Method for preparing a high-purity aqueous solution of tetraalkylammonium hydroxide
By controlling tetraalkylammonium halide content and using cation and chelate resins, the method efficiently reduces chloride ions and metal impurities in tetraalkylammonium hydroxide, addressing corrosion risks in semiconductor manufacturing.
Patent Information
- Application Number
- KR1020267024679
- Authority / Receiving Office
- KR · KR
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2024-03-04
- Filing Date
- 2025-02-25
- Publication Date
- 2026-11-10
AI Technical Summary
Existing methods for producing tetraalkylammonium hydroxide fail to achieve chloride ion concentrations at the mass ppb level and require inefficient double electrolysis processes, leading to potential corrosion risks in semiconductor manufacturing.
Electrolyze tetraalkylammonium salts with controlled tetraalkylammonium halide content within a predetermined range, followed by treatment with cation and chelate resins to reduce chloride ions and metal impurities.
Achieves chloride ion concentrations of 100 to 400 mass ppb and metal impurity levels below 5 ppt in tetraalkylammonium hydroxide, suitable for semiconductor manufacturing without corrosion risks.
Smart Images

Figure PCT00003_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a method for producing a high-purity aqueous solution of tetraalkylammonium hydroxide. Background Technology
[0002] In a wide range of fields, including the manufacture of semiconductor integrated circuits such as LSIs, display surfaces for FPDs, and circuit boards such as magnetic heads, the importance of precision processing technology for forming fine devices or performing micro-processing is increasing. In such precision processing technology, a processing method called photofabrication has become the mainstream. Photofabrication is a technology that forms various devices or wiring patterns by applying a photosensitive resin composition called photoresist to the surface of a workpiece to form a film (resist layer), performing exposure, patterning the film after exposure with a developer (forming a resist pattern), and performing electroforming (specifically, chemical etching, electrolytic etching, electroplating, or a combination thereof) using this as a mask. It is used in the manufacture of various precision components such as semiconductor packages.
[0003] Alkaline aqueous solutions are used as developers in photofabrication as described above, but if such alkaline aqueous solutions contain metal ions, they have an adverse effect on the electrical properties of the resulting semiconductor package. For this reason, alkaline aqueous solutions that do not contain metal ions, such as aqueous solutions of tetraalkylammonium hydroxide compounds like tetramethylammonium hydroxide (TMAH), are widely used as developers.
[0004] An aqueous solution of tetraalkylammonium hydroxide is produced by electrolyzing tetraalkylammonium salts in an electrolytic cell using a cation exchange membrane as a diaphragm. The tetraalkylammonium salts used in this production include chlorides, carboxylates, carbonates, and bicarbonates. Among these, if chlorides are used, contamination is observed in the aqueous solution of tetraalkylammonium hydroxide, which is the target product on the cathode side. Since there is a risk that chloride ions may corrode wiring when the aqueous solution of tetraalkylammonium hydroxide is used for the treatment of semiconductor substrates, it is important to reduce the concentration of chloride ions to the mass ppb level during production. Possible causes for chloride contamination include trace amounts of chloride ions originating from the raw materials permeating through the cation exchange membrane, or trace components contained as impurities in the raw materials reacting or decomposing within the electrolytic cell and contributing to the formation of chloride ions.
[0005] As a method for reducing chloride ions, a method has been proposed to improve the purity of a component referred to as a latent halide, which is a precursor of chloride ions present in an aqueous solution of tetraalkylammonium hydroxide, by heating it at a high temperature and then performing electrolysis (see Patent Document 1). Prior art literature
[0006] Japanese Patent Publication No. 2690730 The problem to be solved
[0007] By the method described in Patent Document 1, an aqueous solution of tetraalkylammonium hydroxide with a chloride ion content reduced to a mass ppm level can be obtained. However, evaluation at a mass ppb level concentration has not been performed, and it is unclear whether an aqueous solution of tetraalkylammonium hydroxide with a chloride ion content reduced to a mass ppb level can be obtained by the method described in Patent Document 1. Furthermore, through the inventors' investigation, it was found that in some cases, the chloride ion concentration cannot be sufficiently reduced during high-temperature treatment.
[0008] In addition, the method described in the above patent document 1 is a process in which an aqueous solution of tetraalkylammonium hydroxide prepared by electrolysis is heated to a high temperature to decompose potential halides, and then electrolyzed again to purify it to a high degree. Since the electrolysis process is required twice, there was a desire for an industrially efficient method for producing an aqueous solution of tetraalkylammonium hydroxide.
[0009] That is, the objective of the present invention is to provide a method for industrially and efficiently producing an aqueous solution of tetraalkylammonium hydroxide with reduced chloride ion concentration. means of solving the problem
[0010] The inventors have conducted thorough investigations to solve the above problem. They found that when a compound (hereinafter referred to as "tetraalkylammonium halide salt") in which at least one hydrogen atom of the alkyl group of the tetraalkylammonium salt is substituted with a chlorine atom is included as an impurity in the tetraalkylammonium salt, the impurity remains stable even after heat treatment at 90°C and cannot be sufficiently removed by heating, and that when an aqueous solution of tetraalkylammonium hydroxide is prepared by subsequent electrolysis, the chloride ion content cannot be removed to a desired level. Therefore, as a result of further investigation, they discovered that it is possible to industrially efficiently produce an aqueous solution of tetraalkylammonium hydroxide with reduced chloride ion concentration by electrolyzing a tetraalkylammonium salt in which the content of the tetraalkylammonium halide salt is within a predetermined range, and thus completed the present invention.
