Coated silicone hydrogel contact lens and method for producing the same
Patent Information
- Application Number
- TW111132859
- Authority / Receiving Office
- TW · TW
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-09-01
- Filing Date
- 2022-08-31
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2042-08-30
AI Technical Summary
Existing methods for producing silicone hydrogel contact lenses are inefficient and environmentally unfriendly due to the use of ophthalmologically incompatible organic solvents, leading to increased production costs and reduced efficiency, and the lenses often have hydrophobic surfaces that adsorb lipids and proteins from the ocular environment.
A method involving a polymerizable composition comprising hydrophilized polysiloxane vinyl cross-linking agents, hydroxyethyl methacrylate, (meth)acrylic acid alkoxyethyl esters, and carboxyl-containing (meth)acryloxy monomers, thermally or actinically cured to form a silicone hydrogel lens precursor, which is then hydrated and coated with a cross-linked hydrophilic polymer, eliminating the need for solvent extraction and surface modification steps.
This method produces optically clear, wettable silicone hydrogel contact lenses with high oxygen permeability and improved surface properties, reducing production costs and environmental impact while enhancing lens compatibility and comfort.
Abstract
Description
Method for producing wettable silicone hydrogel contact lenses This invention relates to a method for producing optically transparent and wettable silicone hydrogel contact lenses in a cost-effective and environmentally friendly manner. This invention also relates to wettable silicone hydrogel contact lenses manufactured according to the method of this invention. In recent years, soft silicone hydrogel contact lenses have become increasingly popular due to their high oxygen permeability and comfort. "Soft" contact lenses conform closely to the shape of the eye, making it difficult for oxygen to bypass the lens. Soft contact lenses must allow oxygen from the surrounding air (i.e., oxygen) to reach the cornea, as the cornea cannot receive oxygen supplied by the blood like other tissues. If insufficient oxygen reaches the cornea, corneal swelling occurs. Prolonged hypoxia causes unwanted blood vessel growth in the cornea. With its high oxygen permeability, silicone hydrogel ("SiHy") contact lenses allow sufficient oxygen to permeate through the lens to the cornea with minimal adverse effects on corneal health. Most commercially available SiHy contact lenses are manufactured using conventional casting molding techniques, which involve the use of a single-use plastic mold and a SiHy lens-forming composition (or SiHy lens formulation) that typically comprises one or more silicone-containing polymerizable components and at least one hydrophilic polymerizable component. However, the silicone-containing polymerizable component and the hydrophilic polymerizable component are not sufficiently miscible (compatible) to form an optically clear lens formulation for manufacturing optically clear SiHy contact lenses. Furthermore, the silicone-containing component is typically insoluble in water or ophthalmologically compatible solvents (as non-reactive diluents). Thus, one or more ophthalmologically incompatible organic solvents must be used in the SiHy lens formulation. Furthermore, some polymerizable components in SiHy lens formulations may not be ophthalmologically compatible. Unreacted and partially reacted polymerizable components remaining in the resulting SiHy contact lenses formed from SiHy lens formulations need to be removed in extraction methods involving one or more ophthalmologically incompatible organic solvents. This lens extraction increases production costs and reduces production efficiency. Due to the use of one or more ophthalmologically incompatible organic solvents in the SiHy lens formulation and in the extraction process, solvent exchange or hydration processes have been performed during production. These processes increase production costs and reduce production efficiency. The use of ophthalmologically incompatible organic solvents in the production of SiHy contact lenses can be expensive and not environmentally friendly. Ideally, the methods used to manufacture SiHy contact lenses should not involve the use of any ophthalmologically incompatible organic solvents. Furthermore, SiHy materials typically possess surfaces, or at least some areas of those surfaces, that are hydrophobic (non-wetting) and readily adsorb lipids or proteins from the ocular environment and can adhere to the eye. Therefore, SiHy contact lenses generally require surface modification. Recently, U.S. Patent Nos. 8,529,057 and 10,449,740 have described novel, cost-effective methods for applying non-silicone hydrogel coatings to SiHy contact lenses, comprising the steps of forming a base coating on the SiHy contact lens, rinsing the SiHy contact lens with the base coating using a solvent (e.g., water, a mixture of water and organic solvents, and / or buffered saline), and directly covalently attaching a partially crosslinked hydrophilic polymer material to the base coating in the lens packaging during autoclaving. The base coating formation and rinsing steps may not be environmentally friendly and / or may increase production costs and reduce production efficiency. Therefore, there is still a need for a cost-effective and environmentally friendly method for producing SiHy contact lenses, especially wettable SiHy contact lenses. In one aspect, the present invention provides a method for producing coated silicone hydrogel contact lenses, comprising the steps of: (1) introducing a polymerizable composition into a lens mold, wherein the polymerizable composition comprises (a) at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) hydroxyethyl methacrylate as desired, and (c) at least one (meth)acrylate C 1-C 2. Alkoxyethyl ester, (d) at least one carboxyl-containing (meth)acryloxy monomer, from about 2% to about 10% by weight relative to the total amount of all polymerizable components, (e) at least one free radical, and (f) at least one solvent selected from the group consisting of water, propylene glycol, polyethylene glycol having a molecular weight of about 400 Daltons or less, and combinations thereof, as needed; (2) thermosetting or photocuring the polymerizable composition in the lens mold to form a silicone hydrogel lens precursor comprising a bulk silicone hydrogel material containing carboxyl groups; (3) hydrating the silicone hydrogel lens precursor obtained in step (2) in water or an aqueous solution, as needed, to obtain a hydrated silicone hydrogel contact lens; and (4) mixing the silicone hydrogel lens precursor obtained in step (2) or step (3) with water. The hydrated silicone hydrogel contact lens obtained therein is heated directly in an aqueous solution having a pH of about 6.5 to about 9.5 and comprising at least one water-soluble, thermally crosslinkable hydrophilic polymer material at a temperature of about 60°C to about 140°C to form a coated silicone hydrogel contact lens. The coated silicone hydrogel contact lens comprises the bulk silicone hydrogel material and a layer of crosslinked hydrophilic polymer material covalently attached to the bulk silicone hydrogel material. The coated silicone hydrogel contact lens exhibits a water breakup time (WBUT) of at least about 5 seconds and an oxygen permeability of at least about 50 bar. On another front, the present invention provides a silicone hydrogel contact lens comprising a bulk silicone hydrogel material and a layer thereon of a non-silicone hydrogel material (i.e., a cross-linked hydrophilic polymer material), wherein the bulk silicone hydrogel material comprises (a) repeating units of at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) repeating units of hydroxyethyl methacrylate as desired, and (c) at least one (meth)acrylate C 1-C (d) A repeating unit of 2-alkoxyethyl ester, and at least one carboxyl-containing repeating unit of a (meth)acryloxy monomer, wherein the layer of the non-silicone hydrogel material is covalently attached to the bulk silicone hydrogel material by the carboxyl group of the repeating unit, wherein the silicone hydrogel contact lens has a water breakup time (WBUT) of at least about 5 seconds, an oxygen permeability of at least about 50 bar, and an elastic modulus from 0.2 MPa to 1.8 MPa. Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. Generally, the nomenclature and laboratory procedures used herein are those well-known and commonly used in the art. Conventional methods are applied to these procedures, as those provided in the art and in various general references. When a term is provided in the singular, the inventors have also considered the plural form of that term. The nomenclature used herein and the laboratory procedures described below are those well-known and commonly used in the art. In this application, as used herein, “about” means a number referred to as “about” that comprises the stated number plus or minus 1% to 10% of that stated number. "Contact lenses" refer to structures that can be placed on or inside the wearer's eye. Contact lenses can correct, improve, or alter a user's vision, but are not required to do so. "Hydrogel contact lenses" refers to contact lenses that contain a hydrogel core material. The hydrogel core material can be a non-silicone hydrogel material or preferably a silicone hydrogel material. "Hydrogel" or "hydrogel material" refers to a cross-linked polymer material having a three-dimensional polymer network (i.e., polymer matrix) that is insoluble in water but can retain at least 10% by weight of water in its polymer matrix when fully hydrated (or in equilibrium). "Silicone hydrogel" or "SiHy" refers to a silicone-containing hydrogel obtained by copolymerization of a polymerizable composition, which includes at least one silicone-containing monomer, at least one silicone-containing macromonomer, or at least one crosslinkable silicone-containing prepolymer. Silicon oxanes, also commonly described as silicones, refer to molecules having at least one -Si-O-Si- moiety, where each Si atom carries two organic groups as substituents. As used in this application, the terms "non-silicone hydrogel" or "non-silicone hydrogel material" can be used interchangeably to refer to a hydrogel that is theoretically free of silicon. As used in this article, "hydrophilic" describes a material or part thereof that will associate with water more easily than lipids. The term "room temperature" refers to a temperature of approximately 17°C to approximately 26°C. The term "soluble" in relation to compounds or materials in solvents means that the compound or material is soluble in a solvent at room temperature (i.e., at a temperature of about 17°C to about 26°C) to obtain a solution having a concentration of at least about 0.5% by weight. The term "insoluble" in relation to compounds or materials in solvents means that the compound or material is soluble in the solvent at room temperature (as defined above) to obtain a solution with a concentration of less than 0.01% by weight. "Ethylene monomers" refer to compounds that have a unique olefinic unsaturated group, are soluble in solvents, and can be photopolymerized or thermally polymerized. The terms "olefinic unsaturated group" or "olefinic bond unsaturated group" are used in a broad sense herein and are intended to include groups containing at least one >C=CH group. 2. Any group of the group. Exemplary olefinic unsaturated groups include, but are not limited to, (methyl)propenyl ( and / or ), allyl, vinyl, styrene, or other compounds containing C=CH 2 groups. "Acrylic monomers" refers to ethylene monomers having a single (meth)acryloxy group. Examples of acrylic monomers include (meth)acryloxy ((meth)acryloyloxy) monomers and (meth)acrylamine monomers. "(meth)acryloxy or (meth)acryloyloxy) monomer" refers to a monomer with a unique or Ethylene monomers with groups. "(meth)acrylamide monomer" refers to monomers containing... or An ethylene monomer with a single unique group, wherein R o H or C 1-C 4-alkyl group. The term "(meth)acrylamide" refers to methacrylamide and / or acrylamide. The term "(meth)acrylate" refers to methacrylates and / or acrylates. "N-vinyl amide monomer" refers to a vinyl group with a nitrogen atom directly attached to the amide group. Acetamine compounds. "Ene monomer" refers to ethylene monomers that have a unique alkenyl group. As used herein, "hydrophilic vinyl monomer," "hydrophilic acrylic monomer," "hydrophilic (meth)acryloxy monomer," or "hydrophilic (meth)acrylamine monomer" refers to vinyl monomers, acrylic monomers, (meth)acryloxy monomers, or (meth)acrylamine monomers that typically produce homopolymers that are water-soluble or capable of absorbing at least 10 percent by weight of water. As used herein, "hydrophobic vinyl monomer," "hydrophobic acrylic monomer," "hydrophobic (meth)acryloxy monomer," or "hydrophobic (meth)acrylamine monomer" refers to vinyl monomers, acrylic monomers, (meth)acryloxy monomers, or (meth)acrylamine monomers that typically produce homopolymers that are insoluble in water or capable of absorbing less than 10% by weight of water. As used in this application, the term "ethylene-based crosslinking agent" refers to an organic compound having at least two olefinically unsaturated groups. "Ethylene-based crosslinking agent" also refers to an ethylene-based crosslinking agent having a molecular weight of 700 Daltons or less. "Acrylic crosslinking agents" refers to ethylene crosslinking agents having at least two (meth)acrylic groups. The term "acrylic repeating unit" refers to repeating units of such polymer materials, each derived from acrylic monomers or crosslinking agents that form the polymer material by free radical polymerization. The term "terminal (meth)acryl" refers to a (meth)acryl group located at one of the two ends of the main chain (or backbone) of an organic compound, as is known to those skilled in the art. As used herein, "photochemical" in relation to the curing, crosslinking, or polymerization of polymerizable components, prepolymers, or materials means curing (e.g., crosslinking and / or polymerization) by photochemical irradiation, such as UV / visible light irradiation, ionizing radiation (e.g., gamma-ray or X-ray irradiation), microwave irradiation, etc. Thermochemical or photochemical curing methods are well known to those skilled in the art. As used in this application, the term "polymer" means a material formed by polymerizing / crosslinking one or more monomers or macromonomers or prepolymers or combinations thereof. "Macromonomer" or "prepolymer" refers to a compound or polymer that contains olefinic unsaturated groups and has a number average molecular weight of more than 700 Daltons. As used in this application, the term "molecular weight" for polymeric materials (including monomeric materials or macromonomeric materials) refers to the unit average molecular weight, unless otherwise specified or unless the test conditions specify otherwise. Those skilled in the art know how to determine the molecular weight of a polymer using known methods, such as GPC (gel permeation chromatography) having one or more of the following: a refractive index detector, a small-angle laser light scattering detector, a multi-angle laser light scattering detector, a differential viscometry detector, a UV detector, and an infrared (IR) detector; or MALDI-TOF MS (matrix-assisted desorption / ionization time-of-flight mass spectrometry). 1 1H NMR (proton nuclear magnetic resonance) spectroscopy, etc. "Polysiloxane segment" or "polydiorganosiloxane segment" can be used interchangeably to refer to polymer chain segments. (i.e., divalent groups), where SN is an integer of 3 or greater and R S1 and R S2 Each of the following groups is selected independently: C 1-C 10 Alkyl; Phenyl; C 1-C 4-alkyl-substituted phenyl; C 1-C 4-Alkoxy-substituted phenyl; phenyl-C 1-C 6-alkyl; C 1-C 10 fluoroalkyl; C 1-C 10 Fluoroethers; aryl; aryl C 1-C 18 Alkyl; -alk-(OC) 2H 4) γ1 -OR o (where alk series C) 1-C 6-alkyldiyl, R o H or C 1-C 4 alkyl groups and γ1 series integers from 1 to 10); C 2-C 40 An organic group having at least one selected from a hydroxyl group (-OH), a carboxyl group (-COOH), or an amino group (-NR). N1 R N1 '), Amino linker -NR N1 - amide linker - CONR N1 -, Acetamide-CONR N1 R N1 ', urethane linker -OCONH- and C 1-C Functional groups of the group consisting of 4 alkoxy groups, or straight-chain hydrophilic polymer chains, wherein R N1 and R N1 'Independently hydrogen or C 1-C 15 alkyl. "Polysiloxane vinyl monomers" refer to compounds that contain at least one polysiloxane segment and a unique olefinic unsaturated group. "Polydiorganosiloxane ethylene crosslinking agent" or "polysiloxane ethylene crosslinking agent" can be used interchangeably to refer to a compound containing at least one polysiloxane segment and at least two olefinic unsaturated groups. "Linear polydiorganosiloxane ethylene crosslinking agent" or "linear polysiloxane ethylene crosslinking agent" can interchangeably refer to a compound comprising a main chain containing at least one polysiloxane segment and being capped at each of the two ends of the main chain by an olefinic unsaturated group. "Extended chain polydiorganosiloxane ethylene crosslinking agent" or "extended chain polysiloxane ethylene crosslinking agent" interchangeably refers to a compound comprising at least two olefinic unsaturated groups and at least two polysiloxane segments, each pair of polysiloxane segments being linked by a divalent group. As used in this article, the term "fluid" indicates that a material can flow like a liquid. As used in this application, the term "optically transparent" in relation to a polymerizable composition means that the polymerizable composition is a transparent solution or liquid mixture (i.e., having 85% or more, preferably 90% or more, of light transmittance in the range of 400 to 700 nm). The term "monovalent group" refers to an organic group obtained by removing a hydrogen atom from an organic compound and forming a bond with another group in the organic compound. Examples include, but are not limited to, alkyl (by removing a hydrogen atom from an alkane), alkoxy (by removing a hydrogen atom from the hydroxyl group of an alkyl alcohol), thiyl (by removing a hydrogen atom from the mercapto group of an alkyl thiol), cycloalkyl (by removing a hydrogen atom from a cycloalkanes), heteroalkyl (by removing a hydrogen atom from a cycloalkanes), aryl (by removing a hydrogen atom from the aromatic ring of an aromatic hydrocarbon), heteroaryl (by removing a hydrogen atom from any ring atom), and amino (by removing a hydrogen atom from an amine). The term "divalent group" refers to an organic group obtained by removing two hydrogen atoms from an organic compound and forming two bonds with two other groups in the organic compound. For example, the alkylene (alkylenyl) divalent group is obtained by removing two hydrogen atoms from an alkane, and the cycloalkylene (cycloalkylenyl) divalent group is obtained by removing two hydrogen atoms from a ring. In this application, the term "substituted" in relation to alkyl or alkylene groups means that the alkyl or alkylene group includes at least one substituent that replaces one hydrogen atom of the alkyl or alkylene group and is selected from the group consisting of: hydroxyl (-OH), carboxyl (-COOH), -NH 2. Thiol group (-SH), C 1-C 4-alkyl, C 1-C 4-alkoxy group, C 1-C 4-alkylthio (alkyl sulfide), C 1-C 4-amino acid, C 1-C 4-alkylamine, di-C 1-C 4. Alkylamine groups and combinations thereof. In this application, the term "polyazoline" refers to The polymer or polymer segment, wherein: R 1 It is hydrogen, methyl, ethyl, N-pyrrolidylmethyl, N-pyrrolidylethyl, N-pyrrolidylpropyl, or -alk-(OC) 2H 4) m3 -OR ” Monovalent groups, of which alk-based C 1-C 4-alkyldiyl; R'' series C 1-C 4-alkyl (preferably methyl); m3 series of integers from 1 to 10 (preferably 1 to 5); x series of integers from 5 to 500. In this application, the term "poly(2-acezoline-co-ethyleneimine)" refers to a poly(2-acezoline-co-ethyleneimine) having the following formula: , wherein: R 1 It is hydrogen, methyl, ethyl, N-pyrrolidylmethyl, N-pyrrolidylethyl, N-pyrrolidylpropyl, or -alk-(OC) 2H 4) m3 -OR ” Monovalent groups, of which alk-based C 1-C 4-alkyldiyl; R'' series C 1-C 4-alkyl (preferably methyl); m3 refers to integers from 1 to 10 (preferably 1 to 5); x refers to integers from 5 to 500; z refers to integers equal to or less than x. Poly(2-acezoline-co-ethyleneimine) is obtained by hydrolyzing polyacezoline. In this application, the term "poly(2-acezoline-co-ethyleneimine)-epimyl chloride" refers to a polymer obtained by reacting poly(2-acezoline-co-ethyleneimine) with epichlorohydrin to convert all or a large percentage (≥ 90%) of the secondary amine groups of poly(2-acezoline-co-ethyleneimine) into azahexacyclobutaneon groups. Examples of poly(2-acezoline-co-ethyleneimine)-epimyl chloride are disclosed in co-pending U.S. Patent Application No. 2016 / 0061995 A1. "Epichlorohydrin-functionalized polyamine" or "epichlorohydrin-functionalized polyamide" refers to a polymer obtained by reacting a polyamine or polyamide with epichlorohydrin to convert all or a large percentage of the secondary amine groups of the polyamine or polyamide into aza-butaneonium groups. The term "polyaminoamine-epimylchlorohydrin" refers to epichlorohydrin-functionalized adipic acid-diethyltriamine copolymer. In this application, the terms "aza-butanetonium" or "3-hydroxyaza-butanetonium" refer to... A positively charged (i.e., cation) divalent group (or group or part). The term "thermally crosslinkable" for polymeric materials or functional groups means that the polymeric material or functional group can undergo a crosslinking (or coupling) reaction with another material or functional group at a relatively elevated temperature (from about 40°C to about 140°C), but the polymeric material or functional group cannot undergo the same crosslinking (or coupling) reaction with another material or functional group to a detectable degree at a temperature from about 5°C to about 15°C for a period of about one hour. As used in this application, the term "phosphatidylcholine" refers to a zwitterionic group. , where n is an integer from 1 to 5, and R 1. R 2 and R 3 are C, which are independent of each other. 