Method and apparatus for forming a continuous web material into a load
By cooling the material contact surface and web material to below 4°C using cooling means, the method and apparatus address overheating issues in continuous web materials, ensuring precise rod formation and improved reproducibility in aerosol-generating article production.
Patent Information
- Application Number
- KR1020227014995
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-10-09
- Filing Date
- 2020-10-08
- Publication Date
- 2026-11-06
- Estimated Expiration
- 2040-10-08
AI Technical Summary
Continuous web materials, particularly those with low glass transition and melting temperatures like polylactic acid, tend to heat up during processing due to friction, leading to irregular folding and reduced reproducibility in the production of aerosol-generating articles.
A method and apparatus that utilize cooling means, such as Peltier elements or cooling fluids, to maintain the material contact surface and web material at temperatures below 4°C, especially during the gathering process, preventing overheating and ensuring precise rod formation.
Prevents overheating, maintains material integrity, and enhances production reproducibility by avoiding material stickiness and damage, allowing for accurate rod diameter maintenance and reduced machine stoppages.
Smart Images

Figure 112022047347812-PCT00002_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a method and apparatus for forming a continuous web material into a rod. In particular, it relates to a method and apparatus for forming a continuous web material used in the manufacture of aerosol-generating articles. Background Technology
[0002] For example, aerosol-generating articles or their components, such as filter plugs or aerosol cooling parts, can be manufactured from continuous web materials, such as cellulose or plastic webs. Due to the special materials used for the production of these parts, some processing steps on the processing line may present additional difficulties when handling these webs. For example, some plastic materials, such as polylactic acid webs, tend to heat up, for instance, due to friction during web handling. This can lead to irregular folding, for instance, in the funneling of the web, and may result in reduced reproducibility of products manufactured from the web. .
[0003] It is desirable to provide a method and apparatus for forming a continuous web material in the production of aerosol-generating articles.
[0004] According to the present invention, a method for forming a continuous web material into a rod is provided. The method comprises the steps of providing a continuous web material having a glass transition temperature of less than 150°C, and gathering the continuous web material from a flat shape into a rod shape by a forming device. The method further comprises the steps of providing a cooling means providing a temperature of less than 4°C, cooling a material contact surface of a forming device to a surface temperature of less than 4°C, and cooling the continuous gathered web material by a cooled material contact surface in contact with the continuous gathered web material. Preferably, the method comprises the step of cooling the continuous gathered web material to a material temperature of less than 4°C, particularly when the web material is in direct contact with a material contact surface.
[0005] The cooling means may be any means for cooling the material contact surface to a temperature of less than 4°C, particularly to a temperature of less than 0°C. The cooling means may be, for example, a Peltier element or a cooling fluid. Using a cooling fluid is very efficient for cooling. Using a Peltier element is a simple method of cooling without the need to handle the fluid.
[0006] Preferably, the cooling means is a cooling fluid having a fluid temperature of less than 4°C, more specifically less than 0°C.
[0007] Friction between the web material and, in particular, the fixed forming device is highest in the final load forming section of the gathering process (garnisher). By supercooling the web material, localized overheating of the web material due to friction when gathered in the forming device can be basically prevented.
[0008] Preferably, local overheating is prevented or at least reduced to a temperature of the web material significantly lower than its melting temperature. Preferably, overheating is prevented or reduced to a temperature of the web material significantly lower than its glass transition temperature.
[0009] Preferably, the web material is cooled so that the temperature of the web is maintained at least 10°C below its glass transition temperature. More preferably, the temperature of the web material is maintained at at least 20°C, at least 40°C, or at least 50°C below its glass transition temperature. If the web material has a glass transition temperature exceeding, for example, 100°C, the temperature of the web material is preferably maintained at a level more than 50°C lower than its glass transition temperature when cooled. For example, if the web material is cooled to less than 4°C when forming the web material, the temperature of the web material drops to about 100°C or much lower than its glass transition temperature.
[0010] Excessive heat can alter the specifications of a material. By preventing overheating of materials having a low glass transition temperature, a low melting temperature, or both, the material is prevented from becoming sticky or partially melting. Consequently, fusion can be prevented when individual folds of such materials are joined together or gathered. Advantageously, changes in the resistance to pull (RTD) of plugs formed by the material from the intended resistance to pull value are reduced or completely avoided. This can increase production reproducibility. Additionally, the adhesion of partially melted or sticky materials to device components can be avoided. Thus, possible device blockage and displacement can be avoided. Alternatively, or additionally, damage to the material can be avoided.
[0011] Advantageously, local overheating of the material is prevented so that the temperature of the web material preferably does not reach the glass transition temperature, and more preferably, does not even reach close to the glass transition temperature. Additionally, the tensile strength of the material may be reduced by heating. Consequently, it may be necessary to reduce the machine speed to prevent the material from rupturing. Thus, machine stoppages and waste caused by the rupture of the material with reduced tensile strength can be avoided. Therefore, preventing or reducing overheating of the material is particularly advantageous for materials having a low glass transition temperature or a low melting temperature, such as, for example, a web of polylactic acid.
