Electroplating device and method for composite copper current collector

By using a copper oxide ball adding device and a base film extension roller assembly in a composite copper current collector electroplating device, combined with a soluble anode and a servo motor synchronous drive module, the problems of base film deformation and uneven copper layer during the electroplating process are solved. The uniformity and efficiency of the copper layer are achieved.

WO2024199261A1PCT designated stage expired Publication Date: 2024-10-03YANGZHOU NANOPORE INNOVATIVE MATERIALS TECH LTD

Patent Information

Application Number
PCT/CN2024/083994
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-03-27
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

In the electroplating process of composite copper current collectors, both clip plating and cathode roller plating have problems such as base film deformation, low conductive efficiency, and uneven copper layers. Especially during cathode roller plating, copper needs to be continuously added to the insoluble anode. The ions cause the electroplated copper layer to be uneven, and the cathode and anode are affected by the electric field force and are difficult to drive at a uniform speed.

Method used

A composite copper current collector electroplating device is designed, which uses a copper oxide ball adding device and a base film extension roller assembly. Through a soluble anode titanium blue plate and a conductive rectifier module, combined with a servo motor synchronous drive module, the copper ion concentration is uniform and uniform. The base film transmits uniformly, regulates current density and electric field strength, and ensures consistent thickness of the copper layer.

Benefits of technology

It achieves the uniformity and stability of the electroplated copper layer, improves the electroplating efficiency, ensures the smooth transmission of the base film in the electrolyte and the high precision and efficiency of the copper layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024083994_03102024_PF_FP_ABST
    Figure CN2024083994_03102024_PF_FP_ABST
Patent Text Reader

Abstract

An electroplating device and method for a composite copper current collector. The device comprises an electrolytic tank (1), wherein four groups of water injection ports (2) and water drainage ports (3) are sequentially provided from one end to the other end of the outside of the front face of the electrolytic tank (1); and a flattening and wrinkle-removing roller (4), a stainless-steel cathode roller member (5), a copper-oxide-ball addition device (6), a rectifier connecting electrically conductive assembly (7), a base-film extension roller assembly (8) and an anode titanium basket double-layer plate (9) are sequentially provided from one end to the other end inside the electrolytic tank (1).
Need to check novelty before this filing date? Find Prior Art

Description

Composite copper current collector electroplating device and method

[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on March 28, 2023, with application number 202310316239.9, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present application relates to the technical field of electroplating of composite current collectors, for example, to an electroplating device and method for a composite copper current collector. Background Art

[0003] The composite copper current collector is formed by dissolving copper ions in an electrolyte and using electroplating technology to evenly plate a copper layer on the upper and lower surfaces of the intermediate base film. During the electroplating process, the base film copper plating layer is plated using two methods: clamp plating and cathode roller plating. In the former, the base film is plated by clamps. Since the clamps squeeze the edge of the base film, the base film is clamped and deformed by the external force of the clamps. When the roller rod is driven, it is easy to cause deviations, resulting in wrinkles and ruptures of the base film. In addition, the number of conductive points plated by the clamps is large, and the number of connectors connected to the power wires is large, resulting in waste of conductive power and high manufacturing costs. The latter is composed of a cathode roller and an insoluble anode titanium blue. When the power is turned on, the anode and cathode are subjected to electric field forces. The cathode roller cannot rotate and roll without external force. Therefore, the cathode roller in the electrolyte is attached by copper ions during electroplating, and the base film copper plating layer is easily damaged by friction. When a servo motor with external force is used to drive the cathode roller to rotate, the base film is still disturbed by the liquid pressure and the length of the electroplating cell through the electrolyte, causing wrinkles in the base film and uneven plating.

[0004] In the process of electroplating using a cathode roller, the insoluble anode in the cathode roller requires continuous addition of copper ions into the electrolyte. However, the uneven concentration of copper ions added to the electrolyte causes uneven electroplating of the copper layer. In addition, the energized anode and cathode cannot rotate by themselves under the action of the electric field force to transmit the base film, resulting in difficulty for the electroplated base film to pass through the electrolyte at a uniform speed, and the problem of consistent thickness of the electroplated copper layer cannot be ensured.

[0005] Summary of the Invention

[0006] The present application provides an electroplating device and method for a composite copper current collector to solve the problems mentioned in the above-mentioned related technologies.