[0011] That is, the first present invention is a method for preparing an aqueous solution of tetraalkylammonium hydroxide by electrolyzing an aqueous solution of tetraalkylammonium salt, characterized in that the content of a tetraalkylammonium halogenated salt relative to the tetraalkylammonium salt in the aqueous solution of the tetraalkylammonium salt is 500 mass ppb or less. In the first present invention, it is preferable that the content of a tetraalkylammonium halogenated salt relative to the tetraalkylammonium salt in the aqueous solution of the tetraalkylammonium salt is 100 to 500 mass ppb, and it is preferable that the tetraalkylammonium salt is tetraalkylammonium chloride. Furthermore, it is preferable to contact the obtained aqueous solution containing tetraalkylammonium hydroxide with a cation exchange resin or a chelate resin.
[0012] In addition, the second present invention is an aqueous solution of tetraalkylammonium hydroxide having a tetraalkylammonium halogenated ion concentration of 100 to 400 mass ppb relative to tetraalkylammonium ions. In the second present invention, it is preferable that the chloride ion concentration of tetraalkylammonium ions is 20 to 60 mass ppb. In addition, it is preferable that the content of each metal impurity including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb is 5 mass ppt or less. Effects of the invention
[0013] According to the manufacturing method of the present invention, the chloride ion concentration of an aqueous solution of tetraalkylammonium hydroxide prepared by using a tetraalkylammonium salt in which the content of the tetraalkylammonium halide salt is within a predetermined range can be reduced. Specifically, it is possible to reduce the concentration to the order of mass ppb with respect to tetraalkylammonium ions. Although the details regarding the reason why the chloride ion concentration in tetraalkylammonium hydroxide can be reduced by the method of the present invention are unclear, the inventors speculate as follows. That is, it is speculated that the tetraalkylammonium halide salt included as an impurity in the tetraalkylammonium salt undergoes electrolytic reduction near the cathode during the electrolysis process, and a decomposition reaction that generates chloride ions occurs. As a result, it is thought that the chloride ion concentration of the aqueous solution of tetraalkylammonium hydroxide increases. In addition, since tetraalkylammonium halides are stable even under high temperature conditions, it is presumed that it is difficult to sufficiently remove them from tetraalkylammonium salts during high temperature treatment. Therefore, it is presumed that the chloride ion concentration in an aqueous solution of tetraalkylammonium hydroxide can be significantly reduced by using a tetraalkylammonium salt in which the tetraalkylammonium halide content is within a predetermined range as a raw material. Brief explanation of the drawing
[0014] FIG. 1 is a simplified diagram illustrating the configuration of an electrolytic cell used in an embodiment of the present invention. Specific details for implementing the invention
[0015] The manufacturing method of the present invention is characterized by using a tetraalkylammonium salt as a raw material, wherein the tetraalkylammonium salt content of the tetraalkylammonium halide is within a predetermined range. The method of the present invention will be described in detail below. Unless otherwise specifically stated in this specification, the notation "A to B" for numerical values A and B shall mean "A or greater and B or less." In such notation, if a unit is attached only to numerical value B, said unit shall also be applied to numerical value A.
[0016] (Aqueous solution of tetraalkylammonium hydroxide)
[0017] Examples of tetraalkylammonium hydroxide (hereinafter also referred to as TAAH) include tetramethylammonium hydroxide (TMAH), tetraethylammonium hydroxide, tetrapropylammonium hydroxide, and trimethylethylammonium hydroxide. Among the above TAAHs, tetramethylammonium hydroxide can be suitably used as it is widely used as a developer in semiconductor manufacturing processes.
[0018] The concentration of halide ions in an aqueous solution of tetraalkylammonium hydroxide can be analyzed by ion chromatography.
[0019] (Aqueous solution of tetraalkylammonium salt)
[0020] The aqueous TAAH solution containing the above TAAH can be prepared by electrolyzing an aqueous tetraalkylammonium salt solution having a desired tetraalkylammonium group, as described below. Specific examples of tetraalkylammonium salts include halides, carbonates, carboxylates, bicarbonates, etc. Among these, halides and carbonates are suitable, and halides are particularly suitable, in that an aqueous TAAH solution with a low content of metal impurities is easily obtained. As for the halides, they may be appropriately selected from chlorides, bromides, and iodides.
[0021] (Tetraalkylammonium halides)
[0022] In the manufacturing method of the present invention, the content of the tetraalkylammonium halide salt relative to the tetraalkylammonium salt in the aqueous solution of the tetraalkylammonium salt needs to be 500 ppb by mass or less. In the manufacturing method of the present invention, the tetraalkylammonium halide salt refers to a compound in which at least one hydrogen atom of a four-alkyl group bonded to a nitrogen atom is halogenated. The halogen of the alkyl halide group is chlorine, bromine, or iodine. Although the number of alkyl halide groups is not a problem, considering that the general method of preparing the tetraalkylammonium salt is a quaternization reaction between a trialkylamine and an alkyl halide, and considering the ease of purification, it is preferable that the number of alkyl halide groups be one, that is, that it be a mono-alkyl (trialkyl)ammonium halide. The number of carbon atoms in the alkyl halide group does not particularly matter, but examples include alkyl halide groups having 1 to 10 carbon atoms, such as methyl halide groups, ethyl halide groups, and propyl halide groups.