1-C 8-alkyl or C 1-C 8-hydroxyalkyl. As used in this application, the term "reactive vinyl monomer" means any vinyl monomer having at least one reactive functional group selected from the group consisting of: carboxyl, primary amine, and secondary amine. As used in this application, the term "non-reactive ethylene monomer" means any ethylene monomer (hydrophilic or hydrophobic ethylene monomer) that does not contain a carboxyl group, a primary amine group, a secondary amine group, an epoxide group, an isocyanate group, an acrylonitrile group, or an azacyclopropane group. Free radical initiators can be photoinitiators or thermal initiators. "Photoinitiators" refer to chemicals that initiate free radical cross-linking / polymerization reactions using light. "Thermal initiators" refer to chemicals that initiate free radical cross-linking / polymerization reactions using heat energy. As used in this application, the term "bulk silicone hydrogel material" in relation to contact lenses can be used interchangeably to mean a layer of silicone hydrogel material that substantially has the three-dimensional shape of a contact lens. The inherent oxygen permeability of the material (Dk) i Oxygen permeability is the rate at which oxygen passes through a material. It is conventionally expressed in baler, where a baler is defined as [(cm²)]. 3 Oxygen (mm) / (cm) 2 (sec)(mm Hg)] x 10 -10 . The "oxygen permeability" Dk / t of an insert or material is the rate at which oxygen will pass through a specific insert or material with an average thickness of t [in mm] over the measured area. Oxygen permeability is conventionally expressed in bulges / mm, where "bulges / mm" is defined as [(cm...]]. 3 Oxygen) / (cm) 2 (s)(mm Hg)] x 10 -9 . The "ion permeability" of a lens is related to its ion flux diffusion coefficient. The ion flux diffusion coefficient D (in mm²) is... 2The unit [ / min] is determined by applying Fick's law as follows: D = -n' / (A x dc / dx) where n' = ion transport rate [mol / min]; A = exposed lens area [mm²]. 2 ]; dc = concentration difference [mol / L]; dx = lens thickness [mm]. The term "modulus" or "elastic modulus" in relation to contact lenses or materials refers to the tensile modulus or Young's modulus as a measure of the stiffness of the contact lens or material. The modulus can be measured according to the procedure described in Example 1. The term "dry lens pre-constituted" refers to a cast-molded contact lens that is obtained by casting polymerizable components in a mold and has not been subjected to extraction and / or hydration (i.e., has not been in contact with water or any organic solvent or any liquid after molding). The term "wettable silicone hydrogel contact lens" means that the silicone hydrogel contact lens has a water breakup time ("WBUT") of at least about 5 seconds, preferably at least about 10 seconds, more preferably at least about 15 seconds, and even more preferably at least about 20 seconds. The water breakup time ("WBUT") can be measured according to the procedure described in Example 1. The term "optically transparent silicone hydrogel contact lens" means that the silicone hydrogel contact lens has a light transmittance of at least 85%, preferably at least 90%, more preferably at least 93%, and even more preferably at least 95% in the range of 400 to 700 nm. The light transmittance of the contact lens in the range of 400 to 700 nm can be measured according to the procedure described in Example 1. The "average water contact angle" refers to the water contact angle obtained by averaging the measurements of at least three individual samples of contact lenses or silicone hydrogel materials (measured using the sessile drop method). In general, this invention relates to a method for producing optically clear and wettable silicone hydrogel contact lenses in a cost-effective and environmentally friendly manner. The invention is based in part on the discovery that selected polymerizable components, such as hydroxyethyl methacrylate, alkoxyethyl methacrylate (e.g., ethoxyethyl methacrylate or methoxyethyl methacrylate), carboxyl-containing (meth)acryloxy monomers (e.g., acrylic acid or methacrylic acid), and hydrophilic polysiloxane-ethylene crosslinking agents, can be formulated in ophthalmologically compatible organic solvents (e.g., propylene glycol) to form lens formulations capable of producing optically clear silicone hydrogel contact lenses with relatively high oxygen permeability (at least 50 lbs). The invention is also based in part on the discovery that cast-molded silicone hydrogel contact lenses do not require extraction and hydration processes and can be directly surface-modified in the packaging solution within the lens packaging during autoclaving. This invention offers the following advantages. First, ophthalmologically incompatible organic solvents are not used in the method of this invention. By eliminating ophthalmologically incompatible organic solvents, the extraction and hydration steps after molding can be eliminated. This greatly simplifies production, significantly reduces production costs, and the production process is environmentally friendly. Second, the step of forming a base coating on the silicone hydrogel contact lens is eliminated. This eliminates the production costs associated with the base coating and rinsing steps. In one aspect, the present invention provides a method for producing coated silicone hydrogel contact lenses, comprising the steps of: (1) introducing a polymerizable composition into a lens mold, wherein the polymerizable composition comprises (a) at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) hydroxyethyl methacrylate as desired, and (c) at least one (meth)acrylate C 1-C 2. Alkoxyethyl ester, (d) at least one carboxyl-containing (meth)acryloxy monomer, from about 2% to about 10% by weight relative to the total amount of all polymerizable components, (e) at least one free radical, and (f) at least one solvent selected from the group consisting of water, propylene glycol, polyethylene glycol having a molecular weight of about 400 Daltons or less, and combinations thereof, as needed; (2) thermosetting or photocuring the polymerizable composition in the lens mold to form a silicone hydrogel lens precursor comprising a bulk silicone hydrogel material containing carboxyl groups; (3) hydrating the silicone hydrogel lens precursor obtained in step (2) in water or an aqueous solution, as needed, to obtain a hydrated silicone hydrogel contact lens; and (4) mixing the silicone hydrogel lens precursor obtained in step (2) or step (3) with water. The hydrated silicone hydrogel contact lens obtained therein is heated directly in an aqueous solution having a pH of about 6.5 to about 9.5 and comprising at least one water-soluble, thermally crosslinkable hydrophilic polymer material at a temperature of about 60°C to about 140°C to form a coated silicone hydrogel contact lens comprising the bulk silicone hydrogel material and a layer of crosslinked hydrophilic polymer material covalently attached to the bulk silicone hydrogel material, wherein the coated silicone hydrogel contact lens exhibits a water breakup time (WBUT) of at least about 5 seconds (preferably at least about 10 seconds, more preferably at least about 15 seconds, and even more preferably at least about 20 seconds) and an oxygen permeability of at least about 50 bar (preferably at least about 60 bar, more preferably at least about 70 bar, and even more preferably at least about 80 bar). According to a preferred embodiment of the invention, the sum of the amounts of components (a) to (e) is at least about 90% by weight relative to the total amount of all polymerizable components in the polymerizable composition, preferably at least about 92% by weight, more preferably at least about 94% by weight, and even more preferably at least about 96% by weight. According to any of the foregoing embodiments of the present invention, the polymerizable composition comprises hydroxyethyl methacrylate. According to any of the foregoing embodiments of the present invention, the polymerizable composition comprises at least one solvent selected from the group consisting of water, propylene glycol, polyethylene glycol having a molecular weight of about 400 Daltons or less, and combinations thereof. According to the present invention, any hydrophilic polysiloxane ethylene crosslinking agent can be used in the present invention, provided that it contains at least about 1.50 (preferably at least about 2.0, more preferably at least about 2.5, and even more preferably at least about 3.0) milliequivalents per gram ("meq / g") of hydrophilic moiety, preferably hydroxyl (-OH), carboxyl (-COOH), or amino (-NHR) groups. N1, where R N1 H or C 1-C 2-alkyl), amide moiety (-CO-NR) N1 R N2 , where R N1 H or C 1-C 2 alkyl and R N2 It is a covalent bond, H, or C 1-C 2-alkyl), NC 1-C 3. Acrylamino group, urethane moiety (-NH-CO-O-), urea moiety (-NH-CO-NH-) polyethylene glycol chains (where n is an integer from 2 to 20 and T) 1-H, methyl or acetyl or phosphocholine), or combinations thereof. In any of the foregoing embodiments, the at least one hydrophilic polysiloxane ethylene crosslinking agent comprises a polysiloxane ethylene crosslinking agent comprising (1) a dimethylsiloxane unit and each having a methyl substituent and a monovalent C having 2 to 6 hydroxyl groups. 4-C 40 The polysiloxane segment of the hydrophilic silicone unit with organic substituents, and (2) two terminal (meth)acrylic groups. More preferably, the at least one hydrophilic polysiloxane vinyl crosslinker comprises a polysiloxane vinyl crosslinker of formula (1). Wherein: υ1 is an integer from 30 to 500 and ω1 is an integer from 1 to 75, provided that ω1 / υ1 is from about 0.035 to about 0.15 (preferably from about 0.040 to about 0.12, and even more preferably from about 0.045 to about 0.10); X 01 System O or NR n , where R n Hydrogen or C 1-C 10 -alkyl; R o It is a hydrogen or methyl group; R 2 and R 3. C that are either substituted or unsubstituted, independent of each other. 1-C 10 alkyl divalent groups or -R 5-OR 6-divalent group, wherein R 5 and R 6. C that are either substituted or unsubstituted, independent of each other. 1-C 10 alkyl divalent group; R Monovalent groups of any one of the four formulas (2) to (7) p1 represents zero or 1; m1 represents integers from 2 to 4; m2 represents integers from 1 to 5; m3 represents integers from 3 to 6; m4 represents integers from 2 to 5; R 7-series hydrogen or methyl; R The 8-series C has a oxidation state of (m² + 1). 2-C 6 hydrocarbon group; R The 9-series C has a oxidation state of (m⁴ + 1). 2-C 6 hydrocarbon group; R 10 It is ethyl or hydroxymethyl; R 11 It is either methyl or hydroxymethyl; R 12 Hydroxyl or methoxy group; X 3-series -S-sulfide bonds or -NR 13 - a tertiary amino bond, where R 13 C 1-C 1. Alkyl, hydroxyethyl, hydroxypropyl, or 2,3-dihydroxypropyl; X 4 series or The amide bond, in which R 14 Hydrogen or C 1-C 10 Alkyl; L PC Tie , , , , ,or divalent groups, where q1 is an integer from 1 to 20, R 15 Straight or branched C 1-C 10 alkyl divalent group, R 16 Straight or branched C 3-C 10 alkyl divalent groups, and R 17 C is a direct bond, a straight chain, or a branch. 1-C 4. Alkyl divalent group. In any of the foregoing embodiments, R A monovalent group of one of the four series formulas (2a) to (2y). Where p1 is zero or 1 (preferably 1), m1 is an integer from 2 to 4 (preferably 3), and R 7-series hydrogen or methyl (preferably hydrogen). In any of the foregoing embodiments, R may alternatively... A monovalent group of one of the four series formulas (3a) to (3y). , where X 4 series or The amide bond, in which R 14 Hydrogen or C 1-C 10 alkyl. In any of the foregoing embodiments, R may alternatively... Monovalent groups of the 4-series formula (4a) or (4b). In any of the foregoing embodiments, R may alternatively... A monovalent group of one of the four series formulas (5a) to (5c). In any of the foregoing embodiments, alternatively, the monovalent group R The groups of the 4-series formula (6), wherein m1 is 3, p1 is 1, and R 7-series hydrogen. This preferred first polysiloxane-ethylene crosslinking agent is represented by formula (A). The terms υ1 and ω1 are as defined above. In any of the foregoing embodiments, R may alternatively... Monovalent groups of the 4-series formula (7a) . The procedure for preparing polysiloxane ethylene crosslinking agents of formula (1) has been described in detail in U.S. Patent No. 10,081,697 and U.S. Patent Application Serial No. 63 / 147624, filed February 9, 2021. According to the present invention, any carboxyl-containing (meth)acryloxy monomer can be used in the present invention. Examples of carboxyl-containing (meth)acryloxy monomers include, but are not limited to, acrylic acid, methacrylic acid, ethyl acrylic acid, propyl acrylic acid, (meth)acryloxyacetic acid, mono-2-[(meth)acryloxy]ethyl succinate, (meth)acryloxypropionic acid, and (meth)acryloxybutyric acid. According to the present invention, the free radical initiator can be a photoinitiator or a thermal initiator. "Photoinitiator" refers to a chemical that initiates a free radical crosslinking / polymerization reaction using light. "Thermal initiator" refers to a chemical that initiates a free radical crosslinking / polymerization reaction using heat energy. Any thermal polymerization initiator can be used in this invention. Suitable thermal polymerization initiators are known to those skilled in the art and include, for example, peroxides, hydroperoxides, azobis(alkyl- or cycloalkylnitrile), persulfates, percarbonates, or mixtures thereof. Examples of preferred thermal polymerization initiators include, but are not limited to, benzoyl peroxide, tert-butyl peroxide, tert-amyl peroxybenzoate, 2,2-bis(tert-butylperoxy)butane, 1,1-bis(tert-butylperoxy)cyclohexane, 2,5-bis(tert-butylperoxy)-2,5-dimethylhexane, 2,5-bis(tert-butylperoxy)-2,5-dimethyl-3-hexyne, bis(1-(tert-butylperoxy)-1-methyl 1,1-Bis(tert-butylperoxy)-3,3,5-trimethylcyclohexane, di-tert-butyl-disperoxyphthalate, tert-butyl hydroperoxide, tert-butyl peracetate, tert-butyl peroxybenzoate, tert-butyl peroxyisopropyl carbonate, acetyl peroxide, lauryl peroxide, decyl peroxide, dicetyl peroxydicarbonate, di(4-tert-butylcyclohexyl)peroxydicarbonate (Perkadox) 16) Di(2-ethylhexyl)peroxydicarbonate, tert-butyl peroxyneoplate (Lupersol 11); tert-butyl peroxy-2-ethylhexanoate (Trigonox 21-C50), 2,4-pentanedione peroxide, diisopropylphenyl peroxide, peracetic acid, potassium persulfate, sodium persulfate, ammonium persulfate, 2,2′-azobis(4-methoxy-2,4-dimethylpentanonitrile) (VAZO 33), 2,2′-azobis[2-(2-imidazolin-2-yl)propane] dihydrochloride (VAZO 44), 2,2′-azobis(2-amidinylpropane) dihydrochloride (VAZO 50), 2,2′-azobis(2,4-dimethylpentanonitrile) (VAZO 52), 2,2′-azobis(isobutyronitrile) (VAZO 64 or AIBN), 2,2′-azobis-2-methylbutyronitrile (VAZO 67), 1,1-azobis(1-cyclohexanecarboxylonitrile) (VAZO 88); 2,2′-azobis(2-cyclopropylpropionitrile), 2,2′-azobis(methyl isobutyrate), 4,4′-azobis(4-cyanopentanoic acid), and combinations thereof. Preferably, the thermal initiator is 2,2′-azobis(isobutyronitrile) (AIBN or VAZO 64). Suitable photoinitiators include benzoyl ether, diethoxyacetophenone, benzoylphosphine oxide, 1-hydroxycyclohexylphenyl ketone, and Darocur and Irgacur types, preferably Darocur 1173® and Darocur 2959®, germanium-based Norrish type I photoinitiators (e.g., those described in US 7,605,190). Examples of benzoylphosphine initiators include 2,4,6-trimethylbenzoyldiphenylphosphine oxide; bis-(2,6-dichlorobenzoyl)-4-N-propenylphosphine oxide; and bis-(2,6-dichlorobenzoyl)-4-N-butanylphosphine oxide. Reactive photoinitiators, for example, that can be incorporated into macromonomers or used as specific monomers, are also suitable. Examples of reactive photoinitiators are those disclosed in EP 632 329. According to any of the foregoing embodiments of the invention, the polymerizable composition may further comprise one or more additional polymerizable components (in addition to components (a) to (e) known to those skilled in the art), provided that the sum of the amounts of those additional polymerizable components is about 10% or less by weight relative to the total amount of all polymerizable components in the polymerizable composition, preferably about 8% or less by weight, more preferably about 6% or less by weight, and even more preferably about 4% or less by weight. According to any of the foregoing embodiments of the present invention, the polymerizable composition may further comprise a non-silicone vinyl crosslinking agent, preferably selected from the group consisting of: ethylene glycol di-(meth)acrylate, diethylene glycol di-(meth)acrylate, triethylene glycol di-(meth)acrylate, tetraethylene glycol di-(meth)acrylate, polyethylene glycol di-(meth)acrylate having a number average molecular weight of 200 to 10,000 Daltons, glycerol di-(meth)acrylate, 1,3-propanediol di-(meth)acrylate, and 1,3-butanediol di-(meth)propylene. Ester, 1,4-butanediol di-(meth)acrylate, glycerol 1,3-diglyceride di-(meth)acrylate, ethyl bis[oxy(2-hydroxypropane-1,3-diyl)] di-(meth)acrylate, bis[2-(meth)propenyloxyethyl] phosphate, trimethylolpropane di-(meth)acrylate, and 3,4-bis[(meth)propenyl]tetrahydrofuran, diacrylamide (i.e., N-(1-sideoxy-2-propenyl)-2-propenylamine), dimethylacrylamide (i.e., N-(1-sideoxy-2-methyl-2-propenyl)-2-propenylamine), dimethylacrylamide (i.e., N-(1-sideoxy-2-methyl-2-propenyl)-2-propenylamine) N,N-di(methyl)propenyl-N-methylamine, N,N-di(methyl)propenyl-N-ethylamine, N,N'-methylenebis(methyl)propenylamine, N,N'-extrinylbis(methyl)propenylamine, N,N'-dihydroxyextrinylbis(methyl)propenylamine, N,N'-extrinylpropylbis(methyl)propenylamine, N,N'-2-hydroxyextrinylpropylbis(methyl)propenylamine, N,N'-2,3-dihydroxyextrinylbutylbis(methyl)propenylamine, 1,3-bis(methyl)propenylamine-propane-2-yl dihydrophosphate (i.e., N,N'-2-phosphatidylinosylpropyl bis(meth)acrylamide), piperazine diacrylamide (or 1,4-bis(meth)acrylpiperamide), triallyl isocyanurate, triallyl cyanurate, and combinations thereof, preferably selected from the group consisting of: ethylene glycol di-(meth)acrylate, diethylene glycol di-(meth)acrylate, triethylene glycol di-(meth)acrylate, tetraethylene glycol di-(meth)acrylate, polyethylene glycol di-(meth)acrylate having a number average molecular weight of 200 to 10,000 Daltons, and combinations thereof. According to any of the foregoing embodiments of the present invention, the polymerizable composition may further comprise other polymerizable materials as known to those skilled in the art, such as UV-absorbing vinyl monomers, polymerizable UV / high-energy ultraviolet ("HEVL") absorbing compounds (including UV / HEVL absorbing vinyl monomers described below, and / or polymerizable Cu(II)-porphyrins described in U.S. Patent Application Publication No. 20150316688), polymerizable photochromic compounds, polymerizable colorants (polymerizable dyes), or combinations thereof. Any suitable UV-absorbing vinyl monomer and UV / HEVL-absorbing vinyl monomer can be used in the polymerizable composition used to prepare the preformed SiHy contact lens of the present invention. Examples of preferred UV-absorbing vinyl monomers and UV / HEVL-absorbing vinyl monomers include, but are not limited to: 2-(2-hydroxy-5-vinylphenyl)-2H-benzotriazole, 2-(2-hydroxy-5-propenyloxyphenyl)-2H-benzotriazole, 2-(2-hydroxy-3-methylpropenylaminomethyl-5-tri-octylphenyl)benzotriazole, 2-(2'-hydroxy-5'-methylpropenylaminophenyl)-5-chlorobenzotriazole, 2-(2'-hydroxy-5'-methylpropenylaminophenyl)-5-methoxybenzotriazole 2-(2'-hydroxy-5'-methacryloxypropyl-3'-tert-butyl-phenyl)-5-chlorobenzotriazole, 2-(2'-hydroxy-5'-methacryloxypropylphenyl)benzotriazole, 2-hydroxy-5-methoxy-3-(5-(trifluoromethyl)-2H-benzo[d][1,2,3]triazol-2-yl)benzyl methacrylate (WL-1), 2-hydroxy-5-methoxy-3-(5-methoxy-2H-benzo[d][1,2,3]triazol-2-yl)benzyl methacrylate (WL-5) ), 3-(5-fluoro-2H-benzo[d][1,2,3]triazol-2-yl)-2-hydroxy-5-methoxybenzyl methacrylate (WL-2), 3-(2H-benzo[d][1,2,3]triazol-2-yl)-2-hydroxy-5-methoxybenzyl methacrylate (WL-3), 3-(5-chloro-2H-benzo[d][1,2,3]triazol-2-yl)-2-hydroxy-5-methoxybenzyl methacrylate (WL-4), 2-hydroxy-5-methoxy-3-(5-methyl-2H-benzo) [d][1,2,3]triazol-2-yl)benzyl methacrylate (WL-6), 2-hydroxy-5-methyl-3-(5-(trifluoromethyl)-2H-benzo[d][1,2,3]triazol-2-yl)benzyl methacrylate (WL-7), 4-allyl-2-(5-chloro-2H-benzo[d][1,2,3]triazol-2-yl)-6-methoxyphenol (WL-8), 2-{2'-hydroxy-3'-tert-5'[3”-(4”-vinylbenzyloxy)propoxy]phenyl}-5-methoxy- 2H-benzotriazole, phenol, 2-(5-chloro-2) H-benzotriazole-2-yl)-6-(1,1-dimethylethyl)-4-vinyl-(UVAM), 2-[2'-hydroxy-5'-(2-methacrylic acid oxyethyl)phenyl)]-2H-benzotriazole (2-acrylic acid, 2-methyl-, 2-[3-(2-... [H-benzotriazol-2-yl)-4-hydroxyphenyl]ethyl ester, Norbloc), 2-{2'-hydroxy-3'-tert-butyl-5'-[3'-methacryloxypropoxy]phenyl}- 2H-benzotriazole, 2-{2'-hydroxy-3'-tert-butyl-5'-[3'-methacryloxypropoxy]phenyl}-5-methoxy- 2H-benzotriazole (UV13), 2-{2'-hydroxy-3'-tert-butyl-5'-[3'-methacryloxypropoxy]phenyl}-5-chloro- 2H-benzotriazole (UV28), 2-[2'-hydroxy-3'-tert-butyl-5'-(3'-acryloxypropoxy)phenyl]-5-trifluoromethyl- 2H-benzotriazole (UV23), 2-(2'-hydroxy-5-methylpropenylaminophenyl)-5-methoxybenzotriazole (UV6), 2-(3-allyl-2-hydroxy-5-methylphenyl)- 2H-benzotriazole (UV9), 2-(2-hydroxy-3-methylallyl-5-methylphenyl)- 2H-benzotriazole (UV12), 2-3'-tert-butyl-2'-hydroxy-5'-(3”-dimethylvinylsilylpropoxy)-2'-hydroxy-phenyl)-5-methoxybenzotriazole (UV15), 2-(2'-hydroxy-5'-methacrylopropyl-3'-tert-butyl-phenyl)-5-methoxy- 2H-benzotriazole (UV16), 2-(2'-hydroxy-5'-propenylated-3'-tert-butyl-phenyl)-5-methoxy- 2H-benzotriazole (UV16A), 3-[3-tert-butyl-5-(5-chlorobenzotriazole-2-yl)-4-hydroxyphenyl]-propyl 2-methacrylate (16-100, CAS#96478-15-8), 2-(3-(tert-butyl)-4-hydroxy-5-(5-methoxy-2H-benzo[d][1,2,3]triazole-2-yl)phenoxy)ethyl methacrylate (16-102); phenol, 2-(5-chloro-2-) H-benzotriazol-2-yl)-6-methoxy-4-(2-propen-1-yl) (CAS#1260141-20-5); 2-[2-hydroxy-5-[3-(methacryloxy)propyl]-3-tert-butylphenyl]-5-chloro-2 H-benzotriazole; phenol, 2-(5-vinyl-2H-benzotriazole-2-yl)-4-methyl-, homopolymer (9CI) (CAS#83063-87-0). According to the invention, the polymerizable composition comprises, by weight, about 0.1% to about 3.0%, preferably about 0.2% to about 2.5%, and more preferably about 0.3% to