Method for forming a field emission cathode - Patents.com
The sol-gel process improves field emission cathode uniformity and stability by using carbon nanotubes and metal oxides, addressing non-uniformity and batch-to-batch issues, resulting in improved emission properties.
Patent Information
- Application Number
- JP2023528967
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-11-17
- Filing Date
- 2021-11-16
- Publication Date
- 2024-11-28
- Estimated Expiration
- 2041-11-16
AI Technical Summary
Existing field emission cathode devices face issues with non-uniform emitter distribution, high surface roughness, and batch-to-batch variations due to poor dispersion and stability of carbon nanotubes, leading to low emission current, high turn-on voltage, and short emission lifetime.
A sol-gel process is employed using a specific ratio of carbon nanotubes and a water-stable conductive polymer, combined with metal oxide sol solutions and polar additives, followed by ultrasonic dispersion and annealing, to form a uniform field emission material precursor, which is then deposited and activated on a substrate.
The method results in a field emission cathode with high emitter density, low surface roughness, and reduced batch-to-batch variations, enhancing emission current, lowering turn-on voltage, and extending emission lifetime.
Smart Images

Figure 0007591656000001 
Figure 0007591656000002 
Figure 0007591656000003
Abstract
Description
[Technical field]
[0001] Field of Disclosure The present application relates to methods of making field emission cathode devices, and more particularly to methods of forming field emission cathodes utilizing a sol-gel process that incorporate carbon nanotubes and metal oxides to improve the field emission properties of the cathodes and field emission cathode devices implementing such cathodes. [Background technology]
[0002] 2. Description of Related Art A field emission cathode device generally includes a cathode substrate (usually composed of a metal or other conductive material such as an alloy, conductive glass, metallized ceramic, doped silicon, etc.), a layer of a field emission material (e.g., nanotubes, nanowires, graphene) disposed on the substrate, and, optionally, an additional layer of an adhesion material disposed between the substrate and the field emission material. Some typical applications of field emission cathode devices include, for example, electronic devices capable of operating in a vacuum environment, field emission displays, and x-ray tubes.
[0003] Carbon nanotubes can be used in the fabrication of cold field emission cathodes. However, carbon nanotubes typically do not disperse well and / or are not stable during current electrophoretic processes, resulting in poor uniformity of the emitters on the cathode surface and large batch-to-batch variations of the cathode. Furthermore, cathodes made by electrophoretic deposition generally vary from batch to batch due to concentration changes of components in the suspension used in the electrophoretic deposition process. This is a major drawback for large-scale industrial production processes.
[0004] Additionally, some processes attempt to improve the uniformity of the emitters on the cathode surface by making the layer material precursor more homogeneous with matrix particles. The particles used in the layer material precursor are not uniform in size with a wide size distribution (e.g., 300 nanometers to 3 micrometers), which results in a high surface roughness of the layer and a wide distribution of emitters at different height levels across the surface of the cathode after the annealing and activation steps. Only those emitters at the highest levels can contribute to electron emission, since those at lower levels are electrically shielded and cannot effectively emit electrons. Furthermore, loose particles remain at lower levels and cannot be completely removed in the activation step, resulting in limited emission characteristics such as low emission current, high turn-on voltage, short emission lifetime, and large batch-to-batch variation.
[0005] Therefore, a need exists for a process to improve the production of field emission matrix materials to obtain field emission cathodes having a high density of emitters distributed on the cathode surface with high uniformity and low batch-to-batch variation, thereby improving the field emission properties of the cathode, such as emission current, turn-on voltage, and emission lifetime. Summary of the Invention
[0006] The above and other needs are met by aspects of the present disclosure, including, without limitation, the following exemplary embodiments, and in one particular aspect, a method of forming a field emission cathode with low surface roughness by using a sol-gel process, the method comprising: mixing a plurality of carbon nanotubes and an aqueous solution containing a water-stable conductive polymer (e.g., poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid)) in a specific ratio of carbon nanotubes to polymer solution (e.g., about 1:10 to about 10:1 by weight) to form a base mixture; and dispersing the base mixture using a powerful ultrasonic dispersion method (e.g., at 1 W / cm). 2and a frequency of about 20-50 kHz), introducing the metal oxide sol solution into the base mixture to form a field emission material precursor (i.e., a conditioned base mixture), and dispersing the field emission material precursor by gentle ultrasonic dispersion (e.g., at a power of 1 W / cm 2 the field emission material precursor to form a stable solution; introducing a polar additive into the stable solution of the field emission material precursor to form a final sol solution as the final field emission material precursor; depositing a layer of the final field emission material on at least a portion of the substrate; drying the layer and substrate at a temperature of about 30° C. to about 150° C. under air or vacuum; annealing the layer and substrate at a temperature of about 500° C. to about 1000° C. under vacuum to form the field emission material; and activating the field emission material to form a field emission cathode, thereby forming the field emission material.
