Manufacturing method of multilayer printed wiring board and multilayer printed wiring board
The method of using low and high filler content adhesive layers with laser removal forms uniform and reliable interlayer connections in multilayer printed wiring boards, addressing non-uniformity and residue issues for high-speed signal transmission.
Patent Information
- Application Number
- JP2020107144
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-06-22
- Publication Date
- 2024-12-09
- Estimated Expiration
- 2040-06-22
AI Technical Summary
Increasing the thickness of the adhesive layer in multilayer printed wiring boards to reduce signal transmission loss and ensure reliable interlayer connections is hindered by decreased fluidity and embeddability of conductive patterns, leading to non-uniform thickness and unreliable interlayer connections due to adhesive residue on metal foils.
A manufacturing method involving a first adhesive layer with low filler content and a second adhesive layer with higher filler content, followed by laser removal to form blind via holes, ensuring uniform thickness and reliable interlayer connections.
Ensures uniform thickness and reliable interlayer connections in multilayer printed wiring boards, supporting high-speed signal transmission with improved dielectric properties and flame retardancy.
Smart Images

Figure 0007596084000001 
Figure 0007596084000002 
Figure 0007596084000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a multilayer printed wiring board and a multilayer printed wiring board, and more particularly to a method for manufacturing a multilayer printed wiring board having a structure in which an inner layer conductive pattern and an outer layer conductive pattern are electrically connected by an interlayer connection path formed in a blind via hole, and a multilayer printed wiring board. [Background technology]
[0002] In recent years, the amount of information processed has increased dramatically in electronic devices such as smartphones, laptops, digital cameras, and game consoles as they become smaller and faster. This has resulted in an ever-increasing trend in the signal transmission speed of printed wiring boards.
[0003] Mobile communication devices such as smartphones have been transitioning to the next-generation communication standard, 5G, since 2019. With 5G, signal frequencies will increase from a few GHz to 20-30 GHz. Furthermore, by around 2022, the frequencies of signals sent and received by communication devices are expected to increase to around 50 GHz.
[0004] As the frequency increases, the signal transmission loss increases, making it increasingly important to reduce the transmission loss in the signal line.
[0005] In order to reduce signal transmission loss, it is desirable to use a material with excellent dielectric properties such as dielectric constant and dielectric tangent (tan δ) for the insulating substrate of the printed wiring board. For example, Patent Document 1 describes a printed wiring board that uses a liquid crystal polymer (LCP). [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2011-66293 A Summary of the Invention [Problem to be solved by the invention]
[0007] Incidentally, in multilayer printed wiring boards for high-speed transmission having a stripline structure or the like, it is desirable to thicken the dielectric layer (insulating base material and adhesive layer) between the signal line of the inner layer and the ground layer of the outer layer. This is because the capacitance between the signal line and the ground layer decreases, allowing the signal line width to be made thicker and reducing conductor resistance loss. In addition, adhesives with excellent dielectric properties (low dielectric constant, low dielectric loss tangent) have been developed in recent years.
[0008] Therefore, it is conceivable to improve the transmission characteristics of multilayer printed wiring boards by increasing the thickness of the adhesive layer. For example, it is conceivable to make the adhesive layer thicker than before, such as making the adhesive layer as thick as the insulating substrate. When trying to increase the thickness of the adhesive layer, it is necessary to use an adhesive containing a filler to ensure the rigidity and elasticity of the adhesive layer.
[0009] However, the fluidity of the adhesive decreases as the filler content increases. Therefore, when an adhesive with a high filler content is used, the embedding ability of the conductive pattern of the inner layer decreases, making it difficult to ensure the uniformity of the thickness of the multilayer printed wiring board. As a result, the variation in the interlayer distance may adversely affect the signal transmission characteristics of the multilayer printed wiring board.
[0010] In addition, when an adhesive with a high filler content is used, it becomes difficult to ensure the reliability of the interlayer connection path (filled via, plated via, etc.) that electrically connects the conductive pattern of the inner layer and the conductive pattern of the outer layer. This is because the adhesive containing a large amount of filler remains on the metal foil exposed at the bottom of the blind via hole for interlayer connection drilled by laser light. Since the adhesive (resin residue) remaining on the metal foil contains a large amount of filler, it cannot be sufficiently removed even by desmearing (plasma treatment, chemical treatment with chemical solution). As a result, the metal foil and the conductive material of the interlayer connection path are not electrically connected, and there is a risk that the reliability of the interlayer connection path cannot be ensured.
[0011] Furthermore, if a large amount of filler is added to the adhesive, the dielectric properties may deteriorate, which may result in deterioration of the transmission properties of the multilayer printed wiring board.
[0012] The present invention has been made based on the above technical recognition, and an object of the present invention is to provide a method for manufacturing a multilayer printed wiring board and a multilayer printed wiring board suitable for high-speed transmission, which can ensure uniformity in the thickness of the multilayer printed wiring board even when the thickness of the adhesive layer is increased.
[0013] Another object of the present invention is to provide a method for manufacturing a multilayer printed wiring board and a multilayer printed wiring board suitable for high-speed transmission, which can ensure the reliability of interlayer connection paths even when the thickness of the adhesive layer is increased. [Means for solving the problem]
[0014] A method for producing a multilayer printed wiring board according to a first aspect of the present invention includes the steps of: A step of embedding a conductive pattern provided on a dielectric layer with a first adhesive layer having a filler content rate equal to or less than a predetermined value; laminating a build-up layer, which is a metal foil-clad laminate or a metal foil, on the first adhesive layer via a second adhesive layer having a filler content greater than the predetermined value; The present invention is characterized by comprising:
[0015] In addition, in the method for producing a multilayer printed wiring board, The first adhesive layer may be free of filler.
[0016] In addition, in the method for producing a multilayer printed wiring board, The predetermined value of the filler content may be 5% by weight.
[0017] In addition, in the method for producing a multilayer printed wiring board, The second adhesive layer may be thicker than the first adhesive layer.
[0018] In addition, in the method for producing a multilayer printed wiring board, The filler may be an inorganic filler having flame retardancy.
[0019] In addition, in the method for producing a multilayer printed wiring board, removing at least the second adhesive layer and the first adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; forming an interlayer connection path that electrically connects the conductive pattern and the metal foil through the blind via hole; The device may further include:
[0020] In addition, in the method for producing a multilayer printed wiring board, The interlayer connection path may be formed so as to connect a ground wiring of the conductive pattern and a ground layer formed by patterning the metal foil.
