Composite oxides for cement admixtures, and methods for manufacturing composite oxides for cement admixtures.
Patent Information
- Application Number
- TW114124569
- Authority / Receiving Office
- TW · TW
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2024-07-05
- Filing Date
- 2025-06-30
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2045-06-29
AI Technical Summary
There is a demand for novel cementitious materials that differ from conventional ones, and existing methods for manufacturing composite oxides for cement admixtures are inadequate.
A composite oxide for cementitious admixtures is formulated with specific ratios of CaO, MgO, Al2O3, and SiO2, with alkalinity B3 of 1.40 to 3.00, value X of 0.79 or more, and value Y of 1.37 or more, and a total iron content of 8.0% by mass or less, manufactured by rapid cooling of the molten state.
The solution provides a novel composite oxide with improved hydraulic properties, glass transition rate, and granular form, enhancing the performance of cementitious materials.
Abstract
Description
[Technical Field]
[0001] This invention relates to a composite oxide for cementitious admixtures. Furthermore, this invention relates to a method for manufacturing the composite oxide for cementitious admixtures. [Previous Technology]
[0002] Cement is widely used as a material in civil engineering. In most cases, cement is manufactured by mixing various cementitious admixtures with composite oxides. For example, as described in Patent Document 1, ordinary Portland cement ash pulverized material is used as a composite oxide for cementitious admixtures. [Prior Art Documents] [Patent Documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 2019-131416 [Summary of the Invention]
[0004] (Problem to be Solved by the Invention) In recent years, there has been a demand for cementitious materials that differ from conventional ones. Therefore, the object of this invention is to provide a novel composite oxide for cementitious materials. Furthermore, the object of this invention also provides a method for manufacturing the composite oxide for cementitious materials. (Technical Means for Solving the Problem)
[0005] The inventors, through in-depth research, completed this invention to solve the above-mentioned problems. Specifically, they discovered that the above-mentioned problems can be solved using the following configuration.
[0006] [1] A composite oxide for cementitious admixtures contains CaO, MgO, Al2O3 and SiO2, wherein the value of alkalinity B3 obtained by dividing the sum of CaO content, MgO and Al2O3 content by SiO2 content is 1.40 to 3.00, the value X of the sum of SiO2 content and Al2O3 content divided by CaO content is 0.79 or more, the value Y of the sum of CaO content and SiO2 content divided by Al2O3 content is 1.37 or more, and the total iron content is 8.0% by mass or less, wherein the unit of content of each component is by mass%. [2] The composite oxide for cementitious admixtures as described in [1], wherein the above value Y is 8.00 or less. [3] The composite oxide for cementitious admixtures as described in [1] or [2], wherein the above total iron content is 3.0% by mass or more. [4] A method for manufacturing a composite oxide for cementitious admixtures, wherein a composite oxide with the following adjusted composition is obtained: containing CaO, MgO, Al2O3 and SiO2, wherein the basicity B3 obtained by dividing the sum of the CaO content, MgO and Al2O3 content by the SiO2 content is 1.40 to 3.00, the value X obtained by dividing the sum of the SiO2 content and Al2O3 content by the CaO content is 0.79 or more, the value Y obtained by dividing the sum of the CaO content and SiO2 content by the Al2O3 content is 1.37 or more, and the total iron content is 8.0% by mass or less; and the composite oxide with the adjusted composition in the molten state is rapidly cooled. [5] In the method for manufacturing a composite oxide for cementitious admixtures as described in [4], when the reduced iron obtained by the direct reduction method is melted in a submerged arc welding furnace, an additive is added to generate slag to obtain the composite oxide with the adjusted composition. (Effects compared to prior art)
[0007] According to the present invention, a novel composite oxide for cementitious admixtures can be provided. Furthermore, the present invention can also provide a method for manufacturing the composite oxide for cementitious admixtures.
Implementation Method
[0008] Hereinafter, the present invention will be described in detail. The following description of the constituent elements is based on a representative embodiment of the present invention, but the present invention is not limited to this embodiment.
[0009] Hereinafter, the meanings of each item in this specification are as follows. The embodiments of the present invention will be described in detail below. However, the embodiments described below are merely examples, and the present invention is not limited to the embodiments described below. Furthermore, the numerical range indicated by "~" in this specification refers to the range including the lower and upper limits of the values described before and after "~".
