Inspection method for optical laminated film and manufacturing method for film product

The method for inspecting optical laminated films by distinguishing between peeling-visible and non-peeling defects through distinct marks addresses the issue of mistakenly marking normal products as defective, ensuring efficient production by preventing defective products from shipment and improving yield.

JP7594917B2Active Publication Date: 2024-12-05NITTO DENKO CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2021002359
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-08
Publication Date
2024-12-05
Estimated Expiration
2041-01-08

AI Technical Summary

Technical Problem

Existing methods for inspecting optical laminated films often mistakenly mark normal products as defective due to high defect detection standards, leading to inefficiencies in production and potential shipment of defective products.

Method used

A method for inspecting optical laminated films that distinguishes between peeling-visible defects and non-peeling defects by using distinct marks, allowing for re-inspection of products without peeling off the surface protection or separator films, and grouping products based on these marks to improve production efficiency.

Benefits of technology

This approach effectively separates normal and defective products, preventing defective products from reaching the market while enhancing production efficiency by allowing re-inspection of marked products without film peeling, thus improving yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007594917000001
    Figure 0007594917000001
  • Figure 0007594917000002
    Figure 0007594917000002
  • Figure 0007594917000003
    Figure 0007594917000003
Patent Text Reader

Abstract

To increase production efficiency while removing defective products.SOLUTION: A method for inspecting an optical laminate film includes the steps of: inspecting a defect in the process of manufacturing an optical laminate film 1a having an optical film 11a, a surface protective film, and a separator film; and applying a mark corresponding to the detected defect to the optical laminate film. A defect revealed upon peeling that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film 1a, and a defect other than the defect revealed upon peeling are distinguished from each other. A first mark 71 corresponding to the defect revealed upon peeling is applied to the optical laminate film 1a, and a second mark 72 corresponding to the defect other than the defect revealed upon peeling, the mark different in pattern from the first mark 71 is applied to the optical laminate film 1a.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for inspecting an optical laminate film including an optical film. [Background technology]

[0002] 2. Description of the Related Art Optical films are used in a variety of applications, including image display devices such as liquid crystal displays and organic EL displays, as well as applications other than image display devices, such as polarized sunglasses and light-control windows. Such optical films are processed into film products having a predetermined planar shape so as to conform to the specifications of the screen of the image display device. In addition, in order to attach the optical film to the screen of the image display device, an adhesive layer may be provided on the back surface of the optical film. In this case, a separator film is attached to conceal the adhesive layer. In addition, a surface protection film is generally attached to the surface of the optical film to protect the product. In the industrial production process, a long strip of optical laminate film (surface protection film / optical film / separator film) is manufactured, and a plurality of sheet-like film products are cut out from the optical laminate film, thereby obtaining the film products.

[0003] In the process of producing the optical laminate film, the film is inspected for defects. For example, Patent Document 1 discloses that in the process of transporting a long strip of film, defects in the film are detected by optical inspection, and the defective portions are marked in predetermined ranges on both sides in the width direction. The inspected film is then cut to form a plurality of products. Of the resulting plurality of products, products with marks are discarded as defective products, and products without marks are shipped as normal products. In this way, quality control is performed to prevent defective products from being shipped. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2001-305070 A Summary of the Invention

[0005] However, some of the products bearing the mark may be normal. For example, when mechanical inspection is performed during the manufacturing process of the optical laminate film, the standard (threshold) for defect detection is often set high in order to reliably eliminate defective products. In that case, products that should be evaluated as not having defects may be marked as having defects due to the high standard. Therefore, rather than uniformly discarding products bearing the mark, it is preferable to reinspect the products and separate them into normal products and defective products in order to improve production efficiency (so-called yield improvement). However, according to the research of the present inventor, when a product made of the optical laminate film is re-inspected from the outside, for example, defects in the optical film may not be detected. It is necessary to avoid the re-inspection from being used to ship a defective product as a normal product. [Problem to be solved by the invention]

[0006] An object of the present invention is to provide an inspection method for an optical laminate film and a manufacturing method for a film product, which can improve production efficiency while eliminating defective products. [Means for solving the problem]

[0007] The present invention Film product manufacturing The method includes, during the process of manufacturing an optical laminate film having an optical film, a surface protective film attached to the front surface of the optical film, and a separator film attached to the back surface of the optical film, an inspection step of inspecting the optical film for defects, and a marking step of attaching a mark corresponding to the defect detected by the inspection to the optical laminate film. After the marking step, a step of cutting out a plurality of film products from the optical laminate film, and a step of grouping the obtained plurality of film products;In the inspection step, a peeling manifestation defect that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film is distinguished from a defect other than the peeling manifestation defect, and in the marking step, a first mark corresponding to the peeling manifestation defect is applied to the optical laminate film, and a second mark corresponding to the defect other than the peeling manifestation defect and having a pattern different from that of the first mark is applied to the optical laminate film. In the grouping step, film products bearing the first mark are grouped into a first group, film products bearing the second mark are grouped into a second group, and film products bearing neither the first mark nor the second mark are grouped into a third group, and the film products in the first group are treated as defective products, and the film products in the second group are reinspected, and film products that pass the reinspection are treated as normal products. .

[0008] The preferred embodiment of the present invention manufacturing The method is such that the first mark and the second mark are each composed of two or more dots arranged in a substantially straight line along the transport direction of the optical laminated film, the first mark includes two or more dots arranged with a spacing smaller than the diameter of one dot, and the second mark does not include two or more dots arranged with a spacing smaller than the diameter of one dot. The preferred embodiment of the present invention manufacturing The method is such that the first mark and the second mark are each composed of two or more dots arranged in a substantially straight line along the transport direction of the optical laminated film, and the dots constituting the first mark and the dots constituting the second mark have different shapes. The preferred embodiment of the present invention manufacturing In the method, the peel-evident defect is a defect that has occurred in the optical film before the surface protective film and the separator film are attached. A preferred inspection method of the present invention includes a peeling evident defect that can be detected by peeling the surface protection film from the optical laminate film, and a peeling evident defect that can be detected by peeling the separator film from the optical laminate film. The preferred embodiment of the present invention manufacturing In the method, the pattern of the first marks corresponding to the peel-evealing defects detectable by peeling the surface protective film is different from the pattern of the first marks corresponding to the peel-evealing defects detectable by peeling the separator film.

[0009] According to another aspect of the present invention, Inspection method for optical laminated film to provide. The present invention Inspection method for optical laminated film teeth, The present invention relates to a method for manufacturing an optical laminate film having an optical film, a surface protective film attached to the front surface of the optical film, and a separator film attached to the back surface of the optical film, the method comprising: an inspection step of inspecting defects in the optical film; and a marking step of applying a mark to the optical laminate film corresponding to the defect detected by the inspection, the method comprising: a step of distinguishing between peel-evealing defects that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film in the inspection step and defects other than the peel-evealing defects, and applying the marking step to the optical laminate film. In the process, a first mark corresponding to the peeling manifestation defect is applied to the optical laminated film, and a second mark corresponding to a defect other than the peeling manifestation defect and having a pattern different from that of the first mark is applied to the optical laminated film, the first mark and the second mark are each composed of two or more dots arranged in an approximately straight line along the conveying direction of the optical laminated film, the first mark includes two or more dots arranged at intervals smaller than the diameter of one dot, and the second mark does not include two or more dots arranged at intervals smaller than the diameter of one dot. Effect of the Invention

