Machine and method

The machine's extended press section and hard-coating device combination address energy and strength challenges in fibrous web production, achieving efficient dewatering and starch penetration for reduced energy use and enhanced web strength.

WO2024200074A1PCT designated stage expired Publication Date: 2024-10-03VOITH PATENT GMBH
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/057157
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-18
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Existing machines for producing fibrous webs face challenges in achieving high dry content without excessive energy consumption and CO2 footprint, while maintaining web strength, due to limitations in press load and starch penetration issues.

Method used

A machine with an extended press section featuring a shoe press with a line load ratio of 0.56 to 1.52 and a coating device with hard rollers (over 55 ShoreD hardness) to enhance dewatering and starch penetration, respectively, allowing for increased dry content and strength with reduced energy use.

Benefits of technology

The solution enables efficient dewatering and strengthening of fibrous webs, particularly in packaging paper production, by optimizing the press section's pressure gradient and coating process, thereby reducing energy costs and environmental impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024057157_03102024_PF_FP_ABST
    Figure EP2024057157_03102024_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a machine for producing or processing a fibrous web, comprising: a press section for pressing the fibrous web, the press section comprising at least one main press which has an extended press nip with a length of at least 100 mm; a coating device for applying a coating medium to at least one side, in particular both sides, of the fibrous web, the coating device comprising an application roller and a counter roller which together form a transfer gap for the transfer of the coating medium from the application roller to the fibrous web, and the coating device being downstream of the press section in the direction of travel of the fibrous web; characterized in that the surface of the application roller and the surface of the counter roller have a hardness of more than 55 Shore D and in that the main press is designed such that a line load ratio LLR of at least 0.56 and at most 1.52 results, wherein the line load ratio LLR is the quotient of a weighted line load WLL and the line load LL, wherein the weighted line load WLL is the result of an integration of the squared local pressure p(x)2 weighted with a weighting factor over the press nip length x, wherein the weighting factor A is 1 / 10 MPa, and wherein the line load LL is the result of an integration of the local pressure p(x) over the press nip length x, so that the following formula results for the line load ratio LLR: (I).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Machine and process

[0002] The invention relates to a machine for producing or processing a fibrous web according to the preamble of claim 1 and to a method using such a machine.

[0003] Machines for producing a fibrous web usually have a press section in which the fibrous web is dewatered or dehumidified using mechanical pressure. The press section is usually located between the forming and drying sections. A particularly efficient type of mechanical dewatering can be achieved using a so-called extended press nip. The advantages of an extended press nip are well known: The press nip is planar and not essentially linear like in conventional roller presses. This means that the pressure exerted on the fibrous web to be dewatered in the press nip in the running direction does not set in suddenly, but can be increased continuously from a low value to a high value. This reduces the risk of the fibrous web to be dewatered being crushed in the press nip.In this way, the fibrous web can be dewatered very efficiently in an extended press nip while preserving its volume. Such a press section is described, for example, in WO2017207475A1.

[0004] Particularly in cardboard applications, but also in flexible packaging, the strength properties of the fiber web are also of primary importance. To increase strength, it is known to apply a starch solution to the fiber web. This can be achieved, for example, using a film press or a size press. Suitable coating devices are described, for example, in DE102008054948 A1 or WO21104742 A1.

[0005] The topics of "energy costs" and "carbon footprint" are playing an increasingly important role in the production of fiber webs. Energy consumption in the dryer section, which is currently almost exclusively steam or gas heated, is a particularly significant factor, as the energy required for this comes largely from fossil fuels such as gas. To save energy and gas here, it would be highly advantageous if the fiber web emerging from the upstream press arrangement already had the highest possible dry content.

[0006] One approach would therefore be to increase the press load, thereby increasing the dry content after the press section. However, this leads to a number of problems. Excessive pressing severely compresses and densifies the fiber web, which, among other things, makes it difficult for the starch to penetrate the downstream coating device.

[0007] In addition, it is technically almost impossible to significantly increase the press load in many existing plants, as the frame of the press section, for example, is not designed for this and would have to be massively reinforced if necessary.