[0010] [Composite Oxide for Cement Admixtures] The composite oxide for cement admixtures of the present invention (hereinafter also referred to as "the composite oxide of the present invention") contains CaO, MgO, Al2O3, and SiO2. Furthermore, in the composite oxide of the present invention, the alkalinity B3 obtained by dividing the sum of the CaO content, MgO content, and Al2O3 content by the SiO2 content is 1.40 to 3.00. Also, in the composite oxide of the present invention, the value X of the sum of the SiO2 content and Al2O3 content divided by the CaO content is 0.79 or more. Also, in the composite oxide of the present invention, the value Y of the sum of the CaO content and SiO2 content divided by the Al2O3 content is 1.37 or more. Also, in the composite oxide of the present invention, the total iron content is 8.0% by mass or less. Furthermore, the unit for the content of each component is by mass%. The composite oxide of the present invention will now be described in detail.
[0011] The composite oxide system of the present invention contains CaO, MgO, Al2O3, and SiO2. The CaO content in the composite oxide of the present invention is not particularly limited as long as it meets the above-mentioned basicity B3 requirement, the above-mentioned value X requirement, and the above-mentioned value Y requirement. Preferably, it is 15.0% by mass or more, more preferably 18.0% by mass or more, more preferably 20.0% by mass or more, and particularly preferably 21.0% by mass or more, 24.0% by mass or more, 28.0% by mass or more, and 30.0% by mass or more. Furthermore, the above-mentioned CaO content is preferably 60.0% by mass or less, more preferably 55.0% by mass or less, more preferably 53.0% by mass or less, and particularly preferably 50.0% by mass or less, 48.0% by mass or less, 46.0% by mass or less, and 44.0% by mass or less.
[0012] The MgO content in the composite oxide of the present invention is only subject to the above-mentioned basicity B3 requirement, and there are no other particular restrictions. It is preferred to be 2.0% by mass or more, more preferably 3.0% by mass or more, more preferably 4.5% by mass or more, and even more preferably 5.0% by mass or more, 5.3% by mass or more, 6.0% by mass or more, and 7.0% by mass or more. Furthermore, the above-mentioned MgO content is preferably 20.0% by mass or less, more preferably 18.0% by mass or less, more preferably 16.0% by mass or less, and even more preferably 15.0% by mass or less, 14.0% by mass or less, 13.0% by mass or less, and 12.0% by mass or less.
[0013] The Al2O3 content in the composite oxide of the present invention is not particularly limited as long as it meets the above-mentioned basicity B3 requirement, the above-mentioned value X requirement, and the above-mentioned value Y requirement. Preferably, it is 8.0% by mass or more, more preferably 10.0% by mass or more, even more preferably 12.0% by mass or more, and particularly preferably 13.0% by mass or more, 14.0% by mass or more, 15.0% by mass or more, and 16.0% by mass or more. Furthermore, the above-mentioned Al2O3 content is preferably 45.0% by mass or less, more preferably 40.0% by mass or less, even more preferably 36.0% by mass or less, and particularly preferably 35.0% by mass or less, 30.0% by mass or less, 27.0% by mass or less, and 25.0% by mass or less.
[0014] The SiO2 content in the composite oxide of the present invention is not particularly limited as long as it meets the above-mentioned basicity B3 requirement, the above-mentioned value X requirement, and the above-mentioned value Y requirement. Preferably, it is 18.0% by mass or more, more preferably 20.0% by mass or more, more preferably 23.0% by mass or more, and particularly preferably 24.0% by mass or more, 25.0% by mass or more, 26.0% by mass or more, and 27.0% by mass or more. Furthermore, the above-mentioned SiO2 content is preferably 50.0% by mass or less, more preferably 45.0% by mass or less, more preferably 42.0% by mass or less, and particularly preferably 41.0% by mass or less, 40.0% by mass or less, 38.0% by mass or less, and 35.0% by mass or less.
[0015] In the composite oxide of the present invention, the total iron content is 8.0% by mass or less. From the viewpoint that the composite oxide of the present invention has a near-white hue, the total iron content is preferably 7.5% by mass or less, more preferably 7.0% by mass or less, even more preferably 6.5% by mass or less, and preferably 6.0% by mass or less, 5.5% by mass or less, and 5.0% by mass or less, in that order. Furthermore, the total iron content of the composite oxide of the present invention is preferably 0.1% by mass or more, more preferably 0.2% by mass or more, even more preferably 0.3% by mass or more, and preferably 0.5% by mass or more, 1.0% by mass or more, 2.0% by mass or more, and 3.0% by mass or more, in that order. Additionally, when reducing the total iron content in the composite oxide of the present invention, it may be necessary to adjust the reaction conditions to improve the recovery rate of metallic iron in the reactor when melting iron sources such as reduced iron. If the total iron content is adjusted to within the above-mentioned range, the production efficiency of the reactor can be improved, and the load on the refractory materials used in the reactor can be reduced, which is therefore preferable. In addition, the so-called "total iron content" refers to the total content of iron (Fe) in the composite oxide as oxides (e.g., FeO, Fe3O4, Fe2O3, etc.) and in the metallic iron form.
