Glass spacer, hard disk reader, and method for manufacturing glass spacer
Patent Information
- Application Number
- LAP724
- Authority / Receiving Office
- LA · LA
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2018-12-14
- Filing Date
- 2019-01-31
- Publication Date
- 2026-06-05
AI Technical Summary
Hard disk drive devices face issues with static electricity accumulation on glass spacers and magnetic disks, leading to attraction of foreign matter and potential damage to the magnetic head, especially when increasing storage capacity by adding more disks, which exacerbates the risk of static discharge and particle attraction.
A ring-shaped glass spacer with a surface resistivity of 10^3 to 10^9 Ω/sq, containing TiO2, Nb2O5, WO3, and Bi2O3, and optionally P2O5, is used, with a reduced surface resistivity achieved through composition and surface treatment to prevent static electricity accumulation, and a manufacturing method involving heat treatment in a reducing atmosphere to enhance conductivity.
The glass spacer effectively suppresses static electricity discharge and reduces the attraction of foreign particles, ensuring stable operation of the hard disk drive device even with multiple disks, by diffusing static electricity through the conductive spindle, thus preventing damage to the magnetic head and maintaining data integrity.
Smart Images

Figure 00000000_0000_ABST 
Figure 00000000_0001_ABST
Abstract
Description
Glass spacer, hard disk drive device, and method for manufacturing a glass spacer
[0001] The present invention relates to a ring-shaped glass spacer provided in contact with a magnetic disk in a magnetic recording hard disk drive, a hard disk drive using this glass spacer, and a method for manufacturing the glass spacer.
[0002] With the recent rise of cloud computing, many hard disk drives (hereinafter also referred to as HDDs) are being used in data centers for the cloud to increase storage capacity.
[0003] HDD devices are equipped with ring-shaped spacers between magnetic disks to hold them apart. These spacers function to ensure that the magnetic disks do not touch each other and are precisely spaced apart in predetermined positions. Traditionally, metal materials with low manufacturing costs have been used for these spacers. However, when a glass substrate is used as the substrate for the magnetic disks, the spacers and magnetic disks are in contact with each other. As a result, changes in temperature within the HDD device cause a difference in thermal expansion between the metal spacers and the glass magnetic disks, causing the magnetic disks to bend, which in turn worsens the levitation of the magnetic head. Poor levitation of the magnetic head is undesirable from the standpoint of reading and writing data to the hard disk. For this reason, in recent years, the use of glass spacers (hereinafter referred to as glass spacers) has been considered to reduce the difference in thermal expansion when glass substrates are used as the substrate for magnetic disks. However, since glass is generally an insulator, static electricity tends to accumulate on the magnetic disks or glass spacers due to friction between the rapidly rotating magnetic disks and glass spacers and the air. When magnetic disks or spacers become charged, they are more likely to attract foreign matter and fine particles. Furthermore, the discharge of accumulated static electricity to the magnetic head can damage the recording and playback elements of the magnetic head, which is undesirable.
[0004] Therefore, a spacer is known in which the surface of the spacer is etched with an etching solution, and then a conductive coating is formed on the surface of the spacer (Patent Document 1). This is said to suppress the charging of magnetic disks and spacers, thereby reducing the adsorption of foreign matter and fine particles.
[0005] Japanese Patent Publication No. 2003-308672
[0006] However, when forming a conductive coating on the surface of a spacer, conventional electroless plating methods result in insufficient adhesion and a lack of dust prevention capabilities. Furthermore, this process complicates the manufacturing process of the spacer and increases manufacturing costs.
[0007] On the other hand, in order to increase the storage capacity of data centers for the cloud, there is a demand for larger storage capacities in each HDD device compared to conventional models. In today's magnetic disks, the levitation distance of the magnetic head relative to the magnetic disk is minimized, allowing many magnetic disks to be mounted in an HDD device. However, this is not sufficient to meet the increased storage capacity requirements of the HDD devices. For this reason, increasing the number of magnetic disks mounted in an HDD device is being considered. Increasing the number of magnetic disks increases the likelihood of damage to the recording and playback elements of the magnetic head due to the discharge of static electricity charged on the magnetic disks to the magnetic head. In addition, the charging of magnetic disks and spacers increases the likelihood of foreign matter and fine particles adsorbing onto the magnetic disks and spacers.
[0008] Therefore, the present invention aims to provide a glass spacer that can suppress the charging of magnetic disks and glass spacers in order to suppress the discharge of static electricity charged on magnetic disks within an HDD device to the magnetic head, or to reduce the adsorption of foreign matter and fine particles onto magnetic disks, a hard disk drive device using this glass spacer, and a method for manufacturing a glass spacer.
[0009] One aspect of the present invention is a ring-shaped glass spacer provided to contact a magnetic disk within a hard disk drive device, wherein the surface resistivity of the glass material of the glass spacer at 22 [°C] is 10 3 to 10 9 [Ω / sq].
