Self-assembled monolayer for selective deposition
Patent Information
- Application Number
- TW111123156
- Authority / Receiving Office
- TW · TW
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-12-17
- Filing Date
- 2022-06-22
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2042-06-21
AI Technical Summary
As integrated circuits shrink in size, reducing via resistance becomes critical to improve performance, and existing methods struggle to effectively minimize overlay and resistivity in metallization layers.
A method involving self-assembled monolayers (SAMs) formed from morpholine or phenanthroline derivatives is used to selectively deposit materials on metallic and non-metallic surfaces, forming a protected metal surface and a liner on dielectric surfaces, utilizing atomic layer deposition techniques to control via resistance.
This approach reduces via resistance, enhancing the performance of electronic components by selectively depositing materials, thereby improving the integrity and conductivity of semiconductor structures.
Smart Images

Figure TWG2TB001919971_001 
Figure TWG2TB001919971_002 
Figure TWG2TB001919971_003
Abstract
Description
[Technical Field]
[0001] The embodiments of this disclosure generally relate to methods for forming semiconductor structures. More specifically, some embodiments of this disclosure relate to methods for selectively depositing a self-assembled monolayer formed of morpholine on a non-metallic surface. [Previous Technology]
[0002] Generally speaking, an integrated circuit (IC) refers to a group of electronic components, such as transistors formed on a small wafer of semiconductor material (usually silicon). Typically, an IC includes one or more metallized layers with metal wires to interconnect the electronic components of the IC and connect them to external connections. Typically, interlayer dielectric material layers are placed between the metallized layers of the IC for insulation.
[0003] As the size of integrated circuits decreases, the spacing between metal lines also decreases. Typically, planar processes are used to fabricate interconnect structures, which involve aligning and connecting one metal layer to another.
[0004] Reducing the resistance of vias is crucial for improving the performance of electronic components. The reduction of via resistance is typically controlled by minimizing the coating and by reducing the resistivity of the via material. Therefore, a method for reducing via resistance is needed. [Summary of the Invention]
[0005] One or more embodiments of this disclosure are directed to a method of forming a self-assembled monolayer (SAM), comprising exposing a substrate having an exposed metal surface to a first precursor comprising a cyanoline or a cyanoline derivative.
[0006] An additional embodiment of this disclosure relates to a selective deposition method, comprising exposing a substrate having an exposed metal surface and an exposed non-metal surface to a first precursor comprising a cyanoline or a cyanoline derivative to form a protected metal surface. Material is selectively deposited on the exposed non-metal surface relative to the protected metal surface.
[0007] Other embodiments of this disclosure relate to a method of forming a semiconductor structure. The method includes selectively forming a self-assembled monolayer (SAM) on a first surface of a substrate by exposing the substrate to a first precursor. The substrate has at least one feature including a first surface and a second surface. The first surface comprises a metallic material, and the second surface comprises a dielectric material. The first precursor comprises a cyanoline or a derivative thereof. A pad is selectively deposited on the second surface by exposing the substrate to a second precursor.
Implementation Method
[0012] Before describing several exemplary embodiments of this disclosure, it should be understood that this disclosure is not limited to the details of the structures or process steps set forth in the following description. Other embodiments can be exemplified in this disclosure, and it can be practiced or performed in various ways.
[0013] As used in this specification and the appended claims, the term "substrate" refers to a surface or part of a surface on which a process is performed. Those skilled in the art will also understand that reference to a substrate may also refer to only a part of a substrate, unless the context clearly indicates otherwise. Furthermore, reference to deposition on a substrate may refer to a bare substrate or a substrate on which one or more films or features are deposited or formed.
[0014] As used herein, "substrate" refers to any substrate or material surface formed on a substrate during manufacturing. For example, depending on the application, substrate surfaces on which processing can be performed include materials such as silicon, silicon oxide, strained silicon, silicon on insulator (SOI), carbon-doped silicon oxide, amorphous silicon, doped silicon, germanium, gallium arsenide, glass, sapphire, and any other materials such as metals, metal nitrides, metal alloys, and other conductive materials. Substrates include, but are not limited to, semiconductor wafers. Substrates may be exposed to pretreatment processes to polish, etch, reduce, oxidize, hydroxylate, anneal, UV cure, electron beam cure, and / or bake the substrate surface. In addition to performing film processing directly on the surface of the substrate itself, any film processing steps disclosed in this disclosure may also be performed on an underlayer formed on the substrate, as disclosed in more detail below, and the term "substrate surface" is intended to include such an underlayer as referred to in the context. Therefore, for example, in the case where a film / layer or part of a film / layer has already been deposited on the substrate surface, the exposed surface of the newly deposited film / layer becomes the substrate surface.
[0015] As used herein, "atomic layer deposition" or "cyclic deposition" refers to the sequential exposure of two or more reactive compounds to deposit a material layer on a substrate surface. As used in this specification and the appended claims, the terms "reactive compound," "reactive gas," "reactive species," "precursor," "process gas," etc., are used interchangeably to refer to a species of substance capable of reacting with the substrate surface or a material on the substrate surface in a surface reaction (e.g., chemisorption, oxidation, reduction). The substrate or a portion of the substrate is sequentially or substantially sequentially exposed to the precursor (or reactive gas). As used throughout the specification, "substantially sequentially" means that the majority of the duration of precursor exposure does not overlap with the exposure of the co-reagent, but there may be some overlap.
