Light emitting element, display device, light emitting element manufacturing method, and method for restoring light emitting characteristics of light emitting element

The use of a metal halide matrix with a specific electronegativity difference in quantum dot light-emitting devices addresses efficiency and leakage issues, and a restoration method through melting and recrystallization improves reliability and efficiency.

WO2024201569A1PCT designated stage expired Publication Date: 2024-10-03SHARP DISPLAY TECHNOLOGY CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/011829
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

The existing light-emitting devices with quantum dots face challenges in maintaining luminous efficiency due to defects in the matrix formed at low temperatures and deterioration at high temperatures, leading to non-luminescent leakage and reduced light-emitting layer characteristics.

Method used

A light-emitting device with a matrix composed of a metal halide having an electronegativity difference of 0.7 or more between the metal and halogen elements, which is formed at a relatively low temperature to minimize defects and maintain efficiency, and a method for restoring light-emitting characteristics by melting and recrystallizing the metal halide in the light-emitting layer.

Benefits of technology

The solution achieves good luminous efficiency and suppresses non-luminescent leakage, while the restoration method improves the long-term reliability of the light-emitting device by enhancing the crystallinity and reducing defects in the metal halide matrix.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023011829_03102024_PF_FP_ABST
    Figure JP2023011829_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A red light emitting element (5R) is provided with an anode (22), a cathode (25), and a red light emitting layer (24REM) provided between the anode (22) and the cathode (25). The red light emitting layer (24REM) includes a plurality of quantum dots (QD) and a matrix (MR) that contains a metal halide (MHa) which comprises a metal element and a halogen element, the metal element being provided at least partially between the plurality of quantum dots (QD) and having an electronegativity difference of 0.7 or greater.
Need to check novelty before this filing date? Find Prior Art

Description

Light-emitting device, display device, method for manufacturing light-emitting device, and method for recovering light-emitting characteristics of light-emitting device

[0001] The present disclosure relates to a light-emitting element, a display device, a method for manufacturing a light-emitting element, and a method for restoring the light-emitting characteristics of a light-emitting element.

[0002] In recent years, quantum dot light-emitting diodes (QLEDs), which are light-emitting elements containing quantum dots, and display devices equipped with QLEDs have been attracting a great deal of attention because of their ability to achieve low power consumption, thinness, high image quality, and the like.

[0003] For example, Patent Document 1 describes nanocrystalline particles containing fluorine, that is, quantum dots containing fluorine in at least a part of the core and shell.

[0004] Japanese Patent Publication "JP 2015-147726"

[0005] It is known that in a light-emitting layer containing a plurality of quantum dots, the characteristics of the light-emitting layer are degraded due to the influence of the spaces existing between the quantum dots.

[0006] Therefore, it is conceivable that the deterioration of the characteristics of the light-emitting layer can be suppressed by using a matrix that fills at least a part of the space that exists between each of the plurality of quantum dots in the light-emitting layer.

[0007] However, the inventors of the present disclosure have found that the following problems occur in the case of a matrix made of a compound containing an element that is not strongly ionic.

[0008] If a matrix composed of a compound containing an element that is not strongly ionic and is contained in the light-emitting layer is formed using a relatively low-temperature process in order to maintain good luminous efficiency of the quantum dots contained in the light-emitting layer, the matrix will contain many defects that can become paths for non-radiative recombination, resulting in the problem that non-radiative leakage in the light-emitting layer cannot be suppressed.

[0009] On the other hand, if a matrix composed of a compound containing an element with low ionicity contained in the light-emitting layer is formed at a relatively high temperature in order to reduce the numerous defects mentioned above, there is a problem that the light-emitting efficiency may not be maintained at a good level due to deterioration of the quantum dots contained in the light-emitting layer.

[0010] Patent Document 1 describes that at least a part of the core and shell of a quantum dot contains fluorine present in the form of, for example, metal fluoride. In the case of the quantum dots containing fluorine described in Patent Document 1, improvement in the properties of the quantum dots themselves can be expected, but there is a problem in that deterioration in the properties of the light-emitting layer due to the influence of spaces existing between the multiple quantum dots is unavoidable.

[0011] One aspect of the present disclosure has been made in consideration of the above-mentioned problems, and aims to provide a light-emitting element having a light-emitting layer that has good light-emitting efficiency and good suppression of non-light-emitting leakage, a method for manufacturing the light-emitting element, a display device including the light-emitting element, and a method for restoring the light-emitting characteristics of the light-emitting element, which restores the light-emitting characteristics (light-emitting efficiency) of the light-emitting element.

[0012] In order to solve the above-mentioned problems, the light-emitting element of the present disclosure comprises an anode, a cathode, and a light-emitting layer provided between the anode and the cathode, wherein the light-emitting layer includes a plurality of quantum dots and a matrix containing a metal halide composed of a metal element and a halogen element, the difference in electronegativity between which is 0.7 or more, provided at least partially between the plurality of quantum dots.

[0013] In order to solve the above-mentioned problems, the display device of the present disclosure includes the light-emitting element.

[0014] In order to solve the above-mentioned problems, the method for manufacturing a light-emitting element according to the present disclosure includes a step of forming a light-emitting layer including a plurality of quantum dots and a matrix containing a metal halide composed of a metal element and a halogen element, the difference in electronegativity between which is 0.7 or more, provided at least in part between the plurality of quantum dots.

[0015] In order to solve the above-mentioned problems, the method for recovering the light-emitting characteristics of a light-emitting element disclosed herein includes a step of melting the metal halide contained in the light-emitting layer of a light-emitting element manufactured by the method for manufacturing a light-emitting element.

[0016] According to one aspect of the present disclosure, it is possible to provide a light-emitting element having a light-emitting layer that has good light-emitting efficiency and good suppression of non-light-emitting leakage, a method for manufacturing a light-emitting element, a display device including the light-emitting element, and a method for restoring the light-emitting characteristics of a light-emitting element that restores the light-emitting characteristics (light-emitting efficiency) of the light-emitting element.

[0017] 9 is a plan view showing a schematic configuration of a display device of Embodiment 1. FIG. 10 is a cross-sectional view showing a schematic configuration of a display region of a display panel included in the display device of Embodiment 1. FIG. 11 is a cross-sectional view showing a schematic configuration of a light-emitting device included in the display device of Embodiment 1. FIG. 12 is a view for explaining a region formed between quantum dots when two adjacent quantum dots among a plurality of quantum dots included in a light-emitting layer included in the light-emitting device shown in FIG. 3 are arranged close to each other. FIG. 13 is a view for explaining a region formed between quantum dots when two adjacent quantum dots among a plurality of quantum dots included in a light-emitting layer included in the light-emitting device shown in FIG. 3 are arranged slightly apart from each other. FIG. 14 is a view schematically showing band levels of a hole transport layer, an electron transport layer, cores of quantum dots included in the light-emitting layer, shells of quantum dots included in the light-emitting layer, and a matrix containing a metal halide included in the light-emitting layer, which are included in the light-emitting device shown in FIG. 3. FIG. 15 is a view showing an example of a process for forming a light-emitting layer included in the light-emitting device shown in FIG. 7. FIG. 16 is a view for explaining a process for forming the light-emitting layer shown in FIG. 7. FIG. 17 is a view showing another example of a process for forming a light-emitting layer included in the light-emitting device shown in FIG. 3. FIG. 18 is a view for explaining a process for forming the light-emitting layer shown in FIG. 13 is a diagram showing an example of a material that can be used as the metal halide contained in the light-emitting layer of the light-emitting element of each color provided in the display device of embodiment 1. FIG. 14 is a cross-sectional view showing a schematic configuration of a light-emitting element provided in the display device of embodiment 2. FIG. 15 is a diagram showing a schematic band level of a hole transport layer containing a metal halide, an electron transport layer, cores of quantum dots included in the light-emitting layer, shells of quantum dots included in the light-emitting layer, and a matrix containing a metal halide included in the light-emitting layer, which are provided in the light-emitting element shown in FIG. 12. FIG. 16 is a cross-sectional view showing a schematic configuration of a light-emitting element provided in the display device of embodiment 3. FIG. 17 is a diagram showing a schematic band level of a hole transport layer, an electron transport layer, an electron blocking layer containing a metal halide, cores of quantum dots included in the light-emitting layer, shells of quantum dots included in the light-emitting layer, and a matrix containing a metal halide included in the light-emitting layer, which are provided in the light-emitting element shown in FIG. 15. FIG. 18 is a plan view showing a schematic configuration of a display device of embodiment 4. FIG. 19 is a diagram showing a heating unit provided in the display device of embodiment 4 shown in FIG.

[0018] The following describes embodiments of the present disclosure with reference to Figures 1 to 17. For the sake of convenience, components having the same functions as those described in specific embodiments will be denoted by the same reference numerals, and descriptions thereof may be omitted.

