Semiconductor structure and manufacturing method therefor

By constructing a buried gate structure in the semiconductor structure and using a combination of dielectric layer, word line, isolation layer and insulating layer, the GIDL problem caused by the overlap of the word line and the drain region is solved, and the performance and stability of the semiconductor structure are improved. sex.

WO2024198373A1PCT designated stage expired Publication Date: 2024-10-03CHANGXIN MEMORY TECH INC
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/131154
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-27
Filing Date
2023-11-13
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

With the development of DRAM integration and consumer demand for miniaturized electronic devices, the size of transistors continues to shrink, resulting in shrinking word line spacing and isolation structures of memory arrays, resulting in gate-induced drain leakage (GIDL) and channel Leakage and other issues pose challenges to device performance and reliability.

Method used

A semiconductor structure is provided, which includes a word line trench in a substrate, a dielectric layer covering the bottom and side walls of the word line trench, the word line is located on the inner wall of the dielectric layer and fills part of the trench, the top of the word line has a protrusion, and the isolation layer fills In the recess of the protruding part, the insulating layer is located above the word line and isolation layer and fills the trench. The dielectric constant of the insulating layer is smaller than the dielectric constant of the isolation layer, forming a buried gate structure to reduce the word line and drain area. of overlapping area and electric field.

Benefits of technology

By reducing the overlapping area and electric field between the word line and the drain region, the gate-induced drain leakage current is significantly reduced, the stability and performance of the semiconductor structure is improved, and power consumption is reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023131154_03102024_PF_FP_ABST
    Figure CN2023131154_03102024_PF_FP_ABST
Patent Text Reader

Abstract

Disclosed are a semiconductor structure and a manufacturing method therefor. The semiconductor structure comprises: a substrate provided with a word line trench, the bottom and the side wall of the word line trench being covered with a dielectric layer; a word line that is located on the inner wall of the dielectric layer and fills part of the word line trench, the top of the word line being provided with a protruding portion that protrudes in the vertical direction; an isolation layer filling a recess on at least one side of the protruding portion; and an insulating layer that is located above the word line and the isolation layer and fully fills the word line trench, the dielectric constant of the insulating layer being less than that of the isolation layer.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor structure and method for manufacturing the same

[0001] Cross-references

[0002] The present disclosure claims priority to Chinese patent application number 2023103043690, entitled “Semiconductor structure and manufacturing method thereof,” filed on March 27, 2023, which is incorporated herein by reference in its entirety. Technical Field

[0003] The present disclosure relates to the field of semiconductors, and in particular to a semiconductor structure and a method for manufacturing the same. Background Art

[0004] Memory is a component used to store programs and various data. Random Access Memory (RAM) commonly used in computer systems can be divided into two types: Dynamic Random Access Memory (DRAM) and Static Random Access Memory (SRAM). DRAM is a commonly used semiconductor memory device in computers, consisting of many repeated memory cells.

[0005] A memory cell typically includes a capacitor and a transistor. The drain of the transistor is connected to a bit line structure, and the source is connected to a capacitor. The capacitor includes a capacitor contact structure and a capacitor. The word line structure of the memory cell can control the opening or closing of the channel region of the transistor, thereby reading the data information stored in the capacitor through the bit line structure, or writing the data information into the capacitor for storage through the bit line structure.

[0006] Summary of the Invention

[0007] The embodiments of the present disclosure provide a semiconductor structure and a method for manufacturing the same, which are at least beneficial to improving the performance of the semiconductor structure.

[0008] According to some embodiments of the present disclosure, on the one hand, embodiments of the present disclosure provide a semiconductor structure, including: a substrate, having a word line groove therein; a dielectric layer, the dielectric layer covering the bottom and sidewalls of the word line groove; a word line, the word line being located on the inner wall of the dielectric layer and filling a portion of the word line groove, the top of the word line having a protrusion protruding in a vertical direction; an isolation layer, the isolation layer filling a recess on at least one side of the protrusion; an insulating layer, the insulating layer being located above the word line and the isolation layer and filling the word line groove, the dielectric constant of the insulating layer being smaller than the dielectric constant of the isolation layer.

[0009] In some embodiments, the material of the isolation layer is a high dielectric constant material, and the dielectric constant of the material of the isolation layer is greater than 10.

[0010] In some embodiments, the word line includes: a gate layer, which fills a portion of the word line trench; a first work function layer, which is located between the dielectric layer and the gate layer; wherein the gate layer has a protrusion higher than the top of the first work function layer, and the isolation layer is located above the first work function layer.

[0011] In some embodiments, the word line includes: a first gate conductive layer, the first gate conductive layer is located on the inner wall of the dielectric layer and fills a portion of the word line trench; a second gate conductive layer, the second gate conductive layer is located above the first gate conductive layer and fills a portion of the word line trench; a first work function layer, the first work function layer is located between the first gate conductive layer and the second gate conductive layer, and is also located between the second gate conductive layer and the dielectric layer; wherein the second gate conductive layer has a protrusion higher than the top of the first work function layer, and the isolation layer is located above the first work function layer.

[0012] In some embodiments, one of the first gate conductive layer or the second gate conductive layer is doped polysilicon.

[0013] In some embodiments, the semiconductor structure also includes: a second work function layer, the second work function layer is located between the dielectric layer and the isolation layer, and the second work function layer is located above the first work function layer, the bottom surface of the second work function layer is flush with the top surface of the first work function layer, and the top of the second work function layer is higher than or flush with the top of the protrusion.

[0014] In some embodiments, the materials of the first work function layer and the second work function layer both include titanium nitride or titanium aluminide.

[0015] In some embodiments, a thickness of the first work function layer is less than a thickness of the second work function layer.

[0016] In some embodiments, a portion of a sidewall of the protrusion is parallel to the vertical direction, and a top surface of the protrusion is parallel to a top surface of the substrate.

[0017] In some embodiments, in a direction perpendicular to the surface of the substrate, a top surface of the isolation layer is higher than or flush with a top surface of the protrusion.

[0018] In some embodiments, the dielectric layer includes: a first dielectric layer, the first dielectric layer covers the bottom and sidewalls of the word line trench; and a second dielectric layer, the second dielectric layer covers the inner wall of the first dielectric layer, wherein the density of the first dielectric layer is greater than the density of the second dielectric layer.