[0007] Another exemplary embodiment provides a method for forming a field emission material precursor, the method including introducing a solution including a plurality of carbon nanotubes and a water stable conductive polymer (e.g., poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid)) into a liquid medium at a specific ratio of carbon nanotubes to polymer solution (e.g., about 1:10 to about 10:1 by weight); and subjecting the plurality of carbon nanotubes and the solution to powerful ultrasonic dispersion (e.g., at 1 W / cm 2 and a frequency of about 20-50 kHz) to form a base mixture; introducing a metal oxide sol solution into the base mixture to form a modified base mixture; and subjecting the modified base mixture including the metal oxide sol solution to gentle ultrasonic dispersion (e.g., at a power of 1 W / cm). 2 and a frequency greater than 50 kHz) to form a stable solution of the field emission material precursor; and introducing a polar additive into the stable solution of the field emission material precursor to form a final sol solution as the final field emission material precursor.
[0008] Another exemplary embodiment provides a method of forming a field emission cathode, the method including depositing a field emission material precursor (e.g., a final field emission material precursor) on at least a portion of a substrate, drying the field emission material and substrate under air or vacuum at a temperature of about 30° C. to about 150° C. such that the final field emission material precursor forms a layer on the substrate, annealing the final field emission material precursor layer and substrate under vacuum at a temperature of about 500° C. to about 1000° C. such that the layer forms a field emission material, and activating the field emission material to form the field emission cathode. These methods provide reduced cathode batch-to-batch variation in mass production processes.
[0009] Yet another exemplary embodiment provides a field emission cathode device, the field emission cathode being fabricated according to any one of the preceding embodiments to obtain a cathode device having improved density and uniformity of field emitters on the cathode surface, thereby resulting in a cathode device having improved field emission properties, such as high emission current, low turn-on voltage, and longer emission lifetime.
[0010] The present disclosure therefore includes, but is not limited to, the following exemplary embodiments:
[0011] Exemplary embodiment 1: A method of forming a field emission cathode, comprising: mixing a plurality of carbon nanotubes and a solution in a specific ratio to form a base mixture, the solution including a water-stable conductive polymer in a liquid medium; and providing a field emission cathode having a current density of 1 W / cm. 2 subjecting the base mixture to an ultrasonic dispersion process at a power of 1 W / cm and a frequency of 20-50 kHz; and introducing a metal oxide sol solution into the base mixture to form a field emission material precursor; 22. The method of claim 1, further comprising: subjecting a field emission material precursor to an ultrasonic dispersion process at a power of less than 1000 kHz and a frequency of more than 50 kHz to form a stable solution of the field emission material precursor; introducing a polar additive into the stable solution of the field emission material precursor to form a final sol solution as the final field emission material precursor; depositing a layer of the final field emission material precursor on at least a portion of a substrate; drying the layer of the final field emission material precursor and the substrate under air or vacuum at a temperature of 30° C. to 150° C. so that the layer of the final field emission material precursor forms a uniform gel layer on the substrate; annealing the gel layer and the substrate under vacuum at a temperature of 500° C. to 1000° C. so that the gel layer forms a field emission material; and activating the field emission material to form a field emission cathode.
[0012] Exemplary embodiment 2: The method of any preceding exemplary embodiment or combination thereof, wherein mixing the plurality of carbon nanotubes and the solution comprises mixing the plurality of carbon nanotubes with a solution comprising poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid) (PEDOT:PSS) polymer and a liquid medium.
[0013] Exemplary embodiment 3: The method of any preceding exemplary embodiment or combination thereof, wherein mixing the plurality of carbon nanotubes with the solution includes mixing the plurality of carbon nanotubes with the PEDOT:PSS solution such that a specific ratio of carbon nanotubes to PEDOT:PSS polymer solution is between 10:1 and 1:10 by weight.
[0014] Exemplary embodiment 4: The method of any preceding exemplary embodiment or combination thereof, wherein mixing the plurality of carbon nanotubes with the solution includes mixing the plurality of carbon nanotubes with the solution, wherein the liquid medium of the solution comprises water.
[0015] Exemplary embodiment 5: The method of any preceding exemplary embodiment or combination thereof, wherein depositing a layer of the final field emission material precursor on the substrate comprises depositing the layer on the substrate via dip coating, spin coating, air knife coating, gravure coating, slot die coating, inkjet printing, spray coating, Mayer bar coating, lithographic coating, flexographic coating, or a combination thereof.