[0019] First Embodiment FIG. 1 is a plan view showing a schematic configuration of a display device 1 according to a first embodiment.

[0020] As shown in FIG. 1 , the display device 1 includes a display panel 30, which includes a frame region NDA and a display region DA. The display region DA of the display panel 30 includes a plurality of pixels PIX, each of which includes a red subpixel RSUB, a green subpixel GSUB, and a blue subpixel BSUB. In this embodiment, a case where one pixel PIX is composed of a red subpixel RSUB, a green subpixel GSUB, and a blue subpixel BSUB is described as an example, but this is not limiting. For example, one pixel PIX may include subpixels of other colors in addition to the red subpixel RSUB, the green subpixel GSUB, and the blue subpixel BSUB. In addition, in this embodiment, an example is given in which a scanning side driving circuit 31 and a data side driving circuit 32 are provided in the frame area NDA of the display panel 30, but this is not limited to this, and at least one of the scanning side driving circuit 31 and the data side driving circuit 32 may be external to the display panel 30.

[0021] FIG. 2 is a cross-sectional view showing a schematic configuration of a display area DA of the display panel 30 provided in the display device 1 of the first embodiment.

[0022] As shown in Figure 2, in the display area DA of the display panel 30 provided in the display device 1, a barrier layer 3, a thin film transistor layer 4 including a transistor TR, a red light-emitting element 5R, a green light-emitting element 5G, a blue light-emitting element 5B and a bank 23, a sealing layer 6, and a functional film 39 are provided on the substrate 12 in this order from the substrate 12 side.

[0023] The red sub-pixel RSUB provided in the display area DA of the display panel 30 includes a red light-emitting element 5R, the green sub-pixel GSUB provided in the display area DA of the display panel 30 includes a green light-emitting element 5G, and the blue sub-pixel BSUB provided in the display area DA of the display panel 30 includes a blue light-emitting element 5B.

[0024] The substrate 12 may be, for example, a resin substrate made of a resin material such as polyimide, or a glass substrate. In this embodiment, since the display device 1 is a flexible display device, a case where a resin substrate made of a resin material such as polyimide is used as the substrate 12 will be described as an example, but this is not limiting. If the display device 1 is a non-flexible display device, a glass substrate can be used as the substrate 12.

[0025] The barrier layer 3 is a layer that prevents foreign substances such as water and oxygen from penetrating into the transistor TR, the red light-emitting element 5R, the green light-emitting element 5G, and the blue light-emitting element 5B, and can be composed of, for example, a silicon oxide film, a silicon nitride film, a silicon oxynitride film, or a laminated film of these, formed by the CVD method.

[0026] The transistor TR portion of the thin film transistor layer 4 including the transistor TR includes the semiconductor film SEM and doped semiconductor films SEM′ and SEM″, an inorganic insulating film 16, a gate electrode G, an inorganic insulating film 18, an inorganic insulating film 20, a source electrode S and a drain electrode D, and a planarization film 21, and the portion of the thin film transistor layer 4 including the transistor TR other than the transistor TR portion includes the inorganic insulating film 16, the inorganic insulating film 18, the inorganic insulating film 20, and the planarization film 21.

[0027] The semiconductor films SEM, SEM', and SEM'' may be made of, for example, low-temperature polysilicon (LTPS) or an oxide semiconductor (for example, an In-Ga-Zn-O based semiconductor). In this embodiment, the case where the transistor TR has a top-gate structure will be described as an example, but the present invention is not limited to this, and the transistor TR may also have a bottom-gate structure.

[0028] The gate electrode G and the source electrode S and drain electrode D can be formed of a single layer or a multilayer film of a metal containing at least one of aluminum, tungsten, molybdenum, tantalum, chromium, titanium, and copper, for example.

[0029] The inorganic insulating films 16, 18 and 20 can be formed of, for example, a silicon oxide film, a silicon nitride film, a silicon oxynitride film, or a laminated film of these films, which are formed by the CVD method.

[0030] The planarizing film 21 can be made of a coatable organic material such as polyimide or acrylic, but may also be made of an inorganic film.

[0031] The red light-emitting element 5R included in the red subpixel RSUB includes an anode 22 above the planarization film 21, a functional layer 24R including a red light-emitting layer, and a cathode 25. The green light-emitting element 5G included in the green subpixel GSUB includes an anode 22 above the planarization film 21, a functional layer 24G including a green light-emitting layer, and a cathode 25. The blue light-emitting element 5B included in the blue subpixel BSUB includes an anode 22 above the planarization film 21, a functional layer 24B including a blue light-emitting layer, and a cathode 25. The insulating bank 23 covering the edge of the anode 22 can be formed by applying an organic material such as polyimide or acrylic and then patterning it by photolithography, for example, but may also be formed from an inorganic film.

[0032] In this embodiment, the red light-emitting element 5R, the green light-emitting element 5G, and the blue light-emitting element 5B have a forward stack structure as an example. However, this is not limited thereto, and the red light-emitting element 5R, the green light-emitting element 5G, and the blue light-emitting element 5B may have an inverted stack structure. The red light-emitting element 5R (see FIG. 3 ) having a forward stack structure includes an anode 22 and a cathode 25 provided above the anode 22. The functional layer 24R including the red light-emitting layer 24REM provided between the anode 22 and the cathode 25 can be configured by stacking, for example, a hole injection layer, a hole transport layer, a red light-emitting layer, an electron transport layer, and an electron injection layer in this order from the anode 22 side. Of the functional layer 24R including the red light-emitting layer 24REM, one or more of the hole injection layer, hole transport layer, electron transport layer, and electron injection layer other than the red light-emitting layer 24REM may be omitted as appropriate. In this embodiment, a case where the functional layer 24R including the red light-emitting layer 24REM is configured by stacking a hole transport layer 24HT, a red light-emitting layer 24REM, and an electron transport layer 24ET in this order from the anode 22 side will be described as an example, but the present invention is not limited thereto. The green light-emitting element 5G having a sequential stack structure includes an anode 22 and a cathode 25 provided above the anode 22. The functional layer 24G including the green light-emitting layer provided between the anode 22 and the cathode 25 can be configured by stacking, for example, a hole injection layer, a hole transport layer, a green light-emitting layer, an electron transport layer, and an electron injection layer in this order from the anode 22 side. Of the functional layer 24G including the green light-emitting layer, one or more of the hole injection layer, hole transport layer, electron transport layer, and electron injection layer other than the green light-emitting layer may be omitted as appropriate. In this embodiment, the functional layer 24G including the green light-emitting layer is configured by laminating, in order from the anode 22 side, a hole transport layer, a green light-emitting layer, and an electron transport layer, as an example, but is not limited to this. The blue light-emitting element 5B having a sequential stack structure includes the anode 22 and the cathode 25 provided as an upper layer than the anode 22, and the functional layer 24B including the blue light-emitting layer provided between the anode 22 and the cathode 25 can be configured by laminating, for example, a hole injection layer, a hole transport layer, a blue light-emitting layer, an electron transport layer, and an electron injection layer, in order from the anode 22 side.In the functional layer 24B including the blue light-emitting layer, one or more layers other than the blue light-emitting layer, namely, the hole injection layer, the hole transport layer, the electron transport layer, and the electron injection layer, may be omitted as appropriate. In this embodiment, the functional layer 24B including the blue light-emitting layer is described by taking as an example a case where the functional layer 24B including the blue light-emitting layer is configured by stacking a hole transport layer, a blue light-emitting layer, and an electron transport layer in this order from the anode 22 side, but is not limited to this.

[0033] The red light-emitting element having an inverted stack structure (not shown) includes a cathode and an anode provided above the cathode. The functional layer including the red light-emitting layer 24REM provided between the cathode and the anode can be formed, for example, by stacking, from the cathode side, an electron injection layer, an electron transport layer, a red light-emitting layer, a hole transport layer, and a hole injection layer. Of the functional layers including the red light-emitting layer 24REM, one or more of the electron injection layer, electron transport layer, hole transport layer, and hole injection layer other than the red light-emitting layer 24REM may be omitted as appropriate. The green light-emitting element having an inverted stack structure (not shown) includes a cathode and an anode provided above the cathode. The functional layer including the green light-emitting layer provided between the cathode and the anode can be formed, for example, by stacking, from the cathode side, an electron injection layer, an electron transport layer, a green light-emitting layer, a hole transport layer, and a hole injection layer. Among the functional layers including the green light-emitting layer, one or more of the electron injection layer, electron transport layer, hole transport layer, and hole injection layer other than the green light-emitting layer may be omitted as appropriate. A blue light-emitting element having an inverted stack structure (not shown) includes a cathode and an anode provided above the cathode, and the functional layer including the blue light-emitting layer provided between the cathode and the anode can be configured by stacking, for example, an electron injection layer, an electron transport layer, a blue light-emitting layer, a hole transport layer, and a hole injection layer in this order from the cathode side. Among the functional layers including the blue light-emitting layer, one or more of the electron injection layer, electron transport layer, hole transport layer, and hole injection layer other than the blue light-emitting layer may be omitted as appropriate.