[0007] The present application provides an electroplating device for a composite copper current collector, comprising: an electrolytic cell, wherein a plurality of water inlets and drain outlets are sequentially provided from one end of the outer side of the front of the electrolytic cell to the other end, and a flattening and wrinkle-removing roller shaft, a stainless steel cathode roller, a copper oxide ball adding device, a rectifier conductive component, a base film extension roller component, and an anode titanium blue double-layer plate are sequentially provided from one end of the interior of the electrolytic cell to the other end, wherein the rectifier conductive component and the base film extension roller component are arranged in an interlaced combination, the rectifier conductive component is fixedly connected to the anode titanium blue double-layer plate, and the copper oxide ball adding device and the anode titanium blue double-layer plate are movably connected;

[0008] The base film stretching roller assembly includes a conductive column, a motor, a gear, a rotating shaft and a transmission wheel. An engine compartment is opened inside the conductive column, and the motor is arranged inside the engine compartment. The top of the motor and a side surface inside the gear are fixedly connected by a sleeve, and the other side surface of the gear and the bottom surface of the rotating shaft are fixedly connected. The side surface of the rotating shaft and the inner wall of the transmission wheel are fixedly connected by a sleeve.

[0009] Optionally, the copper oxide ball adding device includes a gravity sensor plate, a handle, a copper ball grid, a hydraulic cylinder and a ball net, the middle part of the upper surface of the gravity sensor plate and the middle part of the lower surface of the upper end of the copper ball grid are transmission connected through the upper and lower bottom surfaces of the hydraulic cylinder, the middle part of the side surface of the gravity sensor plate is fixedly connected to the end surface of the handle, the bottom of the copper ball grid is fixedly connected to multiple ball nets, and the side of the copper ball grid is provided with multiple liquid holes.

[0010] Optionally, the anode titanium blue double-layer plate includes a titanium blue plate, and a copper ball groove is opened inside the titanium blue plate.

[0011] Optionally, the flattening and wrinkle-removing roller includes a fixed roller frame, a central shaft and a roller, the inner side surfaces of the fixed roller frame are respectively fixedly connected to the bottom surface of the central shaft, and the side surfaces of the central shaft are movably connected to the inner wall of the roller.

[0012] Optionally, the stainless steel cathode roller member includes a group of solid roller piers, and a cathode roller shaft is arranged inside the solid roller piers.

[0013] Optionally, the lower surface shape of the rectifier conductive component is the same as the upper surface shape of the base film extension roller assembly, and both are arc-shaped, which are configured to prevent the base film from being scratched; the number of the anode titanium blue double-layer plates is two, which are placed on the upper and lower sides of the base film respectively, and the distance from the surface of the base film is 2 to 3 cm. The wall thickness of the anode titanium blue double-layer plate is 2 to 5 mm. The anode titanium blue double-layer plate is configured to be a soluble anode, and the upper and lower surfaces of the base film are electroplated by adding copper balls dissolved in the electrolyte to allow copper ions to diffuse into the solution.

[0014] Optionally, the telescopic height of the hydraulic cylinder is 3 to 6 cm, which is configured to adjust the height of the copper ball grid from the surface of the gravity sensor plate and the height of the copper balls in the grid from the base membrane in the electrolyte. When the copper balls inside the copper ball grid are consumed and become smaller during continuous electrolysis, the copper ion concentration of the copper balls and the height from the base membrane are changed, which is used to improve the electroplating efficiency; the shape of the grid is hemispherical, and the diameter of the grid is less than 6 cm. It is configured to evenly add the concentration of copper ions in the electrolyte to increase the dissolved surface area. During the electroplating process, the thickness of the copper plating layer is 900 to 1150 nm.

[0015] Optionally, the copper oxide ball adding device is connected to a copper ion detection module in the electrolyte, and the copper ion detection module in the electrolyte includes a copper ion detector; the copper ion detector is to detect in real time the detection data of the copper ion concentration dissolved in the copper balls placed inside the copper ball grid after contacting the electrolyte, and transmit the detection signal to the copper ion detection module in the electrolyte to judge the copper ion concentration value of the electrolyte. According to the reduction in the mass of the dissolved copper balls during the electrolytic consumption process, the hydraulic cylinder is controlled to raise the copper ball grid according to the pressure sensing of the gravity sensor plate, and the height of the copper ions in the electrolyte from the base membrane is continuously fine-tuned.

