Deep trench device and manufacturing method therefor

By simultaneously fabricating the first trench and the second trench, and depositing polysilicon in the substrate, the problem of complex processes and high costs in the existing technology is solved, and the process of deep trench devices is simplified and the cost is reduced.

WO2024199413A1PCT designated stage expired Publication Date: 2024-10-033PEAK (SHANGHAI) LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/084683
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-29
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

The process of existing deep trench devices is complex and costly, mainly because it is necessary to fabricate the second trench after the first trench is completed and perform multiple polysilicon depositions.

Method used

Using a method of simultaneously fabricating the first trench and the second trench, the width of the second trench is larger than that of the first trench, and the first trench extends into the second doping type buried layer, and the second trench extends into the second doped type buried layer. In a doped type substrate, spacers and polysilicon are deposited on the sidewalls.

Benefits of technology

The process flow is simplified, process costs are reduced, and process steps and material usage are reduced through simultaneous fabrication and deposition of the same type of polysilicon.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024084683_03102024_PF_FP_ABST
    Figure CN2024084683_03102024_PF_FP_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of semiconductors, and provides a deep trench device and a manufacturing method therefor. A first-doping-type substrate is first provided, a second-doping-type buried layer and a first-doping-type epitaxial layer are manufactured on one side of the substrate, and then first trenches and second trenches are manufactured in the epitaxial layer at the same time, wherein the width of the second trenches is larger than that of the first trenches, the first trenches extend into the second-doping-type buried layer, and the second trenches extend into the first-doping-type substrate; and a spacer layer is manufactured on the side walls of the first trenches and the second trenches, and finally second-doping-type polycrystalline silicon is deposited in the first trenches and the second trenches. The deep trench device and the manufacturing method therefor provided by the present application have the advantages of simpler process and lower cost.
Need to check novelty before this filing date? Find Prior Art

Description

Deep trench device and manufacturing method thereof

[0001] The present invention claims priority to Chinese patent application No. 2023103427811, filed with the Patent Office of China on March 31, 2023, entitled “A deep trench device and its manufacturing method”. The entire contents of the application are incorporated herein by reference. Technical Field

[0002] The present application relates to the field of semiconductor technology, and in particular to a deep trench device and a method for manufacturing the same. Background Art

[0003] Currently, when manufacturing second-trench devices, an N-type buried layer is incorporated into the device structure, with the chip connected to the buried layer via the first trench. However, because the N-type buried layer is installed as a single layer, it can short to the grounding area within the P-type substrate during chip slicing, impacting device performance.

[0004] In order to solve this problem, a second trench for isolation is generally set in the existing technology. The depth of the second trench is relatively large, generally up to 20 to 30 μm, and the second trench passes through the N-type buried layer and extends to the substrate area. This can achieve overall isolation of the chip and improve device performance.

[0005] However, this method requires that the second trench be made after the first trench is made, and two steps of polysilicon deposition be performed, resulting in a relatively complex process and relatively high cost.

[0006] In summary, the prior art has the problem that the process of deep trench devices is relatively complex and the cost is relatively high.

[0007] Summary of the Invention

[0008] The purpose of the present application is to provide a deep trench device and a method for manufacturing the same, so as to solve the problem in the prior art that the process of the deep trench device is relatively complex and the cost is relatively high.

[0009] In order to solve the above problems, this application provides the following technical solutions:

[0010] In one aspect, an embodiment of the present application provides a method for manufacturing a deep trench device, the method comprising:

[0011] providing a first doping type substrate;

[0012] Fabricating a second doping type buried layer and a first doping type epitaxial layer based on one side of the substrate;

[0013] A first trench and a second trench are simultaneously formed based on the epitaxial layer; wherein the width of the second trench is greater than the width of the first trench, and the first trench extends into the second doping type buried layer, and the second trench extends into the first doping type substrate;

[0014] forming a spacer layer based on the sidewalls of the first trench and the second trench;

[0015] Second doping type polysilicon is deposited based on the first trench and the second trench.