[0016] The content of each component in the composite oxide of the present invention is determined using XRF (X-ray fluorescence) analysis. Specifically, X-ray fluorescence generated by X-ray irradiation is detected, and then spectroscopic analysis is performed using energy or spectroscopic crystallization to conduct elemental or compositional analysis. Alternatively, if the packing ratio used in manufacturing the composite oxide of the present invention is known, this value can also be used.
[0017] In the composite oxide of the present invention, the value obtained by dividing the sum of the CaO content, MgO and Al2O3 content by the SiO2 content is the alkalinity B3, which is 1.40~3.00. That is, the B3 value belonging to the alkalinity B3 can be calculated by the following formula (1).
[0018] [Number 1]
[0019] In the above formula (1), [CaO], [MgO], [Al2O3] and [SiO2] are the contents of CaO, MgO, Al2O3 and SiO2 in the composite oxide of the present invention, respectively, and the unit is mass%. If the alkalinity B3 is 1.40 or above, when the components contained in the composite oxide of the present invention are dissolved, Ca and Si components will dissolve and hydration reaction will easily occur. From the viewpoint of potential hydraulic properties, alkalinity B3 is preferably 1.45 or above, more preferably 1.50 or above, more preferably 1.60 or above, and preferably 1.65 or above, 1.70 or above, 1.75 or above, and 1.80 or above, in that order. Furthermore, if the alkalinity B3 is below 3.00, the composite oxide of the present invention has moderate potential hydraulic properties, and when mixed in cement, the concrete containing the composite oxide of the present invention can fully exhibit strength. From the perspective of glass transition rate, the basicity B3 is preferably below 2.95, better below 2.90, even better below 2.80, and the best in order are below 2.70, below 2.60, below 2.50, and below 2.40.
[0020] In the composite oxide of the present invention, the sum of the SiO2 content and the Al2O3 content divided by the CaO content, X, is 0.79 or higher. That is, the above value X can be calculated by the following formula (2).
[0021] [Number 2]
[0022] In the above formula (2), [CaO], [Al2O3] and [SiO2] are the contents of CaO, Al2O3 and SiO2 in the composite oxide of the present invention, respectively, and the unit is mass%. If the value X is 0.79 or above, the glass transition rate of the composite oxide of the present invention can be easily improved. The value X is preferably 0.80 or above, more preferably 0.85 or above, more preferably 0.90 or above, and preferably 0.95 or above, 1.00 or above, 1.05 or above, and 1.10 or above in that order. In addition, although there is no particular limitation on the upper limit of the above value X, for example, it is preferably 5.00 or below, more preferably 4.00 or below, more preferably 3.50 or below, and even more preferably 3.00 or below, 2.80 or below, 2.60 or below, and 2.20 or below in that order.
[0023] In the composite oxide of the present invention, the value Y, which is the sum of the CaO content and the SiO2 content divided by the Al2O3 content, is 1.37 or higher. That is, the above value Y can be calculated by the following formula (3).
[0024] [Number 3]
[0025] In the above formula (3), [CaO], [Al2O3] and [SiO2] are the contents of CaO, Al2O3 and SiO2 in the composite oxide of the present invention, respectively, and the unit is mass%. If the value Y is 1.37 or above, the composite oxide of the present invention can be easily formed into granules. The value Y is preferably 1.40 or above, more preferably 1.50 or above, more preferably 1.70 or above, and even more preferably 1.90 or above, 2.10 or above, 2.50 or above, and 2.80 or above. Furthermore, there is no particular limitation on the upper limit of the above value Y, for example, it is 10.00 or below, more preferably 8.00 or below, more preferably 7.00 or below, and especially preferably 6.50 or below, 6.00 or below, 5.60 or below, and 5.00 or below.
[0026] The average particle size of the composite oxide of the present invention, from the viewpoint of use as a cementitious admixture, is preferably 1 to 100 μm. The specific surface area of the composite oxide of the present invention is preferably 3000 to 10000 cm² / g or more. Furthermore, the specific surface area of the composite oxide of the present invention is determined using the Blaine method. The higher the whiteness of the composite oxide of the present invention, the better. The whiteness of the composite oxide of the present invention is preferably greater than 20, and may also exceed 55. The above-mentioned whiteness refers to ISO whiteness.