about 2.0% of one or more UV-absorbing vinyl monomers relative to the amount of all polymerizable components in the polymerizable composition. Examples of preferred photochromic vinyl monomers include polymerizable naphthopiperan, polymerizable benzopiperan, polymerizable indenenaphthopiperan, polymerizable phenanthrenepiperan, polymerizable spiro(benzoindoline)-naphthopiperan, polymerizable spiro(indoline)benzopiperan, polymerizable spiro(indoline)-naphthopiperan, polymerizable spiro(indoline)quinipperan, polymerizable spiro(indoline)piperan, polymerizable phenanthrene, polymerizable spirobenzopiperan; polymerizable spirobenzopiperan, polymerizable spirobenzothiaran, polymerizable naphthonaphthione, polymerizable spiro(indoline)phenanthrene, polymerizable spiro(indoline)pyridinobenzopiperan, polymerizable spiro(benzoindoline)pyridinobenzopiperan Pyridobenzo[a], polymerizable spiro(benzoindoline)phen[a], polymerizable spiro(indoline)-benzo[a], polymerizable diarylethylene, and combinations thereof, as disclosed in U.S. Patent Nos. 4,929,693, 5,166,345, 6,017,121, 7,556,750, 7,584,630, 7,999,989, 8,158,037, 8,697,770, 8,741,188, 9052,438, 9097,916, 9,465,234, 9904,074, 10,197,707, 601,9914, 6,113,814, 6,149,841, 6,296,785, and 6,348,604. According to any of the foregoing embodiments, the polymerizable composition comprises: (a) a component (preferably) from about 30% to about 65% by weight (more preferably from about 35% to about 60%, even more preferably from about 40% to about 60%) relative to the total amount of all polymerizable components; (b) and (c) a component (preferably) from about 30% to about 65% by weight (more preferably from about 35% to about 60%, even more preferably from about 40% to about 60%); and (d) a component (preferably) from about 2% to about 10% by weight (more preferably from about 3% to about 9%, even more preferably from about 4% to about 8%). In any of the foregoing embodiments, the weight ratio of component (c) to component (b) in the polymerizable composition is about 40 to about 10, preferably about 35 to about 15, more preferably about 30 to about 15, and even more preferably about 23 to about 11. Other polymerizable components (materials), including various silicone-containing vinyl monomers, polysiloxane vinyl crosslinking agents, hydrophilic vinyl monomers, and hydrophobic vinyl monomers, are well known to those skilled in the art. One or more of these polymerizable components may be used in the polymerizable composition of the present invention, provided that their amount is less than about 10% by weight relative to the total amount of all polymerizable components in the polymerizable composition (preferably less than about 8% by weight, more preferably less than about 6% by weight, and even more preferably less than about 4% by weight). According to any of the foregoing embodiments, the polymerizable composition may also contain other essential components known to those skilled in the art, such as bioactive agents (e.g., pharmaceuticals, amino acids, polypeptides, proteins, nucleic acids, 2-pyrrolidone-5-carboxylic acid (PCA), α-hydroxy acids, linoleic acid and γ-linoleic acid, vitamins, or any combination thereof), leachable lubricants (e.g., non-crosslinkable hydrophilic polymers having an average molecular weight of 5,000 to 500,000, preferably 10,000 to 300,000, more preferably 20,000 to 100,000 Daltons), leachable tear stabilizers (e.g., phospholipids, monoglycerides, diglycerides, triglycerides, glycolipids, glyceroglycolipids, sphingolipids, sphingolipids, fatty acids having 8 to 36 carbon atoms, fatty alcohols having 8 to 36 carbon atoms, or mixtures thereof), release agents, and mixtures thereof, as known to those skilled in the art. The polymerizable composition of the present invention can be prepared by blending all desired components as known to those skilled in the art. Lens molds for manufacturing contact lenses (including hydrogel contact lenses) are well known to those skilled in the art and are used, for example, in casting molding or rotational casting. For example, a mold (for casting molding) typically comprises at least two mold regions (or portions) or half-molds, namely first and second half-molds. The first half-mold defines a first molding (or optical) surface and the second half-mold defines a second molding (or optical) surface. The first and second half-molds are configured to receive each other such that a lens-forming cavity is formed between the first molding surface and the second molding surface. The molding surface of the half-mold is the cavity-forming surface of the mold and is in direct contact with the polymerizable composition. Methods for manufacturing the mold area for casting contact lenses are generally well known to those skilled in the art. The method of this invention is not limited to any particular method of forming a mold. In fact, any method of forming a mold can be used in this invention. Typically, a lens mold for casting molded contact lenses comprises at least two mold halves (or mold areas), a male mold half and a female mold half. The male mold half has a first molding (or optical) surface that directly contacts the polymerizable composition for casting the molded contact lens and defines the rear (or concave) surface of the molded contact lens; and the female mold half has a second molding (or optical) surface that directly contacts the polymerizable composition and defines the front (or convex) surface of the molded contact lens. The male and female mold halves are configured to receive each other such that a lens forming cavity is formed between the first molding surface and the second molding surface. These half-molds can be formed using various techniques such as injection molding. Methods for manufacturing half-molds for casting contact lenses are generally well known to those skilled in the art. The method of this invention is not limited to any particular method of forming a mold. In fact, any method of forming a mold can be used in this invention. The first and second half-molds can be formed using various techniques, such as injection molding or lathe machining. Examples of suitable methods for forming half-molds are disclosed in U.S. Patent Nos. 4,444,711; 4,460,534; 5,843,346; and 5,894,002. Almost all materials known in the art for manufacturing molds can be used to manufacture molds for producing contact lenses. For example, polymeric materials such as polyethylene, polypropylene, polystyrene, PMMA, and Topas can be used. ® COC grade 8007-S10 (a transparent amorphous copolymer of ethylene and nobornene from Ticona GmbH, Frankfurt, Germany and Summit, New Jersey), etc. Other materials that allow UV light transmission, such as quartz glass and sapphire, can be used. According to the invention, polymerizable components can be dispensed into a lens mold using any known technique. For example, typically a specific amount of polymerizable component is dispensed into a female mold using a dispensing device, and then a male mold is placed on top and the mold is closed. When the mold is closed, any excess polymerizable component is pressed into an overflow area provided on the female mold (or alternatively on the male mold). As is known to those skilled in the art, the molding element (i.e., a closed mold comprising a second polymerizable fluid composition and a partially cross-linked circular layer immersed therein) is then thermo-cured or photo-cured to form a silicone hydrogel lens precursor comprising a bulk silicone hydrogel material containing carboxyl groups. It should be understood that carboxyl groups on and / or near the surface of the bulk silicone hydrogel material can act as reactive sites that can covalently attach to layers of cross-linked hydrophilic polymeric material. After curing, the mold can be opened using any technique known to those skilled in the art. After mold separation, the silicone hydrogel lens is first adhered to one of the male and female mold halves. Silicone hydrogel lens preforms adhered to the semi-mold to which the lens is attached can be removed from the semi-mold and then subjected to one or more molding processes. According to the present invention, the water-soluble and thermally crosslinkable hydrophilic polymer material preferably contains an azacyclobutaneonium group or an epoxy group or a combination thereof. Preferably, the water-soluble and crosslinkable hydrophilic polymer material is a partially crosslinked polymer material comprising a three-dimensional network and thermally crosslinkable groups within or attached to the network, preferably an azacyclobutaneonium group. The term "partially crosslinked" in relation to polymer materials means that the crosslinkable groups of the starting material used to produce the polymer material in the crosslinking reaction have not been completely consumed. For example, such a thermally crosslinkable hydrophilic polymer material contains an azacyclobutaneonium group and is a partial reaction product of at least one azacyclobutaneonium-containing polymer and at least one hydrophilic enhancer (i.e., wetting agent) having at least one carboxyl group, a primary amine group, a secondary amine group, or a thiol group, according to the crosslinking reaction shown in Scheme I. plan I in which X The series -S-*, -OC(=O)-*, or -NR'-*, where R' is hydrogen or C 1-C 20 Unsubstituted or substituted alkyl groups, and * represents an organic group. Examples of preferred water-soluble and thermally crosslinkable hydrophilic polymeric materials comprising epoxy groups include, but are not limited to: one or more multi-arm polyethylene glycols each having a terminal epoxy group; mixtures of multi-arm polyethylene glycols having terminal epoxy groups and one or more polyethylene glycols each having a terminal functional group selected from the group consisting of primary amine groups, secondary amine groups, carboxyl groups, thiol groups, and combinations thereof; partial reaction products of multi-arm polyethylenes having terminal epoxy groups and hydrophilic enhancers having at least one reactive functional group selected from the group consisting of amine groups, carboxyl groups, thiol groups, and combinations thereof (such as the hydrophilic polymers disclosed in U.S. Patent No. 9,505,184 and U.S. Patent No. 6,440,571), or combinations thereof. Examples of preferred water-soluble and thermally crosslinkable hydrophilic polymer materials containing azacyclobutaneonium groups include, but are not limited to, the poly(2-azoline-co-ethyleneimine)-epimyl chloride copolymer disclosed in U.S. Patent No. 9,720,138, the chemically modified poly(2-azoline-co-ethyleneimine)-epimyl chloride copolymer disclosed in U.S. Patent No. 9,720,138, the chemically modified poly(aminoamine-epimyl chloride) disclosed in U.S. Patent No. 8,529,057, the copolymer of azacyclobutaneonium ethylene monomers with one or more hydrophilic ethylene monomers disclosed in U.S. Patent No. 9,422,447, the chemically modified copolymer of azacyclobutaneonium ethylene monomers with one or more hydrophilic ethylene monomers disclosed in U.S. Patent No. 9,422,447, or combinations thereof. According to the present invention, the term "chemically modified" in relation to water-soluble and thermally crosslinkable hydrophilic polymer materials having azacyclobutaneonium groups means that a copolymer of poly(2-azoline-co-ethyleneimine)-epimyl chloride, polyamide-epimyl chloride, or a ethylene monomer containing azacyclobutaneonium partially reacts with a hydrophilic enhancer having at least one reactive functional group selected from the group consisting of amine, carboxyl, thiol, and combinations thereof (i.e., without consuming all of these azacyclobutaneonium groups). Chemically modified poly(2-azoline-co-ethyleneimine)-epimyl chloride copolymers or polyamide-epimyl chloride or ethylene monomers containing azacyclobutaneonium can be particularly useful for relatively thick and soft non-silicone hydrogel coating systems formed on silicone hydrogel contact lenses. Any suitable hydrophilicity enhancer can be used in this invention, provided that it contains at least one amine group, at least one carboxyl group, and / or at least one thiol group. Preferred hydrophilicity enhancers include, but are not limited to, monosaccharides containing primary, secondary, carboxyl, or thiol groups (e.g., 3-amino-1,2-propanediol, 1-mercaptoglycerol, 5-keto-D-gluconic acid, galactosamine, glucosamine, galacturonic acid, gluconic acid, aminogluconic acid, mannosamine, gluconic acid-1,4-lactone, gluconic acid, eurosonic acid). N-methyl-D-glucosamine, 1-amino-1-deoxy-β-D-galactose, 1-amino-1-deoxysorbitol, 1-methylamino-1-deoxysorbitol, N-aminoethylglucosamine (gluconamide); disaccharides containing a primary amino group, a secondary amino group, a carboxyl group or a thiol group (e.g., chondroitin disaccharide sodium salt, di(β-D-piperanoxylosyl)amine, digalacturonic acid, heparin disaccharide, hyaluronic acid disaccharide, lactobionic acid); and oligosaccharides containing a primary amino group, a secondary amino group, a carboxyl group or a thiol group (e.g., carboxymethyl-β-cyclodextrin sodium salt, trigalacturonic acid); and combinations thereof. Another preferred class of hydrophilicity enhancers are hydrophilic polymers having one or more (primary or secondary) amine, carboxyl, and / or thiol groups. More preferably, the content of amine groups (-NHR', where R' is as defined above), carboxyl groups (-COOH), and / or thiol groups (-SH) in the hydrophilic polymer used as a hydrophilicity enhancer is less than about 40% by weight based on the total weight of the hydrophilic polymer, preferably less than about 30%, more preferably less than about 20%, and even more preferably less than about 10%. Preferred hydrophilic polymers as hydrophilic enhancers are polysaccharides containing (primary or secondary) amino or carboxyl groups, such as carboxymethyl cellulose (having a carboxyl content of about 40% or less, the carboxyl content being based on repeating units -[C 6H 10-m O 5(CH 2CO 2H) m The composition of []- is estimated, wherein m is series 1 to 3), carboxyethyl cellulose (with a carboxyl content of about 36% or less, which is based on repeating unit - [C 6H 10-m O 5(C 2H 4CO 2H) m The composition of []- is estimated, where m is series 1 to 3), carboxypropyl cellulose (with a carboxyl content of about 32% or less, which is based on repeating unit - [C 6H 10-m O 5(C 3H 6CO 2H) m The composition of []- is estimated, where m is series 1 to 3), hyaluronic acid (with a carboxyl content of approximately 11%, which is based on the repeating unit -(C 13 H 20 O 9NCO The composition of chondroitin sulfate (which has a carboxyl content of approximately 9.8%, based on the repeating unit -(C)) is estimated. 12 H 18 O 13 NSCO (2H)- composition estimated), or combinations thereof. Another class of preferred hydrophilic polymers as hydrophilicity enhancers includes, but is not limited to: polyethylene glycol (PEG) having mono-amine groups (primary or secondary amine groups), carboxyl groups, or thiol groups (e.g., PEG-NH). 2. PEG-SH, PEG-COOH); H 2N-PEG-NH 2; HOOC-PEG-COOH; HS-PEG-SH; H 2N-PEG-COOH; HOOC-PEG-SH; H 2N-PEG-SH; multi-arm PEG having one or more amino (primary or secondary), carboxyl, or thiol groups; PEG dendritic polymer having one or more amino (primary or secondary), carboxyl, or thiol groups; homopolymers or copolymers of non-reactive hydrophilic vinyl monomers with diamine-(primary or secondary) or dicarboxyl-terminated ends; homopolymers or copolymers of non-reactive hydrophilic vinyl monomers with monoamine-(primary or secondary) or monocarboxyl-terminated ends; copolymers comprising the following components: (1) about 60% or less, preferably from about 0.1% to about 30%, more preferably from about 0.5% to about 20%, and even more preferably from about 1% to about 15% by weight of one or more reactive vinyl monomers, and (2) at least one non-reactive hydrophilic vinyl monomer; and combinations thereof. The combination of one or more reactive vinyl monomers and one or more non-reactive hydrophilic vinyl monomers is as previously described. According to the present invention, the reactive vinyl monomer used to manufacture the hydrophilicity enhancer can be a carboxyl-containing vinyl monomer, a primary amine-containing vinyl monomer, or a secondary amine-containing vinyl monomer. Preferred examples of carboxyl-containing vinyl monomers include, but are not limited to, acrylic acid, methacrylic acid, ethylacrylic acid, N-2-(meth)acrylamide glycolic acid, and combinations thereof. Examples of preferred vinyl monomers containing primary and secondary amino groups include, but are not limited to, N-2-aminoethyl (meth)acrylamide, N-2-methylaminoethyl (meth)acrylamide, N-2-ethylaminoethyl (meth)acrylamide, N-3-aminopropyl (meth)acrylamide, N-3-methylaminopropyl (meth)acrylamide, 2-aminoethyl (meth)acrylate, 2-methylaminoethyl (meth)acrylate, 2-ethylaminoethyl (meth)acrylate, 3-aminopropyl (meth)acrylate, 3-methylaminopropyl (meth)acrylate, 3-ethylaminopropyl (meth)acrylate, 3-amino-2-hydroxypropyl (meth)acrylate, and combinations thereof. According to the present invention, the non-reactive ethylene monomer system used to manufacture the hydrophilicity enhancer is a ethylene monomer free of any carboxyl group, primary amino group, secondary amino group, epoxy group, isocyanate group, acrylonitrile group, or azircyclopropane group. Preferably, the non-reactive ethylene monomer is an uncharged hydrophilic ethylene monomer free of carboxyl or amino groups (any of those described above may be used herein), a phosphatidylcholine-containing ethylene monomer (any of those described above may be used herein), or a combination thereof. Even better, the hydrophilic polymer system used as a hydrophilicity enhancer has a unique -NH group. 2. Poly(ethylene glycol) with -SH or -COOH functional groups; having two selectable groups from -NH 2. Poly(ethylene glycol) with terminal functional groups of -COOH, -SH, and combinations thereof; having one or more functional groups selected from -NH 2. Multi-arm poly(ethylene glycol) with functional groups of -COOH, -SH, and combinations thereof; homopolymers or copolymers of non-reactive hydrophilic vinyl monomers terminated with monoamine, monocarboxyl, diamine, or dicarboxyl groups; copolymers comprising polymers of: (1) a reactive vinyl monomer comprising, by weight, from about 0.1% to about 30%, preferably from about 0.5% to about 20%, more preferably from about 1% to about 15%, and (2) at least one non-reactive vinyl monomer; Examples of preferred reactive vinyl monomers include, but are not limited to, acrylic acid, methacrylic acid, ethylacrylic acid, 2-(meth)acrylaminoglycolic acid, N-2-aminoethyl(meth)acrylamine, N-2-methylaminoethyl(meth)acrylamine, N-2-ethylaminoethyl(meth)acrylamine, N-3-aminopropyl(meth)acrylamine, N-3-methylaminopropyl(meth)acrylamine, 2-aminoethyl(meth)acrylate, 2-methylaminoethyl(meth)acrylate, 2-ethylaminoethyl(meth)acrylate, 3-aminopropyl(meth)acrylate, 3-methylaminopropyl(meth)acrylate, 3-amino-2-hydroxypropyl(meth)acrylate, and combinations thereof. Preferred examples of non-reactive hydrophilic vinyl monomers include, but are not limited to, alkyl (meth)acrylamide (any of those described above), N-2-dimethylaminoethyl (meth)acrylamide, dimethylaminoethyl (meth)acrylate, hydroxyl-containing acrylic monomers (any of those described above), N-vinylamide monomers (any of those described above), methylene-containing pyrrolidone monomers (i.e., pyrrolidone derivatives each having a methylene group linked to a pyrrolidone ring at the 3- or 5-position) (any of those described above), and monomers having a C 1-C 4. Alkoxyethoxy acrylic monomers (any one of those described above), vinyl ether monomers (any one of those described above), allyl ether monomers (any one of those described above), phosphocholine-containing vinyl monomers (any one of those described above), and combinations thereof. Preferably, the non-reactive hydrophilic ethylene monomer is selected from the group consisting of: (meth)acryloxyethylphosphocholine, (meth)acryloxypropylphosphocholine, 4-((meth)acryloxy)butyl-2'-(trimethylammonium)ethyl phosphate, 2-[(meth)acrylamino]ethyl-2'-(trimethylammonium)ethyl phosphate, 3-[(meth)acrylamino]propyl-2'-(trimethylammonium)ethyl phosphate, 4-[(meth)acrylamino]butyl-2'-(trimethylammonium)ethyl phosphate, (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl) (meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, glyceryl methacrylate (GMA), tetra(ethylene glycol)(meth)acrylate, poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, N-vinylmethylamine, N-vinylacetamide, 1-methyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, tetra(ethylene glycol)methyl ether(meth)acrylate, methoxy poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, C with a weight average molecular weight up to 1500 1-C 4-alkoxy polyethylene glycol (meth)acrylate, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) monoallyl ether, poly(ethylene glycol) monoallyl ether, tetra(ethylene glycol) methyl allyl ether, poly(ethylene glycol) methyl allyl ether, vinyl alcohol, allyl alcohol, and combinations thereof, preferably selected from the group consisting of: (meth)acryloxyethylphosphatidylcholine, (meth)acryloxypropylphosphatidylcholine, 4-((meth)acryloxy) Butyl-2'-(trimethylammonium)ethyl phosphate, 2-[(meth)acrylamide]ethyl-2'-(trimethylammonium)ethyl phosphate, 3-[(meth)acrylamide]propyl-2'-(trimethylammonium)ethyl phosphate, 4-[(meth)acrylamide]butyl-2'-(trimethylammonium)ethyl phosphate, (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl) (meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, glyceryl methacrylate (GMA), poly(ethylene glycol) ethyl(meth)acrylamide with a number average molecular weight up to 1500, poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, methoxy-poly(ethylene glycol) ethyl(meth)acrylamide with a number average molecular weight up to 1500, methoxy-poly(ethylene glycol)(meth)acrylate with a weight average molecular weight up to 1500, poly(ethylene glycol) monovinyl ether, poly(ethylene glycol) methyl ethyl ether Alkenyl ethers, poly(ethylene glycol) monoallyl ethers, poly(ethylene glycol) methyl allyl ethers, vinyl alcohol, allyl alcohol, and combinations thereof, and preferably selected from the group consisting of: (meth)acryloxyethylphosphocholine, (meth)acryloxypropylphosphocholine, 