[0016] Optionally, the step of simultaneously forming the first trench and the second trench based on the epitaxial layer includes:

[0017] The first groove and the second groove are manufactured with a width ratio of 2.4 to 2.6.

[0018] Optionally, a width ratio of the first groove to the second groove is 2.5.

[0019] Optionally, before the step of forming a spacer layer based on the sidewalls of the first trench and the second trench, the method further includes:

[0020] oxidizing the sidewalls and bottoms of the first trench and the second trench to form an oxide layer;

[0021] The oxide layer is removed.

[0022] Optionally, the step of forming a spacer layer based on the sidewalls of the first trench and the second trench includes:

[0023] forming a spacer layer based on the sidewalls and bottoms of the first trench and the second trench;

[0024] The spacer layer located at the bottom of the first trench and the second trench is removed.

[0025] Optionally, before the step of depositing polysilicon of the second doping type based on the first trench and the second trench, the method further includes:

[0026] Ion implantation is performed along a preset angle to form a highly doped region at the bottom of the second trench, while the bottom of the first trench remains unchanged.

[0027] Optionally, the step of depositing second doping type polysilicon based on the first trench and the second trench includes:

[0028] Depositing 2.5um to 2.6um of second doped type polysilicon based on the first trench and the second trench;

[0029] The second doping type polysilicon is etched back.

[0030] Optionally, the step of depositing second doping type polysilicon based on the first trench and the second trench includes:

[0031] Performing a first filling of the first trench and the second trench with second doping type polysilicon;

[0032] etching back the second doping type polysilicon to widen the opening of the second trench;

[0033] The first trench and the second trench are refilled with second doping type polysilicon.

[0034] Optionally, after the step of depositing polysilicon of a second doping type based on the first trench and the second trench, the method further includes:

[0035] The polysilicon on the back side of the first doping type substrate is removed.

[0036] On the other hand, an embodiment of the present application further provides a deep trench device, comprising:

[0037] a first doping type substrate;

[0038] a second doping type buried layer and a first doping type epitaxial layer located on one side of the substrate;

[0039] a first trench and a second trench located in the epitaxial layer; wherein the width of the second trench is greater than the width of the first trench, the first trench extends into the second doping type buried layer, and the second trench extends into the first doping type substrate;

[0040] a spacer layer located on sidewalls of the first trench and the second trench;

[0041] Second doping type polysilicon is located in the first trench and the second trench.

[0042] Optionally, a width ratio of the first groove to the second groove is 2.4-2.6.

[0043] Optionally, a width ratio of the first groove to the second groove is 2.5.

[0044] Compared with the prior art, the embodiments of the present application have the following beneficial effects:

[0045] The present application provides a deep trench device and a method for manufacturing the same. The method includes first providing a substrate of a first doping type, then forming a buried layer of a second doping type and an epitaxial layer of a first doping type on one side of the substrate, and then simultaneously forming a first trench and a second trench on the epitaxial layer. The second trench has a width greater than the width of the first trench, and the first trench extends into the buried layer of the second doping type, while the second trench extends into the substrate of the first doping type. A spacer layer is then formed on the sidewalls of the first and second trenches, and finally, polysilicon of a second doping type is deposited on the first and second trenches. Because the first and second trenches are fabricated simultaneously in the present application, and the polysilicon deposited in the first and second trenches is the same type, the fabrication process can be simplified and process costs can be reduced.

[0046] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, preferred embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the following is a brief introduction to the drawings required for use in the embodiments. It should be understood that the following drawings only illustrate certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without creative work.

[0048] FIG1 is a schematic cross-sectional view of a first deep trench device in the prior art.

[0049] FIG2 is a cross-sectional schematic diagram of a second deep trench device in the prior art.

[0050] FIG3 is an exemplary flow chart of a method for manufacturing a deep trench device provided in an embodiment of the present application.

[0051] FIG4 is a schematic cross-sectional view of a deep trench device provided in an embodiment of the present application.

[0052] FIG5 is a schematic cross-sectional view of the manufacturing process of the second doping type buried layer according to an embodiment of the present application.