[0034] The material used for the hole injection layer is not particularly limited as long as it is a hole injection material that can stabilize the injection of holes into the light emitting layer, and for example, a composite of poly(3,4-ethylenedioxythiophene) (PEDOT) and polystyrene sulfonic acid (PSS) (PEDOT:PSS) can be used.

[0035] Examples of materials used for the hole transport layer include organic materials such as poly[(9,9-dioctylfluorenyl-2,7-diyl)-co-(4,4'-(N-(4-sec-butylphenyl))diphenylamine)] (TFB), N,N'-bis(4-butylphenyl)-N,N'-bis(phenyl)-benzidine (poly-TPD), and polyvinylcarbazole (PVK), and nanoparticles having hole transport properties, such as NiO particles.

[0036] The material used for the electron transport layer may be, for example, an organic material such as 2,2′,2″-(1,3,5-benzinetriyl)-tris(1-phenyl-1-H-benzimidazole) (TPBi), or nanoparticles having electron transport properties such as ZnO particles.

[0037] The material used for the electron injection layer is not particularly limited as long as it is an electron injection material that can stabilize the injection of electrons into the light-emitting layer. For example, alkali metals or alkaline earth metals such as aluminum, strontium, calcium, lithium, cesium, magnesium oxide, aluminum oxide, strontium oxide, lithium oxide, lithium fluoride, magnesium fluoride, strontium fluoride, calcium fluoride, barium fluoride, cesium fluoride, polymethyl methacrylate polystyrene sodium sulfonate, oxides of alkali metals or alkaline earth metals, fluorides of alkali metals or alkaline earth metals, organic complexes of alkali metals, etc. may be used.

[0038] In addition, in this embodiment, the functional layer 24R including the red light-emitting layer, the functional layer 24G including the green light-emitting layer, and the functional layer 24B including the blue light-emitting layer each include a hole transport layer formed in the same process using the same material and an electron transport layer formed in the same process using the same material, but this is not limited to this. For example, the hole injection layers included in each of the functional layers 24R, 24G, and 24B may be formed in the same process using the same material, or may be formed in different materials. Alternatively, the hole injection layers included in two of the functional layers 24R, 24G, and 24B may be formed in the same process using the same material, and only the hole injection layer included in the remaining functional layer may be formed in a separate process using a different material. For example, the hole transport layers included in each of the functional layers 24R, 24G, and 24B may be formed from different materials, or the hole transport layers included in two of the functional layers 24R, 24G, and 24B may be formed from the same material in the same process, and only the hole transport layer included in the remaining functional layer may be formed from a different material in a separate process. For example, the electron transport layers included in each of the functional layers 24R, 24G, and 24B may be formed from different materials, or the electron transport layers included in two of the functional layers 24R, 24G, and 24B may be formed from the same material in the same process, and only the electron transport layer included in the remaining functional layer may be formed from a different material in a separate process. Furthermore, the electron injection layers contained in each of the functional layers 24R, 24G, and 24B may be formed using the same material in the same process, or they may be formed using different materials. Alternatively, the electron injection layers contained in two of the functional layers 24R, 24G, and 24B may be formed using the same material in the same process, and only the electron injection layer contained in the remaining functional layer may be formed using a different material in a separate process.

[0039] In this embodiment, a case where the red light emitting element 5R, the green light emitting element 5G, and the blue light emitting element 5B are all QLEDs (quantum dot light emitting diodes) will be described as an example, but the present invention is not limited to this, and it is sufficient that one or more of the red light emitting element 5R, the green light emitting element 5G, and the blue light emitting element 5B are QLEDs. For example, if one of the red light emitting element 5R, the green light emitting element 5G, and the blue light emitting element 5B is a QLED, the remaining two may be OLEDs (organic light emitting diodes), and for example, if two of the red light emitting element 5R, the green light emitting element 5G, and the blue light emitting element 5B are QLEDs, the remaining one may be an OLED.

[0040] In the present embodiment, when the red light-emitting element 5R, the green light-emitting element 5G, and the blue light-emitting element 5B are each a QLED, the light-emitting layer of each light-emitting element contains quantum dots. The quantum dots may have, for example, a core structure, a core / shell structure, a core / shell / shell structure, or a shell structure with a continuously varying core / shell ratio. The shell may completely cover the core or may only partially cover the core. In the case of a unicomponent system, the core portion may be composed of, for example, Si or C. In the case of a binary system, the core portion may be composed of, for example, CdSe, CdS, CdTe, InP, GaP, InN, ZnSe, ZnS, ZnTe, etc. In the case of a ternary system, the core portion may be composed of, for example, CdSeTe, GaInP, ZnSeTe, etc. In the case of a quaternary system, the core portion may be composed of, for example, AIGS, etc. In the case of a binary system, the shell portion can be composed of, for example, CdS, CdTe, CdSe, ZnS, ZnSe, ZnTe, etc., and in the case of a ternary system, the shell portion can be composed of, for example, CdSSe, CdTeSe, CdSTe, ZnSSe, ZnSTe, ZnTeSe, AIP, etc.

[0041] When the quantum dots described above include organic or inorganic ligands (e.g., halogen ligands) disposed on or near the surface of the quantum dots, the quantum dots are referred to as including the organic or inorganic ligands (e.g., halogen ligands).

[0042] The quantum dots have a maximum width excluding the ligand portion of 100 nm or less. The shape of the quantum dots excluding the ligand portion is not particularly limited as long as it satisfies the maximum width, and is not limited to a spherical three-dimensional shape (circular cross-sectional shape). For example, the quantum dots may have a polygonal cross-sectional shape, a rod-like three-dimensional shape, a branch-like three-dimensional shape, a three-dimensional shape with an uneven surface, or a combination thereof.

[0043] A control circuit including a transistor TR for controlling each of the red light emitting element 5R, green light emitting element 5G, and blue light emitting element 5B is provided in the thin film transistor layer 4 including the transistor TR for each of the red sub-pixel RSUB, green sub-pixel GSUB, and blue sub-pixel BSUB. The control circuit including the transistor TR and the light emitting element provided for each of the red sub-pixel RSUB, green sub-pixel GSUB, and blue sub-pixel BSUB are collectively referred to as a sub-pixel circuit.

[0044] 2 may be of either a top-emission type or a bottom-emission type. The red light-emitting element 5R, green light-emitting element 5G, and blue light-emitting element 5B have a forward-laid structure in which the cathode 25 is disposed above the anode 22. To form the red light-emitting element 5R, green light-emitting element 5G, and blue light-emitting element 5B as a top-emission type, the anode 22 may be formed of an electrode material that reflects visible light, and the cathode 25 may be formed of an electrode material that transmits visible light. To form the bottom-emission type, the anode 22 may be formed of an electrode material that transmits visible light, and the cathode 25 may be formed of an electrode material that reflects visible light. On the other hand, when the red light-emitting element, the green light-emitting element, and the blue light-emitting element have an inverted stack structure in which the anode 22 is disposed as an upper layer than the cathode 25, in order to form a top emission type, the cathode 25 may be formed from an electrode material that reflects visible light, and the anode 22 may be formed from an electrode material that transmits visible light, and in order to form a bottom emission type, the cathode 25 may be formed from an electrode material that transmits visible light, and the anode 22 may be formed from an electrode material that reflects visible light.

[0045] The electrode material that reflects visible light is not particularly limited as long as it can reflect visible light and has electrical conductivity. Examples of the electrode material that reflects visible light include metal materials such as Al, Mg, Li, and Ag, alloys of the metal materials, laminates of the metal materials and transparent metal oxides (e.g., indium tin oxide, indium zinc oxide, indium gallium zinc oxide, etc.), and laminates of the alloys and the transparent metal oxides.

[0046] On the other hand, the electrode material that transmits visible light is not particularly limited as long as it can transmit visible light and has conductivity, and examples thereof include transparent metal oxides (e.g., indium tin oxide, indium zinc oxide, indium gallium zinc oxide, etc.), thin films made of metal materials such as Al and Ag, and nanowires made of metal materials such as Al and Ag.

[0047] The anode 22 and the cathode 25 can be formed by a general electrode formation method, for example, a physical vapor deposition (PVD) method such as vacuum deposition, sputtering, EB deposition, or ion plating, or a chemical vapor deposition (CVD) method. The method for patterning the anode 22 and the cathode 25 is not particularly limited as long as it can form the desired pattern with high precision, and specific examples include photolithography and inkjet printing.

