How to recycle interior wall materials

The method regenerates plasma processing apparatus components by using masks and controlled blasting to integrate new thermal sprayed films, addressing burr formation and contamination issues, ensuring a clean processing environment.

JP7587056B2Active Publication Date: 2024-11-19HITACHI HIGH TECH CORP
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2023553262
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-05-23
Publication Date
2024-11-19
Estimated Expiration
2042-05-23

AI Technical Summary

Technical Problem

Conventional methods for regenerating thermal sprayed films on plasma processing apparatus components result in the formation of burrs and foreign matter due to incomplete masking, leading to contamination of the processing chamber.

Method used

A method for regenerating inner wall members in a plasma processing apparatus involves using masks to protect specific areas during thermal spraying, followed by blasting and re-spraying to maintain a consistent film thickness and prevent burr formation, ensuring the new film integrates seamlessly with the existing one.

Benefits of technology

This approach effectively suppresses the generation of foreign matter, maintaining the integrity and cleanliness of the processing chamber by integrating new thermal sprayed films without creating burrs or contamination.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007587056000001
    Figure 0007587056000001
  • Figure 0007587056000002
    Figure 0007587056000002
  • Figure 0007587056000003
    Figure 0007587056000003
Patent Text Reader

Abstract

An inner wall member 40 provided to an inner wall of a processing chamber where plasma processing is formed includes a base material 41, an anode oxide film 42a, and a sprayed coating 42b. The base material 41 has a front surface FS1, a front surface FS2 located at a position higher than the front surface FS1, and a side surface SS1. The method for reproducing the inner wall member 40 includes: (a) a step for covering the anode oxide film 42a exposed from the sprayed coating 42b with a mask material 100; (b) a step for removing the sprayed coating 42b on the front surface FS2 by blast processing, and leaving the sprayed coating 42b on the side surface SS1 and on a portion of the front surface FS1; (c) a step for removing the mask material 100; (d) a step for covering, with a mask material 101, the anode oxide film 42a located at a position separated from the remaining sprayed coating 42b; (e) a step for forming, by thermal spraying, a new sprayed coating 42b on the front surface FS2, on the side surface SS1, and on a portion of the front surface FS1 so as to cover the remaining sprayed coating 42b; and (f) a step for removing the mask material 101.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for regenerating an inner wall member, and more particularly to a method for regenerating an inner wall member provided in an inner wall of a processing chamber in which plasma processing is performed in a plasma processing apparatus. [Background technology]

[0002] Wafers made of semiconductors are processed to manufacture electronic devices. In this manufacturing process, etching using plasma is applied to form circuit structures on the surface of the wafer. In such plasma etching processing, higher processing accuracy and improved yield are required as electronic devices become more highly integrated.

[0003] In a plasma processing apparatus used for plasma etching, a processing chamber is disposed inside a vacuum vessel. The base material of an internal member disposed in the processing chamber is usually made of a metal such as aluminum or stainless steel from the viewpoints of strength and cost. Since the internal member is exposed to plasma, a coating with high plasma resistance is disposed on the surface of the base material. This prevents the surface of the base material from being consumed by plasma for a longer period of time. Alternatively, changes in the amount or nature of interaction between the plasma and the surface of the internal member are suppressed.

[0004] Anodic oxide films and thermal spray films are generally used as coatings with high plasma resistance. However, after long-term use, it is inevitable that the thickness of the thermal spray film will decrease due to deterioration. The surface of the thermal spray film deteriorates after long-term use, and the particles of the thermal spray film are consumed by interaction with the plasma, resulting in a decrease in the thickness of the thermal spray film. If the surface of the substrate is exposed inside the processing chamber, particles of the metal material that constitutes the substrate may adhere to the wafer being processed inside the processing chamber, causing contamination of the wafer. Therefore, the surface of a member having a thermal spray film that has deteriorated, damaged, or worn out due to use is regenerated by a thermal spraying method to form a thermal spray film.

[0005] Patent Document 1 discloses a member for the inner wall of a processing chamber that is provided with such a plasma-resistant coating, and discloses yttrium oxide as an example of the coating.

[0006] Furthermore, Patent Document 2 discloses a technique for re-spraying a thermal sprayed film made of the same material when the thermal sprayed film formed on the surface of a substrate deteriorates after a long period of use. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2004-100039 A [Patent Document 2] JP 2007-332462 A Summary of the Invention [Problem to be solved by the invention]

[0008] In the conventional technology, various problems have arisen due to insufficient consideration of the following points. In the conventional technology, a mask material is provided at the locations where spraying is not desired, and a film is formed at the locations exposed from the mask material. At this time, part of the sprayed film is also formed on the mask material. When the mask material is removed after spraying, the sprayed film formed on the mask material is peeled off from the sprayed film on the main body, so burrs are likely to occur at the locations that come into contact with the mask material. Because the burrs are easily peeled off, the burrs become foreign matter, causing the problem of contamination of the inside of the processing chamber.