[0053] FIG6 is a schematic cross-sectional view corresponding to the manufacturing of the hard mask layer according to an embodiment of the present application.

[0054] FIG7 is a schematic cross-sectional view of the manufacturing process of the first groove and the second groove provided in an embodiment of the present application.

[0055] FIG8 is a schematic cross-sectional view corresponding to S1071 provided in an embodiment of the present application.

[0056] FIG9 is a schematic cross-sectional view corresponding to the manufacturing of the spacer layer according to an embodiment of the present application.

[0057] FIG10 is a schematic cross-sectional view corresponding to the removal of the spacer layer at the bottom of the first trench and the second trench according to an embodiment of the present application.

[0058] FIG11 is a schematic cross-sectional view of an embodiment of the present application after ion implantation. DETAILED DESCRIPTION

[0059] To make the objectives, technical solutions, and advantages of the embodiments of the present application more clear, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the accompanying drawings of the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Generally, the components of the embodiments of the present application described and shown in the drawings herein can be arranged and designed in various different configurations.

[0060] Therefore, the following detailed description of the embodiments of the present application provided in the accompanying drawings is not intended to limit the scope of the present application for protection, but merely represents selected embodiments of the present application. All other embodiments obtained by persons of ordinary skill in the art based on the embodiments in the present application without creative work are within the scope of protection of the present application.

[0061] It should be noted that similar reference numerals and letters represent similar items in the following drawings. Therefore, once an item is defined in one drawing, it does not need to be further defined or explained in subsequent drawings. At the same time, in the description of this application, the terms "first", "second", etc. are only used to distinguish the description and should not be understood as indicating or implying relative importance.

[0062] It should be noted that, in this document, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply the existence of any such actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article, or device comprising a series of elements includes not only those elements, but also other elements not explicitly listed, or elements inherent to such process, method, article, or device. In the absence of further limitations, an element defined by the phrase "comprising a ..." does not exclude the presence of other identical elements in the process, method, article, or device comprising the element.

[0063] In the description of this application, it should be noted that the terms "upper", "lower", "inside", "outside", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, or are the orientations or positional relationships in which the product of the application is usually placed when in use. They are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, they should not be understood as limitations on this application.

[0064] The following describes some embodiments of the present application in detail with reference to the accompanying drawings. In the absence of conflict, the following embodiments and features therein may be combined with each other.

[0065] As described in the background art, the prior art has the problem that the technology of deep trench devices is relatively complex and the cost is relatively high.

[0066] Please refer to Figure 1, which shows a cross-sectional schematic diagram of a deep trench device in the prior art. In the prior art, the trench is connected to the N-type buried layer, and specific devices of the chip can be arranged inside the trench. For example, NMOS and PMOS devices are arranged in Figure 1. Of course, other devices can also be arranged according to actual needs, which is not limited here.

[0067] In the structure shown in Figure 1, when the device needs to be packaged, the P-type substrate is grounded. During the packaging process, the N-type buried layer may be short-circuited with the P-type substrate grounding area. For example, when a short circuit occurs at point A in the figure, since the entire layer of N-type buried layer is at the same potential, the potential of the entire layer of N-type buried layer is 0V, which affects the device performance or may even cause damage to the device.

[0068] In light of this, referring to Figure 2, in the prior art, a second trench is typically provided along with the first trench. The second trench is deeper, with its bottom extending into the P-type substrate. P-type polysilicon is deposited in the second trench, while N-type polysilicon is deposited in the first trench. The second trench divides the N-type buried layer into two regions, one on either side of the second trench, and the two regions of N-type buried layer are isolated from each other. As shown in Figure 2, points A and B are separated by the second trench. Consequently, even if a short circuit occurs at point A, point B will not be affected, ensuring the stability of the device during a short circuit.

[0069] However, the manufacturing process of this structure is relatively complicated. It is necessary to make the first trench first and then the second trench, and different types of polysilicon need to be deposited in the first trench and the second trench. Therefore, the existing technology has the problem of complex process and high process cost for the production of the second trench used for isolation.