[0011] The method of the present invention attaches a first mark corresponding to a peeling manifestation defect, and attaches a second mark corresponding to a defect other than the peeling manifestation defect, the second mark having a different pattern from the first mark. Since a film product with the second mark can be inspected for defects without peeling the film, the film product can be reinspected and separated into normal products and defective products. According to the present invention, it is possible to improve the production efficiency of film products while preventing defective products from being provided to the market. [Brief description of the drawings]

[0012] [Figure 1] FIG. 2 is a side view showing an example of a layer structure of the optical laminate film. [Diagram 2] FIG. 4 is a side view showing another example of the layer structure of the optical laminate film. [Diagram 3] 1 is a schematic side view of a system for implementing the inspection direction and manufacturing method of the present invention; [Figure 4] FIG. 2 is a schematic plan view of the system as seen from the front side. [Diagram 5] FIG. 13 is a reference perspective view for explaining a procedure for detecting defects and identifying defective locations in a pre-process. [Figure 6] FIG. 4 is a plan view showing an example of a first mark corresponding to a defect that can be detected by peeling off a surface protection film. [Figure 7] FIG. 13 is a plan view showing an example of a first mark corresponding to a defect that can be detected by peeling off a separator film. [Figure 8] FIG. 13 is a plan view showing an example of a second mark corresponding to a defect other than a peeling manifestation defect. [Figure 9] FIG. 11 is a plan view showing another example of a first mark corresponding to a defect that can be detected by peeling off a surface protection film. [Figure 10] FIG. 11 is a reference plan view showing the state when cut across the first mark. [Figure 11] FIG. 11 is a reference plan view for conceptually explaining a method for setting a mark pattern. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] In this specification, the prefixes 1, 2, 1-A, 1-B, etc. may be added to terms, but these 1, etc. are added only to distinguish between two or more terms and do not have any special meaning such as the order, superiority, or shape of those terms. In addition, in this specification, the expression "approximately" means that it includes the range acceptable in the technical field of the present invention.

[0014] [Optical laminate film] The optical laminated film has an optical film, a surface protective film attached to the surface of the optical film, and a separator film attached to the back surface of the optical film. The surface protective film is attached to the surface of the optical film in a state in which it can be peeled off by human force. That is, the surface protective film can be peeled off from the optical film by pinching it with fingertips or the like and peeling it off. The surface protective film is usually attached to the optical film via a pressure-sensitive adhesive layer. When the pressure-sensitive adhesive layer is included, peeling occurs between the optical film and the pressure-sensitive adhesive layer, and the surface protective film is peeled off together with the pressure-sensitive adhesive layer. In addition, when the surface protective film and the optical film are made of materials that can be bonded to each other, the surface protective film may be directly attached to the surface of the optical film. The separator film is attached to the back surface of the optical film via a pressure-sensitive adhesive layer in a state in which it can be peeled off by human force. That is, the separator film can be peeled off from the optical film by pinching it with fingertips or the like and peeling it off. In this case, peeling occurs between the separator film and the pressure-sensitive adhesive layer, and only the separator film is peeled off while the pressure-sensitive adhesive layer remains laminated on the back surface of the optical film.

[0015] FIG. 1 shows one example of the layer structure of the optical laminate film, and FIG. 2 shows another example of the layer structure of the optical laminate film. Referring to FIG. 1, the optical laminated film 1 has, in order from the front surface side, a surface protective film 12, a pressure-sensitive adhesive layer 14, an optical film 11, a pressure-sensitive adhesive layer 15, and a separator film 13. The pressure-sensitive adhesive layer 14 is firmly attached to the surface protective film 12 and is releasably attached to the optical film 11. The pressure-sensitive adhesive layer 15 is firmly attached to the optical film 11 and is releasably attached to the separator film 13. The optical film 11 includes an optically functional film. The optical film 11 may include two or more layers of optically functional films, or may be composed of only one layer of optically functional film. In addition, any treatment such as an anti-reflection treatment may be applied to the front surface and / or rear surface of the optical film 11. For example, an anti-reflection layer may be formed by applying an anti-reflection coating to the front surface of the optical film 11.

[0016] Referring to FIG. 2, in another optical laminate film 1, the optical film 11 has two or more kinds of optical functional films. For example, the optical film 11 has first to third optical functional films 111, 112, and 113. The first optical functional film 111 may be, for example, an anti-reflection film, the second optical functional film 112 may be, for example, a polarizing film, and the third optical functional film 113 may be, for example, a retardation film. The surface protective film 12 is releasably attached to the surface of the optical film 11 (in the illustrated example, the first optical functional film 111) via the adhesive layer 14, as described above. In addition, the separator film 13 is releasably attached to the back surface of the optical film 11 (in the illustrated example, the third optical functional film 113) via the adhesive layer 15, as described above. In FIG. 2, the first to third optical function films 111, 112, and 113 are directly bonded to each other, but they may be bonded to each other via an adhesive layer (not shown) between these layers. The optical laminate film 1 is not limited to the layer configuration shown in FIG. 1 and FIG. 2, and can be modified in various ways.

[0017] <Optical film> As described above, the optical film 11 includes an optically functional film. Examples of the optically functional film include a polarizing film, a retardation film, an anti-reflection film, a light diffusion film, a brightness enhancing film, a light reflecting film, and a protective film. The polarizing film is a film that transmits light (polarized light) that vibrates in a specific direction and blocks light that vibrates in other directions. The retardation film is a film that exhibits optical anisotropy, and representative examples include stretched films of acrylic resins, cycloolefin resins, cellulose resins, and the like. As the protective film, a substantially isotropic, colorless, and transparent film is preferably used. For example, the optical film 11 of the optical laminate film 1 illustrated in FIG. 1 has, in order from the front surface side, a first protective film 114, a polarizing film 115, and a second protective film .

[0018] <Surface protection film> The surface protection film 12 is attached to protect the surface of the optical film 11. The surface protection film is usually peeled off appropriately when the film product is used. The surface protection film is preferably a substantially isotropic colorless transparent film. As such a surface protection film, for example, a polyester-based resin such as polyethylene terephthalate or polyethylene naphthalate; a cellulose-based resin such as triacetyl cellulose; a polycarbonate-based resin; an acrylic resin such as polymethyl methacrylate; a styrene-based resin such as polystyrene; an olefin-based resin such as polyethylene or a polyolefin having a cyclic or norbornene structure; a vinyl chloride-based resin; an amide-based resin such as nylon 6; an imide-based resin; a sulfone-based resin; a vinyl alcohol-based resin; a vinylidene chloride-based resin; a vinyl butyral-based resin; an arylate-based resin; a polyoxymethylene-based resin; or the like can be used as the main resin component. The resin film may contain two or more kinds of resins. Among them, it is preferable to use a polyester-based film as the surface protection film because of its excellent optical properties and dimensional stability. The polyester-based film is a film containing, as a main resin component, a resin material having an ester bond, such as polyethylene terephthalate, polyethylene naphthalate, polybutylene terephthalate, etc. The surface protection film may be subjected to an antistatic treatment. The thickness of the surface protection film is not particularly limited and is, for example, 10 μm to 200 μm, preferably 20 μm to 150 μm, and more preferably 30 μm to 100 μm.