[0009] Furthermore, if the anodized film that was covered by the sprayed film is also removed when removing the deteriorated sprayed film, there is a risk that the edge of the anodized film will recede as the number of times the sprayed film is regenerated increases. On the other hand, if the sprayed film is removed so that the sprayed film overlaps with the anodized film, the remaining sprayed film will accumulate with each re-spraying. The accumulated remaining sprayed film is prone to peeling off and can easily become a source of foreign matter.

[0010] The present invention relates to a method for regenerating an internal member of a plasma processing apparatus, the method being capable of suppressing generation of foreign matter. Other objects and novel features will become apparent from the description of this specification and the accompanying drawings. [Means for solving the problem]

[0011] A brief outline of a representative embodiment of the present invention will be described below.

[0012] In one embodiment, a method for regenerating an inner wall member is provided on an inner wall of a processing chamber in which plasma processing is performed in a plasma processing apparatus. The inner wall member includes a base material having a first surface, a second surface located at a higher position than the first surface, and a first side surface connecting the first surface and the second surface, an anodic oxide film formed on the first surface and the first side surface, and a first thermal sprayed film formed on the second surface, the first side surface, and a part of the first surface so as to cover the anodic oxide film on the first side surface and a part of the anodic oxide film on the first surface. The method for regenerating an inner wall member includes the steps of: (a) covering the anodic oxide film exposed from the first sprayed film with a first mask material; (b) after step (a), removing the first sprayed film on the second surface by blasting, while leaving the first sprayed film on the second side surface and a portion of the first surface; (c) after step (b), removing the first mask material; (d) after step (c), covering the anodic oxide film located away from the remaining first sprayed film with a second mask material; (e) after step (d), forming a second sprayed film made of the same material as the first sprayed film by a spraying method on the second surface, the first side surface, and a portion of the first surface so as to cover the remaining first sprayed film; and (f) after step (e), removing the second mask material.

[0013] In one embodiment, a method for regenerating an inner wall member is provided on an inner wall of a processing chamber in a plasma processing apparatus where plasma processing is performed. The inner wall member includes a base material having a first surface, a second surface located at a higher position than the first surface, a first side surface connecting the first surface and the second surface, a third surface located at a higher position than the first surface and lower than the second surface, and a second side surface connecting the first surface and the third surface, an anodic oxide film formed on the third surface, the second side surface, the first surface, and the first side surface, and a first thermal sprayed film formed on the second surface, the first side surface, and a part of the first surface so as to cover the anodic oxide film formed on the first side surface and a part of the anodic oxide film formed on the first surface. The method for regenerating an inner wall member includes: (a) covering the anodized film exposed from the first sprayed film with a first mask material; (b) after the step (a), removing the first sprayed film on the second surface while leaving the first sprayed film on the first side surface and on a part of the first surface by projecting blast particles from a direction from the second surface toward the first surface and inclined at a predetermined angle with respect to the first surface; (c) after the step (b), removing the first mask material; and (d). The method includes the steps of: after step (c), covering the anodic oxide film on the third surface with a second mask material; (e) after step (d), forming a second sprayed film on the second surface, on the first side surface, and on a portion of the first surface by irradiating particles of the same material as the first sprayed film from a direction from the third surface to the first surface and inclined at a predetermined angle with respect to the first surface, so as to cover the remaining first sprayed film; and (f) after step (e), removing the second mask material. Effect of the Invention

[0014] According to one embodiment, it is possible to provide a method for regenerating an internal member in a plasma processing apparatus, which can suppress generation of foreign matter. [Brief description of the drawings]