[0016] In many applications, metals can be grown by atomic layer deposition. One or more embodiments of this disclosure advantageously provide a process for atomic layer deposition to form a metal-containing film. As used in this specification and the appended claims, the term "metal-containing film" refers to a film containing metal atoms and having a metal content greater than or equal to about 1 atomic percent, 2 atomic percent, 3 atomic percent, 4 atomic percent, 5 atomic percent, 10 atomic percent, 15 atomic percent, 20 atomic percent, 25 atomic percent, 30 atomic percent, 35 atomic percent, 40 atomic percent, 45 atomic percent, 50 atomic percent, 55 atomic percent, 60 atomic percent, or 65 atomic percent. In some embodiments, the metal-containing film includes one or more of a metal, a metal nitride, a metal carbide, or a metal oxide. Those skilled in the art will recognize that the use of a molecular formula such as MO (where M is a metal) does not imply a specific stoichiometric relationship between elements, but is merely an identification of the main components of the film. For example, MO refers to a membrane whose main components include metal and oxygen atoms. In some embodiments, based on atomic percentages, the main components of a particular membrane (i.e., the total atomic percentage of a particular atom) are greater than or equal to about 95%, 98%, 99%, or 99.5% of the membrane.
[0017] As used herein, the phrases "metallic material surface" or "non-metallic material surface" refer to the surface of a metallic or non-metallic material, respectively. For the purposes of this disclosure, a non-metallic material is any material that exhibits poor conductor or good insulator properties. Non-metallic materials may include metallic atoms (e.g., tantalum nitride, titanium nitride) and still fall within the category of non-metallic materials. In some embodiments, the term "conductive material" is used instead of "metallic material." In some embodiments, the term "dielectric material" is used instead of "non-metallic material."
[0018] As used herein, the phrase “selective deposition on a first surface relative to a second surface” and similar terms refer to a first amount or thickness deposited on a first surface, a second amount or thickness deposited on a second surface, wherein the second amount or thickness is less than the first amount or thickness, or in some embodiments, no amount or thickness is deposited on the second surface.
[0019] As used herein, the term "relative" does not mean the physical orientation of one surface over another, but rather the relationship of the thermodynamic or kinetic properties of the chemical reactions of one surface relative to the other. For example, selective deposition of a thin film on a metallic surface relative to a nonmetallic surface means that a film is deposited on the metallic surface, while little or no film is deposited on the nonmetallic surface; or that forming a thin film on a metallic surface is thermodynamically or kinetically advantageous relative to forming a film on a nonmetallic surface.
[0020] Reducing the contact resistance (Rc) of semiconductor structures at 3-nanometer nodes (N3) and above is crucial. Therefore, one or more embodiments of this disclosure relate to a method of selectively forming a self-assembled monolayer (SAM) on a first surface of a substrate relative to a second surface. The substrate includes a metallic material (conductive material) having a first surface and a non-metallic material (dielectric material) having a second surface. In some embodiments, the first surface may be described as a metallic material surface or a conductive material surface. In some embodiments, the first surface includes one or more of copper (Cu), cobalt (Co), ruthenium (Ru), tungsten (W), or molybdenum (Mo). In some embodiments, the first surface includes one or more of tungsten (W) or molybdenum (Mo). In some embodiments, the second surface may be described as a non-metallic material surface or a dielectric material surface. In some embodiments, the method described herein has applications in the middle end of line (MEOL) and the back end of line (BEOL).
[0021] Referring to Figure 1, one or more embodiments of this disclosure relate to a method 100 for forming an electronic device. The method shown in Figure 1 represents an integration process.
[0022] Figures 2A to 2G illustrate cross-sectional views of an exemplary apparatus 200 during a processing method 100 according to one or more embodiments of this disclosure. Referring to Figure 2A, a substrate 210 is provided having a barrier layer 215, a metal pad 220, a conductive layer 225, an etch stop layer 230, and a dielectric layer 235 thereon. In one or more embodiments, the dielectric layer 235 has at least one feature 240. In some embodiments, the substrate 210 is a wafer, such as a semiconductor substrate. In some embodiments, the substrate 210 is an etch stop layer on a wafer.
[0023] For illustrative purposes, Figure 2A shows a substrate 210 having a single feature 240. However, those skilled in the art will understand that there may be more than one feature. As shown in Figure 2A, feature 240 includes a first surface 245 and a second surface 250. In some embodiments, the first surface 245 is the bottom surface of feature 240. In some embodiments, the second surface 250 is a sidewall of feature 240. The shape of feature 240 may be any suitable shape, including but not limited to trenches, vias that carry current between layers when filled with metal, and lines that carry current within the same element layer. It should be understood that in one or more embodiments, conductive layer 225 forms metal lines that carry current within the same element layer. In some embodiments, feature 240 defines a gap in dielectric layer 235. As used herein, the term "feature" refers to any intentional surface irregularity. Suitable examples of features include, but are not limited to, trenches having a top, two sidewalls, and a bottom, and peaks having a top and two sidewalls. Features may have any suitable aspect ratio (the ratio of the depth of a feature to the width of a feature). In some embodiments, the aspect ratio is greater than or equal to about 1:1, 2:1, 3:1, 4:1, 5:1, 10:1, 15:1, 20:1, 25:1, 30:1, 35:1 or 40:1.
[0024] In one or more embodiments, the barrier layer 215 is a conformal layer. The barrier layer 215 may comprise any suitable material known to those skilled in the art and may be deposited using any suitable technique known to those skilled in the art. In some embodiments, the barrier layer is selected from titanium nitride (TiN) and tantalum nitride (TaN) or tungsten nitride (WN). In a particular embodiment, the barrier layer 215 comprises tantalum nitride (TaN). In some embodiments, the barrier layer 215 is formed of an ALD. In some embodiments, the barrier layer 215 prevents material from diffusing through itself to the underlying layer.
[0025] In one or more embodiments, the metal pad 220 may comprise any suitable metallic material known to those skilled in the art and may be deposited using any technique known to those skilled in the art. In one or more embodiments, the metal pad 220 comprises one or more of copper (Cu), cobalt (Co), ruthenium (Ru), iridium (Ir), rhodium (Rh), molybdenum (Mo), tungsten (W), aluminum (Al), nickel (Ni), and platinum (Pt). In one or more embodiments, the metal pad 220 comprises one or more of a monolayer of tungsten (W) or a monolayer of molybdenum (Mo). In some embodiments, the metal pad 220 comprises tungsten or molybdenum or is substantially composed of tungsten or molybdenum. As used in this specification and the appended claims, the term "substantially composed of" means that the material is greater than or equal to about 95%, 98%, or 99% of the material on an atomic basis.