[0010] Another aspect of the present invention is also a ring-shaped glass spacer provided to contact a magnetic disk within a hard disk drive device, wherein the surface resistivity of the surface of the glass material of the glass spacer at 22 [°C] is smaller than the surface resistivity of the interior of the glass material at 22 [°C].
[0011] The surface resistivity of the glass material of the glass spacer at 22 [°C] is preferably 10 3 to 10 9 [Ω / sq].
[0012] The glass spacer preferably contains at least one oxide selected from the group consisting of TiO 2 , Nb 2 O 2] 5 , WO 3 , and Bi 2 O 3 . The glass spacer contains P 2 O 5 , contains either Li 2 O or Na 2 O, and preferably contains at least one oxide selected from the group consisting of TiO 2 , Nb 2 O 5 , WO 3 and Bi 2 O 3 .
[0013] The surface roughness Ra of the main surface of the glass spacer that contacts the magnetic disk is preferably 1.0 [μm] or less.
[0014] The surface roughness Rz of the outer peripheral end face of the glass spacer that does not contact the magnetic disk is preferably 1.5 [μm] or more.
[0015] Preferably, the surface roughness Rz of the outer peripheral end face is 20 [μm] or less.
[0016] Preferably, a groove extending along the outer circumference of the glass spacer is formed on the outer peripheral end face of the glass spacer that does not come into contact with the magnetic disk.
[0017] Preferably, the skewness of the outer peripheral end face of the glass spacer that does not come into contact with the magnetic disk is 1.2 or less.
[0018] Yet another aspect of the present invention is a hard disk drive device comprising the glass spacer and the magnetic disk.
[0019] Preferably, the magnetic disk is a disk on which a magnetic film is formed on a glass substrate.
[0020] Preferably, the surface roughness Ra of the main surface of the magnetic disk is 0.3 [nm] or less.
[0021] It is preferable to mount eight or more of the aforementioned magnetic disks.
[0022] Another aspect of the present invention is a method for manufacturing a ring-shaped glass spacer provided in contact with a magnetic disk within a hard disk drive, comprising the steps of: manufacturing a glass spacer material which is the material for the glass spacer; and reducing the surface resistivity on the surface of the glass spacer material by reducing its surface.
[0023] The aforementioned glass spacer has TiO as its glass component. 2 Nb 2 O 5 WO 3 , and Bi 2 O 3 Preferably, the glass spacer contains at least one oxide selected from the group consisting of P. 2 O 5 Includes Li 2 O or Na 2 Contains one of the O's, TiO 2 Nb 2 O5 WO 3 and Bi 2 O 3 Preferably, it contains at least one oxide selected from the group consisting of the following.
[0024] According to the glass spacer, hard disk drive device, and method for manufacturing the glass spacer described above, static charge on the magnetic disk and the glass spacer can be suppressed.
[0025] This is an external perspective view of a spacer according to one embodiment. This is a diagram illustrating the arrangement of a spacer and a magnetic disk according to one embodiment. This is a cross-sectional view of a main part illustrating an example of the structure of an HDD device into which the spacer according to one embodiment is incorporated. This is a diagram illustrating the measurement of the surface resistivity of the spacer according to one embodiment.
[0026] The glass spacer, hard disk drive device, and method for manufacturing the glass spacer of the present invention will be described in detail below. Figure 1 is an external perspective view of a glass spacer (hereinafter simply referred to as "spacer") 1 according to one embodiment, and Figure 2 is a diagram illustrating the arrangement of the spacer 1 and the magnetic disk 5. Figure 3 is a cross-sectional view of a key part illustrating an example of the structure of an HDD device into which the spacer 1 is incorporated.
[0027] As shown in Figure 2, the spacer 1 is incorporated into the HDD device by stacking the magnetic disks 5 and the spacer 1 alternately. As shown in Figure 3, multiple magnetic disks 5 are fitted onto a spindle 14 that rotates connected to a motor 12 via the spacer 1, and then fixed on top of that with screws via a top clamp 16, thereby mounting them at predetermined intervals. As shown in Figure 2, the spacer 1 and the magnetic disks 5 are arranged alternately so that they are located between two magnetic disks 5, maintaining a predetermined gap between adjacent magnetic disks 5. In the following embodiments, the spacer 1 described refers to a spacer provided between two magnetic disks 5 so as to be in contact with the magnetic disks 5, but the spacer targeted by the present invention also includes spacers that are in contact only with the uppermost or lowermost magnetic disk 5. Depending on the specifications of the HDD device, a spacer 1 that is in contact only with the uppermost or lowermost magnetic disk 5 may not be provided.
[0028] As shown in Figure 1, the spacer 1 has a ring shape and comprises an outer circumferential end face 2, an inner circumferential end face 3, and two opposing main surfaces 4. The inner circumferential end face 3 is the surface that contacts the spindle 14 and is a wall surface surrounding a hole with an inner diameter slightly larger than the outer diameter of the spindle 14.