[0016] Exemplary Embodiment 6: The method of any preceding exemplary embodiment or combination thereof, wherein introducing the metal oxide sol solution into the base mixture comprises introducing a metal oxide sol solution selected from the group consisting of aluminum oxide (Al2O3), silicon dioxide (SiO2), titanium dioxide (TiO2), zinc oxide (ZnO), magnesium oxide (MgO), barium oxide (BaO), lead dioxide (PbO2), zirconium dioxide (ZrO2), molybdenum dioxide (MoO2), copper oxide (CuO), vanadium pentoxide (VO5), tin dioxide (SnO2), indium tin oxide (ITO), indium zinc oxide (IZO), and aluminum zinc oxide (AZO), or combinations thereof.
[0017] Exemplary embodiment 7: The method of any preceding exemplary embodiment or combination thereof, wherein introducing a polar additive into the stable solution comprises introducing a polar additive selected from the group consisting of an alcohol, a polyol, ethylene glycol, glycerol, mesoerythritol, xylitol, and D-sorbitol, dimethylformamide (DMF), dimethylsulfoxide (DMSO), dimethylsulfone (DMSO2), N-methyl-2-pyrrolidone (NMP), an ionic liquid, or a combination thereof into the stable solution.
[0018] Exemplary embodiment 8: The method of any preceding exemplary embodiment or combination thereof, wherein depositing a layer of the final field emission material precursor on the substrate comprises depositing a layer of the final field emission material precursor on a substrate comprising a metal, stainless steel, alloy, conductive glass, or ceramic.
[0019] Exemplary embodiment 9: The method of any preceding exemplary embodiment or combination thereof, wherein activating the layer of field emitting material includes applying an adhesive tape to a surface of the field emitting material and removing the adhesive tape from the surface.
[0020] Exemplary embodiment 10: The method of any preceding exemplary embodiment or combination thereof, wherein activating the layer of field emitting material includes applying a curable adhesive to a surface of the field emitting material, exposing the adhesive to a heat source or ultraviolet light to cure the adhesive and form an adhesive film, and removing the adhesive film from the surface.
[0021] Exemplary embodiment 11: A method of forming a field emission material precursor, comprising: introducing a plurality of carbon nanotubes into a liquid medium; and introducing a water-stable conductive polymer into the liquid medium containing the plurality of carbon nanotubes, the plurality of carbon nanotubes being present in a specific ratio to a solution containing the liquid medium and the polymer; and providing a field emission efficiency of 1 W / cm. 2 mixing a plurality of carbon nanotubes and a water stable conductive polymer in a liquid medium via an ultrasonic dispersion process at a power of 1 W / cm and a frequency of 20-50 kHz to form a base mixture; introducing a metal oxide sol solution into the base mixture; 2 The method includes subjecting a base mixture including a metal oxide sol solution to an ultrasonic dispersion process at a power of less than 100 kHz and a frequency of more than 50 kHz to form a stable solution of a field emission material precursor, and introducing a polar additive into the stable solution of the field emission material precursor to form a final field emission material precursor.
[0022] Exemplary embodiment 12: The method of any preceding exemplary embodiment or combination thereof, wherein introducing the plurality of carbon nanotubes into a liquid medium comprises introducing the plurality of carbon nanotubes into water.
[0023] Exemplary embodiment 13: The method of any preceding exemplary embodiment or combination thereof, wherein introducing the water-stable conductive polymer comprises introducing a poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid) (PEDOT:PSS) polymer into the liquid medium.
[0024] Exemplary embodiment 14: The method of any preceding exemplary embodiment or combination thereof, wherein mixing the plurality of carbon nanotubes with the solution includes mixing the plurality of carbon nanotubes with the PEDOT:PSS solution such that a specific ratio of carbon nanotubes to PEDOT:PSS solution is between 10:1 and 1:10 by weight.
[0025] Exemplary Embodiment 15: The method of any preceding exemplary embodiment or combination thereof, wherein introducing the metal oxide sol solution into the base mixture comprises introducing a metal oxide sol solution selected from the group consisting of aluminum oxide (Al2O3), silicon dioxide (SiO2), titanium dioxide (TiO2), zinc oxide (ZnO), magnesium oxide (MgO), barium oxide (BaO), lead dioxide (PbO2), zirconium dioxide (ZrO2), molybdenum dioxide (MoO2), copper oxide (CuO), vanadium pentoxide (VO5), tin dioxide (SnO2), indium tin oxide (ITO), indium zinc oxide (IZO), an AZO compound, or a combination thereof.
[0026] Exemplary embodiment 16: The method of any preceding exemplary embodiment or combination thereof, wherein introducing a polar additive into the stable solution comprises introducing a polar additive selected from the group consisting of alcohol, polyol, ethylene glycol, glycerol, mesoerythritol, xylitol, and D-sorbitol, dimethylformamide (DMF), dimethylsulfoxide (DMSO), dimethylsulfone (DMSO2), N-methyl-2-pyrrolidone (NMP), ionic liquid, or combinations thereof into the stable solution.
