Method for manufacturing optical elements
The nP3 process addresses low accuracy in optical manufacturing by depositing and etching a profiling film to achieve precise geometric variations, improving substrate flatness and light coupling in optical elements.
Patent Information
- Application Number
- KR1020237001009
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-06-08
- Filing Date
- 2021-06-07
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2041-06-07
AI Technical Summary
Current optical manufacturing technologies suffer from low processing accuracy due to light absorption and curing reactions occurring beyond the focused point, leading to inaccuracies in specialized optical components like microlenses and waveguides.
The nanoscale precision programmable profiling (nP3) process deposits a profiling film with a customized thickness profile on a substrate, followed by plasma etching to introduce precise geometric variations, correcting aberrations and improving substrate flatness.
Enhances processing accuracy by allowing controlled customization of geometric parameters, correcting aberrations and ensuring uniform light coupling/intensity across optical elements, particularly in augmented and mixed reality waveguides.
Smart Images

Figure R1020237001009_ABST
Abstract
Description
Technology Field
[0001] (Cross-reference of related applications)
[0002] This application claims priority to the U.S. provisional patent application No. 63 / 036,087, filed on June 8, 2020, titled “Fabrication of Optical Elements,” the contents of which are incorporated herein by reference.
[0003] The present invention generally relates to optical manufacturing, and more specifically to manufacturing an optical element on a substrate using a nanoscale precision programmable profiling process. Background Technology
[0004] Optical manufacturing includes the production of optical components such as lenses, prisms, mirrors, microlenses, gradient-index lenses, diffractive optics, and waveguides. When optical components such as lenses, prisms, and mirrors are manufactured in an optical workshop, various processes such as cutting, grinding, lapping, and polishing may be applied to ultimately produce high-quality optical surfaces.
[0005] However, for specialized optical components such as microlenses, refractive index distributed lenses, diffractive optics, and waveguides, more complex manufacturing techniques are utilized. Examples of these complex manufacturing techniques include magnetorheological finishing, polishing using deformable tools, and computer-controlled polishing.
[0006] Unfortunately, the processing accuracy of currently used optical manufacturing technologies is low. For example, in conventional optical manufacturing methods utilizing ultraviolet irradiation, light is absorbed and a curing reaction occurs not only at the light-focused point but also in the irradiated areas. As a result, the processing accuracy is low.
[0007] In one embodiment of the present invention, a method for introducing a customized variation of a geometric parameter in a nanoscale pattern on a substrate comprises the step of performing a nanoscale precision programmable profiling process in one or more regions of a substrate having a nanoscale pattern, wherein the nanoscale precision programmable profiling process is used to deposit a profiling film with a thickness profile that is a function of the customized variation of the geometric parameter in the nanoscale pattern. The present method further comprises the step of performing a plasma etching process of the material of the profiling film and the nanoscale pattern to convert the thickness profile of the profiling film into a customized variation of the geometric parameter in the nanoscale pattern, wherein the customized variation is a function of the thickness profile of the profiling film.
[0008] In another embodiment of the present invention, a method for correcting one or more aberrations in a waveguide substrate comprises the step of performing a nanoscale precision programmable profiling process on an unpatterned portion of a waveguide substrate by depositing a profiling film on the unpatterned portion of the waveguide substrate along with a customized modification for correcting one or more aberrations in the waveguide substrate.
[0009] In addition, in one embodiment of the present invention, an apparatus for introducing a customized variation of a geometric parameter into a nanoscale pattern on a substrate comprises a profiling module, wherein the profiling module has an inkjet for depositing a profiling film on a substrate with a thickness profile that is a function of the customized variation of the geometric parameter in the nanoscale pattern on the substrate, wherein a plasma etch process for converting the thickness profile of the profiling film into a customized variation of the geometric parameter in the nanoscale pattern on the substrate is performed on the material of the profiling film and the nanoscale pattern, wherein the customized variation is a function of the thickness profile of the profiling film.
[0010] Additionally, in one embodiment of the present invention, the XR device comprises a waveguide manufactured by nanoscale precision programmable profiling for introducing customized variation to geometric parameters of a nanoscale pattern on the waveguide, correction of substrate flatness or total thickness variation errors, and correction of image distortion or optical aberrations.
[0011] The foregoing description outlines the features and technical advantages of one or more embodiments of the present invention in a somewhat general manner to better facilitate the detailed description of the present invention set forth below. Additional features and advantages of the present invention that may form the subject matter of the claims of the present invention will be described below. Brief explanation of the drawing
[0012] The present invention may be better understood when the following detailed description is considered together with the following drawings. FIG. 1 is a schematic diagram of an nP3 device according to one embodiment of the present invention. FIG. 2 is a schematic diagram of a profiling subsystem of an nP3 device according to one embodiment of the present invention. FIG. 3 is a flowchart of a method for manufacturing a device on a flat substrate using a nanoscale precision programmable profiling (nP3) process according to one embodiment of the present invention. FIG. 4a to 4h illustrate cross-sectional views for manufacturing a device on a flat substrate using the processes described in FIG. 3 according to one embodiment of the present invention. FIG. 5 is a flowchart of a method for manufacturing an optical device on a flat substrate using a nanoscale precision programmable profiling (nP3) process together with a superstrate according to one embodiment of the present invention. FIG. 6a to 6h illustrate an optical device on a flat substrate using an nP3 process together with a superstrate using the processes described in FIG. 5 according to one embodiment of the present invention. A cross-sectional view for manufacturing the device is illustrated. FIG. 7 illustrates a waveguide substrate having a nanoscale pattern region as an incoupling diffractive optical element (DE) and an outcoupling DOE according to one embodiment of the present invention. FIG. 8 illustrates a waveguide substrate having a nanoscale pattern region as an incoupling DOE and an outcoupling DOE, with the nanoscale pattern region illustrated with a customized variation of geometric parameters according to one embodiment of the present invention. FIG. 9 illustrates having a plurality of nanoscale pattern regions on the same substrate according to one embodiment of the present invention. FIG. 10 illustrates using an nP3 process on an unpatterned portion of a waveguide substrate to correct aberrations according to one embodiment of the present invention.FIG. 11 illustrates a method for introducing customized deformation to the geometric parameters of a nanoscale pattern using substantially similar etch rates for a profiling and nanoscale pattern material according to one embodiment of the present invention. FIG. 12a to 12d illustrate cross-sectional views for introducing customized deformation to the geometric parameters of a nanoscale pattern using the processes described in FIG. 11 according to one embodiment of the present invention. FIG. 13 illustrates a method for introducing customized deformation to the geometric parameters of a nanoscale pattern using different etch rates for a profiling and nanoscale pattern material according to one embodiment of the present invention. FIG. 14a to 14d illustrate cross-sectional views for introducing customized deformation to the geometric parameters of a nanoscale pattern using the processes described in FIG. 13 according to one embodiment of the present invention. Specific details for implementing the invention
[0013] As mentioned above, the processing accuracy of currently used optical manufacturing technology is low. For example, in conventional optical manufacturing methods utilizing ultraviolet irradiation, light is absorbed and a curing reaction occurs not only at the point of concentration but also in the irradiated parts. As a result, the processing accuracy is low.