[0019] <Separator film> The separator film 13 is attached to conceal the adhesive force of the adhesive layer 15. The separator film is usually peeled off appropriately when using the film product. The separator film is not particularly limited, but usually a film other than an optically functional film is used. Examples of the separator film include resin films; paper; porous films such as woven fabrics, nonwoven fabrics, and mesh fabrics; and foamed resin films. Since the surface smoothness is excellent, resin films are preferably used as the separator film, and more preferably, substantially isotropic colorless and transparent resin films are used. Examples of the resin film include films containing the above-mentioned resins as the main resin component. Examples of the separator film include polyethylene terephthalate films, polybutylene terephthalate films, polyethylene films, polypropylene films, polybutene films, polybutadiene films, polymethylpentene films, polyvinyl chloride films, vinyl chloride copolymer films, polyurethane films, and ethylene-vinyl acetate copolymer films. The thickness of the separator film is not particularly limited and is, for example, 10 μm to 200 μm, and preferably 15 μm to 100 μm.

[0020] <Adhesive layer> The adhesive layers 14 and 15 have adhesiveness at room temperature, and the adhesiveness lasts for a long period of time. The adhesive layers are made of a known adhesive. The adhesive is colorless and transparent, and examples of the adhesive include acrylic adhesives, rubber adhesives, silicone adhesives, urethane adhesives, vinyl alkyl ether adhesives, polyvinylpyrrolidone adhesives, polyacrylamide adhesives, and cellulose adhesives. The thickness of the adhesive layer is not particularly limited, but is, for example, 0.5 μm to 50 μm, and preferably 1 μm to 30 μm.

[0021] [Method of inspecting optical laminated film, method of manufacturing film product, and system for carrying out the same] The optical laminate film inspection method of the present invention includes an inspection step of inspecting defects in an optical film during the manufacturing process of the optical laminate film, and a marking step of attaching a mark corresponding to the defect detected by the inspection to the optical laminate film. In the inspection step, defects that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film and defects other than the above defects are detected and distinguished from each other. In this specification, in order to easily distinguish these defects in terms, defects that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film are referred to as "peeling-evealing defects", and defects other than the peeling-evealing defects are referred to as "non-peeling defects". The non-peeling defects are defects that can be detected in the optical laminate film without peeling off both the surface protective film and the separator film. In the marking step, a first mark corresponding to the peeling manifestation defect is applied to the optical laminated film, and a second mark corresponding to the non-peeling defect and having a pattern different from that of the first mark is applied to the optical laminated film.

[0022] Furthermore, the method for producing a film product of the present invention includes a step of cutting out a plurality of sheet-shaped film products from the optical laminate film (the optical laminate film on which the first mark and the second mark corresponding to each defect are attached) after the marking step according to the inspection method, and a step of grouping the obtained plurality of film products. In the grouping step, the film products with the first mark are classified into a first group, the film products with the second mark are classified into a second group, and the film products with neither the first mark nor the second mark are classified into a third group.

[0023] 3 and 4 are schematic diagrams of a system 9 for carrying out the method of the present invention, although in FIG. 4 a surface protection film is not shown. The system 9 has an optical laminated film 1a manufacturing zone including a process of laminating a surface protective film 12a or the like on the optical film 11a while inspecting the optical film 11a and a marking process, a film product F manufacturing zone in which a plurality of film products F are taken out from the optical laminated film 1a, and a zone in which the plurality of film products F are grouped according to the presence or absence of marks and the type. In the system 9, the optical laminated film 1a is manufactured, the film products F is manufactured, and the film products F is grouped in a single line, but these may be performed separately. For example, the manufacturing process of the optical laminated film 1a and the manufacturing process of the film products F may be performed in separate processes (separate lines). Alternatively, the manufacturing process of the film products F and the grouping process of the film products F may be performed in separate processes.

[0024] Specifically, referring to Figures 3 and 4, the manufacturing zone of the optical laminated film 1a of the system 9 includes a conveying device 21 having a guide roll, a bonding section 22 having a nip roll for bonding a surface protective film 12a and a separator film 13a to the optical film 11a, a length measuring device 23, a reading device 24, two or more inspection devices 31, ..., a control device 25 including a calculation unit and a memory unit, and a marking device 4. The manufacturing zone of the film product F of the system 9 includes conveyors 51, 52 (conveying devices) that transport the optical laminate film 1a and the film product F, a cutting device 6 that cuts the optical laminate film 1a, and a recovery device (not shown) that recovers the cut remaining portion R. In the illustrated example, the surface protective film 12a and the separator film 13a are successively laminated to the optical film 11a after inspection (after the inspection device) in one process, but the present invention is not limited to this. For example, inspection may be performed in one process, the surface protective film 12a may be laminated to the optical film 11a, and inspection may be performed in a separate process, and the separator film 13a may be laminated to the optical film 11a (not illustrated).

[0025] <Optical laminate film manufacturing zone> In the manufacturing zone of the optical laminated film 1a, a conveying device 21 is provided to convey the optical film 11a, the surface protective film 12a, and the separator film 13a. For example, the optical film 11a, the surface protective film 12a, and the separator film 13a are each set in a rolled state and conveyed on the line by the conveying device 21. The optical film 11a is usually manufactured in a pre-process. The pre-process is not shown. For example, as described above, when the optical film has the first protective film 114 / polarizing film 115 / second protective film 116 (see FIG. 1), the optical film is manufactured by manufacturing and laminating these films 114, 115, and 116 in the pre-process. Furthermore, for example, when the optical film has a first optical function film 111 / a second optical function film 112 / a third optical function film 113 (see FIG. 2), the optical film is manufactured by manufacturing and laminating these films 111, 112, and 113 in the previous process. In the illustrated example, the optical film 11a obtained in the previous process is wound into a roll and set in the system 9, but the previous process may be incorporated into the system 9, and the optical film 11a obtained in the previous process may be transported to the system 9 without being wound.

[0026] The transport device 21 transports the film in the transport direction (longitudinal direction). The transport devices 21 are provided corresponding to the optical film 11a, the separator film 13a, and the surface protection film 12a, respectively. The separator film 13a and the surface protection film 12a are transported in synchronization with the transport of the optical film 11a. The transported separator film 13a and the surface protection film 12a are attached to the front and back surfaces of the optical film 11a in a bonding section 22.

[0027] The optical film 11a is provided with an identifier 18. The identifier 18 includes information for identifying the longitudinal position of the optical film 11a. If necessary, the identifier 18 may include any appropriate information, such as a manufacturing number of the optical film and the date and time of adding the identifier. The identifier 18 is, for example, a mechanically readable symbol such as a two-dimensional code. The identifier 18, such as the mechanically readable symbol, is usually printed on the end of the optical film 11a in the width direction. The printing method is not particularly limited, but for example, on-demand printing such as inkjet printing or laser printing is used.

[0028] The length measuring device 23 has a rotary encoder and measures the amount of movement of the optical film 11a. The measured amount of movement of the optical film 11a is sent to the control device 25, where it is stored and used for calculation. The reader 24 reads the identifier 18 and obtains the information contained therein. The information of the identifier 18 (the position in the longitudinal direction of the optical film 11a) is sent to and stored in the control device 25 and is used for calculations.

[0029] The inspection devices 31, ... are devices that detect defects that have occurred in the optical film 11a or defects that have occurred during transportation. Each of the inspection devices 31, ... has an imaging means, an image processing means (not shown) that is electrically connected to the imaging means and performs appropriate image processing on the captured image of the film acquired by the imaging means, and a light source (not shown). The inspection devices 31, ... may further have other members or devices such as a polarizing filter as necessary according to a processing method described later. As the imaging means, a line sensor in which imaging elements are linearly arranged along the width direction of the optical film, or an area sensor in which imaging elements are arranged in a matrix can be used. The field of view of the imaging means is set to be equal to or greater than the effective width of the optical film (the width used for the product). The image processing means extracts a pixel area corresponding to a defect in the film by performing known image processing such as binarization on the captured image. Then, the image processing means identifies the position of the defect in the captured image (the coordinates of the pixel area corresponding to the defect).