[0015] [Figure 1] 1 is a schematic diagram showing a plasma processing apparatus in accordance with a first embodiment. [Diagram 2] 3 is a conceptual diagram showing an inner wall member in the first embodiment. FIG. [Diagram 3] FIG. 2 is a plan view showing an inner wall member in the first embodiment. [Figure 4] 3 is a cross-sectional view showing an inner wall member in the first embodiment. FIG. [Figure 5A] 3 is a cross-sectional view showing a base material of an inner wall member in the first embodiment. FIG. [Figure 5B] 5A to 5C are cross-sectional views showing a manufacturing method of the inner wall member in the first embodiment. [Figure 5C] 5C is a cross-sectional view showing the method of manufacturing the inner wall member subsequent to FIG. 5B. [Figure 5D] 5A to 5C are cross-sectional views showing a method for regenerating an inner wall member in the first embodiment. [Figure 5E] FIG. 5E is a cross-sectional view showing a method for regenerating the inner wall member subsequent to FIG. 5D. [Figure 5F] 5B is a cross-sectional view showing a method for regenerating the inner wall member subsequent to FIG. 5E. [Figure 5G] FIG. 5C is a cross-sectional view showing a method for regenerating the inner wall member subsequent to FIG. 5F. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, the embodiments will be described in detail with reference to the drawings. In all the drawings for explaining the embodiments, the same reference numerals are used for the members having the same functions, and the repeated explanations are omitted. In the following embodiments, the explanations of the same or similar parts will not be repeated as a rule unless it is particularly necessary.

[0017] In addition, the X-direction, Y-direction, and Z-direction described in this application intersect and are perpendicular to each other. Expressions such as "plan view" and "planar view" used in this application mean that a plane formed by the X-direction and the Y-direction is viewed from the Z-direction.

[0018] (Embodiment 1) <Configuration of Plasma Processing Apparatus> An overview of a plasma processing apparatus 1 according to the first embodiment will be described below with reference to FIG.

[0019] The plasma processing apparatus 1 includes a cylindrical vacuum vessel 2, a processing chamber 4 provided inside the vacuum vessel 2, and a stage 5 provided inside the processing chamber 4. The upper part of the processing chamber 4 forms a discharge chamber, which is a space where plasma 3 is generated.

[0020] A disk-shaped window member 6 and a disk-shaped plate 7 are provided above the stage 5. The window member 6 is made of a dielectric material such as quartz or ceramics, and hermetically seals the inside of the processing chamber 4. The plate 7 is provided below the window member 6 so as to be spaced apart from the window member 6, and is made of a dielectric material such as quartz. The plate 7 has a plurality of through holes 8. A gap 9 is provided between the window member 6 and the plate 7, and a processing gas is supplied into the gap 9 when performing plasma processing.

[0021] The stage 5 is used to place the wafer WF when performing plasma processing on the wafer WF, which is the workpiece. The wafer WF is a substrate of a semiconductor material such as silicon, or a laminated structure including a semiconductor element, an insulating film, and a conductive film formed on the substrate. The stage 5 is a cylindrical member whose central axis in the vertical direction is located concentrically with the discharge chamber of the processing chamber 4 or in a position close enough to be considered concentric when viewed from above.

[0022] The space between the stage 5 and the bottom surface of the processing chamber 4 communicates with the space above the stage 5 via a gap between the sidewall of the stage 5 and the side surface of the processing chamber 4. Therefore, by-products, plasma 3, or gas particles generated during processing of the wafer WF placed on the stage 5 are exhausted to the outside of the processing chamber 4 via the space between the stage 5 and the bottom surface of the processing chamber 4.

[0023] Although not shown in detail, the stage 5 has a cylindrical base material made of a metal material. The upper surface of the base material is covered with a dielectric film. A heater is provided inside the dielectric film, and a plurality of electrodes are provided above the heater. A DC voltage is supplied to the plurality of electrodes. This DC voltage causes the wafer WF to be attracted to the upper surface of the dielectric film, and an electrostatic force for holding the wafer WF can be generated inside the dielectric film and the wafer WF. The plurality of electrodes are arranged point symmetrically around the central axis of the stage 5 in the up-down direction, and voltages of different polarities are applied to the plurality of electrodes.

[0024] The stage 5 is provided with multiple coolant channels arranged in a concentric or spiral pattern. With the wafer WF placed on the top surface of the dielectric film, a thermally conductive gas such as helium (He) is supplied to the gap between the bottom surface of the wafer WF and the top surface of the dielectric film. For this reason, piping through which the gas flows is provided inside the substrate and the dielectric film.

[0025] The plasma processing apparatus 1 also includes an impedance matching device 10 and a high-frequency power supply 11. The high-frequency power supply 11 is connected to the substrate of the stage 5 via the impedance matching device 10. During plasma processing of the wafer WF, high-frequency power is supplied from the high-frequency power supply 11 to the substrate in order to form an electric field for attracting charged particles in the plasma on the upper surface of the wafer WF.

[0026] The plasma processing apparatus 1 also includes a waveguide 12, a magnetron oscillator 13, a solenoid coil 14, and a solenoid coil 15. The waveguide 12 is provided above the window member 6, and the magnetron oscillator 13 is provided at one end of the waveguide 12. The magnetron oscillator 13 can oscillate and output an electric field of microwaves. The waveguide 12 is a conduit for propagating the electric field of microwaves, and the electric field of microwaves is supplied to the inside of the processing chamber 4 via the waveguide 12. The solenoid coil 14 and the solenoid coil 15 are provided around the waveguide 12 and the processing chamber 4, and are used as a magnetic field generating means.