[0019] According to some embodiments of the present disclosure, on the other hand, embodiments of the present disclosure further provide a method for manufacturing a semiconductor structure, including: providing a substrate having a word line groove therein; forming a dielectric layer, the dielectric layer covering the bottom and sidewalls of the word line groove; forming a word line, the word line being located on the inner wall of the dielectric layer and filling a portion of the word line groove, the top of the word line having a protrusion protruding in a vertical direction, the top surface of the protrusion being lower than the surface of the substrate; forming an isolation layer, the isolation layer filling a recess on at least one side of the protrusion; forming an insulating layer, the insulating layer being located above the word line and the isolation layer and filling the word line groove, the dielectric constant of the insulating layer being smaller than the dielectric constant of the isolation layer.

[0020] In some embodiments, forming the dielectric layer includes: forming a second dielectric layer using a deposition process, wherein the second dielectric layer covers the bottom and sidewalls of the word line trench; and forming a first dielectric layer on the contact surface between the second dielectric layer and the substrate using a thermal oxidation process, wherein the density of the first dielectric layer is greater than the density of the second dielectric layer.

[0021] In some embodiments, forming a word line includes: forming a first work function layer, the first work function layer covers the inner wall of the dielectric layer; forming a gate layer, the gate layer covers the surface of the first work function layer and fills the word line groove; and patterning the first work function layer and the gate layer so that the gate layer has a protrusion higher than the top of the first work function layer.

[0022] In some embodiments, forming a word line includes: forming a first gate conductive layer, the first gate conductive layer is located on a portion of the inner wall of the dielectric layer and fills a portion of the word line groove; forming a first work function layer, the first work function layer covers the surface of the first gate conductive layer and also covers a portion of the inner wall of the dielectric layer; forming a second gate conductive layer, the second gate conductive layer covers the first work function layer and fills a portion of the word line groove; patterning the second gate conductive layer and the first work function layer so that the second gate conductive layer has a protrusion higher than the top of the first work function layer.

[0023] In some embodiments, after forming the word line and before forming the isolation layer, it also includes: forming a second work function layer, the second work function layer covers a portion of the surface of the dielectric layer and is located above the first work function layer, the bottom surface of the second work function layer is flush with the top surface of the first work function layer, and the top of the second work function layer is higher than or flush with the top of the protrusion. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] One or more embodiments are exemplarily illustrated by the pictures in the corresponding drawings. These exemplified descriptions do not constitute a limitation on the embodiments. Unless otherwise stated, the pictures in the drawings do not constitute a scale limitation. In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the traditional technology, the drawings required in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without making any creative work.

[0025] FIG1 is a schematic diagram of a first semiconductor structure provided by an embodiment of the present disclosure;

[0026] FIG2 is a schematic diagram of a second semiconductor structure provided by an embodiment of the present disclosure;

[0027] FIG3 is a schematic diagram of a third semiconductor structure provided by an embodiment of the present disclosure;

[0028] FIG4 is a schematic diagram of a fourth semiconductor structure provided by an embodiment of the present disclosure;

[0029] FIG5 is a schematic diagram of a fifth semiconductor structure provided by an embodiment of the present disclosure;

[0030] FIG6 is a schematic diagram of a sixth semiconductor structure provided by an embodiment of the present disclosure;

[0031] FIG7 is a schematic diagram of a seventh semiconductor structure provided by an embodiment of the present disclosure;

[0032] FIG8 is a schematic diagram of an eighth semiconductor structure provided by an embodiment of the present disclosure;

[0033] FIG9 is a schematic structural diagram of a substrate provided by another embodiment of the present disclosure;

[0034] FIG10 is a structural schematic diagram corresponding to a step of forming a dielectric layer according to another embodiment of the present disclosure;

[0035] FIG11 is a structural schematic diagram corresponding to another step of forming a dielectric layer provided by another embodiment of the present disclosure;

[0036] FIG12 is a structural diagram corresponding to a step of forming a word line according to another embodiment of the present disclosure;

[0037] FIG13 is a structural diagram corresponding to a step of forming an initial word line according to another embodiment of the present disclosure;

[0038] FIG14 is a structural schematic diagram corresponding to a step of forming a mask layer provided by another embodiment of the present disclosure;

[0039] FIG15 is a structural schematic diagram corresponding to the steps of forming an initial first word line, a mask layer, and an initial second word line according to another embodiment of the present disclosure;

[0040] FIG16 is a structural diagram corresponding to another step of forming a word line according to another embodiment of the present disclosure;

[0041] FIG. 17 is a structural diagram corresponding to yet another step of forming a word line provided in another embodiment of the present disclosure. DETAILED DESCRIPTION

[0042] With the increasing integration of DRAM and consumer demand for miniaturized electronic devices, transistor size continues to shrink, and buried wordline dynamic random access memory (DRAM) has become mainstream to meet the various requirements of semiconductor structures. At the same time, as size shrinks, wordline spacing and the isolation structure of the memory array continue to shrink, and problems such as gate-induced drain leakage (GIDL) and channel leakage in transistors are becoming increasingly serious, posing significant challenges to device performance and reliability. In theory, the gate and drain regions of a transistor structure need to be strictly aligned, but in practice, when doping the drain, an overlap between the drain and gate is unavoidable. For example, for an NMOS tube, when the gate of the NMOS is at a negative voltage, a large electric field will be generated in the overlapping area of ​​the gate and the drain, and a thin depletion region will appear near the gate dielectric layer. Due to the thin depletion region and the higher electric field, an avalanche multiplication effect and a band-to-band tunneling effect will occur (electrons tunnel directly from the valence band of the P region to the conduction band of the N region), thereby generating minority carriers in the drain under the gate and being pushed into the substrate by the negative voltage applied by the gate, thereby increasing the gate-induced drain leakage current.

[0043] According to some embodiments of the present disclosure, an embodiment of the present disclosure provides a semiconductor structure, which is at least beneficial for improving the GIDL effect in the semiconductor structure.

[0044] The following describes various embodiments of the present disclosure in detail with reference to the accompanying drawings. However, those skilled in the art will appreciate that many technical details are provided in the various embodiments of the present disclosure to facilitate a better understanding of the present disclosure. However, even without these technical details and the various variations and modifications based on the following embodiments, the technical solutions claimed in the present disclosure can still be implemented.