[0029] The main surface 4 consists of two parallel surfaces that are in contact with the magnetic disk 5. The spacer 1 is in close contact with the magnetic disk 5 and fixes it in place by friction. In this way, the spacer 1 and the magnetic disk 5 are in contact with each other, so changes in temperature inside the HDD device cause a difference in thermal expansion between the spacer 1 and the magnetic disk 5, resulting in displacement and friction. This makes it easy for static electricity to be generated on the insulator, glass. Also, static electricity is easily generated on the spacer 1 due to friction between the rapidly rotating spacer 1 and the air. When such static electricity is generated on the spacer 1 and the spacer 1 becomes charged, it easily attracts foreign matter and fine particles, and the discharge of accumulated static electricity to the magnetic head can damage the recording and playback elements of the magnetic head, which is undesirable. For this reason, the spacer 1 is made of glass with low surface resistivity that does not easily accumulate static electricity and charges easily. The static electricity generated on the spacer 1 diffuses and flows to the outside (grounded part) through the conductive spindle 14. Therefore, even if static electricity is generated on the magnetic disk 5, it flows from the magnetic disk 5 to the outside (grounded part) through the conductive spindle 14, and also flows to the outside through the spacer 1 and spindle 14, making it difficult for static electricity to accumulate. Consequently, static charge can be suppressed on the spacer 1 and the magnetic disk 5 in contact with the spacer 1.
[0030] Such glass materials can be obtained by defining the composition of the glass, or by reducing the surface of the glass spacer material that forms the basis of the spacer 1, as will be described later.
[0031] According to one embodiment of the spacer 1, the surface resistivity of the glass material of the spacer 1 at 22 [°C] is 10 3 ~10 9The value is [Ω / sq]. Surface resistivity is measured by the four-probe method (in accordance with JIS K7194) or the double-ring method shown in Figure 4 below. Either of the two measurement methods can be used, but the four-probe method is used when the resistance is 10 3 ~10 6 This method is used when measuring glass with a resistance of [Ω], and the double-ring method is used when the resistance is 10 6 ~10 9 This method is preferable for determining the surface resistivity with high accuracy when measuring glass with a resistance of [Ω]. The four-probe method is a measurement method that obtains resistance information by passing current between the two outer terminals of four consecutively arranged terminals and measuring the voltage between the two inner terminals.
[0032] Figure 4 illustrates the measurement of the surface resistivity of spacer 1 (double-ring method). If the surface resistivity of spacer 1 cannot be directly measured, a test piece of the same thickness, made of the same glass composition and treated in the same way as spacer 1, may be measured using the method shown in Figure 4 instead of sample 1. The surface resistivity measured on the test piece can be considered the surface resistivity of spacer 1. In measuring the surface resistivity, as shown in Figure 4, a circular main electrode 20 is provided on the upper surface of spacer 1 (or test piece), a circular counter electrode 22 is provided on the lower surface, and an annular electrode 24 is provided on the upper surface, surrounding the main electrode 20, with its center position being the same as the center position of the main electrode 20. A DC power supply 26 voltage is applied between the main electrode 20 and the counter electrode 22, and the current flowing through the wiring connecting the DC power supply 26 and the counter electrode 22 and the wiring connecting the annular electrode 24 is measured with an ammeter 28. The surface resistivity is calculated by dividing the applied voltage (100 [V]) between the main electrode 20 and the counter electrode 22 by the current value measured by the ammeter 28, and the resistance R is calculated as the resistance R. s Let [Ω] be the surface resistivity ρ according to the following equation (1) s Calculate the surface resistivity ρ [Ω / sq]. s= π・(D+d) / (D-d)・Rs (1) Here, D is the inner diameter [mm] of the annular electrode 24, d is the diameter [mm] of the main electrode 20, and π is pi. For example, when using a test piece, if a size of 45 mm × 50 mm × 10 mm is used, D = 38.1 mm, d = 25.4 mm, and furthermore, the outer diameter of the annular electrode 24 is set to 50.8 mm, and the diameter of the counter electrode 22 is set to 50 mm. Conductive paste is used for the main electrode 20, the counter electrode 22, and the annular electrode 24.