[0027] The waveguide 12 includes a rectangular waveguide section and a circular waveguide section. The rectangular waveguide section has a rectangular cross-sectional shape and extends in the horizontal direction. A magnetron oscillator 13 is provided at one end of the rectangular waveguide section. The circular waveguide section is connected to the other end of the rectangular waveguide section. The circular waveguide section has a circular cross-sectional shape and is configured such that its central axis extends in the vertical direction.

[0028] The plasma processing apparatus 1 further includes a pipe 16 and a gas supply device 17. The gas supply device 17 is connected to the processing chamber 4 via the pipe 16. The processing gas is supplied from the gas supply device 17 through the pipe 16 to the gap 9 and diffuses inside the gap 9. The diffused processing gas is supplied above the stage 5 through the through-hole 8.

[0029] The plasma processing apparatus 1 also includes a pressure adjustment plate 18, a pressure detector 19, a turbo molecular pump 20 which is a high vacuum pump, a dry pump 21 which is a roughing pump, an exhaust pipe 22, and valves 23 to 25. The space between the stage 5 and the bottom surface of the processing chamber 4 functions as a vacuum exhaust section. The pressure adjustment plate 18 is a disc-shaped valve, and by moving up and down above the exhaust port, it increases and decreases the area of ​​the flow path for gas to flow into the exhaust port. In other words, the pressure adjustment plate 18 also serves as a valve that opens and closes the exhaust port.

[0030] The pressure detector 19 is a sensor for detecting the pressure inside the processing chamber 4. A signal output from the pressure detector 19 is sent to a control unit (not shown), which detects the pressure value and outputs a command signal from the control unit in accordance with the detected value. Based on the command signal, the pressure adjustment plate 18 is driven, the vertical position of the pressure adjustment plate 18 changes, and the area of ​​the exhaust flow path increases or decreases.

[0031] The outlet of the turbo molecular pump 20 is connected to a dry pump 21 via a pipe, and a valve 23 is provided in the middle of the pipe. The space between the stage 5 and the bottom surface of the processing chamber 4 is connected to an exhaust pipe 22, and the exhaust pipe 22 is provided with a valve 24 and a valve 25. The valve 24 is a slow exhaust valve for slowly exhausting air with the dry pump 21 so that the processing chamber 4 is brought from atmospheric pressure to a vacuum state, and the valve 23 is a main exhaust valve for quickly exhausting air with the turbo molecular pump 20.

[0032] <Plasma treatment> As an example of the plasma processing, a case where an etching process using the plasma 3 is performed on a predetermined film preliminarily formed on the upper surface of the wafer WF will be illustrated below.

[0033] The wafer WF is placed on the tip of an arm of a vacuum transfer device such as a robot arm from outside the plasma processing device 1, transferred into the inside of the processing chamber 4, and placed on the stage 5. When the arm of the vacuum transfer device leaves the processing chamber 4, the inside of the processing chamber 4 is sealed. Then, a DC voltage is applied to an electrostatic attraction electrode inside the dielectric film of the stage 5, and the wafer WF is held on the dielectric film by the generated electrostatic force.

[0034] In this state, a thermally conductive gas such as helium (He) is supplied to the gap between the wafer WF and the dielectric film through a pipe provided inside the stage 5. In addition, a coolant adjusted to a predetermined temperature by a coolant temperature regulator (not shown) is supplied to a coolant flow path inside the stage 5. This promotes heat transfer between the temperature-adjusted base material and the wafer WF, and the temperature of the wafer WF is adjusted to a value within a range appropriate for starting plasma processing.

[0035] The processing gas, the flow rate and speed of which are adjusted by the gas supply device 17, is supplied into the processing chamber 4 through the pipe 16, and the inside of the processing chamber 4 is exhausted from the exhaust port by the operation of the turbo molecular pump 20. By balancing these two, the pressure inside the processing chamber 4 is adjusted to a value within a range suitable for plasma processing.

[0036] In this state, a microwave electric field is generated from magnetron oscillator 13. The microwave electric field propagates inside waveguide 12 and passes through window member 6 and plate 7. Furthermore, a magnetic field generated by solenoid coils 14 and 15 is supplied to processing chamber 4. Electron cyclotron resonance (ECR) is generated by the interaction between the magnetic field and the microwave electric field. Then, atoms or molecules of the processing gas are excited, ionized, or dissociated, generating plasma 3 inside processing chamber 4.