[0027] The glass transition rate of the composite oxide of the present invention is preferably 90.0% or higher, more preferably 91.0% or higher, and even more preferably 92.0% or higher. The upper limit of the above-mentioned glass transition rate is 100.0% or lower, but in most cases it is 99.9% or lower. The glass transition rate of the composite oxide of the present invention is determined by observation using a polarizing microscope. Specifically, a sample thin film of the composite oxide is prepared, and the glass transition rate (%) of the composite oxide is determined by observation using a polarizing microscope with cross-polarized light.
[0028] The method for manufacturing the composite oxide of the present invention is not particularly limited except for satisfying the above-mentioned requirements. For example, the composite oxide of the present invention can be manufactured using the method for manufacturing the composite oxide of the present invention described later. Preferably, the composite oxide of the present invention is obtained using the method for manufacturing the composite oxide of the present invention described later.
[0029] [Manufacturing Method of Composite Oxide for Cement Admixtures] The manufacturing method of the composite oxide for cement admixtures of the present invention involves obtaining a composite oxide containing CaO, MgO, Al2O3, and SiO2, wherein the sum of the CaO content, MgO content, and Al2O3 content divided by the SiO2 content yields a value that is, an alkalinity B3 of 1.40 to 3.00, a value X of the sum of the SiO2 content and Al2O3 content divided by the CaO content of 0.79 or more, a value Y of the sum of the CaO content and SiO2 content divided by the Al2O3 content of 1.37 or more, and a total iron content of 8.0% by mass or less. The molten composite oxide with adjusted composition is then rapidly cooled. The composite oxide of the present invention can be obtained using the manufacturing method of the composite oxide for cement admixtures of the present invention (hereinafter also referred to as "the manufacturing method of the present invention"). The manufacturing method of the present invention will be described below. Furthermore, the following steps for obtaining the composite oxide with the above-mentioned adjusted composition will be referred to as the "composition adjustment step," and the steps for rapidly cooling the molten composite oxide with the adjusted composition will be referred to as the "quenching step." Each step will be explained below.
[0030] The manufacturing method of the present invention first performs the above-described component adjustment step. The component adjustment step obtains a composite oxide in which CaO, MgO, Al2O3, and SiO2 are adjusted, and the basicity B3, value X, and value Y are within a predetermined range. Furthermore, the definitions of basicity B3, value X, and value Y in the component-adjusted composite oxide are the same as those in the composite oxide of the present invention, and therefore their description is omitted here. Moreover, the preferred ranges of the content of each component in the manufacturing method of the present invention, as well as the preferred ranges of basicity B3, value X, and value Y, are the same as those in the composite oxide of the present invention, and therefore their description is omitted here. In the component adjustment step, the type and dosage of additives used in the component adjustment are adjusted to bring the basicity B3, value X, and value Y to a predetermined range. Furthermore, the total iron content in the composite oxide with adjusted composition, as mentioned above, is preferably 0.1% by mass or more, more preferably 0.2% by mass or more, even more preferably 0.3% by mass or more, and most preferably 0.5% by mass or more, 1.0% by mass or more, 2.0% by mass or more, and 3.0% by mass or more, in that order. Additionally, when the total iron content in the composite oxide with adjusted composition is reduced, there are situations where, when melting iron sources such as reduced iron, it is necessary to adjust the reaction conditions in the reactor to improve the recovery rate of metallic iron. When the total iron content is adjusted to within the above-mentioned range, the reactor's production efficiency can be improved, and the load on the refractory materials used in the reactor can be reduced, which is therefore preferable.
[0031] The method for implementing the composition adjustment step is not particularly limited as long as the composite oxide with the above-mentioned adjusted composition can be obtained. Furthermore, the composite oxide with adjusted composition can be obtained in a solid state or in a molten state. For example, the method for implementing the composition adjustment step can be: a method of mixing and melting the solid monomers of the above-mentioned components, and a method of mixing and melting a composite oxide containing the solids of the above-mentioned components. Alternatively, the composition adjustment step can be implemented by adding the solid monomers of the above-mentioned components or the solid composite oxide containing the above-mentioned components to the molten composite oxide or the melt of the monomers of the above-mentioned components.