[0023] The content of the tetraalkylammonium halogenated salt relative to the tetraalkylammonium salt in the tetraalkylammonium salt aqueous solution can be appropriately determined based on the TAAH aqueous solution obtained after electrolysis if it is 500 mass ppb or less, but it is preferable to be 100 to 500 mass ppb from the perspective of obtaining a TAAH aqueous solution with a low chloride ion content.
[0024] Tetraalkylammonium halides in aqueous solutions of tetraalkylammonium salts can be analyzed by liquid chromatography / mass spectrometry (LC / MS) or ion chromatography.
[0025] Tetraalkylammonium halides are relatively stable to heat and do not undergo thermal decomposition even when heated at 90°C, so removal by heating is difficult. When attempting to remove tetraalkylammonium halides from tetraalkylammonium salts, methods such as treatment by column chromatography packed with ion exchange resin or treatment by electrolyzing tetraalkylammonium halides by passing an electric current in an electrolysis cell can be used.
[0026] In addition, it is speculated that the reason tetraalkylammonium halides exist in tetraalkylammonium salts is that the alkyl halides used as raw materials for tetraalkylammonium salts contain impurities having two or more halogen elements, and these impurities react with trialkylamines to become quaternized, thereby synthesizing tetraalkylammonium halides. For example, methyl chloride, which is a raw material for tetramethylammonium salts, contains dichloromethane as an impurity at levels of several hundred volume ppm. It is predicted that if the dichloromethane in methyl chloride can be reduced to nearly zero, the (chloromethyl)trimethylammonium in tetramethylammonium salts will also be reduced to nearly zero, and the chloride ion concentration relative to tetraalkylammonium ions can be reduced to 20 mass ppb or less.
[0027] (Electrolysis method)
[0028] In the manufacturing method of the present invention, an aqueous TAAH solution is obtained by electrolyzing the aqueous tetraalkylammonium salt solution. As a method of electrolysis, known methods are employed without particular limitation. Generally, an aqueous tetraalkylammonium salt solution is supplied to an electrolytic cell having an intermediate chamber formed by arranging only a cation exchange membrane or a combination of a cation exchange membrane and an anion exchange membrane between a cathode and an anode, an acid is supplied to an anode chamber formed on one side of the chamber, and an aqueous tetraalkylammonium hydroxide solution is obtained from the cathode chamber on the other side.
[0029] This is done by supplying an aqueous acid solution, such as hydrochloric acid, to the anode chamber, an aqueous tetraalkylammonium salt solution to the intermediate chamber formed by the cation exchange membrane and the anion exchange membrane, and high-purity water, particularly ultrapure water or a high-purity aqueous tetraalkylammonium hydroxide solution, to the cathode chamber.
[0030] As for the cation exchange membrane and anion exchange membrane used in the above electrolysis, known materials conventionally used for the production of aqueous tetraalkylammonium hydroxide solutions by electrolysis are used without particular limitation. For example, as a cation exchange membrane, a membrane having a sulfonic acid group, a carboxylic acid group, a phosphate group, etc. may be used, and as an anion exchange membrane, a membrane having one or more strongly basic ion exchange groups such as quaternary ammonium bases, sulfonium bases, phosphonium bases, etc., and primary, secondary, tertiary amines, etc. may be used. In addition, as a gas for the ion exchange membrane, for example, hydrocarbon-based, fluorocarbon-based, or perfluorocarbon-based resins may be used. In particular, as the ion exchange membrane constituting the cathode chamber, an ion exchange membrane using a perfluorocarbon resin as the gas that is stable and has excellent durability under a basic atmosphere is suitable; furthermore, since oxidizing gases such as halogen gas and oxygen gas are generated in the anode chamber, it is desirable to use an ion exchange membrane using a perfluorocarbon-based resin as the gas that has oxidation resistance.
[0031] In addition, as the anode, a so-called insoluble electrode, such as carbon, platinum-coated titanium, ruthenium, or iridium coated on the titanium surface, is suitably used. Furthermore, as the cathode, one that is stable in a strong basic atmosphere and has low overvoltage is suitably used. For example, materials such as SUS316, platinum, and Rainey nickel are suitable.
[0032] In the above electrolytic dialysis, the current density is 1 to 50 A / dm² 2 It is desirable to control the temperature to 30 to 50°C so that it does not exceed 90°C.
[0033] By the manufacturing method of the present invention above, an aqueous solution of tetraalkylammonium hydroxide with a low chloride ion concentration can be obtained. Specifically, an aqueous solution of tetraalkylammonium hydroxide can be obtained in which the concentration of tetraalkylammonium halogenated ions relative to tetraalkylammonium ions is 100 to 400 mass ppb, preferably 100 to 300 mass ppb, and particularly preferably 100 to 200 mass ppb.
[0034] (Removal of metal impurities)
[0035] If metal impurities in the aqueous tetraalkylammonium hydroxide solution obtained by the manufacturing method of the present invention are problematic, the metal impurities in the aqueous tetraalkylammonium hydroxide solution can be removed to obtain an aqueous tetraalkylammonium hydroxide solution with a reduced metal impurity content. Specifically, as a method for removing metal impurities, the aqueous tetraalkylammonium hydroxide solution may be brought into contact with a cation exchange resin or a chelate resin to adsorb the metal impurities onto the cation exchange resin or the chelate resin.