[0016] The base film extension roller assembly is connected to a servo motor synchronous drive module, and the servo motor synchronous drive module includes a uniform speed control unit; the uniform speed control unit controls multiple pairs of motors inside the machine chamber to perform synchronous driving at the same frequency and speed, and uses a transmission wheel to transmit the two sides of the base film in the electrolyte at a constant force at a uniform speed, so that the base film is evenly electroplated during the electroplating process, without wrinkles, and will not be torn or broken due to uneven force.

[0017] Optionally, the stainless steel cathode roller, the rectifier conductive component and the anode titanium blue double-layer plate are all connected to a cathode and anode conductive rectifier modules, and the anode and anode conductive rectifier modules include a rectifier parameter display and control unit; the parameters of the rectifier parameter display and control unit include current density, electric field strength and current magnitude; the rectifier parameter display and control unit is based on the stainless steel cathode roller and the anode titanium blue double-layer plate after being connected to the rectifier conductive component, and according to the thickness requirement of the electrolyte electroplated copper layer, the parameters of the rectifier parameter display and control unit are regulated and set to a uniform copper plating film, wherein the current density in the electroplating electrolyte is proportional to the electric field strength of the stainless steel cathode roller and the anode titanium blue double-layer plate, and satisfies the formula Where D k is the current density, in A / m 2 ; I is the current intensity; S is the total area of ​​the positive and negative electrodes; and D k =γ×E, where D k is the current density, in A / m 2 ; γ is the electrical conductivity, unit is S / m; E is the electric field strength, unit is V / m.

[0018] The present application also provides an electroplating method for a composite copper current collector, which is applied to the electroplating device for the composite copper current collector, comprising: within an electrolytic cell into which an electrolyte is injected, starting a servo motor synchronous drive module connected to a base film stretching roller assembly, and using a constant speed control unit to control the speed of a transmission wheel constantly transmitting the base film in the electrolyte;

[0019] Copper oxide balls are added using a copper oxide ball adding device, the copper oxide balls are placed inside the anode titanium blue double-layer plate, and the copper oxide balls are dissolved in the electrolyte in the electrolytic cell. The copper ion detection module in the electrolyte receives the copper ion concentration in the electrolyte detected by the copper ion detector, and according to the consumption of copper balls in the electroplated copper layer, the hydraulic cylinder is regulated to adjust the position of the copper balls in the ball net from the base film;

[0020] By connecting the current of the stainless steel cathode roller and the anode titanium blue double-layer plate through the rectifier conductive component, the anode and cathode of the electroplating are formed so that the copper ions in the electrolyte are plated onto the upper and lower surfaces of the base film by the electric field force. During the electroplating process, as the speed at which the base film is subjected to constant force transmission is adjusted, multiple parameters of the rectification parameter display and control unit in the anode and cathode conductive rectifier module are adjusted. By controlling the current size, ensuring the electroplating speed, and controlling the current density, the ions are prevented from being charged and breaking through the base film. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] FIG1 is a schematic diagram of the front structure of the electroplating device of the composite copper current collector of the present application.

[0022] FIG2 is a schematic side view of the structure of the electroplating device of the composite copper current collector of the present application.

[0023] FIG3 is a schematic structural diagram of the copper oxide ball adding device and the anode titanium blue double-layer plate of the present application.

[0024] FIG4 is a partial longitudinal cross-sectional view of the base film stretching roller assembly of the present application.

[0025] FIG5 is an exploded schematic diagram of the base film stretching roller assembly of the present application.

[0026] FIG6 is a longitudinal cross-sectional view of the electroplating device of the composite copper current collector of the present application.

[0027] FIG7 is a flow chart of the operation of the electroplating device for the composite copper current collector of the present application.

[0028] FIG8 is a schematic flow chart of the electroplating method of the composite copper current collector of the present application.

[0029] The accompanying drawings are marked as follows: 1, electrolytic cell; 2, water inlet; 3, drain outlet;

[0030] 4. Flattening and wrinkle removal roller; 401. Fixed roller frame; 402. Middle shaft; 403. Roller;

[0031] 5. Stainless steel cathode roller; 501, solid roller pier; 502, cathode roller shaft;

[0032] 6. Copper oxide ball adding device; 601. Gravity sensor plate; 602. Handle; 603. Copper ball grid; 604. Hydraulic cylinder; 605. Liquid hole; 606. Ball net; 7. Connect the rectifier conductive component;

[0033] 8. Base film stretching roller assembly; 801. Conductive column; 802. Machine chamber; 803. Motor; 804. Gear; 805. Rotating shaft; 806. Transmission wheel;

[0034] 9. Anode titanium blue double-layer plate; 901. Titanium blue plate; 902. Copper ball groove;

[0035] 10. Copper ion detection module in electrolyte; 1001. Copper ion detector;

[0036] 11. Anode and cathode conductive rectifier module; 1101. Rectification parameter display and control unit;

[0037] 12. Servo motor synchronous drive module; 1201. Uniform speed control unit. DETAILED DESCRIPTION

[0038] The technical solution of this application is described below through examples.