[0008] The object of the invention is to propose a machine that overcomes the problems of the prior art. Furthermore, the object of the invention is to propose a method for the production of packaging paper webs in particular that enables sufficient web strength while reducing energy costs and a reduced CO2 footprint.

[0009] The object is achieved according to the invention by an embodiment according to the independent claims. Further advantageous embodiments of the present invention can be found in the subclaims.

[0010] With regard to the machine, the object is achieved by a machine for producing or processing a fibrous web, in particular a paper, packaging, or cardboard web, comprising a press section for pressing the fibrous web, wherein the press section comprises at least one main press having an extended press nip with a length of at least 100 mm. If the extended press nip is provided by a shoe press, the counter roll to the shoe preferably also has a diameter of less than 3,000 mm.Furthermore, the machine comprises a coating device for applying a coating medium to at least one, in particular both sides of the fibrous web, wherein the coating device comprises an application roller and a counter roller, which together form a transfer gap for the transfer of the coating medium from the application roller to the fibrous web, wherein the coating device is arranged after the press section, viewed in the running direction of the fibrous web.

[0011] According to the invention, it is provided that the surface of the application roller and the counter roller have a hardness of more than 55 ShoreD, in particular more than 60 ShoreD, preferably more than 80 ShoreD, and that the main press is designed such that a line load ratio LLR of at least 0.56, preferably at least 0.69 and at most 1.52, preferably at most 1.33 results, wherein the line load ratio LLR is the quotient of a weighted line load WLL to the line load LL.

[0012] The weighted line load WLL is defined as the result of an integration of the quadratic local pressure p(x) weighted with a weighting factor A 2 over the press gap length x, where the weighting factor A is one divided by ten megapascals

[0013] The line load LL is the result of an integration of the local pressure p(x) over the press gap length x

[0014] LL-. = p(x)dx so that the following formula results for the line load ratio LLR: The LLR is a dimensionless number.

[0015] While the line load LL is determined by simply taking the integral over the pressure curve in the press nip, the WLL is determined by squaring. The parameter A = 1 / 10 [1 / MPa] is chosen so that the pressure range below 10 MPa is given less weight, while the pressure range above 10 MPa is given greater weight in the WLL calculation. For a better understanding, please refer to the diagram in Figure 3, which schematically illustrates how the line load ratio LLR can be easily determined and understood. First, the actual pressure profile p(x) is determined, i.e. the pressure curve acting over the length x of the extended press nip of the main press. In the present example, the main press has an extended press nip of 260 mm.Furthermore, for the sake of simplicity, it is assumed that the local pressure p(x) increases linearly along the extended press nip from 0 MPa at the beginning of the extended press nip at x=0 mm to 12 MPa at the end of the extended press nip at x=260 mm, so that the pressure profile p(x) is a straight line. The local pressures, which together result in the pressure profile, can be determined, for example, using a pressure film that is inserted into the extended press nip before pressure is applied to it by the main press. The pressure film then measures, e.g. using the piezo effect, exactly where which local pressure is applied in the press nip. The pressure in the cross-machine direction is usually constant, so that only the pressure profile in the machine direction, i.e. along the length of the extended press nip, is important.At most, a slight change in the print in the cross-machine direction may occur in the page margin area, although these effects in the page margin area will be disregarded here. Such printing films with various resolutions are commercially available, for example, from Fujifilm under the brand name "Prescale." Measurements should preferably be taken before the press starts up, after installing a fresh felt, especially a fresh and still dry felt, which serves to guide the fiber web through the extended press nip. Measurements should preferably be taken at the press's maximum operating line load.

[0016] If the pressure profile p(x) is integrated over the length of the extended press nip x, the result is the line load LL. In the present example according to Figure 3, the line load LL corresponds to the triangular area under the straight line that represents the pressure profile p(x). Here it is 1,560 kN / m. In this way, the quality of the measurement taken can be checked very easily, namely by comparing the line load LL determined by integration with the value previously set as the line load LL of the main press. Basically, it should be noted at this point that the line load LL indicates the total force that the main press exerts per meter of width in the cross-machine direction or orthogonal to the direction of movement of the fibrous web.

