery to be recovered, and may be, for example, 3.6V or more and less than 4.1V, 3.8V or more, 3.9V or more, or 4.0V or less. When the voltage for holding the constant voltage is in the range of 3.6V or more and less than 4.1V, capacity recovery can be performed sufficiently.
[0035] In this step, prior to injecting the recovery agent, the voltage of the power storage device may be adjusted to the above-mentioned predetermined voltage. In this case, for example, the power storage device may be charged by constant current charging (CC charging) or constant current constant voltage charging (CCCV charging) to adjust the voltage. This voltage adjustment is not necessary, but it is preferable that the voltage of the power storage device to be recovered is the above-mentioned predetermined voltage.
[0036] In this step, when injecting the recovery agent, the storage device may be opened and the recovery agent may be injected to seal the opening, or the recovery agent may be injected into the storage device by injection or the like to seal the perforation. When injecting the recovery agent, it may be injected under an inert atmosphere such as an argon atmosphere. The recovery agent may be injected so as to be in contact with at least the positive electrode, but may also be mixed with the non-aqueous electrolyte. The injection amount of the recovery agent can be appropriately determined depending on the configuration of the storage device, the degree of deterioration, and the like. The injection amount of the recovery agent may be, for example, 1% or more and 100% or less, 10% or more and 75% or less, or 25% or more and 50% or less with respect to the volume [mL] of the non-aqueous electrolyte contained in the storage device. The constant voltage application may be continued before or during the injection of the recovery agent, or may be started after the injection of the recovery agent while the voltage drop of the storage device due to the supply of metal ions to the positive electrode is negligibly small (for example, within 5 minutes, preferably within 3 minutes, more preferably within 1 minute). The constant voltage application time can be appropriately determined depending on the configuration of the power storage device, the degree of deterioration, the injection amount of the recovery agent, etc. For example, the injection amount of the recovery agent may be fixed, and the constant voltage application time may be adjusted depending on the configuration of the power storage device and the degree of deterioration. The constant voltage application time may be, for example, 1 hour or more and 48 hours or less, 6 hours or more and 36 hours or less, or 12 hours or more and 24 hours or less. In addition, when the constant voltage is applied before the injection of the recovery agent is completed, the constant voltage application time is the constant voltage application time after the injection of the recovery agent is completed.
[0037] In this step, when the recovery agent is injected, a recovery reaction such as that shown in FIG. 2 occurs. FIG. 2 is an explanatory diagram showing an example of the recovery reaction scheme, and is an explanatory diagram showing the scheme when the positive electrode active material is an olivine type compound such as lithium iron phosphate. FIG. 3 shows the potential difference ΔE between the positive electrode and the recovery agent after the recovery agent is injected. rec 3A is an explanatory diagram conceptually showing the change in the recovery voltage when the device is left in an open circuit state after the recovery agent is injected, and FIG. 3B is an estimated diagram when a predetermined voltage is maintained by applying a constant voltage while the recovery agent is being injected. + , the radical anion is Are·-, and the olivine-type compound is Li n-y The example will be MePO4. As shown in FIG. 2, the recovery agent is a compound containing a radical anion of an aromatic hydrocarbon compound and a metal ion, which functions as a reducing agent that donates electrons, so that by acting on a deteriorated positive electrode, electrons and metal ions are donated from the reducing agent to the positive electrode, thereby restoring the capacity. If the recovery agent is simply injected without applying a constant voltage and left in an open circuit state, as shown in FIG. 3A, the positive electrode potential decreases as the recovery reaction progresses, and the potential difference ΔE between the positive electrode and the recovery agent, which is the driving force for the reaction, is rec However, as the recovery reaction progresses, △E rec.1 >△E rec.2 >△E rec.3 Therefore, it is considered that the effect of the recovery agent gradually weakens. On the other hand, when the recovery agent is injected and a certain voltage is maintained by applying a constant voltage, as shown in FIG. 3B, the decrease in the positive electrode potential is suppressed by keeping the battery voltage constant, so that the potential difference ΔE between the positive electrode and the recovery agent, which is the driving force of the reaction, rec However, even if the recovery reaction proceeds, △E rec.1 ≒△E rec.2 ≒△E rec.3It is considered that the potential is kept substantially constant. At this time, the electrons donated from the recovery agent to the positive electrode are immediately sent to the negative electrode by the application of a