[0039] 1 to 6, the present application provides an electroplating device for a composite copper current collector, comprising an electrolytic cell 1, wherein a plurality of water injection ports 2 and drain ports 3 are sequentially provided from one end of the front outer side of the electrolytic cell 1 to the other end, and a flattening and wrinkle removal roller shaft 4, a stainless steel cathode roller 5, a copper oxide ball adding device 6, a rectifier conductive component 7, a base film extension roller assembly 8, and an anode titanium blue double-layer plate 9 are sequentially provided from one end of the interior of the electrolytic cell 1 to the other end, wherein the rectifier conductive component 7 and the base film extension roller assembly 8 are staggered and arranged in a staggered combination, the rectifier conductive component 7 is fixedly connected to the anode titanium blue double-layer plate 9, and the copper oxide ball adding device 6 and the anode titanium blue double-layer plate 9 are movably connected;

[0040] The base film stretching roller assembly 8 includes a conductive column 801, a motor 803, a gear 804, a rotating shaft 805 and a transmission wheel 806. An organic chamber 802 is opened inside the conductive column 801, and the motor 803 is arranged inside the organic chamber 802. The top of the motor 803 and the side surface inside the gear 804 are fixedly connected by a socket, and the other side surface of the gear 804 and the bottom surface of the rotating shaft 805 are fixedly connected. The side surface of the rotating shaft 805 and the inner wall of the transmission wheel 806 are fixedly connected by a socket.

[0041] In one embodiment, the copper oxide ball adding device 6 described in this embodiment includes a gravity sensor plate 601, a handle 602, a copper ball grid 603, a hydraulic cylinder 604 and a ball net 606. The middle part of the upper surface of the gravity sensor plate 601 and the middle part of the lower surface of the upper end of the copper ball grid 603 are transmission connected through the upper and lower bottom surfaces of the hydraulic cylinder 604. The middle part of the side surface of the gravity sensor plate 601 is fixedly connected to the end surface of the handle 602. The bottom of the copper ball grid 603 is fixedly connected to multiple ball nets 606, and the side of the copper ball grid 603 is provided with multiple liquid holes 605.

[0042] In one embodiment, the anode titanium blue double-layer plate 9 includes a titanium blue plate 901 , and a copper ball placement groove 902 is opened inside the titanium blue plate 901 .

[0043] In one embodiment, the flattening and wrinkle removal roller 4 includes a fixed roller frame 401, a central axis 402 and a roller 403. The side surfaces inside the fixed roller frame 401 are fixedly connected to the bottom surfaces of the central axis 402, and the side surfaces of the central axis 402 are movably connected to the inner walls of the roller 403.

[0044] In one embodiment, the stainless steel cathode roller 5 includes a set of fixed roller piers 501 , and a cathode roller shaft 502 is provided inside the fixed roller piers 501 .

[0045] In one embodiment, the lower surface of the rectifier conductive assembly 7 and the upper surface of the base film stretching roller assembly 8 are identical in shape, both being arc-shaped to prevent scratching of the base film. Two anode titanium blue double-layer plates 9 are placed on the upper and lower sides of the base film, 2 to 3 cm from the base film surface. The anode titanium blue double-layer plates 9 have a wall thickness of 2 to 5 mm. The anode titanium blue double-layer plates 9 are configured as soluble anodes. Copper balls are added and dissolved in the electrolyte, allowing copper ions to diffuse into the solution, thereby electroplating the upper and lower surfaces of the base film. The base film is located below the anode titanium blue double-layer plates 9.