[0026] In one or more embodiments, the conductive layer 225 comprises a metal or a metallic material. In some embodiments, the metal or metallic material may be any suitable metallic material. In some embodiments, the metallic material disclosed herein is a conductive material. Suitable metallic materials include, but are not limited to, metals, conductive metal nitrides, conductive metal oxides, metal alloys, silicon, combinations thereof, and other conductive materials.
[0027] The term "oxide" or similar term used in this specification and the appended claims means that a material contains a specific element. This term should not be construed as implying a specific proportion of the element. Therefore, "oxide" or similar terms may include elements in stoichiometric proportions or not.
[0028] In one or more embodiments, the metal or metallic material may include any suitable metal known to those skilled in the art. In some embodiments, the metal or metallic material is selected from one or more of copper (Cu), cobalt (Co), ruthenium (Ru), iridium (Ir), rhodium (Rh), molybdenum (Mo), tungsten (W), aluminum (Al), nickel (Ni), and platinum (Pt). In some embodiments, the metal or metallic material is substantially composed of copper (Cu), cobalt (Co), ruthenium (Ru), iridium (Ir), rhodium (Rh), molybdenum (Mo), tungsten (W), aluminum (Al), nickel (Ni), and platinum (Pt). In some embodiments, the metal or metallic material is substantially composed of copper, cobalt, ruthenium, tungsten, or molybdenum. In some embodiments, the metallic material comprises or is primarily composed of tungsten or molybdenum.
[0029] In one or more embodiments, the etch stop layer 230 comprises any suitable material known to those skilled in the art. In one or more embodiments, the etch stop layer 230 comprises one or more of silicon nitride (SiN), silicon carbide (SiC), aluminum oxide (AlOx), and aluminum nitride (AlN). In some embodiments, the etch stop layer 230 may be deposited using techniques selected from CVD, PVD, and ALD.
[0030] In one or more embodiments, a portion of the metal pad 220 and the etch stop layer 230 are removed, exposing a bottom first surface 245 of at least one feature 240. In some embodiments, the bottom first surface 245 is a portion of the top surface of the conductive material 225, such that a portion of the conductive material 225 is exposed.
[0031] In one or more embodiments, the dielectric layer 235 may be any suitable material. In some embodiments, the dielectric layer 235 isolates adjacent components and prevents leakage. Suitable dielectric materials include, but are not limited to, silicon oxide (e.g., SiO2), silicon nitride (e.g., SiN), silicon carbide (e.g., SiC), and combinations thereof (e.g., SiCON). Suitable dielectric materials further include alumina, aluminum nitride, and low-k dielectric materials. In some embodiments, the dielectric material is primarily composed of silicon dioxide (SiO2). In some embodiments, the dielectric layer 235 comprises silicon nitride. In some embodiments, the dielectric layer 235 is substantially composed of silicon nitride.
[0032] In one or more embodiments, the dielectric layer 235 is deposited using any suitable deposition technique, such as, but not limited to, chemical vapor deposition ("CVD"), physical vapor deposition ("PVD"), molecular beam epitaxy ("MBE"), metal-organic chemical vapor deposition ("MOCVD"), atomic layer deposition ("ALD"), spin coating, or other deposition techniques known to those skilled in the art in the field of microelectronic device fabrication.
[0033] In one or more embodiments, during one or more operations of method 100, the substrate is independently held under an operating pressure. In some embodiments, the operating pressure is less than or equal to 100 Torr, less than or equal to 80 Torr, less than or equal to 70 Torr, less than or equal to 60 Torr, less than or equal to 50 Torr, less than or equal to 40 Torr, less than or equal to 30 Torr, less than or equal to 20 Torr, less than or equal to 15 Torr, less than or equal to 10 Torr, less than or equal to 5 Torr, less than or equal to 1 Torr, less than or equal to 50 Torr, less than or equal to 50 Torr. In some embodiments, the operating pressure is 10 Torr, 20 Torr, 30 Torr, 40 Torr, or 50 Torr. In some embodiments, the substrate 210 is deposited with a self-assembled monolayer (SAM). During the 255 period, the values remained at 1 mTorr to 100 mTorr, 1 mTorr to 80 mTorr, 1 mTorr to 60 mTorr, 1 mTorr to 40 mTorr, 1 mTorr to 20 mTorr, 1 mTorr to 10 mTorr, 1 mTorr to 5 mTorr, 1 mTorr to 1 mTorr, 1 mTorr to 50 mTorr, 1 mTorr to 200 mTorr, 1 mTorr to 100 mTorr, 1 mTorr to 50 mTorr, 500 mTorr to 100 mTorr, 500 mTorr to 80 mTorr, 500 mTorr to 60 mTorr, 500 mTorr to 40 mTorr, and 500 mTorr to 20 mTorr. Pressure ranges from 500 mTorr to 10 Torr, from 500 mTorr to 5 Torr, from 500 mTorr to 1 Torr, from 1 Torr to 100 Torr, from 1 Torr to 80 Torr, from 1 Torr to 60 Torr, from 1 Torr to 40 Torr, from 1 Torr to 20 Torr, from 1 Torr to 10 Torr, from 1 Torr to 5 Torr, from 10 Torr to 100 Torr, from 10 Torr to 80 Torr, from 10 Torr to 60 Torr, from 10 Torr to 40 Torr, from 10 Torr to 20 Torr, from 20 Torr to 100 Torr, from 20 Torr to 80 Torr, from 20 Torr to 60 Torr, or from 20 Torr to 40 Torr.