[0070] In view of this, the present application provides a method for manufacturing a deep trench device, which simplifies the manufacturing process of the second trench by simultaneously manufacturing the first trench and the second trench, thereby achieving the purpose of reducing process costs.

[0071] The following is an exemplary description of the deep trench device manufacturing method provided in this application:

[0072] As an implementation method, referring to FIG3 , the deep trench device manufacturing method includes:

[0073] S102, providing a first doping type substrate;

[0074] S104, forming a second doping type buried layer and a first doping type epitaxial layer based on one side of the substrate;

[0075] S106, simultaneously forming a first trench and a second trench based on the epitaxial layer; wherein the width of the second trench is greater than the width of the first trench, and the first trench extends into the second doping type buried layer, and the second trench extends into the first doping type substrate;

[0076] S108, forming a spacer layer based on the sidewalls of the first trench and the second trench;

[0077] S110 , depositing second doping type polysilicon based on the first trench and the second trench.

[0078] The first doping type and the second doping type described in this application refer to N-type and P-type, respectively. When the first doping type is N-type, the second doping type is P-type; and when the first doping type is P-type, the second doping type is N-type. For ease of explanation, the text and drawings of this application are based on the example of the first doping type being P-type and the second doping type being N-type.

[0079] Please refer to Figure 4, which is a cross-sectional schematic diagram of the deep trench device in the present application, wherein N-type polysilicon is deposited in both the first trench and the second trench, so that the first trench and the second trench can be manufactured simultaneously, simplifying the process flow and reducing process costs. It is only necessary to set the width of the second trench larger than the width of the first trench to ensure that when the bottom of the first trench extends into the N-type buried layer, the second trench can pass through the N-type buried layer and the bottom extends into the P-type substrate.

[0080] As an implementation, see Figure 5. When forming the second-doped buried layer and the first-doped epitaxial layer on one side of the substrate, a 200Å thick oxide layer can be grown on the P-type substrate for masking. Subsequently, when forming the buried layer, high-dose antimony or arsenic implants (1-3E15 / 60keV-80keV) can be used along with high-energy phosphorus co-implantations (1-5E13, 1-1.5MeV). Alternatively, the phosphorus co-implantation can be skipped for better isolation.

[0081] Afterwards, as shown in FIG6 , after annealing the buried layer, the oxide layer can be removed, and a P-type epitaxial layer can be grown on the side of the buried layer away from the substrate. For example, the thickness of the P-type epitaxial layer can be 8um to 13um. Afterwards, a hard mask layer can be formed on the surface of the epitaxial layer to form a trench. The hard mask layer can include an oxide layer, a nitride layer, and a TEOS layer. The thickness of the oxide layer can be 100A to 200A, the thickness of the nitride layer can be 1000A to 2000A, and the thickness of the TEOS can be 2000A to 3000A. Of course, in another implementation, only the oxide layer and the nitride layer can be used as the hard mask layer, which is not limited here.

[0082] Please refer to 7. When forming the first trench and the second trench, the trenches are etched on the epitaxial layer based on the hard mask layer. Specifically, when etching the trenches, the trench area can be defined first, and then etching is performed in the trench area to form the trenches.

[0083] It should be noted that when etching the first groove and the second groove, the first groove and the second groove can be carried out simultaneously. Based on the etching characteristics, when the width of the groove is larger, the depth of the etched groove is deeper. Therefore, this application sets the width of the second groove to be greater than the width of the first groove, thereby ensuring that the depth of the second groove formed by etching is greater than the depth of the first groove.

[0084] To ensure a significant isolation effect for the second trench, its depth needs to differ significantly from that of the first trench. Research has found that optimal results are achieved when the second trench is located at a depth greater than 3 μm within the P-type substrate. This means that the value of X in Figure 7 can be greater than 3 μm. Based on this, the width ratio of the first trench to the second trench is 2.4 to 2.6, with a preferred ratio of 2.5. In other words, in practice, the width of the second trench can be 2.5 times the width of the first trench.