[0045] FIG1 is a schematic diagram of a first semiconductor structure provided in an embodiment of the present disclosure, FIG2 is a schematic diagram of a second semiconductor structure provided in an embodiment of the present disclosure, FIG3 is a schematic diagram of a third semiconductor structure provided in an embodiment of the present disclosure, FIG4 is a schematic diagram of a fourth semiconductor structure provided in an embodiment of the present disclosure, FIG5 is a schematic diagram of a fifth semiconductor structure provided in an embodiment of the present disclosure, FIG6 is a schematic diagram of a sixth semiconductor structure provided in an embodiment of the present disclosure, FIG7 is a schematic diagram of a seventh semiconductor structure provided in an embodiment of the present disclosure, and FIG8 is a schematic diagram of an eighth semiconductor structure provided in an embodiment of the present disclosure. The semiconductor structures provided in this embodiment will be described in detail below with reference to the accompanying drawings, as follows:

[0046] 1 to 8 , a semiconductor structure includes: a substrate 100 having a wordline trench 110 therein; a dielectric layer 101 covering the bottom and sidewalls of the wordline trench 110; a wordline 102 located on the inner wall of the dielectric layer 101 and partially filling the wordline trench 110, with the top of the wordline 102 having a vertically protruding portion 112; an isolation layer 103 filling a recess on at least one side of the protruding portion 112; and an insulating layer 104 located above the wordline 102 and the isolation layer 103 and completely filling the wordline trench 110. The dielectric constant of the insulating layer 104 is less than that of the isolation layer 103.

[0047] The dielectric layer 101 and wordline 102 located within the wordline trench 110 can form a buried gate structure. The buried gate can increase the integration density of the semiconductor structure, while also increasing the area of ​​the channel region, improving the gate's control over the transistor, and reducing the short channel effect. The top of the wordline 102 has a vertically protruding portion 112. When the source and drain regions are formed on both sides of the wordline 102, the overlapping area between the wordline 102 and the drain region can be reduced, thereby reducing gate-induced drain leakage current and improving the performance of the semiconductor structure. In addition, the isolation layer 103 fills the recess on at least one side of the protruding portion 112. The isolation layer 103 can further reduce the possibility of leakage between the wordline 102 and the drain region, significantly reducing the effect of quantum tunneling in the dielectric layer 101, thereby reducing gate-induced drain leakage current and the resulting power consumption, and improving the stability of the semiconductor structure. In addition, the insulating layer 104 is located above the word line 102 and the isolation layer 103 and fully fills the word line trench 110, which can insulate the word line 102 from other structures in the semiconductor structure to prevent leakage between the word line 102 and other structures. The dielectric constant of the insulating layer 104 is smaller than the dielectric constant of the isolation layer 103, that is, the insulation performance of the isolation layer 103 is greater than the insulation performance of the insulating layer 104. The isolation layer 103 can effectively weaken the electric field generated between the word line 102 and the drain region, reduce the gate-induced drain leakage current between the word line 102 and the drain region, and improve the stability of the semiconductor structure.

[0048] Regarding the substrate 100, the material of the substrate 100 includes a basic semiconductor, a compound semiconductor, or an alloy semiconductor. For example, a basic semiconductor includes silicon or germanium (Ge); a compound semiconductor includes silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, and / or Group III-V semiconductor materials; and an alloy semiconductor includes silicon germanium (SiGe), silicon germanium carbide, tin germanium, silicon germanium tin, gallium arsenic phosphide, gallium indium phosphide, gallium indium arsenide, indium gallium arsenide phosphide, aluminum indium arsenide, and / or aluminum gallium arsenide. In some embodiments, the substrate may also be a silicon-on-insulator structure, a silicon-germanium-on-insulator structure, a germanium-on-insulator structure, or a combination thereof.

[0049] It should be noted that in FIG1 , the U-shaped cross-section of the wordline trench 110 along the vertical direction is used as an example, which does not constitute a limitation on the shape of the wordline trench 110. In some embodiments, the wordline trench may also be in an inverted trapezoidal shape or a rectangle, that is, the horizontal width of the wordline trench gradually decreases or remains constant in the direction toward the substrate. It is understood that when the wordline trench is in an inverted trapezoidal shape or a rectangle, the corners at the bottom of the wordline trench may be chamfered to prevent the formation of sharp points after the wordline is filled, which may cause tip discharge, thereby improving the stability of the semiconductor structure.

[0050] Regarding the dielectric layer 101 , the material of the dielectric layer 101 includes silicon oxide, hafnium oxide, titanium oxide, hafnium zirconium oxide, tantalum oxide, hafnium silicate, zirconium oxide or zirconium silicate, etc.

[0051] In some embodiments, referring to FIG. 2 , dielectric layer 101 includes: a first dielectric layer 111, which covers the bottom and sidewalls of wordline trench 110; and a second dielectric layer 121, which covers the inner wall of first dielectric layer 111. The first dielectric layer 111 has a greater density than the second dielectric layer 121. The first dielectric layer 111 facilitates improving the interfacial bonding between the second dielectric layer 121 and substrate 100. Furthermore, the dielectric layer 101, formed by the first and second dielectric layers 111 and 121, has a higher density, which helps prevent charge capture in the dielectric layer 101 and improves the performance of the semiconductor structure.

[0052] Regarding the first dielectric layer 111 and the second dielectric layer 121 , the materials of the first dielectric layer 111 and the second dielectric layer 121 may both include silicon oxide, and the oxygen content of the second dielectric layer 121 is greater than that of the first dielectric layer 111 .

[0053] In some embodiments, the dielectric layer 101 may also be a single-layer structure.

[0054] Regarding the word line 102 , a material of the word line 102 includes at least one of polysilicon, titanium nitride, titanium aluminide, tantalum nitride, nickel silicide, cobalt silicide, tantalum, aluminum, cobalt, titanium, or tungsten.

[0055] In some embodiments, referring to FIG3 , wordline 102 includes: a gate layer 122, which partially fills wordline trench 110; a first work function layer 132, which is located between dielectric layer 101 and gate layer 122; wherein gate layer 122 has a protrusion 112 that is higher than the top of first work function layer 132; and isolation layer 103 is located above first work function layer 132. It will be appreciated that the threshold voltage can depend on the flatband voltage, which in turn can depend on the work function. The work function can be adjusted through various methods, for example, by adjusting the material used for the wordline or by adjusting the material between the wordline and the channel in the substrate. Adjusting the work function may shift the flatband voltage; a high work function may shift the flatband voltage in a positive direction, while a low work function may shift the flatband voltage in a negative direction. Thus, the threshold voltage can be adjusted by shifting the flatband voltage, even when the channel doping concentration is reduced or omitted. Therefore, the first work function layer 132 may be beneficial for adjusting the threshold voltage.

[0056] Regarding the gate layer 122 , the material of the gate layer 122 includes at least one of polysilicon, titanium nitride, titanium aluminide, tantalum nitride, nickel silicide, cobalt silicide, tantalum, aluminum, lanthanum, titanium, or tungsten.