[0046] In one embodiment, the telescopic height of the hydraulic cylinder 604 is described in this embodiment as 3 to 6 cm, which is configured to adjust the height of the copper ball grid 603 from the surface of the gravity sensor plate 601 and to adjust the height of the copper balls in the ball net 606 from the base membrane in the electrolyte. When the copper balls inside the copper ball grid 603 are consumed and become smaller during continuous electrolysis, the copper ion concentration of the copper balls and the height from the base membrane are changed, which is used to improve the electroplating efficiency; the shape of the ball net 606 is hemispherical, and the diameter of the ball net 606 is d, d < 6 cm, and it is configured to uniformly add the concentration of copper ions in the electrolyte to increase the dissolved surface area. During the electroplating process, the thickness of the copper plating layer is 900 to 1150 nm.

[0047] As shown in Figure 7, the present application provides an electroplating device for a composite copper current collector, which includes a copper oxide ball adding device 6 connected to a copper ion detection module 10 in the electrolyte, and the copper ion detection module 10 in the electrolyte includes a copper ion detector 1001; the copper ion detector 1001 is a real-time detection data of the copper ion concentration dissolved in the copper balls placed inside the copper ball grid 603 after contacting the electrolyte, and the detection signal is transmitted to the copper ion detection module 10 in the electrolyte to judge the copper ion concentration value of the electrolyte. According to the reduction in the mass of the dissolved copper balls during the electrolytic consumption process, the hydraulic cylinder 604 is controlled to raise the copper ball grid 603 according to the pressure sensing of the gravity sensor plate 601, and the height of the copper ions in the electrolyte from the base membrane is continuously fine-tuned.

[0048] The base film stretching roller assembly 8 is connected to a servo motor synchronous drive module 12, and the servo motor synchronous drive module 12 includes a uniform speed control unit 1201; the uniform speed control unit 1201 controls multiple pairs of motors 803 inside the machine chamber 802 to perform synchronous driving at the same frequency and speed, and uses the transmission wheel 806 to transmit the two sides of the base film in the electrolyte at a constant force at a uniform speed, so that the base film is evenly electroplated during the electroplating process, without wrinkles, and will not be torn or broken due to uneven force.

[0049] In one embodiment, the present embodiment describes that the stainless steel cathode roller 5, the rectifier conductive component 7 and the anode titanium blue double-layer plate 9 are all connected to the anode and cathode conductive rectifier modules 11, and the anode and cathode conductive rectifier modules 11 include a rectifier parameter display and control unit 1101; the parameters of the rectifier parameter display and control unit 1101 include current density, electric field strength and current magnitude; the rectifier parameter display and control unit 1101 is based on the stainless steel cathode roller 5 and the anode titanium blue double-layer plate 9 After the rectifier conductive component 7 is connected, according to the thickness requirement of the electrolyte electroplated copper layer, the parameters of the rectifier parameter display and control unit 1101 are regulated and set to a uniform copper plating film, wherein the current density in the electroplating electrolyte is proportional to the electric field strength of the stainless steel cathode roller 5 and the anode titanium blue double-layer plate 9, satisfying the formula Where D k is the current density, in A / m 2 ; I is the current intensity; S is the total area of ​​the positive and negative electrodes; and D k =γ×E, where D k is the current density, in A / m 2 ; γ is the electrical conductivity, unit is S / m; E is the electric field strength, unit is V / m.

[0050] As shown in FIG8 , the present application also provides an electroplating method for a composite copper current collector, which is applied to the electroplating device for the composite copper current collector, and includes the following steps.

[0051] S110. Inside the electrolytic cell injected with electrolyte, start the servo motor synchronous drive module connected to the base film stretching roller assembly, and use the uniform speed control unit to control the speed of the transmission wheel to constantly drive the base film in the electrolyte.

[0052] S120. Use a copper oxide ball adding device to add copper oxide balls, place the copper oxide balls inside the anode titanium blue double-layer plate, and dissolve the copper oxide balls in the electrolyte in the electrolytic cell. The copper ion detection module in the electrolyte receives the copper ion concentration in the electrolyte detected by the copper ion detector, and according to the copper ball consumption of the electroplated copper layer, regulate the lifting of the hydraulic cylinder to adjust the position of the copper ball in the ball net from the base membrane.

[0053] S130. Connect the current of the stainless steel cathode roller and the anode titanium blue double-layer plate by connecting the conductive component of the rectifier to form the anode and cathode for electroplating so that the copper ions in the electrolyte are plated onto the upper and lower surfaces of the base membrane by the electric field force. During the electroplating process, according to the speed at which the base membrane is subjected to constant force transmission, adjust multiple parameters of the rectification parameter display and control unit in the anode and cathode conductive rectification module, and prevent the base membrane from being charged and broken down by ions by controlling the current size, ensuring the electroplating speed, and controlling the current density.

