Hierarchically wrinkled structure, method of manufacturing the same and antibacterial material including the same

TWI946152BActive Publication Date: 2026-11-11NATIONAL CHUNG HSING UNIVERSITY
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
TW114143363
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-11-06
Publication Date
2026-11-11
Estimated Expiration
2045-11-05

Smart Images

  • Figure TWG2TB001920904_001
    Figure TWG2TB001920904_001
  • Figure TWG2TB001920904_002
    Figure TWG2TB001920904_002
  • Figure TWG2TB001920904_003
    Figure TWG2TB001920904_003
Patent Text Reader

Abstract

This invention relates to a layered wrinkled structure, its manufacturing method, and an antibacterial material comprising the same. The manufacturing method involves performing multiple surface modification and stress-relieving steps on a stretched polymer substrate to obtain a layered wrinkled structure with improved hydrophobicity and antibacterial properties. Applying the obtained layered wrinkled structure to an antibacterial material can enhance its antibacterial effect.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for manufacturing a layered pleated structure, comprising: A stretching step is performed on a polydimethylsiloxane (PDMS) substrate in a length direction to obtain a first stretched substrate, wherein the stretching rate of the stretching step is 50% to 150%; a first surface modification step is performed on the first stretched substrate to obtain a first surface modified substrate, wherein the first surface modification step includes inductively coupled plasma-reactive ion etching (ICP-RIE), the first surface modified substrate includes a first silicate hard layer and a soft layer, the first silicate hard layer is located on the soft layer, and the thickness of the first silicate hard layer is 100 nm to 500 nm; a first stress relief step is performed on the first surface modified substrate to obtain a first stress-relieved substrate, wherein the stress relief rate of the first stress relief step is 20% to 60%, the first stress-relieved substrate includes a first wrinkled structure, and the first wrinkled structure is located on the soft layer; A second surface modification step is performed on a surface of the first stress-relieving substrate having the first wrinkled structure to obtain a second surface-modified substrate, wherein the second surface modification step includes ultraviolet ozone (UV-Ozone) treatment, the second surface-modified substrate includes a second silicate hard layer located on the soft layer, and the thickness of the second silicate hard layer is 1 μm to 100 μm; a second stress-relieving step is performed on the second surface-modified substrate to obtain a second stress-relieving substrate, wherein the second stress-relieving substrate includes a second wrinkled structure, and the second wrinkled structure is located between the first wrinkled structure and the soft layer; and the first wrinkled structure and the second wrinkled structure on the second stress-relieving substrate are transferred to a second polymer substrate to obtain the layered wrinkled structure, wherein the layered wrinkled structure is located on the second polymer substrate.

2. A method for manufacturing a layered pleated structure as claimed in claim 1, wherein the first pleated structure has a first waveform amplitude, and the first waveform amplitude is from 500 nm to 3 μm.

3. A method for manufacturing a layered pleated structure as described in claim 1, wherein the second pleated structure has a second waveform amplitude, and the second waveform amplitude is from 5 μm to 150 μm.

4. A layered pleated structure, which is manufactured using the manufacturing method of the layered pleated structure described in any one of claims 1 to 3.

5. An antibacterial material comprising the layered pleated structure described in claim 4.

Citation Information

Patent Citations

  • Method for preparing multistage micro-nano fold structure

    CN114318262A

  • Method for producing fully hydrophobic material having layered structure and use thereof

    CN117881524A

  • Fouling-reducing additives, process for production thereof and use thereof in coatings

    TW201418386A