[0030] The inspection devices 31, . . . at least detect defects present in the optical film 11a before at least one of the separator film 13a and the surface protective film 12a is attached. The inspection device can detect various defects such as foreign matter contamination, surface irregularities such as pinholes, bright spots, coating defects, and air bubbles that have occurred in the optical film 11a. These defects are usually defects that have occurred in the optical film 11a before the surface protection film 12a and the separator film 13a are attached. Examples of processing methods for the inspection devices 31, ... include reflection inspection, crossed Nicol transmission inspection, transmission inspection, and oblique transmission inspection.

[0031] The reflection inspection detects defects on the surface of the film by irradiating light from a light source onto the film surface and having the imaging means receive the reflected light. The crossed Nicol transmission inspection detects defects in the optical film as bright spots by irradiating visible light from a light source perpendicularly (or obliquely) onto the film surface, and having the imaging means receive the light transmitted through the polarizing film in the optical film while the polarizing filter is installed immediately before the imaging means so that the absorption axis of the polarizing filter is approximately 90° with respect to the absorption axis of the polarizing film in the optical film. The transmission inspection detects defects in the optical film as shadows by irradiating visible light from a light source perpendicularly onto the film and having the imaging means receive the light transmitted through the film. The oblique transmission inspection detects defects in the optical film as shadows by irradiating visible light from a light source obliquely onto the film surface and having the imaging means receive the light transmitted through the film.

[0032] 3 and 4, for example, a case where four inspection devices 31 to 34 (first to fourth inspection devices 31 to 34) are provided is illustrated. The first inspection device 31 is disposed before the surface protection film 12a is attached. The first inspection device 31 inspects the surface of the optical film 11a for pinholes and coating defects before the surface protection film 12a is attached. The coating defects are also called white spots. For example, reflection inspection is used as a processing method of the first inspection device 31. Defects such as pinholes and coating defects are difficult to detect after the surface protection film 12a is attached to the surface of the optical film 11a. On the other hand, defects such as pinholes can be detected by peeling the surface protection film 12a from the optical laminate film 1a (in a state in which the surface protection film 12a is attached to the optical film 11a) to expose the surface of the optical film 11a, but cannot be detected by peeling only the separator film 13a from the optical laminate film 1a. Such pinholes and coating defects correspond to defects that manifest peeling. In particular, in the case of the optical film 11a having an antireflection layer or antireflection film on its surface, it is more difficult to detect pinholes present on the surface of the antireflection layer or antireflection film (i.e., the surface of the optical film 11a) after the surface protective film 12a is attached.

[0033] The second inspection device 32 is disposed before the separator film 13a is attached. The second inspection device 32 inspects the optical film 11a for the presence or absence of a bright spot before the separator film 13a is attached. For example, a crossed Nicol transmission inspection is used as the second inspection device 32. The bright spot is difficult to detect after the separator film 13a is attached to the back surface of the optical film 11a, and is particularly difficult to detect after the separator film 13a and the surface protective film 12a are attached to the optical film 11a. This is because the phase difference is shifted when the separator film 13a or the like is interposed, so that an accurate crossed Nicol inspection of the polarizing film of the optical film 11a cannot be performed. On the other hand, the defect due to the bright spot can be detected when at least the separator film 13a is peeled off from the optical laminated film 1a (in a state in which the surface protective film 12a is attached to the optical film 11a). Such a bright spot also corresponds to a peeling manifestation defect. In the following, for the sake of explanation, when it is necessary to identify the type of peel manifestation defect, the above-mentioned peel manifestation defect (which cannot be detected when surface protection film 12a is attached) that can be detected by attaching surface protection film 12a and then peeling off surface protection film 12a will be referred to as a "protection-peeling manifestation defect", and the peel manifestation defect (which cannot be detected when separator film 13a is attached) that can be detected by attaching at least separator film 13a and then peeling off separator film 13a will be referred to as a "separator-peeling manifestation defect". In FIG. 4, for convenience, the protection-peeling manifestation defects are represented by plus marks, the separator-peeling manifestation defects are represented by star marks, and the non-peeling defects are represented by diamond marks (the same applies to the other figures).

[0034] The third inspection device 33 is disposed before the separator film 13a and the surface protection film 12a are attached. The third inspection device 33 inspects whether or not there is any foreign matter inside the optical film 11a. For example, a transmission inspection is used as a processing method of the third inspection device 33. The fourth inspection device 34 is disposed before the separator film 13a and the surface protection film 12a are attached. The fourth inspection device 34 inspects whether or not there is any foreign matter inside the optical film 11a. The fourth inspection device 34 uses, for example, oblique transmission inspection as a processing method. The presence or absence of the foreign matter can be detected when the transmission inspection and oblique transmission inspection are performed on the film after the separator film 13a and the surface protection film 12a are attached to the optical film 11a (i.e., the optical laminated film 1a), and when the transmission inspection and oblique transmission inspection are performed on the optical film 11a before at least one of the separator film 13a and the surface protection film 12a is attached. Such inclusion of foreign matter is a defect that can be detected in the state of the optical laminated film 1a, and corresponds to a non-peeling defect. In addition, inspection devices (for example, the third and fourth inspection devices 33, 34) for detecting such non-peeling defects may be disposed after the separator film 13a and the surface protection film 12a are attached. 3 and 4, only imaging means (light sources and the like are not shown) are illustrated as the first to fourth inspection devices 31 to 34. Depending on the processing method and the inspection target, the imaging means and the like may be provided on the front side of the optical film 11a (for example, the first inspection device 31) or on the back side of the optical film 11a (for example, the second inspection device 32).

[0035] Also, in a pre-processing step not shown, the optical film 11a or each film constituting the optical film 11a (e.g., a polarizing film, an optically functional film, etc.) is inspected using an appropriate inspection device. For example, the above-mentioned reflection inspection, crossed Nicol transmission inspection, transmission inspection, oblique transmission inspection, etc. are appropriately performed in the pre-processing step to detect defects (peeling manifestation defects and non-peeling defects) in the optical film 11a. The defects detected in the pre-processing step are stored in a computing device having a memory unit in a state in which the type of defect (peeling manifestation defects and non-peeling defects) is associated with its position information. The inspection in the pre-processing step will be described later.

[0036] The marking device 4 is a device that puts marks on the optical laminated film 1a in order to visually confirm the positions of defects detected by each of the inspection devices 31, .... Defects detected in the previous process are also marked by the marking device 4. In the present invention, marks of different patterns are given to the optical laminated film 1a so that not only the positions of defects but also the types of defects can be visually confirmed. The visual confirmation means that the marks can be identified by human vision. The details of the marks will be described later. The marking device 4 is disposed downstream of the lamination section 22 of the separator film 13a and the surface protection film 12a. The downstream side refers to the leading side in the transport direction of the optical laminated film 1a. The marking device 4 is provided with a printing means, for example, over the entire width direction of the film (the width direction is a direction perpendicular to the transport direction). FIG. 4 illustrates an inkjet printing type marking device, which has a plurality of print heads 41 densely arranged at equal intervals in the width direction of the film. The marking device 4 can print, for example, a plurality of dots on the optical laminated film 1a. In the illustrated example, the marking device 4 is disposed on the front side of the optical laminate film 1a, and therefore marks the front side of the surface protection film 12a. The marking device 4 may also be disposed on the back side of the optical laminate film 1a, and marks may be formed on the back side of the separator film 13a.