constant voltage, and the metal ions supplied to the positive electrode also move to the negative electrode, so that there are vacant orbitals that accept metal ions and electrons while maintaining a high potential at the positive electrode. As a result, even when an electrode with a relatively high resistance is used, it is considered that the reaction driving force can be kept high while recovering the battery capacity (while increasing the amount of metal ions in the battery). Therefore, it is considered that the recovery agent can be effectively used, and the capacity of the battery after recovery is further improved. In addition, it is considered that the activity of the radical anions of the aromatic hydrocarbon compound is appropriately suppressed by the application of a constant voltage, and the residual radical anions of the aromatic hydrocarbon compound are suppressed by the effective use of the recovery agent, so that the deterioration of the charge and discharge characteristics after recovery is further suppressed. In this way, the capacity of the electricity storage device is restored, and an electricity storage device with restored capacity (also called a restored battery) is obtained.
[0038] In the method for recovering an electric storage device described above, the capacity of the electric storage device can be recovered by injecting a predetermined recovery agent. In this recovery method, the capacity of the battery after recovery can be further improved by injecting the recovery agent and maintaining a predetermined voltage by applying a constant voltage. The reason why such an effect is obtained is presumed to be as follows. For example, a recovery agent containing an aromatic hydrocarbon compound in a reduced state and a metal ion acts directly on the positive electrode simply by injecting it into an electric storage device, causing a recovery reaction that supplies electrons and metal ions to the positive electrode. The driving force of this recovery reaction is considered to be the potential difference between the positive electrode and the recovery agent. When the recovery agent is simply injected without applying a constant voltage, the potential of the positive electrode decreases as electrons and metal ions are supplied to the positive electrode, and the potential difference between the positive electrode and the recovery agent becomes smaller. On the other hand, when the recovery agent is injected and a predetermined voltage is maintained by applying a constant voltage, the potential of the positive electrode is kept high even if electrons and metal ions are supplied to the positive electrode, and the potential difference between the positive electrode and the recovery agent is kept high. As a result, the driving force of the recovery reaction is kept high, so that more metal ions can be supplied to the battery. Furthermore, since the recovery treatment is performed using a recovery agent at a temperature higher than room temperature, it is possible to suppress the gelation of the recovery agent and the precipitation of the components contained therein such as the supporting salt, and it is presumed that the dispersibility of the recovery agent can be improved to obtain a higher recovery effect. Furthermore, since the recovery treatment is performed at a higher voltage, it is presumed that the capacity of the positive electrode active material of the olivine type compound can be sufficiently restored and the impact on the negative electrode, etc. is smaller.
[0039] It goes without saying that the present disclosure is in no way limited to the above-described embodiment, and can be embodied in various forms as long as it falls within the technical scope of the present disclosure.
[0040] For example, in the above-described embodiment, a method for recovering an electricity storage device has been described, but in this method for recovering an electricity storage device, a new nonaqueous electrolytic secondary battery with recovered capacity can be manufactured using an electricity storage device with degraded capacity. Therefore, this recovery method may be a method for manufacturing an electricity storage device. This manufacturing method may manufacture an electricity storage device by executing the recovery step in the above-described method for recovering an electricity storage device. The method for manufacturing an electricity storage device may include a preparation step of preparing a capacity-degraded electricity storage device having metal ions as carrier ions, and a recovery step of recovering the capacity of the electricity storage device by the above-described method for recovering an electricity storage device. The electricity storage device prepared in the preparation step may be the same as the degraded battery described in the above-described embodiment. EXAMPLES
[0041] Hereinafter, an example of recovering a lithium ion battery using the recovery method for an electricity storage device of the present disclosure will be described as an embodiment. Note that Experimental Examples 4 to 7 correspond to working examples, and Experimental Examples 1 to 3 correspond to comparative examples. The present disclosure is not limited to the following examples, and it goes without saying that the present disclosure can be implemented in various forms as long as it falls within the technical scope of the present disclosure.