[0033] Surface resistivity is 10 9 If the value exceeds [Ω / sq], the charging of spacer 1 is not sufficiently suppressed, and the surface resistivity is 10 3 If the surface resistivity is less than [Ω / sq], the conductive component in the glass composition becomes excessively high, making the glass surface more susceptible to oxidation, resulting in insufficient weather resistance. Also, if the surface resistivity is less than 10 3 If the surface resistivity is less than [Ω / sq], there is a risk of very slight arcing occurring when installing / removing spacer 1. 3 ~10 9 When the value is [Ω / sq], even if static electricity is generated on the spacer 1 due to friction between the high-speed rotating spacer 1 and the air, or if static electricity generated by friction between the high-speed rotating magnetic disk 5 and the air moves to the spacer 1, the static electricity on the spacer 1 diffuses and flows to the outside via the spindle 14, and the static electricity on the spacer 1 is gently attenuated, so it is less likely to become charged and less likely to discharge. According to another embodiment of the spacer 1, TiO 2 Nb 2 O 5 WO 3 , and Bi 2 O 3 It contains at least one oxide selected from the group consisting of . These oxides are readily reduced, and the presence of these oxides is preferable because it tends to increase conductivity. Further P is added to this oxide. 2 O 5 It is preferable to include P. 2 O 5 It has the effect of promoting the reduction of each of the four oxides mentioned above. 3 ~10 9 When expressed as [Ω / sq], TiO 2 Nb2 O 5 WO 3 , and Bi 2 O 3 The above range of surface resistivity can be achieved by adjusting the content of at least one oxide. From the above viewpoint, the surface resistivity is more preferably 10 8 [Ω / sq] or less, more preferably 10 7 It is less than or equal to [Ω / sq]. According to another embodiment of spacer 1, P 2 O 5 Includes Li 2 O or Na 2 Contains one of the O values, TiO 2 Nb 2 O 5 WO 3 and Bi 2 O 3 It contains at least one oxide selected from the group consisting of the following. However, glass with dispersed conductive metal fine particles and crystallized glass are not preferred as glass for spacer 1. Because these glasses contain fine particles of metal or crystalline components, these can fall off the surface, forming large depressions on the surface. These depressions tend to accumulate minute foreign matter and particles such as dust, and are difficult to clean, which may later contaminate the surface of the magnetic disk. From these viewpoints, amorphous glass is preferred as the glass for spacer 1.
[0034] In yet another embodiment of the spacer 1, the surface resistivity of the glass material surface of the spacer 1 at 22°C is lower than the surface resistivity of the interior of the glass material at 22°C. By making the surface resistivity different between the surface and the interior in this way, specifically by making the surface resistivity of the surface lower than that of the interior, the static electricity generated in the spacer 1 can be efficiently passed to the spindle 14 that is in contact with the surface of the spacer 1, which has a lower surface resistivity. Furthermore, since it is only necessary to reduce the surface resistivity of the surface, there is the advantage of being able to produce it at a low cost, as will be described later. In this case, the surface resistivity of the interior of the spacer 1 is, for example, 10 at 22°C. 10The density is [Ω / sq] or greater. To realize such a configuration, as an example, the spacer 1 has TiO as its glass component. 2 Nb 2 O 5 WO 3 , and Bi 2 O 3 The oxide contains at least one oxide selected from the group consisting of the following, and the surface conductivity of the glass spacer material before it becomes spacer 1 can be improved by reducing it as described later. 2 O 5 It is preferable to include it.
[0035] That is, according to an embodiment related to the manufacture of the spacer 1: - A glass spacer material that forms the ring 1 is produced so as to contact the magnetic disk 5 within the HDD device. The glass spacer material may be produced by any method such as producing plate glass from molten glass obtained by melting glass raw materials by the float method, the overflow down-draw method, etc., cutting this plate glass into a ring shape, molding molten glass by the pressing method, slicing a glass tube produced by the tube drawing method into an appropriate length, etc. - Grinding and / or polishing is performed on the end face (outer peripheral end face or inner peripheral end face) and the main surface of the produced glass spacer material. - Next, the surface of the glass spacer material is reduced. Thereby, the conductivity of the surface of the glass spacer material is improved. That is, a spacer 1 can be obtained in which the surface resistivity of the glass material surface at 22 [°C] is smaller than the surface resistivity of the glass material inside at 22 [°C]. According to an embodiment, the reduction of the surface of the glass spacer material can be performed by placing the glass spacer material in an atmosphere of a reducing gas. Here, the surface resistivity of the glass material inside can be obtained by the above-described method for measuring the surface resistivity using a sample having a new surface formed by exposing the inside by scraping the glass material surface. In addition, although there is volume resistivity as another parameter regarding resistivity, since it is measured for the entire object to be measured, only the resistance of the surface cannot be measured. Also, generally, the numerical values of the surface resistivity and the volume resistivity are different. Furthermore, the static electricity generated on the magnetic disk is transmitted by the contact between the magnetic disk and the spacer 1 and can be released, so the surface resistivity of the surface of the spacer 1 is important. Therefore, it is more appropriate to use the surface resistivity rather than the volume resistivity in the spacer 1. According to an embodiment, the spacer 1 preferably contains at least one oxide selected from the group consisting of TiO 2 , Nb 2 O 5 , WO 3 , and Bi 2 O 3 . Therefore, the glass spacer material also contains, as a glass component, TiO 2 , Nb 2 O5 WO 3 , and Bi 2 O 3 Preferably, the oxide contains at least one oxide selected from the group consisting of the following. 2 O 5 It is preferable if it includes this.
[0036] For example, TiO 2 To explain using this as an example, Ti is reduced through a reduction process. 4+ From Ti 3+ This improves conductivity. Ti 3+ The presence of this element can be confirmed, for example, by ESR (electron spin resonance). Similarly, the conductivity of other elements (tungsten, niobium, bismuth) is improved by reduction treatment.