[0014] The principle of the present invention provides a method for improving process accuracy when fabricating optical devices using a process referred herein as "nanoscale precision programmable profiling (nP3)". The nP3 process can be used in the context of fabricating optical devices, such as waveguides for augmented and mixed reality applications, or diffractive optical devices having one or more different geometric properties (e.g., depth). In one embodiment, such diffractive optical devices are part of a waveguide and can be used for in-coupling light from a projector, pupil dilation, or out-coupling to the eye. Generally, the nP3 process can be applied to introduce desired customized variations to the geometric parameters of existing nanoscale patterns. Discussion regarding the nP3 process is made in international application no. PCT / US 14 / 51526, titled "Programmable Deposition of Thin Films of a User-Defined Profile with Nanometer Scale Accuracy," filed on August 18, 2014, and international application no. PCT / US 21 / 19732, titled "Nanoscale Thin Film Deposition Systems," filed on February 25, 2021, the entire contents of both applications are incorporated herein by reference.
[0015] In one embodiment of the process, a nanoscale precision programmable profiling (nP3) process is performed on a flat substrate. This flat substrate may include one or more regions having a nanoscale pattern, and these nanoscale patterns may be similar or substantially different from region to region. In one embodiment, the flat substrate represents a waveguide substrate used in virtual, augmented, or mixed reality (collectively, XR) applications. In one embodiment, the region having the nanoscale pattern represents a diffractive optical element used for waveguide optical coupling, where the diffractive optical element may be used to incouple light from a projector, dilate the pupil, or outcouple light to the eye. The nP3 process causes a profiling film to be deposited on one or more regions having the nanoscale pattern so that the profiling film has a desired customized thickness variation. In one embodiment, the profiling film has optical properties that substantially match the nanoscale pattern. In one embodiment, the profiling material is a UV-curable polymer resist (e.g., mrUVcur26SF from Microresist Technologies). This thickness variation is a function of a desired customized variation of one or more geometric parameters of the nanoscale pattern, such geometric parameters including, but not limited to, the height of the feature portion of the pattern, the width of the feature portion of the pattern, and the angle of the feature portion of the pattern. The desired customized variation of the geometric parameters may differ from one another in different regions of the substrate having the nanoscale pattern. For example, a first region may require a different height profile compared to a second region, while a third region may have the same variation as the first region but a different orientation. This customized variation of one or more geometric parameters of the nanoscale pattern is intended to provide desirable functional or optical properties to the waveguide.In one embodiment, this characteristic includes maintaining substantially uniform coupling intensity across the outcoupling or pupil dilation optical element. Additionally, in one embodiment, the nanoscale pattern exists on the substrate, whereas in another embodiment, the nanoscale pattern is formed on another material on the substrate, such as a functional film (e.g., a high refractive index polymer material, e.g., Material #18165 of Nippon Telegraph and Telephone-Advanced Technology). As used in this disclosure, the nanoscale pattern material refers to the substrate or the other material mentioned above on the substrate used to form the nanoscale pattern. The thickness profile is transferred to the nanoscale pattern material via a plasma etching process to introduce a desired customized variation of one or more geometric parameters in the nanoscale pattern on the substrate. In one embodiment, multiple iterations of the profiling or plasma etching process are used to introduce the customized variation. An example of the nP3 process on a flat substrate is described below.
[0016] Referring to the drawings in detail, FIG. 1 is a schematic diagram of an nP3 device (100) according to one embodiment of the present invention.
[0017] The nP3 device (100) consists of two main subsystems: profiling (101) and metrology (102). The profiling subsystem includes a web handling module composed of unwind and rewind rollers, rollers for interleaving and de-interleaving, drive rollers, nip rollers for tension control, and precision rollers to ensure a flat area. Sidelays ensure that the webs are wound together without lateral error (telescoping). An inkjet printhead on an alignment stage dispenses the profiling material droplets. A UV lamp and a UV transparent (UVT) chuck are used to create air-pressure induced curvature to cure the profiling material and hold the top plate in place while spreading the profiling material droplets. A flexure bearing stage driven by a voice coil motor holds the substrate chuck under the top plate and is mounted on a linear horizontal stage (103) as illustrated. The measurement subsystem includes a sensor for measuring surface topography (Shack-Hartman sensor, optical profilometer, interferometer, reflectometer, or spectrophotometer) mounted directly above the substrate. A laser beam is guided through the substrate via an automated telescopic system and incident on the sensor. A telescopic system is required when processing curved substrates with a spherical power range. The laser beam alignment system includes a turn mirror that directs the horizontal laser beam vertically upward through the substrate.In one embodiment, the nP3 device (100) also has a communication module that enables local transmission and exchange of data with another computer or another data center / workstation located remotely (e.g., a cloud-based data center, a cloud-based workstation). This data may include measurement data, tool sensor data, drop pattern data, etc.