[0037] When the plasma 3 is generated, high frequency power is supplied from the high frequency power supply 11 to the substrate of the stage 5, a bias potential is formed on the upper surface of the wafer WF, and charged particles such as ions in the plasma 3 are attracted to the upper surface of the wafer WF. This causes an etching process to be performed on a predetermined film on the wafer WF so as to conform to the pattern shape of the mask layer. Thereafter, when it is detected that the processing of the target film has reached its end point, the supply of high frequency power from the high frequency power supply 11 is stopped, and the plasma processing is stopped.

[0038] If no further etching of the wafer WF is required, high vacuum evacuation is performed. Then, after the static electricity is removed and the suction of the wafer WF is released, the arm of the vacuum transfer device enters the inside of the processing chamber 4, and the processed wafer WF is transferred to the outside of the plasma processing device 1.

[0039] <Inner wall material of processing chamber> 1, an inner wall member 40 is provided on the inner wall of a processing chamber 4 in which plasma processing is performed in a plasma processing apparatus 1. The inner wall member 40 functions as, for example, an earth electrode for stabilizing the electric potential of the plasma 3, which is a dielectric material.

[0040] 2, the inner wall member 40 includes a substrate 41 and a coating 42 that covers the surface of the substrate 41. The substrate 41 is made of a conductive material, for example, a metal material such as aluminum, an aluminum alloy, stainless steel, or a stainless steel alloy.

[0041] The inner wall member 40 is exposed to the plasma 3 during plasma processing. If the coating 42 were not present on the surface of the base material 41, the base material 41 would be exposed to the plasma 3, causing corrosion or becoming a source of foreign matter, which could result in contamination of the wafer WF. The coating 42 is provided to suppress contamination of the wafer WF, and is made of a material that is more resistant to the plasma 3 than the base material 41. The coating 42 allows the inner wall member 40 to maintain its function as an earth electrode, and can also protect the base material 41 from the plasma 3.

[0042] Metal materials such as stainless steel alloys or aluminum alloys are also used for the substrate 30 that does not function as an earth electrode. Therefore, the surface of the substrate 30 is also subjected to a treatment for improving resistance to the plasma 3 or a treatment for reducing wear of the substrate 30 in order to suppress corrosion or the generation of foreign matter caused by exposure to the plasma 3. Such treatments include, for example, a passivation treatment, formation of a thermal sprayed film, or formation of a film by a PVD method or a CVD method.

[0043] Although not shown, a cylindrical cover made of ceramics such as yttrium oxide or quartz may be disposed inside the inner wall of the cylindrical substrate 30 in order to reduce wear of the substrate 30 due to the plasma 3. By disposing such a cover between the substrate 30 and the plasma 3, contact between the substrate 30 and highly reactive particles in the plasma 3 or collision between the substrate 30 and charged particles is blocked or reduced. This makes it possible to suppress wear of the substrate 30.

[0044] The configuration of the inner wall member 40 will be described with reference to Figures 3 and 4. Figure 3 is a plan view showing the inner wall member 40, and Figure 4 is a cross-sectional view taken along line AA shown in Figure 3.

[0045] The inner wall member 40 (base material 41) is generally cylindrical with a predetermined thickness between the inner circumference and the outer circumference. The inner wall member 40 is composed of an upper portion 40a, a middle portion 40b, and a lower portion 40c. The upper portion 40a is a portion where the inner diameter and the outer diameter of the cylinder are relatively small, and the lower portion 40c is a portion where the inner diameter and the outer diameter of the cylinder are relatively large. The middle portion 40b is a portion for connecting the upper portion 40a and the lower portion 40c, and is, for example, in the shape of a truncated cone where the inner diameter and the outer diameter of the cylinder change continuously.

[0046] The inner wall member 40 is provided along the inner wall of the processing chamber 4 so as to surround the outer periphery of the stage 5. A thermal sprayed film is formed by a thermal spraying method as part of the coating 42 on the inner periphery surface of the inner wall member 40 (the inner periphery surface of the base material 41). Furthermore, with the inner wall member 40 attached inside the processing chamber 4, an anodic oxide film is formed by anodizing treatment as part of the coating 42 on the outer periphery surface of the inner wall member 40 (the outer periphery surface of the base material 41).