[0037] An example of a reduction treatment is heat treatment of a glass spacer material shaped to a predetermined form in a reducing atmosphere. By performing such a reduction treatment, the surface of the glass spacer material is reduced, thereby lowering the surface resistivity of the glass material surface. Reducing the surface of the glass spacer material is preferable because it is simpler and less expensive than reducing the entire glass, including the interior of the glass spacer. Furthermore, by adjusting the conditions of the reduction treatment, the surface resistivity can be adjusted to a desired range. Examples of reducing gases used as a reducing atmosphere include hydrogen gas. The heat treatment process of glass in a reducing atmosphere is described in detail below.
[0038] First, the glass spacer material, which will serve as spacer 1, is placed in a vacuum / gas-purged furnace and the pressure is reduced. Next, a reducing gas is introduced into the furnace. Then, the furnace is heated to a desired temperature and maintained at that temperature for several minutes to several tens of hours to heat-treat the glass spacer material. It is preferable to set the furnace temperature to a temperature 400°C lower than the glass transition temperature Tg (Tg-400°C) and below the softening point, as this shortens the processing time. Furthermore, the higher the furnace temperature and the longer the processing time, the greater the effect of the reduction treatment, and thus the lower the surface resistance value can be. In other words, the surface resistance value can be adjusted by changing the furnace temperature and processing time.
[0039] In the heat treatment process in the reducing atmosphere described above, if hydrogen gas is used as the reducing gas, the atmosphere inside the furnace may be replaced with a gas other than oxygen, such as nitrogen gas, before replacing the atmosphere with hydrogen gas. By replacing the atmosphere inside the furnace with nitrogen gas or the like once, oxygen inside the furnace is removed, preventing ignition when hydrogen gas is introduced afterward, and allowing the furnace to be heated safely.
[0040] Furthermore, the manufacturing process of the glass spacer material (before reduction treatment) may include a step of melting glass in a reducing atmosphere to obtain molten glass. The reducing atmosphere is preferably a strongly reducing atmosphere. This allows conductivity to be imparted to the inside of the glass spacer material. In this case, the glass spacer material can be used as is without reduction treatment, or it may be subjected to further reduction treatment. Note that the surface resistivity of the glass material when no reduction treatment is performed is, for example, 10 at 22 [°C]. 10 It is greater than or equal to [Ω / sq].
[0041] As an example of the glass in such a spacer 1, the following glass composition can be given: P 2 O 5 37% by mass or less, B 2 O 3 5% by mass or less, Li 2 O 2% by mass or less, N 2 O 10% by mass or less, K 2 O 15% by mass or less, TiO 2 45% by mass or less, Nb 2 O 5 60% by mass or less, WO 3 50% by mass or less, Bi 2 O 3 38% by mass or less. More preferably, for example, the following glass composition may be used: P 2 O 5 20% by mass or more and 30% by mass or less, B 2 O 3 1% by mass or less, Li 2 O 0.5% by mass or less, N 2 O 2% by mass or less, K 2 O 6% by mass or less, TiO 220% by mass or more and 30% by mass or less, Nb 2 O 5 25% by mass or more and 40% by mass or less, WO 3 5% by mass or more and 20% by mass or less, Bi 2 O 3 It is 5% by mass or less.
[0042] Specifically, for example, the following glass composition can be used: P 2 O 5 26.81% by mass, B 2 O 3 0% by mass, Li 2 O 0.08% by mass, N 2 O 0% by mass, K 2 O 4.03% by mass, TiO 2 26.04% by mass, Nb 2 O 5 31.76% by mass, WO 3 11.29% by mass, Bi 2 O 3 0% by mass.
[0043] To produce glass with this composition, fluorides, oxides, hydroxides, carbonates, and nitrates corresponding to the glass components were prepared as raw materials. The raw materials were weighed and blended so that the resulting glass composition would be as described above, and then thoroughly mixed. The resulting blended raw materials (batch raw materials) were heated at 1300°C for 2 to 3 hours to produce molten glass. Water and carbon-containing compounds, i.e., 0.1 wt% to 5 wt% ethanol aqueous solutions, were added to this molten glass by spraying. After that, the molten glass was stirred to homogenize it, clarified, and then poured into a mold preheated to an appropriate temperature. The poured glass was formed into a plate shape, heat-treated at around the glass transition temperature Tg for about 1 hour, and then allowed to cool to room temperature to obtain plate-shaped glass. The content of each glass component in the obtained plate-shaped glass was measured by inductively coupled plasma atomic emission spectrometry (ICP-AES), and the composition was confirmed.