[0017] Based on the measured pressure profile p(x), the curve of the weighted quadratic local pressure can now be easily determined using the following formula: io MPa * P 2This results in the curved curve shown in Figure 3, which intersects the straight line of the pressure profile p(x) at 10 MPa. The area below this curved curve corresponds to the weighted line load WLL. The graph in Figure 3 clearly shows that local pressures of less than 10 MPa lead to a smaller area and pressures of more than 10 MPa lead to an enlarged area compared to the triangular area, which represents the line load LL. In the present example, the weighted line load WLL is 1,250 kN / m. This results in a line load ratio LLR as the quotient of the weighted line load WLL to the line load LL of 0.8, which is within the scope of the claimed invention, namely in the range:

[0018] WLL

[0019] 0.56 < 1.52

[0020] LL In practice, the pressure profile curve p(x) obviously doesn't have to be a straight line. Instead, there is a virtually inexhaustible variety of possible pressure profile curves p(x), even if the line load LL, i.e., the area under the curve, remains constant. The shape of the pressure profile curve p(x) depends significantly on the geometric design of the press elements that form the extended press nip between them, in particular on the geometric design of any press shoe when using a shoe press.

[0021] Until now, only the linear load (LL) was used to characterize the pressure distribution in an extended press nip. However, the inventors recognized that this parameter alone is not sufficient to accurately characterize the pressure distribution and thus also the dewatering behavior in the press nip.

[0022] Since integration involves a certain averaging, a constant pressure curve of p=10 MPa over the entire length of the press nip, for example, yields the same line load as a pressure curve of p=0 MPa in the first half and p=20 MPa in the second half of the shoe length. However, the effect of these two pressure curves on dewatering and on the sheet structure is very different.

[0023] This difference is made visible by the weighting in the WLL. Thus, for the first case (p=10 MPa), WLL = LL, or an LLR = 1, and for the second case, WLL = 1.5 LL, or an LLR = 1.5.

[0024] The ratio therefore allows pressure profiles with the same line load to be easily and efficiently differentiated from one another in terms of their effect, without having to analyze the pressure curve in detail. Generally, for the same line load, pressure profiles with strong pressure fluctuations and higher peak pressures tend to produce larger LLR values ​​than balanced profiles with moderate pressure values.

[0025] The shape of the pressure profile curve p(x) depends significantly on the geometric design of the press elements that form the extended press gap between them, in particular on the geometric design of any press shoe when using a shoe press.

[0026] The line load ratio LLR thus indirectly describes the geometric design of the press elements, in particular of any press shoe. Since there is an incalculably large number of different geometric designs, all of which result in a line load ratio LLR between 0.56 and 1.52, the choice of the line load ratio LLR is appropriate here to describe the inventive solution. It is important that the line load ratio LLR can be determined simply and unambiguously for a press arrangement with a fixed design of the press elements. It is also within the skill of the person skilled in the art, with knowledge of the present invention, to design the press elements such that the desired line load ratio LLR is achieved.

[0027] It is the merit of the inventors to have discovered that particularly efficient dewatering of the fibrous web can be achieved if the line load ratio LLR is at least 0.56 and at most 1.52, in particular 0.69 to 1.33.

[0028] The specified parameter range can also be considered optimal because, while the increased dewatering and thus the higher dry content after pressing are accompanied by a certain degree of compaction and densification of the fibrous web, the sheet structure is still capable of being effectively coated in a suitable coating device, e.g., with a starch solution.

[0029] However, the coating device must meet certain requirements for this. To ensure that sufficient starch still penetrates deep into the sheet structure despite the higher compression of the sheet, the coating device according to aspects of the invention has a so-called "hard" transfer nip. This transfer nip is formed by an applicator roller and a counter roller, wherein the surface of the applicator roller and the counter roller have a hardness of more than 55 ShoreD, in particular more than 60 ShoreD, preferably more than 80 ShoreD. Very high hardness values ​​of 90 ShoreD or 95 ShoreD are also possible. If the coating medium is applied to both sides, each of the rollers assumes the function of both the applicator roller and the counter roller.

[0030] This allows a sufficiently deep penetration of the starch into the leaf structure, especially during application.