[0048] The sealing layer 6 is a light-transmitting film, and can be composed of, for example, an inorganic sealing film 26 that covers the cathode 25, an organic film 27 that is above the inorganic sealing film 26, and an inorganic sealing film 28 that is above the organic film 27. The sealing layer 6 prevents foreign substances such as water and oxygen from penetrating into the red light-emitting element 5R, the green light-emitting element 5G, and the blue light-emitting element 5B.

[0049] The inorganic sealing films 26 and 28 are each an inorganic film, and may be formed, for example, by a CVD method using a silicon oxide film, a silicon nitride film, a silicon oxynitride film, or a laminated film thereof. The organic film 27 is a light-transmitting organic film with a planarizing effect, and may be formed, for example, using a coatable organic material such as acrylic. The organic film 27 may also be formed, for example, by an inkjet method. In this embodiment, the sealing layer 6 is formed of two inorganic films and one organic film disposed between the two inorganic films. However, the stacking order of the two inorganic films and one organic film is not limited to this. Furthermore, the sealing layer 6 may be formed solely of an inorganic film, solely of an organic film, one inorganic film and two organic films, or two or more inorganic films and two or more organic films.

[0050] The functional film 39 is a film having at least one of an optical compensation function, a touch sensor function, and a protection function, for example.

[0051] FIG. 3 is a cross-sectional view showing a schematic configuration of the red light emitting element 5R provided in the display device 1 of the first embodiment.

[0052] As shown in FIG. 3, the red light-emitting element 5R includes an anode 22, a cathode 25, and a red light-emitting layer 24REM provided between the anode 22 and the cathode 25. The red light-emitting layer 24REM includes a plurality of quantum dots QD and a matrix MR including a metal halide MHa, which is provided at least partially between each of the plurality of quantum dots QD and is composed of a metal element and a halogen element, and whose difference in electronegativity is 0.7 or more.

[0053] 3 , the red light-emitting element 5R includes a hole transport layer 24HT as a hole functional layer between the anode 22 and the red light-emitting layer 24REM, and an electron transport layer 24ET as an electron functional layer between the cathode 25 and the red light-emitting layer 24REM. However, the present invention is not limited to this. For example, at least one of the hole transport layer 24HT and the hole injection layer may be provided as a hole functional layer between the anode 22 and the red light-emitting layer 24REM, or the hole functional layer may not be provided between the anode 22 and the red light-emitting layer 24REM. Furthermore, at least one of the electron transport layer 24ET and the electron injection layer may be provided as an electron functional layer between the cathode 25 and the red light-emitting layer 24REM, or the electron functional layer may not be provided between the cathode 25 and the red light-emitting layer 24REM.

[0054] When a matrix composed of a compound containing an element that is not strongly ionic, for example, a matrix composed of zinc sulfide containing zinc (Zn) and sulfur (S), is formed using a relatively low-temperature process (e.g., 25°C or higher and 100°C or lower) in order to maintain good luminous efficiency of the quantum dots (QDs) contained in the light-emitting layer, the matrix contains many defects that can serve as paths for non-radiative recombination, which causes a problem that non-radiative leakage in the light-emitting layer cannot be suppressed. On the other hand, when a matrix composed of zinc sulfide containing zinc (Zn) and sulfur (S) is formed using a relatively high-temperature process in order to reduce the above-mentioned many defects, there is a problem that good luminous efficiency may not be maintained due to deterioration of the quantum dots (QDs) contained in the light-emitting layer.

[0055] Therefore, in this embodiment, the red light-emitting layer 24REM includes a matrix MR containing a metal halide MHa composed of a halogen element, which is an element having stronger ionicity than sulfur (S), and a metal element having an electronegativity difference of 0.7 or more with respect to the halogen element.

[0056] In this embodiment, the metal halide MHa will be described as, for example, copper iodide (CuI) made of copper (Cu (electronegativity = 1.90)), a metal element with strong ionicity, and iodine (I (electronegativity = 2.66)), a halogen element with strong ionicity, or silver iodide (AgI) made of silver (Ag (electronegativity = 1.93)), a metal element with strong ionicity, and iodine (I (electronegativity = 2.66)), a halogen element with strong ionicity. However, the metal halide MHa is not limited to this, as long as it is made of a halogen element with strong ionicity and a metal element whose electronegativity difference with the halogen element is 0.7 or more.

[0057] In the case of a metal halide MHa composed of a halogen element, which is a highly ionic element, and a metal element having an electronegativity difference of 0.7 or more with respect to the halogen element, a precipitate of highly crystalline metal halide MHa crystals can be produced simply by mixing a solution containing the halogen element with a solution containing the metal element, even at a relatively low temperature (e.g., 25°C or higher and 100°C or lower), for example, at room temperature.

[0058] Therefore, in the case of the matrix MR containing the metal halide MHa contained in the red light-emitting layer 24REM, it is not necessary to form it using a relatively high-temperature process that would reduce the luminous efficiency of the quantum dots QD contained in the light-emitting layer, and even if it is formed using a relatively low-temperature process (e.g., 25°C or higher and 100°C or lower), it is possible to suppress the occurrence of defects that could become paths for non-radiative recombination.

[0059] As described above, the red light emitting element 5R can include the red light emitting layer 24REM having good luminous efficiency and good suppression of non-luminous leakage.

[0060] 3, the case where the red light-emitting layer 24REM provided in the red light-emitting element 5R includes a matrix MR containing a metal halide MHa has been described, but the green light-emitting layer provided in the green light-emitting element 5G and the blue light-emitting layer provided in the blue light-emitting element 5B shown in Fig. 2 also each include a matrix MR containing a metal halide MHa. This is not limiting, and at least one of the red light-emitting layer provided in the red light-emitting element 5R, the green light-emitting layer provided in the green light-emitting element 5G, and the blue light-emitting layer provided in the blue light-emitting element 5B shown in Fig. 2 may include a matrix MR containing a metal halide MHa.

[0061] As described above, when the quantum dots QD have, for example, a core structure, a core / shell structure, a core / shell / shell structure, or a shell structure with a continuously changing core / shell ratio, and in any of the materials that can constitute the quantum dots QD, the crystal system of the crystalline structure of the quantum dots QD is a cubic system. In an emitting layer including such cubic quantum dots QD and a matrix MR containing a metal halide MHa, when the metal halide MHa is crystal-grown at a relatively low temperature (e.g., 25°C or higher and 100°C or lower), for example, at room temperature, the metal halide MHa grows on the crystalline structure of the quantum dots QD as a base, thereby realizing a matrix MR with high crystallinity, and the crystal system of the crystal structure of the metal halide MHa is also a cubic system. When the crystal system of the crystalline structure of the quantum dots QD and the crystal system of the crystalline structure of the metal halide MHa are the same as described above, dangling bonds can be reduced in the matrix MR containing the metal halide MHa.

[0062] As described above, in this embodiment, the matrix MR containing the metal halide MHa has high crystallinity, and the crystal system of the crystal structure of the metal halide MHa is the same as the crystal system of the crystal structure of the quantum dots QD. However, this is not limited to this. The matrix MR containing the metal halide MHa may have higher crystallinity than, for example, a matrix composed of a compound containing an element with low ionicity, such as a matrix composed of ZnS. The level of crystallinity can be determined, for example, by using a transmission electron microscope (TEM) to compare and observe the matrix MR containing the metal halide MHa with a matrix composed of a compound containing an element with low ionicity. Furthermore, the crystal system of the crystal structure of the metal halide MHa and the crystal system of the crystal structure of the quantum dots QD may be different.

[0063] 3, when the quantum dot QD has a core CO and a shell SH, it is preferable to grow a metal halide MHa as a crystal at a relatively low temperature (e.g., 25°C or higher and 100°C or lower), for example, at room temperature, using the crystal structure of the shell SH of the quantum dot QD as a base, and to make the crystal system of the crystal structure of the metal halide MHa the same as that of the crystal structure of the quantum dot QD in an emitting layer containing the quantum dot QD and a matrix MR containing the metal halide MHa. When the crystal system of the crystal structure of the shell SH of the quantum dot QD and the crystal system of the crystal structure of the metal halide MHa are the same as described above, dangling bonds can be reduced in the matrix MR containing the metal halide MHa.

[0064] Furthermore, when the quantum dot QD has a core structure having only a core CO, it is preferable to grow a crystal of the metal halide MHa using the crystalline structure of the core CO of the quantum dot QD as a base at a relatively low temperature (e.g., 25°C or higher and 100°C or lower), for example, at room temperature, and to make the crystalline system of the crystalline structure of the core CO of the quantum dot QD and the crystalline system of the crystalline structure of the metal halide MHa the same in an emitting layer containing the quantum dot QD and a matrix MR containing the metal halide MHa. When the crystalline system of the crystalline structure of the core CO of the quantum dot QD and the crystalline system of the crystalline structure of the metal halide MHa are the same as described above, dangling bonds can be reduced in the matrix MR containing the metal halide MHa.