[0044] In one embodiment, the surface roughness Ra of the main surface 4 of the spacer 1 is preferably 1.0 μm or less. Since the spacer 1 is in close contact with the magnetic disk 5 and fixes the magnetic disk 5 by frictional force, the higher the surface smoothness, the larger the contact area and the greater the frictional force. From this point of view, the surface roughness Ra of the main surface 4 is, for example, 1.0 μm or less. The surface roughness Ra is preferably 0.5 μm or less. Note that the smaller the surface roughness Ra of the main surface 4 of the spacer 1, the greater the adhesion force with the magnetic disk 5. Here, Ra, Rz, and skewness Sk, which will be described as surface roughness parameters hereafter, conform to JIS B 0601-2001. Ra is the arithmetic mean roughness, and Rz is the maximum height. Surface roughness is calculated from data measured using, for example, a stylus-type surface roughness meter. Note that a stylus with a tip radius of curvature of 2 μm and a cone taper angle of 60° can be used. Regarding other measurement and calculation parameters, the measurement length can be set to 80 μm, the measurement resolution (pitch) to 0.1 μm, the scan speed to 0.1 mm / second, the cutoff value of the low-pass filter (Ls) to 2.5 μm, and the cutoff value of the high-pass filter (Lc) to 80 μm. When measuring surface roughness parameters using a stylus, the surface roughness is measured by scanning the stylus in the thickness direction of the spacer 1. This allows for accurate evaluation of surface roughness even when numerous fine grooves are formed in the circumferential direction across the entire end face of the spacer 1. If the stylus is scanned along the grooves in the circumferential direction, the groove irregularities may not be evaluated. In other words, if grooves extending in one direction are formed on the surface to be measured, the stylus should be scanned in a direction perpendicular to the direction of extension of these grooves. As for the values of the above surface roughness parameters, for example, the surface of the part to be evaluated can be measured five times, and the average value of the five obtained can be used.
[0045] The outer peripheral end face 2 is an end face that does not come into contact with the magnetic disk 5 and the spindle 14. Preferably, the surface roughness Rz, i.e., the maximum height Rz, of the outer peripheral end face 2 is 1.5 μm or more. Preferably, the surface roughness Rz is 20 μm or less. The reason for making the surface roughness Rz of the outer peripheral end face 2 1.5 μm or more is to allow the gripping jig of the assembly device to easily grip and remove the spacer 1 when removing a specific magnetic disk 5 from the HDD device 10, which is assembled by stacking the magnetic disk 5 and spacer 1 as shown in Figure 2 and fitting it onto the spindle 14 of the HDD device 10. In other words, it is to prevent the gripping jig from slipping when gripping the outer peripheral end face 2 of the spacer 1 and removing it from the spindle 14. Since the magnetic disk 5 and spacer 1 are pressed and fixed by the top clamp 16, the spacer 1 tends to adhere closely to the magnetic disk 5, making it easy for the gripping jig of the assembly device to fail to remove it. If the surface roughness Rz is less than 1.5 μm, the number of extraction failures increases sharply. If the surface roughness Rz exceeds 20 μm, when the spacer is gripped by the gripping jig, the surface of the gripping jig is scraped by the surface irregularities of the outer peripheral end face 2, increasing the likelihood of generating foreign matter such as particles. In this respect, it is preferable that the surface roughness Rz is 20 μm or less. To further reduce the possibility of generating foreign matter such as particles, it is even more preferable that the surface roughness Rz is 10 μm or less. Furthermore, even if there are no extraction failures when the surface roughness Rz is less than 2.0 μm, particles may be generated due to strong friction during extraction. Therefore, it is even more preferable that Rz is 2.0 μm or more.
[0046] According to one embodiment, it is preferable that grooves (grooves) extending along the outer circumference of the spacer 1 are formed on the outer peripheral end face 2. In other words, it is preferable that the grooves are formed along the circumferential direction on the outer peripheral end face 2 of the spacer 1. It is more preferable that the grooves are formed over the entire surface of the outer peripheral end face 2. If there is a chamfered surface, the grooves do not need to be formed on the surface of the chamfered surface. Such grooves can increase the frictional force between the gripping jig of the assembly device and the outer peripheral end face 2, thereby reducing the chances of extraction failure. Such grooves can be confirmed by a laser optical microscope or SEM. The width of the grooves is preferably 10 μm or more on average, in order to ensure sufficient frictional force to prevent extraction failure. On the other hand, if the grooves are too large, burrs are more likely to occur on the convex ridges between the grooves. As will be described in detail later, burrs tend to generate particles when gripping. Therefore, it is preferable that the groove width is 300 μm or less on average. The average value of the groove width can be roughly calculated from the number of grooves within a predetermined length range in the thickness direction of the outer peripheral end face 2. The groove depth is preferably 20 μm or less on average, and more preferably 10 μm or less. In addition, one to three recessed structures may be provided along the circumference of the outer circumferential end face of the spacer for purposes such as preventing deflection of the magnetic disk 5 during assembly. The depth of these recessed structures is generally 100 μm or more, which is clearly larger than the grooves (grooves) mentioned above, and they are easily recognizable by visual inspection and are distinct from the grooves (grooves). It is also possible to use both the recessed structures and the grooves (grooves) in combination. In this case, at least the grooves (grooves) should be provided on the outer circumferential end faces other than those with recessed structures.