[0054] In one embodiment, the present embodiment describes the following steps:

[0055] Step 1: Inside the electrolytic cell 1 filled with electrolyte, start the servo motor synchronous drive module 12 in the base film stretching roller assembly 8, and use the uniform speed control unit 1201 to control the speed of the transmission wheel 806 to constantly transmit the base film in the electrolyte.

[0056] Step 2. At the same time, copper oxide balls are added using the copper oxide ball adding device 6, and the copper oxide balls are placed inside the anode titanium blue double-layer plate 9, and the copper oxide balls are dissolved in the electrolyte in the electrolytic cell 1. The copper ion detection module 10 in the electrolyte receives the copper ion concentration in the electrolyte detected by the copper ion detector 1001, and according to the copper ball consumption of the electroplated copper layer, the hydraulic cylinder 604 is regulated to rise and fall to adjust the position of the copper ball in the ball net 606 from the base membrane.

[0057] Step three: connect the current of the stainless steel cathode roller 5 and the anode titanium blue double-layer plate 9 through the rectifier conductive component 7 to form the anode and cathode of the electroplating, so that the copper ions in the electrolyte are plated onto the upper and lower surfaces of the base film by the electric field force. During the electroplating process, as the base film is subjected to the constant force transmission speed, multiple parameters of the rectification parameter display and control unit 1101 in the anode and cathode conductive rectifier module 11 are adjusted, such as controlling the current size, ensuring the electroplating speed, and controlling the current density to prevent the charged ions from breaking through the base film.

[0058] This application has the following effects:

[0059] 1. The present application adopts the structure of a copper oxide ball adding device. In the method of electroplating copper layer with cathode roller and anode titanium blue, copper oxide balls are added to the soluble anode titanium blue and dissolved into the electrolyte to adjust the copper ion concentration. The area of ​​the copper balls contacting the electrolyte is evenly distributed through the ball net, and the position of the consumed copper balls from the base film is regulated by the hydraulic cylinder. The function of uniform copper ion concentration in the electrolyte and uniform copper plating layer of the base film is achieved, thereby improving the electroplating efficiency and achieving the effect of uniform film plating.

[0060] 2. The present application adopts the structure of a base film stretching roller assembly, and adopts a built-in motor of a conductive column connected to a servo motor synchronous drive module for synchronous operation, so that the uniform speed control unit can control the speed of the constant force transmission base film, and transmit the electroplated base film through a set of clockwise and counterclockwise rotation of the transmission wheels, thereby realizing the function of constant force transmission of the electroplated base film, which will not cause uneven force and tearing and rupture of the base film, and reduces the tension of the base film running in the electrolyte, thereby achieving the effect of stable operation of the base film and stable electroplated copper layer.

[0061] 3. This application adopts a system module consisting of a copper ion detection module in the electrolyte, an anode and cathode conductive rectification module, and a servo motor synchronous drive module. Through systematic intelligent control, it collects copper ion concentration signals, and realizes the function of high-precision electroplating composite copper current collector according to the speed of transmitting the base film, and controlling the current size and current density during electroplating, thereby achieving the accuracy, efficiency and stability of the electroplated copper layer.

Claims

1. An electroplating device for a composite copper current collector, comprising: An electrolytic cell, wherein multiple groups of water injection ports and drainage ports are sequentially arranged from one end to the other end of the outer side of the front of the electrolytic cell, and a flattening and wrinkle-removing roller shaft, a stainless steel cathode roller, a copper oxide ball adding device, a rectifier conductive component, a base film extension roller component and an anode titanium blue double-layer plate are sequentially arranged from one end to the other end of the inside of the electrolytic cell, wherein the rectifier conductive component and the base film extension roller component are arranged alternately, the rectifier conductive component is fixedly connected to the anode titanium blue double-layer plate, and the copper oxide ball adding device and the anode titanium blue double-layer plate are movably connected; The base film stretching roller assembly includes a conductive column, a motor, a gear, a rotating shaft and a transmission wheel. A machine chamber is opened inside the conductive column, and the motor is arranged inside the machine chamber. The top of the motor is fixedly sleeved with a side surface inside the gear, and the other side surface of the gear is fixedly connected to the bottom surface of the rotating shaft. The side surface of the rotating shaft is fixedly sleeved with the inner wall of the transmission wheel.