[0032] Furthermore, the implementation method of the composition adjustment step can also be, for example, using slag produced in the metal smelting or refining step as a raw material. Iron is a preferred example of the metal. That is, iron and steel slag can also be used as raw materials. Also, the composition adjustment step can be implemented by adjusting the composition of the generated slag (e.g., iron and steel slag) during the metal smelting or refining step. There are no particular limitations on iron and steel slag; examples include blast furnace slag, converter slag, electric furnace slag, slag produced by direct ironmaking, and slag produced by smelting reduction ironmaking. The composition adjustment method can be, for example, mixing solid monomers of the above-mentioned components into iron and steel slag, mixing composite oxides containing solids of the above-mentioned components into iron and steel slag, or mixing other iron and steel slags into iron and steel slag. Furthermore, the method of adjusting the composition is that when slag is generated by adding the components that constitute the above-mentioned iron and steel slags, solid monomers of the above-mentioned components can be added, composite oxides containing the solids of the above-mentioned components can be added, or one or more other iron and steel slags can be added.
[0033] The aforementioned blast furnace slag includes slag recovered when iron is recovered from iron ore using a reduction method by adding coke, limestone, etc., to iron ore charged into the blast furnace, resulting in slag with a density lower than that of pig iron. Furthermore, the aforementioned blast furnace slag also includes slag produced as a byproduct of the so-called "blast furnace-converter process." The aforementioned electric arc furnace slag includes slag produced as a byproduct of the electric arc furnace steelmaking process. In the electric arc furnace steelmaking process, cold iron sources (e.g., scrap iron, reduced iron, etc.) are generally heated and melted using electricity.
[0034] In particular, as a method for implementing the composition adjustment step, it is preferable to adjust the composition of the iron and steel slag; more preferably, it is preferable to add additives to the slag during the melting of reduced iron obtained by direct reduction in an electric furnace (preferably a submerged arc welding furnace) to obtain a composite oxide with adjusted composition. Examples of such additives include: monomers of the aforementioned components, and composite oxides containing the aforementioned components, more specifically including: lime (CaO), silica sand (SiO2), and magnesium oxide (MgO), and byproducts containing such composite oxides (e.g., slag, used brick dust, and dust).
[0035] In the above-described method of using slag produced in the metal smelting or refining steps as raw materials, although ferrous and steel slag is mainly described, other slags may also be used. Other slags may include, for example, non-ferrous metal slags such as nickel-iron slag and copper slag, as well as waste melting slag, sewage sludge slag, etc.
[0036] In the manufacturing method of the present invention, a rapid cooling step is performed on a molten composite oxide with adjusted composition. The composite oxide with adjusted composition is as described above. The rapid cooling step can be performed by a known method, such as cooling the molten composite oxide by blowing out a refrigerant. The refrigerant can be a liquid or a gas. Examples of liquids include water. Examples of gases include inert gases such as argon and nitrogen, and air. The flow rate of the refrigerant can be adjusted appropriately.
[0037] A composite oxide with a high glass transition rate can be easily obtained by using a rapid quenching step. The preferred range of the glass transition rate of the composite oxide is as described above. Furthermore, by using a composite oxide with the above-described adjusted composition, granular composite oxides can be easily obtained by a rapid quenching step. The term "granular" refers to a non-fibrous form, specifically meaning that the ratio of the major axis to the minor axis (major axis / minor axis) is less than 10.0.
[0038] In addition, in order to obtain a solid composite oxide with adjusted composition in the above composition adjustment step, the above rapid cooling step is performed after melting the composite oxide with adjusted composition.
[0039] In the manufacturing method of the present invention, steps other than the above-mentioned component adjustment step and quenching step may also be implemented. For example, a particle size adjustment step may be included to adjust the particle size of the composite oxide obtained by the above-mentioned quenching step. There are no particular limitations on the implementation method of the particle size adjustment step. For example, a known pulverizing method can be used to pulverize the obtained composite oxide. The preferred particle size of the pulverized composite oxide is as described above. Pulverizing methods include, for example, ball milling, needle milling, and jet milling. Furthermore, after pulverizing, the composite oxide can also be classified using a known classification method. Classification methods include, for example, dry classification, and more specifically, sieving and air classifying.
[0040] [Use of Composite Oxide for Cement Admixtures] The composite oxide for cement admixtures (composite oxide) of the present invention can be used as a cement admixture. Hereinafter, cement containing the composite oxide of the present invention will be described.
[0041] The composite oxide of the present invention is preferably used in a blend of materials, such as mixed cement. The aforementioned mixed cement contains the composite oxide of the present invention and other components. Other components may include, for example, Portland cement. Portland cement can be ordinary Portland cement, and ordinary Portland cement may also contain cement ash. Furthermore, other components may include, for example, early-strength Portland cement that exhibits strength in a shorter period, medium-heat Portland cement with lower calorific value, and low-heat Portland cement.