[0034] In some embodiments, the temperature of the substrate is controlled during method 100. The temperature of the substrate may also be referred to as the operating temperature. In some embodiments, the operating temperature is less than or equal to 450°C, less than or equal to 400°C, less than or equal to 350°C, less than or equal to 300°C, less than or equal to 275°C, less than or equal to 250°C, less than or equal to 225°C, less than or equal to 200°C, less than or equal to 150°C, less than or equal to 100°C, or less than or equal to 80°C. In some embodiments, the operating temperature is within the range of 60°C to 450°C, 60°C to 350°C, 60°C to 250°C, 60°C to 150°C, 60°C to 100°C, 100°C to 450°C, 100°C to 350°C, 100°C to 250°C, 100°C to 200°C, 200°C to 450°C, 200°C to 350°C, 200°C to 300°C, 300°C to 450°C, 300°C to 350°C, or 400°C to 450°C during the deposition of the self-assembled monolayer (SAM) 255.
[0035] Referring to Figure 1, exemplary method 100 begins with an optional pre-cleaning operation 102. The pre-cleaning operation can be any suitable pre-cleaning process known to those skilled in the art. Suitable pre-cleaning operations include, but are not limited to, soaking, natural oxide removal, etc. In some embodiments, pre-cleaning operation 102 cleans a first surface 245 and a second surface 250. In some embodiments, pre-cleaning operation 102 results in the formation of substantially oxide-free surfaces, such as the first surface 245 and / or the second surface 250. As used herein, the term "substantially oxide-free" means that the surface has less than 10%, less than 5%, less than 4%, less than 3%, less than 2%, or less than 1% oxygen on an atomic basis.
[0036] In operation 104, a substrate is exposed to a first precursor to deposit a self-assembled monolayer (SAM) 255. As used herein, the phrase "substrate exposed to" means that the substrate, including the various materials and layers thereon, is exposed as a whole to the process or conditions described. Figure 2B illustrates the self-assembled monolayer (SAM) 255 deposited on a first surface 245 of feature 240. In some embodiments, the self-assembled monolayer (SAM) 255 is selectively deposited on the first surface 245 relative to the second surface 250. In some embodiments, the self-assembled monolayer (SAM) is not deposited on the second surface 250 of feature 240. In one or more embodiments, the self-assembled monolayer (SAM) 255 is deposited on the exposed first surface 245 of the conductive layer 225 at the bottom of feature 240. Note that, as described above, a portion of the metal pad 220 and a portion of the etch stop layer 230 are removed, for example, by etching, to expose a portion, such as the first surface 245 of the conductive layer 225 at the bottom of feature 240. In some embodiments, operation 104 is a dry deposition process. In some embodiments, the surface having a self-assembled monolayer (SAM) 255 thereon is referred to as a protected surface.
[0037] In some embodiments, "selectively" means that the formation rate of the material on the selected surface is greater than or equal to about 1.5 times, 2 times, 3 times, 4 times, 5 times, 7 times, 10 times, 15 times, 20 times, 25 times, 30 times, 35 times, 40 times, 45 times, or 50 times that on the non-selected surface. In other words, the process selectivity of the selected surface relative to the non-selected surface is greater than or equal to about 3:2, 2:1, 3:1, 4:1, 5:1, 7:1, 10:1, 15:1, 20:1, 25:1, 30:1, 35:1, 40:1, 45:1, or 50:1.
[0038] In one or more embodiments, the first precursor is reversibly bonded to a metal. In some embodiments, the self-assembled monolayer (SAM) 255 formed from the first precursor remains substantially intact during subsequent operations of method 100. As used herein, the term "substantially" means that up to 99%, 98%, 95%, 90%, or 80% of the self-assembled monolayer (SAM) 255 remains intact during subsequent operations of method 100.
[0039] In some embodiments, the first precursor comprises phenobarbital or a derivative thereof. For the avoidance of doubt, phenobarbital is an organic heterocyclic compound having the following structure: such compounds are also known as 1,10-phenobarbital.
[0040] In some embodiments, the first precursor comprises a phenobarbital derivative. In this sense, a "phenobarbital derivative" is any compound having a phenobarbital "core" that is substituted at any of the eight available carbons. For the avoidance of doubt, the eight available carbons are conventionally numbered 2-9, as follows:
[0041] In some embodiments, the first compound is substituted with an alkyl group. In some embodiments, the first compound is substituted with an alkenyl or aryl group. In some embodiments, the first compound is substituted with a C1-C18 group, a C4-C12 group, or a C6-C10 group. "C1-C18 group" and the like, as used in this sense, comprises 1-18 carbon atoms. In some embodiments, the alkyl or alkenyl group is a linear group (e.g., a straight-chain saturated or unsaturated hydrocarbon). In some embodiments, the alkyl or alkenyl group is a branched group (e.g., a branched-chain saturated or unsaturated hydrocarbon). In some embodiments, the alkyl, alkenyl, or aryl group is a cyclic group (e.g., a cyclic saturated or unsaturated hydrocarbon).
[0042] In some embodiments, the first compound is substituted with one group, two groups, four groups, or more groups (e.g., six groups, eight groups). In some embodiments, the substitutions are symmetrical. Symmetrical substitution is a substitution that is a mirror image of the substitutions between carbons 5 and 6 and the two nitrogen atoms in a plane. For example, substitutions at carbons 4 and 7 would be symmetrical.
[0043] In some embodiments, when the metal surface 245 contains tungsten, molybdenum or a combination thereof, the self-assembled monolayer (SAM) 255 selectively blocks the metal surface 245, but keeps the non-metallic surface 250 intact during subsequent operations of method 100.