2. The device according to claim 1, wherein: The copper oxide ball adding device includes a gravity sensor plate, a handle, a copper ball grid, a hydraulic cylinder and a ball net. The middle part of the upper surface of the gravity sensor plate and the middle part of the lower surface of the upper end of the copper ball grid are transmission connected through the upper and lower bottom surfaces of the hydraulic cylinder. The middle part of the side surface of the gravity sensor plate is fixedly connected to the end surface of the handle. A plurality of ball nets are fixedly connected to the bottom of the copper ball grid. A plurality of liquid holes are provided on the side surface of the copper ball grid.

3. The device according to claim 1, wherein: The anode titanium blue double-layer plate comprises a titanium blue plate, and a copper ball groove is provided inside the titanium blue plate.

4. The device according to claim 1, wherein: The flattening and wrinkle-removing roller shaft comprises a fixed roller frame, a central shaft and a roller. The inner side surfaces of the fixed roller frame are respectively fixedly connected to the bottom surface of the central shaft, and the side surfaces of the central shaft are movably sleeved and connected to the inner wall of the roller.

5. The device according to claim 1, wherein: The stainless steel cathode roller member comprises a group of solid roller piers, and a cathode roller shaft is arranged inside the solid roller piers.

6. The device according to claim 1, wherein: The lower surface shape of the rectifier conductive component is the same as the upper surface shape of the base film extension roller component. The number of the anode titanium blue double-layer plates is two, which are placed on the upper and lower sides of the base film respectively, and the distance from the surface of the base film is 2 to 3 cm. The wall thickness of the anode titanium blue double-layer plate is 2 to 5 mm, and the anode titanium blue double-layer plate is configured to be a soluble anode.

7. The device according to claim 2, wherein: The telescopic height of the hydraulic cylinder is 3-6 cm; the shape of the ball net is hemispherical, and the diameter of the ball net is less than 6 cm.

8. The device according to claim 7, wherein: The copper oxide ball adding device is connected to a copper ion detection module in the electrolyte, and the copper ion detection module in the electrolyte includes a copper ion detector; the base film extension roller assembly is connected to a servo motor synchronous drive module, and the servo motor synchronous drive module includes a uniform speed control unit.

9. The device according to claim 7, wherein: The stainless steel cathode roller, the rectifier conductive component and the anode titanium blue double-layer plate are all connected to anode and cathode conductive rectification modules, and the anode and cathode conductive rectification modules include a rectification parameter display and control unit; the parameters of the rectification parameter display and control unit include current density, electric field strength and current size.

10. A method for electroplating a composite copper current collector, applied to an electroplating device for a composite copper current collector according to any one of claims 1 to 9, comprising: Inside the electrolytic cell into which the electrolyte is injected, the servo motor synchronous drive module connected to the base film stretching roller assembly is started, and the speed of the base film in the electrolyte is controlled by the constant speed control unit; The copper oxide balls are added by using a copper oxide ball adding device, the copper oxide balls are placed inside the anode titanium blue double-layer plate, and the copper oxide balls are dissolved in the electrolyte in the electrolytic cell, the copper ion concentration in the electrolyte detected by the copper ion detector is received by the copper ion detection module in the electrolyte, and the position of the copper ball in the ball net from the base film is adjusted by regulating the lifting of the hydraulic cylinder according to the copper ball consumption of the electroplated copper layer; The current of the stainless steel cathode roller and the anode titanium blue double-layer plate is connected by connecting the rectifier conductive component to form the anode and cathode for electroplating so that the copper ions in the electrolyte are plated onto the upper and lower surfaces of the base film by the electric field force. During the electroplating process, according to the speed at which the base film is subjected to constant force transmission, multiple parameters of the rectification parameter display and control unit in the anode and cathode conductive rectification module are adjusted to prevent the ions from being charged and breaking through the base film by controlling the current size, ensuring the electroplating speed, and controlling the current density.

Citation Information

Patent Citations

  • Flattening roller, conveying mechanism and treatment device

    CN110685005A

  • Production and processing system of conductive film

    CN114717621A

  • Electroplating device for composite copper current collector

    CN116479505A

  • Full-automatic electroplating assembly line

    CN210765568U

  • Method for producing two layer circuit board by plating process and plating device therefor

    JP2007246962A

Cited By

  • Electroplating process and device for positive electrode and negative electrode of lithium battery tab

    CN119710881A