[0042] In the above-mentioned mixed cement, the content of composite oxides relative to the total mass of composite oxides and other components is preferably 10-90%. [Example]
[0043] Hereinafter, the present invention will be described in more detail with reference to embodiments. The materials, amounts, proportions, processing contents, and processing order shown in the following embodiments can be appropriately modified without departing from the spirit of the present invention. Therefore, the scope of the present invention should not be limited by the embodiments shown below.
[0044] [Example 1] <Manufacturing of Composite Oxide> The amounts of CaO reagent, SiO2 reagent, Al2O3 reagent, MgO reagent, and Fe3O4 reagent were adjusted to be in the proportions shown in Table 1 below, relative to the remelted blast furnace slag, to obtain a composite oxide with adjusted composition. Water was sprayed onto the molten composite oxide to rapidly cool and solidify it, thus obtaining the composite oxide. The obtained composite oxide was micronized to a specific surface area of 3000~5000 cm2 / g. The basicity B3, value X, and value Y of the obtained composite oxide were calculated using formulas (1)~(3) above. The results are shown in Table 1 below.
[0045] <Determination> The glass transition rate of the composite oxide obtained in Example 1 was determined by the method described above. The results are shown in Table 1 below.
[0046] Furthermore, the activity index of the composite oxide obtained in Example 1 was measured at 7 days, 28 days, and 91 days. The determination of the activity index of the composite oxide at 7 days, 28 days, and 91 days was carried out according to the "Blast Furnace Slag Micropowder for Concrete" specified in JIS A 6206-2:2010. Specifically, the activity index was calculated by dividing the compressive strength (%) of a 40mm × 40mm × 160mm prismatic mortar made by replacing 50% by mass of ordinary cement with the composite oxide by the compressive strength (%) of mortar made using only ordinary cement. That is, the compressive strength of mortar formed by replacing 50% cement with the composite oxide and the compressive strength of mortar made using only cement were measured, and then the activity index of the composite oxide was measured. The results of the activity index are shown in Table 1 below.
[0047] [Examples 2-22] Except for adjusting the amount of the above-mentioned reagents added so that the content of each component constituting the composite oxide is as shown in Table 1 below, the composite oxides were obtained in the same manner as in Example 1. Furthermore, the glass transition rate and activity index were measured in the same manner as in Example 1.
[0048] [Examples 23-33] Except for adjusting the amount of the above reagents added so that the content of each component constituting the composite oxide is as shown in Table 1 below, and blowing air to rapidly cool and solidify it, the composite oxide was obtained in the same manner as in Example 1. Furthermore, the glass transition rate and activity index were measured in the same manner as in Example 1.
[0049] [Comparative Examples 1-12] Except for adjusting the amount of the above-mentioned reagents added so that the content of each component constituting the composite oxide is as shown in Table 1 below, the composite oxides were obtained in the same manner as in Example 1. Furthermore, the glass transition rate and activity index were measured in the same manner as in Example 1.
[0050] [Results] The composition and measurement results of the composite oxides of the Examples and Comparative Examples are shown in Table 1 (Part 1 and Part 2). In Table 1, the "T.Fe" column indicates the value of total iron content. In Table 1, the "Properties of Composite Oxides after Rapid Cooling" column indicates the properties of the composite oxides after rapid cooling. The "Appearance" column indicates the shape of the composite oxides. When the ratio of the major axis to the minor axis of the composite oxide exceeds 10.0, it is recorded as "fibrous"; when the ratio is less than 10.0, it is recorded as "granular". Furthermore, in Table 1, the "Color" column indicates that those with an ISO whiteness greater than 55 are marked as "white", those greater than 20 and less than 55 are marked as "grayish-white to blue", and those less than 20 are marked as "black".