[0012] At the glass transition temperature, the solid material changes into a rubber-elastic state and transforms into a soft, molten material. For example, amorphous or semicrystalline plastic materials may become sticky and undergo changes in their stability. The transition to the rubber-elastic state or yield range is continuous. At the glass transition temperature, the material does not undergo a phase transition. Therefore, the glass transition temperature is not related to an exact temperature, but to a temperature range. This temperature range can be several degrees around the specific glass transition temperature, for example, within 5 degrees, or tens of degrees, for example, within ±20 degrees.
[0013] Furthermore, it is known that when cooled to very low temperatures, continuous material may break or be unintentionally damaged during handling. However, compared to cooling through direct contact with a cooling fluid, it has been found that when cooled through a cold contact surface, the web material does not unintentionally break or breaks only to a very limited extent. Additionally, cooling through contact with a cooled contact surface has the advantage of precisely cooling the web material at the location where friction occurs at the interface between the forming device and the continuous web material collected within the forming device.
[0014] Furthermore, in the final rod-forming region, the accuracy requirements for the rod diameter are strict. Although it is difficult to maintain these under various compressive strengths of the cooling fluid introduced into the web material, this can be effectively achieved using a cooling surface.
[0015] In addition, it has been found that using a cooling means that provides a cooling temperature of less than 4°C to cool a contact surface to less than 4°C, and having a cooled contact surface, also cooling a web material, preferably to a temperature of less than 4°C, provides very good results in preventing overheating of a web material having a low glass transition temperature, such as a polylactic acid material, when collected, for example. In particular, it has been found that good results in preventing overheating of a web material having a low glass transition temperature can be achieved by using a cooling means that provides a cooling temperature of less than 0°C, for example, -0°C to -5°C.
[0016] These measurements were found to provide very good results for fixed forming elements, particularly in fixed funnel-shaped forming devices with a production speed of about 200 to 500 meters / minute.
[0017] Throughout the specification, the term "cooling" is used to refer to an active step for limiting, maintaining, or reducing the temperature of a continuous web material, a section of a continuous web material, or an element in contact with the continuous web material, thereby preventing further increase in the temperature of the continuous web material.
[0018] The terms "upstream" and "downstream" are used herein with respect to the direction of transport of a continuous web material in individual elements of the device or the device performing the method, wherein downstream is the production direction.
[0019] Generally, whenever the term “about” is used with respect to a specific value throughout this application, it should be understood to mean that the value following the term “about” does not necessarily have to be exactly that specific value due to technical considerations. However, the term “about” with respect to a specific value should be understood as always including and explicitly disclosing the specific value following the term “about”.
[0020] The term “gathering” is used throughout this specification to refer to a reduction in the width of a continuous web material. By gathering, the continuous material is reduced along the lateral direction of the material and across the length and transport direction of the material. Gathering may be, for example, compression of the material, funnel and rod shapes, or a combination of the aforementioned processes. Gathering involves a reduction in the width of the continuous web material, for example, by simply pushing the side of the continuous material against the longitudinal central axis of the continuous material.
[0021] Gathering can be performed continuously or in stages. Gathering can be performed within one or more parts of a forming device.
[0022] The gathered material used herein may be a partially gathered material or a final gathered material. The partially gathered material has a reduced width compared to a continuous web material such as that supplied to the apparatus performing the method according to the present invention. The partially gathered material may also have a reduced width compared to a partially gathered material having a previous portion that has already passed through a forming apparatus. The partially gathered material has a width greater than the width of the final load shape of the continuous material. Frequently, a reduction in the width of the web material results in an increase in the height of the gathered material.
[0023] Preferably, the gathering includes the formation of a longitudinal fold that forms a channel along the length of the gathered web material.
[0024] It may be advantageous to crimp the web material before gathering it. In particular, crimping can improve control over how the web material is gathered. Crimping is a process in which ripples are introduced into the web material. The crimping depth of the ripples can be variable and can also be quantified as the amplitude of the ripples.
[0025] Preferably, the crimped web material has a wave amplitude or crimp depth of 50 μm to 300 μm, more preferably about 100 μm to about 250 μm.
[0026] Cooling of the continuous web material within the forming device through the cooled contact surface also supports the gathering or forming step. The material contact surface is part of the forming device and includes a shape for forming the continuous web material or for maintaining the continuous web material in a specific shape according to this shape.
[0027] In a stepwise gathering forming process, the web material is gathered to a specific rod diameter in the first stage. In an additional gathering forming stage, the web material is gathered to smaller rod diameters down to a final diameter.
[0028] The final rod shape may have an outer diameter of 5 mm to 12 mm, preferably 6 mm to 10 mm.
[0029] Preferably, the rod manufactured by the method of the present invention has a circular or elliptical cross section.
[0030] Preferably, the method comprises the step of gathering a continuous web material into a rod shape in stages. Preferably, in the first gathering step, the method comprises the step of gathering a continuous web material from a flat shape into a rod shape having a first diameter. In the second gathering step, the method may further comprise the step of gathering a continuous web material from a rod shape having a first diameter to a final rod shape having a final diameter, wherein the final diameter is smaller than the first diameter.
[0031] In a preferred embodiment, the first diameter is in the range of 2 cm to 5 cm.
[0032] In a preferred embodiment, the final diameter is up to 12 mm.