[0036] Here, in the present invention, metal impurities are specifically elements including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb, and their content is evaluated as the total content thereof. In addition, in the present invention, the content of the metal impurities in the aqueous tetraalkylammonium hydroxide solution refers to the value analyzed by an inductively coupled plasma mass spectrometer (ICP-MS).
[0037] Since the above tetraalkylammonium hydroxide aqueous solution exhibits basicity in neutral to basic conditions, the above cation exchange resin can be used effectively whether it is a strong acidic cation exchange resin in which the cation exchange group is a sulfonic acid group, or a weak acidic cation exchange resin in which the cation exchange group is a carboxyl group or a phenolic hydroxyl group.
[0038] However, since the aqueous solution of tetraalkylammonium hydroxide may exhibit acidity due to the incorporation of trace amounts of acid during its manufacturing process, it is preferable to use a strong acidic cation exchange resin capable of exchange even in the strong acid range. Additionally, the acid may be neutralized with a hydroxide having quaternary ammonium ions, such as the aqueous solution of tetraalkylammonium hydroxide, and then brought into contact with a weak acidic cation exchange resin.
[0039] The above-mentioned strong acid cation exchange resin generally has a structure in which a sulfonic acid group is introduced into a crosslinkable resin matrix comprising a copolymer of a monovinyl monomer, which is a cation exchanger introduction precursor, and a crosslinkable monomer. Examples of the monovinyl monomer, which is the cation exchanger introduction precursor, include alkyl-substituted styrenes such as styrene, methylstyrene, and ethylstyrene, and halogen-substituted styrenes such as bromostyrene; these may be used individually or in a mixture of two or more types. Among these, styrene or a monomer primarily composed of styrene is particularly preferred as the monovinyl monomer.
[0040] In addition, as crosslinkable monomers, crosslinkable monomers having multiple vinyl groups such as divinylbenzene, trivinylbenzene, divinyltoluene, divinylnaphthalene, divinylxylene, divinylbiphenyl, bis(vinylphenyl)methane, bis(vinylphenyl)ethane, bis(vinylphenyl)propane, and bis(vinylphenyl)butane may be used as single types or as a mixture of two or more types. Among these, divinylbenzene is particularly preferred as a crosslinkable monomer.
[0041] On the other hand, the weak acid cation exchange resin may be a copolymer of a monovinyl monomer having the above-mentioned weak acid cation exchange group, such as acrylic acid or methacrylic acid, and a crosslinkable monomer. Particularly preferably, it is an acrylic acid-divinylbenzene copolymer or a methacrylic acid-divinylbenzene copolymer.
[0042] The shape of such cation exchange resin may be any shape, such as a gel type or a macroporous type, but since a larger contact area between the ion exchange resin and the liquid facilitates the diffusion of metal ions within the ion exchange resin, the macroporous type is more suitablely used in the present invention.
[0043] In addition, the cation exchange resin used in the present invention preferably has a cation exchange capacity of 1.0 to 5.0 equivalents / L, and more preferably in the range of 1.5 to 3.0 equivalents / L. The shape of the resin body of the cation exchange resin is not particularly limited and may be in the form of a film, but is generally preferred to be in the form of particles.
[0044] Furthermore, the above-mentioned chelating resin refers to a resin in which functional groups forming complexes with metal ions have been introduced. Since it exhibits selective adsorption properties for specific metal ions, it is applied in the purification of brine, the purification of plating solutions, and the removal of harmful metals. It is also suitable for the recovery of precious metals such as platinum and palladium.
[0045] The functional groups of chelate resins generally have structures such as NO-based, SN-based, NN-based, OO-based, and PN-based groups containing two or more electron-donating elements such as N, S, O, and P.
[0046] Examples of functional groups of such chelate resins include iminodiacetic acid, polyamine, primary amine, methylglucarmine, amidoxime, isothiouronium, thiol, sulfonic acid, phosphonic acid, aminophosphate, bispicorylamine, semithiocarbamic acid, etc. Among these, iminodiacetic acid and aminophosphate are more preferred because they are representative functional groups of chelate resins and exhibit broad selectivity toward metals.
[0047] The shape of such chelating resin may be any shape, such as a gel type or a macroporous type, but since a larger contact area between the chelating resin and the liquid facilitates the diffusion of metal ions within the chelating resin, the macroporous type is more suitablely used in the present invention.
[0048] Here, the counter ions of the above-mentioned cation exchange resin or chelate resin (hereinafter collectively referred to as "cation exchange resin, etc.") exist in metal ion type and non-metal ion type, but either can be used. Specifically, as a non-metal ion type counter ion, in addition to hydrogen ions, ammonium ions (NH4 + It is used to contain ) or primary to quaternary ammonium ions, etc.
[0049] In the present invention, the counterion, such as a cation exchange resin, is preferably of the non-metallic ion type, and particularly preferably of the hydrogen ion type. The counterion is an ammonium ion (NH4 + In the case of ) or primary to quaternary ammonium ion types, excluding the state in which the cation is a quaternary ammonium ion such as the above tetraalkylammonium hydroxide aqueous solution, there is a risk that the tetraalkylammonium hydroxide aqueous solution obtained by the elution of the said different type of cation may be contaminated by a different type of ammonium compound, and if this occurs, separation becomes difficult.