[0021] A method for producing a multilayer printed wiring board according to a second aspect of the present invention includes the steps of: A step of preparing a double-sided metal foil-clad laminate having a first insulating substrate having a first main surface and a second main surface opposite to the first main surface, a first metal foil provided on the first main surface, and a second metal foil provided on the second main surface; patterning the first metal foil to form a conductive pattern; forming a first adhesive layer, the first adhesive layer having a filler content of a predetermined value or less, on the first main surface so as to embed the conductive pattern; forming a second adhesive layer on the first adhesive layer, the second adhesive layer having a filler content greater than the predetermined value; A step of preparing a single-sided metal foil-clad laminate including a second insulating substrate having a third main surface and a fourth main surface opposite to the third main surface, and a third metal foil provided on the third main surface; laminating the single-sided metal foil-clad laminate on the second adhesive layer such that the fourth principal surface is in contact with the second adhesive layer; removing at least the second adhesive layer and the first adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; The present invention is characterized by comprising:
[0022] A method for producing a multilayer printed wiring board according to a third aspect of the present invention includes the steps of: A step of preparing a first single-sided metal foil-clad laminate having a first insulating substrate having a first main surface and a second main surface opposite to the first main surface, and a first metal foil provided on the first main surface; patterning the first metal foil to form a conductive pattern; forming a first adhesive layer, the first adhesive layer having a filler content of a predetermined value or less, on the first main surface so as to embed the conductive pattern; forming a second adhesive layer on the first adhesive layer, the second adhesive layer having a filler content greater than the predetermined value; preparing a second single-sided metal foil-clad laminate having a second insulating substrate having a third main surface and a fourth main surface opposite to the third main surface, and a second metal foil provided on the third main surface; laminating the second single-sided metal foil-clad laminate on the second adhesive layer such that the fourth principal surface is in contact with the second adhesive layer; forming a third adhesive layer on the second main surface of the first insulating base material, the third adhesive layer having a filler content greater than the predetermined value; preparing a third single-sided metal foil-clad laminate having a third insulating substrate having a fifth main surface and a sixth main surface opposite to the fifth main surface, and a third metal foil provided on the sixth main surface; laminating the third single-sided metal foil-clad laminate on the third adhesive layer such that the fifth main surface is in contact with the third adhesive layer; removing at least the second adhesive layer and the first adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; The present invention is characterized by comprising:
[0023] A method for producing a multilayer printed wiring board according to a fourth aspect of the present invention includes the steps of: A step of preparing a first single-sided metal foil-clad laminate comprising: a first insulating substrate having a first main surface and a second main surface opposite to the first main surface; and a first metal foil provided on the second main surface of the first insulating substrate via a first adhesive layer having a filler content greater than a predetermined value; forming a second adhesive layer on the first main surface of the first insulating base material, the second adhesive layer having a filler content equal to or less than the predetermined value; providing a second metal foil over the second adhesive layer; patterning the second metal foil to form a conductive pattern; forming a third adhesive layer, the third adhesive layer having a filler content equal to or less than the predetermined value, on the second adhesive layer so as to embed the conductive pattern; preparing a second single-sided metal foil-clad laminate comprising: a second insulating base material having a third main surface and a fourth main surface opposite to the third main surface; and a third metal foil provided on the third main surface of the second insulating base material via a fourth adhesive layer having a filler content greater than the predetermined value; laminating the second single-sided metal foil-clad laminate on the third adhesive layer such that the fourth principal surface is in contact with the third adhesive layer; removing at least the fourth adhesive layer, the second insulating base material, and the third adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; The present invention is characterized by comprising:
[0024] The multilayer printed wiring board according to the present invention comprises: a dielectric layer having a first major surface and a second major surface opposite the first major surface; a conductive pattern provided on the first main surface of the dielectric layer; a first adhesive layer provided on the dielectric layer so as to embed the conductive pattern therein, the first adhesive layer having a filler content of a predetermined value or less; a second adhesive layer provided on the first adhesive layer, the second adhesive layer having a filler content greater than the predetermined value; a build-up layer, which is a metal foil-clad laminate or a metal foil, laminated on the second adhesive layer; The present invention is characterized by comprising:
[0025] In the multilayer printed wiring board, The semiconductor device may further include an interlayer connection path that electrically connects the conductive pattern and the metal foil through a blind via hole that penetrates from the metal foil to the first adhesive layer.
[0026] In the multilayer printed wiring board, The interlayer connection path may electrically connect a ground wiring of the conductive pattern and a ground layer formed by patterning the metal foil.
[0027] In the multilayer printed wiring board, The optical fiber may further include a build-up layer which is a metal foil-clad laminate or a metal foil laminated on the second main surface of the dielectric layer via an adhesive layer.
[0028] In the multilayer printed wiring board, the first adhesive layer may have a filler content of 5% by weight or less. Effect of the Invention
[0029] According to the present invention, it is possible to provide a manufacturing method for a multilayer printed wiring board and a multilayer printed wiring board suitable for high-speed transmission, which can ensure uniformity in the thickness of the multilayer printed wiring board even when the thickness of the adhesive layer is increased. [Brief description of the drawings]
[0030] [Figure 1] 1 is a plan view of a high-frequency signal transmission component according to an embodiment of the present invention; [Diagram 2] 2 is a plan view showing signal lines and ground wiring in inner layers in a region R of a multilayer printed wiring board according to an embodiment of the present invention. FIG. [Figure 3A] 2A to 2C are cross-sectional views illustrating steps in a method for manufacturing a multilayer printed wiring board according to the first embodiment. [Figure 3B] 3B is a cross-sectional view illustrating steps in the method for manufacturing the multilayer printed wiring board according to the first embodiment, following FIG. 3A. [Figure 3C] 3B, a cross-sectional view illustrating the steps of the method for manufacturing the multilayer printed wiring board according to the first embodiment. [Figure 4A] 10A to 10C are cross-sectional views illustrating steps in a method for manufacturing a multilayer printed wiring board according to a second embodiment. [Figure 4B] 4B is a cross-sectional view illustrating steps in a method for manufacturing a multilayer printed wiring board according to a second embodiment, following FIG. 4A. [Figure 4C] 4C is a cross-sectional view illustrating steps in a method for manufacturing a multilayer printed wiring board according to a second embodiment, following FIG. 4B. [Figure 4D] 4D is a cross-sectional view illustrating steps in a method for manufacturing a multilayer printed wiring board according to a second embodiment, following FIG. 4C. [Figure 5A] 10A to 10C are cross-sectional views illustrating steps in a method for manufacturing a multilayer printed wiring board according to a third embodiment. [Figure 5B] 5B is a cross-sectional view illustrating steps in a method for manufacturing a multilayer printed wiring board according to a third embodiment, following FIG. 5A. [Figure 5C] 5B, a cross-sectional view illustrating the steps of a method for manufacturing a multilayer printed wiring board according to a third embodiment. [Figure 5D] 5D is a cross-sectional view illustrating steps in a method for manufacturing a multilayer printed wiring board according to a third embodiment, following FIG. 5C. [Figure 6] FIG. 2 is a diagram showing the configuration of a test piece used in a test relating to residual film and flame retardancy. [Figure 7] FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In each drawing, components having equivalent functions are given the same reference numerals. The drawings are schematic, and the relationship between thickness and planar dimensions (aspect ratio), the thickness ratio of each layer, etc. do not necessarily match the actual ones.