[0065] In this embodiment, the shell SH of the quantum dot QD is made of a metal sulfide, but is not limited thereto. An example of the metal sulfide is zinc sulfide (e.g., ZnS) composed of zinc (Zn) and sulfur (S). The crystal system of the crystal structure of zinc sulfide (e.g., ZnS) is a cubic zinc blende structure. When the shell SH of the quantum dot QD is made of zinc sulfide, it is preferable to grow a crystal of the metal halide MHa on the crystal structure of the shell SH of the quantum dot QD at a relatively low temperature (e.g., 25°C or higher and 100°C or lower), for example, at room temperature, and to make the crystal system of the crystal structure of the metal halide MHa the same as the cubic zinc blende structure, which is the crystal system of the crystal structure of the shell SH of the quantum dot QD, in an emitting layer including the quantum dot QD containing the shell SH made of zinc sulfide and the matrix MR containing the metal halide MHa. When the crystal system of the crystal structure of the shell SH of the quantum dot QD and the crystal system of the crystal structure of the metal halide MHa are the same as described above, dangling bonds can be reduced in the matrix MR containing the metal halide MHa.

[0066] In this embodiment, the metal halide MHa is composed of one type of metal element and one type of halogen element, for example, copper (I) iodide (CuI) or silver (I) iodide (AgI), but is not limited to this. For example, the metal halide MHa may be composed of two or more types of metal elements and one or more types of halogen element. For example, the metal halide MHa may be composed of two types of metal elements, Cu and Ag, and one type of halogen element, I. The crystal of such a metal halide MHa is a CuI-AgI mixed crystal. In the case of a metal halide MHa composed of two or more types of metal elements and one or more types of halogen elements, it is preferable to grow the metal halide MHa as a crystal at a relatively low temperature (e.g., 25°C or higher and 100°C or lower), for example, at room temperature, using the crystal structure of the core CO or the crystal structure of the shell SH of the quantum dot QD as a base, and to make the crystal system of the crystal structure of the metal halide MHa containing copper iodide and silver iodide the same as the crystal system of the crystal structure of the core CO of the quantum dot QD or the crystal system of the crystal structure of the shell SH of the quantum dot QD in the light-emitting layer containing the quantum dot QD and the matrix MR containing the metal halide MHa.

[0067] The crystal structure of copper(I) iodide (CuI) is the same cubic zinc blende structure as InP, ZnSe, and ZnS, which are often used as colloidal quantum dot (QD) materials, and therefore, crystal growth is performed using the crystal structure of the quantum dot (QD) as a template (base). Note that NaCl and other materials that have the same cubic crystal system as the quantum dot (QD) are also grown using the crystal structure of the quantum dot (QD) as a base, but in order to reduce dangling bonds at the interface, it is more preferable that not only the crystal system (cubic crystal) but also the crystal structure (zinc blende structure) including the atomic arrangement are identical.

[0068] In this embodiment, as shown in Figure 3, an example is given in which each of the multiple quantum dots QDs is embedded in a matrix MR containing a metal halide MHa, i.e., the matrix MR containing the metal halide MHa surrounds each of the multiple quantum dots QDs. However, this is not limited to this, and it is sufficient that the matrix MR containing the metal halide MHa is provided at least partially between each of the multiple quantum dots QDs.

[0069] Figure 4 is a diagram for explaining the region R formed between quantum dot QD1 and quantum dot QD2 when two adjacent quantum dots QD1 and QD2 are arranged close to each other among the multiple quantum dots QD contained in the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in Figure 3.

[0070] Figure 5 is a diagram for explaining the region R formed between quantum dot QD1 and quantum dot QD2 when two adjacent quantum dots QD1 and QD2 are arranged a short distance apart from each other among the multiple quantum dots QD contained in the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in Figure 3.

[0071] The region R shown in Figures 4 and 5 is a region surrounded by two straight lines (common circumscribing lines) tangent to the peripheries of two adjacent quantum dots QD1 and QD2 and the opposing peripheries of the two adjacent quantum dots QD1 and QD2. Whether the two adjacent quantum dots QD1 and QD2 are arranged close to each other as shown in Figure 4 or the two adjacent quantum dots QD1 and QD2 are arranged slightly apart as shown in Figure 5, the region R exists and is filled with a matrix MR containing a metal halide MHa. "The matrix MR containing a metal halide MHa is filled between the two adjacent quantum dots QD1 and QD2" means that the region R shown in Figures 4 and 5 is filled with the matrix MR containing the metal halide MHa. In the present disclosure, two adjacent quantum dots QD1 and QD2 may be held by the presence of a matrix MR containing a metal halide MHa in the region R, and for example, at least a portion of the region R may be filled with a matrix MR containing a metal halide MHa. For example, in the red light-emitting layer 24REM shown in FIG. 3, it is preferable that the spaces between each of the multiple quantum dots QD1 and QD2 be filled with a matrix MR.

[0072] In this embodiment, the region R formed between two adjacent quantum dots QD1 and QD2 shown in Figures 4 and 5, i.e., the space between multiple quantum dots QD, is filled with a matrix MR containing a metal halide MHa, as an example, but the present invention is not limited to this.

[0073] In addition, the statement that the quantum dots QD1 and QD2 are held by a matrix MR containing a metal halide MHa present in the region R formed between two adjacent quantum dots QD1 and QD2 means that at least a portion of the region R is filled with a matrix MR containing a metal halide MHa, and includes not only the case where the entire region R is filled with a matrix MR containing a metal halide MHa, but also the case where only a portion of the region R is filled with a matrix MR containing a metal halide MHa.

[0074] The matrix MR containing the metal halide MHa may be formed so as to fill the region (space) of the light-emitting layer other than the plurality of quantum dots QDs. Furthermore, as shown in FIG. 3, the matrix MR containing the metal halide MHa may form the outer edge of the light-emitting layer (e.g., the red light-emitting layer 24REM), and the plurality of quantum dots QDs may be located away from the outer edge. That is, the matrix MR containing the metal halide MHa may contain a plurality of quantum dots QDs. Furthermore, at least a portion of the outer edge of the light-emitting layer may be composed of the matrix MR containing the metal halide MHa and the quantum dots QDs. Furthermore, each of the plurality of quantum dots QDs may be embedded at intervals in the matrix MR containing the metal halide MHa. Here, the outer edge refers to the first surface of the light-emitting layer (e.g., the surface of the red light-emitting layer 24REM in contact with the electron transport layer 24ET shown in FIG. 3) and the second surface of the light-emitting layer (e.g., the surface of the red light-emitting layer 24REM in contact with the hole transport layer 24HT shown in FIG. 3).

[0075] The matrix MR containing the metal halide MHa may include a continuous film. A continuous film means a film that is not divided by materials other than the material that constitutes the continuous film. The continuous film may be an integrated film that is connected without interruption by chemical bonds of the metal halide MHa contained in the matrix MR. The continuous film may be, for example, 1000 nm thick in a plane direction perpendicular to the film thickness direction. 2 It may be formed as a film having an area of ​​more than 100 μm.

[0076] The phrase "a matrix containing a metal halide is provided at least partially between each of the quantum dots" means that a matrix containing a metal halide is filled between at least two quantum dots QDs or is in contact with the quantum dots QDs. Furthermore, the composition of the matrix can be identified by analyzing the material of the matrix located between the two quantum dots QDs, and if there is a gap between the two quantum dots QDs, the composition of the matrix can be identified by analyzing the material of the inner wall of the gap.

[0077] 6 is a diagram schematically showing the band levels of the hole transport layer 24HT, the electron transport layer 24ET, the core CO of the quantum dot QD contained in the red light-emitting layer 24REM, the shell SH of the quantum dot QD contained in the red light-emitting layer 24REM, and the matrix MR containing the metal halide MHa contained in the red light-emitting layer 24REM, which are provided in the red light-emitting element 5R shown in FIG.

[0078] 6 , the band gap (CO(Bg)), which is the difference between the conduction band lower end (CO(CBM)) and the valence band upper end (CO(VBM)) of the core CO of the quantum dot QD included in the red light-emitting layer 24REM provided in the red light-emitting element 5R, is 2.0 eV. Although not shown, the band gap, which is the difference between the conduction band lower end and the valence band upper end of the core of the quantum dot included in the green light-emitting layer provided in the green light-emitting element 5G, is 2.3 eV, and the band gap, which is the difference between the conduction band lower end and the valence band upper end of the core of the quantum dot included in the blue light-emitting layer provided in the blue light-emitting element 5B, is 2.8 eV.