[0044] In one or more embodiments, substrate 210 may be exposed to the first precursor at any suitable flow rate to form a self-assembled monolayer (SAM) 255. In some embodiments, substrate 210 is exposed to the first precursor at flow rates ranging from 50 sccm to 2000 sccm, 100 sccm to 2000 sccm, 500 sccm to 2000 sccm, 1000 sccm to 2000 sccm, 1500 sccm to 2000 sccm, 50 sccm to 100 sccm, and 75 sccm to 100 sccm. In some embodiments, the flow rate of the first precursor is less than or equal to 2000 sccm, less than or equal to 1500 sccm, less than or equal to 1000 sccm, less than or equal to 600 sccm, less than or equal to 500 sccm, less than or equal to 400 sccm, less than or equal to 300 sccm, less than or equal to 250 sccm, less than or equal to 200 sccm, less than or equal to 150 sccm, less than or equal to 100 sccm, less than or equal to 75 sccm, or less than or equal to 50 sccm.
[0045] In some embodiments, the substrate 210 is immersed in the vapor of the first precursor. In some embodiments, the substrate 210 is immersed in the liquid of the first precursor. In some embodiments, the immersion period may be any suitable period for forming the self-assembled monolayer (SAM) 255. In some embodiments, the immersion time is greater than or equal to 10 seconds, greater than or equal to 20 seconds, greater than or equal to 30 seconds, greater than or equal to 45 seconds, greater than or equal to 60 seconds, greater than or equal to 80 seconds, greater than or equal to 120 seconds, greater than or equal to 150 seconds, or greater than or equal to 200 seconds.
[0046] In one or more embodiments, the first precursor is a liquid at the operating temperature and / or operating pressure. In one or more embodiments, the first precursor is a solid at the operating temperature and / or operating pressure. In some embodiments, the first precursor is stored in an ampoule or cylinder from which it is conveyed to the substrate 210. In some embodiments, the first precursor has a vapor pressure ranging from 0.1 Torr to 150 Torr, from 0.1 Torr to 100 Torr, from 0.1 Torr to 50 Torr, from 0.1 Torr to 10 Torr, from 0.1 Torr to 1 Torr, from 0.1 Torr to 0.5 Torr, from 0.5 Torr to 150 Torr, from 0.5 Torr to 100 Torr, from 0.5 Torr to 50 Torr, from 0.5 Torr to 10 Torr, from 0.5 Torr to 1 Torr, from 1 Torr to 150 Torr, from 1 Torr to 100 Torr, from 1 Torr to 50 Torr, from 10 Torr to 100 Torr, from 10 Torr to 50 Torr, from 50 Torr to 150 Torr, from 50 Torr to 100 Torr, or from 100 Torr to 150 Torr at the operating temperature and / or operating pressure. In some embodiments, at operating temperature and / or operating pressure, the first precursor has a vapor pressure greater than or equal to about 0.1 Torr.
[0047] In one or more embodiments, the first precursor further includes a carrier gas. In some embodiments, the carrier gas is a non-reactive gas. In some embodiments, the carrier gas includes an inert gas. In some embodiments, the inert gas includes one or more of helium (He), neon (Ne), or argon (Ar). In some embodiments, the carrier gas includes argon (Ar).
[0048] In some embodiments, a carrier gas flow is configured to transport the first precursor from the container to the substrate 210. In some embodiments, the flow rate of the argon (Ar) gas configured to transport the first precursor to the substrate 210 is controlled.
[0049] Referring to Figure 1, in operation 106, substrate 210 is exposed to a second precursor to selectively deposit a pad on second surface 250. Figure 2C illustrates a pad 260 selectively deposited on second surface 250. In some embodiments, pad 260 is formed on second surface 250 instead of first surface 245. In some embodiments, pad 260 is a conformal layer. Pad 260 may comprise any suitable material known to those skilled in the art and may be deposited using any suitable technique known to those skilled in the art. In some embodiments, pad 260 comprises a metal nitride. In some embodiments, pad 260 comprises tantalum nitride (TaN), titanium nitride (TiN), or a combination thereof. In some embodiments, pad 260 has the same properties as barrier layer 215. In some embodiments, pad 260 is selectively deposited via atomic layer deposition (ALD). In some embodiments, self-assembled monolayer (SAM) 255 selectively blocks metal interface 245 while keeping non-metallic surface 250 intact for selective ALD deposition. In some embodiments, the pad 260 is deposited by sequentially exposing the substrate 210 to a metal precursor and a reactant. In some embodiments, the pad 260 is formed without the use of plasma. In some embodiments, the thickness of the pad 260 is in the range of about 2 angstroms to about 20 angstroms. In some embodiments, the pad 260 is formed in a single ALD cycle. In some embodiments, the pad 260 is formed in 2 to 40 ALD cycles. In one or more embodiments, each ALD cycle is configured to deposit a pad 260 with a thickness of about 0.5 angstroms.
[0050] Referring to Figure 1, in operation 108, the self-assembled monolayer (SAM) 255 is removed. Figure 2D illustrates the self-assembled monolayer (SAM) 255 removed from the first surface 245. The self-assembled monolayer (SAM) 255 is removed by an etching process. In some embodiments, the etching process may include any suitable means, including but not limited to a plasma cleaning process. In one or more embodiments, the self-assembled monolayer (SAM) 255 is removed by a plasma treatment. In some embodiments, the plasma includes one or more of hydrogen (H2), nitrogen (N2), or argon (Ar) plasmas. As used herein, a plasma comprising hydrogen, nitrogen, or argon means a plasma formed from the molecular form of a specified species. In some embodiments, the plasma is substantially composed of hydrogen, nitrogen, argon, or a combination thereof. In some embodiments, the self-assembled monolayer (SAM) 255 is removed without causing substantial damage to the pad 260.
[0051] The power of the plasma may vary depending on the composition, filler and / or thickness of the self-assembled monolayer (SAM) and the composition and / or thickness of the surrounding material. In some embodiments, the plasma power is in the range of about 20 W to about 500 W, about 20 W to about 400 W, about 20 W to about 250 W, about 50 W to about 500 W, about 100 W to about 450 W, about 100 W to about 500 W, or about 200 W to about 400 W. In some embodiments, the plasma power is about 50 W, about 200 W, or about 400 W.