[0027] Exemplary embodiment 17: A method of forming a field emission cathode, comprising: depositing a final field emission material precursor on at least a portion of a substrate according to a method described in any preceding exemplary embodiment or a combination thereof; drying the final field emission material precursor and substrate under air or vacuum at a temperature between 30°C and 150°C such that the final field emission material precursor forms a layer on the substrate; annealing the layer and substrate under vacuum at a temperature between 500°C and 1000°C such that the layer forms a field emission material; and activating the field emission material to form the field emission cathode.
[0028] Exemplary embodiment 18: The method of any preceding exemplary embodiment or combination thereof, wherein depositing a final field emission material precursor on at least a portion of the substrate comprises depositing a final field emission material precursor on at least a portion of the substrate comprising a metal, stainless steel, alloy, conductive glass, or ceramic.
[0029] Exemplary embodiment 19: The method according to any preceding exemplary embodiment or combination thereof, wherein depositing the final field emission material precursor on at least a portion of the substrate comprises depositing the final field emission material precursor on at least a portion of the substrate via dip coating, spin coating, air knife coating, gravure coating, slot die coating, inkjet printing, spray coating, Mayer bar coating, lithographic coating, flexographic coating, or a combination thereof.
[0030] Exemplary embodiment 20: The method of any preceding exemplary embodiment or combination thereof, wherein activating the field emitting material includes applying an adhesive tape to a surface of the field emitting material and removing the adhesive tape from the field emitting material.
[0031] Exemplary embodiment 21: The method of any preceding exemplary embodiment or combination thereof, wherein activating the field emission material includes applying a curable adhesive to a surface of the field emission material, exposing the adhesive to a heat source or ultraviolet light to cure the adhesive and form an adhesive film, and removing the adhesive film from the surface.
[0032] Exemplary embodiment 22: A field emission cathode device comprising a field emission cathode made according to the method of any preceding exemplary embodiment or a combination thereof.
[0033] These and other features, aspects, and advantages of the present disclosure will become apparent upon reading the following detailed description in conjunction with the accompanying drawings, which are briefly described below. The present disclosure includes any combination of two, three, four, or more features or elements described in the present disclosure, regardless of whether such features or elements are explicitly combined in the description of a particular embodiment herein or otherwise described. The present disclosure is intended to be read holistically, whereby any separate features or elements of the present disclosure should be considered as intended, i.e., combinable, in any of its aspects and embodiments, unless the context of the present disclosure clearly indicates otherwise.
[0034] It will be understood that the summary of this specification is provided merely for the purpose of summarizing some exemplary aspects to provide a basic understanding of the present disclosure. Therefore, it will be understood that the above exemplary aspects are merely examples and should not be interpreted in any way as narrowing the scope or spirit of the present disclosure. It will be understood that the scope of the present disclosure encompasses many potential aspects, some of which will be further described below in addition to those summarized herein. Furthermore, other aspects and advantages of such aspects disclosed herein will become apparent from the following detailed description taken in conjunction with the accompanying drawings, which illustrate by way of example the principles of the described aspects.
[0035] Having thus described the disclosure in general terms, reference is now made to the accompanying drawings, which are not necessarily drawn to scale. [Brief description of the drawings]
[0036] [Figure 1] 1A-1C are schematic diagrams illustrating examples of the nature of a field emission material deposition layer engaged with a field emission cathode and a cathode substrate, according to one or more embodiments of the present disclosure. [Diagram 2] 1 illustrates an example method of forming a field emission material precursor according to one or more embodiments of the present disclosure. [Diagram 3] 1 illustrates an example method of forming a field emission cathode according to one or more embodiments of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0037] Detailed Description of the Disclosure The present disclosure will now be described more fully hereinafter with reference to the accompanying drawings, in which some, but not all, aspects of the present disclosure are shown. Indeed, the present disclosure may be embodied in many different forms and should not be construed as limited to the aspects set forth herein, but rather, these aspects are provided so that this disclosure will satisfy applicable legal requirements. Like numbers refer to like elements throughout.
[0038] FIG. 1 shows an example of a field emission cathode 100 including a substrate 102 and a layer of a field emission material 104 disposed on the substrate 102, and optionally an additional layer of an adhesive material (not shown) disposed between the substrate 102 and the field emission material 104. The substrate 102 may be made of a conductive material, such as a metallic material, such as a solid metal or alloy (e.g., stainless steel, doped silicon), a conductive glass (e.g., indium tin oxide (ITO) coated glass or other molten glass having a conductive coating on its surface), or a conductive ceramic (e.g., a metallized ceramic, such as aluminum oxide, beryllium oxide, and aluminum nitride). The field emission material 104 includes a plurality of carbon nanotubes (CNTs) disposed within a matrix material. A typical CNT / matrix field emission material has a high surface roughness, for example, a surface including emitters disposed in layers of different heights across the surface of the cathode, and a mixture of emitters disposed in layers of lower heights, because many unattached particles are not removed therefrom during the activation process.