[0079] In this embodiment, as described above, zinc sulfide (e.g., ZnS) is used as the shell SH of the quantum dot QD, and the band gap, which is the difference between the conduction band minimum (SH(CBM)) and the valence band maximum (SH(VBM)) of the shell SH of the quantum dot QD, is 3.4 eV.

[0080] In this embodiment, as described above, copper (I) iodide (CuI) is used as the metal halide MHa, and the matrix MR containing the metal halide MHa, i.e., the band gap (MR(Bg)), which is the difference between the conduction band minimum (MR(CBM)) and the valence band maximum (MR(VBM)) of the metal halide MHa, is 3.1 eV.

[0081] As described above, the matrix MR containing the metal halide MHa, i.e., the band gap (MR(Bg)) of the metal halide MHa, is equal to or larger than the band gap of the core of the quantum dot, so that leakage via the metal halide MHa can be suppressed and effective carrier injection into the quantum dot can be performed.

[0082] In the following, a method for manufacturing a light-emitting element, which includes a step of forming a matrix MR containing a metal halide MHa and a light-emitting layer containing a plurality of quantum dots, will be described using the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in FIG. 3 as an example. However, the green light-emitting layer provided in the green light-emitting element 5G shown in FIG. 2 or the blue light-emitting layer provided in the blue light-emitting element 5B shown in FIG. 2 can also be formed in a similar manner.

[0083] For example, the manufacturing method of the red light-emitting element 5R shown in FIG. 3 includes a step of forming a red light-emitting layer 24REM including a plurality of quantum dots QD and a matrix MR including a metal halide MHa composed of a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more, provided at least in part between each of the plurality of quantum dots QD.

[0084] 3 may be formed using a quantum dot solution containing a solvent, quantum dots QDs, and a metal halide MHa dispersed or dissolved in the solvent. The solvent can be appropriately selected in consideration of the dispersibility of the quantum dots QDs and the dispersibility or solubility of the metal halide MHa, and the solubility (erosion) of the underlayer of the light-emitting layer (e.g., the hole transport layer 24HT). For example, hexane, toluene, and n-octane can be suitably used.

[0085] The step of forming the red light-emitting layer 24REM may include a step of forming a quantum dot layer containing a plurality of quantum dots QDs on a substrate (e.g., on a hole transport layer 24HT provided on the substrate) (see step S1 of FIG. 8 and step S1 of FIG. 10 ), and a step of forming a matrix MR on the quantum dot layer using a metal halide solution containing a solvent and a metal halide MHa dispersed or dissolved in the solvent. The solvent can be appropriately selected taking into consideration the dispersibility or solubility of the metal halide MHa and the solubility (erosion) of the underlayer of the light-emitting layer (e.g., the hole transport layer 24HT). For example, acetonitrile or ethanol can be suitably used.

[0086] To form a matrix MR containing metal halide MHa at low temperatures, it is desirable to apply a solution in which metal halide MHa is dispersed or dissolved, and then re-form the metal halide MHa with the same composition when the solvent evaporates. Such materials are generally found in ionic crystals such as NaCl, and materials with particularly strong ionic properties can be obtained by recrystallization at room temperature.

[0087] Therefore, in this embodiment, the metal halide MHa will be described as copper(I) iodide (CuI) composed of copper (Cu), a metal element with strong ionicity, and iodine (I), a halogen element with strong ionicity, with a difference in electronegativity indicating the strength of ionicity of 0.7 or more. However, the metal halide MHa may be, for example, silver(I) iodide (AgI), as long as it is composed of a metal element with strong ionicity and a halogen element with strong ionicity, with a difference in electronegativity indicating the strength of ionicity of 0.7 or more.

[0088] A metal halide MHa such as copper(I) iodide (CuI) or silver(I) iodide (AgI) can be obtained by recrystallization at a relatively low temperature, for example, from 25°C to 100°C. Even if the step of forming the light-emitting layer as described above is carried out at a relatively low temperature from 25°C to 100°C, it is possible to form a light-emitting layer including a matrix MR containing the metal halide MHa obtained by recrystallization.

[0089] In this embodiment, the case where the process of forming the light-emitting layer is performed in a temperature range of 25°C or higher and 100°C or lower has been described as an example, but this is not limited to this. The process of forming the light-emitting layer may be performed at a temperature below 25°C or higher than 100°C as long as the metal halide MHa can be obtained by recrystallization and the light-emitting properties of the quantum dots QD are not deteriorated within the temperature range.

[0090] In this embodiment, the shell SH of the quantum dot QD is formed of zinc sulfide (e.g., ZnS), and the crystal system of the crystal structure of zinc sulfide is a cubic zinc blende structure.Since the metal halide MHa grows using the shell SH of the quantum dot QD as a base, the crystal system of the crystal structure of the metal halide MHa also is a cubic zinc blende structure.

[0091] It is preferable that each of the quantum dots QDs used in the above-mentioned process of forming the light-emitting layer contains an organic ligand in order to ensure dispersion stability in the solvent and modify surface defects of the quantum dots QDs. However, the presence of insulating organic ligands remaining in the light-emitting layer after forming the light-emitting layer is undesirable because it increases the driving voltage of the light-emitting device. Therefore, in this embodiment, the amount of organic ligand remaining in the light-emitting layer after forming the light-emitting layer is reduced. When using a metal halide solution containing a solvent and a metal halide MHa dissolved in the solvent, for example, after forming a quantum dot layer containing quantum dots QDs having organic ligands, the organic ligands of the quantum dots QDs in the quantum dot layer may be replaced with inorganic ligands (e.g., halogen ligands) or may be removed. Furthermore, when using a quantum dot solution containing a solvent, quantum dots QDs, and a metal halide MHa dissolved in the solvent, for example, the quantum dot solution may be produced using quantum dots QDs having inorganic ligands (e.g., halogen ligands).

[0092] FIG. 7 is a diagram showing an example of a process for forming the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in FIG.

[0093] FIG. 8 is a diagram for explaining the process of forming the red light-emitting layer 24REM shown in FIG.

[0094] As shown in FIGS. 7 and 8, the matrix MR containing the metal halide MHa can be formed at a temperature of, for example, 25° C. or higher and 100° C. or lower by a solution method such as the SILAR (Successive Ionic Layer Adsorption and Reaction) method.

[0095] As shown in FIGS. 7 and 8, a case will be described here in which a matrix MR containing copper (I) iodide (CuI) as the metal halide MHa is formed by the SILAR method, but the present invention is not limited to this.

[0096] The process of forming the red light-emitting layer 24REM included in the red light-emitting element 5R includes the steps of: forming a quantum dot layer containing a plurality of quantum dots QDs on a substrate (e.g., on a hole transport layer 24HT provided on a substrate) (step S1 in FIGS. 7 and 8 ); a first solution treatment step of treating the quantum dot layer using a first solution containing ions of the metal element (e.g., Cu) or ions of the halogen element (e.g., I); and, after the first solution treatment step, a second solution treatment step of treating the quantum dot layer using a second solution containing ions of the other of the metal element (e.g., Cu) or ions of the halogen element (e.g., I). Note that in the process of forming the quantum dot layer containing a plurality of quantum dots QDs shown in step S1 in FIG. 8 , a case where three quantum dots QDs are stacked in the thickness direction will be described as an example, but the present invention is not limited thereto; the quantum dots QDs may be arranged without being stacked, or may be stacked two or more times in the thickness direction.

[0097] In the first solution treatment step (step S2 in FIG. 7 ) of this embodiment, a solution that serves as an ion source for the metal element (e.g., Cu) may be applied to the quantum dot layer to adsorb Cu ions onto the surface of the quantum dots QDs, or the quantum dot layer may be immersed in a solution that serves as an ion source for the metal element (e.g., Cu) to adsorb Cu ions onto the surface of the quantum dots QDs.

[0098] Thereafter, a rinsing step (step S3 in FIGS. 7 and 8) for removing excess Cu ions may be carried out as needed.

[0099] Then, in the second solution treatment step (step S4 in FIG. 7 ) of this embodiment, a solution that serves as an ion source of the halogen element (e.g., I) may be applied to the quantum dot layer to cause I ions to be adsorbed onto the surface of the quantum dots QDs and react with Cu ions, or the quantum dot layer may be immersed in a solution that serves as an ion source of the halogen element (e.g., I) to cause I ions to be adsorbed onto the surface of the quantum dots QDs and react with Cu ions.

[0100] Thereafter, a rinsing step (step S5 in FIGS. 7 and 8) for removing excess I ions may be carried out as needed.

[0101] By repeating the above-described steps S2 to S5 shown in FIG. 7 a predetermined number of times, a light-emitting layer including quantum dots QD embedded in a matrix MR containing copper (I) iodide (CuI), which is a metal halide MHa, can be formed (step S6 in FIGS. 7 and 8).