[0033] Most of the heat is generated when the continuous web material is most compressed, and thus when the web material is compressed to its final load diameter. The continuous web material may be cooled during the first and second gathering steps. Preferably, the continuous web material may be cooled at least during the second gathering step and may be cooled only during the second gathering step. Cooling of the material contact surface is achieved by providing a cooling means that is in thermal contact with the forming device. Preferably, cooling of the material contact surface is achieved by providing a cooling fluid into or through the forming device. The cooling fluid may be a cooling liquid, for example, a mixture of water and glycol. Preferably, a mixture of about 50% water and about 50% glycol is used as the cooling fluid.
[0034] When operating, the cooling means provides a cooling temperature of less than 4°C. The cooling means may provide a cooling temperature of less than 2°C, 0°C, less than -2°C, less than -4°C, less than -6°C, less than -8°C, less than -10°C, or less than -20°C. Preferably, the cooling temperature is in the range of 3°C to -45°C, preferably 3°C to -20°C, and more preferably 0°C to -10°C.
[0035] When using a cooling fluid, the cooling fluid has a fluid temperature of less than 4°C. The cooling fluid may have a cooling temperature of less than 2°C, 0°C, less than -2°C, less than -4°C, less than -6°C, less than -8°C, less than -10°C, less than -15°C, less than -20°C, or less than -20°C. Preferably, the fluid temperature is in the range of 3°C to -30°C, preferably 3°C to -20°C, and more preferably 0°C to -15°C.
[0036] The surface temperature of the material contact surface is less than 4°C. The surface temperature of the material contact surface may be less than 2°C, 0°C, less than -2°C, less than -4°C, less than -6°C, less than -8°C, less than -10°C, less than -15°C, less than -20°C, or less than -25°C. Preferably, the surface temperature of the material contact surface is in the range of 4°C to -25°C, preferably 4°C to -20°C, more preferably 0°C to -15°C, for example, the surface temperature is about -5°C.
[0037] Preferably, the web material is cooled to a material temperature of less than 4°C. The web material may be cooled to a temperature of -30°C to 4°C, -20°C to 4°C, or -10°C to 0°C.
[0038] Preferably, the lower the surface temperature of the contact surface is controlled, the higher the speed of the web material passing through the contact surface.
[0039] Preferably, the method includes an additional step of measuring the cooling temperature of a cooling means, for example, a cooling fluid.
[0040] The above method may further include the step of providing a funnel to collect the web material. The funnel may include a cooling finger that contacts the web material in the highest compression area. The cooling finger may include a reservoir for a cooling fluid. Providing a reservoir for a cooling fluid can advantageously increase the thermal capacity of the cooling finger, in particular, where the reservoir is filled with a cooling fluid. The cooling effect may be further improved by circulating the cooling fluid within the reservoir or exchanging it continuously (or alternatively discontinuously).
[0041] The above method may further include the step of providing a cooling bar. The cooling bar may come into contact with the rods collected after the cooling funnel.
[0042] The step of measuring the temperature may be performed in the storage tank or inside the storage tank. The step of measuring the temperature may be performed at a cooling bar. Preferably, the method includes the step of cooling the fluid in the storage tank to a temperature of +4°C to -10°C. Preferably, the method includes the step of cooling the fluid at the end of the cooling bar to a temperature of +4°C to -10°C.
[0043] Accurately measuring the material temperature of a continuous web is difficult. Since the accumulation and generation of frictional heat can be a rapidly changing process, measurements of material temperature are often not very precise, particularly in terms of local material temperatures. For example, in a nearly final accumulated load of continuous web material, a large temperature difference may exist between the center of the load and locations on the periphery of the load.
[0044] Accordingly, preferably, the surface temperature of the cooled contact surface is measured. Preferably, the surface temperature of the cooled contact surface is measured during operation, and therefore preferably during the execution of the method according to the present invention or during the operation of the device according to the present invention. Preferably, the surface temperature of the cooled contact surface is measured while the continuous web material passes through and contacts the cooled contact surface. By measuring and controlling the surface temperature of the contact surface, the material temperature of the collected continuous web material can be controlled according to defined material parameters and process parameters. Preferably, the surface temperature of the cooled contact surface is measured at different locations during the forming process, for example, at different locations of the forming device.
[0045] The above method is,
[0046] - A step of packaging a continuous, rod-shaped, collected web material into a continuous strip of packaging material equipped with an adhesive;
[0047] - A step of cooling the rod contact surface of a rod cooling device having a cooling means to a rod contact surface temperature of less than 4°C, and a step of bringing a packaged rod of a continuous collected web material into contact with the cooled rod contact surface;
[0048] Accordingly, the method may include the step of cooling the packaging material wrapped around the load of the continuous collected web material by means of a cooled load contact surface that is equipped with an adhesive and contacts the packaged load. Preferably, the packaging material wrapped around the collected web material is cooled to a packaging temperature of less than 4°C.
[0049] After the continuous web material is gathered into a final rod shape, the rod proceeds to the packaging stage. There, the packaging material supplied with adhesive closes itself to wrap the web material and form a wrapped continuous rod of web material.