[0039] Forming a layer of field emission material 104' through a sol-gel process and incorporating a metal oxide sol solution results in a gel layer of CNT / PEDOT:PSS / metal oxide matrix in a nanometer composite structure, which is uniform in texture and is formed on the surface of the substrate 102. After drying, annealing, and activation, a field emission cathode is obtained with a less rough field emission material layer and high emitter density, high emission current, low turn-on voltage, and long life characteristics. In particular, incorporating a metal oxide sol solution instead of matrix particles results in a homogenous precursor solution that can be deposited on the substrate surface. The deposition of the field emission material on the substrate 102 can be performed through any of the coating processes disclosed herein. After activation, the surface of the cathode has a low surface roughness (e.g., the emitter height is less variable and most of the non-adhered particles have been removed). Two layers (high roughness layer 104 and low roughness layer 104') are shown in FIG. 1 for comparison.
[0040] Thus, the cathode has improved field emission properties with high density and uniformity of emitters as well as low batch-to-batch variation that can meet the requirements of mass production for industrial applications. FIG. 2 illustrates a method 200 for forming a field emission material precursor including carbon nanotubes and metal oxide. In one aspect of the method, a liquid medium such as water is provided (step 210) into which a plurality of carbon nanotubes and a poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid) (PEDOT:PSS) polymer are introduced in a specific ratio, such as a ratio of a plurality of carbon nanotubes to a solution including liquid medium and polymer ranging from about 10:1 to about 1:10 by weight (step 220). In some embodiments, other liquid media including water-stable conductive polymers may be used. In step 230, the solution of the plurality of carbon nanotubes and PEDOT:PSS is mixed via a strong ultrasonic dispersion process to form a base mixture. The mixing was performed at low frequency (20-50 kHz) and high power (>1 W / cm) for a period ranging from about 1 min to about 30 min. 2). A metal oxide sol solution is then introduced into the base mixture (step 240) to form a conditioned base mixture. The conditioned base mixture (i.e., including the metal oxide sol) is subjected to a mild ultrasonic dispersion process to form a stable solution of the field emission material precursor (i.e., a homogenous precursor sol) (step 250). The mild ultrasonic dispersion process is performed using high frequency (>50 kHz) and low power (<1 W / cm 2 ) for a period ranging from about 30 minutes to about 24 hours. At step 260, a polar additive is introduced into the stable solution to form a final sol solution as the final field emission material precursor. In various embodiments, the final field emission material precursor may include carbon nanotubes, PEDOT:PSS, a metal oxide sol, and one or more additives.
[0041] The specific composition and amounts of components may vary to suit a particular application. For example, in some embodiments, the metal oxide sol solution may include, for example, aluminum oxide (Al2O3), silicon dioxide (SiO2), titanium dioxide (TiO2), zinc oxide (ZnO), magnesium oxide (MgO), barium oxide (BaO), lead dioxide (PbO2), zirconium dioxide (ZrO2), molybdenum dioxide (MoO2), copper oxide (CuO), vanadium pentoxide (VO5), tin dioxide (SnO2), indium tin oxide (ITO), indium zinc oxide (IZO), and aluminum zinc oxide (AZO). The metal oxide sol may be dispersed in the base mixture at about 0.1 wt% to about 20 wt% of the total liquid medium. In various embodiments, the polar additive may include one or more of alcohols, polyols such as ethylene glycol, glycerol, mesoerythritol, xylitol, and D-sorbitol, dimethylformamide (DMF), dimethylsulfoxide (DMSO), dimethylsulfone (DMSO2), N-methyl-2-pyrrolidone (NMP), ionic liquids, or combinations thereof. The concentration of the polar additive may be from about 0.1 wt% to about 20 wt% of the total liquid medium. Carbon nanotubes may be produced by chemical vapor deposition processes, laser ablation processes, and / or arc discharge methods.
[0042] Once the final field emission material precursor is formulated in a stable sol solution, the final field emission material precursor may be deposited on at least a portion of a substrate (step 270). A layer of the final field emission material precursor is deposited on the substrate via dip coating, spin coating, air knife coating, gravure coating, slot die coating, inkjet printing, spray coating, Mayer bar coating, lithographic coating, flexographic coating, or a combination thereof. The substrate may include metal, stainless steel, alloy, conductive glass, or ceramic. The substrate may be provided to a suitable facility, for example, via a robotic material handling system or manually by a user. The substrate is configured to receive a layer of the final field emission material precursor thereon.