[0052] The duration of plasma exposure may vary depending on the composition, filler and / or thickness of the self-assembled monolayer (SAM) 255 and the composition and / or thickness of the surrounding material. In some embodiments, the time period of substrate exposure to plasma ranges from about 2 seconds to about 60 seconds, from about 3 seconds to about 30 seconds, or from about 5 seconds to about 10 seconds. In some embodiments, the time period of substrate exposure to plasma is about 3 seconds, about 5 seconds, about 10 seconds, or about 30 seconds.
[0053] Referring to Figure 1, in operation 110, the pad 260 may be densified by a densification process. Figure 2F shows the pad 260 being densified to extend on a portion of the facing feature 245 of the etch stop layer 230. In some embodiments, the densification process includes physical vapor deposition (PVD). In some embodiments, physical vapor deposition (PVD) includes doped physical vapor deposition. In some embodiments, after the densification process, the thickness of the pad 260 is in the range of 5 to 20 mm.
[0054] In some embodiments, operations 108 and 110 are performed simultaneously. Therefore, in some embodiments, the removal of the self-assembled monolayer (SAM) 255 and the densification of the pad 260 are performed simultaneously. In some embodiments, the etching of the self-assembled monolayer (SAM) 255 and the densification of the pad 260 are performed simultaneously. In some embodiments, the selective removal and densification of the pad 260 are performed simultaneously.
[0055] Referring to Figures 1 and 2E, in operation 112, an adhesive layer 265 is deposited on the barrier layer 260 and the first surface 245. Figure 2F illustrates the adhesive layer 265 deposited on the barrier layer 260 and the first surface 245. In some embodiments, the adhesive layer 265 is conformally deposited on the barrier layer 260 and the first surface 245. In some embodiments, the thickness of the adhesive layer 265 on the barrier layer 260 is the same as the thickness of the adhesive layer 265 on the first surface 245. In some embodiments, the thickness of the adhesive layer 265 on the barrier layer 260 is different from the thickness of the adhesive layer 265 on the first surface 245. In some embodiments, the thickness of the adhesive layer 265 on the barrier layer 260 is greater than the thickness of the adhesive layer 265 on the first surface 245. In some embodiments, the adhesive layer 265 comprises any suitable material known to those skilled in the art and can be deposited using any suitable technique known to those skilled in the art. In one or more embodiments, the adhesive layer 265 includes one or more of cobalt (Co) and ruthenium (Ru). In some embodiments, the adhesive layer 265 includes a cobalt, ruthenium (Ru), or a ruthenium / cobalt (Ru / Co) binary layer.
[0056] Referring to Figures 1 and 2G, in operation 114, method 100 includes depositing a conductive material 270 in at least one feature 240 by exposing a substrate to a third precursor. In some embodiments, the third precursor comprises a metal. In some embodiments, the third precursor comprises copper. In some embodiments, the conductive material 270 is deposited on an adhesive layer 265 via a gap-filling process. In some embodiments, the gap-filling process includes bottom-up filling or conformal filling. Figure 2G illustrates the conductive material 270 forming interconnects within feature 245.
[0057] The conductive material 270 may be any suitable material known to those skilled in the art. In some embodiments, the conductive filler material 270 includes one or more of copper (Cu), tungsten (W), and molybdenum (Mo). In some embodiments, the conductive filler material 270 includes copper (Cu). In a particular embodiment, the conductive material 270 includes copper.
[0058] In some embodiments, feature 240 includes a bottom and a top. In some embodiments, the bottom includes a through-hole. In some embodiments, the top includes a trench. In some embodiments, a first conductive filler material is grown in a bottom-up manner to fill the through-hole portion constituting the lower part of feature 240. In some embodiments, a second conductive material is deposited in the upper part. In some embodiments, the first conductive material and the second conductive material are the same. In some embodiments, the first conductive material and the second conductive material are different. In some embodiments, the entire feature 240 is filled with a single conductive material at a time to fill the lower and upper parts of feature 240 in one process.
[0059] The conductive material 270 may be deposited using any suitable technique known to those skilled in the art. In some embodiments, the conductive material 270 is deposited using one or more of a chemical vapor deposition (CVD) process, an atomic layer deposition (ALD) process, or a physical vapor deposition (PVD) process. In some embodiments, the conductive material 270 is deposited to overfill the feature 240 and form a capping layer on the surface of the substrate 210. The capping layer is then removed using any suitable technique, such as etching or chemical-mechanical planarization (CMP).
[0060] Without being bound by theory, it is believed that the self-assembled monolayer (SAM) 255 increases the resistance of the conductive filler 270 only slightly compared to the resistance increase typically seen in most barrier layers (e.g., film 260). Therefore, removing the self-assembled monolayer (SAM) 255 is an optional process that can further reduce the resistance of the conductive filler 270. In some embodiments, the removal of the self-assembled monolayer (SAM) 255 reduces the resistance of the metal interconnect 270 by 30%, 20%, 10%, or 5%.
[0061] Other embodiments of this disclosure pertain to a processing tool 900 used to form the apparatus and method, as shown in Figure 3. Various multiprocessing platforms can be used, including CENTURA®, DUAL ACP, PRODUCER® GT, and ENDURA® platforms and other processing systems provided by Applied Materials®. In one or more embodiments, the clustering tool 900 includes at least one central transfer station 921, 931 having a plurality of sides. Robots 925, 935 are located within the central transfer stations 921, 931 and are configured to move robot pallets and wafers to each of the plurality of sides.
[0062] The cluster tool 900 includes a plurality of processing chambers 902, 904, 906, 908, 910, 912, 914, 916, and 918, also referred to as processing stations, connected to a central transfer station. Each processing chamber provides an independent processing area isolated from adjacent processing stations. The processing chambers can be any suitable chamber, including but not limited to selective metal deposition chambers; barrier metal deposition chambers; metal deposition chambers; PVD metal deposition chambers; CVD metal deposition chambers; self-assembled monolayer (SAM) deposition chambers; pad metal deposition chambers; plasma chambers; pre-cleaning chambers; etching chambers; transfer spaces; wafer orientation / degassing chambers; cryogenic cooling chambers, etc. The specific arrangement of the processing chambers and components may vary depending on the cluster tool and should not be considered as limiting the scope of this disclosure.