[0050] For packaging materials used to wrap collected web material, an adhesive is provided along at least the seams to seal the wrapper around the web material. This adhesive can be heated and then applied to the packaging material while hot. Alternatively or additionally, the packaging material may be equipped with an adhesive, which liquefies when the packaging material containing the adhesive is heated. Regardless of the application process, heat is supplied to the packaged load of web material. It has been found that the heat supplied when packaging the load can have the same negative effects on the web material as previously described in relation to heat generated by friction. This is particularly true when applied to web materials having a low glass transition temperature or a low melting temperature. Therefore, preferably, the heat supplied when packaging the web material should be limited, or the heat should be avoided from penetrating into the temperature-sensitive web material. For example, it has been found that conventional cooling of the packaged load by air can stabilize the adhesive on the packaging material but may not prevent heat from penetrating into the web material. In particular, it was found that when a packaged rod is cooled using a cooling means that provides a temperature of less than 4°C, the effect of the heated adhesive on the web material can be reduced or even avoided. In particular, the packaged rod can be cooled by contact with a rod contact surface having a rod contact surface temperature of less than 4°C.
[0051] Preferably, the wrapper is cooled to a packaging temperature of less than 4°C. The wrapper may be cooled to a temperature of, for example, -30°C to 4°C, -20°C to 4°C, or -10°C to 0°C.
[0052] After the packing material is packed around the load and closed, the reproducibility of the manufactured continuous load of the web material can be improved by supercooling the continuous web material during collection and supercooling the packed load of the web material. Material parameters can be maintained constant or within small variations, and melting of the material can be prevented or strongly limited during collection and packing.
[0053] According to the present invention, an apparatus for forming a continuous web material into a rod is also provided. The apparatus includes a forming device for forming a continuous web material from a flat shape into a rod shape. The forming device includes a funnel portion for providing a rod shape to the continuous web material. The forming device includes a material contact surface for contacting the continuous web material that can be guided through the funnel portion. The apparatus also includes a cooling means for providing a cooling temperature of less than 4°C. The forming device is connected to the cooling means and is suitable for cooling the material contact surface of the forming device to a surface temperature of less than 4°C. Here, the material contact surface is arranged along the length of the funnel portion of the forming device and is gathered in the funnel portion while cooling the continuous web material.
[0054] Preferably, the cooling means is a source of cooling fluid having a temperature of less than 4°C. In these embodiments, the molding device is fluidly connected to the source of cooling fluid.
[0055] Preferably, the device includes a packaging device for packaging a rod-shaped web material into a continuous strip of packaging material. An adhesive is provided on the packaging material.
[0056] Preferably, the device includes a load cooling device comprising a load contact surface for contacting a packaged load of web material. The load cooling device is suitable for cooling the load contact surface of the packaging device to a load contact surface temperature of less than 4°C. By doing so, the packaging material packaged around the load of web material is cooled to a packaging temperature, preferably a packaging temperature of less than 4°C.
[0057] To cool the rod contact surface, the rod cooling device is connected to a cooling means that provides a cooling temperature of less than 4°C. Preferably, to cool the rod contact surface, the rod cooling device is fluidly connected to a source of cooling fluid having a fluid temperature of less than 4°C.
[0058] The same cooling means providing a cooling temperature of less than 4°C can be used to cool the molding device and the rod cooling device. Separate cooling means can be used for the molding device and the rod cooling device. The separate cooling means can, for example, provide different temperatures or can be based on different cooling methods, such as cooling means in the form of a Peltier element or using a cooling fluid.
[0059] For example, the same source of cooling fluid having a fluid temperature of less than 4°C may be used to cool a molding device and a load cooling device. Separate sources of cooling fluid may be used for the molding device and the load cooling device. Separate sources of cooling fluid may include, for example, cooling fluids having different temperatures or different fluid compositions.
[0060] The advantages of a device for supercooling a web material while the web is gathered and formed into a load, preferably also while it is supercooled after being formed into a load and packaged, have been described in connection with the method according to the present invention and will not be repeated.
[0061] The step of gathering the continuous web material from a flat shape into a rod shape preferably includes the step of gathering the continuous web material continuously in a direction perpendicular to the conveying direction of the continuous web material. This gathering is preferably performed by a stationary forming device. This is a particularly simple method of gathering the web material compared to, for example, using a moving forming device.
[0062] Preferably, the forming device includes a funnel portion, and at least a portion of the funnel portion includes an upper funnel portion and a lower transfer plane including a converging groove extending in the longitudinal direction.
[0063] The upper funnel portion and the lower transfer plane can together form a forming device. The upper funnel portion and the lower transfer plane can also at least partially form a forming element. Thus, additional forming elements may be provided to form an extra funnel portion or a winding device arranged upstream of the forming device, for example, the forming device. The extra funnel portion may be, for example, a metal funnel. Preferably, the funnel is coated with or composed of an anti-friction material.
[0064] In some embodiments, the upper funnel portion forms half of the forming device, for example, the upper half. In these embodiments, the lower transfer plane forms the other half of the forming device, for example, the lower half of the forming device.
[0065] The upper funnel portion provides a concave circumferential shape to a portion of the continuous web material. A lower feed plane or groove extending within the feed plane closes the funnel portion along the remaining circumference so that the continuous material is guided within the forming device.