[0037] The detection of defects and the identification of their positions by the inspection devices 31, ... in the illustrated example, and further the application of marks by the marking device 4 are performed, for example, as follows. The inspection devices 31, ... detect defects and identify the type of the defect (whether it is a peeling manifestation defect or a non-peeling defect) and the position of the defect (the distance from the edge of the optical film 11a in the width direction to the defect). The position of the defect can be identified by the coordinates of a pixel area corresponding to the defect in the captured image. For example, the first inspection device 31 detects a protection-peeling manifestation defect and identifies the position of the defect, the second inspection device 32 detects a separator-peeling manifestation defect and identifies the position of the defect, and the third inspection device 33 detects a non-peeling defect and identifies the position of the defect. The control device 25 receives an input of the movement amount of the optical film 11a in the conveying direction from the length measuring device 23. The control device 25 calculates the timing at which the defect will reach the marking device 4 based on the position of the defect identified by each inspection device 31, ... and the amount of movement of the optical film 11a measured by the length measuring device 23. The control device 25 operates the marking device 4 at the calculated timing. The marking device 4 prints a mark on the front (or back) of the optical laminated film 1a corresponding to the type of defect. For example, a first mark is printed on the front (or back) of the optical laminated film 1a corresponding to a protection-peeling manifestation defect, which is a defect detected by the first inspection device 31. In FIG. 4, a group of multiple dots shown near the plus sign is the first mark 71 (a mark corresponding to a protection-peeling manifestation defect).

[0038] The second inspection device 32 also detects the defect (separator-peeling manifestation defect) and identifies its position in the same manner as above. Then, the marking device 4 prints a first mark 71 on the front surface (or back surface) of the optical laminated film 1a in correspondence with the separator-peeling manifestation defect. In FIG. 4, a group of multiple dots shown near the star mark is the first mark 71 (the mark corresponding to the separator-peeling manifestation defect). In the following, when it is necessary to distinguish between the first mark 71 corresponding to the protection-peeling manifestation defect and the first mark 71 corresponding to the separator-peeling manifestation defect in terms of terminology, the former will be referred to as the "1-A mark 71A" and the latter will be referred to as the "1-B mark 71B."

[0039] The third inspection device 33 and the fourth inspection device 34 also detect defects (non-peeling defects) and identify their positions in the same manner as above. Then, the marking device 4 prints a second mark on the front (or back) of the optical laminated film 1a in correspondence with the non-peeling defects. In FIG. 4, a group of multiple dots shown near the diamond mark is the second mark 72 (a mark corresponding to the non-peeling defect).

[0040] Also, for defects detected in the previous process, marks are applied to the optical laminated film 1a by the marking device 4. Specifically, FIG. 5 is a reference diagram that shows a schematic method of detecting defects in the previous process and identifying their positions. Referring to the reference diagram of FIG. 5, the inspection device P1 that performs the film inspection in the previous process detects a defect D in the optical film 11F (or each film constituting the optical film) and identifies the position of the defect D in the captured image (the coordinates of the pixel area corresponding to the defect D). This information is input to the calculation device P2. On the other hand, the calculation device P2 receives input of the movement amount of the optical film 11F in the conveying direction from the length measuring device P3, and also sequentially receives information of the identifier 18 read by the reading device P4 (the position in the longitudinal direction of the optical film 11F). Therefore, the calculation device P2 can grasp how much the optical film 11F has moved in the conveying direction between the time when the identifier 18 is read and the time when the defect D is detected (the time when the coordinates of the pixel area corresponding to the defect in the captured image are identified). Based on the amount of movement of the optical film 11F between these two points in time and the coordinates of the pixel area corresponding to the defect in the captured image, the calculation device P2 can calculate the distance X1 (the distance along the longitudinal direction of the optical film) from a predetermined identifier (the identifier indicated by the reference symbol 18-Z in FIG. 5) to the defect D. Also, based on the coordinates of the pixel area corresponding to the defect in the captured image, the calculation device P2 can calculate the distance Y1 (the distance along the width direction of the optical film) from the edge in the width direction of the optical film 11F to the defect. The calculation device P2 associates and stores at least the information of the predetermined identifier 18-Z, the position information (X1, Y1) of the defect based on the identifier 18-Z, and the type of the defect. The stored defect information (hereinafter, referred to as defect information of the previous process) is organized into a database and stored in the storage unit of the calculation device P2. The control device 25 of the system 9 obtains information of the identifier 18 by the reading device 24, and extracts the defect information of the previous process based on this information. The control device 25 calculates the timing at which the defect in the previous process reaches the marking device 4 based on the defect information of the previous process (position information of the defect and the type of the defect obtained in the previous process) and the movement amount of the optical film 11a measured by the length measuring device 23. The control device 25 operates the marking device 4 at the calculated timing. The marking device 4 prints a mark on the front (or back) of the optical laminate film 1a corresponding to the type of defect detected in the previous process. For example, if the defect information of the previous process is a peeling manifestation defect, a first mark is printed on the front (or back) of the optical laminate film 1a, and if it is a non-peeling defect, a second mark is printed on the front (or back) of the optical laminate film 1a.

[0041] <Details of each mark> 3, 4, 6 to 8, the first mark 71 and the second mark 72 have different patterns. The 1-A mark 71A and the 1-B mark 71B may have the same pattern (same mark), or may have different patterns. Preferably, the 1-A mark 71A and the 1-B mark 71B have different patterns. The pattern includes a design. Marks with different patterns include, for example, a case where the contrasting marks have different designs in a plan view, a case where the contrasting marks are each composed of a plurality of designs, and the designs are the same but the arrangement of the designs is different, a case where the contrasting marks are each composed of a plurality of designs, and at least one design selected from the designs is different and the arrangement of the designs is the same or different, and the like.

[0042] The marks (first mark 71 and second mark 72) are preferably composed of two or more dots arranged in a substantially straight line along the transport direction of the optical laminate film 1a. Such marks composed of dots can be easily printed on the optical laminate film 1a by a marking device 4 having an inkjet printer, a laser printer, or the like. The first mark 71 and the second mark 72, each consisting of two or more dots, have different patterns due to the difference in the arrangement of the dots. The two or more dots correspond to the above-mentioned multiple designs. In more detail, in the illustrated example, the dots constituting the first mark 71 and the dots constituting the second mark 72 are both approximately circular (same design) in plan view, but are arranged differently. Therefore, the first mark 71 and the second mark 72 have different patterns. Although not shown, the first mark 71 and the second mark 72 each consisting of two or more dots may have different patterns by making the shapes of the dots different from each other. For example, the dots constituting the first mark 71 may be substantially triangular in plan view, and the dots constituting the second mark 72 may be substantially X-shaped in plan view. The first mark 71 and the second mark 72 each consisting of dots of different shapes (different designs) have different patterns from each other. In addition, the 1-A mark 71A and the 1-B mark 71B, which are each made up of two or more dots, have different patterns due to the different arrangement of the dots. In the illustrated example, the dots are both approximately circular in plan view, but are arranged differently. In the illustrated example, the dots are generally circular in plan view, but the shape of the dots is not limited to this and may be, for example, generally elliptical, generally rectangular, generally triangular, generally X-shaped, etc. The number of dots constituting the first mark 71 and the number of dots constituting the second mark 72 are not particularly limited as long as they are 2 or more. However, if the numbers are too small, it may be difficult to visually recognize the difference between the patterns of both marks, and if the numbers are too large, there is a high probability that the dots will remain in a defect-free film product F when cutting out the film product F from the optical laminated film 1a. From this perspective, the number of dots constituting the first mark 71 and the number of dots constituting the second mark 72 are each independently preferably 3 to 12, more preferably 4 to 10.