[0018] Referring again to FIG. 1, the nP3 device (100) further includes a granite base and a support table (104).
[0019] Referring to FIG. 2, FIG. 2 is a schematic diagram of a profiling subsystem (200) of an nP3 device (100) according to one embodiment of the present invention.
[0020] As illustrated in FIG. 2, the profiling subsystem (200) comprises an electric interleaf / de-interleaf roller (201), a nip roller (213), a sidelay module (202), precision idlers (203), a UV clear vacuum chuck (119), a stage (204) driven by a voice coil motor (VCM) for vertical, tip, and tilt movements, a motorized supply and take-up roller (205), a drive roller (206), a curing module (207), a stationary inkjet printhead (208), a profiling material (209), a rigid substrate (210), a vacuum pin chuck (211), and a large travel stage (212). In one embodiment, the rigid substrate (210) is nominally flat or nominally non-flat (e.g., spherical, non-spherical). As used herein, "rigid" substrate means having a permanent shape and form. As used herein, "nominally flat" means a surface having a distinct contact area large enough that individual contacts are dispersed and forces acting through adjacent points do not affect each other. As used herein, "nominally non-flat" refers to a surface that is not nominally flat.
[0021] As shown in FIG. 2, the inkjet printhead (208) is fixed in a large direction of movement (212).
[0022] Additionally, FIG. 2 illustrates the web path followed by the top plate and interleaf film during removal and reapplication. In FIG. 2, tension control is achieved through the nip and drive roller assembly (see 213 and 206). In one embodiment, a polyurethane roller is used to apply normal pressure to the drive roller (206) to improve friction and allow for higher tension limited by the motor capacity. In one embodiment, it is ensured that the nip roller (213) is axially parallel to the drive roller (206). A UV lamp is positioned directly above the profiling area. A UV clear vacuum chuck (119) is located between the top plate and the UV lamp. A precision idler (203) flattens the top plate and minimizes out-of-plane errors and in-plane shear errors. A stage (204) driven by a voice coil motor is mounted on a horizontal XY stage. The substrate is moved from the jetting station to the profiling station and then to the measurement station using the XY stage.
[0023] FIG. 3 is a flowchart of a method (300) for manufacturing a device on a flat substrate using a nanoscale precision programmable profiling (nP3) process according to an embodiment of the present invention. FIGS. 4a to 4h illustrate cross-sectional views for manufacturing a device on a flat substrate using the processes described in FIG. 3 according to an embodiment of the present invention.
[0024] Referring to FIG. 3 together with FIG. 4a through 4h, in process (301), a profiling material (401) is distributed onto a substrate (402) using an inkjet (403) as shown in FIG. 4a. In one embodiment, the profiling material distribution location is determined using an algorithm executed at one of a local computer, a remote computer, and a cloud-based computer.
[0025] In process (302), as shown in FIG. 4b, the top plate (404) is placed under the UV transparent (UVT) chuck (405) and the tension is adjusted.
[0026] In process (303), as shown in FIG. 4c, the top plate (404) is chucked using a UVT chuck (405). Also in process (303), as shown in FIG. 4c, air pressure is added to initiate contact (contact between the top plate (404) and the substrate (402).
[0027] In process (304), as shown in FIG. 4d, the air pressure gradually increases until all droplets are merged.
[0028] In process (305), pressure is continuously applied with air bars along with a UV flash (406) to form a contiguous film (407) as illustrated in FIGS. 4e to 4f.
[0029] In process (306), as illustrated in FIG. 4F, the substrate (402) is separated from the top plate (404) using a vertical chuck motion (VCM) stage (408).
[0030] In process (307), as shown in FIG. 4g, the substrate (402) and VCM stage (408) are moved to the measurement station (409) using the x stage (410).
[0031] In process (308), as shown in FIG. 4h, the xy stage is scanned to perform optical measurements at all points on the substrate (402) through a laser beam (411) (corresponding to the final substrate profile).
[0032] A more detailed description of the method (300) in relation to FIGS. 4a through 4h is provided below.
[0033] Referring to FIGS. 3 and FIGS. 4a through 4h, during the process of manufacturing an optical element on a flat substrate (402) using nP3, a pattern of profiling material (401) is created and distributed over a wide area on the flat substrate (402). In one embodiment, the substrate (402) may have existing nanoscale features or patterns, and since these nanoscale features can interact with electromagnetic radiation to induce a diffraction effect, they may correspond to an optical element or a diffractive optical element. The pattern of inkjet droplets or profiling material (401) is created to describe a desired film thickness profile based on spreading, merging, and filling in the presence of existing features on the substrate (402) and customized spatial deformation of one or more geometric parameters of the features. This is achieved through the XY motion of the substrate (402) synchronized with the jetting cycles. In one embodiment, the substrate (402) is moved to a profiling zone under an ultraviolet (UV) lamp and a UV transparent (UVT) chuck (405).