[0051] [Table 1] Table 1 (Firstly) composition Equations (1) to (3) quenching medium Properties of composite oxides after rapid cooling evaluate CaO SiO2 Al2O3 MgO T.Fe B3 X Y Appearance color glass transition rate Activity index [%] quality% quality% quality% quality% quality% % 7 days 28 days 91 days Example 1 45.0 35.9 14.0 5.0 0.1 1.78 1.11 5.78 water granular white 99.5 60 94 104 Example 2 41.0 40.1 13.0 5.1 0.8 1.47 1.30 6.24 water granular white 98.1 59 90 97 Example 3 43.0 36.3 13.5 5.2 2.0 1.70 1.16 5.87 water granular white 97.8 57 93 98 Example 4 46.0 31.1 14.5 4.9 3.5 2.10 0.99 5.32 water granular white 98.0 59 95 108 Example 5 42.0 32.9 15.0 5.3 4.8 1.89 1.14 4.99 water granular white 97.1 61 94 107 Example 6 44.0 28.6 15.1 5.7 6.6 2.27 0.99 4.81 water granular Grayish white ~ blue 97.6 64 97 112 Example 7 41.0 31.1 14.8 5.4 7.7 1.97 1.12 4.87 water granular Grayish white ~ blue 99.4 67 96 110 Example 8 43.0 29.1 14.7 5.2 8.0 2.16 1.02 4.90 water granular Grayish white ~ blue 96.2 61 97 108 Example 9 35.0 40.2 16.3 8.0 0.5 1.48 1.61 4.61 water granular white 97.7 60 92 103 Example 10 43.0 29.5 17.3 8.2 2.0 2.32 1.09 4.19 water granular white 93.4 67 94 109 Example 11 32.0 40.3 15.3 9.1 3.3 1.40 1.74 4.73 water granular white 98.4 62 88 99 Example 12 41.0 26.4 18.0 10.0 4.6 2.61 1.08 3.74 water granular white 94.2 59 93 109 Example 13 38.0 23.7 21.7 8.7 7.9 2.89 1.19 2.84 water granular Grayish white ~ blue 93.4 74 92 110 Example 14 33.0 29.8 24.5 12.0 0.7 2.33 1.65 2.56 water granular white 97.4 74 96 108 Example 15 21.0 35.7 25.1 13.4 4.8 1.67 2.90 2.26 water granular white 98.4 64 94 107 Example 16 26.0 23.6 26.7 15.7 8.0 2.90 1.93 1.86 water granular Grayish white ~ blue 96.0 67 92 107 Example 17 48.0 28.5 12.0 8.4 3.1 2.40 0.84 6.38 water granular white 95.6 59 95 109 Example 18 48.0 25.1 13.0 8.6 5.3 2.77 0.79 5.62 water granular Grayish white ~ blue 90.6 77 94 112 Example 19 42.0 24.9 20.2 12.5 0.4 3.00 1.07 3.31 water granular white 90.2 71 92 106 Example 20 28.0 25.6 35.0 11.0 0.4 2.89 2.16 1.53 water granular white 93.8 76 95 106 Example 21 24.0 30.7 36.0 8.7 0.6 2.24 2.78 1.52 water granular white 97.4 76 97 108 Example 22 24.0 25.4 36.0 13.7 0.9 2.90 2.56 1.37 water granular white 94.1 74 94 104
[0052] [Table 2] Table 1 (Secondly) composition Equations (1) to (3) quenching medium Properties of composite oxides after rapid cooling evaluate CaO SiO2 Al2O3 MgO T.Fe B3 X Y Appearance color glass transition rate Activity index [%] quality% quality% quality% quality% quality% % 7 days 28 days 91 days Example 23 45.0 28.1 19.0 7.3 0.6 2.54 1.05 3.85 Air granular white 94.6 78 97 110 Example 24 42.0 24.5 23.0 8.4 2.1 3.00 1.13 2.89 Air granular white 90.3 69 94 107 Example 25 37.0 30.9 18.4 9.1 4.6 2.09 1.33 3.69 Air granular white 97.6 54 96 114 Example 26 39.0 30.0 16.9 7.4 6.7 2.11 1.20 4.08 Air granular Grayish white ~ blue 98.6 64 97 106 Example 27 33.0 33.9 18.4 6.9 7.8 1.72 1.58 3.64 Air granular Grayish white ~ blue 98.7 72 96 107 Example 28 37.0 41.3 14.2 7.4 0.1 1.42 1.50 5.51 Air granular white 99.0 59 88 100 Example 29 53.0 29.7 12.0 5.0 0.3 2.36 0.79 6.89 Air granular white 91.3 68 96 114 Example 30 20.0 28.3 35.0 16.0 0.7 2.51 3.17 1.38 Air granular white 92.6 69 97 108 Example 31 40.0 33.8 17.1 5.1 4.0 1.84 1.27 4.32 Air granular white 98.4 72 92 104 Example 32 46.0 23.5 16.2 8.1 6.2 2.99 0.86 4.29 Air granular Grayish white ~ blue 91.2 82 91 98 Example 33 42.0 27.6 13.2 9.2 8.0 2.33 0.97 5.27 Air granular Grayish white ~ blue 97.4 78 94 107 Comparative Example 1 42.0 29.1 14.8 5.8 8.3 2.15 1.05 4.80 water granular black 88.6 67 83 89 Comparative Example 2 43.0 22.3 14.6 7.6 12.5 2.92 0.86 4.47 water granular black 84.5 68 81 88 Comparative Example 3 34.0 20.2 13.7 7.6 24.5 2.74 1.00 3.96 water granular black 87.6 59 77 79 Comparative Example 4 50.0 24.4 15.4 10.0 0.2 3.09 0.80 4.83 water Grain