[0085] For example, when the width of the first trench is 0.8 μm, the width of the second trench can be selected to be 2 μm. With this setting, during the etching process, it is only necessary to control the depth of the first trench, that is, to ensure that the etching of the first trench stops at the second doping type buried layer, and the etching of the second trench must stop at the first doping type substrate.

[0086] Of course, the above-mentioned ratio of the groove width is only an example. In practical applications, the ratio of the groove width may not be limited thereto. For example, in another example, the width of the first groove is 0.8 um, and the width of the second groove is 1.2 um.

[0087] Since the sidewalls of the trenches may be damaged after the first trench and the second trench are formed, in one implementation, the method further includes:

[0088] S1071, oxidizing the sidewalls and bottoms of the first trench and the second trench to form an oxide layer;

[0089] S1072, remove the oxide layer.

[0090] Referring to FIG. 8 , before forming the spacer layer, the sidewalls of the first trench and the second trench are processed using an oxide layer as a sacrificial layer, so that the sidewalls of the first trench and the second trench are smoother.

[0091] Optionally, an oxide layer of 110A can be grown along the side walls of the first trench and the second trench as a sacrificial layer, and then the oxide layer can be removed using a wet etching process, thereby removing the damage to the side walls of the first trench and the second trench caused by etching, making the side walls smoother. In addition, the openings of the first trench and the second trench can be widened, making the subsequent polysilicon deposition process more convenient.

[0092] After the sidewall processing is completed, a spacer layer can be formally formed along the surface of the first trench and the second trench. Please refer to Figure 9. In one implementation, the spacer layer includes an oxide layer and a nitride layer, and the oxide layer and the nitride layer are both relatively thin. The thickness of the oxide layer is 100A~200A, and the thickness of the nitride layer is 100A~300A. Of course, a pure oxide layer can also be used to achieve isolation. For example, an oxide layer with a thickness of 300A~1000A is selected as the spacer layer to achieve better isolation effect.

[0093] Furthermore, after growing the spacer layer, it is necessary to remove the spacer layer at the bottom of the first and second trenches. This allows for direct electrical connection between the polysilicon and the N-type buried layer after subsequent polysilicon deposition, and the trench sidewalls are isolated from the epitaxial layer by the spacer layer. The structure after removing the spacer layer at the bottom of the first and second trenches is shown in Figure 10. It should be noted that when removing the spacer layer at the bottom of the trench, a dry selective etching process is used, and the TEOS used as the mask layer is also partially etched, for example, by 1000 Å.

[0094] Since the second doped type polysilicon is deposited based on the first trench and the second trench during the subsequent deposition of polysilicon, and the second trench is directly connected to the first doped type substrate, a PN junction will be formed at the bottom of the second trench after the polysilicon is deposited, resulting in a larger contact resistance.

[0095] Therefore, in one implementation, in order to reduce the contact resistance, ion implantation can be performed on the bottom of the second trench so that the ion concentration in the bottom area of ​​the second trench is higher, forming a highly doped area. Moreover, since the elements to be implanted are Group III elements, ion implantation cannot be performed into the first trench.

[0096] On this basis, the method also includes:

[0097] Ion implantation is performed along a preset angle to form a high-doping region at the bottom of the second trench, while the bottom of the first trench remains unchanged.

[0098] Because the width of the second trench is greater than that of the first trench, a small-angle implantation ensures that the bottom of the first trench is not affected during ion implantation into the bottom of the second trench. The applicant has found that the preset angle is 4° to 6°. For example, during ion implantation, a low-energy 5keV, high-dose 5E15 boron implantation with a tilt angle of 5° is used.

[0099] For example, taking the width of the first groove as 0.8um and the width of the second groove as 2um as an example, when the depth of the first groove is 12.4um and the depth of the second groove is 28.6um, the preset angle is 4°; when the depth of the first groove is 9.1um and the depth of the second groove is 22.8um, the preset angle is 5°; when the depth of the first groove is 7.6um and the depth of the second groove is 19.0um, the preset angle is 6°. The structure after ion implantation is shown in Figure 11.