[0063] In one or more embodiments, the clustering tool 900 includes a self-assembled monolayer (SAM) deposition chamber for exposing a substrate to planar hydrocarbons and forming a self-assembled monolayer (SAM). In one or more embodiments, the clustering tool 900 includes a pre-cleaning chamber connected to a central transfer station.
[0064] In the embodiment shown in Figure 3, the factory interface 950 is connected to the front end of the clustering tool 900. The factory interface 950 includes a loading chamber 954 and an unloading chamber 956 on the front end 951 of the factory interface 950. Although the loading chamber 954 is shown on the left and the unloading chamber 956 is shown on the right, those skilled in the art will understand that this is merely one possible configuration.
[0065] The size and shape of the loading chamber 954 and the unloading chamber 956 may vary depending on, for example, the substrate being processed in the clustering tool 900. In the illustrated embodiment, the size of the loading chamber 954 and the unloading chamber 956 is adapted to accommodate a wafer cassette in which a plurality of wafers are located.
[0066] Robot 952 is located within the factory interface 950 and can move between loading chamber 954 and unloading chamber 956. Robot 952 is capable of transferring wafers from cassettes in loading chamber 954 to loading gate chamber 960 via the factory interface 950. Robot 952 is also capable of transferring wafers from loading gate chamber 962 to cassettes in unloading chamber 956 via the factory interface 950. Those skilled in the art will understand that the factory interface 950 may have more than one robot 952. For example, the factory interface 950 may have a first robot that transfers wafers between loading chamber 954 and loading gate chamber 960, and a second robot that transfers wafers between loading gate chamber 962 and unloading chamber 956.
[0067] The clustering tool 900 shown has a first portion 920 and a second portion 930. The first portion 920 is connected to the factory interface 950 through loading gate chambers 960, 962. The first portion 920 includes a first transfer chamber 921 in which at least one robot 925 is located. The robot 925 is also referred to as a robotic wafer transfer mechanism. The first transfer chamber 921 is centrally located relative to the loading gate chambers 960, 962, processing chambers 902, 904, 916, 918 and buffer chambers 922, 924. In some embodiments, the robot 925 is a multi-armed robot capable of independently moving more than one wafer at a time. In one or more embodiments, the first transfer chamber 921 includes more than one robotic wafer transfer mechanism. The robot 925 in the first transfer chamber 921 is configured to move wafers between chambers surrounding the first transfer chamber 921. A single wafer is carried on a wafer transfer tray located at the distal end of the first robotic mechanism.
[0068] After the wafer is processed in the first section 920, it can be transferred through a passage chamber to the second section 930. For example, chambers 922 and 924 can be unidirectional or bidirectional passage chambers. For example, passage chambers 922 and 924 can be used to cryogenically cool the wafer before processing in the second section 930, or to allow the wafer to cool or be post-processed before being transferred back to the first section 920.
[0069] The system controller 990 communicates with the first robot 925, the second robot 935, the first plurality of processing chambers 902, 904, 916, 918, and the second plurality of processing chambers 906, 908, 910, 912, 914. The system controller 990 may be any suitable component capable of controlling the processing chambers and robots. For example, the system controller 990 may be a computer including a central processing unit, memory, suitable circuitry, and storage devices.
[0070] The process can typically be stored as a software routine in the memory of the system controller 990. When the processor executes the software routine, the processing chamber can execute the process of this disclosure. The software routine can also be stored and / or executed by a second processor (not shown), located remotely from the hardware controlled by the processor. Some or all of the methods of this disclosure can also be executed in hardware. Thus, the process can be implemented in software and executed in hardware using a computer system as, for example, an application-specific integrated circuit or other type of hardware implementation, or as a combination of software and hardware. When executed by the processor, the software routine transforms a general-purpose computer into a dedicated computer (controller) that controls the operation of the chamber, thereby executing the process.
[0071] In one or more embodiments, the processing tool 900 includes central transfer stations 921, 931, each including at least one robot 925, 935 configured to move wafers; one or more of a selective via-fill station, a reverse selective deposition station, a self-assembled monolayer (SAM) formation station, a CVD station, and a PVD station connected to the central transfer stations; an optional pre-cleaning station connected to the central transfer stations; and at least one controller connected to one or more of the central transfer stations, selective via-fill station, reverse selective deposition station, self-assembled monolayer (SAM) formation station, CVD station, PVD station, or optional pre-cleaning station. In one or more embodiments, the at least one controller has at least one configuration selected from the following: a configuration for moving wafers between stations using robots; a configuration for selectively filling vias; a configuration for exposing a substrate to planar hydrocarbons and forming a self-assembled monolayer (SAM); a configuration for reverse selective deposition of a barrier layer; a configuration for depositing metal; and a configuration for pre-cleaning wafers.
[0072] In one or more embodiments, the processing tool includes: a pre-cleaning chamber having a substrate support; a selective metal deposition chamber; a barrier metal deposition chamber; a metal deposition chamber; a PVD metal deposition chamber; a CVD metal deposition chamber; optionally, a self-assembled monolayer (SAM) deposition chamber with optional pre-cleaning; optionally, a pad metal deposition chamber; optionally, a plasma chamber; optionally, an etching chamber; a robot configured to enter the pre-cleaning chamber, the selective deposition chamber, the optional self-assembled monolayer (SAM) deposition chamber, the barrier metal deposition chamber, the PVD metal deposition chamber, the optional plasma chamber; and the optional etching chamber, the optional pad metal deposition chamber, etc. The CVD metal deposition chamber and PVD metal deposition chamber; and a controller connected to a pre-cleaning chamber, a selective deposition chamber, an optional self-assembled monolayer (SAM) deposition chamber, a barrier metal deposition chamber, a PVD metal deposition chamber, and an optional plasma chamber; and an optional etching chamber, an optional pad metal deposition chamber, a CVD metal deposition chamber, and a PVD metal deposition chamber, and a robot, wherein the controller has one or more configurations selected from: cleaning a substrate, selectively forming a self-assembled monolayer (SAM), selectively depositing a pad, forming a metal pad as needed, forming a metallized layer, etching the substrate as needed, and removing the self-assembled monolayer (SAM) as needed.