[0050] Meanwhile, in the case of the hydrogen ion type, hydrogen ions are released through exchange with metal ions, but if the aqueous solution of tetraalkylammonium hydroxide is a hydroxide, it is neutralized to become water, so no contamination occurs. Furthermore, even if the aqueous solution of tetraalkylammonium hydroxide is not a hydroxide, if the acid derived from the released hydrogen ions is neutralized by adding a hydroxide having the same quaternary ammonium ion as the aqueous solution of tetraalkylammonium hydroxide, the acid becomes the aqueous solution of tetraalkylammonium hydroxide and water, and the contamination is easily removed. It is preferable that the hydrogen ion type be part of the counter ion, and in that case, it is preferable that at least 1 mol% is the hydrogen ion type, more preferable that at least 3 mol% is better, particularly preferable that at least 10 mol% is particularly preferable, and most preferable that at least 20 mol% is best.
[0051] Here, in the present invention, the counter ion, such as a cation exchange resin, can be quantified by ion chromatography by contacting it with an acid to elute non-metal ions, excluding metal ions and hydrogen ions. Additionally, hydrogen ions can be quantified by contacting them with a salt to elute the hydrogen ions and performing a neutralization titration.
[0052] In cases where the above-mentioned cation exchange resin, etc., has a counter ion of the non-metallic ion type, can only be prepared with a counter ion of the metallic ion type, or where a certain amount of metal ions is contained and the concentration of the metal ions is to be reduced, the metal ions can be removed by contacting it with an aqueous solution containing cations other than metal ions, thereby obtaining it as a non-metallic ion type. However, as mentioned above, in highly crosslinked cation exchange resins, etc., large cations such as tetraalkylammonium ions are difficult to diffuse into the resin. Therefore, it is desirable to contact it with an aqueous solution containing small cations that can easily penetrate into the resin and rapidly exchange with metal ions. A preferred form thereof is an aqueous solution in which the cation is a hydrogen ion, that is, it is desirable to contact it with an acid.
[0053] The aqueous acid solution used for the above contact is an aqueous solution of an inorganic acid such as sulfuric acid, hydrochloric acid, or nitric acid, and from the perspective of preventing deterioration of the resin material, it is preferable to use an aqueous solution of hydrochloric acid or an aqueous solution of sulfuric acid. In addition, although the concentration of the acid can be used without limitation, contact with a high concentration of acid may cause the counter-ion to be exchanged in a short time and lead to cracking or failure due to rapid volume changes; therefore, it is preferable to have a concentration of 1 mol / L or less, more preferably 0.5 mol / L or less, and even more preferably 0.3 mol / L or less. It is preferable to treat with an acid equivalent to 1.2 to 5 times the total amount of exchangers, such as the cation exchange resin used, and more preferable to treat with an acid equivalent to 1.5 to 3 times.
[0054] There are no particular restrictions on whether the contact treatment between the above-mentioned acid solution and the cation exchange resin is performed in a batch or through-liquid manner. In the case of a through-liquid method in which a resin tower is formed, either an upward or downward flow may be used, and it is preferable to pass an acid containing an amount equivalent to at least three times the amount of the exchanger of the cation exchange resin, etc. being treated. Although there is no specific specification for the flow rate, it is preferable to perform it in the range of SV=1 to 20 (1 / hr) from the perspective of treatment time and efficiency. In addition, in the case of a batch method, it is preferable to perform liquid exchange three or more times with an acid equivalent to 3 to 15 times the total amount of the exchanger of the cation exchange resin, etc. being treated.
[0055] In addition, if the content of metal ions contained in the aqueous acid solution is high, metal ions may remain in the cation exchange resin, etc., depending on the concentration, which may reduce the exchange amount of metal ions during purification or, in some cases, release them, potentially causing contamination. For this reason, it is desirable that the total content of metal impurities, including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb contained in the aqueous acid solution be 100 ppt or less, more preferably 10 ppt or less, and even more preferably 1 ppt or less.
[0056] In addition, it is desirable to wash the cation exchange resin, etc. with ultrapure water after contacting it with the above-mentioned aqueous acid solution. By doing so, unnecessary acid that is attached to the surface of the resin or does not enter as a counterion is removed, thereby preventing the incorporation of acid into subsequent processes. Since the aqueous solution of tetraalkylammonium hydroxide is a hydroxide, if acid remains in the cation exchange resin, etc., rapid exothermic reaction occurs due to the neutralization reaction, and there is a risk of resin destruction due to rapid swelling of the resin; therefore, it is desirable to perform washing with ultrapure water.
[0057] In addition, when a cation exchange resin, etc., in which the counter ion is of the hydrogen ion type, is brought into contact with an aqueous solution of tetraalkylammonium hydroxide, the concentration, contact method, and metal ion content thereof are suitably used in the same manner as the specifications described for the above-mentioned aqueous acid solution. In addition, it is also desirable to wash the cation exchange resin, etc., with ultrapure water after contacting it with an aqueous solution of tetraalkylammonium hydroxide.