[0100] When depositing the second doped type polysilicon, as an implementation method, 2.5um to 2.6um of the second doped type polysilicon may be deposited based on the first trench and the second trench, and the second doped type polysilicon may be etched back.

[0101] In the prior art, 5000A of polysilicon is generally deposited. In this application, since a deeper second trench is provided, in order to ensure that the second trench can be filled with sufficient polysilicon, thicker polysilicon can be deposited, and then the excess polysilicon can be removed.

[0102] Furthermore, when depositing polysilicon, a gap may exist in the center of the second trench. To reduce the gap, polysilicon may be deposited in two steps. On this basis, S110 includes:

[0103] Performing a first filling of the first trench and the second trench with second doping type polysilicon;

[0104] etching back the second doped type polysilicon to widen the opening of the second trench;

[0105] The first trench and the second trench are refilled with second doping type polysilicon.

[0106] After the first step of polysilicon deposition, a polysilicon dry etch-back process may be added to widen the opening of the second trench, thereby better filling the polysilicon again and reducing the voids in the trench.

[0107] After depositing polysilicon, the mask layer needs to be removed. For example, a CMP polishing process can be used to polish away excess polysilicon on the surface, stopping at the TEOS or nitride layer. It should be noted that when depositing polysilicon, polysilicon will also exist on the back of the substrate. Therefore, in order to reduce the problem of substrate warping, the polysilicon on the back of the first doping type substrate can be removed first, and then the polysilicon on the surface of the epitaxial layer can be etched back.

[0108] When performing polysilicon etching back, the polysilicon is etched back by dry etching to keep the top surface of the polysilicon and the silicon surface at the same level, using TEOS residue or nitride hard mask layer as a protective layer, and then removing the TEOS and nitride layers.

[0109] Devices are then fabricated in the area surrounding the first trench. Subsequent processes are conventional and will not be detailed here. Taking the CMOS device process as an example, subsequent fabrication involves STI, LOCOS, well implantation, gate, LDD implantation, spacers, source / drain implantation, oxide, ILD (interlayer dielectric), contact layer, BEoL metal layer, and passivation.

[0110] Based on the above implementation, the embodiment of the present application further provides a deep trench device. Please refer to FIG4 . The deep trench device includes:

[0111] a first doping type substrate;

[0112] A second doping type buried layer and a first doping type epitaxial layer located on one side of the substrate;

[0113] A first trench and a second trench are located in the epitaxial layer; wherein the width of the second trench is greater than the width of the first trench, and the first trench extends into the second doping type buried layer, and the second trench extends into the first doping type substrate;

[0114] a spacer layer located on the sidewalls of the first trench and the second trench;

[0115] The second doping type polysilicon is located in the first trench and the second trench.

[0116] The width ratio of the first groove to the second groove is 2.4-2.6. Preferably, the width ratio of the first groove to the second groove is 2.5.

[0117] In summary, the present application provides a deep trench device and a method for manufacturing the same. First, a first-doping type substrate is provided. Next, a second-doping type buried layer and a first-doping type epitaxial layer are formed on one side of the substrate. Then, a first trench and a second trench are simultaneously formed on the epitaxial layer. The width of the second trench is greater than the width of the first trench, and the first trench extends into the second-doping type buried layer, while the second trench extends into the first-doping type substrate. A spacer layer is then formed on the sidewalls of the first and second trenches. Finally, second-doping type polysilicon is deposited on the first and second trenches. Because the first and second trenches are fabricated simultaneously in the present application, and the type of polysilicon deposited in the first and second trenches is the same, the fabrication process can be simplified, saving process costs.

[0118] The above description is merely a preferred embodiment of the present application and is not intended to limit the present application. Various modifications and variations are possible for those skilled in the art. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present application shall be included within the scope of protection of the present application.