[0066] Preferably, the funnel portion has an internal concave shape to provide a circular or elliptical circumferential shape to the continuous web material. In particular, the material contact surface of the forming device, more specifically the upper funnel portion, may have a concave shape. Preferably, the material contact surface of the forming device has a converging concave shape that converges in the direction of transport of the web material.
[0067] Preferably, the surface temperature of the material contact surface is measured at one, more preferably two or more locations on the contact surface.
[0068] An extra funnel portion arranged upstream of a forming device, preferably comprising a funnel with a cooled contact surface, comprises a structural surface. The structure can reduce direct contact between the funnel surface and the web material passing through the funnel. This can reduce the generation of frictional heat. The structure can also reduce the cooling action of the funnel on the web material.
[0069] Preferably, the surface structure of the funnel is selected such that contact or non-contact between the structured surface of the funnel and the continuous web material changes as the web material passes through the funnel. Preferably, the structure is selected such that the same portion of the web material passing through the structured surface of the funnel does not constantly or permanently contact the structure of the structured surface of the funnel.
[0070] The structure may be a regular structure or a random structure. The structure may be, for example, a wavy line structure, a branching or converging line structure, and preferably a dimple structure in which the dimples are arranged in a manner that the dimples are laterally displaced when viewed along the transport direction of the web material.
[0071] The transfer plane of the forming device can serve to support a continuous strip of packaging material. The forming method preferably includes the step of guiding a continuous strip of packaging material along the transfer plane of the forming device.
[0072] A continuous web material can be arranged on a packaging material and transported on the packaging material in a downstream transport direction. Preferably, the grooves within the transport plane are concave shapes that converge laterally. The grooves may extend along the entire length or only along a portion of the length of the transport plane.
[0073] The packing material forms an inner liner of a groove that partially packs the continuously gathered web material. After the continuous web material is gathered into its final rod shape, the packing material is completely wrapped around the rod, securing the rod in its rod shape. This continuous or merged rod formation and packing is particularly advantageous for elastic web materials that tend to resist gathering, such as many types of plastic foil.
[0074] Advantageously, the load cooling device is arranged downstream of the forming device and downstream of the packaging device. Additionally, the load cooling device may be integrated within the packaging device or packaging element so that cooling of the packaging material can occur simultaneously with or immediately after packaging.
[0075] Preferably, the rod contact surface of the rod cooling device has a concave shape. Preferably, the shape of the rod contact surface is constant along the length of the rod cooling device.
[0076] Preferably, a portion of the load cooling device including a load contact surface is detachably mounted on a transfer plane. This allows the packaging process to be observed. Preferably, the load contact surface is in contact with the packaging material. Preferably, the load contact surface is in thermal contact with at least a thermally conductive portion of the load cooling device, and preferably, the load contact surface is in thermal contact with a thermally conductive portion of the packaging device.
[0077] The rod contact surface extends along the longitudinal extension of the rod or along the conveying direction. The rod contact surface may have a length of about 10 cm to about 80 cm, preferably about 30 cm to 60 cm, in the conveying direction of the web material.
[0078] Preferably, the temperature of the rod contact surface is measured at one, more preferably two or more, location along the length of the rod contact surface.
[0079] The material contact surface extends along the funnel section in the direction of the web material's transport. The material contact surface may extend from the upstream end of the funnel section to the downstream end of the funnel section. In particular, the material contact surface may extend from the upstream end of the upper funnel section to the downstream end of the upper funnel section. Accordingly, the supercooling of the continuous web material occurs in the gathering section, where most of the friction occurs and most of the heat due to frictional forces is generated. The material contact surface may extend from the upstream end of the forming device to the downstream end of the forming device. Accordingly, the web material can be cooled from a flat rod shape to a final rod shape during gathering.
[0080] The material contact surface and the rod contact surface extend along at least a portion of the circumference or periphery of the gathered web material or rod. The contact surface may extend about 90 to 360 degrees along the circumference of the web material. Thus, the cooled contact surface may partially or wholly surround the web material. Preferably, the contact surface extends at least about 90 degrees along the circumference of the web material. More preferably, the contact surface extends at least about 180 degrees along the circumference of the web material. Preferably, the contact surface is cooled through thermal contact with a cooling means, preferably a cooling fluid.
[0081] The actively cooled part of the device is in thermal contact with another part of the device, so that the contact surface can be cooled through thermal contact with the actively cooled part of the device.
[0082] Preferably, the actively cooled upper funnel portion is in thermal contact with the transfer plane. Perhaps through a strip of packing material arranged beneath the web material, a groove within the transfer plane acting as a lower contact surface for the web material can be cooled through thermal contact with the upper funnel portion. Accordingly, a 360-degree cooling contact surface is available for the web material gathered between the upper funnel portion and the lower transfer plane.
[0083] Preferably, the device component in thermal contact with the contact surface is made of a good thermal conductor, for example, metal. Preferably, the thermally conductive material used for the cooling element or the connecting component between the cooling element and the contact surface has a thermal conductivity of at least 10 W / mK. Preferably, the thermally conductive material used to cool the web material in the device of the present invention has a thermal conductivity of at least 200 W / mK.