[0058] Furthermore, in the present invention, the method of contacting the above-mentioned cation exchange resin, etc. with an aqueous solution of tetraalkylammonium hydroxide may be of any form, whether batch type or liquid-through type, but industrially, the liquid-through type is preferred. In the liquid-through type, purification is performed by providing a resin tower and passing the liquid through. The direction of the liquid flow may be either an upward flow or a downward flow, but from the perspective of increasing purification efficiency, a downward flow is preferred. The conditions for the liquid flow are preferably a space velocity SV of 1 to 20 (1 / hr), and more preferably a space velocity of 5 to 20 (1 / hr).
[0059] The throughput for contacting the aqueous tetraalkylammonium hydroxide solution is generally efficient at 100 (L / L-resin) or more. As mentioned above, since the excellent metal ion removal effect in the method of the present invention is significantly exhibited when the throughput of the crude aqueous tetraalkylammonium hydroxide solution is large, it is more effective to have a condition where the throughput is 2,000 (L / L-resin) or more, and more preferably 10,000 (L / L-resin) or more, relative to the crude aqueous tetraalkylammonium hydroxide solution. However, since the metal ion removal effect is reduced if the throughput becomes excessively large, the throughput is generally 10 8 It is desirable to keep it below (L / L-resin) and, in particular, below 50,000 (L / L-resin).
[0060] For cation exchange resins, etc., in which the metal ion removal effect is reduced in this way, it is efficient to perform the above acid treatment as a resin regeneration treatment, then resume the flow of liquid, and repeat the purification. In addition, two or more resin towers may be passed through in succession.
[0061] Meanwhile, for purification by batch method, it is preferable to perform immersion in an aqueous tetraalkylammonium hydroxide solution of 200 (L / L-resin) or more, in order to significantly demonstrate the excellent removal effect of the metal ions. In addition, it is preferable to repeat the batch treatment so that the metal ions can be further reduced. The number of repetitions is preferably 2 to 5 times.
[0062] In the method of the present invention, if the aqueous solution of tetraalkylammonium hydroxide contains particulate metal impurities, it is preferable to remove them by performing a filter treatment as a pre-process or post-process before contacting with a cation exchange resin, etc. If the aqueous solution of tetraalkylammonium hydroxide contains particulate metal impurities or resin particles, it may interfere with the action of removing metal ions by the cation exchange resin, etc. in the present invention, or cause clogging in the case of a water-through type; therefore, it is preferable to perform a filter treatment as a pre-process. Furthermore, since there is a risk that particulate metal impurities remaining after contact with the cation exchange resin, etc., and in some cases, broken pieces of the cation exchange resin, etc., may be mixed in, it is also preferable to perform the filter treatment as a post-process.
[0063] The average pore diameter of the filter used is preferably 1 μm or less, and more preferably 0.02 to 1 μm. Here, if the average pore diameter of the filter is unclear, the value measured by the bubble point method is used as the average pore diameter.
[0064] It is preferable that the inner walls of the devices, such as containers, tanks, resin towers, and piping used to carry out the manufacturing method of the present invention be made of a material that is chemically resistant and also minimizes metal contamination. For this reason, it is preferable that they be made of or lined with polyethylene, polypropylene, or fluoropolymer resins. In particular, fluoropolymer resins are optimal from the perspective of preventing metal contamination. It is preferable that the surfaces of these components be cleaned in advance before use, and it is preferable to clean them by, for example, using an aqueous solution of tetraalkylammonium hydroxide or an acid.
[0065] (Aqueous solution of tetraalkylammonium hydroxide)
[0066] By the above method, a high-purity aqueous solution of tetraalkylammonium hydroxide with reduced metal ions is effectively prepared. Specifically, it is possible to obtain an aqueous solution of tetraalkylammonium hydroxide in which the total content of metal impurities including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb is 100 ppt or less, more preferably 50 ppt or less, and even more preferably 20 ppt or less. It is also possible to make the aqueous solution of tetraalkylammonium hydroxide such that the content of each of these metal elements is 30 ppt or less, more preferably 10 ppt or less, and even more preferably 5 ppt or less.
[0067] In addition, because the aqueous solution of tetraalkylammonium hydroxide is strongly alkaline, some metal elements other than the metal elements mentioned above may take the form of anions or nonions, and the removal effect may not be sufficient.
[0068] The concentration of tetraalkylammonium hydroxide in the aqueous solution of tetraalkylammonium hydroxide can be appropriately set according to the desired purpose. Specifically, it can be appropriately set in the range of 0.5 to 40 mass%.
[0069] Examples
[0070] The present invention will be explained in more detail below with reference to examples, but the present invention is not limited to these examples in any way. Furthermore, in the following Examples 1 to 3 and Comparative Examples 1 to 3, a three-chamber structure with an anion exchange membrane and a cation exchange membrane arranged as shown in FIG. 1, with an effective area of 1 dm² 2 An electrolytic device was prepared. Additionally, a platinum-plated titanium plate was used for the anode, and SUS316 was used for the cathode.
[0071] 0.5 oz of sulfuric acid is added to the anode chamber of the above electrolytic device, and a test solution of 2.5 oz of tetramethylammonium chloride is added between the anion exchange membrane and the cation exchange membrane on the cathode side, while an aqueous solution of quaternary ammonium hydroxide is circulated to the cathode chamber, thereby achieving a current density of 30 A / dm² 2 Electrolysis was carried out continuously while maintaining the temperature at 40°C. During continuous operation, the concentration of tetramethylammonium hydroxide in the cathode chamber was set to 2.0. Likewise, to keep the concentration of the liquid circulating through each chamber constant, pure water was added when the concentration increased, and its components were added when it decreased.