[0057] In some embodiments, referring to FIG4 , the word line 102 includes: a first gate conductive layer 142 , the first gate conductive layer 142 is located on the inner wall of the dielectric layer 101 and fills a portion of the word line trench 110 ; a second gate conductive layer 152 , the second gate conductive layer 152 is located above the first gate conductive layer 142 and fills a portion of the word line trench 110 ; a first work function layer 132 , the first work function layer 132 is located between the first gate conductive layer 142 and the second gate conductive layer 152 , and is also located between the second gate conductive layer 152 and the dielectric layer 101 ; wherein the second gate conductive layer 152 has a protrusion 112 higher than the top of the first work function layer 132 , and the isolation layer 103 is located above the first work function layer 132 . In this way, the first gate conductive layer 142 located at the bottom of the word line trench 110 can serve as a first word line to control the channel at the bottom of the word line trench 110. The second gate conductive layer 152 and the first work function layer 132 located on the first gate conductive layer 142 can serve as a second word line to control the channels on both sides of the word line trench 110. The first word line and the second word line together constitute the word line 102, so that the word line 102 can control the channels at the bottom and sidewalls of the word line trench 110 respectively, thereby improving the control ability of the word line 102. Among them, the first work function layer 132 located between the first gate conductive layer 142 and the second gate conductive layer 152 can serve as an adhesion layer between the first gate conductive layer 142 and the second gate conductive layer 152, so as to facilitate the interface bonding between the first gate conductive layer 142 and the second gate conductive layer 152; in addition, the first work function layer 132 can also serve as a barrier layer between the first gate conductive layer 142 and the second gate conductive layer 152, which is beneficial to avoid diffusion between the first gate conductive layer 142 and the second gate conductive layer 152, improve the performance of the first gate conductive layer 142 and the second gate conductive layer 152, and thereby improve the stability of the semiconductor structure.

[0058] Regarding the first work function layer 132 , the material of the first work function layer 132 includes titanium, tantalum, titanium-tantalum alloy, titanium nitride, titanium aluminide, or the like.

[0059] In some embodiments, the substrate on both sides of the word line trench may have a source region (not shown) and a drain region (not shown), and the top surface of the first work function layer 132 may be higher than or flush with the bottom surface of the source region or the drain region.

[0060] In some embodiments, either the first gate conductive layer 142 or the second gate conductive layer 152 is doped polysilicon. For example, the doping ions may be P-type or N-type doping ions. N-type ions may specifically be phosphorus ions, arsenic ions, or antimony ions; P-type ions may specifically be boron ions, indium ions, or boron fluoride ions. Doping polysilicon helps improve the conductivity of the first gate conductive layer 142 or the second gate conductive layer 152, reduce word line resistance, reduce latency, and improve the signal transmission efficiency of the word line 102. Polysilicon can be doped with impurities of different polarities to change its work function. By making either the first gate conductive layer 142 or the second gate conductive layer 152 of doped polysilicon, the threshold voltage of the first gate conductive layer 142 or the second gate conductive layer 152 and the first work function layer 132 can be controlled together.

[0061] In some embodiments, referring to Figures 5 and 6, the semiconductor structure also includes: a second work function layer 162, the second work function layer 162 is located between the dielectric layer 101 and the isolation layer 103, and the second work function layer 162 is located above the first work function layer 132, the bottom surface of the second work function layer 162 is flush with the top surface of the first work function layer 132, the second work function layer 162 is electrically contacted with the first work function layer 132, and the top of the second work function layer 162 is higher than or flush with the top of the protrusion 112. The second work function layer 162 can improve the interface state between the isolation layer 103 and the dielectric layer 101, and the bottom of the second work function layer 162 is in electrical contact with the word line 102. In the vertical direction, the second work function layer 162 and the protruding portion 112 of the word line are located in corresponding height intervals. This can make it easier for the word line 102 to drive electrons in the gate-drain overlap region to move toward the channel, thereby reducing the number of electrons in the gate-drain overlap region and reducing the electric field in the gate-drain overlap region, thereby suppressing the GIDL current in the gate-drain overlap region. At the same time, because electrons are more easily driven to move toward the channel, the movement of electrons can be effectively controlled without applying a large driving voltage to achieve regulation of the threshold voltage.

[0062] In some embodiments, the work function of the material of the first work function layer 132 is greater than the work function of the material of the second work function layer 162. As a result, the word line 102 located below the protrusion 112 is less sensitive to electrons in the channel, making it less likely to induce leakage current in the channel. At the same time, the channel can accommodate more electrons. Furthermore, the smaller work function of the second work function layer 162 allows electrons in the gate-drain overlap region to flow more easily into the channel, thereby reducing the GIDL current in the gate-drain overlap region and adjusting the threshold voltage.

[0063] The second work function layer 162 may be made of titanium, tantalum, a titanium-tantalum alloy, titanium nitride, or titanium aluminide. For example, when the second work function layer 162 is made of titanium aluminide and the isolation layer 103 is made of hafnium dioxide, titanium aluminide can effectively improve the interface state between hafnium dioxide and the dielectric layer 101.

[0064] In some embodiments, the material of the first work function layer 132 is different from the material of the second work function layer 162. In some embodiments, the material of the first work function layer 132 is the same as the material of the second work function layer 162.

[0065] In some embodiments, the thickness of the first work function layer 132 is less than the thickness of the second work function layer 162 in a direction perpendicular to the sidewalls of the word line trench 110. As a result, the second work function layer 162 can be closer to the protrusion 112, so that the bottom of the second work function layer 162 is in electrical contact with the word line 102, thereby facilitating the control of the threshold voltage and improving the performance of the semiconductor structure.

[0066] In some embodiments, the thickness of the first work function layer 132 ranges from 2 to 5 nm, for example, 2 nm, 2.5 nm, 2.8 nm, 3.1 nm, 3.2 nm, 3.6 nm, 4.1 nm, 4.7 nm, or 5 nm. It is understood that the thicker the first work function layer 132, the more difficult it is for the corresponding word line to drive the transistor, and the thinner the first work function layer 132, the less conducive it is to regulating the threshold voltage. Therefore, the thickness of the first work function layer 132 needs to be adjusted within an appropriate range to improve the performance of the semiconductor structure. In some embodiments, the thickness of the second work function layer 162 ranges from 3 to 7 nm, for example, 3.2 nm, 3.6 nm, 4.1 nm, 4.7 nm, 5.5 nm, 6.0 nm, 6.9 nm, or 7 nm. Similarly, the thickness of the second work function layer 162 needs to be within an appropriate range to facilitate the flow of electrons in the channel to the channel, thereby improving the stability of the semiconductor structure.