2-[(meth)acrylamino]ethyl-2'-(trimethylammonium)ethyl phosphate, 3-[(meth)acrylamino]propyl-2'-(trimethylammonium)ethyl phosphate, (meth)acrylamine, dimethyl (meth)acrylamine, N-2-hydroxyethyl (meth)acrylamine, N,N-bis(hydroxyethyl) (meth)acrylamine, N-2,3-dihydroxypropyl (meth)acrylamine, N-tris(hydroxymethyl)methyl(meth)acrylamide, poly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, poly(ethylene glycol)(meth)acrylate having a number average molecular weight of up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, methoxypoly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, methoxypolyethylene glycol(meth)acrylate having a weight average molecular weight of up to 1500, and combinations thereof. Functionalized PEG and multi-armed PEG with functional groups can be obtained from various commercial suppliers, such as Polyscience and Shearwater Polymers, Inc. Homopolymers or copolymers of one or more nonreactive hydrophilic vinyl monomers or phosphatidylcholine-containing vinyl monomers, which are monoamine-, monocarboxyl-, diamine-, or dicarboxyl-terminated, may be prepared according to the procedures described in U.S. Patent No. 6,218,508 (which is incorporated herein by reference in its entirety). For example, to prepare a diamine- or dicarboxyl-terminated homopolymer or copolymer of a nonreactive hydrophilic vinyl monomer, a chain transfer agent having an amino or carboxyl group (e.g., 2-aminoethanethiol, 2-mercaptopropionic acid, thioglycolic acid, thiolactic acid, or other hydroxythiols, aminothiols, or carboxyl-containing thiols), and, if desired, other vinyl monomers, are copolymerized with the reactive vinyl monomer (having an amino or carboxyl group) in the presence of a free radical initiator (thermally or photochemically). Typically, the molar ratio of the chain transfer agent to all vinyl monomers except the reactive vinyl monomer is from about 1:5 to about 1:100, while the molar ratio of the chain transfer agent to the reactive vinyl monomer is 1:1. In this preparation, the chain transfer agent having an amino or carboxyl group is used to control the molecular weight of the resulting hydrophilic polymer and to form the terminus of the resulting hydrophilic polymer, thereby providing the resulting hydrophilic polymer with one terminal amino or carboxyl group, while the reactive vinyl monomer provides another terminal carboxyl or amino group to the resulting hydrophilic polymer. Similarly, in order to prepare homopolymers or copolymers of non-reactive hydrophilic vinyl monomers with monoamine or monocarboxyl groups, the non-reactive vinyl monomers, chain transfer agents having amino or carboxyl groups (e.g., 2-aminoethanethiol, 2-mercaptopropionic acid, thioglycolic acid, thiolactic acid, or other hydroxythiols, aminothiols, or carboxyl-containing thiols), and other vinyl monomers as desired, are copolymerized (thermally or photochemically) in the absence of any reactive vinyl monomers. Copolymers comprising non-reactive hydrophilic vinyl monomers and reactive vinyl monomers (e.g., carboxyl-containing vinyl monomers, primary amine-containing vinyl monomers, or secondary amine-containing vinyl monomers) can be prepared according to any well-known free radical polymerization method or obtained from commercial suppliers. Copolymers comprising methacryloxyethylphosphatidylcholine and carboxyl-containing vinyl monomers (or amine-containing vinyl monomers) are available from NOP (e.g., LIPIDURE®-AC01 and AE). The weight average molecular weight M of a hydrophilic polymer having at least one amine, carboxyl, or thiol group (as a hydrophilicity enhancer) w Preferably, the amount is from about 500 to about 2,000,000, even more preferably from about 1,000 to about 500,000, and even more preferably from about 5,000 to about 250,000 Daltons. Water-soluble and thermally crosslinkable hydrophilic polymer materials can be prepared according to the methods disclosed in U.S. Patent Application Publication No. US 2019 / 0179055 A1 and U.S. Patent Nos. 8529057, 9422447, and 9720138. In a preferred embodiment, the water-soluble thermally crosslinkable polymer material can be obtained by heating an aqueous reactive solution to a temperature from about 35°C to about 85°C and maintaining that temperature for a sufficient period of time (about 8 hours or less, preferably about 5 hours, more preferably from about 2 hours to about 4 hours), the aqueous reactive solution comprising at least one nitrogen-containing heterocyclic butaneonium polymer and at least one hydrophilic enhancer (i.e., wetting agent) having at least one reactive functional group selected from the group consisting of amine, carboxyl, mercapto, and combinations thereof. The aqueous reactive solution preferably comprises one or more ionic compounds from about 70 mM to about 170 mM (preferably about 90 mM to about 150 mM, more preferably from about 100 mM to about 130 mM) and has a pH of at least 8.0 (preferably at least 8.5, more preferably at least 9.0, and even more preferably at least 9.5). It should be understood that the reaction time should be long enough to covalently attach the hydrophilic reinforcing agent to the polymer chain of the nitrogen-containing heterocyclic butanetonium polymer, but short enough not to consume all the nitrogen-containing heterocyclic butanetonium groups of the polymer and not to form a gel (i.e., not water-soluble) (due to too many crosslinks formed between the nitrogen-containing heterocyclic butanetonium polymer and the hydrophilic reinforcing agent). The resulting polymer material is a slightly crosslinked polymer material with a highly branched structure and still contains thermally crosslinkable nitrogen-containing heterocyclic butanetonium groups. Those familiar with this technology understand well how to adjust the pH of reactive mixtures, for example, by adding a base (e.g., NaOH, KOH, NH4OH). 4OH (or mixtures thereof) or acids (e.g., HCl, H+) 2SO 4. H 3PO 4. Citric acid, acetic acid, boric acid, or mixtures thereof. According to the present invention, any ionic compound can be used in reactive mixtures. Preferably, the ionic compound is one used as an ion tension modifier and an ion buffer used in ophthalmic solutions. Examples of preferred ion tension modifiers include, but are not limited to, sodium chloride, potassium chloride, and combinations thereof. Examples of preferred ion buffers include various salts of phosphate (e.g., NaH+). 2PO 4. Na 2HPO 4. Na 3PO 4. KH 2PO 4. K 2HPO 4. K 3PO 4. (or mixtures thereof), various salts of boric acid (e.g., sodium borate, potassium borate, or mixtures thereof), various salts of citric acid (e.g., monosodium citrate, disodium citrate, trisodium citrate, monopotassium citrate, dipotassium citrate, tripotassium citrate, or mixtures thereof), and various salts of carbonic acid (e.g., Na+). 2CO 3. NaHCO3 3. K 2CO 3. KHCO 3. or a mixture thereof). An aqueous reactive solution for preparing a water-soluble, thermally crosslinkable polymer material can be prepared by dissolving a desired amount of a polymer containing a nitrogen-containing heterocyclic butaneonium, a desired amount of a hydrophilic enhancer having at least one reactive functional group, and a desired amount of other components (e.g., ion buffers, ion tension modifiers, etc.) in water (or a mixture of water and a small amount of water-soluble organic solvent) to form an aqueous solution, and then adjusting the pH of the aqueous solution (if necessary). According to the present invention, the concentration ratio of the hydrophilicity enhancer relative to the nitrogen-containing heterocyclic butanetonium polymer in the aqueous reactive solution must be selected such that the resulting water-soluble thermally crosslinkable polymer material is insoluble in water (i.e., less than 0.005 g / 100 ml of water at room temperature) and does not consume more than about 99%, preferably about 98%, more preferably about 97%, and even more preferably about 96% of the nitrogen-containing heterocyclic butanetonium polymer nitrogen-containing butanetonium groups. In a preferred embodiment, the aqueous reactive solution comprises, by weight, from 0.01% to 10% (preferably from 0.05% to 5% by weight, more preferably from 0.08% to 1% by weight, and even more preferably from 0.1% to 0.4% by weight) of a nitrogen-containing heterocyclic butanetonium polymer and by weight, from about 0.01% to 10% (preferably from 0.02% to 5% by weight, more preferably from 0.05% to 2% by weight, and even more preferably from 0.08% to 1.0% by weight) of a hydrophilic enhancer having at least one reactive functional group (carboxyl, primary amine, secondary amine), wherein the concentration ratio of the nitrogen-containing heterocyclic butanetonium polymer to the hydrophilic enhancer is from about 1000:1 to 1:1000 (preferably from about 500:1 to about 1:1000). 500, more preferably from about 250:1 to about 1:250, and even more preferably from about 100:1 to about 1:100. In a preferred embodiment, the water-soluble, thermally crosslinkable polymeric material comprises (i) from about 20% to about 95% by weight of a first polymer chain derived from polyamide-epimine or poly(2-azoline-co-ethyleneimine)-epimine, (ii) from about 5% to about 80% by weight of a hydrophilic portion or a second polymer chain derived from at least one hydrophilic reinforcing agent having at least one reactive functional group selected from the group consisting of amine, carboxyl, thiol, and combinations thereof (preferably carboxyl or thiol), wherein the hydrophilic portion or the second polymer chain is covalently attached to the first polymer chain by one or more covalent bonds formed between a aziridine group of polyamide-epimine or poly(2-azoline-co-ethyleneimine)-epimine and an amine, carboxyl, or thiol group of the hydrophilic reinforcing agent, and (iii) The azacyclobutaneonium group is part of the first polymer chain or is covalently attached to a side group or end group of the first polymer chain. The composition of the chemically modified poly(2-azoline-co-ethyleneimine)-epimole or the chemically modified polyamide-epimole is determined by the composition of the reactant mixture used for this polymer according to the crosslinking reaction shown in Scheme I above (based on the total weight of the reactants). For example, if the reactant mixture contains about 75% by weight of polyamide-epimole and about 25% by weight of at least one hydrophilic reinforcing agent based on the total weight of the reactants, the resulting chemically modified polyamide-epimole contains about 75% by weight of a first polymer chain derived from polyamide-epimole and about 25% by weight of a hydrophilic portion or a second polymer chain derived from said at least one hydrophilic reinforcing agent. According to the present invention, the heating step is preferably performed by autoclaving the silicone hydrogel lens pretreatment, which is to be immersed in a packaging solution (i.e., a buffer aqueous solution) in the sealed lens packaging, at a temperature of about 115°C to about 125°C for about 20-90 minutes. According to this embodiment of the present invention, the packaging solution is an ophthalmologically safe buffer aqueous solution after autoclaving. Lens packaging (or containers) is well known to those skilled in the art for autoclaving and storing soft contact lenses. Any lens packaging can be used in this invention. Preferably, the lens packaging is a blister pack comprising a base and a cover, wherein the cover is removably sealed to the base, and wherein the base includes a cavity for receiving a sterile packaging solution and the contact lens. Before being distributed to users, the lenses are packaged in individual containers, sealed, and sterilized (e.g., by autoclaving at approximately 120°C or higher for at least 30 minutes). Those familiar with this technology should have a good understanding of how to seal and sterilize the lens packaging. According to the present invention, the packaging solution contains at least one buffer and one or more other components known to those skilled in the art. Examples of other components include, but are not limited to, tensile agents, surfactants, antimicrobial agents, preservatives, and lubricants (e.g., cellulose derivatives, polyvinyl alcohol, polyvinylpyrrolidone). The packaging solution contains a buffer amount sufficient to maintain the pH of the packaging solution within a desired range (e.g., preferably from about 6.8 to about 8.5, more preferably from about 7.0 to 8.2, and even more preferably from about 7.2 to about 8.0). Higher pH values have been found to be desirable for ensuring that all or a significant portion of the carboxyl groups of the bulk silicone hydrogel material are ionized. Therefore, the resulting silicone hydrogel contact lenses become dimensionally stable in the packaging solution during autoclaving and storage and can exhibit improved lubricity. Any known physiologically compatible buffer can be used. Suitable buffers as components of the contact lens care composition according to the present invention are known to those skilled in the art. Preferably, a phosphate buffer (consisting essentially of a monodihydrogen phosphate (e.g., NaH+)) is used. 2PO 4. KH 2PO 4. or mixtures thereof) and dihydrogen phosphates (e.g., Na+) 2HPO 4. K 2HPO 4. A mixture of the present and present solutions (or mixtures thereof) is used to maintain the pH of the packaged solution. In various preferred embodiments, the total concentration of monohydrogen phosphate and dihydrogen phosphate is at least 30 mM (preferably at least 35 mM, more preferably at least 40 mM, and even more preferably at least 45 mM). Preferably, the solutions according to the invention are prepared in a manner that makes them isotonic with tears. A solution isotonic with tears is generally understood to be a solution with a concentration equivalent to that of a 0.9% sodium chloride solution (308 mOsm / kg). Deviations from this concentration may occur throughout. The isotonicity with tears or even another desired tone can be adjusted by adding organic or inorganic substances that affect tone. Suitable ocularly acceptable tone-regulating agents include, but are not limited to, sodium chloride, potassium chloride, glycerol, propylene glycol, polyols, mannitol, sorbitol, xylitol, and mixtures thereof. The tone of the packaged solution is typically adjusted to from about 200 to about 450 mOsm, preferably from about 250 to 350 mOsm. In a preferred embodiment, one or more organic tensile agents (e.g., glycerol, propylene glycol, polyethylene glycol having a number average molecular weight of 200 to 800 Daltons, mannitol, sorbitol, xylitol, and mixtures thereof) are present in an amount of at least 70 mM (preferably at least 90 mM, more preferably at least 110 mM, and even more preferably at least 130 mM) to adjust the tensile of the packaging solution. It has been found that the resulting silicone hydrogel contact lenses can exhibit improved lubricity when the ionic strength of the packaging solution decreases (e.g., by replacing a portion of the NaCl with an organic tensile agent (e.g., propylene glycol)). In a preferred embodiment, the packaging solution comprises, by weight, preferably from about 0.01% to about 2%, more preferably from about 0.05% to about 1.5%, even more preferably from about 0.1% to about 1%, and most preferably from about 0.2% to about 0.5% of a water-soluble, thermocrosslinkable hydrophilic polymer material having a nitrogen-containing butaneonium group. On another front, the present invention provides a coated silicone hydrogel contact lens comprising a bulk silicone hydrogel material and a layer thereon of a non-silicone hydrogel material (i.e., a cross-linked hydrophilic polymer material), wherein the bulk silicone hydrogel material comprises (a) repeating units of at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) repeating units of hydroxyethyl methacrylate, and (c) at least one (meth)acrylic acid C 1-C (d) a repeating unit of 2-alkoxyethyl ester, and (e) a repeating unit of at least one carboxyl-containing (meth)acryloxy monomer, and (f) a repeating unit of at least one polymerizable component selected from the group consisting of: non-silicone vinyl crosslinking agents, UV-absorbing vinyl monomers, polymerizable UV / high-energy ultraviolet light absorbing compounds, polymerizable photochromic compounds, polymerizable colorants, and combinations thereof, provided that component (e) is present. The amount is less than 10% by weight relative to the total weight of the bulk silicone hydrogel material in a dry state, wherein the non-silicone hydrogel material layer is covalently attached to the bulk silicone hydrogel material by the carboxyl groups of the carboxyl repeating units, wherein the silicone hydrogel contact lens has a water breakup time (WBUT) of at least about 5 seconds (preferably at least about 10 seconds, more preferably at least about 15 seconds, and even more preferably at least about 20 seconds), an oxygen permeability (Dk) of at least about 50 bar (preferably at least about 60 bar, more preferably at least about 70 bar, and even more preferably at least about 80 bar), and an elastic modulus from 0.2 MPa to 1.8 MPa (preferably from about 0.2 MPa to about 1.5 MPa, more preferably from about 0.3 MPa to about 1.2 MPa, and even more preferably from about 0.4 MPa to about 1.0 MPa). It should be understood that the amount of component (e) relative to the total weight of the bulk silicone hydrogel material in a dry state can be calculated based on the weight percentage of component (e) relative to the total weight of all polymerizable components in the polymerizable composition used to form the bulk silicone hydrogel material. In various preferred embodiments, the bulk silicone hydrogel material further comprises: a repeating unit of at least one non-silicone ethylene crosslinking agent; a repeating unit of at least one UV-absorbing ethylene monomer; a repeating unit of at least one polymerizable UV / HEVL-absorbing compound; a repeating unit of at least one polymerizable photochromic compound; or a combination thereof. In various preferred embodiments, the non-silicone hydrogel material is: (1) a crosslinked polymer material comprising at least 25% (preferably at least 35% by moles, more preferably at least 45% by moles, and even more preferably at least 55% by moles) repeating monomer units of at least one hydrophilic vinyl monomer selected from the group consisting of: alkyl (meth)acrylamide (any one described below), N-2-dimethylaminoethyl (meth)acrylamide, dimethylaminoethyl (meth)acrylate, hydroxyl-containing acrylic monomers (any one described below), N-vinylamide monomers (any one described below), methylene-containing pyrrolidone monomers (i.e., pyrrolidone derivatives each having a methylene group linked to a pyrrolidone ring at the 3- or 5-position) (any one described below), having C 1-C 4-alkoxyethoxy acrylic monomers (any one described below), vinyl ether monomers (any one described below), allyl ether monomers (any one described below), and combinations thereof (preferably selected from the group consisting of: (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl)(meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, glyceryl methacrylate (GMA), tetra(ethylene glycol)(meth)acrylate, poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, N-vinylmethylamine, N-vinylacetamide, 1-methyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, tetra(ethylene glycol)methyl ether(meth)acrylate, methoxy poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, C with a weight average molecular weight up to 1500 1-C 4-Alkoxy polyethylene glycol (meth)acrylate, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) monoallyl ether, poly(ethylene glycol) monoallyl ether, tetra(ethylene glycol) methyl allyl ether, poly(ethylene glycol) methyl allyl ether, vinyl alcohol, allyl alcohol, and combinations thereof, preferably selected from the group consisting of: (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl) (meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, glyceryl methacrylate (GMA), poly(ethylene glycol) ethyl(meth)acrylamide with a number average molecular weight up to 1500, poly(ethylene glycol) (meth)acrylate with a number average molecular weight up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, methoxy poly(ethylene glycol) ethyl(meth)acrylamide with a number average molecular weight up to 1500, and poly(ethylene glycol) ethyl(meth)acrylamide with a number average molecular weight up to 1500. Methoxylated polyethylene glycol (meth)acrylates, poly(ethylene glycol) monovinyl ethers, poly(ethylene glycol) methyl vinyl ethers, poly(ethylene glycol) monoallyl ethers, poly(ethylene glycol) methyl allyl ethers, vinyl alcohol, allyl alcohol, and combinations thereof, preferably selected from the group consisting of: (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl) (meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-tris(hydroxymethyl)methyl(meth)acrylamide, poly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, poly(ethylene glycol)(meth)acrylate having a number average molecular weight of up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, methoxy-poly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, methoxy-polyethylene glycol(meth)acrylate having a weight average molecular weight of up to 1500, and combinations thereof; (2) A crosslinked polymer material comprising at least 25% (preferably at least 35% by mole, more preferably at least 45% by mole, and even more preferably at least 55% by mole) repeating monomer units of at least one phosphatidylcholine-containing vinyl monomer (any one described below), wherein the phosphatidylcholine-containing vinyl monomer is preferably selected from the group consisting of: (meth)acryloyloxyethylphosphatidylcholine, ... (2) Acryloxypropylphosphocholine, 4-((meth)acryloxy)butyl-2'-(trimethylammonium)ethyl phosphate, 2-[(meth)acrylamino]ethyl-2'-(trimethylammonium)ethyl phosphate, 3-[(meth)acrylamino]propyl-2'-(trimethylammonium)ethyl phosphate, 4-[(meth)acrylamino]butyl-2'-(trimethylammonium)ethyl phosphate, and combinations thereof; (3) Crosslinked polymer materials comprising poly(ethylene glycol) chains, preferably directly derived from (a) having a unique -NH 2. Poly(ethylene glycol) with -SH or -COOH functional groups, (b) having two groups