[0072] After performing continuous operation for one month, the (chloromethyl)trimethylammonium ion concentration and chloride ion concentration in the cathode chamber were confirmed by the following method.
[0073] (Chloromethyl)trimethylammonium ions were measured under the following LC / MS conditions, and the concentration was calculated using the peak area.
[0074] (LC / MS conditions)
[0075] Device System: Shimadzu Seisakusho Liquid Chromatograph Mass Spectrometer Model LCMS-2020
[0076] Column: Atlantis HILIC silica (Nihon Waters)
[0077] - Particle size 3㎛, inner diameter 2.1㎜ × length 150㎜
[0078] Column temperature: 40℃
[0079] Mobile phase: Acetonitrile / 50 mM ammonium formate aqueous solution containing 0.02% formic acid = 30 / 70 (V / V)
[0080] Flow rate: 0.2 mL / min
[0081] Ionization method: ESI positive
[0082] Interface voltage: +4.5kV
[0083] Measurement mode: SIM mode m / z 118
[0084] Nebulizer gas flow rate: 1.5L / min
[0085] DL Temperature: 250℃
[0086] Heat block temperature: 400℃
[0087] Drying gas flow rate: 15L / min
[0088] Chloride ions were measured under the following ion chromatography conditions, and the concentration was calculated using the peak area.
[0089] (Ion chromatography conditions)
[0090] Device System: Thermo Fisher Scientific Model Integrion
[0091] Separation column: AS-18 IC column (Thermo Fisher Scientific)
[0092] - Particle size 7.5㎛, inner diameter 2㎜ × length 250㎜
[0093] Column temperature: 35℃
[0094] Mobile phase: 20 mM aqueous potassium hydroxide solution
[0095] Detection method: Electrical conductivity
[0096] Sample loop: 100μL
[0097] Sample conditions: 25% TMAH aqueous solution + ultrapure water (diluted 1:1)
[0098] (Example 1)
[0099] An aqueous solution of tetramethylammonium chloride containing 221 mass ppb of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was used as a raw material and subjected to electrolysis to produce an aqueous solution of tetramethylammonium hydroxide. For the prepared aqueous solution of tetramethylammonium hydroxide, the concentration of (chloromethyl)trimethylammonium ions relative to tetramethylammonium ions was 246 mass ppb, and the concentration of chloride ions relative to tetraalkylammonium ions was 25 mass ppb.
[0100] (Example 2)
[0101] An aqueous solution of tetramethylammonium chloride containing 442 mass ppb of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was used as a raw material and subjected to electrolysis to produce an aqueous solution of tetramethylammonium hydroxide. For the prepared aqueous solution of tetramethylammonium hydroxide, the concentration of (chloromethyl)trimethylammonium ions relative to tetramethylammonium ions was 295 mass ppb, and the concentration of chloride ions relative to tetraalkylammonium ions was 59 mass ppb.
[0102] (Example 3)
[0103] Purification by electrolysis of an aqueous solution of tetramethylammonium chloride containing 660 mass ppb of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was carried out. A single-chamber electrolytic device (effective area 1 dm²) with an anion exchange membrane and a cation exchange membrane separated from the electrolytic device shown in Fig. 1 2 ) was prepared. The electrodes were also prepared in the same way. An aqueous solution of tetramethylammonium chloride was added to the electrolytic device, and a current density of 30 A / dm² was applied. 2The temperature was maintained at 40°C, and an electric current was applied continuously for 10 hours. As a result, the content of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was reduced to 332 mass ppb. This aqueous tetramethylammonium chloride solution was used as a raw material and subjected to electrolysis to produce an aqueous tetramethylammonium hydroxide solution. For the prepared aqueous tetramethylammonium hydroxide solution, the concentration of (chloromethyl)trimethylammonium ions relative to tetramethylammonium ions was 345 mass ppb, and the concentration of chloride ions relative to tetraalkylammonium ions was 39 mass ppb.
[0104] (Comparative Example 1)
[0105] An aqueous solution of tetramethylammonium chloride containing 663 mass ppb of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was used as a raw material and subjected to electrolysis to produce an aqueous solution of tetramethylammonium hydroxide. For the prepared aqueous solution of tetramethylammonium hydroxide, the concentration of (chloromethyl)trimethylammonium ions relative to tetramethylammonium ions was 443 mass ppb, and the concentration of chloride ions relative to tetraalkylammonium ions was 98 mass ppb.
[0106] (Comparative Example 2)
[0107] An aqueous solution of tetramethylammonium chloride containing 1769 mass ppb of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was used as a raw material and subjected to electrolysis to produce an aqueous solution of tetramethylammonium hydroxide. For the prepared aqueous solution of tetramethylammonium hydroxide, the concentration of (chloromethyl)trimethylammonium ions relative to tetramethylammonium ions was 1477 mass ppb, and the concentration of chloride ions relative to tetraalkylammonium ions was 246 mass ppb.