[0047] The sprayed film is formed not only on the inner peripheral surface of the substrate 41, but also on the outer peripheral surface of the substrate 41 via the upper end of the upper portion 40a. This is because there is a risk that particles of the plasma 3 may flow from the inner peripheral side of the inner wall member 40 to the outer peripheral side of the inner wall member 40 at the upper portion 40a and interact with the outer peripheral surface of the substrate 41. Therefore, it is necessary to form a sprayed film on the outer peripheral surface of the substrate 41 up to the region where the particles of the plasma 3 are expected to flow. In FIG. 4, such a region is shown as region 50.

[0048] <Structure of inner wall member and manufacturing method thereof in embodiment 1> 5A to 5G are enlarged cross-sectional views of region 50. The structure of inner wall member 40 and its manufacturing method will be described below with reference to FIGS. 5A to 5C. Inner wall member 40 in the first embodiment includes substrate 41, anodized film 42a, and sprayed film 42b, as described below. Anodized film 42a and sprayed film 42b each constitute a part of coating 42.

[0049] Fig. 5A shows the substrate 41 before the anodized film 42a and the thermal sprayed film 42b are formed. As shown in Fig. 5A, the substrate 41 in the first embodiment has two steps in the X direction from the inner periphery side of the inner wall member 40 (the inner periphery side of the substrate 41) to the outer periphery side of the inner wall member 40 (the outer periphery side of the substrate 41).

[0050] That is, the base material 41 has a surface FS1, a surface FS2, a side surface SS1, a surface FS3, and a side surface SS2 on the outer circumferential side of the base material 41. The surface FS2 is located at a higher position than the surface FS1. The side surface SS1 connects the surfaces FS1 and FS2. The surface FS3 is located at a higher position than the surface FS1 and at a lower position than the surface FS2. The side surface SS2 connects the surfaces FS1 and FS3.

[0051] The distance L1 between the surface FS1 and the surface FS2 corresponds to the height of one of the steps and is, for example, 0.6 mm. The distance L2 between the surface FS1 and the surface FS3 corresponds to the height of the other step and is, for example, 0.1 mm.

[0052] 5B, before the thermal sprayed film 42b is formed, the anodic oxide film 42a is formed by anodizing. The anodic oxide film 42a is formed on the surface FS3, the side surface SS1, the surface FS1, and the side surface SS2. When the substrate 41 is made of aluminum or an aluminum alloy, for example, the anodic oxide film 42a is an alumite coating.

[0053] Next, the anodic oxide film 42a on the surface FS3 is covered with a mask material 100. The mask material 100 is a jig or the like. In this state, the sprayed film 42b is formed by a thermal spraying method. In this thermal spraying method, plasma is generated under atmospheric pressure, and particles of yttrium oxide, yttrium fluoride, or a material containing these are supplied into the plasma to semi-molten the particles. The semi-molten particles 200 are irradiated onto the surfaces FS1 and FS2. Here, the particles 200 are irradiated from a direction from the surface FS3 toward the surface FS1 and from a direction inclined at a predetermined angle θ1 with respect to the surface FS1.

[0054] 5C, by the above-mentioned thermal spraying method, a thermal sprayed film 42b is formed on the surface FS2, the side surface SS1, and a part of the surface FS1. The thermal sprayed film 42b is formed so as to cover the anodic oxide film 42a on the side surface SS1 and a part of the anodic oxide film 42a on the surface FS1. By irradiating the particles 200 from a direction tilted at the angle θ1, the particles 200 are not irradiated onto the surface FS1 near the mask material 100, and the thermal sprayed film 42b is formed at a position away from the mask material 100. In other words, the thermal sprayed film 42b is formed at a position away from the surface FS3 and the side surface SS2.

[0055] Thereafter, the mask material 100 is removed. At this time, the mask material 100 is not in contact with the sprayed film 42b. Therefore, the problem of the conventional technology that burrs are generated and the inside of the processing chamber 4 is contaminated by the burrs becoming foreign matter can be solved.

[0056] The surface irregularities of the sprayed film 42b are configured, for example, so that the arithmetic mean roughness (surface roughness) Ra is not more than 8. The average size of each particle of the sprayed film 42b (average particle diameter) is, for example, not less than 10 μm and not more than 50 μm in volume-based D50.

[0057] In region 50, surface FS1, surface FS2, surface FS3, side SS1 and side SS2 are covered with at least one of anodized film 42a or sprayed film 42b, thereby preventing substrate 41 from being exposed to plasma 3 during plasma treatment.

[0058] <Method of Regenerating Inner Wall Member in First Embodiment> 5D to 5G, a method for recycling the inner wall member 40 will be described below. Note that the method for recycling the inner wall member 40 can also be considered as a manufacturing method for the inner wall member 40 following the method shown in FIG. 5C.