selected from -NH 2. Poly(ethylene glycol) with terminal functional groups of -COOH, -SH, and combinations thereof, (c) having one or more of the following selected from -NH 2. Multi-arm poly(ethylene glycol) with functional groups consisting of -COOH, -SH, and combinations thereof, and (d) combinations thereof. Examples of alkyl (meth)acrylamide include, but are not limited to, (meth)acrylamide, N,N-dimethyl (meth)acrylamide, N-ethyl (meth)acrylamide, N,N-diethyl (meth)acrylamide, N-propyl (meth)acrylamide, N-isopropyl (meth)acrylamide, N-3-methoxypropyl (meth)acrylamide, and combinations thereof. Examples of hydroxyl-containing acrylic monomers include, but are not limited to, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl) (meth)acrylamide, N-3-hydroxypropyl (meth)acrylamide, N-2-hydroxypropyl (meth)acrylamide, and N-2,3-dihydroxypropyl (meth)acrylamide. N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, 3-hydroxypropyl(meth)acrylate, 2-hydroxypropyl(meth)acrylate, glyceryl methacrylate (GMA), di(ethylene glycol)(meth)acrylate, tri(ethylene glycol)(meth)acrylate, tetra(ethylene glycol)(meth)acrylate, poly(ethylene glycol)(meth)acrylate having a number average molecular weight of up to 1500, poly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, and combinations thereof. Examples of preferred N-vinylpyridine monomers include, but are not limited to, N-vinylpyrrolidone (also known as, N-vinyl-2-phenylenevinylpyrrolidone). - Pyrrolidone), N-vinyl-3-methyl-2-pyrrolidone, N-vinyl-4-methyl-2-pyrrolidone, N-vinyl-5-methyl-2-pyrrolidone, N-vinyl-6-methyl-2-pyrrolidone, N-vinyl-3-ethyl-2-pyrrolidone, N-vinyl-4,5-dimethyl-2-pyrrolidone, N-vinyl-5,5-dimethyl-2-pyrrolidone, N-vinyl-3,3,5-trimethyl-2-pyrrolidone, N-vinylpiperidone (also known as N-vinyl-2-piperidone), N-vinyl-3-methyl-2-piperidone, N-vinyl-4-methyl-2-piperidone, N-vinyl-5-methyl-2-piperidone, N-vinyl-6-methyl-2-piperidone, N-vinyl-6-ethyl-2-piperidone, N-vinyl 3,5-Dimethyl-2-piperidinone, N-vinyl-4,4-dimethyl-2-piperidinone, N-vinylcaprolactone (also known as N-vinyl-2-caprolactone), N-vinyl-3-methyl-2-caprolactone, N-vinyl-4-methyl-2-caprolactone, N-vinyl-7-methyl-2-caprolactone, N-vinyl-7-ethyl-2-caprolactone, N-vinyl... N-vinyl-3,5-dimethyl-2-caprolactone, N-vinyl-4,6-dimethyl-2-caprolactone, N-vinyl-3,5,7-trimethyl-2-caprolactone, N-vinyl-N-methylacetamide, N-vinylmethylacetamide, N-vinyl isopropylamide, N-vinyl-N-ethylacetamide, N-vinyl-N-ethylmethylacetamide, and mixtures thereof. Preferably, the N-vinylamide monosystem comprises N-vinylpyrrolidone, N-vinyl-N-methylacetamide, or combinations thereof. Preferred ones contain methylene (=CH) Examples of pyrrolidone monomers include, but are not limited to, 1-methyl-3-methylene-2-pyrrolidone, 1-ethyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 1-ethyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, 5-ethyl-3-methylene-2-pyrrolidone, 1-n-propyl-3-methylene-2-pyrrolidone, 1-n-propyl-5-methylene-2-pyrrolidone, 1-isopropyl-3-methylene-2-pyrrolidone, 1-isopropyl-5-methylene-2-pyrrolidone, 1-n-butyl-3-methylene-2-pyrrolidone, 1-tert-butyl-3-methylene-2-pyrrolidone, and combinations thereof. The better one has C 1-C Examples of 4-alkoxyethoxy acrylic monomers include, but are not limited to, ethylene glycol methyl ether (meth)acrylates, di(ethylene glycol) methyl ether (meth)acrylates, tri(ethylene glycol) methyl ether (meth)acrylates, tetra(ethylene glycol) methyl ether (meth)acrylates, and C64 monomers having a weight average molecular weight of up to 1500. 1-C 4-Alkoxy poly(ethylene glycol) (meth)acrylate, methoxy-poly(ethylene glycol) ethyl (meth)acrylamide having a number average molecular weight of up to 1500, and combinations thereof. Examples of preferred vinyl ether monomers include, but are not limited to, ethylene glycol monovinyl ether, di(ethylene glycol) monovinyl ether, tri(ethylene glycol) monovinyl ether, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, ethylene glycol methyl vinyl ether, di(ethylene glycol) methyl vinyl ether, tri(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, and combinations thereof. Examples of preferred allyl ether monomers include, but are not limited to, allyl alcohols, ethylene glycol monoallyl ethers, di(ethylene glycol) monoallyl ethers, tri(ethylene glycol) monoallyl ethers, tetra(ethylene glycol) monoallyl ethers, poly(ethylene glycol) monoallyl ethers, ethylene glycol methyl allyl ethers, di(ethylene glycol) methyl allyl ethers, tri(ethylene glycol) methyl allyl ethers, tetra(ethylene glycol) methyl allyl ethers, poly(ethylene glycol) methyl allyl ethers, and combinations thereof. Preferred examples of phosphatidylcholine-containing ethylene monomers include, but are not limited to, (meth)propenyloxyethylphosphatidylcholine (also known as MPC), or 2-((meth)propenyloxy)ethyl-2'-(trimethylammonium)ethyl phosphate, (meth)propenyloxypropylphosphatidylcholine (also known as 3-((meth)propenyloxy)propyl-2'-(trimethylammonium)ethyl phosphate), 4-((meth)propenyloxy)butyl-2'-(trimethylammonium)ethyl phosphate, and 2-[(meth)propenylamino]ethyl-2'-(trimethylammonium) 3-[(meth)acrylamide]propyl-2'-(trimethylammonium)ethyl phosphate, 4-[(meth)acrylamide]butyl-2'-(trimethylammonium)ethyl phosphate, 5-((meth)acryloxy)pentyl-2'-(trimethylammonium)ethyl phosphate, 6-((meth)acryloxy)hexyl-2'-(trimethylammonium)-ethyl phosphate, 2-((meth)acryloxy)ethyl-2'-(triethylammonium)ethyl phosphate, 2-((meth)acryloxy)ethyl-2'-(triethylammonium)ethyl phosphate 2-((meth)propenyloxy)ethyl-2'-(trimethylammonium)ethyl phosphate, 2-((meth)propenyloxy)propyl-2'-(trimethylammonium)ethyl phosphate, 2-((meth)propenyloxy)butyl-2'-(trimethylammonium)ethyl phosphate, 2-((meth)propenyloxy)pentyl-2'-(trimethylammonium)ethyl phosphate, 2-((meth)propenyloxy)hexyl-2'-(trimethylammonium)ethyl phosphate, 2-(vinyloxy)ethyl-2'-(trimethylammonium)ethyl phosphate Ammonium-2'-(trimethylammonium-2'-)ethyl phosphate, 2-(vinyloxycarbonyl)ethyl-2'-(trimethylammonium-2'-)ethyl phosphate, 2-(allyloxycarbonyl)ethyl-2'-(trimethylammonium-2'-)ethyl phosphate, 2-(vinylcarbonylamino)ethyl-2'-(trimethylammonium-2'-)ethyl phosphate, 2-(allyloxycarbonylamino)ethyl-2'-(trimethylammonium-2'-)ethyl phosphate, 2-(butenyloxy)ethyl-2'-(trimethylammonium-2'-)ethyl phosphate, and combinations thereof. Various embodiments of hydrophilic polysiloxane vinyl crosslinking agents, carboxyl-containing (meth)acryloxy monomers, non-silicone vinyl crosslinking agents, UV-absorbing vinyl monomers; polymerizable UV / HEVL absorbing compounds; polymerizable photochromic compounds, free radical initiators, other polymerizable components known to be suitable for manufacturing silicone hydrogel contact lenses, and water-soluble and thermally crosslinkable hydrophilic polymer materials for forming non-silicone hydrogel coatings on silicone hydrogel contact lenses are described above and can be used in this aspect of the present invention. The coated silicone hydrogel contact lens of the present invention further has: a balanced water content (i.e., when fully hydrated) of about 20% to about 75% by weight (preferably from about 25% to about 70%, more preferably from about 30% to about 65%); a friction rating of about 3.0 or lower (preferably about 2.5 or lower, more preferably about 2 or lower, and even more preferably about 1.5 or lower); an average water contact angle of about 90 degrees or lower (preferably about 80 degrees or lower, more preferably about 70 degrees or lower, and even more preferably about 60 degrees or lower) by the seat-drop method; or a combination thereof. Although various embodiments of the invention have been described using specific terms, apparatus, and methods, such descriptions are for illustrative purposes only. The terms used are descriptive and not restrictive. As will be apparent to those skilled in the art, many variations and modifications of the invention can be made by those skilled in the art without departing from the spirit and scope of the novel concept disclosed herein. Furthermore, it should be understood that various aspects of the various embodiments of the invention can be interchanged, in whole or in part, or can be combined and / or used in any way, as described below: 1. A method for producing coated silicone hydrogel contact lenses, comprising the steps of: (1) introducing a polymerizable composition into a lens mold, wherein the polymerizable composition comprises (a) at least one hydrophilic polysiloxane ethylene crosslinking agent, (b) hydroxyethyl methacrylate as desired, (c) at least one (meth)acrylic acid C 1-C (2) Alkoxyethyl ester, (d) at least one carboxyl-containing (meth)acryloxy monomer, from about 2% to about 10% by weight relative to the total amount of all polymerizable components, (e) at least one free radical, and (f) at least one solvent selected from the group consisting of water, propylene glycol, polyethylene glycol having a molecular weight of about 400 Daltons or less, and combinations thereof, as needed; (2) thermosetting or photocuring the polymerizable composition in the lens mold to form a silicone hydrogel lens precursor comprising a bulk silicone hydrogel material containing carboxyl groups; (3) hydrating the silicone hydrogel lens precursor obtained in step (2) in water or an aqueous solution, as needed, to obtain a hydrated silicone hydrogel contact lens; and (4) mixing the silicone hydrogel lens precursor obtained in step (2) or step (3) with water. The hydrated silicone hydrogel contact lens obtained therein is directly heated in an aqueous solution having a pH of about 6.8 to about 8.5 and comprising at least one water-soluble, thermally crosslinkable hydrophilic polymer material at a temperature of about 60°C to about 140°C to form a coated silicone hydrogel contact lens comprising the bulk silicone hydrogel material and a layer of crosslinked hydrophilic polymer material covalently attached to the bulk silicone hydrogel material, wherein the coated silicone hydrogel contact lens exhibits a water breakup time (WBUT) of at least about 5 seconds and an oxygen permeability of at least about 50 bar. 2. The method as described in Embodiment 1, wherein the sum of the amounts of components (a) to (e) is at least about 90% by weight relative to the total amount of all polymerizable components in the polymerizable composition. 3. The method of Embodiment 1, wherein the sum of the amounts of components (a) to (e) is at least about 92% by weight relative to the total amount of all polymerizable components in the polymerizable composition. 4. The method of Embodiment 1, wherein the sum of the amounts of components (a) to (e) is at least about 94% by weight relative to the total amount of all polymerizable components in the polymerizable composition, and more preferably at least about 96% by weight. 5. The method of Embodiment 1, wherein the sum of the amounts of components (a) to (e) is at least about 96% by weight relative to the total amount of all polymerizable components in the polymerizable composition. 6. The method of any one of Embodiments 1 to 5, wherein the polymerizable composition comprises component (a) in an amount ranging from about 30% to about 65% by weight relative to the total amount of all polymerizable components. 7. The method of any one of embodiments 1 to 5, wherein the polymerizable composition comprises component (a) in a weight percentage of about 35% to about 60% of the total amount of all polymerizable components. 8. The method of any one of embodiments 1 to 5, wherein the polymerizable composition comprises component (a) in a weight percentage of about 40% to about 60% of the total amount of all polymerizable components.9. The method of any one of embodiments 1 to 8, wherein the polymerizable composition comprises components (b) and (c) in weight of about 30% to about 65% of the total amount of all polymerizable components. 10. The method of any one of embodiments 1 to 8, wherein the polymerizable composition comprises components (b) and (c) in weight of about 35% to about 60% of the total amount of all polymerizable components. 11. The method of any one of embodiments 1 to 8, wherein the polymerizable composition comprises components (b) and (c) in weight of about 40% to about 60% of the total amount of all polymerizable components. 12. The method of any one of embodiments 1 to 11, wherein the polymerizable composition comprises component (d) in weight of about 2% to about 10% of the total amount of all polymerizable components. 13. The method of any one of embodiments 1 to 11, wherein the polymerizable composition comprises component (d) in an amount from about 3% to about 9% by weight relative to the total amount of all polymerizable components. 14. The method of any one of embodiments 1 to 11, wherein the polymerizable composition comprises component (d) in an amount from about 4% to about 8% by weight relative to the total amount of all polymerizable components. 15. The method of any one of embodiments 1 to 14, wherein the weight ratio of component (c) to component (b) in the polymerizable composition is from about 40 to about 20. 16. The method of any one of embodiments 1 to 14, wherein the weight ratio of component (c) to component (b) in the polymerizable composition is from about 35 to about 15. 17. The method of any one of embodiments 1 to 14, wherein the weight ratio of component (c) to component (b) in the polymerizable composition is from about 30 to about 15. 18. The method of any one of embodiments 1 to 17, wherein the polymerizable composition further comprises one or more polymerizable components selected from the group consisting of: (g) a non-silicone ethylene crosslinking agent, (h) a UV-absorbing ethylene monomer, (i) a polymerizable UV / high-energy ultraviolet light absorbing compound, (j) a polymerizable photochromic compound, (k) a polymerizable colorant, and (l) a combination thereof, provided that the sum of components (g) to (l) is less than 10% by weight relative to the amount of all polymerizable components.19. The method of embodiment 18, wherein the polymerizable composition further comprises a non-silicone vinyl crosslinking agent selected from the group consisting of: ethylene glycol di-(meth)acrylate, diethylene glycol di-(meth)acrylate, triethylene glycol di-(meth)acrylate, tetraethylene glycol di-(meth)acrylate, polyethylene glycol di-(meth)acrylate having a number average molecular weight of 200 to 10,000 Daltons, glycerol di-(meth)acrylate, 1,3-propanediol Di-(meth)acrylate, 1,3-butanediol di-(meth)acrylate, 1,4-butanediol di-(meth)acrylate, glycerol 1,3-diglyceride di-(meth)acrylate, ethyl bis[oxy(2-hydroxypropane-1,3-diyl)] di-(meth)acrylate, bis[2-(meth)acryloxyethyl]phosphate, trimethylolpropane di-(meth)acrylate, and 3,4-bis[(meth)acrylyl]tetrahydrofuran, diacrylamide ( That is, N-(1-sideoxy-2-propenyl)-2-propenylamine), dimethylpropenylamine (i.e., N-(1-sideoxy-2-methyl-2-propenyl)-2-methyl-2-propenylamine), N,N-di(meth)propenyl-N-methylamine, N,N-di(meth)propenyl-N-ethylamine, N,N'-methylenebis(meth)propenylamine, N,N'-ethylbis(meth)propenylamine, N,N'-dihydroxyethylbis(meth)propenylamine, N... N,N'-propylpropylbis(meth)acrylamide, N,N'-2-hydroxypropylpropylbis(meth)acrylamide, N,N'-2,3-dihydroxypropylbutylbis(meth)acrylamide, 1,3-bis(meth)acrylamide-propane-2-yl dihydrophosphate (i.e., N,N'-2-phosphatidylinosylpropylpropylbis(meth)acrylamide), piperidine diacrylamide (or 1,4-bis(meth)acrylyl piperidine), triallyl isocyanurate, triallyl cyanurate, and combinations thereof. 20. The method of embodiment 19, wherein the non-silicone ethylene crosslinking agent is selected from the group consisting of: ethylene glycol di-(meth)acrylate, diethylene glycol di-(meth)acrylate, triethylene glycol di-(meth)acrylate, tetraethylene glycol di-(meth)acrylate, polyethylene glycol di-(meth)acrylate having a number average molecular weight of 200 to 10,000 Daltons, and combinations thereof. 21. The method of any one of embodiments 1 to 20, wherein the heating step is preferably performed by autoclaving the silicone hydrogel lens pre-substrate to be immersed in a packaging solution (i.e., a buffered aqueous solution) in a sealed lens package at a temperature of about 115°C to about 125°C for about 20-90 minutes.22. The method of any one of embodiments 1 to 21, wherein the at least one water-soluble and thermally crosslinkable hydrophilic polymer material comprises azacyclobutaneonium groups, epoxy groups, or combinations thereof. 23. The method of embodiment 22, wherein the at least one water-soluble and thermally crosslinkable hydrophilic polymer material has a three-dimensional network and thermally crosslinkable groups within or attached to the network. 24. The method of embodiment 22, wherein the at least one water-soluble and thermally crosslinkable hydrophilic polymer material is: one or more multi-arm polyethylene glycols each having a terminal epoxy group; a mixture of multi-arm polyethylene glycols having terminal epoxy groups and one or more polyethylene glycols each having a terminal functional group selected from the group consisting of primary amine groups, secondary amine groups, carboxyl groups, thiol groups, and combinations thereof; a partial reaction product of multi-arm polyethylene having terminal epoxy groups and a hydrophilic reinforcing agent having at least one reactive functional group selected from the group consisting of amine groups, carboxyl groups, and thiol groups; or combinations thereof. 25. The method of embodiment 22, wherein the at least one water-soluble and thermally crosslinkable hydrophilic polymer material comprises a nitrogen-containing butanetonium group and is a partial reaction product of a nitrogen-containing butanetonium polymer and a hydrophilicity enhancer having at least one reactive functional group selected from the group consisting of primary amine groups, secondary amine groups, carboxyl groups, thiol groups, and combinations thereof. 26. The method of embodiment 25, wherein the nitrogen-containing butanetonium polymer is a poly(2-azoline-co-ethyleneimine)-epimyl chloride copolymer, a polyamide-epimyl chloride, a copolymer of a nitrogen-containing butanetonium ethylene monomer and one or more hydrophilic ethylene monomers, or a combination thereof. 27. The method of embodiment 25 or 26, wherein the hydrophilicity enhancer is: a monosaccharide containing a primary amino group, a secondary amino group, a carboxyl group, or a thiol group; a disaccharide containing a primary amino group, a secondary amino group, a carboxyl group, or a thiol group; an oligosaccharide containing a primary amino group, a secondary amino group, a carboxyl group, or a thiol group; or a combination thereof. 28. The method of embodiment 25 or 26, wherein the hydrophilicity enhancer is a hydrophilic polymer having one or more primary or secondary amino groups, one or more carboxyl groups, one or more thiol groups, or a combination thereof. 29. The method of embodiment 28, wherein the hydrophilicity enhancer is a polysaccharide having a primary amino group, a secondary amino group, a carboxyl group, or a combination thereof. 30. The method of embodiment 28, wherein the hydrophilicity enhancer has a unique -NH group. 2. Poly(ethylene glycol) with -SH or -COOH functional groups; having two selectable groups from -NH 2. Poly(ethylene glycol) with terminal functional groups of -COOH, -SH, and combinations thereof; having one or more functional groups selected from -NH 2. Multi-arm poly(ethylene glycol) with functional groups of -COOH, -SH, and combinations thereof; homopolymers or copolymers of non-reactive hydrophilic vinyl monomers with monoamine, monocarboxyl, diamine, or dicarboxyl-terminated groups; copolymers which are polymers comprising: (1) a reactive vinyl monomer from about 0.1% to about 30% (preferably from about 0.5% to about 20%, more preferably from about 1% to about 15%), and (2) at least one non-reactive hydrophilic vinyl monomer, wherein the reactive vinyl monomer system has vinyl monomers with functional groups selected from the group consisting of carboxyl, primary amine, and secondary amine groups, wherein the non-reactive hydrophilic monomer system does not contain any hydrophilic vinyl monomers with carboxyl, primary amine, secondary amine, epoxy, isocyanate, acrylonitrile, or aziridine groups. 31. The method as described in Embodiment 30, wherein the reactive vinyl monopolymer is composed of acrylic acid, methacrylic acid, ethylacrylic acid, 2-(meth)acrylaminoglycolic acid, N-2-aminoethyl(meth)acrylamine, N-2-methylaminoethyl(meth)acrylamine, N-2-ethylaminoethyl(meth)acrylamine, N-3-aminopropyl(meth)acrylamine, N-3-methylaminopropyl(meth)acrylamine, 2-aminoethyl(meth)acrylate, 2-methylaminoethyl(meth)acrylate, 2-ethylaminoethyl(meth)acrylate, 3-aminopropyl(meth)acrylate, 3-methylaminopropyl(meth)acrylate, 3-amino-2-hydroxypropyl(meth)acrylate, or combinations thereof. The non-reactive hydrophilic ethylene monomer is selected from the group consisting of: (meth)acryloxyethylphosphocholine, (meth)acryloxypropylphosphocholine, 4-((meth)acryloxy)butyl-2'-(trimethylammonium)ethyl phosphate, 2-[(meth)acrylamino]ethyl-2'-(trimethylammonium)ethyl phosphate, 3-[(meth)acrylamino]propyl-2'-(trimethylammonium)ethyl phosphate, 4-[(meth)acrylamino]butyl-2'-(trimethylammonium)ethyl phosphate, (meth)acrylamide, dimethyl(meth)acrylamide, N-2-hydroxyethyl(meth)acrylamide, N,N-bis(hydroxyethyl)(meth)acrylamide, N-2,3-dihydroxypropyl(meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, glyceryl methacrylate (GMA), tetra(ethylene glycol)(meth)acrylate, poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, N-vinylmethylamine, N-vinylacetamide, 1-methyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, tetra(ethylene glycol)methyl ether(meth)acrylate, methoxy poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, C with a weight average molecular weight up to 1500 1-C 4-Alkoxy polyethylene glycol (meth)acrylate, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) monoallyl ether, poly(ethylene glycol) monoallyl ether, tetra(ethylene glycol) methyl allyl ether, poly(ethylene glycol) methyl allyl ether, vinyl alcohol, allyl alcohol, and combinations thereof. 32. The method as described in any one of embodiments 1 to 31, wherein the aqueous solution has a pH from about 7.0 to about 8.2, and wherein the aqueous solution contains, by weight, at least one of the aforementioned water-soluble and thermally crosslinkable hydrophilic polymeric materials from about 0.01% to about 2% (preferably from about 0.05% to about 1.5%, more preferably from about 0.1% to about 1%, and even more preferably from about 0.2% to about 0.5%). 