[0043] Moreover, the dots (marks) are represented by using any colored ink such as black ink, red ink, etc. Furthermore, when the marking device 4 is a laser printing type, the dots (marks) are represented by using any colored toner such as black toner, red toner, etc. The ink or toner representing the mark is one that can be removed without damaging the film after reinspection.

[0044] As described above, the first mark 71 and the second mark 72 have different patterns. For example, the first mark 71 consisting of a plurality of dots includes two or more dots arranged in the transport direction with an interval smaller than the diameter of one dot. For example, the second mark 72 consisting of a plurality of dots includes two or more dots arranged in the transport direction with an interval larger than the diameter of one dot, and does not include two or more dots arranged with an interval smaller than the diameter of one dot. The first mark 71 and the second mark 72 can be visually recognized by the difference in their patterns depending on whether or not they include two or more dots arranged with an interval smaller than the diameter of one dot. In other words, the first mark 71 and the second mark 72 can be distinguished from each other. Hereinafter, a spacing smaller than the diameter of one dot will be referred to as a "small spacing", and a spacing equal to or larger than the diameter of one dot will be referred to as a "large spacing".

[0045] Fig. 6 is a plan view showing an example of a 1-A mark 71A (one of the first marks 71) represented in correspondence with a protection-peeling manifestation defect. Fig. 7 is a plan view showing an example of a 1-B mark 71B (another of the first marks 71) represented in correspondence with a separator-peeling manifestation defect. Fig. 8 is a plan view showing an example of a second mark 72 represented in correspondence with a non-peeling defect. As shown in FIG. 6, the 1-A mark 71A is attached at one location for one protection-peeling manifestation defect. Similarly, the 1-B mark 71B is attached at one location for one separator-peeling manifestation defect (see FIG. 7). Similarly, the second mark 72 is attached at one location for one non-peeling defect (see FIG. 8). In FIG. 6 to FIG. 8, each of the marks 71A, 71B, and 72 is arranged on one widthwise side with respect to the corresponding defect. Note that each of the marks 71A, 71B, and 72 may be arranged on the other widthwise side (the other widthwise side is the side opposite to the one widthwise side). For example, as shown in FIG. 9, the 1-A mark 71A may be attached on the other widthwise side of one protection-peeling manifestation defect. Although not particularly shown, the 1-B mark 71B and the second mark 72 may also be attached on the other widthwise side as in FIG. 9. 6 to 9, the marks 71A, 71B, and 72 are placed so that the defect is located approximately midway between the top dot (the top dot is marked with the symbol d-1) and the bottom dot (the bottom dot is marked with the symbol d-2) on the paper, but the defect may be located closer to the top dot or the bottom dot. In addition, in FIG. 6 to 9, the marks 71A, 71B, and 72 are placed near the corresponding defects, but each of the marks 71A, 71B, and 72 may overlap a part of the defect. Each of the marks 71A, 71B, and 72 is placed corresponding to the defect, not to indicate the exact position of the defect, but to the extent that it is possible to know that the defect is located approximately near the mark.

[0046] 6 and 7, the 1-A mark 71A and the 1-B mark 71B are common in that they both include two or more dots d arranged in the transport direction with a small interval SW. On the other hand, the 1-A mark 71A does not include two or more dots d arranged with a large interval, whereas the 1-B mark 71B is different in that it includes two or more dots d arranged with a large interval LW. Therefore, the difference in the patterns of the 1-A mark 71A and the 1-B mark 71B can be visually recognized. In the illustrated example, the 1-A mark 71A is composed of eight dots d aligned in the transport direction with a small interval SW. The 1-B mark 71B is composed of two or more units (three in the illustrated example) aligned with a large interval LW, with two dots d aligned in the transport direction with a small interval SW as one unit.

[0047] 8, the second mark 72 is composed of two or more dots d arranged in the transport direction with a large interval LW. The second mark 72 does not include two dots arranged in the transport direction with a small interval. In the illustrated example, the second mark 72 is composed of four dots d arranged in the transport direction with a large interval LW.

[0048] The diameter of one dot d is the diameter of the dot d. When the dot d is not substantially circular in plan view, the diameter of the dot d is the diameter equivalent to a circle. It is preferable that the diameters of the dots d constituting the first mark 71 and the second mark 72 are the same. The specific dimension of the diameter of the dot d is not particularly limited, but is, for example, 2 mm to 5 mm, and preferably 2.5 mm to 4 mm.

[0049] The small intervals SW are smaller than the diameter of the dots d. The specific dimensions of the small intervals SW are, for example, less than 2 mm, preferably 1 mm or less, and more preferably 0.5 mm or less. The lower limit of the small intervals SW is zero. When the small intervals SW are zero, the dots d adjacent to each other in the width direction are substantially in contact with each other. For marks having sub-intervals SW, all the sub-intervals SW are preferably the same. The large interval LW is equal to or larger than the diameter of the dot d. The specific dimension of the large interval LW is, for example, 2 mm or more, preferably 2.5 mm or more, and more preferably 3 mm or more. There is no particular upper limit to the large interval LW, but if it is too large, the adjacent dots d will be too far apart, so the large interval LW is practically 8 mm or less, and preferably 6 mm or less. For marks with large spacings LW, it is preferred that all large spacings LW are the same.

[0050] Since the first mark 71 and the second mark 72 are the arrangement of dots d having the above-mentioned preferable small intervals SW and large intervals LW, the following relationship is established. Conceptually, when the first mark 71 is superimposed on the second mark 72 (that is, when the multiple dots d of the first mark 71 are printed and superimposed on the second mark 72 consisting of multiple dots d), the second mark 72 disappears. A conceptual mark represented by superimposing the first mark 71 on the second mark 72 includes two or more dots d lined up in the transport direction with a small interval SW. Therefore, the conceptual mark represented by the superimposition is not the second mark 72 but the first mark 71. Therefore, the first mark 71 and the second mark 72 have a relationship in which when the first mark 71 is superimposed on the second mark 72, the second mark 72 disappears. Due to this relationship, even if a peeling manifestation defect and a non-peeling defect exist in the same position and the first mark 71 and the second mark 72 are printed corresponding to each defect, the first mark 71 will be clearly indicated on the optical laminated film 1a. As described below, a film product having a peeling manifestation defect (film product F with the first mark 71) is not subject to reinspection and is uniformly treated as a defective product. As described above, by clearly indicating the first mark 71 (the first mark 71 is a mark that indicates the presence of a peeling manifestation defect), it is possible to reliably exclude film products having a peeling manifestation defect from being subject to reinspection.

[0051] Furthermore, by configuring the first mark 71 to include two or more dots d arranged with a small interval SW therebetween and by configuring the second mark 72 to include no two or more dots arranged with a small interval between them, the following advantages are obtained. As described later, the film product is cut out from the optical laminate film. At this time, it may rarely occur that the film product is cut across the mark. When the film product is cut across the mark, a part of the cut mark remains on one of the two adjacent film products with the cutting line as the boundary, and the remaining part of the cut mark remains on the other of the products. Since the mark does not indicate the exact position of the defect, it is not possible to determine whether the defect corresponding to the mark exists in the one product or the other product. Therefore, both the one product and the other product must be treated as products with marks. In addition, when the film product is cut across the mark, it must be avoided to confuse and group the two adjacent film products, one of which is a product with a first mark and the other is a product with a second mark. Therefore, it is desirable to make it possible to visually recognize that the two adjacent film products are products with the same mark.