[0119] It will be apparent to those skilled in the art that the present application is not limited to the details of the exemplary embodiments described above and that the present application can be implemented in other specific forms without departing from the spirit or essential characteristics of the present application. Therefore, the embodiments should be considered in all respects as illustrative and non-restrictive, and the scope of the present application is defined by the appended claims, not the foregoing description, and all variations within the meaning and range of equivalents of the claims are intended to be included therein. Any reference sign in a claim should not be construed as limiting the claim to which it relates.

Claims

1. A method for manufacturing a deep trench device, characterized in that: The deep trench device manufacturing method comprises: providing a first doping type substrate; Fabricating a second doping type buried layer and a first doping type epitaxial layer based on one side of the substrate; A first trench and a second trench are simultaneously formed based on the epitaxial layer; wherein the width of the second trench is greater than the width of the first trench, and the first trench extends into the second doping type buried layer, and the second trench extends into the first doping type substrate; forming a spacer layer based on the sidewalls of the first trench and the second trench; Second doping type polysilicon is deposited based on the first trench and the second trench.

2. The method for manufacturing a deep trench device according to claim 1, wherein: The step of simultaneously forming a first trench and a second trench based on the epitaxial layer comprises: The first groove and the second groove are manufactured with a width ratio of 2.4 to 2.

6.

3. The method for manufacturing a deep trench device according to claim 2, wherein: The width ratio of the first groove to the second groove is 2.

5.

4. The method for manufacturing a deep trench device according to claim 1, wherein: Before the step of forming a spacer layer based on the sidewalls of the first trench and the second trench, the method further includes: Oxidizing the sidewalls and bottoms of the first trench and the second trench to form an oxide layer; The oxide layer is removed.

5. The method for manufacturing a deep trench device according to claim 1, wherein: The step of forming a spacer layer based on the sidewalls of the first trench and the second trench comprises: Forming a spacer layer based on the sidewalls and bottoms of the first trench and the second trench; The spacer layer at the bottom of the first trench and the second trench is removed.

6. The method for manufacturing a deep trench device according to claim 1, wherein: Before the step of depositing second doping type polysilicon based on the first trench and the second trench, the method further includes: Ion implantation is performed along a preset angle to form a high-doping region at the bottom of the second trench, and the bottom of the first trench remains unchanged.

7. The method for manufacturing a deep trench device according to claim 1, wherein: The step of depositing second doping type polysilicon based on the first trench and the second trench comprises: Depositing 2.5um to 2.6um of second doped type polysilicon based on the first trench and the second trench; The second doping type polysilicon is etched back.

8. The method for manufacturing a deep trench device according to claim 1, wherein: The step of depositing second doping type polysilicon based on the first trench and the second trench comprises: Performing a first filling of the first trench and the second trench with second doping type polysilicon; Performing etching back on the second doping type polysilicon to widen the opening of the second trench; The first trench and the second trench are refilled with second doping type polysilicon.

9. The method for manufacturing a deep trench device according to claim 1, wherein: After the step of depositing second doping type polysilicon based on the first trench and the second trench, the method further includes: The polysilicon on the back side of the first doping type substrate is removed.

10. A deep trench device, characterized in that: The deep trench device comprises: a first doping type substrate; A second doping type buried layer and a first doping type epitaxial layer located on one side of the substrate; A first trench and a second trench located in the epitaxial layer; wherein the width of the second trench is greater than the width of the first trench, and the first trench extends into the second doping type buried layer, and the second trench extends into the first doping type substrate; a spacer layer located on the sidewalls of the first trench and the second trench; The second doping type polysilicon is located in the first trench and the second trench.

11. The deep trench device according to claim 10, characterized in that: The width ratio of the first groove to the second groove is 2.4-2.

6.

12. The deep trench device according to claim 11, characterized in that: The width ratio of the first groove to the second groove is 2.5.

Citation Information

Patent Citations

  • Substrate contact etch process

    CN107851577A

  • Semiconductor device and manufacturing method thereof

    CN114420631A

  • Deep groove device and manufacturing method thereof

    CN116798940A

  • Semiconductor structure and method

    US20070018195A1

  • Semiconductor device and method of fabricating the same

    US20130207183A1