[0043] The sol layer may be subjected to one or more other processes after deposition on the substrate, such as drying, annealing, and activation processes. After drying, a uniform gel layer of CNT / PEDOT:PSS / metal oxide matrix material is formed from the sol layer on the substrate surface, which is then annealed. The field emission cathode is formed after activating the deposited layer on the substrate to form a field emission material.
[0044] FIG. 3 illustrates a method 300 for forming a field emission cathode using a field emission material including carbon nanotubes and metal oxides. In one embodiment of the method, a substrate such as those described above is provided to equipment configured for performing a deposition process (step 310). The method further includes forming a field emission material from a field emission material precursor (step 320). In some cases, the field emission material is created as a field emission material precursor before the substrate is provided, for example, as a final field emission material precursor disclosed herein. A layer of the final field emission material precursor is deposited on at least a portion of the substrate (step 330). The substrate may be made of a metal such as stainless steel, an alloy, a conductive glass, or a metallized ceramic. The substrate may be provided to a suitable equipment, for example, via a robotic material handling system or manually by a user.
[0045] The substrate and the layer of the final field emission material precursor deposited thereon are then subjected to a drying process (step 340) and an annealing process (step 350) to form the field emission material. The drying process may be performed at a temperature of about 30°C to about 150°C under air or vacuum. The annealing process may be performed at a temperature of about 500°C to about 1000°C under vacuum. In step 360, the layer of field emission material is activated to obtain a field emission cathode. The activation may be performed by applying an adhesive (e.g., an adhesive tape or a curable adhesive material) to the surface of the layer of field emission material and removing the adhesive from the layer of field emission material.
[0046] Step 370 illustrates one example of a method for forming a field emission material precursor. In step 370, a plurality of carbon nanotubes and a PEDOT:PSS polymer are mixed in a liquid medium, such as water, in a specific ratio (e.g., about 1:10 to about 10:1 by weight) of the plurality of carbon nanotubes to the solution including the liquid medium and the polymer. The components can be mixed via a strong ultrasonic dispersion process to form a base mixture, as described above. A metal oxide sol solution is then dispersed in the base mixture. The adjusted base mixture can be subjected to a gentle ultrasonic dispersion process, as described above, to form a stable suspension of the field emission material precursor. A polar additive is then added to the stable solution to form a final sol solution as the final field emission material precursor. In various embodiments, the final field emission material precursor can include carbon nanotubes, PEDOT:PSS, a metal oxide sol, and one or more additives.
[0047] The specific composition and amounts of components may vary to suit a particular application. For example, in some embodiments, the metal oxide sol solution may include, for example, aluminum oxide (Al2O3), silicon dioxide (SiO2), titanium dioxide (TiO2), zinc oxide (ZnO), magnesium oxide (MgO), barium oxide (BaO), lead dioxide (PbO2), zirconium dioxide (ZrO2), molybdenum dioxide (MoO2), copper oxide (CuO), vanadium pentoxide (VO5), tin dioxide (SnO2), indium tin oxide (ITO), indium zinc oxide (IZO), AZO compounds, or combinations thereof. The metal oxide sol may be dispersed in the base mixture at about 0.1 wt% to about 20 wt% of the total liquid medium. In various embodiments, the polar additive may include one or more of alcohols, polyols such as ethylene glycol, glycerol, mesoerythritol, xylitol, and D-sorbitol, dimethylformamide (DMF), dimethylsulfoxide (DMSO), dimethylsulfone (DMSO2), N-methyl-2-pyrrolidone (NMP), ionic liquids, or combinations thereof. The concentration of the polar additive may be from about 0.1 wt% to about 20 wt% of the total liquid medium. Carbon nanotubes may be produced by chemical vapor deposition processes, laser ablation processes, and / or arc discharge methods.
[0048] The aforementioned method provides a nanometer composite structured CNT / PEDOT:PSS / metal oxide matrix material layer, which is uniform in texture when formed on the surface of the substrate. After drying and annealing under vacuum, the resulting field emission cathode is activated. The formed field emission material layer of the cathode has the properties of low surface roughness, high emitter density, high emission current, low turn-on voltage, and long life. The batch-to-batch variation of the cathode is significantly reduced, which is important for industrialized production and applications.
[0049] Many modifications and other embodiments of the invention described herein will occur to those skilled in the art to which these disclosed embodiments pertain with the benefit of the teachings presented in the foregoing description and the associated drawings. It should therefore be understood that the embodiments of the invention are not limited to the specific embodiments disclosed, and that modifications and other embodiments are intended to be included within the scope of the invention. Furthermore, while the foregoing description and the associated drawings describe exemplary embodiments related to certain exemplary combinations of elements and / or functions, it should be understood that different combinations of elements and / or functions may be provided by alternative embodiments without departing from the scope of the disclosure. In this regard, for example, combinations of elements and / or functions different from those explicitly described above are also contemplated to be within the scope of the disclosure. Although specific terms have been employed herein, they are used in a generic and descriptive sense only and not for purposes of limitation.