[0034] In one embodiment, the top plate (404) is positioned below the UVT chuck (405), and the tension of the top plate (404) is adjusted to a desired level as required by the final surface profile. The top plate (404) may be a textured or patterned roll, wherein the lateral spatial length scale of the texture or pattern is at least one order of magnitude smaller than the lateral spatial length scale of the desired profile. In one embodiment, the UVT chuck (405) is used to hold the top plate (404) in place. A voice coil motor-driven stage with a substrate (402) mounted on the chuck is moved to the profiling zone with the help of a horizontal XY stage. The vertical tip tilt movement of the vertical chuck motion (VCM) stage (408) enables proper alignment and gap control of the substrate (402) and the top plate (404). Increased air pressure within the cavity creates a curvature of the top plate web that allows droplets to merge and form a contiguous film (407). This process can relieve trapped bubbles. In one embodiment, a camera mounted on the UVT chuck (405) is used to observe bubble capture. Using image processing, bubbles are identified, and air is automatically pumped to the top plate (404) at a target location so that the profiling material (401) droplets diffuse and the bubbles are relieved. After a specific time required for capillary forces to create the desired topography, the profiling material is UV-cured. In one embodiment, a VCM stage (408) is used to separate the substrate (402) from the top plate (404) through vertical movement.
[0035] In one embodiment, the substrate (402) is moved to a measurement station (409) together with a VCM stage (408). In one embodiment, the VCM stage (408) helps align the surface of the substrate (402) at the measurement point with the optical axis of an optical measurement device such as a profilometer, a Schark-Hartmann wavefront sensor, an interferometer, a reflectometer, etc. In one embodiment, a machine command (e.g., a droplet pattern) to obtain a desired thickness profile is determined using an automated algorithm.
[0036] For the nP3 process, instead of using inkjet for the programmable film, one alternative embodiment involves the use of a substantially uniform profiling film deposited on a substrate using techniques such as spin-coating, slot-die coating, or dip coating. The uniform film is not only able to fill the existing features of the substrate but is also sufficiently thick to substantially match the highest thickness that must exist after obtaining the customized profile. In this case, the customized profile is obtained by differential heating of the profiling film using a device such as a profiling material (e.g., methyl methacrylate) or one or more spatial light modulators (e.g., an array of digital micromirror devices) connected to a lamp emitting radiation of a desired wavelength (e.g., 3.3 micrometers) absorbed by the substrate, or an array of microheaters on the substrate chuck. In one embodiment, differential heating can induce flow in the coated film through one or more mechanisms, such as a thermal gradient, Marangoni flow due to a surface tension gradient, evaporation, or a composition gradient. In one embodiment, a flow model of the film can be used to determine spatial and temporal differential heating characteristics so that the flow transient provides a desired film thickness profile. The film is then crosslinked to "freeze" the transient state. This alternative embodiment may be used with or without a top plate based on the need to control evaporation or add an additional control knob to the flow of the coated film.
[0037] FIG. 5 is a flowchart of a method (500) for manufacturing an optical element on a flat substrate using a nanoscale precision programmable profiling (nP3) process together with a top plate according to an embodiment of the present invention. FIG. 6a to 6h illustrate cross-sectional views for manufacturing an optical element on a flat substrate using the nP3 process together with a top plate using the processes described in FIG. 5 according to an embodiment of the present invention.
[0038] Referring to FIG. 5 together with FIG. 6a through 6h, in process (501), as illustrated in FIG. 6a, the profiling material (601) is distributed onto a substrate (602) using an inkjet (603). In one embodiment, the distribution location of the profiling material is determined using an algorithm executed at one of a local computer, a remote computer, and a cloud-based computer.
[0039] In process (502), the top plate (604) is positioned under the ultraviolet transparent (UVT) chuck (605) as shown in FIG. 6b.
[0040] In process (503), the top plate (604) spreads the profiling material (601) as shown in FIG. 6c by initiating contact with the profiling material (601).
[0041] In process (504), the top plate (604) continues to be in contact with the profiling material (601) to form an adjacent film (606) with a thickness variation (thickness profile) as shown in FIG. 6d.
[0042] In an optional process (505), as shown in FIG. 6e, if possible, the thickness profile of an adjacent film (606) is further adjusted by differential heating (607).
[0043] In process (506), the adjacent film (606) is exposed to ultraviolet (UV) light (608) so that the adjacent film (606) is cured and a cured adjacent film (609) is formed as shown in FIG. 6f.
[0044] In process (507), as shown in FIG. 6g, the top plate (604) is separated from the substrate (602).
[0045] In process (508), optical measurements are performed at all points on the substrate (602) through a laser beam (610) from a measurement station (611) as shown in FIG. 6h.
[0046] In one alternative embodiment, an optical element can be manufactured on a flat substrate using the nP3 process without using a top plate by simply performing the processes (501 and 505-508) as described above. In this embodiment, after dispensing the profiling material onto the substrate, the thickness profile of the profiling material is adjusted using differential heating.
[0047] In one embodiment, the nP3 process can be applied to the field of precision optics as described below.