[0031] This is particularly relevant for penetration-driven strengths such as the flat crush resistance (“Corrugated Medium Test”, CMT) according to DIN EN ISO 7263, SCT, the strip crush test (SCT test) according to ISO 9895, DIN 54518 or TAPPI T 826 and the S-test.

[0032] Although the increased compression of the sheet in the press makes penetration more difficult, it can prove advantageous if the hard transfer nip succeeds in bringing the starch into the core of the sheet structure. This is because the increased compression of the web increases the proportion of fiber-to-fiber intersections (fibers are brought closer together by compressing the sheet structure). The strength-enhancing starch acts as a kind of adhesive, particularly at these intersections, thus stabilizing the overall fiber-based structure of the sheet. A higher proportion of fiber-to-fiber intersections also increases starch efficiency, as the probability of reinforcing one of these intersections increases with the same amount of starch applied.

[0033] Thus, the inventive combination of pressure profile in the press nip (described by the LLR value) with a hard transfer nip in the coating device provides both resource savings due to the higher dry content after the press section and the possibility of increasing the strength or efficiency of the coating medium used.

[0034] The line load ratio can advantageously be between 0.71 and 1.35, particularly preferably between 0.73 and 1.14. Especially when retrofitting existing systems, which are limited by the existing frame, press design, or existing hydraulics, line load ratios between 0.61 and a maximum of 1.01, preferably at least 0.66 and a maximum of 0.89, can also deliver advantageous results.

[0035] In addition, the machine can further comprise a pre-press positioned upstream of the main press in the direction of travel of the fibrous web, preferably immediately upstream, wherein the pre-press in particular has an extended press nip with a length of at least 100 mm. Tandem presses of this type are known per se. Both in a new system and, especially, during a rebuild, such a second press can be very advantageous for achieving a high dry content after the press section.

[0036] A longer press nip length generally allows for greater flexibility in the design of the pressure profile, and thus, within the scope of aspects of the present invention, also greater freedom in adjusting the LLR. Thus, it is advantageous if the press nip of the main press and / or the press nip of the pre-press has a length of at least 150 mm, in particular at least 190 mm.

[0037] To achieve the length of the press nip and also to adjust the pressure profile, it is very advantageous if the main press and / or the pre-press is a shoe press, which comprises a press shoe with a substantially concavely curved surface and a shoe press sleeve rotatably mounted around the press shoe. Such shoe presses are known per se to those skilled in the art.

[0038] In the coating device, it is advantageous for at least one roller (the transfer roller or the counter roller) to be designed as a deflection-adjusting roller. This is important, for example, to ensure a defined transfer gap, since the hard rollers can hardly compensate for irregularities through deformation. A machine according to aspects of the presented invention can be used very advantageously for the production or processing of a fibrous web.

[0039] It is particularly preferred for use in the production of packaging papers such as testliner, kraftliner or other corrugated board base papers.

[0040] The particularly preferred embodiment of the process comprises the use of a starch solution as the coating medium.

[0041] In preferred embodiments, it can be provided that the peak pressure in the press nip of the main press is at least 8 MPa, preferably at least 10 MPa, particularly preferably between 12 MPa and 20 MPa.

[0042] The higher peak pressure is generally beneficial for greater dewatering. However, especially in existing systems, excessive peak pressure can overload the existing press components. Furthermore, as described above, high peak pressure tends to lead to higher LLR values. Therefore, there is a risk that excessive peak pressure will exceed the LLR range. Therefore, it may also be beneficial to keep the peak pressure below 20 MPa, possibly even below 18 MPa.

[0043] The line load in the press nip of the main press can be at least 500 kN / m, preferably at least 1000 kN / m, particularly preferably over 1300 kN / m.

[0044] To ensure the transfer of the coating medium through the hard transfer gap and the penetration of the coating medium into the fibrous web, a nip load of at least 60 kN / m in the transfer gap is advantageous. Preferably, the coating device can also be operated with higher loads, in particular 70 kN / m or more.

[0045] The parameters of the coating medium, especially a starch solution, can further positively influence the penetration of the medium into the fibrous web. For example, the viscosity of the coating medium, especially the starch solution, can be selected to be less than 80 mPas, especially less than 60 mPas.

[0046] When viscosity is mentioned in this application, unless explicitly stated otherwise, this means the Brookfield viscosity measured at 50°C and 100 rpm.