[0052] Fig. 10 is a reference diagram of a case where the film is cut across the first mark 71. Since the first mark 71 includes two or more dots d arranged with a small interval SW, when the film is cut across the first mark 71, two or more dots d arranged with a small interval SW are attached to each of the two film products Fa and Fb adjacent to each other at the cutting line C. Even when the film is cut at the point shown by the dashed line in Fig. 10, one of the film products Fa has one dot d arranged with a small interval SW and less than one dot d. Therefore, when the film is cut across the first mark 71, the adjacent film products Fa and Fb can be visually recognized as products with the first mark 71 attached, at least with the small interval SW as a marker. In particular, when the small intervals SW are very small, for example, when the small intervals SW are less than 2 mm, preferably 1 mm or less, it is very rare for the cutting line to overlap the small intervals SW, so that the small intervals SW remain in each of the adjacent film products Fa and Fb and can be visually recognized.

[0053] On the other hand, the second mark 72 does not include two or more dots d arranged with a small interval SW. Therefore, when cut across the second mark 72, two film products F adjacent to each other on the cutting line do not have two or more dots d arranged with a small interval SW. Therefore, when cut across the second mark 72, the absence of at least a small interval SW is a mark that indicates that the adjacent film products F are both products with the second mark 72. Therefore, even if the film product F is cut across the mark, it is possible to reliably prevent the film product F, which may have a peel-evident defect, from being treated as a normal product.

[0054] The first marks 71 (1-A marks 71A, 1-B marks 71B) and the second marks 72 are not limited to the dot patterns shown in Fig. 6 to Fig. 8, and can be changed as appropriate. By setting the number and arrangement of the dots d, the first marks 71 including two or more dots d arranged with the small interval SW and the second marks 72 including two or more dots d arranged with the large interval LW can be set to various patterns. For example, as shown in FIG. 11, assume that a plurality of dot formation imaginary parts 78 are arranged in a substantially straight line at equal intervals along the conveying direction of the optical laminated film 1a. The plurality of dot formation imaginary parts 78 are substantially the same shape and size. The dashed line in FIG. 11 represents the dot formation imaginary parts 78. The dot formation imaginary parts 78 are parts that can display dots d when the dot formation imaginary parts 78 are printed (i.e., parts that become dots d when colored with ink or the like), and are merely conceptual parts. The interval between adjacent dot formation imaginary parts 78 corresponds to the small interval SW. Note that FIG. 11 illustrates an example in which eight dot formation imaginary parts 78 are arranged at equal intervals, but the number is not limited to this. The first mark 71 can be constructed by selecting at least two adjacent dot formation imaginary parts 78 from the plurality of dot formation imaginary parts 78 and printing the formation imaginary parts 78. On the other hand, the second mark 72 can be constructed by selecting only at least two non-adjacent dot formation imaginary parts 78 from the plurality of dot formation imaginary parts 78 and printing the formation imaginary parts 78. For example, the 1-B mark 71B shown in FIG. 7 is obtained by printing the first, second, fourth, fifth, seventh, and eighth dot formation imaginary parts 78 from the top of the paper among the dot formation imaginary parts 78 in FIG. 11. The second mark 72 shown in FIG. 8 is obtained by printing the first, third, fifth, and seventh dot formation imaginary parts 78 from the top of the paper among the dot formation imaginary parts 78 in FIG. 11.

[0055] Returning to FIG. 4, when the long strip-shaped optical laminated film 1a containing defects passes through the marking device 4, marks 71 and 72 corresponding to the respective defects are applied to the optical laminated film 1a.

[0056] <Film product manufacturing zone> In a film product manufacturing zone of the system 9, a plurality of film products F are cut out from the optical laminate film 1a that has been inspected and marked. 3 and 4, in the film product manufacturing zone, conveyors 51 and 52 convey the marked optical laminate film 1a downstream. In the illustrated example, the conveyors 51 and 52 have endless belts, but the conveyors 51 and 52 are not limited thereto. The cutting device 6 is disposed downstream of the marking device 4. The cutting device 6 has a cutting blade 61 for cutting out a film product F from the optical laminate film 1a, a blade receiving sheet 62 for receiving the cutting edge of the cutting blade 61, and a base 63 disposed on the back surface of the blade receiving sheet 62 (see FIG. 3). In the illustrated example, the belt of the conveyor 51 also serves as the blade receiving sheet 62, but the blade receiving sheet 62 and the conveyor 51 belt may be provided separately. The cutting blade 61 is pressed against the conveyed long strip-shaped optical laminate film 1a to cut the optical laminate film 1a, thereby continuously forming a plurality of film products F. Usually, after cutting, at least both ends in the width direction of the optical laminate film 1a are collected as cutting residual parts R (so-called scraps). The collection direction of the cutting residual parts R is indicated by a hollow arrow in FIG. 3, and the conveying direction of each film is indicated by an arrow. In the illustrated example, a cutting type in which the cutting residual parts R are generated only at both ends is illustrated. In this type, the gap between adjacent film products F is approximately equal to the blade thickness of the cutting blade 61. The optical laminate film 1a may also be cut in a cutting manner that leaves a cutting residual portion R between adjacent film products F. In this type, the gap between adjacent film products F becomes sufficiently larger than the blade thickness.

[0057] The layer structure of the obtained film product F is the same as that of the optical laminated film 1a. In the illustrated example, a film product F having a substantially rectangular shape (substantially rectangular or substantially square) in plan view is formed by the cutting device 6. However, the film product F formed is not limited to a substantially rectangular shape (substantially rectangular), and may be a substantially polygonal shape such as a substantially triangular shape or a substantially hexagonal shape, a substantially circular shape, a substantially elliptical shape, or a combination of these shapes. In this specification, the term "substantially" in the terms "substantially rectangular", "substantially triangular" and "substantially polygonal" includes, for example, a shape with chamfered corners, a shape with a part of a side slightly bulging or recessed, a shape with a slightly curved side, and the like. In addition, the term "substantially" in the terms "substantially circular" and "substantially elliptical" includes, for example, a shape with a part of a periphery slightly bulging or recessed, a shape with a part of a periphery slightly straight or oblique, and the like. Furthermore, in the illustrated example, the film product F is cut out so that one side of the approximately rectangular film product F is approximately parallel to the conveying direction, but the film product F may also be cut out so that one side of the approximately rectangular film product F is inclined with respect to the conveying direction. 4, film products F with a first mark 71, film products F with a second mark 72, and film products F with no mark are transported downstream of the cutting device 6. Note that some film products F may have both the first mark 71 and the second mark 72.

[0058] In the grouping zone, film products F bearing the first mark 71 are grouped into a first group G1, film products F bearing the second mark 72 are grouped into a second group G2, and film products F bearing neither the first mark 71 nor the second mark 72 are grouped into a third group G3. The grouped film products F are then accumulated and grouped together. Film products F bearing both the first mark 71 and the second mark 72 are grouped into the first group G1. The grouping may be done by a machine, a human, or a combination of humans and machines. For example, as shown in Figures 3 and 4, a sorting device 8 having an imaging means (such as a camera), an image processing means, and a removal means is disposed in the process in which each film product F is conveyed downstream of the cutting device 6. The film product F is imaged by the imaging means of the sorting device 8, and the image processing means performs appropriate image processing on the image, thereby sorting out products F with a first mark 71, products F with a second mark 72, and products F without a mark. Products F with the first mark 71 and products F with the second mark 72 are removed from the production line by a removal means (not shown), and are separated and accumulated into a first group G1 and a second group G2, respectively. Products F without a mark are left on the production line as they are and accumulated into a third group G3.