[0048] Precision optical devices include mirrors and lenses for various applications. Depending on the application, these devices may need to be fabricated from various substrate materials and may be flat, freeform, or nominally curved. The nP3 process may be used to modify the existing topography of the substrate to match the desired topography or to create a completely different profile from a starting substrate. In some applications, a functional film is deposited on the substrate due to the nP3 process. For example, in optical applications, the functional material may be a film with a refractive index that matches the refractive index of the substrate. For example, a high-index polymer resist (e.g., #18165 from Nippon Telegraph and Telephone-Advanced Technology) may be used on a high-index waveguide substrate (e.g., Schott Realview). In one embodiment, the nP3 process is performed on the patterned surface of the high-index waveguide substrate. For some applications, a sacrificial film (e.g., mrUVcur26SF from Microresist Technologies) in the nP3 process can be used to transfer the film profile to a substrate or underlying nanoscale patterning material via an etching process after deposition. These applications include, for example, high-intensity laser beam optics, where the presence of a polymer film can degrade the functionality of the substrate and therefore must be removed. To achieve the desired match between the etching rate of the sacrificial profiling material and the underlying nanoscale patterning material, the etching process is typically performed in a plasma chamber. The etching gases used may be a combination of O2, inert gases (e.g., Ar), fluorinated gases (CHF3, CF4, SF6, etc.), or other halogen gases (Cl2, HBr, etc.).In one embodiment, the ratio of the etching rates of the profiling film and the nanoscale pattern material is substantially matched. In one embodiment, the profiling film has optical properties substantially matched to the nanoscale pattern, and these optical properties include refractive indices at one or more wavelengths. In one embodiment, the desired match between the etching rates can be adjusted to a ratio between 0.05:1 and 20:1. This adjustment can be performed by adjusting the relative flow rates between the physical (O2, inert gas) and chemical (fluorinated chemistry, other halogens) etching components. For example, increasing the flow rates of O2 and Ar increases the etching rate of the polymer material, while the etching rate of materials such as fused silica is substantially unaffected. In one embodiment, the etching rate of the polymer resist is between 10 and 1000 nm / min. In one embodiment, the etching process itself may be divided into multiple coarse or fine iterations, where a significant amount of material can be removed in the coarse process at a high etching rate for high throughput, and errors in the desired profile are corrected in the fine process. Intermediate measurements may be performed between the coarse and fine processes. Additionally, in some applications, an additional uniform film may be deposited on the nP3 profiling film. For example, a uniform metal layer may be deposited after the nP3 process to provide the substrate with optical reflection properties with an appropriate profile. Some exemplary applications of the nP3 process for precision optical surfaces are described below.
[0049] Augmented Reality (AR) / Mixed Reality (MR), commonly known as "XR" headsets, must use high-refractive-index waveguides to propagate light from a display to the pupil near the eye. This virtual image is superimposed onto the real world perceived by the eye. These waveguides typically have gratings that couple at least one wavelength of light incident from a microdisplay to the gratings at an angle that causes the light to undergo total internal reflection into the waveguide. The light is then coupled outward using one or more gratings. These waveguides are fabricated on substrates that require excellent flatness and / or total thickness variation (TTV). This is because if significant deviations occur in a flat waveguide with a TTV close to zero, the light beam may deviate from the desired path or the diameter of the light beam may change, causing the virtual image to be distorted relative to the real image. Furthermore, these headsets may have multiple waveguides, each processing one or more wavelengths. Therefore, if each waveguide moves the beam differently from other waveguides in the same headset, chromatic aberration may be induced in the combined image.
[0050] The more reflections a waveguide has, the more severe the image distortion becomes at its exit pupil. Increasing the distance between the incoupling and outcoupling gratings or between the exit pupils increases the number of reflections. Therefore, if the waveguide is imperfect, light rays traveling further inside the waveguide experience greater deviation than desired. Reducing the substrate thickness to decrease the weight of the waveguide and the headset itself also increases the number of reflections.
[0051] The nP3 process for a flat substrate of the present invention can be used to correct the flatness and TTV of a transparent waveguide substrate by depositing a film that corrects the inherent TTV and / or flatness error of the substrate. In one embodiment, the starter substrate may be of low quality that does not meet flatness / TTV specifications. In one embodiment, the starter substrate may be a substrate with a thickness thinner than currently available (e.g., 100 micrometers). In one embodiment, the starter substrate has specifications that meet the desired specifications and obtain substantial improvement after the nP3 process. Since waveguide substrates generally have a refractive index of 1.6 or higher, a sacrificial film may be used to deposit a profile and then transfer it to the substrate. Alternatively, high-refractive-index profiling materials, such as Microresist® and high-refractive-index profiling materials developed by Nippon Telegraph and Telephone-Advanced Technology, can also be used as functional films left where the index is nearly identical to the refractive index of the substrate and spurious reflections at the interface do not cause a substantial loss of light intensity. In one embodiment, flatness / TTV correction can be combined with moth-eye textured structure for anti-reflective properties. In one embodiment, both sides of the substrate may be profiled and also have textured.
[0052] In addition to the foregoing, the nP3 process can also be used to correct TTV / flatness errors of the finished waveguide by profiling the unpatterned portions of the waveguide substrate. These errors may be the result of inherent TTV / flatness errors in the starter substrate or previous manufacturing processes. For example, nanoimprint lithography leaves a residual layer, and the non-uniformity of this residual layer can increase flatness / TTV errors. Furthermore, the deposition of films, such as anti-reflective coatings, may have inherent non-uniformity, which can contribute to flatness / TTV errors. Additionally, TTV / flatness deformation expected during subsequent processes, such as packaging, can also generate additional TTV / flatness errors. Based on measurements performed on the same finished waveguide, a profile can be calculated based on a model that predicts the dependence of image transformation, magnification, and other distortions and aberrations on the TTV / flatness deviation of the finished waveguide, or based on measurements of actual aberrations. This unpatterned portion may be the entire surface without nanoscale features that form a diffractive optical element. In one embodiment, the unpatterned portion of the substrate (e.g., waveguide substrate) has a nanoscale texture. Additionally, the profiling material may be left on the substrate if the refractive index of the profiling film substantially matches the refractive index of the substrate at the wavelength of interest. If the refractive indices do not match, a nanotextured moth-eye structure can be used to reduce parasitic reflections at the interface.
[0053] Diffractive optical elements are used for various purposes in XR waveguide substrates. Incoupling diffractive optical elements are used to couple light from a projector into a waveguide. These diffractive optical elements may be diffractive gratings (e.g., binary gratings, phase gratings, surface relief gratings, Bragg gratings, 1D gratings, 2D gratings, slanted gratings, multilevel gratings, or combinations of some of these), volume holograms, or photonic crystals. This coupled light is totally reflected through the waveguide substrate. During total internal reflection, the light may be affected by additional diffractive optical elements in its path. These diffractive optical elements may also be diffractive gratings (e.g., binary gratings, phase gratings, surface relief gratings, Bragg gratings, 1D gratings, 2D gratings, multilevel gratings, or combinations of some of these), volume holograms, or photonic crystals. These devices are intended to expand the image to at least one dimension, preferably two, so that light is emitted into the eye and the image can be viewed from different locations within the so-called eye box. The expanded and outcoupled light must not suffer significant distortion in image quality compared to the quality of the image incoupled from the projector into the waveguide. Several factors determine image quality. Diffractive optical devices cause light to diffract by many orders, with the first order having the highest intensity and being primarily used for imaging. However, various other orders of lower intensity may exist, and intensity loss may occur whenever light interacts with the diffractive optical device. Furthermore, diffraction characteristics and diffraction efficiency depend on wavelength, meaning that light of different wavelengths is diffracted at different angles.