[0042] [Experimental Example 1] (Electricity storage device (pre-degraded battery)) The positive electrode was made of a positive electrode mixture containing 92% by mass of LiFePO4 (LFP, synthetic product) as a positive electrode active material, 5% by mass of acetylene black (manufactured by Denka Co., Ltd.) as a conductive material, and 3% by mass of polyvinylidene fluoride (manufactured by Kureha Co., Ltd.) as a binder, with a basis weight of 7 mg / cm. 2 The negative electrode was prepared by forming a negative electrode mixture on one side of an aluminum current collector foil so that the negative electrode active material was 98% by mass (OMAC1.5s, manufactured by Osaka Gas Chemicals), the negative electrode active material was 1% by mass (carboxymethyl cellulose, manufactured by Daicel), and the negative electrode active material was 1% by mass (styrene butadiene rubber, manufactured by JSR), with a basis weight of 4 mg / cm. 2The electrolyte was prepared by dissolving LiPF6 at a concentration of 1.1M in a mixed solvent containing 30% by volume of ethylene carbonate, 40% by volume of dimethyl carbonate, and 30% by volume of ethyl methyl carbonate. A polypropylene separator impregnated with 1 mL of electrolyte was sandwiched between the positive and negative electrodes to prepare a laminate cell. This was used as the pre-degradation battery. The electrode area of the cell was 10 cm2 for both the positive and negative electrodes. 2 When the resistance of the battery before deterioration was measured with a digital multimeter, the cell resistance was 10 Ω cm 2 In this electricity storage device, the lower limit discharge voltage was 3.0 V and the upper limit charge voltage was 4.1 V, which were determined according to the battery configuration.
[0043] (Deteriorated battery) The laminated cell thus produced was charged to a capacity (SOC=50%, 6mAh) equivalent to 50% of the cell's electric capacity (12mAh) in the voltage range of 3.0V to 3.65V, and Li was extracted from the positive electrode to obtain a simulated positive electrode with reduced capacity (also called a degraded positive electrode). The cell was then disassembled, the degraded positive electrode was removed, and a laminated cell was produced in the same manner as the pre-degraded battery, except that this degraded positive electrode was used as the positive electrode. This was the degraded battery.
[0044] (Recovery Agent) In an inert atmosphere, naphthalene was dissolved in dimethoxyethane (DME) solvent to a concentration of 1.0 mol / L, and then lithium metal equivalent to 1.0 mol / L was added and stirred, and a dark green radical anion liquid composition (lithium naphthalenide / DME) was prepared as an arenide solution by the reaction shown in the above formula (7). Then, the arenide solution and the above electrolyte were mixed in a volume ratio of 5:5 to prepare a recovery agent. In addition to LiPF6, lithium bis(fluorosulfonyl)imide (LiFSI) was used as the supporting salt contained in the electrolyte. In addition, the same process as above was performed except that tetrahydrofuran (THF) was used instead of DME as the solvent for the arenide solution, and a radical anion liquid composition (lithium naphthalenide / THF) was prepared.
[0045] (Recovery of degraded batteries) The deteriorated battery prepared above was adjusted to the cell voltage shown in Table 1, and the recovery agent prepared above was added using a 0.5 mL pipette. Recovery treatment was performed for 24 hours under constant voltage or open circuit conditions at the cell voltages shown in Table 1. The increase in capacity before and after treatment was calculated from the capacity after addition and treatment relative to the capacity before addition. In addition, after the recovery treatment, a charge / discharge test was performed at 1.2 mA in the voltage range of 3.0 V to 3.65 V described above, the discharge capacity was measured, and the capacity change (recovery capacity: mAh) relative to the capacity before addition was calculated.