[0047] According to one embodiment, the skewness Sk, a parameter that determines the shape of the surface irregularities of the outer peripheral end face 2, is preferably 1.2 or less. If the skewness Sk is greater than 1.2, the surface shape will have relatively sparse sharp protrusions, increasing the likelihood that the sharp protrusions will break when the spacer 1 is gripped, or that the surface of the gripping jig will be scraped, generating foreign matter such as particles. The lower limit of the skewness Sk is not particularly limited, but for example, it is -2. That is, it is more preferable that the skewness Sk is within the range of -2 to +1.2. The skewness Sk is more preferably 0.5 or less, and even more preferably 0 or less, from the viewpoint of reducing the number of sharp protrusions. When forming the grooves (grooves) described above on the outer peripheral end face 2, if there are large burrs in the convex shape between the grooves, the skewness Sk tends to exceed 1.2. In this respect as well, it is preferable that the skewness Sk is 1.2 or less.
[0048] Skewness Sk is a dimensionless parameter obtained by dividing the mean cube of the surface roughness measurement data by the cube of the root mean square height of the surface roughness measurement data. Skewness Sk evaluates the symmetry between the protrusion and groove shapes of the surface roughness and has positive and negative values. The larger the positive value of Skewness Sk, the more steep the protrusion shapes and the gentler the groove shapes, indicating a surface unevenness. The larger the negative absolute value of Skewness Sk, the steeper the groove shapes and the more gentle the protrusion shapes, indicating a surface unevenness. By creating a surface unevenness with a predetermined range of skewness and surface roughness Rz, the frictional force between the gripping jig of the assembly device and the outer peripheral end face 2 can be increased, thereby suppressing failures in removing the spacer 1 and suppressing the generation of foreign matter such as particles.
[0049] The magnetic disk 5 in contact with the spacer 1 is preferably made of a glass substrate with a magnetic film formed on it. Since both the spacer 1 and the magnetic disk 5 are made of glass material, the thermal expansion of the spacer 1 and the magnetic disk 5 can be made approximately the same, and the generation of particles caused by displacement due to differences in thermal expansion can be suppressed.
[0050] Furthermore, according to one embodiment, the spacer 1 and the magnetic disk 5 are in close contact and the magnetic disk 5 is fixed by frictional force. Since the contact area increases and the frictional force increases, it is preferable that the surface roughness Ra of the main surface of the magnetic disk 5 that is in contact with the spacer 1 is 0.3 [nm] or less.
[0051] Such a spacer 1 is suitable for HDD devices that mount eight or more magnetic disks 5. When eight or more magnetic disks 5 are mounted in an HDD device, rather than the usual six, it becomes necessary to press (clamp) the magnetic disks 5 and spacer 1 more firmly with the top clamp 16, requiring a larger pressing pressure from the top clamp 16. This increases the contact force between the spacer 1 assembled in the HDD device and the magnetic disks 5. However, if misalignment occurs due to the difference in thermal expansion between the spacer 1 and the magnetic disks 5, the large pressing pressure makes particle generation more likely. For similar reasons, the spacer 1 of this embodiment is more suitable for use in HDD devices that mount nine or more magnetic disks 5, and even more suitable for use in HDD devices that mount ten or more magnetic disks 5.
[0052] [Example 1] To confirm the effect of spacer 1, spacer 1 was fabricated and the following experiment was conducted. The fabricated spacer 1 had an inner diameter of 25 mm, an outer diameter of 32 mm, a thickness of 2 mm, a chamfer angle of 45 degrees, and a radial width of 150 μm. Spacer 1 was made by cutting a plate of glass made from the glass material containing the above-mentioned oxide into a ring shape, and then grinding and polishing the surface roughness of the end face and main surface, such as Ra and Rz, to be within a predetermined range. After that, the entire surface was reduced by heat treatment under a hydrogen atmosphere. In other words, spacer 1 was made from a reduced material. Furthermore, in order to obtain information on the surface resistivity ρs of the fabricated spacer 1, bulk plate glass was fabricated from the same glass composition containing the same oxide as spacer 1. A plate-shaped glass was cut into a predetermined shape, and the main surface was ground and polished in the same way as the spacer 1 to obtain a plate-shaped glass with the same thickness as the spacer 1 and a surface roughness equivalent to that of the main surface of the spacer 1. After that, the entire surface was reduced by heat treatment in a hydrogen atmosphere to obtain a test specimen. The surface resistivity ρs of the test specimen was determined by measuring the resistance Rs using the measurement method shown in Figure 4. The applied voltage was 100 [V], D = 38.1 mm, d = 25.4 mm, the outer diameter of the annular electrode 24 = 50.8 mm, and the diameter of the counter electrode 22 = 50 mm. Conductive paste was used for the main electrode 20, counter electrode 22, and annular electrode 24. The surface resistivity ρs obtained by measurement was 4.2 × 10⁻¹⁴ at 22 [°C]. 7 The value was [Ω / sq]. At this time, the surface resistivity ρs at the center in the thickness direction was 2.7 × 10⁻⁶. 10The coefficient of static electricity was [Ω / sq]. Each of the seven fabricated spacers 1 was inserted between eight glass magnetic disks (with magnetic films already applied) and assembled into an HDD device. The device was then operated continuously for one week in a constant temperature and humidity chamber while the magnetic head was performing seek operations. No particular problems occurred. Specifically, no foreign matter adhered to the magnetic disks due to static electricity buildup, and this did not cause the HDD device to crash by getting stuck between the head and the magnetic disks. Nor did the magnetic head suffer electrostatic discharge damage due to minute discharges occurring between the magnetic head and the magnetic disks. In other words, it was confirmed that using spacers 1 in an HDD device can suppress static electricity buildup on the magnetic disks 5 and spacers 1.