[0054] Furthermore, due to manufacturing errors that cause the diffractive optical element (DOE) structure to deviate undesirably from the designed structure, the wavelength of the first-order diffracted light may shift or its intensity may change undesirably. For example, the intensity of diffracted light is known to be controlled by the height or depth of the grating. However, as a portion of the light is outcoupled from one region, the remainder continues to propagate within the waveguide and is outcoupled from other parts of the waveguide. If the grating depth is constant everywhere, the intensity of the light outcoupled from the beginning of the waveguide, where the incident intensity is maximum, will be exponentially higher than the intensity of the light outcoupled from the end of the waveguide, where the incident intensity decreases exponentially because a significant portion of the light is outcoupled from the earlier part of the waveguide. Therefore, to obtain uniform light intensity across an eye box with multiple pupils, it is desirable to have a non-uniform grating height such that the grating efficiency, or the ratio of outcoupled light, starts low at the beginning of the waveguide and gradually increases at the end of the waveguide. In one embodiment, to form a color image in the eye, three different DOE designs for three primary color wavelength bands are required so that they can be combined to provide the necessary image. Dispersion in the color spectrum due to the aforementioned factors can cause undesirable chromatic aberration in the image.
[0055] Referring to FIG. 7, FIG. 7 illustrates a waveguide substrate having nanoscale pattern regions as in-coupling DOE and out-coupling DOE according to one embodiment of the present invention.
[0056] As illustrated in FIG. 7, the projector (701) injects a virtual image into a waveguide (702) in which the coupling DOE (703) couples light (704) to the waveguide (702). Then, the actual image is transmitted through the waveguide (702).
[0057] As additionally illustrated in FIG. 7, the outcoupling DOE (705) couples light (706) from the eye box (707) to the outside of the waveguide (702).
[0058] Additionally, as shown in FIG. 7, the real image (708) is transmitted through the waveguide (702).
[0059] Referring to FIG. 8, according to one embodiment of the present invention, FIG. 8 illustrates a waveguide substrate in which a nanoscale pattern region is shown with a customized variation of geometric parameters and the nanoscale pattern region is represented as an incoupling DOE and an outcoupling DOE.
[0060] As illustrated in FIG. 8, the projector (801) injects a virtual image into a waveguide (802) in which an incoupling DOE (803) (having a customized variation of geometric parameters) couples light (804) to the waveguide (802). Then, the real image is transmitted through the waveguide (802).
[0061] As additionally illustrated in FIG. 8, the outcoupling DOE (805) (having a customized variation for geometric parameters) couples light (806) from the eye box (807) to the outside of the waveguide (802).
[0062] Additionally, as shown in FIG. 8, the actual image (808) is transmitted through the waveguide (802).
[0063] As previously described, FIGS. 7 and 8 illustrate a waveguide substrate having nanoscale pattern regions as incoupling DOE and outcoupling DOE according to an embodiment of the present invention. Likewise, as previously described, the substrate described herein may include one or more regions having nanoscale patterns, and such nanoscale patterns may be similar or substantially different from region to region. For example, as illustrated in FIG. 9, FIG. 9 illustrates having a plurality of nanoscale pattern regions (901) on the same substrate (902) according to an embodiment of the present invention.
[0064] Additionally, as described above, the nP3 process can also be used to correct TTV / flatness errors of the finished waveguide by profiling the unpatterned portion of the waveguide substrate. FIG. 10 illustrates the use of the nP3 process on the unpatterned portion of the waveguide substrate to correct aberrations according to one embodiment of the present invention. In particular, in this case, the use of the nP3 process to correct TTV errors is illustrated. The profiling material has a refractive index substantially similar to that of the substrate and is left behind the substrate at the wavelength of interest. By correcting TTV and other substrate distortion errors, optical aberrations (e.g., image misalignment between the real image and the virtual image, shift in image focus, etc.) and dispersion errors are minimized.
[0065] As illustrated in FIG. 10, a projector (1001) injects a virtual image into a waveguide (1002) in which an incoupling DOE (1003) couples light (1004) to the waveguide (1002), wherein the waveguide (1002) includes a profiling material on a substrate (1005). Then, a real image is transmitted through the waveguide (1002).
[0066] As additionally illustrated in FIG. 10, the outcoupling DOE (1006) couples light (1007) from the eye box (1008) to the outside of the waveguide (1002).
[0067] Additionally, as shown in FIG. 10, the actual image (1009) is transmitted through the waveguide (1002).
[0068] In one embodiment, the principle of the present invention utilizes controlled and customized variations of one or more geometric parameters of the DOE to achieve desired uniformity in diffraction characteristics and / or efficiency by overcoming manufacturing errors, or to achieve controlled variations in diffraction characteristics and / or efficiency. For a 1D grating, the geometric parameters may be the depth or height of the grating feature, the lateral width of the feature, the orientation of the grating, i.e., the angle formed by the lines of the grating with respect to the axis of a given waveguide, the width of the feature, or the angle of the feature with respect to the horizontal plane. In one embodiment, the height varies in the range of 10 to 400 nm. For a 2D grating with a polygonal shape, the geometric parameters that may have controlled variations may be the depth of the grating feature in one or more directions, the orientation of the 2D grating with respect to a given axis of the waveguide substrate, the relative spacing between two polygons constituting the 2D grating, or the angle formed by one side of the polygon with respect to the horizontal line. In one embodiment, the height varies in the range of 10 to 400 nm. This embodiment specifically discloses the use of controlled and customized variations of one or more geometric parameters in a diffractive optical element for a waveguide substrate, but such use can be extended to the use of introducing customized and controlled variations of one or more geometric parameters in a nanoscale pattern. In one embodiment, the use of such controlled variations is intended to compensate for errors in a previous manufacturing process or errors expected in a subsequent manufacturing process.
[0069] In a typical example, a diffraction grating is fabricated using nanoimprint lithography with a master template. The master template can be fabricated using standard lithography techniques such as e-beam lithography or photolithography. If one or more controlled variations of grating parameters are introduced into the master template itself, fabricating the template using the aforementioned lithography techniques can become very expensive. The principle of the present invention utilizes an nP3 process to introduce controlled, programmable / custom variations to one or more diffraction grating parameters on the master template. For example, a controlled variation of the grating depth is initiated. To this end, a master template is first fabricated on silicon, fused silica, or other substrates using standard lithography techniques without the desired parametric depth variation. Subsequently, the nP3 process is used to fill the grating with a UV-curable polymer and deposit a film with a desired thickness profile on the filled grating. This process can be performed as a single step. Here, the nP3 droplet generation algorithm is modified to account for the volume of liquid used to fill the grid and the volume of liquid required to generate a controlled profile, and this profile can be linear, parabolic, or other polynomials of one or more dimensions.
[0070] Additionally, this profile may have different orientations. For example, a portion of the DOE on the waveguide may have varying depth profiles in one direction, while other portions of the same DOE or different DOEs may have varying depth profiles in different directions. Furthermore, in one embodiment, the transition from regions with different orientations of the grid depth profile may occur within 5 micrometers to 10 millimeters. In one embodiment, this process is performed in multiple iterations, wherein the first iteration may be used to substantially planarize the grid shape, and one or more subsequent iterations may be used to obtain a desired film thickness profile in one or more different directions. In one embodiment, the film thickness on the grid structure after the planarization process is substantially uniform, wherein the average film thickness may be selected to mitigate defects caused by bubbles trapped in the polymer film. For example, individual droplets merged in the 1D grid structure preferentially flow in a direction parallel to the grid lines. The flow of these droplets is controlled by pressure applied by the top plate during the nP3 process. If the average film thickness is suboptimal, reducing the pressure of the film may cause bubbles to persist longer than desired. Therefore, to maintain the number of defects below a defined tolerance, the average film thickness can be selected based on nanoscale pattern geometry and desired throughput. This can also be achieved with the help of a model. Additionally, this process can correct for undesirable variations in the depth or other geometric parameters of the waveguide substrate fabricated to match desired specifications. For example, a waveguide substrate can be fabricated and its performance measured. If the performance is undesirable, the above nP3 process can be applied so that the deposited film thickness profile and subsequent plasma etching (described below) can generate the desired profile of the geometric parameters.
[0071] After obtaining a desired profile from the polymer film, a plasma etching process is applied to the waveguide substrate. In the etching process, the polymer film and the waveguide substrate are etched in plasma chemistry that produces substantially similar etching rates for both the polymer and the underlying substrate, where the underlying substrate may be silicon (Si), fused silica, high refractive index glass (e.g., Schott Realview®), etc. This ensures that the deposited profile is directly transferred to the underlying substrate such that the desired parameters of the diffraction grating (e.g., depth) are identical to the parameter variations appearing in the film thickness profile. Furthermore, if the relative etching rates between the film and the substrate are modulated to have a ratio other than 1, the transferred profile of the grating depth is proportional to the ratio of the etching depth. In one embodiment, the nP3 process and the etching process are performed simultaneously across regions of the nanoscale pattern on the substrate.
[0072] Adjusting these etching rate ratios can be an additional control knob for obtaining a desired profile. The substrate may be cleaned to remove residual resist or contamination from the etching. At the end of the process, it is desirable to maintain the surface roughness of the substrate substantially similar to the value prior to nP3 or increase it to 1 nm or less. In one embodiment, the average surface roughness of a nanoscale pattern with a customized variation is substantially the same as the average surface roughness of a nanoscale pattern without a customized variation.
[0073] Referring to FIG. 11, FIG. 11 illustrates a method (1100) for introducing a customized deformation to a geometric parameter (e.g., height) of a nanoscale pattern using substantially similar etching rates for profiling and nanoscale pattern materials according to one embodiment of the present invention. FIG. 12a through 12d illustrate cross-sectional views for introducing a customized deformation to a geometric parameter (e.g., height) of a nanoscale pattern using the processes described in FIG. 11 according to one embodiment of the present invention.
[0074] As described in more detail below, FIGS. 11 and 12a through 12d illustrate the use of an nP3 process in conjunction with a plasma etching process on an exemplary lattice structure to introduce customized variations to the geometric parameters (e.g., height) of a nanoscale pattern.
[0075] Referring to FIG. 11 together with FIG. 12a through 12d, in process (1101), a profiling film (1201) having a programmable thickness variation is deposited on a starting nanoscale pattern (1202) on a substrate (1203) (an exemplary lattice structure) by an nP3 process as shown in FIG. 12a and FIG. 12b.
[0076] In process (1102), the materials of the profiling film (1201) and the nanoscale pattern (1202) are etched in a plasma etching process using substantially similar etching rates for the profiling and nanoscale pattern materials as shown in FIG. 12c.
[0077] In process (1103), the remaining profiling film (1201) is removed using a wet process (e.g., Piranha clean) or a dry process (e.g., UV ozone cleaning, O2 ashing, etc.) to form a structure as shown in FIG. 12d.
[0078] As illustrated in FIGS. 12c and 12d, the materials of the profiling film (1201) and the nanoscale pattern (1202) are etched in a plasma etching process at similar etching rates. Examples of introducing customized variations to geometric parameters (e.g., height) of the nanoscale pattern, where the etching rates for the profiling and nanoscale pattern materials are substantially different, are discussed below together with FIGS. 13 and FIGS. 14a through 14d.
[0079] Referring to FIG. 13, FIG. 13 illustrates a method (1300) for introducing a customized deformation to a geometric parameter (e.g., height) of a nanoscale pattern using substantially different etching rates for profiling and nanoscale pattern materials according to one embodiment of the present invention. FIG. 14a through 14d illustrate cross-sectional views for introducing a customized deformation to a geometric parameter (e.g., height) of a nanoscale pattern using the processes described in FIG. 13 according to one embodiment of the present invention.
[0080] Referring to FIG. 13 together with FIG. 14a to 14d, in process (1301), a profiling film (1401) having a programmable thickness variation is deposited on a starting nanoscale pattern (1402) on a substrate (1403) (an exemplary lattice structure) by an nP3 process as shown in FIG. 14a and FIG. 14b.
[0081] In process (1302), the materials of the profiling film (1401) and the nanoscale pattern (1402) are etched in a plasma etching process using substantially different etching rates for the profiling and nanoscale pattern materials as shown in FIG. 14c.
[0082] In process (1303), the remaining profiling film (1401) is removed using a wet process (e.g., pyranha cleaning) or a dry process (e.g., UV ozone cleaning, O2 ashing, etc.) to form a structure as shown in FIG. 14d.
[0083] As a result of applying the aforementioned principles of the present invention, processing accuracy is improved when fabricating optical elements.
[0084] Various embodiments of the present invention are described by way of example and are not limited to the disclosed embodiments. It will be apparent to those skilled in the art that various modifications and variations are possible without departing from the scope and spirit of the described embodiments. The terms used herein have been selected to best describe the principles of the embodiments, the practical application or technical improvement of the technology found in the prior art, or to enable those skilled in the art to understand the embodiments disclosed herein.
Claims
Claim 1 A method for introducing a customized variation of a geometric parameter into a nanoscale pattern on a substrate, comprising: performing a nanoscale precision programmable profiling process in one or more regions of the substrate having a non-patterned portion of the substrate; depositing a profiling film having a thickness profile that is a function of the customized variation of the geometric parameter on the non-patterned portion of the substrate to correct one or more aberrations of the substrate, wherein the customized variation of the geometric parameter is calculated based on a measurement of an actual aberration; and performing a plasma etch process of the material of the profiling film and the nanoscale pattern to convert the thickness profile of the profiling film into the customized variation of the geometric parameter in the nanoscale pattern, wherein the customized variation is a function of the thickness profile of the profiling film. Claim 2 The method of claim 1, wherein the nanoscale pattern is one or more of a 1D diffraction grating, a 2D diffraction grating, a multilevel grating, a slanted grating, a surface relief grating, a Bragg grating, a volume hologram, and a photonic crystal. Claim 3 The method of claim 1, wherein the substrate is a high-index waveguide substrate, the method is performed on a patterned surface of the high-index waveguide substrate, and the nanoscale pattern comprises a diffraction optical element. Claim 4 A method according to claim 1, wherein the geometric parameters include one or more of the depth or height of a feature, the lateral width of a feature, and an angle in one dimension with respect to a horizontal plane. Claim 5 In claim 1, one or more characteristics of the customized variation are different in different regions of the nanoscale pattern on the substrate. Claim 6 A method according to claim 1, wherein the process of performing the nanoscale precision programmable profiling process and the process of performing the plasma etching process are performed simultaneously across a plurality of regions of the nanoscale pattern on the substrate. Claim 7 A method according to claim 1, wherein the customized modification is achieved in multiple iterations of the process of performing the nanoscale precision programmable profiling process and the process of performing the plasma etching process. Claim 8 In claim 1, the average surface roughness of the nanoscale pattern having the customized deformation is substantially the same as the average surface roughness of the nanoscale pattern without the customized deformation. Claim 9 A method according to claim 1 in which the ratio of the etching rates of the profiling film and the nanoscale pattern material substantially matches. Claim 10 A method according to claim 1, wherein the ratio of the etching rates of the profiling film and the nanoscale pattern material is adjusted between 0.05 and 20. Claim 11 A method according to claim 1 in which customized spatial deformation is achieved in the profiling film using one or more of inkjet, differential heating using a superstrate, and differential heating without a superstrate. Claim 12 A method according to claim 1, wherein the profiling film has optical properties substantially corresponding to the nanoscale pattern. Claim 13 delete Claim 14 delete Claim 15 delete Claim 16 delete Claim 17 delete Claim 18 An apparatus for introducing a customized variation of a geometric parameter into a nanoscale pattern on a substrate, comprising a profiling module, wherein the profiling module has an inkjet for depositing a profiling film on the substrate with a thickness profile that is a function of the customized variation of the geometric parameter in the nanoscale pattern on the substrate, and a plasma etch process for converting the thickness profile of the profiling film into the customized variation of the geometric parameter in the nanoscale pattern is performed on the material of the profiling film and the nanoscale pattern to correct one or more aberrations of the substrate, wherein the customized variation is a function of the thickness profile of the profiling film, and the customized variation of the geometric parameter for correcting one or more aberrations is calculated based on the measured value of the actual aberration. Claim 19 In claim 18, the substrate comprises a waveguide substrate, wherein the substrate has a region having an optical element having the customized variation of the geometric parameter in the nanoscale pattern on the substrate. Claim 20 delete
Citation Information
Patent Citations
Multi-layer diffractive eyepiece
JP2019528474A