[0032] <High frequency signal transmission component 100> First, a high-frequency signal transmission component 100 according to an embodiment will be described with reference to Fig. 1. Fig. 1 shows a plan view of the high-frequency signal transmission component 100. This high-frequency signal transmission component 100 is provided inside the housing of an information processing terminal such as a smartphone or a tablet terminal, and electrically connects an antenna that transmits and receives wireless signals to a main body substrate on which a signal processing chip is mounted.
[0033] As shown in FIG. 1, high-frequency signal transmission component 100 includes multilayer printed wiring board 110 constituting a long, thin, belt-like cable portion, and connector 120 provided at an end of multilayer printed wiring board 110. As shown in FIG.
[0034] Multilayer printed wiring board 110 is a flexible printed wiring board (FPC) having flexibility, and has a three-layer stripline structure in which a signal line is sandwiched between upper and lower ground layers via a dielectric layer.
[0035] 2, as an inner layer wiring pattern of multilayer printed wiring board 110, signal lines 112 and ground lines 113 are provided so as to extend in the longitudinal direction of multilayer printed wiring board 110. Signal lines 112 and ground lines 113 are provided alternately on dielectric layer 111. A high frequency signal of, for example, several GHz to several tens of GHz is input to signal line 112. Ground line 113 is electrically connected to an outer ground layer (not shown) through interlayer connection path 114 such as a filled via or a plated via. The number of signal lines 112 is not limited to that shown in the figure.
[0036] Connector 120 is provided at an end of multilayer printed wiring board 110 and is electrically connected to, for example, a main board or an antenna. Connector 120 has connection pin 121 electrically connected to signal line 112 and connection pin 122 electrically connected to ground wiring 113.
[0037] The signal lines of multilayer printed wiring board 110 may be provided as differential lines. In this case, two signal lines are provided to run parallel to each other without a ground wiring in between. Also, multiple pairs of differential lines may be provided with a ground wiring between them. Alternatively, a single-ended transmission line and a differential line may be provided in a mixed manner.
[0038] Furthermore, the planar shape of the signal line 112 and the ground wiring 113 is not limited to a straight line as shown in Fig. 2. For example, they may have a shape as described in JP 2019-106508 A.
[0039] (First embodiment) The method for manufacturing a printed wiring board according to the first embodiment will be described with reference to cross-sectional process views of FIGS. 3A to 3C.
[0040] First, as shown in Fig. 3A(1), a double-sided metal foil-clad laminate 10 is prepared. This double-sided metal foil-clad laminate 10 has an insulating substrate 11, a metal foil 12 provided on the upper surface of this insulating substrate 11, and a metal foil 13 provided on the lower surface of the insulating substrate 11. The metal foils 12 and 13 are formed on the insulating substrate 11 via a seed layer (not shown) formed on the main surface of the insulating substrate 11.
[0041] The material of the insulating substrate 11 is not particularly limited, but may be, for example, polyimide (PI), modified polyimide (MPI), polyethylene naphthalate (PEN), polyether ether ketone (PEEK), liquid crystal polymer (LCP), fluororesin (PFA, PTFE, etc.), etc. From the viewpoint of reducing transmission loss of high-speed signals, an insulating material with a small relative dielectric constant and dielectric tangent (tan δ) is desirable.
[0042] The insulating base material 11 has a thickness of, for example, 25 μm. The metal foils 12 and 13 are, for example, copper foils having a thickness of 12 μm. The metal foils 12 and 13 may be made of a metal other than copper (silver, aluminum, etc.).
[0043] 3A(2), the metal foil 12 of the double-sided metal foil-clad laminate 10 is patterned by a known photofabrication method to form a conductive pattern 12a. The conductive pattern 12a includes a signal line pattern corresponding to the signal line 112 described above and a ground wiring pattern corresponding to the ground wiring 113.
[0044] 3A(3), an adhesive layer 14 is formed on the upper surface of the insulating base material 11 so as to bury the conductive pattern 12a therein. The adhesive layer 14 has a thickness of, for example, 17 μm.
[0045] The adhesive layer 14 may be formed by applying an adhesive onto the insulating substrate 11, or may be formed by laminating a protective film with an adhesive layer (not shown) having an adhesive layer formed on one side of a protective film (coverlay) onto the insulating substrate 11 and then peeling off the protective film.
[0046] The filler content of the adhesive layer 14 is equal to or less than a predetermined value (for example, equal to or less than 5% by weight). Preferably, the adhesive layer 14 does not contain any filler. An adhesive with a low filler content has high fluidity, and therefore can improve the embedding property of the conductive pattern 12a. As a result, the thickness uniformity of the multilayer printed wiring board can be improved.
[0047] 3A(4), adhesive layer 15 is formed on adhesive layer 14. Adhesive layer 15 may be formed by applying an adhesive onto adhesive layer 14, or may be formed by laminating a protective film with an adhesive layer (not shown) having an adhesive layer formed on one side of a protective film onto adhesive layer 14, and then peeling off the protective film.
[0048] The adhesive layer 15 is an adhesive layer containing a filler, and the filler content is greater than a predetermined value. The filler content is determined by the thickness of the adhesive layer 15, the degree of thickness uniformity required for the multilayer printed wiring board, and the like. For example, the filler content of the adhesive layer 15 is 25% by weight. The thickness of the adhesive layer 15 is, for example, 20 μm.
[0049] The filler material is not particularly limited, but an inorganic filler having heat resistance and flame retardancy may be used to improve the heat resistance and flame retardancy of the multilayer printed wiring board. In this case, for example, a filler containing a metal phosphinate-based flame retardant (such as aluminum phosphinate) is used.
[0050] The material for the adhesive layers 14 and 15 is thermosetting and has sufficient adhesive strength. For example, an adhesive containing polyolefin, polystyrene, polyimide, etc. as a main component is used. Note that an adhesive having dielectric properties equal to or greater than those of the insulating substrate 11 may be used.
[0051] Next, as shown in Fig. 3B(1), a build-up layer made of a single-sided metal foil-clad laminate 20 is laminated on the adhesive layer 15. The single-sided metal foil-clad laminate 20 has an insulating substrate 21 and a metal foil 22 provided on the upper surface of the insulating substrate 21. The metal foil 22 is formed on the insulating substrate 21 via a seed layer (not shown).
[0052] The material of the insulating substrate 21 is not particularly limited, but may be the same as that of the insulating substrate 11. From the viewpoint of reducing transmission loss of high-speed signals, an insulating material with a small relative dielectric constant and dielectric loss tangent is preferable.
[0053] The insulating base material 21 has a thickness of, for example, 25 μm. The metal foil 22 is, for example, a copper foil having a thickness of 12 μm. The metal foil 22 may be made of a metal other than copper (silver, aluminum, etc.).
[0054] The step of laminating the build-up layers is performed by laminating the single-sided metal foil-clad laminate 20 on the adhesive layer 15 so that the insulating substrate 21 faces the adhesive layer 15, and then applying heat and pressure using a vacuum press or vacuum laminator. The heat treatment in this step cures the adhesive layers 14 and 15, and the laminate shown in FIG. 3B(1) is obtained.
[0055] 3B(2), the metal foil 22 is irradiated with a laser beam to remove the metal foil 22, the insulating base material 21, the adhesive layer 15, and the adhesive layer 14, thereby forming a blind via hole (BVH) H1 with the conductive pattern 12a (ground wiring) exposed at the bottom surface. Note that the metal foil 22 may be patterned in advance to form a conformal mask having an opening at the position where the blind via hole is to be formed, and the blind via hole H1 may be formed using the conformal mask.
[0056] More specifically, a CO2 laser machine is used to irradiate a laser pulse to a predetermined position of the laminate to drill a hole. The diameter of the blind via hole H1 is, for example, φ150 μm to 200 μm. Then, a desmear process is performed to remove the resin residue (residual film) of the conductive pattern 12a. As described above, since the filler content of the adhesive layer 14 in which the conductive pattern 12a is embedded is equal to or less than a predetermined value, the residual film can be removed by the desmear process.
[0057] Similarly, as shown in FIG. 3B(2), the metal foil 13 and the insulating base material 11 are removed by irradiating the metal foil 13 with a laser beam to form a blind via hole H2 with the conductive pattern 12a (ground wiring) exposed at the bottom. The diameter of the blind via hole H2 is, for example, φ150 μm to φ200 μm. In the desmearing process of the blind via hole H2, the back surface treatment film (Ni / Cr film, etc.) of the conductive pattern 12a is removed.
[0058] 3C(1), the blind via hole H1 is filled with conductive paste 31, and the blind via hole H2 is filled with conductive paste 32 by a printing method such as screen printing. The conductive pastes 31 and 32 are made by dispersing metal particles in a resin binder, which is a paste-like thermosetting resin.
[0059] After the conductive pastes 31 and 32 are filled, the conductive pastes 31 and 32 are subjected to a heat treatment. This causes the metal particles contained in the conductive pastes 31 and 32 to be metallically bonded to each other, and completes the thermosetting reaction of the binder resin in the conductive pastes 31 and 32. In this way, filled vias 31c and 32c are formed as interlayer connection paths, as shown in FIG. 3C(2).
[0060] 3C(2), the metal foils 13 and 22 are patterned by a known fabrication method to form the conductive patterns 13a and 22a. The conductive patterns 13a and 22a include a ground layer electrically connected to the filled vias 31c and 32c.
[0061] Thereafter, if necessary, surface treatment of the wiring layer exposed to the outside, formation of a surface protection film, external processing, etc. are performed.
[0062] Through the above steps, the multilayer printed wiring board 1 according to the first embodiment is obtained, as shown in FIG. 3C(2).
[0063] In the above manufacturing method, the adhesive layer 15 is formed on the adhesive layer 14, and then the single-sided metal foil-clad laminate 20 is laminated thereon, but this is not limited to the above. For example, the adhesive layer 15 may be formed on the lower surface of the insulating substrate 21 of the single-sided metal foil-clad laminate 20, and the single-sided metal foil-clad laminate 20 may be laminated on the adhesive layer 14.
[0064] Furthermore, the thickness of insulating base material 11 may be approximately the sum of the thicknesses of insulating base material 21 and adhesive layer 15. This results in a multilayer printed wiring board 1 having a structure that is approximately symmetrical in the thickness direction with conductive pattern 12a at the center.
[0065] The double-sided metal foil-clad laminate 10 may have metal foils 12 and 13 formed on an insulating substrate 11 via an adhesive layer (not shown). Similarly, the single-sided metal foil-clad laminate 20 may have metal foil 22 formed on an insulating substrate 21 via an adhesive layer (not shown).
[0066] In the above manufacturing method, the single-sided metal foil-clad laminate 20 is used as the build-up layer, but the present invention is not limited to this, and a metal foil may be used as the build-up layer. In this case, the metal foil is laminated directly on the adhesive layer 15.
[0067] In the above manufacturing method, a filled via is formed by hardening a conductive paste as an interlayer connection path, but this is not limiting, and a plated via may be formed. In this case, a metal plating layer (e.g., a copper plating layer) is formed on the inner wall of the blind via holes H1 and H2 to form a plated via that electrically connects the conductive pattern 12a and the metal foils 13 and 22.
[0068] As described above, in the first embodiment, the conductive pattern 12a formed on the insulating substrate 11 is covered with the adhesive layer 14 having a filler content rate equal to or lower than a predetermined value. Then, a build-up layer (metal foil-clad laminate or metal foil) is laminated on the adhesive layer 14 via the adhesive layer 15 having a filler content rate higher than a predetermined value.
[0069] As a result, according to the first embodiment, even if the thickness of adhesive layer 15 is increased in order to thicken the dielectric layer between conductive pattern 12a and conductive pattern 22a, it is possible to ensure the uniformity of the thickness of multilayer printed wiring board 1. As a result, it is possible to provide a multilayer printed wiring board suitable for transmitting high-speed signals.
[0070] Furthermore, since the conductive pattern 12a is embedded in the adhesive layer 14, it is possible to prevent a residual film from being generated on the conductive pattern 12a when forming the blind via hole H1. That is, the residual film on the conductive pattern 12a can be removed by a desmear process after drilling as in the conventional method. Therefore, according to this embodiment, even if an adhesive layer with a high filler content is formed, the reliability of the interlayer connection path can be ensured.
[0071] Furthermore, since adhesive layer 15 contains a flame-retardant filler at a content equal to or greater than a predetermined value, a multilayer printed wiring board having excellent heat resistance and flame retardancy can be provided.
[0072] Furthermore, since the adhesive layer 14 in which the conductive pattern 12a is embedded has a low filler content, it is possible to ensure sufficient adhesive strength between the adhesive layer 14 and the insulating substrate 11. As a result, it is possible to provide a multilayer flexible printed wiring board that is strong against bending.
[0073] Furthermore, in the first embodiment, since the signal lines of the conductive pattern 12a are embedded in an adhesive layer with a low filler content (that is, a low dielectric constant), it is possible to improve the transmission characteristics of high-speed signals.
[0074] Second embodiment Next, a method for manufacturing a printed wiring board according to a second embodiment will be described with reference to the process cross-sectional views of Figures 4A to 4D. In each figure, the same components as those in the first embodiment are given the same reference numerals. One of the differences from the first embodiment is that in the second embodiment, a single-sided metal foil-clad laminate is used as a starting material, and a build-up layer is laminated not only on the upper surface side but also on the lower surface side.
[0075] First, a single-sided metal foil-clad laminate 10A is prepared as shown in Fig. 4A(1). This single-sided metal foil-clad laminate 10A has an insulating base material 11 and a metal foil 12 provided on the upper surface of this insulating base material 11. The metal foil 12 is formed on the insulating base material 11 via a seed layer (not shown) formed on the main surface of the insulating base material 11.
[0076] Next, as shown in FIG. 4A(2), the metal foil 12 of the single-sided metal foil clad laminate 10A is patterned by a known photofabrication method to form a conductive pattern 12a.
[0077] Next, as shown in FIG. 4A(3), an adhesive layer 14 is formed on the upper surface of the insulating base material 11 so as to bury the conductive pattern 12a therein.
[0078] Next, as shown in FIG. 4A(4), an adhesive layer 15 is formed on the adhesive layer 14.
[0079] 4B(1), a build-up layer made of a single-sided metal foil-clad laminate 20 is laminated on the adhesive layer 15. In this embodiment, no heat and pressure treatment is performed in this step.
[0080] 4B(2), an adhesive layer 15A is formed on the lower surface of the insulating base material 11. The adhesive layer 15A may be formed by applying an adhesive to the lower surface of the insulating base material 11, or may be formed by laminating a protective film with an adhesive layer (not shown) having an adhesive layer formed on one surface of a protective film onto the lower surface of the insulating base material 11, and then peeling off the protective film.
[0081] The adhesive layer 15A is an adhesive layer containing a filler, and the filler content is greater than a predetermined value. The filler content is determined by the thickness of the adhesive layer 15A, the degree of thickness uniformity required for the multilayer printed wiring board, and the like. For example, the filler content of the adhesive layer 15A is 25% by weight. The thickness of the adhesive layer 15A is, for example, 20 μm. The material of the filler of the adhesive layer 15A is the same as that of the adhesive layer 15 described in the first embodiment. An adhesive containing a flame-retardant filler may be used.
[0082] Next, as shown in Fig. 4C(1), a build-up layer made of a single-sided metal foil-clad laminate 20A is laminated on the adhesive layer 15A. The single-sided metal foil-clad laminate 20A has an insulating substrate 23 and a metal foil 24 provided on the upper surface of the insulating substrate 23. The metal foil 24 is formed on the insulating substrate 23 via a seed layer (not shown).
[0083] The material of the insulating base material 23 is not particularly limited, but may be the same as the materials of the insulating base materials 11 and 21. The material of the metal foil 24 is the same as the metal foil 22 described in the first embodiment.
[0084] The process of laminating the buildup layers is performed by laminating the single-sided metal foil-clad laminate 20A on the adhesive layer 15A so that the insulating base material 23 faces the adhesive layer 15A, and then applying heat and pressure using a vacuum press or vacuum laminator. The heat treatment in this process hardens the adhesive layers 14, 15, and 15A, and a laminate shown in FIG. 4C(1) is obtained. Note that, in this example, the upper and lower buildup layers (single-sided metal foil-clad laminates 20 and 20A) are laminated and then the heat and pressure treatment is performed all at once, but this is not limited thereto, and the heat and pressure treatment may be performed separately after laminating each buildup layer.
[0085] Next, as shown in Fig. 4C(2), the metal foil 22 is irradiated with a laser beam to remove the metal foil 22, the insulating base material 21, the adhesive layer 15 and the adhesive layer 14, thereby forming a blind via hole H1A with the conductive pattern 12a (ground wiring) exposed at the bottom surface. The details of this process are the same as those of the first embodiment, so a detailed description is omitted. Note that the metal foil 22 may be patterned in advance to form a conformal mask having an opening at the position where the blind via hole is to be formed, and the blind via hole H1A may be formed using the conformal mask.
[0086] 4C(2), the metal foil 24, the insulating base material 23, the adhesive layer 15A, and the insulating base material 11 are removed by irradiating the metal foil 24 with a laser beam to form a blind via hole H2A with the conductive pattern 12a (ground wiring) exposed at the bottom surface. The metal foil 24 may be patterned in advance to form a conformal mask having an opening at the position where the blind via hole is to be formed, and the blind via hole H2A may be formed using the conformal mask.
[0087] Next, as shown in Fig. 4D(1), the blind via hole H1A is filled with conductive paste 31A, and the blind via hole H2A is filled with conductive paste 32A by a printing method such as screen printing. The conductive pastes 31A and 32A are similar to the conductive pastes 31 and 32 described in the first embodiment.
[0088] After the conductive pastes 31A and 32A are filled, they are subjected to a heat treatment, thereby forming filled vias 31Ac and 32Ac as interlayer connection paths, as shown in FIG.
[0089] Next, as shown in FIG. 4D(2), the metal foils 22 and 24 are patterned by a known fabrication method to form the conductive patterns 22a and 24a including ground layers electrically connected to the filled vias 31c and 32c.
[0090] Thereafter, if necessary, surface treatment of the wiring layer exposed to the outside, formation of a surface protection film, external processing, etc. are performed.
[0091] Through the above steps, a multilayer printed wiring board 1A according to the second embodiment is obtained, as shown in FIG. 4D(2).
[0092] According to the second embodiment, similarly to the first embodiment, it is possible to ensure the uniformity of the thickness of the multilayer printed wiring board 1 and also to ensure the reliability of the interlayer connection paths.
[0093] Furthermore, according to the second embodiment, even if the same single-sided metal foil-clad laminates 10A, 20, and 20A are used (i.e., the insulating base materials 11, 21, and 23 have the same thickness), a multilayer printed wiring board having a structure that is almost symmetrical in the thickness direction around the conductive pattern 12a (signal line) can be obtained. This makes it possible to provide a multilayer printed wiring board with excellent bending properties.
[0094] Furthermore, since the adhesive layers 15, 15A contain a flame-retardant filler at a content equal to or greater than a predetermined value, a multilayer printed wiring board having excellent heat resistance and flame retardancy can be provided.
[0095] In the above manufacturing method, the adhesive layer 15A is formed on the lower surface of the insulating base material 11, and then the single-sided metal foil-clad laminate 20A is laminated thereon, but this is not limited to the above. For example, the adhesive layer 15A may be formed on the insulating base material 23 of the single-sided metal foil-clad laminate 20A, and the single-sided metal foil-clad laminate 20A may be laminated on the insulating base material 11.
[0096] In the above manufacturing method, the single-sided metal foil-clad laminate 20, 20A is used as the build-up layer, but the invention is not limited to this and a metal foil may be used as the build-up layer. In this case, the metal foil is laminated directly on the adhesive layer 15, 15A.
[0097] In the above manufacturing method, a filled via is formed by hardening a conductive paste as an interlayer connection path, but this is not limiting, and a plated via may be formed. In this case, a metal plating layer (e.g., a copper plating layer) is formed on the inner wall of the blind via holes H1A and H2A to form a plated via that electrically connects the conductive pattern 12a and the metal foils 22 and 24.
[0098] The single-sided metal foil clad laminate 10A may be one in which the metal foil 12 is formed on the insulating substrate 11 via an adhesive layer (not shown). Similarly, the single-sided metal foil clad laminate 20 may be one in which the metal foil 22 is formed on the insulating substrate 21 via an adhesive layer (not shown). The single-sided metal foil clad laminate 20A may be one in which the metal foil 24 is formed on the insulating substrate 23 via an adhesive layer (not shown).
[0099] (Third embodiment) Next, a method for manufacturing a printed wiring board according to a third embodiment will be described with reference to the process cross-sectional views of Figures 5A to 5D. In each figure, the same components as those in the first embodiment are denoted by the same reference numerals. One of the differences from the first embodiment is that in the third embodiment, a conductive pattern 12a is formed on an adhesive layer.
[0100] First, as shown in Fig. 5A(1), a single-sided metal foil clad laminate 10B is prepared. The single-sided metal foil clad laminate 10B has an insulating base material 11 and a metal foil 13 provided on the lower surface of the insulating base material 11 via an adhesive layer 11a. The adhesive layer 11a has a filler content greater than a predetermined value (for example, 25% by weight). The filler material of the adhesive layer 11a is the same as that of the adhesive layer 15 described in the first embodiment. The adhesive layer 11a may contain a flame-retardant filler.
[0101] 5A(2), an adhesive layer 16 having a filler content of a predetermined value (for example, 5% by weight) or less is formed on the upper surface of the insulating substrate 11 of the single-sided metal foil-clad laminate 10B. The adhesive layer 16 may be formed by applying an adhesive to the upper surface of the insulating substrate 11, or by laminating a protective film with an adhesive layer (not shown) having an adhesive layer formed on one side of a protective film onto the upper surface of the insulating substrate 11, and then peeling off the protective film. The adhesive layer 16 does not have to contain a filler.
[0102] Next, as shown in FIG. 5A(3), a metal foil 17 is provided on the adhesive layer 16. The metal foil 17 is, for example, a copper foil, and preferably a low-roughness copper foil. The material of the metal foil 17 is not limited to copper. More specifically, in this process, the metal foil 17 is placed on the adhesive layer 16, and then a heat and pressure treatment is performed using a vacuum press device or a vacuum laminator device to harden the adhesive layer 16 and adhere the metal foil 17 to the adhesive layer 16.
[0103] 5A(4), the metal foil 17 is patterned to form a conductive pattern 17a. The conductive pattern 17a includes a signal line pattern corresponding to the signal line 112 described above and a ground line pattern corresponding to the ground line 113.
[0104] 5B(1), an adhesive layer 18 having a filler content of a predetermined value (for example, 5% by weight) or less is formed on the adhesive layer 16 so as to bury the conductive pattern 17a. The adhesive layer 18 may be formed by applying an adhesive onto the adhesive layer 16, or by laminating a protective film with an adhesive layer (not shown) having an adhesive layer formed on one side of a protective film onto the adhesive layer 16, and then peeling off the protective film. The adhesive layer 18 does not have to contain a filler.
[0105] Next, as shown in FIG. 5B(2), a build-up layer made of a single-sided metal foil-clad laminate 20B is laminated on the adhesive layer 18. This single-sided metal foil-clad laminate 20B has an insulating base material 21 and a metal foil 22 provided on the upper surface of the insulating base material 21 via an adhesive layer 21a. The adhesive layer 21a has a filler content greater than a predetermined value (for example, 25% by weight). The filler material of the adhesive layer 21a is the same as that of the adhesive layer 15 described in the first embodiment. The adhesive layer 21a may contain a flame-retardant filler.
[0106] The step of laminating the build-up layer is performed by laminating the single-sided metal foil-clad laminate 20B on the adhesive layer 18 so that the insulating substrate 21 faces the adhesive layer 18, and then applying heat and pressure using a vacuum press or vacuum laminator. The heat treatment in this step hardens the adhesive layer 18, and the laminate shown in FIG. 5B(2) is obtained.
[0107] 5C(1), the metal foil 22 is irradiated with a laser beam to remove the metal foil 22, the adhesive layer 21a, the insulating base material 21, and the adhesive layer 18, thereby forming a blind via hole H1B with the conductive pattern 17a (ground wiring) exposed on the bottom surface. Similarly, the metal foil 13 is irradiated with a laser beam to remove the metal foil 13, the adhesive layer 11a, the insulating base material 11, and the adhesive layer 16, thereby forming a blind via hole H2B with the conductive pattern 17a exposed on the bottom surface. Note that the metal foils 22 and 13 may be patterned in advance to form a conformal mask having an opening at the position where the blind via hole is to be formed, and the blind via holes H1B and H2B may be formed using the conformal mask.
[0108] The details of the method for forming the blind via holes H1B, H2B are the same as those of the first and second embodiments. Since the conductive pattern 17a is embedded in the adhesive layer 18 having a filler content rate of a predetermined value or less, the residual film on the surface of the conductive pattern 17a can be removed by a desmear process after the laser drilling process, because the conductive pattern 17a is formed on the adhesive layer 16 having a filler content rate of a predetermined value or less. Similarly, since the conductive pattern 17a is formed on the adhesive layer 16 having a filler content rate of a predetermined value or less, the residual film on the back surface of the conductive pattern 17a can be removed by a desmear process after the laser drilling process.
[0109] 5C(2), the blind via hole H1B is filled with conductive paste 31B, and the blind via hole H2B is filled with conductive paste 32B by a printing method such as screen printing. The conductive pastes 31B and 32B are made by dispersing metal particles in a resin binder, which is a paste-like thermosetting resin, and are similar to the conductive pastes 31 and 32 of the first embodiment.
[0110] After the conductive pastes 31B and 32B are filled, the conductive pastes 31B and 32B are subjected to a heat treatment. This causes the metal particles contained in the conductive pastes 31B and 32B to be metallically bonded to each other, and completes the thermosetting reaction of the binder resin in the conductive pastes 31B and 32B. In this way, filled vias 31Bc and 32Bc are formed as interlayer connection paths, as shown in FIG. 5D.
[0111] 5D, the metal foils 13 and 22 are patterned by a known fabrication method to form the conductive patterns 13a and 22a. The conductive patterns 13a and 22a include a ground layer electrically connected to the filled vias 31Bc and 32Bc.
[0112] Thereafter, if necessary, surface treatment of the wiring layer exposed to the outside, formation of a surface protection film, external processing, etc. are performed.
[0113] Through the above steps, a multilayer printed wiring board 1B according to the third embodiment is obtained, as shown in FIG. 5D.
[0114] According to the third embodiment, similarly to the first embodiment, it is possible to ensure uniformity in the thickness of the multilayer printed wiring board 1 and also to ensure the reliability of the interlayer connection paths.
[0115] Furthermore, according to the third embodiment, even if the same single-sided metal foil-clad laminates 10B and 20B (i.e., the insulating base materials 11 and 21 have the same thickness) are used, a multilayer printed wiring board having a structure that is almost symmetrical in the thickness direction about the conductive pattern 17a (signal line) can be obtained. This makes it possible to provide a multilayer printed wiring board with excellent bending properties.
[0116] Furthermore, according to the third embodiment, the signal line of the conductive pattern 17a is sandwiched above and below between the adhesive layers 16 and 18, which have a low filler content (i.e., a low dielectric constant), thereby improving the transmission characteristics of high-speed signals.
[0117] Furthermore, according to the third embodiment, the conductive pattern 17a is made of low-roughness copper foil, so that signal loss of high-speed signals can be reduced.
[0118] In the above manufacturing method, a filled via is formed by hardening a conductive paste as an interlayer connection path, but the present invention is not limited to this, and a plated via may be formed. In this case, a metal plating layer (e.g., a copper plating layer) is formed on the inner wall of the blind via holes H1B and H2B to form a plated via that electrically connects the conductive pattern 17a and the metal foils 13 and 22.
[0119] <Tests related to residual film and flame retardancy> FIG. 6(1) is a cross-sectional view showing the configuration of a test piece for testing the presence or absence of residual film generation during blind via hole formation. The test piece is composed of an insulating substrate, a copper foil provided on the insulating substrate, and a first adhesive layer and a second adhesive layer formed on the copper foil. A 25 μm thick polyimide film was used as the insulating substrate. The thickness of the copper foil is 12 μm. The first adhesive layer and the second adhesive layer were formed using an adhesive whose main component is a polyolefin-based heat-resistant resin. A filler containing aluminum phosphinate was used. The test was performed by irradiating the second adhesive layer with a laser pulse from a CO2 laser processing machine to perform perforation, then performing a desmear process and checking whether or not there was any resin residue on the copper foil exposed at the bottom of the blind via hole.
[0120] FIG. 6(2) is a cross-sectional view showing the structure of a test piece for testing the flame retardancy of a printed wiring board. The test piece has a structure in which a first adhesive layer, a second adhesive layer, and a second insulating substrate are laminated in this order on a first insulating substrate, and the outer surfaces of the first insulating substrate and the second insulating substrate are covered and protected with a coverlay (25 μm thick). A liquid crystal polymer film with a thickness of 25 μm was used as the first insulating substrate and the second insulating substrate. The first adhesive layer and the second adhesive layer have the same structure as those in FIG. 6(1). The test was a 20 mm vertical flame burning test (V test) according to the UL94 standard. Specifically, one end of the test piece was exposed to a flame for 10 seconds, and the afterflame time was measured.
[0121] 7 shows the results of tests relating to residual film and flame retardancy for Examples 1 and 2 and Comparative Examples 1 to 4. In all of Examples 1 and 2 and Comparative Examples 1 to 4, the sum of the thicknesses of the first adhesive layer and the second adhesive layer was 25 μm.
[0122] Regarding the residual film test, a residual film was observed on the copper foil even after the desmear treatment in Comparative Example 1 in which the first adhesive layer was not provided, and Comparative Example 2 in which the filler content of the first adhesive layer was high. On the other hand, no resin residue was observed in Examples 1 and 2 and Comparative Examples 3 and 4 in which the amount of flame retardant added was low (0 or 5 wt%). From this test result, it can be said that the occurrence of resin residue on the bottom surface of the blind via hole can be prevented by setting the filler content of the first adhesive layer to at least 5 wt% or less.
[0123] In the flame retardancy test, in Examples 1 and 2 and Comparative Examples 1 and 2, in which the second adhesive layer with a high filler content was 20 μm or thicker, the afterflame time was less than 10 seconds, satisfying the V-0 class flame retardancy. On the other hand, in Comparative Example 3, in which the second adhesive layer was 15 μm thick, the afterflame time was about 10 seconds, and in Comparative Example 4, in which the second adhesive layer was not provided, the afterflame time was longer than 10 seconds. From these test results, it can be said that by providing a second adhesive layer with a filler content of 25% by weight or more and a thickness of 20 μm or more, a specified flame retardancy (V-0 class) can be ensured even when a first adhesive layer with a low filler content is provided.
[0124] Based on the above description, a person skilled in the art may be able to conceive additional effects and various modifications of the present invention, but the aspects of the present invention are not limited to the individual embodiments described above. Elements of different embodiments may be appropriately combined. Various additions, modifications, and partial deletions are possible within the scope of the conceptual idea and intent of the present invention derived from the contents defined in the claims and their equivalents. [Explanation of symbols]
[0125] 1,1A,1B Multilayer printed wiring board 10 Double-sided metal foil laminate 10A, 10B Single-sided metal foil laminate 11 Insulating substrate 11a,21a Adhesive layer 12,13 Metal foil 12a, 13a Conductive pattern 14,16,18 Adhesive layer 17 Metal foil 15,15A adhesive layer 20, 20A, 20B Single-sided metal foil laminate 21,23 Insulating substrate 22,24 Metal foil 22a Conductive pattern 31,32 Conductive paste 31c,32c Filled via 100 High frequency signal transmission parts 110 Multilayer printed wiring board 111 Dielectric layer 112 Signal Line 113 Ground wiring 114 Interlayer connection 120 Connector 121,122 Connection pins H1,H2 blind via holes
Claims
1. a step of embedding the conductive pattern provided on the dielectric layer with a first adhesive layer having a filler content of a predetermined value or less, being thermosetting and not being photosetting; laminating a build-up layer, which is a metal foil-clad laminate or a metal foil, on the first adhesive layer via only a second adhesive layer, which has a filler content greater than the predetermined value, is thermosetting, and is not photosetting; curing the first adhesive layer and the second adhesive layer by heat treatment; removing at least the second adhesive layer and the first adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; forming an interlayer connection path that electrically connects the conductive pattern and the metal foil through the blind via hole; A method for manufacturing a multilayer printed wiring board, comprising:
2. 2. The method for manufacturing a multilayer printed wiring board according to claim 1, wherein the first adhesive layer does not contain a filler.