[0047] Furthermore, the temperature of the coating medium during application to the transfer roller may be at least 50°C. Higher temperatures such as 60°C, 70°C, and more are also possible.

[0048] In addition, it may be advantageous if the solids content of the coating medium is below 20 wt%, in particular below 15 wt%.

[0049] The advantages of the invention are particularly evident in the case of fibers with a high content of recycled paper, particularly when at least 20% by weight, in particular 50% by weight, in particular at least 80% by weight of the fiber is obtained from recycled paper for the production of the fibrous web. In particular, this can be OCC-

[0050] Fibers are made from used packaging material 25 ("OCC_ Old Corrugated Containerboard"), which are characterized by particularly high resistance, even to high peak pressures. These materials are, on the one hand, more difficult to process, meaning they require greater effort and / or

[0051] Pressure dewatering is easier than virgin fiber-based materials. On the other hand, the strength potential of recycled fibers is lower than that of virgin fibers due to multiple passages through stock preparation and a paper machine.

[0052] A machine or method according to aspects of the invention can increase dewatering in the press and simultaneously increase the strength of the final product. This proves particularly advantageous for corrugated board base papers that are largely or exclusively made from recycled fibers.

[0053] In advantageous embodiments, it can be provided that the moisture content and / or the moisture cross-section of the fibrous web is determined after the main press, and the nip load or nip profile of the coating device is controlled or regulated based on these values. For this purpose, it is particularly advantageous if one of the rollers of the coating device is designed as a deflection-adjustment roller.

[0054] The invention is explained below with reference to figures. The invention is not limited to the embodiments shown in the figures. The figures show in detail:

[0055] Figure 1: a press section comprising a main press and a pre-press according to one aspect of the invention;

[0056] Figure 2: an enlarged and detailed view of the main press of the

[0057] Press arrangement shown in Figure 1,

[0058] Figure 3: an example pressure curve in the extended press nip of the

[0059] main press,

[0060] Figure 4 shows a coating device according to a further aspect of the invention.

[0061] Figure 1 shows a very schematic view of a press section comprising a main press 1 and a pre-press 11 arranged directly upstream in the direction of movement BR of a fibrous web 8. In this exemplary embodiment, both the main press 1 and the pre-press 11 are designed as shoe presses and thus each have an extended press nip 7. Alternatively, however, the pre-press 11 could not have an extended press nip 7 and / or the pre-press 11 and the main press 1 could share a common central roller. The central roller would then be a press element by means of which both the extended press nip of the pre-press 11 and the extended press nip 7 of the main press 1 would be formed.

[0062] Figure 2 shows an enlarged and detailed illustration of the main press 1, which is of particular importance according to the invention. This press is designed to be operated with a line load LL of at least 500 kN / m, for example 1,200 kN / m. The extended press nip 7 of the main press 1 is provided by two press elements, namely a shoe press roll 2 and a counter roll 3. The shoe press roll 2 comprises a press shoe 5, which is supported on a stationary yoke 4, and a shoe press sleeve 6, which is arranged so as to be rotatable around the press shoe 5. The fibrous web 8 is preferably guided through the extended press nip 7 in a sandwich-like manner between two press felts 9. The press shoe 5 has a substantially concavely shaped surface over which the shoe press sleeve 6 runs, while the press shoe 5 presses it with a high compressive force F in the direction of the counter roll (press) 3.The geometric design of the pressing elements, in particular of the press shoe 5, is selected in such a way that, for example, a line load ratio LLR of at least 0.56 and at most 1.52 results.

[0063] The compressive force F is preferably selected to be large enough that the peak pressure acting on the fibrous web 8 in the extended press nip 7 is at least 8 MPa. The length of the extended press nip 7 of the main press 1 is at least 150 mm, preferably at least 190 mm.