[0084] For example, a continuous web material as used herein is a web of material used, for example, in the manufacture of an aerosol generating article for an electronic smoking device. Preferably, the continuous web material is a plastic web, for example, a continuous web of polylactic acid. The continuous web material may be an aerosol-forming substrate.
[0085] In some embodiments, a continuous web material may be immersed or impregnated with an aerosol-forming material. Then, such a continuous web material may be a non-aerosol-forming substrate. Immersion or impregnation may be performed before crimping, before gathering of the continuous web material, or during gathering. Preferably, when heating the aerosol-forming substrate or when heating the continuous web material immersed or impregnated with the aerosol-forming material, the material is released from the substrate or the web material, and this material may form an inhalable aerosol.
[0086] Preferably, the continuous web material is formed into an endless rod shape for the subsequent manufacture of individual plugs. When the rod is formed, a susceptor may be inserted into the rod. For example, a susceptor strip may be inserted into the continuous web material during the gathering of the web material. By this, an induction-heatable rod or plug may be manufactured.
[0087] Preferably, the continuous web material is pretreated before being formed in the device according to the present invention. The pretreatment is, for example, crimping or embossing, or both.
[0088] Preferably, the method comprises the step of providing a crimped continuous web material having crimps arranged longitudinally. The crimps are arranged in the transport direction of the web material. When gathered, the continuous web material forms longitudinal channels along the crimps. The longitudinal channels define the suction resistance of an article formed by the gathered web material or including plugs of the gathered web material. By preventing the merging of these longitudinal channels by the melting of the web material upon gathering, reproducibility of the suction resistance of the gathered web material can be achieved. Preventing the merging of longitudinal channels is particularly advantageous when using otherwise substantially gas impermeable web material.
[0089] The continuous web material used in the method according to the present invention has a glass transition temperature of less than 150°C. Preferably, the continuous web material has a glass transition temperature of less than 100°C. Since the glass transition temperature is less than the melting temperature, the continuous web material also preferably has a melting temperature of about 150°C or less. Since the glass transition temperature refers to a range rather than an exact temperature, the glass transition temperature preferably includes ±20°C around a specific glass temperature, and more preferably ±5°C around a specific glass transition temperature.
[0090] Preferably, the continuous web material has a porosity of less than about 5%, preferably less than about 2%. Most preferably, the continuous web material is gas impermeable, for example, air impermeable.
[0091] Preferably, the material used to form the continuous rod has low porosity or is substantially non-porous.
[0092] Porosity is defined herein as a measure of pores or openings extending through a web material. For example, if a web material contains openings or pores that add up to 50% of the web area, the porosity will be 50%. Likewise, if a web material is completely dense without pores extending through the material, the web material has 0% porosity. Porosity may be measured or calculated using known methods.
[0093] The rod is composed of, for example, a web material such as a polymer web or polyethylene (having a glass transition temperature of about -130°C to about -80°C; a melting temperature of about 115°C to about 130°C), polypropylene (having a glass transition temperature of about -20°C to about 0°C; a melting temperature of about 130°C to about 170°C), polyvinyl chloride (having a glass transition temperature of about 60°C to about 87°C; a melting temperature of about 160°C to about 260°C), polyethylene terephthalate (having a glass transition temperature of about 70°C; a melting temperature of less than about 250°C), polylactic acid (having a glass transition temperature of about 50°C to about 65°C; a melting temperature of about 155°C), or cellulose acetate (having a glass transition temperature of about 100°C to about 130°C; a melting temperature of about 170°C to about 240°C). It can be formed from web materials selected from the military.
[0094] The apparatus and method according to the present invention are particularly suitable for materials having a low glass transition temperature. A continuous web material formed in the apparatus and formed according to the present invention has a glass transition temperature of less than 150°C, for example, less than 100°C. Preferably, the continuous web material is a plastic material, for example, polylactic acid. The continuous material may be a crimped continuous web material. Brief explanation of the drawing
[0095] The present invention is further described in relation to embodiments illustrated by the following drawings, wherein: FIG. 1 is a schematic diagram of the funnel stage of the rod manufacturing process; Figure 2 shows a molding and cooling device; Figure 3 shows the device of Figure 2 having a load cooling device. Specific details for implementing the invention
[0096] Fig. 1 The manufacturing process schematically illustrated in and Fig. 2In the apparatus illustrated in [Image], a continuous web material (1), for example, polylactic acid, is released from a storage bobbin (not shown). The web of polylactic acid is preferably transferred through a compression process to a molding process in a molding device (2), for example, in which the web material (1) is collected and compressed into a continuous load.
[0097] The web material (1) enters the half-funnel of the upper molding element (20) in the processing and transfer direction indicated by arrow 100.
[0098] Rod forming is performed through an upper forming element (20) and a lower closing element (21). The upper forming element (20) is arranged opposite the closing element (21). The forming element (20) is a semi-funnel and forms the web material (1) from the top. The closing element (21) is a transfer plane containing a groove, where a packaging material, e.g., a wrapping paper (5), is guided within the groove to wrap the rod-shaped web material (1) along the web material. At the bottom of the forming device (2), along the transfer plane, the web material (1) also comes into contact with the wrapping paper (5), which moves along the transfer direction (100) at the same speed as the web material (1). The wrapping paper (5) is placed on a garnish tape (51) that pulls the wrapping paper (5). By doing so, the web material (1) is also pulled into and through the funnel of the forming device (2).