3. 2. The method for manufacturing a multilayer printed wiring board according to claim 1, wherein the predetermined value of the filler content is 5% by weight.
4. 4. The method for manufacturing a multilayer printed wiring board according to claim 1, wherein the second adhesive layer is thicker than the first adhesive layer.
5. 5. The method for producing a multilayer printed wiring board according to claim 1, wherein the filler is an inorganic filler having flame retardancy.
6. The step of forming the interlayer connection path includes: filling the blind via holes with a conductive paste; a step of forming a filled via that electrically connects the conductive pattern and the metal foil by heating and hardening the filled conductive paste; The method for producing a multilayer printed wiring board according to any one of claims 1 to 5, further comprising the steps of:
7. The step of forming the interlayer connection path includes: The method for manufacturing a multilayer printed wiring board according to any one of claims 1 to 5, further comprising a step of forming a plated via that electrically connects the conductive pattern and the metal foil by forming a metal plating layer on the inner wall of the blind via hole.
8. The method for manufacturing a multilayer printed wiring board according to any one of claims 1 to 7, characterized in that the interlayer connection path is formed so as to connect a ground wiring of the conductive pattern and a ground layer formed by patterning the metal foil.
9. A step of preparing a double-sided metal foil-clad laminate having a first insulating substrate having a first main surface and a second main surface opposite to the first main surface, a first metal foil provided on the first main surface, and a second metal foil provided on the second main surface; patterning the first metal foil to form a conductive pattern; forming a first adhesive layer having a filler content of a predetermined value or less, having thermosetting properties, and not having photosetting properties, on the first main surface so as to embed the conductive pattern; forming a second adhesive layer on the first adhesive layer, the second adhesive layer having a filler content greater than the predetermined value, being thermosetting and not being photosetting; A step of preparing a single-sided metal foil-clad laminate including a second insulating substrate having a third main surface and a fourth main surface opposite to the third main surface, and a third metal foil provided on the third main surface; laminating the single-sided metal foil-clad laminate on the second adhesive layer such that the fourth principal surface is in contact with the second adhesive layer; curing the first adhesive layer and the second adhesive layer by heat treatment; removing at least the second adhesive layer and the first adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; A method for manufacturing a multilayer printed wiring board, comprising:
10. A step of preparing a first single-sided metal foil-clad laminate including a first insulating substrate having a first main surface and a second main surface opposite to the first main surface, and a first metal foil provided on the first main surface; patterning the first metal foil to form a conductive pattern; forming a first adhesive layer, the first adhesive layer having a filler content of a predetermined value or less, on the first main surface so as to embed the conductive pattern; forming a second adhesive layer on the first adhesive layer, the second adhesive layer having a filler content greater than the predetermined value; preparing a second single-sided metal foil-clad laminate having a second insulating substrate having a third main surface and a fourth main surface opposite to the third main surface, and a second metal foil provided on the third main surface; laminating the second single-sided metal foil-clad laminate on the second adhesive layer such that the fourth principal surface is in contact with the second adhesive layer; forming a third adhesive layer on the second main surface of the first insulating base material, the third adhesive layer having a filler content greater than the predetermined value; preparing a third single-sided metal foil-clad laminate having a third insulating substrate having a fifth main surface and a sixth main surface opposite to the fifth main surface, and a third metal foil provided on the sixth main surface; laminating the third single-sided metal foil-clad laminate on the third adhesive layer such that the fifth main surface is in contact with the third adhesive layer; removing at least the second adhesive layer and the first adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; A method for manufacturing a multilayer printed wiring board, comprising:
11. A step of preparing a first single-sided metal foil-clad laminate including a first insulating substrate having a first main surface and a second main surface opposite to the first main surface, and a first metal foil provided on the second main surface of the first insulating substrate via a first adhesive layer having a filler content greater than a predetermined value; forming a second adhesive layer on the first main surface of the first insulating base material, the second adhesive layer having a filler content equal to or less than the predetermined value; providing a second metal foil over the second adhesive layer; patterning the second metal foil to form a conductive pattern; forming a third adhesive layer, the third adhesive layer having a filler content equal to or less than the predetermined value, on the second adhesive layer so as to embed the conductive pattern; preparing a second single-sided metal foil-clad laminate comprising: a second insulating substrate having a third main surface and a fourth main surface opposite to the third main surface; and a third metal foil provided on the third main surface of the second insulating substrate via a fourth adhesive layer having a filler content greater than the predetermined value; laminating the second single-sided metal foil-clad laminate on the third adhesive layer such that the fourth principal surface is in contact with the third adhesive layer; removing at least the fourth adhesive layer, the second insulating base material, and the third adhesive layer with a laser beam to form a blind via hole having the conductive pattern exposed at a bottom surface; A method for manufacturing a multilayer printed wiring board, comprising:
12. a dielectric layer having a first major surface and a second major surface opposite the first major surface; a conductive pattern provided on the first main surface of the dielectric layer; a first adhesive layer that is provided on the dielectric layer so as to bury the conductive pattern, the first adhesive layer having a filler content of a predetermined value or less and a thermosetting property but not a photosetting property; a second adhesive layer provided on the first adhesive layer, the second adhesive layer having a filler content greater than the predetermined value and a thermosetting property and not a photosetting property; a build-up layer, which is a metal foil-clad laminate or a metal foil, laminated on the second adhesive layer; an interlayer connection path that electrically connects the conductive pattern and the metal foil through a blind via hole that penetrates from the metal foil to the first adhesive layer; A multilayer printed wiring board comprising:
13. 13. The multilayer printed wiring board according to claim 12, wherein the interlayer connection path electrically connects a ground wiring of the conductive pattern and a ground layer formed by patterning the metal foil.
14. 14. The multilayer printed wiring board according to claim 12 or 13, further comprising a build-up layer which is a metal foil-clad laminate or a metal foil laminated on the second main surface of the dielectric layer via an adhesive layer.
15. 15. The multilayer printed wiring board according to claim 12, wherein the filler content in the first adhesive layer is 5% by weight or less.
Citation Information
Patent Citations
Manufacture of thin multi-layered printed circuit board
JP1999046063A
Resin substrate, method of manufacturing the same, and conductive paste
JP2011066293A
Manufacturing method of wiring board
JP2013038280A
Laminate structure and photosensitive dry film used in the same
JP2013232665A
Manufacturing method of flexible printed circuit board, and intermediate product used for manufacturing flexible printed circuit board
JP2015177164A