[0059] Furthermore, as described above, when the first marks 71 are subdivided into two types, 1-A marks 71A and 1-B marks 71B, it is also possible to further divide the first group G1 into two groups (1-A group and 1-B group). That is, film products F bearing the 1-A mark 71A may be grouped as the 1-A group, and film products F bearing the 1-B mark 71B may be grouped as the 1-B group. In this way, by further dividing the first group G1, the occurrence rate of the protection-peeling manifestation defect and the occurrence rate of the separator-peeling manifestation defect can be grasped separately. In this way, grasping the occurrence rates of the two defects separately can contribute to improving production efficiency in the future.

[0060] [Distinguishing and handling of normal and defective products] The film product F in the third group G3 is treated as a normal product. The film products F in the first group G1 are treated as defective products. The film products F in the second group G2 are reinspected. As a result of the reinspection, the film products F that are determined to have no defects are treated as normal products, and the film products F that are determined to have defects are treated as defective products. The normal products are provided to the market after being subjected to appropriate treatment as necessary, while the defective products are discarded or subjected to material recycling.

[0061] According to the present invention, defective products are not provided to the market, and production efficiency of film products can be improved. Specifically, a group of marked film products may contain a mixture of normal products (actually free of defects) and defective products (actually defective). In particular, it is desirable to set the standard (threshold) for defect detection high in order to reliably exclude defective products from shipments, but this increases the possibility that normal and defective products will be mixed in the marked group. Therefore, if all marked film products are discarded, there is a high possibility that normal products will also be discarded. For this reason, production efficiency (yield rate) can be improved by reinspecting marked film products and selecting normal products from among them. However, as described above, there are two types of defects: peeling-evealing defects and non-peeling defects. Peeling-evealing defects cannot be detected unless at least one of the surface protective film and the separator film is peeled off. Non-peeling defects can also be detected in the state of the film product (the state of the optical laminate film). The present inventors focused on these types of defects and decided to group film products according to the type of defect and determine whether or not reinspection is necessary.

[0062] The film products F of the first group G1 cannot be reinspected unless the surface protection film 12a and / or the separator film 13a are peeled off. If the surface protection film 12a and the like are peeled off and reinspected, the surface protection film 12a and the like must be neatly attached as before, but such a task is extremely difficult. For this reason, the film products F of the first group G1 are uniformly treated as defective products. By uniformly treating the film products F of the first group G1 as defective products, it is possible to prevent defective products from being provided to the market. On the other hand, the film products F of the second group G2 can be reinspected for defects without peeling off the film. By treating the film products F that do not actually have defects as normal products as a result of the reinspection, it is possible to increase production efficiency. The second mark 72 is displayed on the film products F of the second group G2 that are determined to be normal products by the reinspection. Therefore, the second mark 72 is completely erased and the products are shipped as normal products. Thus, according to the present invention, it is possible to reliably remove defective products and reduce the possibility of them being released onto the market to almost zero, and also to increase the production efficiency of film products. The reinspection may be performed automatically, mechanically, manually using various devices, or both mechanically and manually. It is preferable that at least a human perform the reinspection, as this is expected to produce more accurate results. The film products F of the second group G2 to be reinspected are relatively small in quantity, so even if a human inspects them precisely, this has little effect on the product cost. For this reason, by having at least a human perform the reinspection, defective products can be reliably removed as defective products. [Explanation of symbols]

[0063] 1,1a Optical laminated film 11,11a Optical film 12,12a Surface protection film 13,13a Separator film 71 1st Mark 72 2nd Mark G1 1st Group G2 2nd Group G3 3rd Group d,d-1,d-2 dots Spacing smaller than the diameter of the SW dot LW Dot diameter or larger

Claims

1. In the process of manufacturing an optical laminate film having an optical film, a surface protective film attached to a front surface of the optical film, and a separator film attached to a rear surface of the optical film, an inspection step of inspecting the optical film for defects; a marking step of marking the optical laminate film with a mark corresponding to the defect detected by the inspection; After the marking step, cutting a plurality of film products from the optical laminate film; and grouping the resulting plurality of film products, In the inspection step, a peeling evident defect that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film is distinguished from a defect other than the peeling evident defect; In the marking step, a first mark corresponding to the peeling manifestation defect is attached to the optical laminate film, and a second mark corresponding to a defect other than the peeling manifestation defect and having a pattern different from that of the first mark is attached to the optical laminate film; In the grouping step, film products bearing the first mark are grouped into a first group, film products bearing the second mark are grouped into a second group, and film products bearing neither the first mark nor the second mark are grouped into a third group, the film products in the first group are treated as defective products, and the film products in the second group are reinspected, and film products that pass the reinspection are treated as normal products. A method for manufacturing film products.

2. The first mark and the second mark are each composed of two or more dots arranged in a substantially straight line along a transport direction of the optical laminate film, the first mark includes two or more dots arranged at intervals smaller than the diameter of one dot, The method for producing a film product according to claim 1 , wherein the second mark does not include two or more dots arranged at an interval smaller than the diameter of one dot.

3. The first mark and the second mark are each composed of two or more dots arranged in a substantially straight line along a transport direction of the optical laminate film, The method for producing a film product according to claim 1 or 2, wherein the dots constituting the first mark and the dots constituting the second mark have different shapes.

4. The method for producing a film product according to claim 1 , wherein the peel-evident defect is a defect that has occurred in the optical film before the surface protective film and the separator film are attached.

5. The method for manufacturing a film product described in any one of claims 1 to 4, wherein the peeling evident defect includes a peeling evident defect that can be detected by peeling the surface protective film from the optical laminate film, and a peeling evident defect that can be detected by peeling the separator film from the optical laminate film.

6. The method for manufacturing a film product described in claim 5, wherein the pattern of the first marks corresponding to peel-evealing defects that can be detected by peeling off the surface protective film is different from the pattern of the first marks corresponding to peel-evealing defects that can be detected by peeling off the separator film.

7. In a process for manufacturing an optical laminate film having an optical film, a surface protective film attached to a front surface of the optical film, and a separator film attached to a rear surface of the optical film, an inspection process for inspecting defects in the optical film; A marking step of marking the optical laminate film with a mark corresponding to the defect detected by the inspection, In the inspection step, a peeling evident defect that can be detected by peeling at least one of the surface protective film and the separator film from the optical laminate film is distinguished from a defect other than the peeling evident defect; In the marking step, a first mark corresponding to the peeling manifestation defect is attached to the optical laminate film, and a second mark corresponding to a defect other than the peeling manifestation defect and having a pattern different from that of the first mark is attached to the optical laminate film; The first mark and the second mark are each composed of two or more dots arranged in a substantially straight line along a transport direction of the optical laminate film, the first mark includes two or more dots arranged at intervals smaller than the diameter of one dot, The second mark does not include two or more dots arranged at an interval smaller than the diameter of one dot.

Citation Information

Patent Citations

  • Inspection method of and inspection device for function film

    JP2001165865A

  • Method and device for marking defect in sheet product

    JP2001305070A

  • Evaluator for cut sheet piece and disposition determining method for cut sheet piece

    JP2007057278A

  • Defect marking method and defect marking device, method for manufacturing original fabric and original fabric, and method for manufacturing sheet and sheet

    JP2018146580A

  • Defect-containing strip and method for detecting such defects

    US20100162865A1