[0059] 5C is placed in a processing chamber 4 for a predetermined period of time and exposed to the plasma 3. The sprayed film 42b exposed to the plasma 3 is modified or worn out, so it is necessary to remove the sprayed film 42b and regenerate a new sprayed film 42b.

[0060] 5D, the anodized film 42a exposed from the sprayed film 42b is covered with a mask material 101. The mask material 101 is made of a material having properties that prevent it from being removed by a blasting process described later, and is, for example, a jig or a resin tape.

[0061] Next, a blasting treatment is performed on the thermal sprayed film 42b. The blasting treatment is performed by projecting blast particles 300 from a direction from the surface FS2 toward the surface FS1 and from a direction inclined at a predetermined angle θ2 with respect to the surface FS1. The blast particles 300 collide with the particles of the thermal sprayed film 42b, and the thermal sprayed film 42b is removed by a physical action.

[0062] 5E, the above-mentioned blasting process removes the sprayed film 42b on the front surface FS2, while leaving the sprayed film 42b on the side surface SS1 and on a part of the front surface FS1. By appropriately selecting the angle θ2 of the projected blast particles 300, it is possible to leave a part of the sprayed film 42b. Thereafter, the mask material 101 is removed.

[0063] Next, as shown in Fig. 5F, the anodic oxide film 42a on the surface FS3 is covered with a mask material 100. That is, the anodic oxide film 42a located at a position away from the remaining sprayed film 42b is covered with the mask material 100. Next, a new sprayed film 42b is formed by irradiating semi-molten particles 200 by a spraying method. The method and conditions for forming the new sprayed film 42b are the same as those described in Fig. 5B.

[0064] That is, particles of the same material as the remaining sprayed film 42b are irradiated from a direction from surface FS3 toward surface FS1 and from a direction inclined at a predetermined angle θ1 with respect to surface FS1. As a result, as shown in Fig. 5G, a new sprayed film 42b is formed on surface FS2, side surface SS1, and part of surface FS1 so as to cover the remaining sprayed film 42b. Thereafter, mask material 100 is removed.

[0065] 5G, the mask material 100 is not in contact with the sprayed film 42b. Therefore, the problem of the conventional technology that burrs are generated and the inside of the processing chamber 4 is contaminated by the burrs becoming foreign matter can be solved.

[0066] Furthermore, if too much new sprayed film 42b is formed, the upper part of sprayed film 42b may come into contact with the upper part of mask material 100, which may cause burrs when removing mask material 100. Therefore, it is preferable to stop the irradiation of particles 200 before sprayed film 42b and mask material 100 come into contact with each other.

[0067] In this way, the sprayed film 42b can be regenerated, and the inner wall member 40 is regenerated to the state shown in FIG. 5C. The initially formed sprayed film 42b and the newly formed sprayed film 42b are made of the same material. The sprayed film 42b remaining after the blasting process is not directly exposed to the plasma 3 during the plasma processing, and is an area that has undergone almost no modification. Therefore, the remaining sprayed film 42b and the new sprayed film 42b are integrated into the same high-quality sprayed film 42b.

[0068] Thereafter, if the inner wall member 40 is exposed to the plasma 3 again and the sprayed film 42b is modified, the steps of FIGS. 5D to 5G can be repeated to regenerate the sprayed film 42b and regenerate the inner wall member 40.

[0069] Although the present invention has been specifically described based on the above embodiment, the present invention is not limited to the above embodiment and can be modified in various ways without departing from the spirit of the present invention. [Explanation of symbols]

[0070] 1. Plasma processing equipment 2 Vacuum container 3. Plasma 4 Processing Room 5 Stage 6 Window Materials 7 Plate 8 Through holes 9 Gap 10 Impedance Matching Box 11 High frequency power supply 12 Waveguide 13 Magnetron Oscillator 14 Solenoid coil 15 Solenoid coil 16 Piping 17 Gas supply equipment 18 Pressure adjustment plate 19 Pressure detector 20 Turbomolecular Pump 21 Dry Pump 22 Exhaust piping 23~25 Valve 30 Base material 40 Inner wall material 40a Upper 40b middle part 40c bottom 41 Base material 42 Membrane 42a Anodic oxide film 42b Thermal spray coating 50 areas 100, 101 Mask material 200 Semi-molten particles 300 blast particles FS1~FS3 Surface SS1, SS2 Side WF Wafer (material to be processed)