[0067] It should be noted that the shape of the protrusion 112 shown in Figures 1 to 6 does not constitute a limitation on the shape of the protrusion 112. In some embodiments, part of the sidewall of the protrusion 112 is parallel to the vertical direction, and the top surface of the protrusion 112 is parallel to the surface of the substrate 100. For example, the shape of the protrusion 112 can be rectangular. It is understood that when the shape of the protrusion 113 is rectangular, the top and bottom corners of the protrusion 112 can be chamfered, such as by isotropic wet etching, to avoid the protrusion 112 having a tip and causing a tip discharge phenomenon. In addition, the sidewalls of the protrusion 112 are parallel to the vertical direction. Compared with the Ω-shaped protrusion 112, it can avoid the dimensional change of the protrusion 112 causing a tip at the top or bottom corner of the protrusion 112, thereby avoiding the tip discharge effect.

[0068] In some embodiments, the top surface of the isolation layer is higher than or flush with the top surface of the protrusion in a direction perpendicular to the substrate surface. That is, the isolation layer may be located only in the depression on at least one side of the protrusion, or may cover the top surface of the protrusion, i.e., wrap around the protrusion, to improve the isolation between the top of the word line and other structures.

[0069] In some embodiments, the isolation layer 103 is made of a high-k dielectric material, for example, a dielectric constant greater than 10. For example, the isolation layer may be made of a high-k dielectric material such as hafnium oxide, titanium oxide, hafnium zirconium oxide, tantalum oxide, hafnium silicate, zirconium oxide, or zirconium silicate. Using a high-k dielectric material as the isolation layer 103 can significantly reduce the quantum tunneling effect of the dielectric layer 101, thereby reducing gate leakage current and the resulting power consumption.

[0070] The insulating layer 104 is made of silicon oxide, silicon nitride, or silicon oxynitride, etc. The insulating layer 104 is located above the word line 102 and the isolation layer 103 and fills the word line trench 110 to insulate the word line 102 from other structures in the semiconductor structure.

[0071] In some embodiments, referring to FIG. 7 , a substrate 100 may include multiple wordline trenches 110. The substrate 100 includes active areas arranged in an array, each of which intersects two wordlines. For example, a vertical cross-section of each active area may include two wordline trenches 110, as shown in FIG. Isolation structures 105 are provided on opposite sides of the active areas traversed by the two wordline trenches 110 to prevent mutual interference between wordlines 102 within wordline trenches 110 in adjacent active areas. Thus, the dielectric layer 101 and wordlines 102 within the wordline trenches 110 can form the gates of transistor structures. The substrate 100 on either side of the wordline trenches 110 can be used to form the source regions S or drain regions D of the transistor structures. Furthermore, the substrate 100 between two adjacent wordline trenches 110 can serve as two transistor source regions S or drain regions D, thereby facilitating improved semiconductor structure integration density.

[0072] In some embodiments, the lower surface of the source region S or the drain region D is further away from the substrate 100 than the lower surface of the isolation layer 103, and the lower surface of the source region S or the drain region D is closer to the substrate 100 than the upper surface of the isolation layer 103. This is conducive to reducing the possibility of leakage between the word line 102 and the drain region D, significantly reducing the effect of quantum tunneling in the dielectric layer 101, and further reducing gate-induced drain leakage current and the power consumption caused by it, thereby improving the stability of the semiconductor structure.

[0073] Regarding the isolation structure 105 , the material of the isolation structure 105 includes at least one of silicon oxide, silicon nitride, or silicon oxynitride.

[0074] It should be noted that the structures of the different word lines in the above embodiments can be combined with the application scenario shown in FIG7 to form a new embodiment. For example, referring to FIG8 , the word line 102 includes: a first gate conductive layer 142, the first gate conductive layer 142 is located on the inner wall of the dielectric layer 101 and fills a portion of the word line trench 110; a second gate conductive layer 152, the second gate conductive layer 152 is located above the first gate conductive layer 142 and fills a portion of the word line trench 110; a first work function layer 132, the first work function layer 132 is located between the first gate conductive layer 142 and the second gate conductive layer 152, and is also located between the second gate conductive layer 152 and the dielectric layer 101; wherein the second gate conductive layer 152 is located between the first gate conductive layer 142 and the second gate conductive layer 152. The conductive layer 152 has a protrusion 112 that is higher than the top of the first work function layer 132, and the isolation layer 103 is located above the first work function layer 132. The semiconductor structure also includes: a second work function layer 162, which is located between the dielectric layer 101 and the isolation layer 103 and above the first work function layer 132. The bottom surface of the second work function layer 162 is flush with the top surface of the first work function layer 132, and the top of the second work function layer 162 is higher than or flush with the top of the protrusion 112. In this way, the beneficial effects described in the above embodiments can be achieved in the application scenario shown in Figure 7.

[0075] The semiconductor structure provided by the embodiment of the present disclosure can form a buried gate structure by using the dielectric layer 101 and the word line 102 located in the word line trench 110. The buried gate can improve the integration density of the semiconductor structure, while also increasing the area of ​​the channel region, improving the gate's control over the transistor, and reducing the short channel effect. The top of the word line 102 has a protrusion 112 that protrudes in a vertical direction. When the source region and the drain region are formed on both sides of the word line 102, the overlapping area between the word line 102 and the drain region can be reduced, thereby reducing the gate-induced drain leakage current and improving the performance of the semiconductor structure. In addition, the isolation layer 103 fills the recess on at least one side of the protrusion. The isolation layer 103 can further reduce the possibility of leakage between the word line 102 and the drain region, thereby significantly reducing the effect of quantum tunneling of the dielectric layer 101, thereby reducing the gate-induced drain leakage current and the power consumption caused by it, and improving the stability of the semiconductor structure. In addition, the insulating layer 104 is located above the word line 102 and the isolation layer 103 and fully fills the word line trench 110, which can insulate the word line 102 from other structures in the semiconductor structure to prevent leakage between the word line 102 and other structures. The dielectric constant of the insulating layer 104 is smaller than the dielectric constant of the isolation layer 103, that is, the insulation performance of the isolation layer 103 is greater than the insulation performance of the insulating layer 104. The isolation layer 103 can effectively weaken the electric field generated between the word line 102 and the drain region, reduce the gate-induced drain leakage current between the word line 102 and the drain region, and improve the stability of the semiconductor structure.

[0076] According to some embodiments of the present disclosure, another embodiment of the present disclosure provides a method for manufacturing a semiconductor structure, which can be used to form the above-mentioned semiconductor structure to improve the performance of the semiconductor structure. It should be noted that for the parts that are the same or corresponding to the above-mentioned embodiments, reference can be made to the corresponding description of the above-mentioned embodiments, and will not be repeated in detail below.

[0077] FIG9 is a schematic structural diagram of a substrate provided in another embodiment of the present disclosure, FIG10 is a schematic structural diagram corresponding to a step of forming a dielectric layer provided in another embodiment of the present disclosure, FIG11 is a schematic structural diagram corresponding to another step of forming a dielectric layer provided in another embodiment of the present disclosure, FIG12 is a schematic structural diagram corresponding to a step of forming a word line provided in another embodiment of the present disclosure, FIG13 is a schematic structural diagram corresponding to a step of forming an initial word line provided in another embodiment of the present disclosure, FIG14 is a schematic structural diagram corresponding to a step of forming a mask layer provided in another embodiment of the present disclosure, FIG15 is a schematic structural diagram corresponding to a step of forming an initial first word line, a mask layer, and an initial second word line provided in another embodiment of the present disclosure, FIG16 is a schematic structural diagram corresponding to another step of forming a word line provided in another embodiment of the present disclosure, and FIG17 is a schematic structural diagram corresponding to yet another step of forming a word line provided in another embodiment of the present disclosure. The semiconductor structure manufacturing method provided in this embodiment will be described in detail below with reference to the accompanying drawings, as follows:

[0078] 1 , 3 to 6 , and 9 to 17 , a method for manufacturing a semiconductor structure includes:

[0079] 9 , a substrate 100 is provided, and a word line trench 110 is formed in the substrate 100 .

[0080] In some embodiments, the process used to form the word line trench 110 may be a dry etching process or a wet etching process.

[0081] 10 , a dielectric layer 101 is formed to cover the bottom and sidewalls of the word line trench 110 .

[0082] In some embodiments, referring to FIG. 11 , forming the dielectric layer 101 includes: forming a second dielectric layer 121 using a deposition process, where the second dielectric layer 121 covers the bottom and sidewalls of the wordline trench 110; and forming a first dielectric layer 111 using a thermal oxidation process at the interface between the second dielectric layer 121 and the substrate 100, wherein the density of the first dielectric layer 111 is greater than the density of the second dielectric layer 121. The deposition process can form a second dielectric layer 121 with good uniformity, and the thermal oxidation process can further oxidize the substrate 100, thereby increasing the density of the second dielectric layer 121. The greater density of the first dielectric layer 111 than the second dielectric layer 121 can help improve the interfacial bonding strength between the second dielectric layer 121 and the substrate 100.

[0083] In some embodiments, the deposition process may be a chemical vapor deposition (CVD) process, a physical vapor deposition (PVD) process, or an atomic layer deposition (ALD) process.

[0084] In some embodiments, the thermal oxidation process may employ an oxidation process such as wet or dry thermal oxidation in an environment including oxides, water vapor, nitric oxide, or a combination thereof, or by an in-situ steam generation (ISSG) process in an environment including oxygen, water vapor, nitric oxide, or a combination thereof.

[0085] 12 , a word line 102 is formed. The word line 102 is located on the inner wall of the dielectric layer 101 and partially fills the word line trench 110 . The top of the word line 102 has a protrusion 112 protruding vertically. The top surface of the protrusion 112 is lower than the surface of the substrate 100 .

[0086] It should be noted that in FIG12 , the top of the protrusion 212 is shown to be parallel to the surface of the substrate 100, and the sidewalls of the protrusion 212 are parallel to the vertical direction. This does not limit the shape of the protrusion 212. In some embodiments, the connecting section between the sidewall of the protrusion and the dielectric layer 101 may also be a curved surface.

[0087] In some embodiments, the step of forming the protrusion 112 of the word line 102 includes: referring to FIG13 , forming an initial word line 302, the initial word line 302 being located on the surface of the dielectric layer 101 and filling a portion of the word line trench 110; referring to FIG14 , forming a mask layer 301, the mask layer 301 being located on a portion of the surface of the initial word line 302, the orthographic projection of the mask layer 301 on the surface of the substrate 100 being located within the orthographic projection of the word line trench 110 on the surface of the substrate 100; removing a portion of the mask layer 301 in a direction perpendicular to the surface of the substrate 100 to expose the initial word line 302; returning to FIG12 , removing the mask layer 301, the remaining initial word line 302 serving as the word line 102, and the top of the word line 102 having the protrusion 112.

[0088] It should be noted that in FIG14 , the orthographic projection of the mask layer 301 on the surface of the substrate 100 is taken as an example, in which the orthographic projection of the mask layer 301 on the surface of the substrate 100 is completely within the orthographic projection of the initial word line 302 on the surface of the substrate 100. The fact that the protrusion 112 formed thereby forms depressions on both sides perpendicular to the direction in which the word line 102 extends does not define the positional relationship between the orthographic projection of the mask layer 301 on the surface of the substrate 100 and the orthographic projection of the initial word line 302 on the surface of the substrate 100. In some embodiments, the orthographic projection of the mask layer on the surface of the substrate may be inscribed within the orthographic projection of the initial word line on the surface of the substrate, thereby forming a depression only on one side of the protrusion perpendicular to the direction in which the word line extends.

[0089] In some embodiments, the step of forming the protrusion 112 of the word line 102 includes: referring to FIG15 , forming an initial first word line 312, the initial first word line 312 being located on the surface of the dielectric layer 101 and filling a portion of the word line trench 110; forming a mask layer 301, the mask layer 301 being located on the inner wall of the dielectric layer 101, and having a bottom surface flush with a top surface of the initial first word line 312; forming an initial second word line 322, the initial second word line 322 filling a groove formed by the surface of the initial first word line 312 and the surface of the mask layer 301, the initial first word line 312 and the initial second word line 322 being made of the same material; returning to FIG12 , removing the mask layer 301, the initial first word line 312 and the initial second word line 322 together forming the word line 102, and the initial second word line 322 serving as the protrusion 112.

[0090] It should be noted that in FIG15 , the mask layer 301 is positioned on both inner walls of the dielectric layer 101 along a direction perpendicular to the word line 102. The resulting protrusion 112 forms depressions on both sides of the protrusion along the direction perpendicular to the word line 102. This does not limit the positional relationship between the mask layer 301 and the inner wall of the dielectric layer 101. In some embodiments, the mask layer may be positioned only on one inner wall of the dielectric layer along the direction perpendicular to the word line, thereby forming a depression only on the side of the protrusion along the direction perpendicular to the word line.

[0091] Regarding the mask layer 301 , the material forming the mask layer 301 includes silicon nitride or photoresist.

[0092] In some embodiments, referring to Figure 16, forming the word line 102 includes: forming a first work function layer 132, the first work function layer 132 covers the inner wall of the dielectric layer 101; forming a gate layer 122, the gate layer 122 covers the surface of the first work function layer 132 and fills the word line trench 110; patterning the first work function layer 132 and the gate layer 122 so that the gate layer 122 has a protrusion 112 that is higher than the top of the first work function layer 132.

[0093] In some embodiments, referring to Figure 17, forming the word line 102 includes: forming a first gate conductive layer 142, the first gate conductive layer 142 is located on a portion of the inner wall of the dielectric layer 101 and fills a portion of the word line trench 110; forming a first work function layer 132, the first work function layer 132 covers the surface of the first gate conductive layer 142 and also covers a portion of the inner wall of the dielectric layer 101; forming a second gate conductive layer 152, the second gate conductive layer 152 covers the first work function layer 132 and fills a portion of the word line trench 110; and patterning the second gate conductive layer 152 and the first work function layer 132 so that the second gate conductive layer 152 has a protrusion 112 that is higher than the top of the first work function layer 132.

[0094] Regarding the first work function layer 132 , the material forming the first work function layer 132 includes titanium, tantalum, titanium-tantalum alloy, titanium nitride, titanium aluminide, and the like.

[0095] In some embodiments, either the first gate conductive layer 142 or the second gate conductive layer 152 is doped polysilicon. For example, the dopant ions may be P-type or N-type dopant ions. N-type ions may specifically be phosphorus ions, arsenic ions, or antimony ions; and P-type ions may specifically be boron ions, indium ions, or boron fluoride ions. Doping polysilicon can improve the conductivity of the first gate conductive layer 142 or the second gate conductive layer 152, reduce word line resistance, minimize RC delay, and improve signal transmission efficiency of the word line 102.

[0096] Referring back to Figures 1, 3 and 4, an isolation layer 103 is formed, and the isolation layer 103 fills the recess on at least one side of the protrusion 112; an insulating layer 104 is formed, and the insulating layer 104 is located above the word line 102 and the isolation layer 103 and fills the word line trench 110. The dielectric constant of the insulating layer 104 is less than the dielectric constant of the isolation layer 103.

[0097] 1 , 3 and 4 , the isolation layer 103 is used as an example to illustrate the recesses on both sides of the protrusion 112. In some embodiments, the isolation layer 103 may only fill the recess on one side of the protrusion 112.

[0098] Isolation layer 103 may be formed from a material having a high dielectric constant, such as hafnium oxide, titanium oxide, hafnium zirconium oxide, tantalum oxide, hafnium silicate, zirconium oxide, or zirconium silicate. Using a high dielectric constant material for isolation layer 103 significantly reduces quantum tunneling in the dielectric layer, thereby reducing gate leakage current and the resulting power consumption.

[0099] Regarding the insulating layer 104 , the material forming the insulating layer 104 includes silicon oxide, silicon nitride, silicon oxynitride, or the like.

[0100] In some embodiments, referring to FIG5 and FIG6 , after forming the word line 102 and before forming the isolation layer 103, the process may further include forming a second work function layer 162. The second work function layer 162 covers a portion of the surface of the dielectric layer 101 and is located above the first work function layer 132. The bottom surface of the second work function layer 162 is flush with the top surface of the first work function layer 132, and the top of the second work function layer 162 is higher than or flush with the top of the protrusion 112. The second work function layer 162 can improve the interface state between the isolation layer 103 and the dielectric layer 101. The bottom of the second work function layer 162 is in electrical contact with the word line 102, making it easier for the word line 102 to drive electrons in the gate-drain overlap region to move toward the channel, thereby reducing the number of electrons in the gate-drain overlap region and the electric field in the gate-drain overlap region, thereby suppressing the GIDL current in the gate-drain overlap region. At the same time, because electrons are more easily driven toward the channel, the movement of electrons can be effectively controlled without applying a large driving voltage, thereby achieving regulation of the threshold voltage.

[0101] The second work function layer 162 may be formed of a material including titanium, tantalum, a titanium-tantalum alloy, titanium nitride, or titanium aluminide. For example, when the second work function layer 162 is made of titanium aluminide and the isolation layer 103 is made of hafnium dioxide, titanium aluminide can effectively improve the interface state between the hafnium dioxide and the dielectric layer 101.

[0102] The semiconductor structure manufacturing method provided by the embodiment of the present disclosure can form a buried gate structure by forming a dielectric layer 101 and a word line 102 located in a word line trench 110. The buried gate can improve the integration density of the semiconductor structure, while also increasing the area of ​​the channel region, improving the gate's control over the transistor, and reducing the short channel effect. Among them, the top of the word line 102 has a protrusion 112 that protrudes in the vertical direction. When the source region and the drain region are formed on both sides of the word line 102, the overlapping area between the word line 102 and the drain region can be reduced, thereby reducing the gate-induced drain leakage current and improving the performance of the semiconductor structure. In addition, the isolation layer 103 fills the recess on at least one side of the protrusion. The isolation layer 103 can further reduce the possibility of leakage between the word line 102 and the drain region, thereby significantly reducing the effect of quantum tunneling of the dielectric layer 101, thereby reducing the gate-induced drain leakage current and the power consumption caused by it, and improving the stability of the semiconductor structure. In addition, the insulating layer 104 is located above the word line 102 and the isolation layer 103 and fully fills the word line trench 110, which can insulate the word line 102 from other structures in the semiconductor structure to prevent leakage between the word line 102 and other structures. The dielectric constant of the insulating layer 104 is smaller than the dielectric constant of the isolation layer 103, that is, the insulation performance of the isolation layer 103 is greater than the insulation performance of the insulating layer 104. The isolation layer 103 can effectively weaken the electric field generated between the word line 102 and the drain region, reduce the gate-induced drain leakage current between the word line 102 and the drain region, and improve the stability of the semiconductor structure.

[0103] Those skilled in the art will appreciate that the above-mentioned embodiments are specific examples for implementing the present disclosure, and that in actual applications, various changes may be made thereto in form and detail without departing from the spirit and scope of the present disclosure.

Claims

1. A semiconductor structure comprising: A substrate (100), wherein a word line groove (110) is provided in the substrate (100); A dielectric layer (101), the dielectric layer (101) covering the bottom and sidewalls of the word line trench (110); A word line (102), the word line (102) being located on the inner wall of the dielectric layer (101) and filling a portion of the word line groove (110), and the top of the word line (102) having a protruding portion (112) protruding in a vertical direction; an isolation layer (103), the isolation layer (103) filling the recess on at least one side of the protrusion (112); An insulating layer (104), the insulating layer (104) is located above the word line (102) and the isolation layer (103) and fills the word line groove (110), and the dielectric constant of the insulating layer (104) is smaller than the dielectric constant of the isolation layer (103).

2. The semiconductor structure according to claim 1, wherein: The material of the isolation layer (103) is a high dielectric constant material, and the dielectric constant of the material of the isolation layer (103) is greater than 10.

3. The semiconductor structure according to claim 1, wherein: The word line (102) comprises: A gate layer (122), wherein the gate layer (122) fills a portion of the word line trench (110); A first work function layer (132), the first work function layer (132) being located between the dielectric layer (101) and the gate layer (122); The gate layer (122) has the protruding portion (112) which is higher than the top of the first work function layer (132), and the isolation layer (103) is located above the first work function layer (132).

4. The semiconductor structure according to claim 1, wherein: The word line (102) comprises: A first gate conductive layer (142), the first gate conductive layer (142) being located on the inner wall of the dielectric layer (101) and filling a portion of the word line trench (110); A second gate conductive layer (152), the second gate conductive layer (152) is located above the first gate conductive layer (142) and fills a portion of the word line trench (110); A first work function layer (132), wherein the first work function layer (132) is located between the first gate conductive layer (142) and the second gate conductive layer (152), and is also located between the second gate conductive layer (152) and the dielectric layer (101); The second gate conductive layer (152) has the protruding portion (112) which is higher than the top of the first work function layer (132), and the isolation layer (103) is located above the first work function layer (132).

5. The semiconductor structure according to claim 4, wherein: One of the first gate conductive layer (142) or the second gate conductive layer (152) is doped polysilicon.

6. The semiconductor structure according to claim 3 or 4, wherein: Also includes: A second work function layer (162), wherein the second work function layer (162) is located between the dielectric layer (101) and the isolation layer (103), and the second work function layer (162) is located above the first work function layer (132), the bottom surface of the second work function layer (162) is flush with the top surface of the first work function layer (132), and the top of the second work function layer (162) is higher than or flush with the top of the protrusion (112).

7. The semiconductor structure according to claim 6, wherein: The materials of the first work function layer (132) and the second work function layer (162) both include titanium nitride or titanium aluminide.

8. The semiconductor structure according to claim 6, wherein: The thickness of the first work function layer (132) is smaller than the thickness of the second work function layer (162).

9. The semiconductor structure according to claim 1, wherein: Part of the side wall of the protruding portion (112) is parallel to the vertical direction, and the top surface of the protruding portion (112) is parallel to the top surface of the base.

10. The semiconductor structure according to claim 1, wherein: In a direction perpendicular to the surface of the substrate, the top surface of the isolation layer (103) is higher than or flush with the top surface of the protrusion (112).

11. The semiconductor structure according to claim 1, wherein: The dielectric layer (101) comprises: A first dielectric layer (111), the first dielectric layer (111) covering the bottom and sidewalls of the word line trench (110); A second dielectric layer (121), wherein the second dielectric layer (121) covers the inner wall of the first dielectric layer (111), wherein the density of the first dielectric layer (111) is greater than the density of the second dielectric layer (121).

12. A method for manufacturing a semiconductor structure, comprising: Providing a substrate (100), wherein the substrate (100) has a word line groove (110); forming a dielectric layer (101), wherein the dielectric layer (101) covers the bottom and sidewalls of the word line trench (110); forming a word line (102), wherein the word line (102) is located on the inner wall of the dielectric layer (101) and fills a portion of the word line groove (110), the top of the word line (102) has a protruding portion (112) protruding in a vertical direction, and the top surface of the protruding portion (112) is lower than the surface of the substrate (100); forming an isolation layer (103), wherein the isolation layer (103) fills the recess on at least one side of the protrusion (112); An insulating layer (104) is formed, wherein the insulating layer (104) is located above the word line (102) and the isolation layer (103) and fills the word line groove (110), and the dielectric constant of the insulating layer (104) is smaller than the dielectric constant of the isolation layer (103). Electrical constant.

13. The method for manufacturing a semiconductor structure according to claim 12, wherein: Forming the dielectric layer (101) includes: A second dielectric layer (121) is formed by a deposition process, wherein the second dielectric layer (121) covers the bottom and sidewalls of the word line trench (110); A first dielectric layer (111) is formed on a contact surface between the second dielectric layer (121) and the substrate (100) by a thermal oxidation process, wherein the density of the first dielectric layer (111) is greater than the density of the second dielectric layer (121).

14. The method for manufacturing a semiconductor structure according to claim 12, wherein: Forming the word line (102) includes: forming a first work function layer (132), wherein the first work function layer (132) covers the inner wall of the dielectric layer (101); forming a gate layer (122), wherein the gate layer (122) covers the surface of the first work function layer (132) and completely fills the word line trench (110); The first work function layer (132) and the gate layer (122) are patterned so that the gate layer (122) has the protruding portion (112) higher than the top of the first work function layer (132).

15. The method for manufacturing a semiconductor structure according to claim 12, wherein: Forming the word line (102) includes: forming a first gate conductive layer (142), wherein the first gate conductive layer (142) is located on a portion of the inner wall of the dielectric layer (101) and fills a portion of the word line trench (110); forming a first work function layer (132), wherein the first work function layer (132) covers the surface of the first gate conductive layer (142) and also covers a portion of the inner wall of the dielectric layer (101); forming a second gate conductive layer (152), wherein the second gate conductive layer (152) covers the first work function layer (132) and fills a portion of the word line trench (110); The second gate conductive layer (152) and the first work function layer (132) are patterned so that the second gate conductive layer (152) has the protruding portion (112) higher than the top of the first work function layer (132).

16. The method for manufacturing a semiconductor structure according to claim 14 or 15, characterized in that: After forming the word line (102) and before forming the isolation layer (103), the method further comprises: A second work function layer (162) is formed, wherein the second work function layer (162) covers a portion of the surface of the dielectric layer (101) and is located above the first work function layer (132), the bottom surface of the second work function layer (162) is flush with the top surface of the first work function layer (132), and the top of the second work function layer (162) is higher than or flush with the top of the protrusion (112).

Citation Information

Patent Citations

  • Transistor having dual work function buried gate electrode and method for fabricating the same

    CN104810390A

  • Memory transistor, word line structure of memory transistor and word line preparing method

    CN110610940A

  • Method for manufacturing semiconductor device having buried gate electrodes

    CN111490095A

  • Semiconductor structure and manufacturing method

    CN111900201A

  • Semiconductor structure and manufacturing method thereof

    CN116017977A