size white 87.6 84 86 87 Comparative Example 5 47.0 23.9 14.6 12.1 2.4 3.08 0.82 4.86 water Grain size white 87.6 84 85 84 Comparative Example 6 28.0 40.3 21.3 6.7 3.7 1.39 2.20 3.21 water Grain size white 87.6 45 56 76 Comparative Example 7 29.0 45.3 17.8 7.6 0.3 1.20 2.18 4.17 water Grain size white 87.6 39 51 70 Comparative Example 8 54.0 28.5 12.4 4.7 0.4 2.49 0.76 6.65 water granular white 84.5 67 78 86 Comparative Example 9 54.0 27.3 14.7 3.8 0.2 2.66 0.78 5.53 water granular white 88.7 69 76 88 Comparative Example 10 20.0 26.1 33.8 19.4 0.7 2.80 3.00 1.36 water fibrous white 89.0 78 79 83 Comparative Example 11 18.0 25.7 34.0 17.6 4.7 2.71 3.32 1.29 water fibrous white 87.9 83 82 84 Comparative Example 12 21.0 24.0 33.4 14.6 7.0 2.88 2.73 1.35 water fibrous Grayish white ~ blue 88.1 82 83 86
[0053] The results shown in Table 1 confirm that, compared to the composite oxides of Comparative Examples 1-12, the composite oxides of Examples 1-33 exhibited improved glass transition rates and superior activity indices at a material age of 91 days. (Industrial Applicability)
[0054] The composite oxide for cement admixtures of the present invention can be applied to cement raw materials and is expected to be usable in various industrial fields.
Claims
1. A composite oxide for cementitious admixtures, comprising CaO, MgO, Al2O3, and SiO2, wherein the alkalinity B3 (the sum of CaO, MgO, and Al2O3 contents divided by the SiO2 content) is 1.40~3.00; the value X (the sum of SiO2 and Al2O3 contents divided by the CaO content) is 0.79 or higher; the value Y (the sum of CaO and SiO2 contents divided by the Al2O3 content) is 1.37 or higher; the total iron content is 8.0% by mass or less; the CaO content is 21.0~53.0% by mass; the MgO content is 4.5~16.0% by mass; the Al2O3 content is 14.2~36.0% by mass; and the SiO2 content is 23.5~42.0% by mass. The unit of measurement for the content of each component is mass.
2. As in claim 1, the composite oxide for cement admixtures, wherein, The above values for Y are below 8.
00.
3. The composite oxide for cementitious admixtures as requested in item 1 or 2, wherein, The total iron content mentioned above is 3.0% by mass or more.
4. A method for manufacturing a composite oxide for cementitious admixtures, comprising obtaining a composite oxide with the following adjusted composition: containing CaO, MgO, Al2O3 and SiO2; the basicity B3 obtained by dividing the sum of CaO, MgO and Al2O3 content by the SiO2 content is 1.40 to 3.00; the value X of the sum of SiO2 content and Al2O3 content divided by the CaO content is 0.79 or more; the value Y of the sum of CaO content and SiO2 content divided by the Al2O3 content is 1.37 or more; the total iron content is 8.0% by mass or less; the CaO content is 21.0 to 53.0% by mass; the MgO content is 4.5 to 16.0% by mass; the Al2O3 content is 14.2 to 36.0% by mass; and the SiO2 content is 23.5 to 42.0% by mass; and the above-mentioned composite oxide with adjusted composition in a molten state is rapidly cooled.
5. The method for manufacturing the composite oxide for cementitious admixtures as described in claim 4, wherein, When reducing iron obtained by direct reduction is melted in a submerged arc welding furnace, additives are added to produce slag, thereby obtaining a composite oxide with the above-mentioned adjusted composition.
Citation Information
Patent Citations
Method of producing ferrate cement by utilizing high activative slag of revolving furnace steel smelting
CN1004546B
A kind of low-carbon cement clinker and its preparation method and application
CN105669056B
A preparation method of modified slag wool reinforced cement concrete pavement
CN106904919B
Method for preparing cement mixture by utilizing converter slag
CN108609875A
High-iron phase-modified gehlenite high-activity cement clinker as well as preparation and application thereof
CN115159873A