[0102] When the above-described SILAR method is used to form a light-emitting layer containing a matrix MR containing a metal halide MHa and quantum dots QDs, it is more desirable that the organic ligands attached to the quantum dots QDs are removed before the first solution treatment step (step S2 in FIG. 7 ), for example, by cleaning the surfaces of the quantum dots QDs with ethanol or the like. However, if the solvent used in the first solution treatment step (step S2 in FIG. 7 ) is a solvent that dissolves the organic ligands, the organic ligands can be removed in the first solution treatment step (step S2 in FIG. 7 ), and therefore the prior organic ligand removal step can be omitted.

[0103] 7 and 8 , by adjusting the number of stacked quantum dots QDs in step S1 or the number of repetitions of steps S2 to S5 shown in FIGS. 7 and 8 , it is possible to create a difference in matrix concentration, for example, such that the matrix concentration above the light-emitting layer is higher than the matrix concentration below the light-emitting layer. In this case, organic ligands may remain on the side where the matrix concentration is lower. In the region where the matrix concentration is high, the reduction in insulating organic ligands and the increase in matrix concentration improve carrier conduction.

[0104] FIG. 9 is a diagram showing another example of a process for forming the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in FIG.

[0105] FIG. 10 is a diagram for explaining the process of forming the red light-emitting layer 24REM shown in FIG.

[0106] As shown in FIGS. 9 and 10, the matrix MR containing the metal halide MHa can be formed at a temperature of, for example, 25° C. or higher and 100° C. or lower by a solution method such as a CBD (Chemical Bath Deposition) method.

[0107] As shown in FIGS. 9 and 10, a case will be described here in which a matrix MR containing copper (I) iodide (CuI) as a metal halide MHa is formed using the CBD method, but the present invention is not limited to this.

[0108] The process of forming the red light-emitting layer 24REM provided in the red light-emitting element 5R includes the steps of: forming a quantum dot layer including a plurality of quantum dots QDs on a substrate (e.g., on a hole transport layer 24HT provided on a substrate) (step S1 in FIGS. 9 and 10 ); immersing the substrate on which the quantum dot layer has been formed in a first solution including ions of either the metal element (e.g., Cu) or the halogen element (e.g., I) (step S12 in FIG. 9 ); and dripping a second solution including ions of the other of the metal element (e.g., Cu) and the halogen element (e.g., I) while the substrate is immersed in the first solution (step S13 in FIGS. 9 and 10 ).

[0109] In the immersion step (step S12 in FIG. 9) of this embodiment, the substrate on which the quantum dot layer is formed is immersed in a solution that serves as an ion source of the metal element (for example, Cu).

[0110] Then, in the second solution dropping step of this embodiment (step S13 in FIGS. 9 and 10), while the substrate is immersed in the solution that serves as an ion source for the metal element (e.g., Cu), a solution that serves as an ion source for the halogen element (e.g., I) is dropped to cause a CBD reaction.

[0111] As a result of the above, a light-emitting layer including quantum dots QD embedded in a matrix MR containing copper (I) iodide (CuI), which is a metal halide MHa, can be formed (step S6 in FIGS. 9 and 10).

[0112] When the above-mentioned CBD method is used, a light-emitting layer containing a matrix MR containing a metal halide MHa and quantum dots QD can be formed with fewer steps than when the above-mentioned SILAR method is used.

[0113] When using the above-mentioned CBD method to form a light-emitting layer containing a matrix MR containing a metal halide MHa and quantum dots QDs, it is more desirable that the organic ligands attached to the quantum dots QDs are removed before the immersion step (step S12 in Figure 9 ) by, for example, washing the surface of the quantum dots QDs with ethanol or the like. However, if the solvent used in the immersion step (step S12 in Figure 9 ) is a solvent that dissolves the organic ligands, the organic ligands can be removed in the immersion step (step S12 in Figure 9 ), and therefore the preliminary organic ligand removal step can be omitted.

[0114] FIG. 11 is a diagram showing an example of a material that can be used as the metal halide MHa contained in the light-emitting layer of the light-emitting element of each color provided in the display device 1 of the first embodiment.

[0115] Up to now, the metal halide MHa has been described as being, for example, copper (I) iodide (CuI) or silver (I) iodide (AgI), but is not limited thereto.

[0116] For example, the metal halide MHa may be appropriately selected from the metal fluorides, metal chlorides, metal bromides, and metal iodides shown in FIG. 11 and may be composed of a metal element with strong ionicity and a halogen element with strong ionicity, the difference in electronegativity indicating the strength of ionicity being 0.7 or more.

[0117] [Embodiment 2] Next, embodiment 2 of the present disclosure will be described with reference to Figures 12 and 13. The red light-emitting element 5R' provided in the display device of this embodiment differs from the light-emitting elements of each color provided in the display device 1 described in embodiment 1 in that it includes a hole transport layer 24HT' containing a metal halide MHa1 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more. The rest is as described in embodiment 1. For convenience of explanation, components having the same functions as those shown in the drawings of embodiment 1 are designated by the same reference numerals, and their description will be omitted.

[0118] FIG. 12 is a cross-sectional view showing a schematic configuration of a red light emitting element 5R' provided in the display device of the second embodiment.

[0119] 12 , the red light-emitting element 5R′ includes, as a red functional layer 24R′ including the red light-emitting layer 24REM, a hole transport layer 24HT′ including a metal halide MHa1 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more, the red light-emitting layer 24REM, and the electron transport layer 24ET. However, the present invention is not limited to this. For example, the red light-emitting element 5R′ may include a hole functional layer between the anode 22 and the red light-emitting layer 24REM. The hole functional layer may include at least one of a hole transport layer and a hole injection layer, and at least one of the hole transport layer and the hole injection layer may include a metal halide MHa1 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more.

[0120] In the red light-emitting element 5R′ shown in FIG. 12 , a hole transport layer 24HT′ in contact with the red light-emitting layer 24REM is provided between the anode 22 and the red light-emitting layer 24REM, and the hole transport layer 24HT′ in contact with the red light-emitting layer 24REM contains a metal halide MHa1 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more, and the crystal system of the crystal structure of the metal halide MHa contained in the red light-emitting layer 24REM is the same as the crystal system of the crystal structure of the metal halide MHa1 contained in the hole transport layer 24HT′.

[0121] Although not shown, in the red light-emitting element 5R′, a hole injection layer in contact with the red light-emitting layer 24REM may be provided between the anode 22 and the red light-emitting layer 24REM, and the hole injection layer in contact with the red light-emitting layer 24REM contains a metal halide MHa1 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more, and the crystal system of the crystal structure of the metal halide MHa contained in the red light-emitting layer 24REM and the crystal system of the crystal structure of the metal halide MHa1 contained in the hole injection layer in contact with the red light-emitting layer 24REM may be the same.

[0122] In this embodiment, the case where the metal halide MHa and the metal halide MHa1 are each copper (I) iodide (CuI) will be described as an example, but the present invention is not limited to this. The metal halide MHa and the metal halide MHa1 can each be appropriately selected from the metal halides described in the above-mentioned first embodiment, and the metal halide MHa and the metal halide MHa1 may be the same metal halide or different metal halides.

[0123] Since copper (I) iodide (CuI) exhibits p-type conduction, when a layer made of metal halide MHa1 that does not contain quantum dots QD is formed on the anode 22 side of the red light-emitting layer 24REM, it can be used as a hole transport layer 24HT′ or a hole injection layer.

[0124] In addition, copper (I) iodide (CuI) is a good hole transport material, and by placing a layer of copper (I) iodide (CuI) without containing quantum dots QD adjacent to the red light-emitting layer 24REM, the luminous efficiency and brightness of the red light-emitting element 5R' can be improved.

[0125] 12 includes, before the step of forming the red light-emitting layer 24REM, a step of forming a hole functional layer (e.g., a hole transport layer 24HT′) containing a metal halide MHa1 consisting of a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more. However, the present invention is not limited to this. For example, if the red light-emitting element 5R′ is a light-emitting element having an inverted stack structure, the method includes, after the step of forming the red light-emitting layer 24REM, a step of forming a hole functional layer (e.g., a hole transport layer 24HT′) containing a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more. Note that the method of forming the hole functional layer containing the metal halide MHa1 is the same as the method of forming the matrix MR containing the metal halide MHa described in embodiment 1, and therefore, description thereof will be omitted here.

[0126] Figure 13 is a diagram schematically showing the band levels of the hole transport layer 24HT' containing a metal halide MHa1, the electron transport layer 24ET, the core CO of the quantum dot QD contained in the red light-emitting layer 24REM, the shell SH of the quantum dot QD contained in the red light-emitting layer 24REM, and the matrix MR containing a metal halide MHa contained in the red light-emitting layer 24REM, which are provided in the red light-emitting element 5R' shown in Figure 12.