[0046] [Experimental Examples 1-3] In the above test, the solvent of the arenide solution was DME, the supporting salt of the electrolyte contained in the recovery agent was LiPF6, the arenide solution and the electrolyte were mixed and left to stand, the temperature of the recovery agent was set to 25°C, and the voltage was held constant at 3.6 V, which was Experimental Example 1. Moreover, the supporting salt of the electrolyte contained in the recovery agent was LiFSI, and after the recovery agent was added, the recovery treatment was performed with an open circuit, which was the same as Experimental Example 1, which was Experimental Example 2. Moreover, the supporting salt of the electrolyte contained in the recovery agent was LiFSI, which was the same as Experimental Example 1, which was Experimental Example 3.
[0047] [Experimental Examples 4-7] In the above test, the solvent of the arenide solution was DME, the supporting salt of the electrolyte contained in the recovery agent was LiFSI, and the arenide solution and the electrolyte were mixed and then put into the cell at a recovery agent temperature of 40° C. immediately, and the voltage was held constant at 3.6 V. This was taken as Experimental Example 4. Experimental Example 5 was the same as Experimental Example 4 except that the voltage was held constant at 4.0 V. Experimental Example 6 was the same as Experimental Example 4 except that the supporting salt of the electrolyte contained in the recovery agent was LiPF6. Experimental Example 7 was the same as Experimental Example 4 except that the solvent of the arenide solution was THF.
[0048] [Results and Discussion] The compositions of the arenide solutions, the supporting salts of the electrolyte added to the recovery agent, their mixing ratios, the timing of introducing the recovery agent into the deteriorated cells and the solution temperature of the recovery agent at the time of introduction, the voltage conditions for the recovery treatment, the voltage treatment conditions, and the capacity change after the recovery treatment in Experimental Examples 1 to 7 are summarized in Table 1. Fig. 4 shows charge / discharge curves before and after the recovery treatment in Experimental Examples 1 to 7, and Figs. 4A to 4G are for Experimental Examples 1 to 7, respectively. Fig. 5 shows the measurement results of the capacity change after the recovery treatment in Experimental Examples 1 to 7.
[0049] As shown in Table 1 and Figures 4 and 5, in the recovery treatment at a cell voltage of 3.6 V, where the temperature of the recovery agent was low in Experimental Examples 1 to 3, the capacity was not recovered and even decreased, whether the cell voltage was held at a constant voltage or an open circuit was held. This was presumed to be because unreacted substances from the solution of the recovery agent added remained under the recovery condition of 3.6 V, causing the negative electrode member to deteriorate. On the other hand, in Experimental Example 4, where the temperature of the recovery agent was higher, it was found that the capacity could be recovered, although the recovery width was small. It was also found that a higher recovery capacity could be obtained by the constant voltage treatment at 4.0 V in Experimental Examples 5 and 6. This is because the cell voltage for holding the constant voltage in the recovery treatment was held at a higher voltage of 4.0 V, which allowed the lithium naphthalenide added to transfer electrons and Li +It was presumed that this was because the unreacted lithium naphthalenide was decomposed while supplying lithium naphthalenide, thereby preventing the capacity recovery and subsequent side reactions. In addition, the results of Experimental Examples 5 and 6 showed that the higher the solution temperature of the recovery agent, the less the effect of the type of supporting salt in the electrolyte on the capacity recovery effect. In addition, the results of Experimental Example 7 showed that a good recovery capacity could be obtained even if the solvent for the arenide solution was DME or THF. It was confirmed that the recovery agent. When the solution temperature was less than 36°C, precipitates were formed and the fluidity decreased.