33. The method of any one of Embodiments 1 to 31, wherein the aqueous solution has a pH of about 7.2 to about 8.0, and wherein the aqueous solution contains, by weight, at least one water-soluble and thermally crosslinkable hydrophilic polymer material of the aforementioned, from about 0.01% to about 2% (preferably from about 0.05% to about 1.5%, more preferably from about 0.1% to about 1%, and even more preferably from about 0.2% to about 0.5%). 34. The method of any one of Embodiments 1 to 33, wherein the aqueous solution contains a mixture of a monohydrogen phosphate and a dihydrogen phosphate to maintain the pH of the aqueous solution, wherein the total concentration of the monohydrogen phosphate and the dihydrogen phosphate is at least 30 mM. 35. The method of Embodiment 34, wherein the total concentration of the monohydrogen phosphate and the dihydrogen phosphate is at least 35 mM. 36. The method of embodiment 34, wherein the total concentration of the monohydrogen phosphate and the dihydrogen phosphate is at least 40 mM. 37. The method of embodiment 34, wherein the total concentration of the monohydrogen phosphate and the dihydrogen phosphate is at least 45 mM. 38. The method of any one of embodiments 1 to 37, wherein the tensile strength of the aqueous solution is adjusted to about 200 to about 450 milliosmol (mOsm), wherein the aqueous solution contains one or more organic tensile agents selected from the group consisting of glycerol, propylene glycol, polyethylene glycol having a number average molecular weight of 200 to 800 Daltons, mannitol, sorbitol, xylitol, and mixtures thereof, wherein the total concentration of the one or more organic tensile agents is at least 70 mM. 39. The method of embodiment 38, wherein the total concentration of the one or more organic tensile agents is at least 90 mM. 40. The method as described in Embodiment 38, wherein the total concentration of the one or more organic tensile agents is at least 110 mM. 41. The method as described in Embodiment 38, wherein the total concentration of the one or more organic tensile agents is at least 130 mM.42. A coated silicone hydrogel contact lens comprising: a bulk silicone hydrogel material; and a layer of non-silicone hydrogel material thereon, wherein the bulk silicone hydrogel material comprises (a) repeating units of at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) repeating units of hydroxyethyl methacrylate as desired (but preferably), and (c) at least one (meth)acrylic acid C. 1-C (d) a repeating unit of 2-alkoxyethyl ester, and (e) a repeating unit of at least one carboxyl-containing (meth)acryloxy monomer, and (f) a repeating unit of at least one polymerizable component selected from the group consisting of: non-silicone vinyl crosslinking agents, UV-absorbing vinyl monomers, polymerizable UV / high-energy ultraviolet light absorbing compounds, polymerizable photochromic compounds, polymerizable colorants, and combinations thereof, provided that the amount of component (e) is less than 10% by weight relative to the total weight of the bulk silicone hydrogel material in a dry state, wherein the layer of the non-silicone hydrogel material is covalently attached to the bulk silicone hydrogel material by the carboxyl groups of the repeating unit containing the carboxyl groups, wherein the silicone hydrogel contact lens has a water breakup time (WBUT) of at least 5 seconds, an oxygen permeability (Dk) of at least 50 bar, and an elastic modulus from about 0.2 MPa to about 1.8 MPa. 43. A coated silicone hydrogel contact lens as described in Embodiment 42 or a method as described in any one of Embodiments 1 to 41, wherein the coated silicone hydrogel contact lens has a water breakup time (WBUT) of at least about 10 seconds. 44. A coated silicone hydrogel contact lens as described in Embodiment 42 or a method as described in any one of Embodiments 1 to 41, wherein the coated silicone hydrogel contact lens has a water breakup time (WBUT) of at least about 15 seconds. 45. A coated silicone hydrogel contact lens as described in Embodiment 42 or a method as described in any one of Embodiments 1 to 41, wherein the coated silicone hydrogel contact lens has a water breakup time (WBUT) of at least about 20 seconds. 46. A coated silicone hydrogel contact lens as described in any one of Embodiments 42 to 45 or a method as described in any one of Embodiments 1 to 41 and 43 to 45, wherein the coated silicone hydrogel contact lens has an oxygen permeability (Dk) of at least about 60 bar. 47. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 45, or a method as described in any one of embodiments 1 to 41 and 43 to 45, wherein the coated silicone hydrogel contact lens has an oxygen permeability (Dk) of at least about 70 bar. 48. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 45, or a method as described in any one of embodiments 1 to 41 and 43 to 45, wherein the coated silicone hydrogel contact lens has an oxygen permeability (Dk) of at least about 80 bar. 49. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 48, or a method as described in any one of embodiments 1 to 41 and 43 to 48, wherein the coated silicone hydrogel contact lens has an elastic modulus from about 0.2 MPa to about 1.5 MPa.50. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 48, or a method as described in any one of embodiments 1 to 41 and 43 to 48, wherein the coated silicone hydrogel contact lens has an elastic modulus from about 0.3 MPa to about 1.2 MPa. 51. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 48, or a method as described in any one of embodiments 1 to 41 and 43 to 48, wherein the coated silicone hydrogel contact lens has an elastic modulus from about 0.4 MPa to about 1.0 MPa. 52. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 51, or a method as described in any one of embodiments 1 to 41 and 43 to 51, wherein the coated silicone hydrogel contact lens has an equilibrium water content from about 20% to about 75% by weight (i.e., when fully hydrated). 53. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 51, or a method as described in any one of embodiments 1 to 41 and 43 to 51, wherein the coated silicone hydrogel contact lens has an equilibrium water content of about 25% to about 70% by weight (i.e., when fully hydrated). 54. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 51, or a method as described in any one of embodiments 1 to 41 and 43 to 51, wherein the coated silicone hydrogel contact lens has an equilibrium water content of about 30% to about 65% by weight (i.e., when fully hydrated). 55. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 54, or a method as described in any one of embodiments 1 to 41 and 43 to 54, wherein the coated silicone hydrogel contact lens has a friction rating of about 3.0 or lower. 56. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 54, or a method as described in any one of embodiments 1 to 41 and 43 to 54, wherein the coated silicone hydrogel contact lens has a friction rating of about 2.5 or lower. 57. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 54, or a method as described in any one of embodiments 1 to 41 and 43 to 54, wherein the coated silicone hydrogel contact lens has a friction rating of about 2 or lower. 58. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 54, or a method as described in any one of embodiments 1 to 41 and 43 to 54, wherein the coated silicone hydrogel contact lens has a friction rating of about 1.5 or lower. 59. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 58 or a method as described in any one of embodiments 1 to 41 and 43 to 58, wherein the coated silicone hydrogel contact lens has an average water contact angle of about 90 degrees or less by means of a seated drop method.60. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 58, or a method as described in any one of embodiments 1 to 41 and 43 to 58, wherein the coated silicone hydrogel contact lens has an average water contact angle of about 80 degrees or less by the seat drop method. 61. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 58, or a method as described in any one of embodiments 1 to 41 and 43 to 58, wherein the coated silicone hydrogel contact lens has an average water contact angle of about 70 degrees or less, or even more preferably about 60 degrees or less, by the seat drop method. 62. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 58, or a method as described in any one of embodiments 1 to 41 and 43 to 58, wherein the coated silicone hydrogel contact lens has an average water contact angle of about 60 degrees or less by the seat drop method. 63. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 62 or a method as described in any one of embodiments 1 to 41 and 43 to 62, wherein the at least one hydrophilic polysiloxane ethylene crosslinking agent comprises at least about 1.50 milliequivalents / gram ("meq / g") of hydrophilic portion, preferably hydroxyl (-OH), carboxyl (-COOH), or amino (-NHR). N1 , where R N1 H or C 1-C 2-alkyl), amide moiety (-CO-NR) N1 R N2 , where R N1 H or C 1-C 2 alkyl and R N2 It is a covalent bond, H, or C 1-C 2-alkyl), NC 1-C 3. Acrylamino group, urethane moiety (-NH-CO-O-), urea moiety (-NH-CO-NH-) polyethylene glycol chains (where n is an integer from 2 to 20 and T) 64. A coated silicone hydrogel contact lens or method as described in Embodiment 63, wherein the at least one hydrophilic polysiloxane ethylene crosslinking agent comprises at least about 2.0 meq / g of hydrophilic portion. 65. A coated silicone hydrogel contact lens or method as described in Embodiment 63, wherein the at least one hydrophilic polysiloxane ethylene crosslinking agent comprises at least about 2.5 meq / g of hydrophilic portion. 66. A coated silicone hydrogel contact lens or method as described in Embodiment 63, wherein the at least one hydrophilic polysiloxane ethylene crosslinking agent comprises at least about 3.0 meq / g of hydrophilic portion. 67. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 66, or a method as described in any one of embodiments 1 to 41 and 43 to 66, wherein the at least one hydrophilic polysiloxane-ethylene crosslinking agent comprises (1) a dimethylsiloxane unit and each having a methyl substituent and a monovalent C having 2 to 6 hydroxyl groups. 4-C 40 The polysiloxane segment of the hydrophilic silicone unit with organic substituents, and (2) two terminal (meth)acrylic groups. 68. A coated silicone hydrogel contact lens or method as described in embodiment 67, wherein the at least one hydrophilic polysiloxane ethylene crosslinking agent comprises a polysiloxane ethylene crosslinking agent of formula (1). Where: υ1 is an integer from 30 to 500 and ω1 is an integer from 1 to 75, provided that ω1 / υ1 is from approximately 0.035 to approximately 0.15; X 01 System O or NR n , where R n Hydrogen or C 1-C 10 -alkyl; R o It is a hydrogen or methyl group; R 2 and R 3. C that are either substituted or unsubstituted, independent of each other. 1-C 10 alkyl divalent groups or -R 5-OR 6-divalent group, wherein R 5 and R 6. C that are either substituted or unsubstituted, independent of each other. 1-C 10 alkyl divalent group; R Monovalent groups of any one of the four formulas (2) to (7) p1 represents zero or 1; m1 represents integers from 2 to 4; m2 represents integers from 1 to 5; m3 represents integers from 3 to 6; m4 represents integers from 2 to 5; R 7-series hydrogen or methyl; R The 8-series C has a oxidation state of (m² + 1). 2-C 6 hydrocarbon group; R The 9-series C has a oxidation state of (m⁴ + 1). 2-C 6 hydrocarbon group; R 10 It is ethyl or hydroxymethyl; R 11 It is either methyl or hydroxymethyl; R 12 Hydroxyl or methoxy group; X 3-series -S-sulfide bonds or -NR 13 - a tertiary amino bond, where R 13 C 1-C 1. Alkyl, hydroxyethyl, hydroxypropyl, or 2,3-dihydroxypropyl; X 4 series or The amide bond, in which R 14 Hydrogen or C 1-C 10 Alkyl; L PC Tie , , , , ,or divalent groups, where q1 is an integer from 1 to 20, R 15 Straight or branched C 1-C 10 alkyl divalent group, R 16 Straight or branched C 3-C 10 alkyl divalent groups, and R 17 C is a direct bond, a straight chain, or a branch. 1-C 4. An alkyl divalent group. 69. A coated silicone hydrogel contact lens or method as described in Example 68, wherein, in formula (1), R Monovalent groups of any one of the four formulas (2a) to (2y) Where p1 is zero or 1, m1 is an integer from 2 to 4, and R 70. A coated silicone hydrogel contact lens or method as described in embodiment 68, wherein, in formula (1), R Monovalent groups of any one of the four series formulas (3a) to (3y) , where X 4 series or The amide bond, in which R 14 Hydrogen or C 1-C 10 Alkyl group. 71. The coated silicone hydrogel contact lens or method as described in embodiment 68, wherein, in formula (1), R Monovalent groups of the 4-series formula (4a) or (4b) 72. The coated silicone hydrogel contact lens or method as described in embodiment 68, wherein, in formula (1), R Monovalent groups of any one of the four series formulas (5a) or (5c). 73. The coated silicone hydrogel contact lens or method as described in embodiment 68, wherein, in formula (1), R The monovalent groups of the 4-series formula (6), wherein m1 is 3, p1 is 1, and R 74. The coated silicone hydrogel contact lens or method as described in Embodiment 68, wherein, in formula (1), R The monovalent group of the 4-series formula (7), wherein L PC Tie 75. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 74, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising at least 25% (preferably at least 35% by moles, more preferably at least 45% by moles, and even more preferably at least 55% by moles) of at least one repeating monomer unit of a hydrophilic vinyl monomer selected from the group consisting of: N,N-dimethyl(meth)acrylamide, N-ethyl(meth)acrylamide, N,N-di ... N-propylmethacrylamide, N-isopropylmethacrylamide, N-3-methoxypropylmethacrylamide, N-2-dimethylaminoethylmethacrylamide, dimethylaminoethyl methacrylate, N-2-hydroxyethylmethacrylamide, N,N-bis(hydroxyethyl)methacrylamide, N-3-hydroxypropylmethacrylamide, N-2-hydroxypropylmethacrylamide, N-2,3-dihydroxypropylmethacrylamide N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, 3-hydroxypropyl(meth)acrylate, 2-hydroxypropyl(meth)acrylate, glyceryl methacrylate (GMA), di(ethylene glycol)(meth)acrylate, tri(ethylene glycol)(meth)acrylate, tetra(ethylene glycol)(meth)acrylate, poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, and the highest Number average molecular weights of poly(ethylene glycol) ethyl(meth)acrylamide, N-vinylpyrrolidone, N-vinyl-3-methyl-2-pyrrolidone, N-vinyl-4-methyl-2-pyrrolidone, N-vinyl-5-methyl-2-pyrrolidone, N-vinyl-6-methyl-2-pyrrolidone, N-vinyl-3-ethyl-2-pyrrolidone, N-vinyl-4,5-dimethyl-2-pyrrolidone, N-ethylene Alkenyl-5,5-dimethyl-2-pyrrolidone, N-vinyl-3,3,5-trimethyl-2-pyrrolidone, N-vinylpiperidone, N-vinyl-3-methyl-2-piperidone, N-vinyl-4-methyl-2-piperidone, N-vinyl-5-methyl-2-piperidone, N-vinyl-6-methyl-2-piperidone, N-vinyl-6-ethyl-2-piperidone, N-vinyl-3,5-dimethyl-2-piperidone N-vinyl-4,4-dimethyl-2-piperidinone, N-vinylcaprolactone, N-vinyl-3-methyl-2-caprolactone, N-vinyl-4-methyl-2-caprolactone, N-vinyl-7-methyl-2-caprolactone, N-vinyl-7-ethyl-2-caprolactone, N-vinyl-3,5-dimethyl-2-caprolactone, N-vinyl-4,6-dimethyl-2-caprolactone, N-vinyl-3,5,7-Trimethyl-2-caprolactam, N-vinyl-N-methylacetamide, N-vinylmethamide, N-vinylacetamide, N-vinylisopropylamine, N-vinyl-N-ethylacetamide, N-vinyl-N-ethylmethamide, 1-methyl-3-methylene-2-pyrrolidone, 1-ethyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 1-ethyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, 5-ethyl-3-methylene-2-pyrrolidone, 1-n-propyl- 3-Methylene-2-pyrrolidone, 1-n-propyl-5-methylene-2-pyrrolidone, 1-isopropyl-3-methylene-2-pyrrolidone, 1-isopropyl-5-methylene-2-pyrrolidone, 1-n-butyl-3-methylene-2-pyrrolidone, 1-tributyl-3-methylene-2-pyrrolidone, ethylene glycol methyl ether (meth)acrylate, di(ethylene glycol) methyl ether (meth)acrylate, tri(ethylene glycol) methyl ether (meth)acrylate, tetra(ethylene glycol) methyl ether (meth)acrylate, C with a weight average molecular weight up to 1500, 1-C 4-Alkoxy poly(ethylene glycol) (meth)acrylate, methoxy-poly(ethylene glycol)ethyl (meth)acrylamide having a number average molecular weight of up to 1500, ethylene glycol monovinyl ether, di(ethylene glycol) monovinyl ether, tri(ethylene glycol) monovinyl ether, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, ethylene glycol methyl vinyl ether, di(ethylene glycol) methyl vinyl ether, tri(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, and combinations thereof. 76. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 74, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising at least 25% (preferably at least 35% by moles, more preferably at least 45% by moles, and even more preferably at least 55% by moles) of at least one repeating monomer unit of a hydrophilic vinyl monomer selected from the group consisting of: (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl)(meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl(meth)acrylate, glyceryl methacrylate (GMA), tetra(ethylene glycol)(meth)acrylate, poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, N-vinylmethylamine, N-vinylacetamide, 1-methyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, tetra(ethylene glycol)methyl ether(meth)acrylate, methoxy poly(ethylene glycol)ethyl(meth)acrylamide with a number average molecular weight up to 1500, C with a weight average molecular weight up to 1500 1-C 4-Alkoxy polyethylene glycol (meth)acrylate, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) monoallyl ether, poly(ethylene glycol) monoallyl ether, tetra(ethylene glycol) methyl allyl ether, poly(ethylene glycol) methyl allyl ether, vinyl alcohol, allyl alcohol, and combinations thereof. 77. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 74, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising at least 25% (preferably at least 35% by moles, more preferably at least 45% by moles, and even more preferably at least 55% by moles) of at least one repeating monomer unit of a hydrophilic vinyl monomer selected from the group consisting of: (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl)(meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl(meth)acrylamide, 2-hydroxyethyl (meth)acrylate, glyceryl methacrylate (GMA), poly(ethylene glycol) ethyl(meth)acrylamide having a number average molecular weight of up to 1500, poly(ethylene glycol)(meth)acrylate having a number average molecular weight of up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, methoxypoly(ethylene glycol) ethyl(meth)acrylamide having a number average molecular weight of up to 1500, methoxypoly(ethylene glycol)(meth)acrylate having a weight average molecular weight of up to 1500, poly(ethylene glycol) monovinyl ether, poly(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) monoallyl ether, poly(ethylene glycol) methyl allyl ether, vinyl alcohol, allyl alcohol, and combinations thereof. 78. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 74, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising at least 25% (preferably at least 35% by moles, more preferably at least 45% by moles, and even more preferably at least 55% by moles) of at least one repeating monomer unit of a hydrophilic vinyl monomer selected from the group consisting of: (meth)acrylamide, dimethyl (meth)acrylamide, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl)(meth)acrylamide, N-2,3-dihydroxypropyl (meth)acrylamide, N-tris(hydroxymethyl)methyl(meth)acrylamide, poly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, poly(ethylene glycol)(meth)acrylate having a number average molecular weight of up to 1500, N-vinylpyrrolidone, N-vinyl-N-methylacetamide, methoxypoly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, methoxypolyethylene glycol(meth)acrylate having a weight average molecular weight of up to 1500, and combinations thereof. 79. The coated silicone hydrogel contact lens as described in any one of embodiments 42 to 78, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising at least 25% (preferably at least 35% by mole, more preferably at least 45% by mole, and even more preferably at least 55% by mole) repeating monomer units of at least one phosphatidylcholine-containing vinyl monomer. 80. The coated silicone hydrogel contact lens as described in Embodiment 79, wherein the at least one phosphatidylcholine-containing ethylene monomer is selected from the group consisting of: (meth)propenyloxyethylphosphatidylcholine, (meth)propenyloxypropylphosphatidylcholine, 4-((meth)propenyloxy)butyl-2'-(trimethylammonium)ethyl phosphate, 2-[(meth)propenylamino]-ethyl-2'-(trimethylammonium)ethyl phosphate, 3-[(meth)propenylamino]propyl-2'-(trimethylammonium)ethyl phosphate, 4-[(meth)propenylamino]butyl-2'-(trimethylammonium)ethyl phosphate, and combinations thereof. 81. A coated silicone hydrogel contact lens as described in any one of embodiments 42 to 80, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising a poly(ethylene glycol) chain. 