[0073] The terms "one embodiment," "some embodiments," "one or more embodiments," or "an embodiment" used in this specification refer to a specific feature, structure, material, or characteristic described in connection with the embodiment, which is included in at least one embodiment of this disclosure. Therefore, the appearance of phrases such as "in one or more embodiments," "in some embodiments," "in one embodiment," or "in one embodiment" throughout this specification does not necessarily refer to the same embodiment of this disclosure. Furthermore, in one or more embodiments, a particular feature, structure, material, or characteristic may be combined in any suitable manner.
[0074] Although this disclosure has been described with reference to specific embodiments, those skilled in the art should understand that the embodiments are only for illustrating the principles and applications of this disclosure. It will be apparent to those skilled in the art that various modifications and alterations can be made to the methods and apparatus of this disclosure without departing from the spirit and scope of this disclosure. Therefore, this disclosure may include modifications and alterations within the scope of the appended claims and their equivalents. [Simplified Explanation of the Diagram]
[0008] In order to understand the above features of this disclosure in detail, the present disclosure, which has been briefly summarized above, can be described in more detail with reference to the embodiments, some of which are illustrated in the accompanying drawings. However, it should be noted that the drawings only illustrate typical embodiments of this disclosure and should not be considered as limiting its scope, as other equivalent embodiments are permissible.
[0009] Figure 1 illustrates a process flow diagram of a method according to one or more embodiments of the present disclosure;
[0010] Figures 2A to 2G illustrate cross-sectional views of an exemplary substrate during processing according to one or more embodiments of this disclosure; and
[0011] Figure 3 illustrates an exemplary clustering tool according to one or more embodiments of this disclosure. [Biomaterial Storage]
[0076] Domestic storage information (please note in order of storage institution, date, and number): None. International storage information (please note in order of storage country, institution, date, and number): None.
Claims
1. A method for forming a self-assembled monolayer (SAM), comprising the steps of: exposing a substrate having an exposed metal surface and an exposed non-metal surface to a first precursor comprising a phenobarbital or a phenobarbital derivative, and depositing the self-assembled monolayer (SAM) on the exposed metal surface, the SAM being selectively formed on the metal surface relative to the non-metal surface.
2. The method as described in claim 1, wherein the exposed metal surface comprises one or more of copper (Cu), cobalt (Co), ruthenium (Ru), tungsten (W), or molybdenum (Mo).
3. The method as described in claim 2, wherein the exposed metal surface comprises one or more of tungsten (W) or molybdenum (Mo).
4. The method as described in claim 1, wherein the phenobarbital derivative comprises symmetrical substitution.
5. The method as described in claim 1, wherein the phenobarbital derivative comprises two or more substitutions.
6. The method as described in claim 5, wherein the phenobarbital derivative is substituted at carbons 4 and 7.
7. The method as described in claim 5, wherein the phenobarbital derivative is substituted at carbons 5 and 6.
8. The method as described in claim 1, wherein the phenocyanate derivative is substituted with at least one C6-C10 alkyl group.
9. The method as described in claim 1, wherein the phenophylline derivative is substituted with at least one aryl group.
10. A selective deposition method comprising the steps of: exposing a substrate having an exposed metal surface and an exposed non-metal surface to a first precursor comprising a morpholine or a morpholine derivative to form a protected metal surface; and selectively depositing a material on the exposed non-metal surface relative to the protected metal surface.
11. The method as described in claim 10, wherein the material is deposited with a selective deposition ratio greater than 5:
1.
12. A method of forming a semiconductor structure, the method comprising the steps of: selectively forming a self-assembled monolayer (SAM) on a first surface of a substrate by exposing a substrate to a first precursor, the substrate having at least one feature including the first surface and a second surface, the first surface comprising a metallic material, the second surface comprising a dielectric material, and the first precursor comprising cyanoline or a derivative thereof; and selectively depositing a pad on the second surface by exposing the substrate to a second precursor.
13. The method as described in claim 12 further includes the step of cleaning the substrate before depositing the self-assembled monolayer (SAM) to form a first surface that is substantially free of oxides.
14. The method as described in claim 12, wherein the first surface comprises one or more of copper (Cu), cobalt (Co), ruthenium (Ru), tungsten (W), or molybdenum (Mo).
15. The method as described in claim 12 further includes the step of densifying the pad by a PVD process.
16. The method as described in claim 12 further includes the step of removing the self-assembled monolayer (SAM).
17. The method as described in claim 12 further includes the step of depositing an adhesive layer on the substrate after depositing the pad.
18. The method of claim 12 further includes the step of: depositing a conductive material in the at least one feature by exposing the substrate to a third precursor, the third precursor comprising a metal.
19. The method as described in claim 18, wherein the step of depositing the conductive material includes one or more of a bottom-up gap filling and a conformal gap filling.
Citation Information
Patent Citations
Target analyte detection using asymmetrical self-assembled monolayers
US20020121314A1
Enzyme Triggered Redox Altering Chemical Elimination (E-Trace) Immunoassay
US20110033869A1
Schemes for Selective Deposition for Patterning Applications
US20190287807A1
Apparatus and methods for controlled electrochemical surface modification
US20200087810A1
A process for preparing electroactive layer on the gold electrode surface, a biosensor comprising the electrode and use thereof
WO2015183110A1