[0099] The groove within the transfer plane of the closing element (21) typically takes on a progressively concave shape to support the compression and molding of the web material (1). Downstream of the molding device (2), the packaging material is folded and closed to form a continuous cylindrical packaging rod, preferably a polylactic acid rod wrapped in paper. The rod can subsequently be cut into individual plugs, thereby generating components or parts used in the manufacturing process of an aerosol-generating article.
[0100] At a conveying speed of about 200 meters / min to about 500 meters / min, substantial friction occurs between the web material (1) and the fixed forming device (2), which is preferably metal. In the region where the web material is most compressed, the web material is heated the most. This is indicated by line 200 in FIG. 1.
[0101] As shown in FIG. 2, the web material is gathered slightly in the upstream funnel (22). The upstream funnel (22) is made of metal having a structured surface to reduce contact between the web material (1) and the surface of the upstream funnel (22).
[0102] The structure of the funnel surface is a dimple structure in which the dimples are arranged laterally displaced from each other when viewed along the direction of transport of the web material. Accordingly, when the web material (1) passes through the upper funnel (22), it makes discontinuous contact with the wall surface of the upstream funnel (22).
[0103] In addition, the material of the upstream funnel (22) is an anti-friction material or has an anti-friction coating.
[0104] To avoid friction-related overheating of the web material (1) exceeding the glass transition temperature or melting temperature of the web material, the contact surface of the upper funnel part (20) is cooled.
[0105] The contact surface is cooled to a temperature below 0°C by using a cooling fluid having a temperature below 0°C. For example, the contact surface of the half-funnel part (20), as well as the cooling fluid, has a temperature of about -5°C. Preferably, the cooling fluid is a mixture of 50% water and 50% glycol.
[0106] A cooling element (34) is arranged on top of an upper half-funnel (20). The cooling element (34) is cooled by a cooling fluid circulating through a cooling fluid circuit within the cooling element (34). The cooling element (34) is in direct contact with the upper half-funnel (20) and can be manufactured as a single piece together with the upper half-funnel (34). The cooling element (34) maintains the wall surface of the funnel at a temperature below 0°C. As the web material (1) comes into direct contact with the wall surface of the funnel, the web material is cooled through the contact surface of the funnel wall. The cooling element is partially hollow, creating an internal reservoir of about 100 milliliters.
[0107] The cooling fluid is introduced into the upstream portion of the cooling element (34) through the fluid inlet (23) and passes inward along the cooling element (34). The cooling fluid leaves the cooling element (34) at the downstream end of the cooling element at the fluid outlet (24). The cooling element (34) through which the cooling fluid passes is in thermal contact with the upper half-funnel (20) and the contact surface of the upper half-funnel. The upper half-funnel, as well as the cooling element (34), are made of a thermally conductive material, such as a metal like copper.
[0108] Preferably, the closing element (21), particularly the transfer plane including the groove, is in thermal contact with the cooled upper half-funnel (20). Through this thermal contact, the lower surface of the continuous web material (1) passing through the forming device (2) is also indirectly cooled by the cooling element (34). Preferably, the closing element (21) is made of a thermally conductive material, such as metal, to support the heat transfer of cold air from the cooling element (34) to the groove within the transfer plane.
[0109] The contact surface has a concave shape that converges toward the contact surface and the downstream end of the upper half-funnel (20). Accordingly, the web material (1) is gathered and formed into a rod shape in the forming device and is cooled constantly by the contact surface having a temperature of less than 0°C. Thus, the temperature of the web material is maintained much lower than its melting temperature and much lower than its glass transition temperature.
[0110] Preferably, the web material itself is cooled to a temperature below 4°C. In the case of a polylactic acid web, the temperature of the material is preferably maintained below 30°C. Preferably, this is achieved by lowering the temperature of the cooling fluid in the reservoir of the cooling element (34) to about -5°C.
[0111] Examples of lengths (37) in which the web material is cooled while in direct contact with the cooled contact surface of the forming device (2) are about 0.05 meters and 0.5 meters. Preferably, these lengths correspond to the length of the upper half-funnel (20) of the forming element.
[0112] Fig. 3 In this, part of the molding device (2) of FIG. 2, as well as the packaging part and load cooling device (6) arranged downstream, can also be seen.
[0113] The web material (1) formed into a rod in the forming device (2) is completely wrapped in a packaging material in the rod forming device (50). In the rod forming device (50), the packaging material (5) has a glue joint and closes itself to form a wrapped rod of the web material.
[0114] The load cooling device (6) is arranged immediately downstream of the packaging device. The load cooling device (6) includes a longitudinal body (60) arranged over the conveying plane (11) and over the groove (12) where the packaged load of the web material is guided.
[0115] The body (60) of the rod cooling device (6) includes a cooling fluid inlet (63) at its upstream end and a cooling fluid outlet (64) at its downstream end. Preferably, the cooling fluid is the same as the cooling fluid used to cool the molding device (2). The cooling fluid for cooling the packaged rod has a temperature of less than 0°C, for example, about -5°C. The cooling fluid passes through the rod cooling device (6) and cools the rod cooling contact surface (61) of the rod cooling device (6) to a temperature of less than 0°C.
[0116] The rod contact surface extends along the body (60) and preferably has a concave shape to make clean contact with the wrapped rod of web material passing under the rod contact surface (61).
[0117] At least one body (60) having a load cooling device (6) or a load contact surface (61) is rotatable around an arm so as to be lifted from a cooling position into a contracted position. In the cooling position, the load cooling device (6) essentially forms a loop over a garnish tape (51) guided along a transfer plane (11). In FIG. 3, the load cooling device (6) is shown in the contracted position. In the contracted position, the load cooling device (6) allows free access and visibility to the load cooling portion of the packaging and manufacturing processes.
Claims
Claim 1 A method for forming a continuous web material into a rod, the method comprising: - providing a continuous web material having a glass transition temperature of less than 150°C; - gathering the continuous web material from a flat shape into a rod shape by a forming device; - providing a cooling means providing a temperature of less than 4°C and cooling the material contact surface of the forming device to a surface temperature of less than 4°C; and - cooling the continuous gathered web material by the cooled material contact surface in contact with the continuous gathered web material. Claim 2 A method for forming a continuous web material into a load according to claim 1, further comprising the step of cooling the continuous collected web material to a material temperature of less than 4°C. Claim 3 A method for forming a continuous web material into a rod, wherein, in claim 1 or 2, the cooling means is a mixture of a cooling fluid and a glycol. Claim 4 A method for forming a continuous web material into a rod, wherein, in paragraph 3, the cooling means provides a cooling temperature of 3°C to -45°C. Claim 5 A method for forming a continuous web material into a rod according to claim 1, wherein the surface temperature of the material contact surface is 3°C to -45°C. Claim 6 A method for forming a continuous web material into a load, wherein, in claim 1, the step of guiding a continuous strip of packaging material along a transfer plane of the forming device is further included. Claim 7 A method for forming a continuous web material into a rod according to claim 1, comprising a step of stepwise gathering the continuous web material into a rod shape, wherein the step includes a first gathering step of gathering the continuous web material from a flat shape into a rod shape having a first diameter; and a second gathering step of further gathering the continuous web material from the rod shape having a first diameter into a final rod shape having a final diameter smaller than the first diameter. Claim 8 A method for forming a continuous web material into a rod according to claim 1, further comprising: - a step of packaging a continuous collected web material in the shape of a rod with a continuous strip of packaging material having an adhesive; - a step of cooling a rod contact surface of a rod cooling device having the cooling means to a rod contact surface temperature of less than 4°C and bringing the packaged rod of the continuous collected web material into contact with the cooled rod contact surface; and accordingly, a step of cooling the packaging material packaged around the rod of the continuous collected web material by the cooled rod contact surface having an adhesive and contacting the packaged rod. Claim 9 A method for forming a continuous web material into a rod according to claim 8, wherein the continuous web material has a glass transition temperature of less than 100°C. Claim 10 A method for forming a continuous web material into a rod, wherein, in claim 9, the continuous web material is a plastic material, for example, polylactic acid. Claim 11 A device for forming a continuous web material into a rod, wherein the device comprises: a forming device for forming a continuous web material from a flat shape into a rod shape, wherein the forming device comprises a funnel portion for providing a rod shape to the continuous web material, wherein the forming device comprises a material contact surface for contacting the continuous web material that is guideable through the funnel portion; and the device further comprises a cooling means for providing a cooling temperature of less than 4°C, wherein the forming device is connected to the cooling means and is suitable for cooling the material contact surface of the forming device to a surface temperature of less than 4°C, and the material contact surface is arranged along the length of the funnel portion of the forming device and is collected in the funnel portion while cooling the continuous web material. Claim 12 In claim 11, the apparatus for forming a continuous web material into a rod further comprises: a packaging device for packaging the rod-shaped web material into a continuous strip of packaging material; and a rod cooling device comprising a rod contact surface for contacting the packaged rod of the web material, wherein the rod cooling device is suitable for cooling the rod contact surface of the packaging device to a rod contact surface temperature of less than 4°C, and accordingly, cooling the packaging material packaged around the rod of the web material. Claim 13 An apparatus for forming a continuous web material into a rod, wherein, in paragraph 12, the material contact surface and the rod contact surface have a concave shape. Claim 14 An apparatus for forming a continuous web material into a rod, wherein the funnel portion comprises an upper funnel portion and a lower transfer plane including a converging groove extending in the longitudinal direction. Claim 15 An apparatus for forming a continuous web material into a rod, wherein the material contact surface extends from the upstream end of the upper funnel portion to the downstream end of the upper funnel portion.
Citation Information
Patent Citations
Production method of filter rod with tai chi appearance and equipment thereof
CN101926510A
Improved filter rod maker for handling stiff wrapping web material
EP3328221B1
Machine for making rods of smokable material and cooling apparatus therefor
US20050109352A1
Method and apparatus for shaping substantially flat continuous material
US20170332695A1
Method for shaping a continuous web material into a rod
WO2018210982A1