82. A coated silicone hydrogel contact lens as described in embodiment 81, wherein the poly(ethylene glycol) chain is directly derived from (a) having a unique -NH... 2. Poly(ethylene glycol) with -SH or -COOH functional groups, (b) having two groups selected from -NH 2. Poly(ethylene glycol) with terminal functional groups of -COOH, -SH, and combinations thereof, (c) having one or more of the following selected from -NH 2. Multi-arm poly(ethylene glycol) with functional groups consisting of -COOH, -SH, and combinations thereof, and (d) combinations thereof. The above disclosure will enable those skilled in the art to practice this invention. Various modifications, variations, and combinations can be made to the various embodiments described herein. To enable the reader to better understand the specific embodiments and advantages, reference is recommended to the following examples. It is intended that this specification and examples be considered exemplary. Example 1 Oxygen permeability measurement Unless otherwise specified, determine the oxygen permeability (Dk / t) and inherent (or edge-corrected) oxygen permeability (Dk) of the lens and lens material according to the procedure described in ISO 18369-4. i or Dk c ). Water breakage time ( WBUT )test The surface hydrophilicity of the lens (after autoclaving) is assessed by determining the time required for the water film on the lens surface to begin to break down, according to the procedure described in Example 1 of U.S. Patent Application Publication No. 20210181379 A1. Balanced water content The equilibrium water content (EWC) of the contact lens was determined according to the procedure described in Example 1 of U.S. Patent Application Publication No. 20210181379 A1. elastic modulus The elastic modulus of the contact lens was determined according to the procedure described in Example 1 of U.S. Patent Application Publication No. 20210181379 A1. Light transmittance The contact lens is manually placed in a specially manufactured sample holder or similar device that maintains the shape of the lens as if it were placed on the eye. This holder is then immersed in a quartz cell with a 1 cm path length containing phosphate-buffered saline (PBS, pH approximately 7.0–7.4) as a reference. A UV / visible spectrophotometer, such as a Varian Cary 3E UV-Vis spectrophotometer with a LabSphere DRA-CA-302 beam splitter or similar, can be used in this measurement. Percentage transmittance spectra are collected in the wavelength range of 250–800 nm, with %T values collected at 0.5 nm intervals. The light transmittance of the contact lens is the average % transmittance between 400 nm and 700 nm. Water contact angle ( WCA Measurements were taken using a DSA 10 droplet shape analysis system from Krüss GmbH, Germany, with pure water (Fluka, surface tension 72.5 mN / m at 20°C) via the seated drop method. For measurement purposes, the contact lens was removed from the storage solution using tweezers, and excess solution was removed by gentle shaking. The contact lens was placed on the anode of the lens mold and gently blotted dry with a clean cloth. A water droplet (approximately 1 µl) was then added to the apex of the lens, and the change in the contact angle of the droplet over time (WCA(t), circular fitting model) was monitored. WCA was calculated by extrapolating the curve WCA(t) to t = 0. Determining the diameter of hydrated contact lenses The lens diameter of the hydrated contact lens is determined according to the procedure described in Example 1 of U.S. Patent Application Publication No. 20210181379 A1. Lubricity assessment. The lubricity of contact lenses is evaluated using a finger-feel lubricity test, which qualitatively characterizes the smoothness of the lens surface on a friction scale from 0 to 4. The higher the friction scale, the lower the smoothness (or lubricity). Commercial lenses: DAILIES® TOTAL1®; ACUVUE® OASYS TM ACUVUE® ADVANCE PLUS TM The DAILIES® Aqua Comfort Plus® and AIR OPTIX® lenses are assigned abrasion ratings (hereinafter referred to as "FR") of 0, 1, 2, 3, and 4, respectively. They are used as standard lenses to determine the abrasion rating of the lens being tested. Rinse samples in PBS for at least two 30-minute washes, then transfer to fresh PBS for evaluation. Before evaluation, wash hands with soap, rinse thoroughly with DI water, and dry with a KimWipe® towel. Process the samples between your fingers and assign values to each sample relative to the standard lenses described above. For example, if a lens is determined to be only slightly better than AIR OPTIX... ® Lenses, then they are assigned the number 3. The value of the friction rating is obtained by averaging the results of at least two friction ratings of contact lenses by two or more individuals and / or by averaging the friction ratings of two or more contact lenses (from the same batch of lens production) by one person. The finger lubricity (i.e., friction level) of the contact lens can be determined directly out-of-pack (OOP) according to the procedure described above, but after soaking in PBS for ≥ 30 min. chemicals The following abbreviations are used in the following examples: HEMA represents hydroxyethyl methacrylate; EOEMA represents ethoxyethyl methacrylate; MAA represents methacrylic acid; AA represents acrylic acid; PEG-DA represents poly(ethylene glycol) diacrylate (Mn ~ 800 g / mol); PG represents propylene glycol; Vazo 52 represents 2,2'-azobis(2,4-dimethylpentanonitrile); Vazo 67 represents 2,2'-azobis(2-methylbutanonitrile); Perkadox 16 represents bis(4-tert-butylcyclohexyl)peroxydicarbonate; MPC represents 2-methacryloxyethylphosphocholine; EGMA represents 2-methoxyethyl methacrylate; AMA represents allyl methacrylate; TEGDMA represents tris(ethylene glycol)di-methacrylate; TEGDVE is tris(ethylene glycol)divinyl ether; Nobloc is 2-[3-(2H-benzotriazol-2-yl)-5-hydroxyphenyl]ethyl methacrylate; RB247 is Reactive Blue 247; PBS represents phosphate-buffered saline with a pH of 7.2 ± 0.2 at 25°C and containing approximately 0.044 wt.% NaH. 2PO 4·H 2O, about 0.388 wt.% Na 2HPO 4.2H 2O and approximately 0.79 wt.% NaCl, where wt.% indicates weight percentage; HO-PDMS-MA indicates glycidyl methacrylate and The reaction products, where n = 4-10; "G2" macromonomer represented by formula (A) is a di-methacryloxypropyl-terminated polysiloxane (Mn ~ 8K g / mol, OH content ~ 3.5 meq / g). Example 2 Phosphate buffered saline (PBR) PBS ) Phosphate buffered saline is prepared by the following method: NaH 2PO 4•H 2O, Na 2HPO 4•2H 2O and NaCl are dissolved in a given volume of purified water (distilled or deionized) to have the following composition: approximately 0.044 w / w% NaH 2PO 4•H 2O, approximately 0.388 w / w / % Na 2HPO 4•2H 2O, and approximately 0.79 w / w% NaCl. Packaged saline - brine -1 Preparation Copolymer 845 series N-vinylpyrrolidone and dimethylaminoethyl methacrylate (M w ~ 700,000 - 1,200,000 g / mol, by comparing GPC with polyethylene oxide standards, M w / M n The copolymer (~ 5.7 - 8.5) was obtained from ISP. (CH) 3O(EO) 45 (BO) 10 The poly(ethylene glycol)-poly(butanediol) block copolymer was prepared according to the procedure described in US 8318144. The packaged brine is prepared by dissolving all components in 1 L of water to have the following composition: 0.77% NaCl by weight; 0.076% NaH by weight. 2PO 4H 2O; 0.47% Na by weight 2HPO 47H 2O; 1.0% by weight copolymer-845; and 0.015% by weight CH 3O(EO) 45 (BO) 10 . Inner coating of brine - IPC-1 Preparation IPC brine (IPC-1) was prepared by mixing an appropriate amount of poly(AAm-co-AA) or other wetting agent with PAE in phosphate-buffered saline and pretreating at a temperature for a desired time. The sodium salt of poly(AAm-co-AA) (90 / 10) (poly(AAm-co-AA) 90 / 10, Mw 200,000) was purchased from Polysciences, Inc. and used as received. Kymene or PAE solutions of varying solids content were purchased as aqueous solutions from Solenis and used as received. 0.07% PAAm-PAA and approximately 0.1% Kymene were mixed in PBS and pretreated at 60°C for approximately 6 hours. After heat pretreatment, the IPC brine was filtered through a 0.22-micron membrane filter and cooled to room temperature. 5 ppm hydrogen peroxide can be added to the final IPC brine to prevent bioburden growth, and the IPC brine can be filtered using a 0.22 micron membrane filter. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 1. [Table 1] These formulations were prepared by adding the listed components to a clean bottle in the target amounts and mixing with a stir bar at 600 rpm for 30 minutes at room temperature. After all solids were dissolved, the formulation was filtered using a 2.7 µm glass microfiber (GMF) filter. Cast-molded silicone hydrogel contact lenses Purge the lens preparation with nitrogen gas for 30 to 35 minutes at room temperature. 2. The purged lens formulation is introduced into a polypropylene mold and thermo-cured in an oven under nitrogen under the following curing conditions: gradually decreasing from room temperature to 55°C at a ramp rate of about 7°C / min; holding at 55°C for about 30 minutes; gradually decreasing from 55°C to 80°C at a ramp rate of about 7°C / min; holding at 80°C for about 30 minutes; gradually decreasing from 80°C to 100°C at a ramp rate of about 7°C / min; and holding at 100°C for about 30 minutes. The mold is then opened and the molded lens is removed from the mold. The lenses were then hydrated in packaged saline for 30 minutes, inspected, and packaged in glass vials in packaged saline for sterilization (autoclaving at 121°C for 45 minutes). Lens characteristics are listed in Table 2. [Table 2] *Dry lenses: SiHy lens pre-processed. OOP indicates outer packaging. Example 3 Polyacrylic acid ( PAA Preparation of solution Polyacrylic acid (PAA) (Carbopol® 907 polymer from Lubrizol, Mw 82k) was dissolved in propylene glycol to a concentration of 5% by weight. Packaged saline - brine -2 Preparation Polyvinylpyrrolidone (PVP) (M n ~360K (from Sigma) was dissolved in the PBS prepared in Example 2 to have a concentration of 1% by weight. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 3. [Table 3] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / lens removal, the SiHy lens preform was immersed in saline solution 2 for approximately 30 minutes, inspected, and packaged in glass vials in packaged saline solution for sterilization (autoclaving at 121°C for 45 minutes). Lens characteristics are listed in Table 4. [Table 4] Example 4 Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 5. [Table 5] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / lens removal, the SiHy lens preform was placed, inspected, and packaged in glass vials of IPC-1 prepared in Example 2 for sterilization (autoclaving at 121°C for 45 minutes). Lens characteristics are listed in Table 6. [Table 6] Example 5 Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 7. [Table 7] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / lens removal, the SiHy lens preform was placed, inspected, and packaged in glass vials of IPC-1 prepared in Example 2 for sterilization (autoclaving at 121°C for 45 minutes). Lens characteristics are listed in Table 8. [Table 8] Example 6 Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 9. [Table 9] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the IPC-1 prepared in Example 2 within a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). Lens properties are listed in Table 10. [Table 10] Lens diameter data were measured both outside the packaging and after immersion in PBS for a certain period of time, according to the procedure described in Example 1. As shown in Table 11, the lens diameter of both types of lenses increased over time during PBS immersion. [Table 11] It is believed that, for this increase in diameter, the packaged saline solution (0.85 mL of IPC-1) may not have a sufficiently high pH and / or sufficient buffering capacity to neutralize the carboxylic acid groups (i.e., methacrylic acid) in the bulk SiHy material. Therefore, when the SiHy lens is pre-placed in PBS, the phosphate in the PBS (i.e., the more buffering) can retain the ability to deprotonate the carboxylic acid and cause the lens to swell. To support this assumption, the buffer capacity of IPC-1 is calculated to make [Na 2HPO 4.2H 2O] = 21.8 mM; [NaH 2PO 4·H [2O] = 3.2 mM. By assuming 1) the dry lens weight is 20 mg and 2) the packaged saline volume is 0.85 mL, the concentrations of carboxyl groups (from MAA or AA) are calculated to be 16.4 mM and 19.6 mM, respectively. Based on these conclusions, it is evident that the buffering capacity (especially for neutralizing diphosphates of carboxylic acids) is too close to the acid concentration required to neutralize all or most of the acid groups. Example 7 Phosphate buffer (Pb) PB ) An aqueous solution, namely phosphate buffer (PB), is prepared by: adding NaH+ to the phosphate buffer solution. 2PO 4•H 2O, Na 2HPO 4•2H 2O is dissolved in a given volume of purified water (distilled or deionized) to have the following composition: approximately 1.164 w / w% Na 2HPO 4•2H 2O, approximately 0.044 w / w / % NaH 2PO 4•H 2O. Inner coating of brine - IPC-2 Preparation IPC brine (IPC-2) was prepared by blending IPC-1 prepared in Example 2 and PB prepared above in a 1:1 weight ratio. The composition of IPC-2 is: ~0.05% PAE by weight; 0.035% poly(AAm-co-AA) (90 / 10) by weight; and 0.776% Na by weight. 2HPO 4•2H 2O, 0.044% NaH by weight 2PO 4•H 2O, and 0.395% NaCl by weight. Compared to IPC-1, IPC-2 has twice the Na content. 2HPO 4•2H The concentration of 2O was reduced, while the concentrations of PAE, poly(AAm-co-AA), and NaCl in IPC-2 were reduced by half. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 12. [Table 12] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the IPC-1 prepared in Example 2 in a dew drop blister shell and then sterilized (autoclaved at 121°C for 45 minutes). Lens properties are compiled in Tables 13 and 14. Clearly, after replacing IPC-1 with IPC-2 (which has a higher diphosphate concentration and a higher pH), the lens diameter became significantly more stable when immersed in PBS, and finger lubrication also appeared to be improved. These property improvements were achieved despite IPC-2 containing only half the PAE / poly(AAm-co-AA) concentration compared to IPC-1. [Table 13] [Table 14] Example 8 Inner coating of brine - IPC-3 Preparation IPC brine (IPC-3) was prepared by blending IPC-2 prepared in Example 7, PB prepared in Example 7, and propylene glycol (PG) in a weight ratio of 50:50:1. The composition of IPC-3 is: ~0.05% PAE by weight; 0.035% poly(AAm-co-AA) (90 / 10) by weight; and 0.768% Na by weight. 2HPO 4•2H 2O, 0.044% NaH by weight 2PO 4•H 2O, 0.196% NaCl by weight; and 0.99% PG by weight. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 15. [Table 15] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of IPC-2 or higher prepared in Example 7 in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). Lens properties (lens diameter and finger lubricity) are compiled in Table 16. As shown in the table, the lens diameter is stable in PBS. IPC-3 can provide even better finger lubricity compared to IPC-2, likely due to its lower NaCl concentration, which further enhances the carboxylate-IPC feed misalignment and their subsequent reactions during autoclaving. [Table 16] Example 9 Inner coating of brine - IPC-4 Preparation IPC-4 brine was prepared based on the following composition: ~0.05% PAE by weight; 0.035% poly(AAm-co-AA) (90 / 10) by weight; and 0.776% Na by weight. 2HPO 4•2H 2O, 0.044% NaH by weight 2PO 4•H 2O, 0.198% NaCl by weight; and 0.0005% hydrogen peroxide and 1% glycerol by weight. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 17. [Table 17] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of IPC-2 or higher prepared in Example 7 in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). Lens characteristics are compiled in Tables 18 and 19. As shown in the tables, the lens diameter shifts slightly in PBS. This is likely due to the glycerol diffusion effect. [Table 18] [Table 19] Example 10 Inner coating of brine - IPC-4 Preparation The preparation of IPC brine (IPC-4) is the same as in Example 9. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 20. [Table 20] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of IPC-2 or higher prepared in Example 7 in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). Lens properties are compiled in Tables 21 and 22. As shown in the tables, the lens diameter still shows a slight offset in PBS. This indicates the presence of other factors, such as the AA to HEMA ratio. A 10⁻⁵ composition results in an IP value < 1. This means that the lens subsequently formed will not allow ion permeation in an aqueous medium. [Table 21] [Table 22] Example 11 Inner coating of brine - IPC-5 Preparation IPC-5 brine was prepared based on the following composition: ~0.05% PAE by weight; 0.035% poly(AAm-co-AA) (90 / 10) by weight; and 0.776% Na by weight. 2HPO 4•2H 2O, 0.044% NaH by weight 2PO 4•H 2O, 0.160% NaCl by weight; and water to a final volume of 100%. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 23. [Table 23] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the prepared IPC-5 in a dew drop blister shell and then sterilized (autoclaved at 121°C for 45 minutes). Lens characteristics are compiled in Tables 24 and 25. [Table 24] [Table 25] Example 12 Inner coating of brine - IPC-5 Preparation The preparation of IPC brine (IPC-5) is the same as in Example 11. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 26. [Table 26] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was packaged in 0.85 mL of IPC-5 prepared in Example 11 in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). [Table 27] Lens properties are compiled in Tables 27 and 28. As shown in the tables, the MPC in the formulation plays a significant role in lens IP improvement. [Table 28] Example 13 Inner coating of brine - IPC-5 Preparation The preparation of IPC brine (IPC-5) is the same as in Example 11. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 29. [Table 29] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / lens removal, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the prepared IPC-5 brine in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). [Table 30] Lens characteristics are compiled in Tables 30 and 31. This demonstrates that the MPC to HEMA ratio is another factor affecting lens IP. [Table 31] Example 15 Inner coating of brine - IPC-5 Preparation The preparation of IPC brine (IPC-5) is the same as in Example 11. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 32. [Table 32] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / lens removal, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the prepared IPC-5 brine in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). [Table 33] Lens characteristics are compiled in Table 33. Experiments show that MPC also improves lens clarity. Example 16 Inner coating of brine - IPC-5 Preparation The preparation of IPC brine (IPC-5) is the same as in Example 11. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 34. [Table 34] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / lens removal, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the prepared IPC-5 brine in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). [Table 35] The lens IP values are listed in Table 35. Experiments show that small amounts of NVP, AMA, or TEGDVE in the formulation do not improve the lens IP. Example 17 Inner coating of brine - IPC-5 Preparation The preparation of IPC brine (IPC-5) is the same as in Example 11. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 36. [Table 36] Cast-molded silicone hydrogel contact lenses The SiHy lens preform (dry lens) was cast according to the procedure described in Example 2. After dry demolding / removal of the lens, the SiHy lens preform (dry lens) was individually packaged in 0.85 mL of the prepared IPC-5 brine in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes). [Table 37] Example 18 Inner coating of brine - IPC-7 Preparation IPC brine (IPC-7) was prepared based on the following composition: ~0.05% PAE by weight; 0.07% poly(AAm-co-AA) (90 / 10) by weight; 0.776% Na2HPO4·2H2O by weight; 0.044% NaH2PO4·H2O by weight; 0.160% NaCl by weight; and water to a final volume of 100%. Inner coating of brine - IPC-7B Preparation IPC brine (IPC-7B) was prepared based on the following composition: ~0.05% PAE by weight; 0.07% poly(AAm-co-AA) (90 / 10) by weight; 0.776% Na2HPO4·2H2O by weight; 0.044% NaH2PO4·H2O by weight; 0.160% NaCl by weight; 10 ppm EDTA; and water to 100% as needed. Preparation of polymerizable components Polymerizable compositions (SiHy lens formulations) were prepared to have the compositions shown in Table 38. [Table 38] Cast-molded silicone hydrogel contact lenses According to the procedure described in Example 2, SiHy lens preforms (dry lenses) are cast from lens formulations 17-1 and 17-3. The following describes the casting of SiHy lens preforms (dry lenses) using lens formulations 17-2 and 17-4. The lens formulations were then purged with nitrogen gas for 30 to 35 minutes at room temperature. N... 2. The swept lens formulation is introduced into a polypropylene mold and heat-cured in an oven under nitrogen under the following curing conditions: gradually decreasing from room temperature to 55°C at a ramp rate of about 7°C / min; holding at 55°C for about 30 minutes; gradually decreasing from 55°C to 100°C at a ramp rate of about 7°C / min; and holding at 100°C for about 100 minutes. After dry demolding / lens removal, the SiHy lens pre-material (dry lens) is individually packaged in 0.85 mL of the prepared IPC-7 or IPC-7B saline solution in a dew drop blister shell, and then sterilized (autoclaved at 121°C for 45 minutes) [Table 39]. EtB% represents elongation at break; SBQ% represents Sudan Black measure, which is determined in the Sudan Black staining test and measured on a scale of 0-100%. All disclosures, patents and patent applications that have been cited in this application and are incorporated herein by reference in their entirety. none none none
Claims
1. A method for producing coated silicone hydrogel contact lenses, comprising the following steps: (1) Introducing a polymerizable composition into a lens mold, wherein the polymerizable composition comprises (a) at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) at least one C1-C2 alkoxyethyl ester of (meth)acrylate, (c) at least one carboxyl-containing (meth)acryloxy monomer in weight from about 2% to about 10% relative to the total amount of all polymerizable components, and (d) at least one free radical; (2) Thermally or photocuring the polymerizable composition in the lens mold to form a silicone hydrogel lens primer comprising a bulk silicone hydrogel material comprising carboxyl groups; and (3) Step (2) The silicone hydrogel lens obtained therein is first heated directly in an aqueous solution having a pH of 6.8 to 8.5 and comprising at least one water-soluble, thermally crosslinkable hydrophilic polymer material at a temperature of 60°C to 140°C to form a coated silicone hydrogel contact lens. The coated silicone hydrogel contact lens comprises the bulk silicone hydrogel material and a layer of crosslinked hydrophilic polymer material covalently attached to the bulk silicone hydrogel material. The coated silicone hydrogel contact lens exhibits a water breakup time (WBUT) of at least 5 seconds and an oxygen permeability of at least 50 bar.