[0053] [Examples 2-6] Spacer 1 and test specimens with the same glass composition as those prepared in Example 1 were prepared, and the conditions of the reduction treatment (temperature and treatment time in the furnace) were varied to investigate the change in surface resistivity ρs on the surface and inside the test specimens (Examples 2-6). For the internal surface resistivity ρs, the surface of the test specimen was ground and polished to expose the central portion in the thickness direction and measure it. The measurement results, including those for Example 1, are shown in Table 1 below.
[0054]
[0055] In each of the Examples 2 to 6 shown in Table 1, the seven spacers 1 were inserted between eight glass magnetic disks (with magnetic films or the like already applied) and assembled into an HDD device. The device was then continuously operated for one week in a constant temperature and humidity chamber while the magnetic head was performing seek operations, and no particular problems occurred. Specifically, no foreign matter adhered to the magnetic disks due to static electricity buildup, and the HDD device did not crash due to being trapped between the head and the magnetic disks. Nor did the magnetic head suffer electrostatic discharge damage due to minute discharges occurring between the magnetic head and the magnetic disks. That is, by changing the reduction treatment conditions, the surface resistivity on the surface was increased to 10 3 ~10 9 It was confirmed that the spacer 1, with a surface resistivity of [Ω / sq] on its surface that is smaller than that of the interior, can suppress electrostatic charging of the magnetic disk 5 and the spacer 1.
[0056] Although the glass spacer, hard disk drive device, and method for manufacturing the glass spacer of the present invention have been described in detail above, the present invention is not limited to the above embodiments and examples, and various improvements and modifications may be made without departing from the spirit of the present invention.
[0057] 1 Spacer 2 Outer circumference end face 3 Inner circumference end face 4 Main surface 5 Magnetic disk 10 Hard disk drive unit 12 Motor 14 Spindle 16 Top clamp 20 Main electrode 22 Counter electrode 24 Annular electrode 26 DC power supply 28 Ammeter
Claims
1. A ring-shaped glass spacer that is provided in contact with a magnetic disk in a hard disk drive device, wherein the surface resistivity of the glass material of the glass spacer at 22°C is 10 3 ~10 9 [Ω / sq].
2. A ring-shaped glass spacer that is placed in contact with a magnetic disk inside a hard disk drive device, characterized in that the surface resistivity of the glass material surface of the glass spacer at 22°C is lower than the surface resistivity of the interior of the glass material at 22°C.
3. The surface resistivity of the glass material of the glass spacer at 22°C is 10 3 ~10 9 3. The glass spacer according to claim 2, wherein the surface roughness is [Ω / sq].
4. The glass spacer is made of TiO 2 , Nb 2 O 5 , W.O. 3 , and Bi 2 O 3 4. The glass spacer according to claim 1, comprising, as a glass component, at least one oxide selected from the group consisting of:
5. A glass spacer according to any one of claims 1 to 4, wherein the surface roughness Ra of the main surface of the glass spacer that comes into contact with the magnetic disk is 1.0 μm or less.
6. A glass spacer according to any one of claims 1 to 5, wherein the outer peripheral edge of the glass spacer that does not come into contact with the magnetic disk has a surface roughness Rz of 1.5 μm or more.
7. A glass spacer according to claim 6, wherein the surface roughness Rz of the outer peripheral end face is 20 μm or less.
8. The glass spacer according to any one of claims 1 to 7, wherein a groove extending along the outer periphery of the glass spacer is formed on the outer peripheral end face of the glass spacer that does not come into contact with the magnetic disk.
9. The glass spacer according to any one of claims 1 to 8, wherein the skewness of the outer peripheral end surface of the glass spacer that does not come into contact with the magnetic disk is 1.2 or less.
10. A hard disk drive device comprising the glass spacer according to any one of claims 1 to 9 and the magnetic disk.
11. The hard disk drive device according to claim 10, wherein the magnetic disk is a disk having a magnetic film formed on a glass substrate.
12. The hard disk drive device according to claim 11, wherein the surface roughness Ra of the main surface of the magnetic disk is 0.3 nm or less.
13. The hard disk drive device according to any one of claims 10 to 12, which is equipped with eight or more magnetic disks.
14. A method for manufacturing a ring-shaped glass spacer that is arranged to contact a magnetic disk within a hard disk drive device, comprising the steps of: preparing a glass spacer material that is the raw material for the glass spacer; and reducing the surface resistivity of the surface of the glass spacer material by reducing the surface of the glass spacer material.
15. The glass spacer contains TiO as a glass component. 2 , Nb 2 O 5 , W.O. 3 , and Bi 2 O 3 The method for producing a glass spacer according to claim 14, wherein the glass spacer comprises at least one oxide selected from the group consisting of: