Magnetic compensation MTJ device, manufacturing method therefor, and MRAM device

By adding a magnetic compensation layer to the MTJ device to offset the leakage magnetic field under temperature changes, the problem of unbalanced data retention capabilities of the MTJ device at different temperatures is solved, and its reliability and yield are improved.

WO2024198492A1PCT designated stage expired Publication Date: 2024-10-03ZHEJIANG HIKSTOR TECHOGY CO LTD

Patent Information

Application Number
PCT/CN2023/137150
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2023-12-07
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

The data retention capabilities of existing MTJ devices in high and low resistance states at different temperatures vary greatly, affecting their reliability and yield.

Method used

Design a magnetically compensated MTJ device by adding a magnetic compensation layer to the side of the MTJ unit to ensure that within the preset temperature range, the ratio of the net residual magnetization of the magnetic compensation layer to the net residual magnetization of the SAF fixed layer does not exceed 1.2, and The magnetic flip field of the magnetic compensation layer is larger than that of the free layer, thereby canceling out the leakage magnetic fields at different temperatures.

Benefits of technology

It effectively balances the high and low resistance state data retention capabilities of MTJ devices at different temperatures, improving the reliability and yield of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023137150_03102024_PF_FP_ABST
    Figure CN2023137150_03102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided are a magnetic compensation MTJ device, a manufacturing method therefor, and an MRAM device. The magnetic compensation MTJ device comprises an MTJ unit, an isolation layer, and a magnetic compensation layer which are sequentially arranged in a stacked manner. The MTJ unit comprises a free layer, a potential barrier layer, and a SAF fixing layer which are arranged in a stacked manner. At the same temperature within a preset temperature range, the ratio of a SAF fixing layer net residual magnetization intensity corresponding to the SAF fixing layer to a magnetic compensation layer net residual magnetization intensity corresponding to the magnetic compensation layer does not exceed a first given range, and the magnetic compensation layer net residual magnetization intensity and the SAF fixing layer net residual magnetization intensity are in opposite directions. A magnetic flip field of the magnetic compensation layer is larger than a magnetic flip field of the free layer. The magnetic compensation MTJ device makes a leakage magnetic field generated by the magnetic compensation layer at a position corresponding to the free layer and a leakage magnetic field generated by the fixing layer counteract each other at the same temperature within a certain range, thereby guaranteeing the balance of the data retention capability of the MTJ device.
Need to check novelty before this filing date? Find Prior Art

Description

A magnetically compensated MTJ device and its manufacturing method, and MRAM device Technical Field

[0001] The present disclosure relates to the field of magnetic memory, and in particular to a magnetically compensated MTJ device and a manufacturing method thereof, and an MRAM device. Background Art

[0002] Magnetic random access memory (MRAM) consists of a magnetic tunnel junction (MTJ) array. The core structure of the MTJ includes a free layer, a barrier layer, and a pinned layer. The free and pinned layers are magnetic multilayer films, while the barrier layer is a very thin insulating layer, typically less than 2nm thick. During normal operation of the MTJ, the magnetization direction of the pinned layer remains unchanged, while the magnetization direction of the free layer can be changed by an external magnetic field or input current. The resistance of the MTJ is determined by the relative magnetization directions of the free and pinned layers. When the magnetization directions of the free and pinned layers are parallel, the MTJ is in a low-resistance state; when the magnetization directions of the free and pinned layers are antiparallel, the MTJ is in a high-resistance state. MTJ devices record data information based on the high and low resistance states of the MTJ.

[0003] To reduce the impact of the fixed layer's leakage magnetic field on the free layer, a pinned layer based on an artificial antiferromagnetic structure (SAF) is used. The leakage magnetic fields of the various magnetic layers within the fixed layer of the artificial antiferromagnetic structure at the free layer cancel each other out, making the data retention difficulty in the two magnetization states of the free layer close to the same, thereby ensuring the balance of the data retention capabilities of the MTJ device in different resistance states. However, in existing MTJ films, to meet specific performance requirements, such as strong perpendicular magnetic anisotropy (PMA) and high magnetoresistance (TMR), the pinned layer and reference layer are made of different materials, and their magnetization strengths have different temperature response. Furthermore, the actual use of MTJ devices is complex and the ambient temperature is variable. As a result, the leakage magnetic fields of the SAF-based fixed layer at the free layer cannot cancel each other out as the temperature changes. In other words, the data retention capabilities of the high and low resistance states vary significantly at different temperatures, which is detrimental to the reliability and yield of the MTJ device.

[0004] Therefore, how to ensure the balance of data retention capabilities of MTJ devices in different resistance states at different temperatures and improve the reliability of MTJ devices has become an urgent problem to be solved by those skilled in the art.

[0005] Summary of the Invention

[0006] The present disclosure aims to provide a magnetically compensated MTJ device, a manufacturing method thereof, and an MRAM device to solve the problem in the prior art that the data retention capabilities of MTJ devices in high and low resistance states vary greatly at different temperatures.

[0007] In order to solve the above technical problems, the present disclosure provides a magnetic compensation MTJ device, comprising an MTJ unit, an isolation layer and a magnetic compensation layer stacked in sequence;

[0008] The MTJ unit includes a free layer, a barrier layer and a SAF fixed layer arranged in a stacked manner;

[0009] At the same temperature within the preset temperature range, a ratio of a net residual magnetization intensity of the SAF pinned layer corresponding to the SAF pinned layer to a net residual magnetization intensity of the magnetic compensation layer corresponding to the magnetic compensation layer does not exceed a first given range, and a direction of the net residual magnetization intensity of the magnetic compensation layer is opposite to that of the net residual magnetization intensity of the SAF pinned layer;

[0010] The magnetic switching field of the magnetic compensation layer is greater than the magnetic switching field of the free layer.

[0011] Optionally, in the magnetic compensation MTJ device, the magnetic compensation layer includes a first compensation sublayer, a reverse coupling layer, and a second compensation sublayer stacked in sequence.

[0012] Optionally, in the magnetically compensated MTJ device, the first compensation sublayer and / or the second compensation sublayer is a composite layer.

[0013] Optionally, in the magnetic compensation MTJ device, the composite layer includes an anisotropic auxiliary layer and a magnetic layer that are stacked.

[0014] Optionally, in the magnetically compensated MTJ device, the anisotropic auxiliary layer includes at least one of a magnesium oxide layer and a cobalt layer;

[0015] When the anisotropic auxiliary layer is a magnesium oxide layer, the magnetic layer includes at least one of a cobalt layer, an iron layer, a nickel layer, a cobalt boride layer, an iron boride layer, a nickel boride layer, a cobalt iron layer, an iron nickel layer, a cobalt nickel layer, a cobalt iron boron layer, a cobalt iron platinum layer, a cobalt iron palladium layer, a cobalt iron terbium layer, a cobalt iron chromium layer, and a cobalt iron gadolinium layer;

[0016] When the anisotropic auxiliary layer is a cobalt layer, the magnetic layer includes at least one of a platinum layer, a palladium layer, and a nickel layer.

[0017] Optionally, in the magnetically compensated MTJ device, the reverse coupling layer includes at least one of an iridium layer and a ruthenium layer.

[0018] Optionally, in the magnetically compensated MTJ device, the first given range is 0.8 to 1.2, inclusive.

[0019] Optionally, the magnetically compensated MTJ device further includes an antiferromagnetic pinning layer;

[0020] The antiferromagnetic pinning layer is arranged on a surface of the magnetic compensation layer away from the isolation layer.

[0021] An MRAM device includes any one of the above-mentioned magnetically compensated MTJ devices.

[0022] A method for manufacturing a magnetically compensated MTJ device, comprising:

[0023] Acquiring data of a to-be-processed MTJ unit, wherein the to-be-processed MTJ unit corresponding to the data of the to-be-processed MTJ unit includes a free layer, a barrier layer, and a SAF fixed layer that are stacked;

[0024] Determine reference temperature-dependent magnetization data based on the MTJ unit data to be processed, wherein the reference temperature-dependent magnetization data is data on the corresponding relationship between the net residual magnetization intensity of the SAF pinned layer and the temperature within a preset temperature range;

[0025] Determining magnetic compensation layer data based on the reference temperature-dependent magnetization data so that a ratio of a net residual magnetization intensity of the magnetic compensation layer to a net residual magnetization intensity of the SAF pinned layer at the same temperature within a preset temperature range, corresponding to the magnetic compensation layer data, does not exceed a first given range, the net residual magnetization intensity of the magnetic compensation layer and the net residual magnetization intensity of the SAF pinned layer are in opposite directions, and the magnetic reversal field of the magnetic compensation layer is greater than the magnetic reversal field of the free layer;

[0026] The MTJ unit to be processed is set according to the data of the MTJ unit to be processed, the magnetic compensation layer is set according to the magnetic compensation layer data, and an isolation layer is set between the MTJ unit to be processed and the magnetic compensation layer to obtain a finished MTJ device.

[0027] The magnetic compensation MTJ device provided by the present disclosure includes an MTJ unit, an isolation layer and a magnetic compensation layer stacked in sequence; the MTJ unit includes a free layer, a barrier layer and a SAF fixed layer stacked in sequence; at the same temperature within a preset temperature range, the ratio of the net residual magnetization intensity of the SAF fixed layer corresponding to the SAF fixed layer to the net residual magnetization intensity of the magnetic compensation layer corresponding to the magnetic compensation layer does not exceed a first given range, and the direction of the net residual magnetization intensity of the magnetic compensation layer is opposite to that of the net residual magnetization intensity of the SAF fixed layer; the magnetic reversal field of the magnetic compensation layer is greater than the magnetic reversal field of the free layer.

[0028] The present disclosure adds a magnetic compensation layer to one side of the MTJ unit. The net residual magnetization intensity of the magnetic compensation layer is similar to that of the SAF pinned layer at the same temperature, but the magnetization direction is opposite. This allows the leakage magnetic field generated by the magnetic compensation layer and the leakage magnetic field generated by the pinned layer at the corresponding position of the free layer to cancel each other out within a certain range and the same temperature. This ensures the balance of data retention capabilities of the MTJ device in different resistance states at different temperatures, improving the reliability and yield of the MTJ device. The present disclosure also provides a method for manufacturing a magnetically compensated MTJ device and an MRAM device with the above-mentioned beneficial effects. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions of the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.

[0030] FIG1 is a schematic structural diagram of a specific embodiment of a magnetically compensated MTJ device provided by the present disclosure;

[0031] FIG2 is a schematic structural diagram of a specific embodiment of a magnetically compensated MTJ device provided by the present disclosure;

[0032] FIG3 is a schematic structural diagram of another specific embodiment of a magnetically compensated MTJ device provided by the present disclosure;

[0033] FIG4 is a schematic structural diagram of another specific embodiment of the magnetically compensated MTJ device provided by the present disclosure;

[0034] FIG5 is a schematic structural diagram of another specific embodiment of the magnetically compensated MTJ device provided by the present disclosure;

[0035] FIG6 is a flow chart of a specific embodiment of a method for manufacturing a magnetically compensated MTJ device provided in the present disclosure. DETAILED DESCRIPTION

[0036] The SAF structure is a Co / Pt, Co / Pd or Co / Ni multilayer film, which generates antiferromagnetic coupling through the coupling layer inside, so that the leakage magnetic fields of the fixed layer magnetic layers cancel each other in the free layer. The leakage magnetic field cancellation can be expressed by the offset field (H offset ) to characterize. offset The value of H is relevant to the data retention time and bit failure of the MTJ device. offset is not 0, the free layer magnetic moment will always be in a non-zero leakage magnetic field, causing the MTJ device to tend to maintain a specific resistance state (high resistance state or low resistance state), and the corresponding data retention time of this resistance state is longer than that of another resistance state. Therefore, in the present disclosure, the leakage magnetic field generated by the magnetic compensation layer 30 at the corresponding position of the free layer of the MTJ device and the leakage magnetic field generated by the fixed layer cancel each other out at the same temperature within a certain range, which can also be regarded as H at different temperatures. offset The values ​​are close.

[0037] In order to enable those skilled in the art to better understand the present disclosure, the present disclosure is further described in detail below in conjunction with the accompanying drawings and specific embodiments. Obviously, the embodiments described are only a portion of the embodiments of the present disclosure, and not all of them. Based on the embodiments of the present disclosure, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present disclosure.

[0038] The core of the present disclosure is to provide a magnetic compensation MTJ device, a structural diagram of a specific embodiment of which is shown in FIG1 , referred to as specific embodiment 1, comprising an MTJ unit, an isolation layer 20 and a magnetic compensation layer 30 stacked in sequence;

[0039] The MTJ unit includes a free layer 11, a barrier layer 12 and a SAF fixed layer 13 which are stacked;

[0040] At the same temperature within the preset temperature range, the ratio of the net residual magnetization intensity of the SAF pinned layer 13 to the net residual magnetization intensity of the magnetic compensation layer 30 does not exceed a first given range, and the direction of the net residual magnetization intensity of the magnetic compensation layer is opposite to that of the net residual magnetization intensity of the SAF pinned layer;

[0041] The magnetic switching field of the magnetic compensation layer 30 is greater than the magnetic switching field of the free layer 11 .

[0042] Of course, in actual production, the net residual magnetization intensity of the magnetic compensation layer should be ensured to be the same as that of the SAF pinned layer at the same temperature as much as possible, so that the leakage magnetic fields generated by the magnetic compensation layer 30 and the SAF pinned layer 13 at corresponding positions of the free layer 11 cancel each other out.

[0043] In the present disclosure, the net residual magnetization intensity of the magnetic compensation layer refers to the leakage magnetic field generated by the compensation layer at the corresponding position of the free layer. Similarly, the net residual magnetization intensity of the SAF pinned layer refers to the leakage magnetic field generated by the SAF pinned layer 13 at the corresponding position of the free layer.

[0044] It should be noted that the ratio of the net residual magnetization of the SAF pinned layer to the net residual magnetization of the magnetic compensation layer in this disclosure does not involve a description of direction through the ratio. Of course, a certain direction can also be defined as the positive direction, in which case the ratio is always less than 0. The net residual magnetization of the magnetic compensation layer can be adjusted by adjusting the structure, size, and material of the magnetic compensation layer 30 through a combination of simulation calculations and actual production testing, and will not be further elaborated here.

[0045] The isolation layer 20 includes one or more non-magnetic metals, alloys, oxides and nitrides and can be a single layer or a multilayer film, and is used to eliminate magnetic coupling between the free layer 11 or the fixed layer and the magnetic compensation layer 30 .

[0046] It is easy to see that the magnetic reversal field of the magnetic compensation layer 30 is greater than the magnetic reversal field of the free layer 11. Otherwise, the free layer 11 will remain stable and unreversed while the magnetic compensation layer 30 undergoes reversal. Therefore, the magnetic reversal field of the magnetic compensation layer 30 is made greater than the magnetic reversal field of the free layer 11 in order to further improve the operating stability and reliability of the MTJ device.

[0047] As a preferred embodiment, the magnetic compensation layer 30 includes a first compensation sublayer 31 , a reverse coupling layer 33 and a second compensation sublayer 32 which are stacked in sequence.

[0048] The magnetic compensation layer 30 in the present disclosure can be disposed on either side of the MTJ unit, that is, it can be disposed on the side of the SAF pinned layer 13 (as shown in FIG1 ) or on the side of the free layer 11 (as shown in FIG3 ).

[0049] As a specific embodiment, the magnetic compensation layer 30 and / or the isolation layer 20 can also be arranged at a position outside the MTJ film of the MRAM device (including only part of the structure in the MTJ device, see Figure 4), such as the position of the bottom electrode 002 or the top electrode 001 in contact with the MTJ film, which can also achieve a similar effect, and this disclosure is not limited to this.

[0050] Since the first compensation sublayer 31 and the second compensation sublayer 32 are connected via the reverse coupling layer 33, it is readily apparent that the magnetization directions of the first compensation sublayer 31 and the second compensation sublayer 32 are opposite. Referring to FIG1 (the SAF pinned layer 13 in FIG1 includes a reference layer 13A, a coupling layer 13B, and a pinned layer 13C), the two magnetic layers with opposite directions forming the magnetic compensation layer 30 can significantly enhance the magnetic reversal field of the magnetic compensation layer 30, making the magnetic compensation layer 30 less susceptible to reversal under external environmental influences (such as high temperatures and complex electromagnetic environments), thereby improving the operating stability and reliability of the device. Of course, the magnetic compensation layer 30 can also be a single layer or other film layer, and this is not limited in this disclosure.

[0051] Specifically, reverse coupling layer 33 includes at least one of an iridium (Ir) layer and a ruthenium (Ru) layer. These two materials are well-established and offer good coupling properties. Other materials may also be used depending on the application. Reverse coupling layer 33 may be a single layer or a multi-layer composite layer. Furthermore, reverse coupling layer 33 may be a mixture, such as a layer made of metallic iridium and metallic ruthenium.

[0052] Furthermore, the first compensation sublayer 31 and / or the second compensation sublayer 32 is a composite layer.

[0053] Of course, the closer the ratio of the net residual magnetization intensity of the magnetic compensation layer to the net residual magnetization intensity of the SAF fixed layer is to 1, the better the balance effect of the data retention capability of the MTJ device in different resistance states. In this preferred embodiment, the first compensation sublayer 31 and / or the second compensation sublayer 32 are designed in the form of a composite layer, which can make the control accuracy of the magnitude and direction of the reinforcement intensity of the first compensation sublayer 31 and / or the second compensation sublayer 32 higher, and better adjust the leakage magnetic field intensity of the SAF fixed layer 13 at the corresponding position of the free layer 11, so as to further improve the balance of the data retention capability of the MTJ device in different resistance states.

[0054] Furthermore, the composite layer includes an anisotropic auxiliary layer and a magnetic layer that are stacked.

[0055] In this preferred embodiment, the first compensation sublayer 31 and / or the second compensation sublayer 32 is a composite layer including an anisotropic auxiliary layer and a magnetic layer. The anisotropic auxiliary layer is a layer that can cooperate with the corresponding magnetic layer to enhance the perpendicular magnetic anisotropy of the corresponding compensation sublayer. Improving the perpendicular magnetic anisotropy can further enhance the working stability of the MTJ device.

[0056] Specifically, the anisotropic auxiliary layer includes at least one of a magnesium oxide (MgO) layer and a cobalt (Co) layer;

[0057] When the anisotropic auxiliary layer is a magnesium oxide layer, the magnetic layer includes at least one of a cobalt layer, an iron layer (Fe), a nickel (Ni) layer, a cobalt boride (CoB) layer, an iron boride (FeB) layer, a nickel boride (NiB) layer, a cobalt iron (CoFe) layer, an iron nickel (NiFe) layer, a cobalt nickel (CoNi) layer, a cobalt iron boron (CoFeB) layer, a cobalt iron platinum (CoFePt) layer, a cobalt iron palladium (CoFePd) layer, a cobalt iron terbium (CoFeTb) layer, a cobalt iron chromium (CoFeCr) layer, and a cobalt iron gadolinium (CoFeGd) layer;

[0058] When the anisotropic auxiliary layer is a cobalt layer, the magnetic layer includes at least one of a platinum (Pt) layer, a palladium (Pd) layer, and a nickel (Ni) layer.

[0059] The combination of each of the above-mentioned anisotropic auxiliary layers and the corresponding magnetic layer is a composite layer combination with good perpendicular magnetic anisotropy obtained through extensive theoretical calculations and experimental verification. Of course, other composite layer combinations can also be selected according to actual conditions, or any of the above-mentioned magnetic layers can be directly selected as the magnetic compensation layer 30 (i.e., a single-layer magnetic compensation layer 30), and this is not limited in this disclosure. Referring to FIG. 2 , FIG. 2 is a specific embodiment of the structure corresponding to FIG. 1 , wherein the free layer 11 includes two cobalt iron boron layers and a tungsten (W) layer disposed between the two cobalt iron boron layers, the barrier layer 12 is a magnesium oxide layer, the reference layer 13A is sequentially composed of a cobalt iron boron layer, a tungsten layer, and a cobalt / platinum composite layer, the coupling layer 13B is a ruthenium layer, the pinning layer 13C is a cobalt layer and a cobalt / platinum composite layer, the isolation layer 20 is a ruthenium / tantalum composite layer, and the magnetic compensation layer 30 is sequentially composed of a cobalt layer, a ruthenium layer, and a cobalt-nickel composite layer. The "number + A" within each layer in FIG. 2 represents the thickness of the layer, where A is the thickness unit in angstroms.

[0060] As a specific embodiment, the first given range is 0.8 to 1.2, including endpoint values ​​such as any one of 0.80, 1.05, or 1.20. The above range is the optimal parameter range obtained through extensive theoretical calculations and practical tests. Within the above range, after the leakage magnetic fields generated by the magnetic compensation layer 30 and the SAF pinned layer 13 at corresponding positions in the free layer cancel each other out, the residual magnetic field strength will not significantly affect the magnetic field reversal of the free layer 11, thereby ensuring consistent data retention capabilities of the MTJ component in different resistance states. Of course, this range can also be adjusted according to actual conditions.

[0061] The magnetic compensation MTJ device provided by the present disclosure includes an MTJ unit, an isolation layer 20 and a magnetic compensation layer 30 stacked in sequence; the MTJ unit includes a free layer 11, a barrier layer 12 and a SAF pinned layer 13 stacked; at the same temperature within a preset temperature range, the ratio of the net residual magnetization intensity of the SAF pinned layer corresponding to the SAF pinned layer 13 to the net residual magnetization intensity of the magnetic compensation layer corresponding to the magnetic compensation layer 30 does not exceed a first given range, and the direction of the net residual magnetization intensity of the magnetic compensation layer is opposite to that of the net residual magnetization intensity of the SAF pinned layer; the magnetic reversal field of the magnetic compensation layer 30 is greater than the magnetic reversal field of the free layer 11. The present disclosure adds a magnetic compensation layer 30 on one side of the MTJ unit. The net residual magnetization intensity of the magnetic compensation layer 30 is similar to the net residual magnetization intensity of the SAF fixed layer 13 at the same temperature, but the magnetization directions are opposite. Therefore, at the corresponding position of the free layer, the leakage magnetic field generated by the magnetic compensation layer 30 and the leakage magnetic field generated by the fixed layer cancel each other out at the same temperature within a certain range, thereby ensuring the balance of the data retention ability of the MTJ device in different resistance states at different temperatures, and improving the reliability and yield of the MTJ device.

[0062] On the basis of the first embodiment, the stability of the magnetic compensation layer 30 is further improved to obtain the second embodiment, the structure of which is shown in FIG5 , including an MTJ unit, an isolation layer 20 and a magnetic compensation layer 30 stacked in sequence;

[0063] The MTJ unit includes a free layer 11, a barrier layer 12 and a SAF fixed layer 13 which are stacked;

[0064] At the same temperature within the preset temperature range, the ratio of the net residual magnetization intensity of the SAF pinned layer 13 to the net residual magnetization intensity of the magnetic compensation layer 30 does not exceed a first given range, and the direction of the net residual magnetization intensity of the magnetic compensation layer is opposite to that of the net residual magnetization intensity of the SAF pinned layer;

[0065] The magnetic reversal field of the magnetic compensation layer 30 is greater than the magnetic reversal field of the free layer 11;

[0066] Also includes an antiferromagnetic pinning layer 40;

[0067] The antiferromagnetic pinning layer 40 is disposed on a surface of the magnetic compensation layer 30 away from the isolation layer 20 .

[0068] The difference between this embodiment and the above embodiment is that an antiferromagnetic pinning layer 40 is added to the magnetic compensation layer 30 in this embodiment, and the rest of the structure is the same as that in the above embodiment.

[0069] In this specific embodiment, an antiferromagnetic pinning layer 40 is provided on the other side of the magnetic compensation layer 30 . The antiferromagnetic pinning layer 40 can further increase the magnetization direction stability of the adjacent magnetic compensation layer 30 , thereby improving the working stability of the MTJ device.

[0070] Of course, in combination with the foregoing, the magnetic compensation layer 30 in this specific embodiment can be a composite layer or a single layer film, and the present disclosure does not limit this.

[0071] The present disclosure further provides a method for manufacturing a magnetically compensated MTJ device, a flow chart of a specific embodiment of which is shown in FIG6 , referred to as specific embodiment three, comprising:

[0072] S101: Acquire data of an MTJ cell to be processed, wherein the MTJ cell to be processed corresponding to the data of the MTJ cell to be processed includes a free layer, a barrier layer, and a SAF fixed layer that are stacked.

[0073] The MTJ unit data to be processed is basic data of the MTJ unit to be processed, such as size, thickness, structure, components, etc.

[0074] S102: Determine reference temperature-dependent magnetization data according to the MTJ unit data to be processed, wherein the reference temperature-dependent magnetization data refers to data on the corresponding relationship between the net residual magnetization intensity of the SAF pinned layer and the temperature within a preset temperature range.

[0075] In this step, a specific MTJ unit to be processed can be produced based on the data of the MTJ unit to be processed. Then, experiments can be conducted to obtain reference temperature-dependent magnetization data by subjecting the produced MTJ unit to different temperatures. Of course, other methods can also be used to obtain reference temperature-dependent magnetization data, such as computer simulation or deep learning, and this disclosure is not limited thereto.

[0076] S103: Determine magnetic compensation layer data based on reference temperature-dependent magnetization data, so that the ratio of the net residual magnetization intensity of the magnetic compensation layer to the net residual magnetization intensity of the SAF pinned layer at the same temperature within a preset temperature range of the magnetic compensation layer corresponding to the magnetic compensation layer data does not exceed a first given range, the net residual magnetization intensity of the magnetic compensation layer is in opposite directions to the net residual magnetization intensity of the SAF pinned layer, and the magnetic reversal field of the magnetic compensation layer is greater than the magnetic reversal field of the free layer.

[0077] After determining the reference temperature-dependent magnetization data, it is only necessary to adjust the structure, size, composition, and other factors of the magnetic compensation layer 30 so that the net residual magnetization intensity of the magnetic compensation layer 30 at different temperatures corresponds to the reference temperature-dependent magnetization data in magnitude but is opposite in direction. Of course, the closer the ratio of the net residual magnetization intensity of the magnetic compensation layer to the net residual magnetization intensity of the SAF pinned layer is to 1, the better.

[0078] S104: setting the MTJ unit to be processed according to the data of the MTJ unit to be processed, setting the magnetic compensation layer according to the magnetic compensation layer data, and setting an isolation layer between the MTJ unit to be processed and the magnetic compensation layer to obtain a finished MTJ device.

[0079] The manufacturing method of the magnetically compensated MTJ device in this specific embodiment corresponds to the magnetically compensated MTJ device described above, and will not be described in detail here.

[0080] The present invention provides a method for manufacturing a magnetically compensated MTJ device, comprising: obtaining data of an MTJ unit to be processed; the MTJ unit to be processed corresponding to the data of the MTJ unit to be processed includes a stacked free layer, a barrier layer, and a SAF pinned layer; determining reference temperature-variable magnetization data based on the data of the MTJ unit to be processed; the reference temperature-variable magnetization data refers to data on the corresponding relationship between the net residual magnetization intensity of the SAF pinned layer and the temperature within a preset temperature range; determining magnetic compensation layer data based on the reference temperature-variable magnetization data, so that the ratio of the net residual magnetization intensity of the magnetic compensation layer to the net residual magnetization intensity of the SAF pinned layer at the same temperature within the preset temperature range of the magnetic compensation layer corresponding to the magnetic compensation layer data does not exceed a first given range, the net residual magnetization intensity of the magnetic compensation layer is in opposite directions to the net residual magnetization intensity of the SAF pinned layer, and the magnetic reversal field of the magnetic compensation layer is greater than the magnetic reversal field of the free layer; setting the MTJ unit to be processed based on the data of the MTJ unit to be processed, setting the magnetic compensation layer based on the data of the magnetic compensation layer, and setting an isolation layer between the MTJ unit to be processed and the magnetic compensation layer, to obtain a finished MTJ device. The present disclosure adds a magnetic compensation layer on one side of the MTJ unit, so that the leakage magnetic field generated by the magnetic compensation layer at the corresponding position of the free layer and the leakage magnetic field generated by the SAF fixed layer cancel each other out at the same temperature within a certain range, thereby ensuring the balance of the data retention ability of the MTJ device in different resistance states at different temperatures, and improving the reliability and yield of the MTJ device.

[0081] The present disclosure also provides an MRAM device, comprising any of the magnetically compensated MTJ devices described above. The magnetically compensated MTJ device provided by the present disclosure comprises an MTJ unit, an isolation layer 20, and a magnetic compensation layer 30 stacked in sequence; the MTJ unit comprises a free layer 11, a barrier layer 12, and a SAF pinned layer 13 stacked in sequence; at the same temperature within a preset temperature range, the ratio of the net remanent magnetization of the SAF pinned layer 13 to the net remanent magnetization of the magnetic compensation layer 30 does not exceed a first given range, and the direction of the net remanent magnetization of the magnetic compensation layer is opposite to that of the SAF pinned layer; and the magnetic reversal field of the magnetic compensation layer 30 is greater than the magnetic reversal field of the free layer 11. The present disclosure adds a magnetic compensation layer 30 on one side of the MTJ unit. The net residual magnetization intensity of the magnetic compensation layer is similar to the net residual magnetization intensity of the SAF fixed layer at the same temperature, but the magnetization direction is opposite. Therefore, at the corresponding position of the free layer, the leakage magnetic field generated by the magnetic compensation layer and the leakage magnetic field generated by the fixed layer cancel each other out at the same temperature within a certain range, thereby ensuring the balance of the data retention ability of the MTJ device in different resistance states at different temperatures, and improving the reliability and yield of the MTJ device.

[0082] The various embodiments in this specification are described in a progressive manner, with each embodiment focusing on its differences from the other embodiments. Reference can be made to the descriptions of the identical or similar parts between the various embodiments. For the devices disclosed in the embodiments, since they correspond to the methods disclosed in the embodiments, the descriptions are relatively simple, and the relevant parts can be referred to the descriptions of the methods.

[0083] It should be noted that, in this specification, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or device comprising a series of elements includes not only those elements, but also other elements not explicitly listed, or elements inherent to such process, method, article, or device. In the absence of further limitations, an element defined by the phrase "comprising a..." does not exclude the presence of additional identical elements in the process, method, article, or device comprising the element.

[0084] The above describes in detail the magnetically compensated MTJ device, its manufacturing method, and MRAM device provided by the present disclosure. This article uses specific examples to illustrate the principles and implementation methods of the present disclosure. The description of the above embodiments is only intended to help understand the methods and core concepts of the present disclosure. It should be noted that for those skilled in the art, without departing from the principles of the present disclosure, several improvements and modifications can be made to the present disclosure, and these improvements and modifications also fall within the scope of protection of the claims of the present disclosure.

Claims

1. A magnetic compensation MTJ device, comprising an MTJ unit, an isolation layer and a magnetic compensation layer stacked in sequence; The MTJ unit includes a free layer, a barrier layer and a SAF fixed layer which are stacked; At the same temperature within the preset temperature range, the ratio of the net residual magnetization intensity of the SAF fixed layer corresponding to the SAF fixed layer to the net residual magnetization intensity of the magnetic compensation layer corresponding to the magnetic compensation layer does not exceed the first given range, and the net residual magnetization intensity of the magnetic compensation layer is opposite to the direction of the net residual magnetization intensity of the SAF fixed layer; The magnetic switching field of the magnetic compensation layer is greater than the magnetic switching field of the free layer.

2. The magnetically compensated MTJ device according to claim 1, in, The magnetic compensation layer includes a first compensation sublayer, a reverse coupling layer and a second compensation sublayer which are stacked in sequence.

3. The magnetically compensated MTJ device according to claim 2, in, The first compensation sublayer and / or the second compensation sublayer is a composite layer.

4. The magnetically compensated MTJ device according to claim 3, in, The composite layer includes an anisotropic auxiliary layer and a magnetic layer which are stacked.

5. The magnetically compensated MTJ device according to claim 4, in, The anisotropic auxiliary layer includes at least one of a magnesium oxide layer and a cobalt layer; When the anisotropic auxiliary layer is a magnesium oxide layer, the magnetic layer includes at least one of a cobalt layer, an iron layer, a nickel layer, a cobalt boride layer, an iron boride layer, a nickel boride layer, a cobalt iron layer, an iron nickel layer, a cobalt nickel layer, a cobalt iron boron layer, a cobalt iron platinum layer, a cobalt iron palladium layer, a cobalt iron terbium layer, a cobalt iron chromium layer and a cobalt iron gadolinium layer; When the anisotropic auxiliary layer is a cobalt layer, the magnetic layer includes at least one of a platinum layer, a palladium layer and a nickel layer.

6. The magnetically compensated MTJ device according to claim 2, in, The reverse coupling layer includes at least one of an iridium layer and a ruthenium layer.

7. The magnetically compensated MTJ device according to claim 1, in, The first given range is from 0.8 to 1.2, including endpoint values.

8. The magnetically compensated MTJ device according to any one of claims 1 to 7, in, Also included is an antiferromagnetic pinning layer; The antiferromagnetic pinning layer is disposed on a surface of the magnetic compensation layer away from the isolation layer.

9. An MRAM device, in, The MRAM device comprises the magnetically compensated MTJ device according to any one of claims 1 to 8.

10. A method for manufacturing a magnetically compensated MTJ device, include: Acquire the MTJ unit data to be processed, wherein the MTJ unit to be processed corresponding to the MTJ unit data to be processed includes a free layer, a barrier layer and a SAF fixed layer which are stacked; Determine reference temperature-dependent magnetization data according to the MTJ unit data to be processed, wherein the reference temperature-dependent magnetization data is data of a corresponding relationship between a net residual magnetization intensity of the SAF fixed layer corresponding to the SAF fixed layer and a temperature within a preset temperature range; Determine the magnetic compensation layer data according to the reference temperature-dependent magnetization data, so that the ratio of the net residual magnetization intensity of the magnetic compensation layer corresponding to the magnetic compensation layer data at the same temperature within the preset temperature range to the net residual magnetization intensity of the SAF fixed layer does not exceed a first given range, and the net residual magnetization intensity of the magnetic compensation layer is opposite to the direction of the net residual magnetization intensity of the SAF fixed layer, and the magnetic reversal field of the magnetic compensation layer is greater than the magnetic reversal field of the free layer; The MTJ unit to be processed is set according to the MTJ unit data to be processed, the magnetic compensation layer is set according to the magnetic compensation layer data, and an isolation layer is set between the MTJ unit to be processed and the magnetic compensation layer to obtain a finished MTJ device.

Citation Information

Patent Citations

  • Stram with compensation element

    CN102224546A

  • Magnetic tunnel junction for STT-MRAM

    CN105428522A

  • Vertical-magnetization magneto-resistance random access memory

    CN105552214A

  • Compensation of a bias magnetic field in a storage surface of a magnetoresistive storage cell

    CN1550018A

  • Stram with compensation element and method of making the same

    US20100226169A1

Cited By

  • Storage element, storage device, and electronic device

    EP4683453A4