[0064] At such peak pressures, it has proven particularly advantageous if the shoe press cover 6 consists at least partially of polyurethane, which is formed by reacting a prepolymer and a crosslinking component, wherein the prepolymer is a reaction product of 1,4-phenylene diisocyanate (PPDI) and a polyol component containing at least one polyether polyol and / or at least one polycarbonate polyol, and wherein the crosslinking component contains a C2-14 diol. For example, the shoe press cover 6 can have a reinforcing structure made of threads embedded in the polyurethane layer, wherein the prepolymer of the polyurethane layer consists of 50 wt. % of a mixture of 1,4-phenylene diisocyanate (PPDI) and C5-6 polycarbonate diol and 50 wt.-% of a mixture of 1,4-phenylene diisocyanate (PPDI) and polytetramethylene ether glycol (PTMEG), and wherein the crosslinker comprises polytetramethylene ether glycol (PTMEG) and 1,6-hexanediol or is preferably formed substantially therefrom. The pre-press 11 shown schematically in Figure 1 can and is preferably designed differently than the main press 1. In particular, unlike the main press 1, it can be designed such that the line load ratio LLR of the pre-press 11 is less than 0.56, preferably less than 0.52. The pre-press 11 serves in the press arrangement in particular to sufficiently pre-consolidate the fibrous web 8 for passage through the main press 1 so that it is not compressed to an unacceptable extent despite a relatively high peak pressure in the second press 1.

[0065] The fibrous web 8 preferably serves for the production of a packaging paper web or is such a packaging paper web. Furthermore, the fibrous web can consist of at least 20 wt.% or 30 wt.%, preferably at least 50 wt.%, of OCC fibers, which are characterized by particularly high resistance even to high peak pressures.

[0066] The press arrangement 1 according to the invention could theoretically also comprise more presses than just the pre-press 11 and the main press 1. However, the main press 1 is preferably the last press of the press arrangement, ie, the last press before the fibrous web 8 is transferred to a drying section downstream of the press arrangement.

[0067] Figure 4 shows a coating device for use in a machine according to aspects of the invention. Specifically, Figure 4 shows a first roll 21 and a second roll 22 forming a transfer nip 23. The fibrous web 8, which may be, for example, a testliner (TL) or corrugated board (CM) web, passes through the transfer nip 23.

[0068] Starch is applied to the surface of the rollers 21, 22 through two nozzles 25 and transferred from there to the web 8 in the gap. The nozzles 25 can be, for example, curtain application nozzles 25, spray nozzles 25, or other suitable application units. Since the starch is applied to both sides in Fig. 4, each of the rollers 21, 22 assumes the function of both the application roller and the counter roller (coating device).

[0069] In order to achieve a better transfer of the starch to the web 8, the rollers 21, 22 have a hardness of more than 55 ShoreD, in particular more than 60 ShoreD, preferably more than 80 ShoreD.

[0070] The diameter of the two rollers 21, 22 is chosen to be the same in the example of Fig. 4, for example in the range between 0.7 m and 1.8 m, but can be larger or smaller depending on the application.

[0071] The starch used can, for example, have a solids content between 6% and 20%, preferably between 8% and 18%.

[0072] In addition, a viscosity of between 5 mPas and 80 mPas, preferably between 10 mPas and 60 mPas, can be selected for the starch. The starch temperature during application to rollers 21 and 22 can be 50°C or more.

[0073] The transfer gap 23 can advantageously be operated with a nip load of more than 60 kN / m, in particular more than 70 kN / m.

[0074] List of reference symbols

[0075] 1 main press

[0076] 2 shoe press rollers

[0077] 3 Counter roller (press)

[0078] 4 standing yoke

[0079] 5 press shoe

[0080] 6 Shoe press cover

[0081] 7 extended press nip

[0082] 8 Fibrous web

[0083] 9 Press felt

[0084] 10 Press arrangement

[0085] 11 Pre-press

[0086] 21 Application roller, counter roller (coating device)

[0087] 22 Application roller, counter roller (coating device)