Claims

1. A method for regenerating an inner wall member provided on an inner wall of a processing chamber in which plasma processing is performed in a plasma processing apparatus, comprising the steps of: The inner wall member is a substrate having a first surface, a second surface located at a higher position than the first surface, and a first side surface connecting the first surface and the second surface; an anodic oxide film formed on the first surface and the first side surface; a first sprayed film formed on the second surface, the first side surface, and a portion of the first surface so as to cover the anodic oxide film on the first side surface and a portion of the anodic oxide film on the first surface; Equipped with (a) covering the anodized film exposed from the first thermal sprayed film with a first mask material; (b) after the step (a), removing the first sprayed film on the second surface by a blasting process while leaving the first sprayed film on the first side surface and a part of the first surface; (c) removing the first mask material after the step (b); (d) after the step (c), covering the remaining anodized film located away from the first sprayed film with a second mask material; (e) forming a second sprayed film made of the same material as the first sprayed film by a spraying method on the second surface, the first side surface, and a part of the first surface so as to cover the remaining first sprayed film after the step (d); (f) removing the second mask material after the step (e); The method for regenerating an inner wall member comprises the steps of:

2. The method for regenerating an inner wall member according to claim 1, the base material has a third surface located at a higher position than the first surface and lower than the second surface, and a second side surface connecting the first surface and the third surface; the anodic oxide film is also formed on the third surface and the second side surface; In the step (d), the anodic oxide film on the third surface is covered with the second mask material.

3. The method for regenerating an inner wall member according to claim 2, In the step (e), the second sprayed film is formed by irradiating particles of the same material as the first sprayed film from a direction from the third surface toward the first surface and inclined at a predetermined angle with respect to the first surface.

4. The method for regenerating an inner wall member according to claim 3, The method for regenerating an inner wall member, wherein in the step (e), the irradiation of the particles is stopped before the second sprayed film and the second mask material come into contact with each other.

5. The method for regenerating an inner wall member according to claim 1, A method for regenerating an inner wall member, wherein in step (b), the blasting treatment is performed by projecting blast particles from a direction from the second surface to the first surface and inclined at a predetermined angle with respect to the first surface.

6. The method for regenerating an inner wall member according to claim 1, The substrate has a cylindrical shape having a predetermined thickness between an inner periphery and an outer periphery, The method for recycling an inner wall member, wherein the first surface, the second surface and the first side surface are provided on the outer periphery of the base material.

7. A method for regenerating an inner wall member provided on an inner wall of a processing chamber in which plasma processing is performed in a plasma processing apparatus, comprising the steps of: The inner wall member is a base material having a first surface, a second surface located at a higher position than the first surface, a first side surface connecting the first surface and the second surface, a third surface located at a higher position than the first surface and lower than the second surface, and a second side surface connecting the first surface and the third surface; an anodic oxide film formed on the third surface, the second side surface, the first surface, and the first side surface; a first sprayed film formed on the second surface, the first side surface, and a portion of the first surface so as to cover the anodic oxide film formed on the first side surface and a portion of the anodic oxide film formed on the first surface; Equipped with (a) covering the anodized film exposed from the first thermal sprayed film with a first mask material; (b) after the step (a), a step of projecting blast particles from a direction from the second surface toward the first surface and from a direction inclined at a predetermined angle with respect to the first surface, thereby removing the first sprayed film on the second surface and leaving the first sprayed film on the first side surface and a part of the first surface; (c) removing the first mask material after the step (b); (d) after the step (c), covering the anodic oxide film on the third surface with a second mask material; (e) after the step (d), forming a second sprayed film on the second surface, the first side surface, and a part of the first surface so as to cover the remaining first sprayed film by irradiating particles of the same material as the first sprayed film from a direction from the third surface toward the first surface and inclined at a predetermined angle with respect to the first surface; (f) removing the second mask material after the step (e); The method for regenerating an inner wall member comprises the steps of:

8. The method for regenerating an inner wall member according to claim 7, The method for regenerating an inner wall member, wherein in the step (e), the irradiation of the particles is stopped before the second sprayed film and the second mask material come into contact with each other.

9. The method for regenerating an inner wall member according to claim 7, The substrate has a cylindrical shape having a predetermined thickness between an inner periphery and an outer periphery, A method for recycling an inner wall member, wherein the first surface, the second surface, the third surface, the first side surface and the second side surface are provided on the outer periphery of the base material.

Citation Information

Patent Citations

  • Plasma treatment apparatus and manufacturing method of parts for the apparatus

    JP2002203838A

  • Rare earth oxide thermal spraying member and powder for thermal spraying

    JP2004100039A

  • Component and method for using the same for semiconductor manufacturing equipment

    JP2004134690A

  • Plasma processing apparatus

    JP2006222240A

  • Method for regenerating plasma treatment container, member inside the plasma treatment container, method for manufacturing the member inside the plasma treatment container and apparatus for plasma treatment