2. The method as described in claim 1, wherein, The sum of the amounts of components (a) through (d) is at least 90% by weight relative to the total amount of all polymerizable components in the polymerizable composition.
3. The method as described in claim 1, wherein, The polymerizable composition comprises, by weight, a component (a) and a component (b) comprising, by weight, 30% to 65% of the total amount of all polymerizable components.
4. The method as described in claim 1, wherein, The polymerizable composition further comprises at least one of the following: (e) hydroxyethyl methacrylate; and (f) at least one solvent selected from the group consisting of water, propylene glycol, polyethylene glycol having a molecular weight of about 400 Daltons or less, and combinations thereof.
5. The method as described in claim 4, wherein, The sum of the amounts of components (a) through (e) is at least 90% by weight relative to the total amount of all polymerizable components in the polymerizable composition.
6. The method as described in claim 4, wherein, The polymerizable composition comprises (a) and (b) components, which are 30% to 65% by weight relative to the total amount of all polymerizable components.
7. The method as described in claim 4, wherein, The weight ratio of component (b) to component (e) in the polymerizable composition is 40 to 20.
8. The method as described in claim 1, wherein, The polymerizable composition further comprises one or more polymerizable components selected from the group consisting of: (g) a non-silicone ethylene crosslinking agent, (h) a UV-absorbing ethylene monomer, (i) a polymerizable UV / high-energy ultraviolet light absorbing compound, (j) a polymerizable photochromic compound, (k) a polymerizable colorant, and (l) a combination thereof, provided that the sum of components (g) to (l) is less than 10% by weight relative to the amount of all polymerizable components.
9. The method as described in claim 4, wherein, The polymerizable composition further comprises one or more polymerizable components selected from the group consisting of: (g) a non-silicone ethylene crosslinking agent, (h) a UV-absorbing ethylene monomer, (i) a polymerizable UV / high-energy ultraviolet light absorbing compound, (j) a polymerizable photochromic compound, (k) a polymerizable colorant, and (l) a combination thereof, provided that the sum of components (g) to (l) is less than 10% by weight relative to the amount of all polymerizable components.
10. The method as described in any one of claims 1 to 9, further comprising: After step (2) and before step (3), the silicone hydrogel lens obtained in step (2) is prehydrated in water or an aqueous solution to obtain a hydrated silicone hydrogel contact lens, and in step (3), the hydrated silicone hydrogel contact lens is directly heated in an aqueous solution having a pH of 6.8 to 8.5 and comprising at least one water-soluble, thermally crosslinkable hydrophilic polymer material at a temperature of 60°C to 140°C to form the coated silicone hydrogel contact lens.
11. The method as described in any one of claims 1 to 9, wherein, The heating step is performed by autoclaving the silicone hydrogel lens material, which is to be immersed in a packaging solution that serves as a buffer solution within the sealed lens packaging, at a temperature of 115°C to 125°C for approximately 20-90 minutes.
12. The method as described in claim 11, wherein, The at least one water-soluble and thermally crosslinkable hydrophilic polymer material comprises a nitrogen-containing butaneonium group, an epoxy group, or a combination thereof.
13. The method as described in claim 12, wherein, The at least one water-soluble and thermally crosslinkable hydrophilic polymer material is: one or more multi-arm polyethylene glycols each having a terminal epoxy group; a mixture of multi-arm polyethylene glycols having terminal epoxy groups and one or more polyethylene glycols each having a terminal functional group selected from the group consisting of primary amine groups, secondary amine groups, carboxyl groups, thiol groups, and combinations thereof; a partial reaction product of multi-arm polyethylene having a terminal epoxy group and a hydrophilic reinforcing agent having at least one reactive functional group selected from the group consisting of amine groups, carboxyl groups, and thiol groups; or a combination thereof.
14. The method as described in claim 12, wherein, The at least one water-soluble and thermally crosslinkable hydrophilic polymer material comprises a nitrogen-containing heterocyclic butaneonium group and is a partial reaction product of a polymer containing nitrogen-containing heterocyclic butaneonium and a hydrophilic enhancer having at least one reactive functional group selected from the group consisting of primary amine groups, secondary amine groups, carboxyl groups, thiol groups, and combinations thereof.
15. The method as described in claim 14, wherein, The polymer system of nitrogen-containing heterocyclic butaneon is poly(2-azoline-co-ethyleneimine)-epimyl chloride copolymer, polyamide-epimyl chloride, copolymer of nitrogen-containing heterocyclic butaneon ethylene monomers with one or more hydrophilic ethylene monomers, or combinations thereof, wherein the hydrophilicity enhancer is: (a) a monosaccharide containing a primary amino group, a secondary amino group, a carboxyl group, or a thiol group; (b) a disaccharide containing a primary amino group, a secondary amino group, a carboxyl group, or a thiol group; (c) an oligosaccharide containing a primary amino group, a secondary amino group, a carboxyl group, or a thiol group; (d) a polysaccharide having a primary amino group, a secondary amino group, a carboxyl group, or a combination thereof; (e) a poly(ethylene glycol) having a unique -NH2, -SH, or -COOH functional group; (f) a poly(ethylene glycol) having two terminal functional groups selected from the group consisting of -NH2, -COOH, -SH, and combinations thereof; (g) (h) A multi-arm poly(ethylene glycol) having one or more functional groups selected from the group consisting of -NH2, -COOH, -SH, and combinations thereof; (i) a homopolymer or copolymer of a non-reactive hydrophilic vinyl monomer that is terminally capped with a monoamine, monocarboxyl, diamine, or dicarboxyl group; (j) a copolymer comprising (1) from 0.1% to 30% of a reactive vinyl monomer and (2) at least one non-reactive hydrophilic vinyl monomer; wherein the reactive vinyl monomer is a vinyl monomer having functional groups selected from the group consisting of carboxyl, primary amine, and secondary amine groups, and wherein the non-reactive hydrophilic monomer is free of any hydrophilic vinyl monomer having a carboxyl, primary amine, secondary amine, epoxy, isocyanate, acrylonitrile, or aziridine group; or (j) a combination thereof.
16. The method as described in any one of claims 1 to 9, wherein, The coated silicone hydrogel contact lens has an elastic modulus from 0.2 MPa to 1.8 MPa, a balance water content from 20% to 75% by weight (i.e., when fully hydrated), a friction rating of 3.0 or lower, and an average water contact angle of 90 degrees or lower by the seat drop method.
17. The method as described in claim 16, wherein, The at least one hydrophilic polysiloxane ethylene crosslinker comprises at least about 1.50 milliequivalents per gram ("meq / g") of a hydrophilic moiety which is a hydroxyl (-OH), carboxyl (-COOH), amino (-NHRN1, wherein RN1 is H or C1-C2 alkyl), acetylamine (-CO-NRN1RN2, wherein RN1 is H or C1-C2 alkyl and RN2 is covalent, H, or C1-C2 alkyl), N-C1-C3 acetylamine, urethane (-NH-CO-O-), urea (-NH-CO-NH-), polyethylene glycol chain (where n is an integer from 2 to 20 and T1 is H, methyl, acetyl, or phosphatidylcholine group), or a combination thereof.
18. The method as described in claim 17, wherein, The at least one hydrophilic polysiloxane ethylene crosslinking agent comprises (1) a polysiloxane segment comprising a dimethylsiloxane unit and a hydrophilic silicate unit having a methyl substituent and a monovalent C4-C40 organic group substituent having 2 to 6 hydroxyl groups, and (2) two terminal (meth)acrylic groups.
19. The method as described in claim 18, wherein, The at least one hydrophilic polysiloxane ethylene crosslinking agent comprises a polysiloxane ethylene crosslinking agent of formula (1) wherein: υ1 is an integer from 30 to 500 and ω1 is an integer from 1 to 75, provided that ω1 / υ1 is from about 0.035 to about 0.15; X01 is O or NRn, wherein Rn is hydrogen or C1-C10-alkyl; Ro is hydrogen or methyl; R2 and R3 are independently substituted or unsubstituted C1-C10 alkyl divalent groups or -R5-O-R6- divalent groups, wherein R5 and R6 are independently substituted or unsubstituted C1-C10 alkyl divalent groups; R4 is a monovalent group of any one of formulas (2) to (7); p1 is zero or 1; m1 is an integer from 2 to 4; m2 is an integer from 1 to 5; m3 is an integer from 3 to 6; m4 is an integer from 2 to 5. R7 refers to hydrogen or methyl; R8 refers to C2-C6 hydrocarbon groups with a valence of (m2 + 1); R9 refers to C2-C6 hydrocarbon groups with a valence of (m4 + 1); R10 refers to ethyl or hydroxymethyl; R11 refers to methyl or hydroxymethyl; R12 refers to hydroxy or methoxy; X3 refers to -S-sulfur bonds or -NR13-tertiary amino bonds, wherein R13 is C1-C1 alkyl, hydroxyethyl, hydroxypropyl, or 2,3-dihydroxypropyl; X4 refers to amide bonds, wherein R14 is hydrogen or C1-C10 alkyl; LPC is a divalent group of , , , , , or , where q1 is an integer from 1 to 20, R15 is a straight-chain or branched C1-C10 alkyl divalent group, R16 is a straight-chain or branched C3-C10 alkyl divalent group, and R17 is a direct bond or a straight-chain or branched C1-C4 alkyl divalent group.
20. A coated silicone hydrogel contact lens comprising: a bulk silicone hydrogel material; and a layer of non-silicone hydrogel material thereon, wherein the bulk silicone hydrogel material comprises (a) a repeating unit of at least one hydrophilic polysiloxane vinyl crosslinking agent, (b) a repeating unit of at least one C1-C2 alkoxyethyl ester of (meth)acrylate, and (c) a carboxyl-containing repeating unit of at least one carboxyl-containing (meth)acryloxy monomer, wherein the layer of non-silicone hydrogel material is covalently attached to the bulk silicone hydrogel material by means of the carboxyl groups of the carboxyl-containing repeating units, wherein the coated silicone hydrogel contact lens has a water breakup time (WBUT) of at least 5 seconds, an oxygen permeability (Dk) of at least 50 bar, and a pressure ranging from 0.2 MPa to 1.8 MPa. The elastic modulus is MPa, the equilibrium water content is 20% to 75% by weight (i.e., when fully hydrated), the friction rating is 3.0 or lower, and the average water contact angle is 90 degrees or lower by the seat drop method.
21. The coated silicone hydrogel contact lens as described in claim 20, wherein, The at least one hydrophilic polysiloxane ethylene crosslinker comprises at least about 1.50 milliequivalents per gram ("meq / g") of a hydrophilic moiety which is a hydroxyl (-OH), carboxyl (-COOH), amino (-NHRN1, wherein RN1 is H or C1-C2 alkyl), acetylamine (-CO-NRN1RN2, wherein RN1 is H or C1-C2 alkyl and RN2 is covalent, H, or C1-C2 alkyl), N-C1-C3 acetylamine, urethane (-NH-CO-O-), urea (-NH-CO-NH-), polyethylene glycol chain (where n is an integer from 2 to 20 and T1 is H, methyl, acetyl, or phosphatidylcholine group), or a combination thereof.
22. The coated silicone hydrogel contact lens as described in claim 21, wherein, The at least one hydrophilic polysiloxane ethylene crosslinking agent comprises (1) a polysiloxane segment comprising a dimethylsiloxane unit and a hydrophilic silicate unit having a methyl substituent and a monovalent C4-C40 organic group substituent having 2 to 6 hydroxyl groups, and (2) two terminal (meth)acrylic groups.
23. The coated silicone hydrogel contact lens as described in claim 22, wherein, The at least one hydrophilic polysiloxane ethylene crosslinking agent comprises a polysiloxane ethylene crosslinking agent of formula (1) wherein: υ1 is an integer from 30 to 500 and ω1 is an integer from 1 to 75, provided that ω1 / υ1 is from 0.035 to 0.15; X01 is O or NRn, wherein Rn is hydrogen or C1-C10-alkyl; Ro is hydrogen or methyl; R2 and R3 are independently substituted or unsubstituted C1-C10 alkyl divalent groups or -R5-O-R6- divalent groups, wherein R5 and R6 are independently substituted or unsubstituted C1-C10 alkyl divalent groups; R4 is a monovalent group of any one of formulas (2) to (7); p1 is zero or 1; m1 is an integer from 2 to 4; m2 is an integer from 1 to 5; m3 is an integer from 3 to 6; m4 is an integer from 2 to 5; R7 is hydrogen or methyl; R8 refers to C2-C6 hydrocarbon groups with a valence of (m2 + 1); R9 refers to C2-C6 hydrocarbon groups with a valence of (m4 + 1); R10 refers to ethyl or hydroxymethyl; R11 refers to methyl or hydroxymethyl; R12 refers to hydroxy or methoxy; X3 refers to a -S-sulfur bond or a -NR13-tertiary amino bond, wherein R13 is a C1-C1 alkyl, hydroxyethyl, hydroxypropyl, or 2,3-dihydroxypropyl; X4 refers to an amide bond, wherein R14 is hydrogen or a C1-C10 alkyl; LPC refers to divalent groups of , , , , , or , wherein q1 is an integer from 1 to 20, R15 is a straight-chain or branched C1-C10 alkyl divalent group, R16 is a straight-chain or branched C3-C10 alkyl divalent group, and R17 is a direct bond or a straight-chain or branched C1-C4 alkyl divalent group.
24. The coated silicone hydrogel contact lens as described in any one of claims 20 to 23, wherein, The bulk silicone hydrogel material further comprises at least one of the following: (d) repeating units of hydroxyethyl methacrylate; and (e) repeating units of at least one polymerizable component selected from the group consisting of: non-silicone vinyl crosslinking agents, UV-absorbing vinyl monomers, polymerizable UV / high-energy ultraviolet light absorbing compounds, polymerizable photochromic compounds, polymerizable colorants, and combinations thereof, provided that the amount of component (e) is less than 10% by weight relative to the total weight of the bulk silicone hydrogel material in a dry state.
25. A coated silicone hydrogel contact lens as described in any one of claims 20 to 23, wherein, This non-silicone hydrogel material is a cross-linked polymer material comprising, on a molar basis, at least 25% of repeating monomer units of at least one hydrophilic vinyl monomer selected from the group consisting of: N,N-dimethyl (meth)acrylamide, N-ethyl (meth)acrylamide, N,N-diethyl (meth)acrylamide, N-propyl (meth)acrylamide, N-isopropyl (meth)acrylamide, N-3-methoxypropyl (meth)acrylamide, N-2-dimethylaminoethyl (meth)acrylamide, dimethylaminoethyl (meth)acrylate, N-2-hydroxyethyl (meth)acrylamide, N,N-bis(hydroxyethyl)(meth)acrylamide, N-3-Hydroxypropyl (meth)acrylamide, N-2-Hydroxypropyl (meth)acrylamide, N-2,3-Dihydroxypropyl (meth)acrylamide, N-Tris(hydroxymethyl)methyl (meth)acrylamide, 2-Hydroxyethyl (meth)acrylate, 3-Hydroxypropyl (meth)acrylate, 2-Hydroxypropyl (meth)acrylate, Glyceryl methacrylate (GMA), Di(ethylene glycol)(meth)acrylate, Tri(ethylene glycol)(meth)acrylate, Tetra(ethylene glycol)(meth)acrylate, Poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500, Poly(ethylene glycol)(meth)acrylate with a number average molecular weight up to 1500 (Alcohol) Ethyl (Methyl) Acrylamide, N-vinylpyrrolidone, N-vinyl-3-methyl-2-pyrrolidone, N-vinyl-4-methyl-2-pyrrolidone, N-vinyl-5-methyl-2-pyrrolidone, N-vinyl-6-methyl-2-pyrrolidone, N-vinyl-3-ethyl-2-pyrrolidone, N-vinyl-4,5-dimethyl-2-pyrrolidone, N-vinyl-5,5-dimethyl-2-pyrrolidone, N-vinyl-3,3,5-trimethyl-2-pyrrolidone, N-vinylpiperidone, N-vinyl-3-methyl-2-piperidone, N-vinyl-4-methyl-2-piperidone, N- Vinyl-5-methyl-2-piperidinone, N-vinyl-6-methyl-2-piperidinone, N-vinyl-6-ethyl-2-piperidinone, N-vinyl-3,5-dimethyl-2-piperidinone, N-vinyl-4,4-dimethyl-2-piperidinone, N-vinylcaprolactone, N-vinyl-3-methyl-2-caprolactone, N-vinyl-4-methyl-2-caprolactone, N-vinyl-7-methyl-2-caprolactone, N-vinyl-7-ethyl-2-caprolactone, N-vinyl-3,5-dimethyl-2-caprolactone, N-vinyl-4,6-dimethyl-2-caprolactone, N-vinyl-3,5,7-Trimethyl-2-caprolactam, N-vinyl-N-methylacetamide, N-vinylmethacinamide, N-vinylacetamide, N-vinylisopropylamine, N-vinyl-N-ethylacetamide, N-vinyl-N-ethylmethacinamide, 1-methyl-3-methylene-2-pyrrolidone, 1-ethyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 1-ethyl-5-methylene-2-pyrrolidone Methyl-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, 5-ethyl-3-methylene-2-pyrrolidone, 1-n-propyl-3-methylene-2-pyrrolidone, 1-n-propyl-5-methylene-2-pyrrolidone, 1-isopropyl-3-methylene-2-pyrrolidone, 1-isopropyl-5-methylene-2-pyrrolidone, 1-n-butyl-3-methylene-2-pyrrolidone, 1-tertiary Butyl-3-methylene-2-pyrrolidone, ethylene glycol methyl ether (meth)acrylate, di(ethylene glycol) methyl ether (meth)acrylate, tri(ethylene glycol) methyl ether (meth)acrylate, tetra(ethylene glycol) methyl ether (meth)acrylate, C1-C4-alkoxy poly(ethylene glycol) (meth)acrylate having a weight average molecular weight of up to 1500, methoxy-poly(ethylene glycol)ethyl(meth)acrylamide having a number average molecular weight of up to 1500, ethylene glycol monovinyl ether, di(ethylene glycol) monovinyl ether, tri(ethylene glycol) monovinyl ether, tetra(ethylene glycol) monovinyl ether, poly(ethylene glycol) monovinyl ether, ethylene glycol methyl vinyl ether, di(ethylene glycol) methyl vinyl ether, tri(ethylene glycol) methyl vinyl ether, tetra(ethylene glycol) methyl vinyl ether, poly(ethylene glycol) methyl vinyl ether, and combinations thereof.
26. The coated silicone hydrogel contact lens as described in any one of claims 20 to 23, wherein the non-silicone hydrogel material is a cross-linked polymer material comprising at least 25% repeating monomer units of at least one phosphatidylcholine-containing vinyl monomer on a molar basis.
27. A coated silicone hydrogel contact lens as described in any one of claims 20 to 23, wherein, This non-silicone hydrogel material is a cross-linked polymer material containing poly(ethylene glycol) chains.
28. The coated silicone hydrogel contact lens as described in claim 27, wherein, The poly(ethylene glycol) chain is directly derived from (a) a poly(ethylene glycol) having a single -NH2, -SH, or -COOH functional group, (b) a poly(ethylene glycol) having two terminal functional groups selected from the group consisting of -NH2, -COOH, -SH, and combinations thereof, (c) a multi-arm poly(ethylene glycol) having one or more functional groups selected from the group consisting of -NH2, -COOH, -SH, and combinations thereof, and (d) combinations thereof.
Citation Information
Patent Citations
Weekly and monthly disposable water gradient contact lenses
TW201927349A
Method for coating silicone hydrogels
US20090186229A1