[0088] 23 Transfer gap

[0089] 25 application nozzle

[0090] BR direction of movement

[0091] F compressive force

Claims

Patent claims 1.) Machine for producing or processing a fibrous web (8), in particular a paper, packaging or cardboard web (8), comprising a press section for pressing the fibrous web, wherein the press section comprises at least one main press (1) having an extended press nip (7) with a length of at least 100 mm, further comprising a coating device for applying a coating medium to at least one, in particular both sides of the fibrous web (8), wherein the coating device comprises an applicator roll (21, 22) and a counter roll (21, 22), which together form a transfer nip (23) for transferring the coating medium from the applicator roll (21, 22) to the fibrous web (8), wherein the coating device is arranged after the press section as viewed in the running direction (BR) of the fibrous web (8), characterized in that the surface of the applicator roll (21, 22) and the counter roll (21,22) have a hardness of more than 55 ShoreD, in particular more than 60 ShoreD, preferably more than 80 ShoreD, and that the main press (1) is designed in such a way that a line load ratio LLR of at least 0.56, preferably at least 0.69 and at most 1.52, preferably at most 1.33 results, wherein the line load ratio LLR is the quotient of a weighted line load WLL to the line load LL, wherein the weighted line load WLL is the result of an integration of the quadratic local pressure p(x) weighted with a weighting factor A, 2 over the press gap length x, where the weighting factor A is one divided by ten megapascals, and where the line load LL is the result of an integration of the local pressure p(x) over the press gap length x, so that the line load ratio LLR is given by the following formula: Machine according to claim 1, characterized in that the Line load ratio LLR is at least 0.71 and at most 1.35, preferably at least 0.73 and at most 1.

14. Machine according to one of the preceding claims, characterized in that the machine further comprises a pre-press (11) arranged upstream of the main press (1) in the running direction (BR) of the fibrous web (8), preferably immediately upstream, wherein the pre-press (11) has in particular an extended press nip (7) with a length of at least 100 mm. Machine according to claim 3, characterized in that the Line load ratio LLR of the pre-press (11) is less than 0.56, preferably less than 0.

52. Machine according to one of the preceding claims, characterized in that the main press (1) and / or the pre-press (11) is a shoe press, which comprises a press shoe (5) with a substantially concavely curved surface and a shoe press cover (6) rotatably mounted around the press shoe (5). Method for producing or processing a fibrous web (8) using a machine according to one of the preceding claims 1 to 5 and 15, wherein in particular a starch solution is used as the coating medium. Method according to claim 6, characterized in that the Peak pressure in the extended press nip (7) of the main press (1 ) at least 8 MPa, preferably at least 10 MPa, particularly preferably between 12 MPa and 20 MPa. Method according to one of claims 6 or 7, characterized in that the line load in the extended press nip (7) of the main press (1) is at least 500 kN / m, preferably at least 1000 kN / m, particularly preferably more than 1300 kN / m. Method according to one of claims 6 to 8, characterized in that the transfer nip (23) is operated with a nip load of more than 60 kN / m, in particular more than 70 kN / m. Method according to one of claims 6 to 9, characterized in that the viscosity of the coating medium is selected to be less than 80 mPas, in particular less than 60 mPas. Method according to one of claims 6 to 10, characterized in that the temperature of the coating medium during application to the transfer roller (21, 22) is at least 50°C.Method according to one of claims 6 to 11, characterized in that the solids content of the coating medium is below 20 wt%, in particular below 15 wt%. Method according to one of claims 6 to 12, characterized in that for producing the fibrous web (8), at least 20 wt%, preferably at least 50 wt%, in particular at least 80 wt% of the fiber is obtained from waste paper. Method according to one of claims 6 to 13, characterized in that the moisture content and / or the moisture cross-section of the fibrous web (8) is determined downstream of the main press (1). and the nip load or the nip profile of the coating device is controlled or regulated on the basis of these values. Machine according to one of claims 1 to 6, characterized in that at least the application roller (21, 22) and / or the counter roller (21, 22) is designed as a bending adjustment roller.

Citation Information

Patent Citations

  • Device for coating a fluid to pasty coating medium such as glue, starch or coating color on a side of a running paper, cardboard or other fiber material web, comprises two rotatable transfer elements or rotatable endless bands

    DE102008054948A1

  • Machine for dewatering and drying a fibrous web

    WO2017207475A1

  • Coating pulp webs

    WO2021104742A1

  • Coating of fiber webs

    DE202019005628U1

  • Dewatering and drying press especially for tissue and hygiene papers - includes two shoe press units, in the first of which an increase in nip pressure takes place over the first third or two thirds of the nip length.

    DE29624464U1