[0050] Terms such as first, second, etc. may be used herein to describe various steps or calculations, but it should be understood that these steps or calculations should not be limited by these terms. These terms are used only to distinguish one operation or calculation from another. For example, a first calculation may be referred to as a second calculation, and similarly, a second step may be referred to as a first step, without departing from the scope of this disclosure. As used herein, the term "and / or" and the " / " symbol include any and all combinations of one or more of the associated listed items.
[0051] As used herein, the singular forms "a," "an," and "the" are intended to include the plural forms unless the context clearly dictates otherwise. It will be further understood that the terms "comprises," "comprising," "includes," and / or "including," as used herein, specify the presence of stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof. Thus, the terminology used herein is merely for the purpose of describing particular embodiments and is not intended to be limiting.
Claims
1. 1. A method of forming a field emission cathode, comprising the steps of: mixing a plurality of carbon nanotubes and a solution in a specific ratio to form a base mixture, the solution comprising a water-stable conductive polymer in a liquid medium; 1 W / cm 2 subjecting said base mixture to an ultrasonic dispersion process at a power of 1000 Hz and a frequency of 20-50 kHz; introducing a metal oxide sol solution into the base mixture to form a field emission material precursor; 1 W / cm to form a stable solution of the field emission material precursor. 2 subjecting said field emission material precursor to an ultrasonic dispersion process at a power of less than 1000 Hz and at a frequency of more than 50 kHz; introducing a polar additive into the stable solution of the field emission material precursor to form a final sol solution as a final field emission material precursor; depositing a layer of said final field emission material precursor over at least a portion of a substrate; drying the layer of final field emission material precursor and the substrate at a temperature between 30° C. and 150° C. under air or vacuum so that the layer of final field emission material precursor forms a uniform gel layer on the substrate; annealing the gel layer and the substrate at a temperature between 500° C. and 1000° C. under vacuum so that the gel layer forms a field emission material; activating the field emission material to form the field emission cathode. A method comprising:
2. 2. The method of claim 1, wherein mixing the plurality of carbon nanotubes with the solution comprises mixing the plurality of carbon nanotubes with the solution comprising poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid) (PEDOT:PSS) polymer and the liquid medium.
3. 3. The method of claim 2, wherein mixing the plurality of carbon nanotubes with the solution comprises mixing the plurality of carbon nanotubes with the PEDOT:PSS solution such that the specified ratio of carbon nanotubes to PEDOT:PSS polymer solution is between 10:1 and 1:10 by weight.
4. The method of claim 1 , wherein mixing the plurality of carbon nanotubes with the solution comprises mixing the plurality of carbon nanotubes with the solution, the liquid medium of the solution comprising water.
5. 10. The method of claim 1, wherein depositing the layer of the final field emission material precursor on the substrate comprises depositing the layer on the substrate via dip coating, spin coating, air knife coating, gravure coating, slot die coating, inkjet printing, spray coating, Mayer bar coating, lithographic coating, flexographic coating, or combinations thereof.
6. Introducing the metal oxide sol solution into the base mixture comprises introducing aluminum oxide (Al 2 O 3 ), silicon dioxide (SiO 2 ), titanium dioxide (TiO 2 ), zinc oxide (ZnO), magnesium oxide (MgO), barium oxide (BaO), lead dioxide (PbO 2 ), zirconium dioxide (ZrO 2 ), molybdenum dioxide (MoO 2 ), copper oxide (CuO), vanadium pentoxide (V 2 O 5 ), tin dioxide (SnO 2 2. The method of claim 1, comprising introducing the metal oxide sol solution selected from the group consisting of: indium tin oxide (ITO), indium zinc oxide (IZO), and aluminum zinc oxide (AZO), or combinations thereof.
7. Introducing the polar additive into the stable solution includes introducing into the stable solution an alcohol, a polyol, ethylene glycol, glycerol, mesoerythritol, xylitol, and D-sorbitol, dimethylformamide (DMF), dimethylsulfoxide (DMSO), dimethylsulfone (DMSO 2 2. The method of claim 1, comprising introducing said polar additive selected from the group consisting of: N-methyl-2-pyrrolidone (NMP), an ionic liquid, or a combination thereof.
8. 10. The method of claim 1 , wherein depositing the layer of the final field emission material precursor on the substrate comprises depositing the layer of the final field emission material precursor on the substrate comprising a metal, stainless steel, alloy, conductive glass, or ceramic.
9. activating the layer of field emission material includes: applying an adhesive tape to a surface of said field emission material; removing the adhesive tape from the surface; The method of claim 1 , comprising:
10. activating the layer of field emission material includes: applying a curable adhesive to a surface of the field emission material; exposing the adhesive to a heat source or ultraviolet light to cure the adhesive and form the adhesive into an adhesive film; removing the adhesive film from the surface; The method of claim 1 , comprising:
11. 1. A method of forming a field emission material precursor, comprising: Introducing a plurality of carbon nanotubes into a liquid medium; introducing a water-stable conductive polymer into the liquid medium containing the plurality of carbon nanotubes, the plurality of carbon nanotubes being present in a specific ratio relative to the liquid medium and the solution containing the polymer; 1 W / cm to form the base mixture 2 mixing the plurality of carbon nanotubes and the water-stable conductive polymer in the liquid medium via an ultrasonic dispersion process at a power of 1000 Hz and a frequency of 20-50 kHz; introducing a metal oxide sol solution into the base mixture; 1 W / cm to form a stable solution of the field emission material precursor 2 subjecting the base mixture containing the metal oxide sol solution to an ultrasonic dispersion process at a power of less than 1000 Hz and a frequency of more than 50 kHz; introducing a polar additive into said stable solution of said field emission material precursor to form a final field emission material precursor; A method comprising:
12. The method of claim 11 , wherein introducing the plurality of carbon nanotubes into the liquid medium comprises introducing the plurality of carbon nanotubes into water.
13. 12. The method of claim 11, wherein the introducing a water stable conductive polymer comprises introducing a poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonic acid) (PEDOT:PSS) polymer into the liquid medium.
14. 14. The method of claim 13, wherein mixing the plurality of carbon nanotubes with the solution comprises mixing the plurality of carbon nanotubes with the PEDOT:PSS solution such that the specified ratio of carbon nanotubes to PEDOT:PSS solution is between 10:1 and 1:10 by weight.
15. Introducing the metal oxide sol solution into the base mixture comprises introducing aluminum oxide (Al 2 O 3 ), silicon dioxide (SiO 2 ), titanium dioxide (TiO 2 ), zinc oxide (ZnO), magnesium oxide (MgO), barium oxide (BaO), lead dioxide (PbO 2 ), zirconium dioxide (ZrO 2 ), molybdenum dioxide (MoO 2 ), copper oxide (CuO), vanadium pentoxide (V 2 O 5 ), tin dioxide (SnO 2 12. The method of claim 11, comprising introducing the metal oxide sol solution selected from the group consisting of: indium tin oxide (ITO), indium zinc oxide (IZO), an AZO compound, or a combination thereof.
16. Introducing the polar additive into the stable solution includes introducing into the stable solution an alcohol, a polyol, ethylene glycol, glycerol, mesoerythritol, xylitol, and D-sorbitol, dimethylformamide (DMF), dimethylsulfoxide (DMSO), dimethylsulfone (DMSO 2 12. The method of claim 11, comprising introducing the polar additive selected from the group consisting of: N-methyl-2-pyrrolidone (NMP), an ionic liquid, or a combination thereof.
17. 1. A method of forming a field emission cathode, comprising the steps of: depositing the final field emission material precursor of claim 11 on at least a portion of a substrate; drying the final field emission material precursor and the substrate at a temperature between 30° C. and 150° C. under air or vacuum so that the final field emission material precursor forms a layer on the substrate; annealing the layer and the substrate at a temperature between 500° C. and 1000° C. under vacuum so that the layer forms a field emission material; activating the field emission material to form the field emission cathode; A method comprising:
18. 20. The method of claim 17, wherein depositing the final field emission material precursor onto the at least a portion of the substrate comprises depositing the final field emission material precursor onto the at least a portion of the substrate comprising a metal, stainless steel, alloy, conductive glass, or ceramic.
19. 20. The method of claim 17, wherein depositing the final field emission material precursor onto the at least a portion of the substrate comprises depositing the final field emission material precursor onto the at least a portion of the substrate via dip coating, spin coating, air knife coating, gravure coating, slot die coating, inkjet printing, spray coating, Mayer bar coating, lithographic coating, flexographic coating, or combinations thereof.
20. activating the field emission material includes applying an adhesive tape to a surface of said field emission material; removing the adhesive tape from the field emission material; 20. The method of claim 17, comprising:
21. activating the field emission material includes applying a curable adhesive to a surface of the field emission material; exposing the adhesive to a heat source or ultraviolet light to cure the adhesive and form the adhesive into an adhesive film; removing the adhesive film from the surface; 20. The method of claim 17, comprising:
Citation Information
Patent Citations
Conductive polymer composition and film made therefrom
JP2011517468A
Field emission devices including nanotubes or other nanoscale articles
US20130113359A1