[0050] As shown in Experimental Examples 1 to 3, layered rock salt type LiNi 0.8 Co 0.15 Al 0.05 O2(NCA) and LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 In the recovery process under the same treatment conditions as O2(NCM), etc., a sufficient recovery effect was not obtained in the electricity storage device using olivine-type LiFePO4 as the positive electrode active material. On the other hand, as shown in Experimental Examples 4 to 7, in the electricity storage device using LiFePO4 as the positive electrode active material, it was revealed that the capacity recovery can be sufficiently executed by performing a recovery process in which the solution temperature of the recovery agent is set to 36°C or higher, or even 40°C or higher, and a relatively high voltage of 3.6V to 4.0V is maintained from the time of the introduction of the recovery agent. In addition, it was presumed that the electrolyte to be mixed with the recovery agent contains the same type of battery solvent as that used in the electricity storage device and has a supporting salt containing an imide-based anion. In this regard, it is presumed that the layered rock salt type positive electrode active material has a low resistance, and therefore the recovery effect can be obtained regardless of the state of the recovery agent. On the other hand, since the olivine type positive electrode active material has a higher resistance than the layered rock salt type positive electrode active material, it is thought that one of the reasons for this is that it is affected by the state of the recovery agent and it is difficult to obtain the recovery effect by treating it in the same way as the layered rock salt type positive electrode active material.
[0051] [Table 1] [Explanation of symbols]
[0052] 20 electricity storage device, 21 battery case, 22 positive electrode, 23 negative electrode, 24 separator, 25 gasket, 26 sealing plate, 27 non-aqueous electrolyte.
Claims
1. A method for recovering the capacity of an electricity storage device that uses metal ions as carrier ions, comprising the steps of: a recovery step of injecting a recovery agent, which is a solution containing an aromatic hydrocarbon compound in a reduced state and the same type of metal ions as the carrier ions, into the electricity storage device containing an olivine type compound as a positive electrode active material at a predetermined temperature range higher than room temperature, and maintaining a predetermined voltage lower than the full charge voltage by applying a constant voltage, thereby recovering the capacity of the electricity storage device; Recovery methods including.
2. The recovery method according to claim 1 , wherein the recovery step comprises injecting the recovery agent at a temperature in the range of 36° C. or more and 45° C. or less.
3. The recovery method according to claim 1 or 2, wherein the recovery step comprises applying a constant voltage of the predetermined voltage in a range of 3.6 V or more and less than 4.1 V.
4. In the recovery step, the recovery agent containing at least one of a reduced form of a compound of formula (1) and a reduced form of a compound of formula (2) is used as the aromatic hydrocarbon compound in a reduced state. The recovery method according to any one of claims 1 to 3. 【Chemistry 1】
5. The recovery method according to any one of claims 1 to 4, wherein the recovery step uses the recovery agent obtained by mixing an arenide solution containing the aromatic hydrocarbon compound in a reduced state, metal ions of the same type as the carrier ions, and an organic solvent, and an electrolyte solution containing a battery solvent and a supporting salt used in the electricity storage device.
6. 6. The recovery method according to claim 5, wherein the recovery step uses the recovery agent containing the organic solvent, which is at least one of dimethoxyethane (DME) and tetrahydrofuran (THF), and the supporting salt containing an imide-based anion.
7. The recovery method according to claim 5 or 6, wherein in the recovery step, the recovery agent is added to the electricity storage device immediately after the arenide solution and the electrolyte are mixed.
8. A recovery step of recovering the capacity of the electricity storage device having a deteriorated capacity, the electricity storage device having a metal ion as a carrier ion, by the recovery method according to any one of claims 1 to 7; A method for manufacturing an electricity storage device comprising the steps of:
Citation Information
Patent Citations
Active material for lithium secondary battery, its manufacturing method, and lithium secondary battery
JP2009104794A
Power storage device and charging method thereof
JP2014143185A
Lithium ion secondary battery and battery system
JP2016076358A
Manufacturing method of power storage device and pre-doping method of power storage device
JP2018026497A
Method and system for recovering capacity of secondary battery
JP2018092748A