[0108] (Comparative Example 3)
[0109] A tetramethylammonium chloride aqueous solution containing 660 mass ppb of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride was subjected to heat treatment at 90°C for 5 hours. As a result, the content of (chloromethyl)trimethylammonium chloride relative to tetramethylammonium chloride remained almost unchanged at 652 mass ppb. This tetramethylammonium chloride aqueous solution was used as a raw material and subjected to electrolysis to produce an aqueous tetramethylammonium hydroxide solution. For the prepared aqueous tetramethylammonium hydroxide solution, the concentration of (chloromethyl)trimethylammonium ions relative to tetramethylammonium ions was 492 mass ppb, and the concentration of chloride ions relative to tetraalkylammonium ions was 103 mass ppb.
[0110] The results of Examples 1 to 3 and Comparative Examples 1 to 3 are shown in Table 1.
[0111]
[0112] (Example 4)
[0113] The aqueous solution of tetramethylammonium hydroxide with a chloride ion concentration of 25 mass ppb obtained in Example 1 above was used as the crude aqueous solution of tetramethylammonium hydroxide. For this crude aqueous solution of tetramethylammonium hydroxide, the content of metal impurities was measured, and the content of each metal impurity including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb is shown in Table 2.
[0114] (Method for measuring the content of metal impurities in an aqueous solution of tetraalkylammonium hydroxide)
[0115] The concentrations of Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb were measured using an inductively coupled plasma mass spectrometer (ICP-MS). Additionally, the lower measurement limit was 1 ppt, and values less than 1 ppt were defined as <1 ppt.
[0116] Next, 100 ml of macroporous styrene-based iminodiacetic acid functional group chelate resin D5341 (cation exchange capacity 2.5 equivalents / L, manufactured by Purolite) was packed into a column with a diameter of 22 mm × 750 mm. To this packed column, as a pretreatment,
[0117] 1) Ultrapure water cleaning,
[0118] 2) 0.3 mol / L hydrochloric acid treatment,
[0119] 3) Ultrapure water treatment,
[0120] 4) Treatment with 0.45 mol / L aqueous tetramethylammonium hydroxide solution,
[0121] 5) Ultrapure water treatment,
[0122] The liquids were passed through in the order of [ ]. The volume of each liquid passed was set to 3L, and the space velocity was set to SV=5(1 / hr).
[0123] In addition, each of the 0.3 mol / L hydrochloric acid and 0.45 mol / L aqueous tetramethylammonium hydroxide solutions had a total content of metal impurities including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb of 100 ppt or less. In addition, for the ultrapure water, a liquid was used in which the total content of each metal impurity including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb was 1 ppt or less.
[0124] An aqueous solution of tetramethylammonium hydroxide was passed through the above column under conditions of 2,000 L and SV=20 (1 / hr). After the flow rate reached 200 L (2,000 L / L-resin), 500 L (5,000 L / L-resin), 1,000 L (10,000 L / L-resin), and 2,000 L (20,000 L / L-resin), 1 L of each solution was collected and the content of metal impurities was measured. The results are shown in Table 2.
[0125]
[0126] In Example 4, which was treated with an aqueous solution of tetramethylammonium hydroxide containing 500 mass ppt or less of each metal impurity including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb, excellent reduction effect of metal impurity concentration was exhibited at the beginning of treatment when the flow rate was 200 L (2000 L / L-resin) due to contact with a chelate resin in which the counter ion is of the non-metal ion type, and this effect was maintained up to at least 2,000 L (20000 L / L-resin). Explanation of the symbols
[0127] 1: Positive electrode 2: Cathode 3: Power 4: Anode chamber 5: Raw Materials Room 6: Cathode chamber 9: Proton penetration inhibitory layer 10: Gas layer A: Anion exchange membrane C1: Cation exchange membrane
Claims
Claim 1 A method for preparing an aqueous solution of tetraalkylammonium hydroxide by electrolyzing an aqueous solution of tetraalkylammonium salt, characterized in that the content of the tetraalkylammonium halogenated salt relative to the tetraalkylammonium salt in the aqueous solution of the tetraalkylammonium salt is 500 mass ppb or less. Claim 2 A method for preparing an aqueous solution of tetraalkylammonium hydroxide according to claim 1, wherein the content of the tetraalkylammonium halogenated salt relative to the tetraalkylammonium salt in the aqueous solution of the tetraalkylammonium salt is 100 to 500 mass ppb. Claim 3 A method for preparing an aqueous solution of tetraalkylammonium hydroxide according to claim 1 or 2, wherein the tetraalkylammonium salt is tetraalkylammonium chloride. Claim 4 A method for preparing an aqueous solution of tetraalkylammonium hydroxide by contacting an aqueous solution containing tetraalkylammonium hydroxide obtained by the method described in claim 1 with a cation exchange resin or a chelate resin. Claim 5 An aqueous solution of tetraalkylammonium hydroxide having a tetraalkylammonium halogenated ion concentration of 100 to 400 mass ppb relative to tetraalkylammonium ions. Claim 6 In claim 5, an aqueous solution of tetraalkylammonium hydroxide having a chloride ion concentration relative to tetraalkylammonium ions of 20 to 60 mass ppb. Claim 7 An aqueous solution of tetraalkylammonium hydroxide according to claim 5 or 6, wherein the content of each metal impurity including Li, Na, Mg, Al, K, Ca, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Mo, Ag, Cd, Sn, Ba, and Pb is 5 mass ppt or less.