[0127] In this embodiment, as described above, copper (I) iodide (CuI) is used as each of the metal halide MHa and the metal halide MHa1. As shown in FIG. 13 , the matrix MR containing the metal halide MHa, i.e., the band gap (MR(Bg)) which is the difference between the conduction band bottom (MR(CBM)) and the valence band top (MR(VBM)) of the metal halide MHa, is 3.1 eV. The hole transport layer 24HT′ containing the metal halide MHa1, i.e., the band gap which is the difference between the conduction band bottom (24HT′(CBM)) and the valence band top (24HT′(VBM)) of the metal halide MHa1, is also 3.1 eV.

[0128] In this embodiment, a red light-emitting element 5R' provided in a display device has been described as an example, but this is not limited to this, and a similar configuration can also be used for a green light-emitting element or a blue light-emitting element provided in a display device.

[0129] [Embodiment 3] Next, embodiment 3 of the present disclosure will be described with reference to Figures 14 and 15. The red light-emitting element 5R'' provided in the display device of this embodiment differs from the light-emitting elements of each color provided in the display devices described in embodiments 1 and 2 in that it includes an electron blocking layer 24EB containing a metal halide MHa2 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more. The rest is as described in embodiments 1 and 2. For convenience of explanation, components having the same functions as those shown in the drawings of embodiments 1 and 2 are designated by the same reference numerals, and their description will be omitted.

[0130] FIG. 14 is a cross-sectional view showing a schematic configuration of a red light emitting element 5R'' provided in the display device of the third embodiment.

[0131] 15 is a diagram schematically showing the band levels of the hole transport layer 24HT, the electron transport layer 24ET, the electron blocking layer 24EB containing the metal halide MHa2, the core CO of the quantum dot QD contained in the red light-emitting layer 24REM, the shell SH of the quantum dot QD contained in the red light-emitting layer 24REM, and the matrix MR containing the metal halide MHa contained in the red light-emitting layer 24REM, which are provided in the red light-emitting element 5R'' shown in FIG.

[0132] 14 , the red light-emitting element 5R″ includes, as a red functional layer 24R″ including a red light-emitting layer 24REM, a hole-transport layer 24HT, a red light-emitting layer 24REM, an electron-blocking layer 24EB including a metal halide MHa2 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more, and an electron-transporting layer 24ET. However, the present invention is not limited to this. For example, in the red light-emitting element 5R″, an electron-blocking layer 24EB may be provided between the red light-emitting layer 24REM and the electronic functional layer (at least one of the electron-transporting layer 24ET and the electron-injection layer), and the electron-blocking layer 24EB may include a metal halide MHa2 composed of a metal element and a halogen element whose electronegativity difference is 0.7 or more.

[0133] In the red light-emitting element 5R'' shown in FIG. 14, an electron blocking layer 24EB in contact with the red light-emitting layer 24REM is provided between the cathode 25 and the red light-emitting layer 24REM, and the electron blocking layer 24EB in contact with the red light-emitting layer 24REM contains a metal halide MHa2 composed of a metal element and a halogen element whose difference in electronegativity is 0.7 or more, and the crystal system of the crystal structure of the metal halide MHa contained in the red light-emitting layer 24REM is the same as the crystal system of the crystal structure of the metal halide MHa2 contained in the electron blocking layer 24EB.

[0134] In this embodiment, the case where the metal halide MHa and the metal halide MHa2 are each copper (I) iodide (CuI) will be described as an example, but the present invention is not limited to this. The metal halide MHa and the metal halide MHa2 can each be appropriately selected from the metal halides described in the above-mentioned first embodiment, and the metal halide MHa and the metal halide MHa2 may be the same metal halide or different metal halides.

[0135] Copper (I) iodide (CuI) exhibits p-type conduction and, as shown in FIG. 15 , the conduction band minimum (24EB(CBM)) of the electron blocking layer 24EB is shallow, making it possible to block electrons. When a layer made of a metal halide MHa2 that does not contain quantum dots QDs is formed closer to the cathode 25 than the red light-emitting layer 24REM, it can be used as the electron blocking layer 24EB.

[0136] In the red light emitting element 5R'' having the electron blocking layer 24EB, the electron excess state in the red light emitting layer 24REM can be improved, and therefore the light emitting efficiency can be improved.

[0137] 14 includes, after the step of forming the red light-emitting layer 24REM, a step of forming an electron blocking layer 24EB including a metal halide MHa2 composed of a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more. However, the method is not limited to this. For example, if the red light-emitting element 5R'' is a light-emitting element having an inverted stack structure, the method includes, before the step of forming the red light-emitting layer 24REM, a step of forming an electron blocking layer 24EB including a metal halide MHa2 composed of a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more. Note that the method of forming the electron blocking layer 24EB including the metal halide MHa2 is the same as the method of forming the matrix MR including the metal halide MHa described in the first embodiment, and therefore, description thereof will be omitted here.

[0138] In this embodiment, as described above, copper (I) iodide (CuI) is used as each of the metal halide MHa and the metal halide MHa2. As shown in FIG. 15 , the matrix MR containing the metal halide MHa, i.e., the band gap (MR(Bg)) which is the difference between the conduction band bottom (MR(CBM)) and the valence band top (MR(VBM)) of the metal halide MHa, is 3.1 eV. The electron blocking layer 24EB containing the metal halide MHa2, i.e., the band gap which is the difference between the conduction band bottom (24EB(CBM)) and the valence band top (24EB(VBM)) of the metal halide MHa2, is also 3.1 eV.

[0139] In this embodiment, a red light-emitting element 5R'' provided in a display device has been described as an example, but this is not limited to this, and a similar configuration can also be used for a green light-emitting element or a blue light-emitting element provided in a display device.

[0140] Although not shown, the red light emitting element 5R'' shown in FIG. 14 may include a hole transport layer 24HT' provided in the red light emitting element 5R' shown in FIG. 12, instead of the hole transport layer 24HT.

[0141] [Embodiment 4] Next, embodiment 4 of the present disclosure will be described with reference to Figures 16 and 17. The display device 1a of this embodiment differs from the display devices described in embodiments 1 to 3 in that it includes a heating unit 33 for performing a process of melting the metal halide MHa. The rest is as described in embodiments 1 to 3. For convenience of explanation, members having the same functions as the members shown in the drawings of embodiments 1 to 3 are assigned the same reference numerals, and their description will be omitted.

[0142] FIG. 16 is a plan view showing a schematic configuration of a display device 1a according to the fourth embodiment.

[0143] FIG. 17 is a diagram showing the heating unit 33 provided in the display device 1a of the fourth embodiment shown in FIG.

[0144] As shown in Figure 17, the display device 1a is separately equipped with a heating unit 33 for performing the process of melting the metal halide MHa, so the scanning side driving circuit 31a and the data side driving circuit 32a may have the same configuration as the scanning side driving circuit 31 and the data side driving circuit 32 provided in the display device 1 shown in Figure 1 which does not have the heating unit 33.

[0145] As shown in FIG. 17, the heating section 33 only needs to heat the area containing the metal halide MHa, and therefore may be arranged to overlap only the display area DA of the display panel 30, but is not limited to this.

[0146] In the case where a heating unit 33 is separately provided as in the display device 1a, the step of melting the metal halide MHa can be performed even before forming the cathode 25 of the light-emitting element. For example, the step of melting the metal halide MHa can be performed after forming the electron transport layer 24ET on the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in FIG. 3. That is, the step of melting the metal halide MHa can be performed during the manufacturing process of the light-emitting element.

[0147] In addition, when a heating unit 33 for performing a process of melting the metal halide MHa is separately provided, as in the display device 1a, it is preferable to ensure the heat resistance of the display panel 30. For example, the heat resistance of the display panel 30 can be ensured by changing the organic layers included in the display panel 30 to inorganic layers and omitting any organic layers that can be omitted. For example, the heat resistance of the light-emitting element can be ensured by forming the hole transport layer 24HT from NiO particles, forming the electron transport layer 24ET from ZnO particles, and using inorganic ligands (e.g., halogen ligands) as the ligands included in the quantum dots QD.

[0148] For example, in the red light-emitting layer 24REM provided in the red light-emitting element 5R shown in FIG. 3, at the interface between the quantum dots QD and the matrix MR containing the metal halide MHa, the halogen element of the metal halide MHa terminates the outermost surface of the shell SH of the quantum dots QD. However, over time or long-term operation, the halogen element desorbs, generating defects on the surface of the quantum dots QD. Furthermore, crystal defects generated in the matrix MR containing the metal halide MHa also cause non-radiative leakage, resulting in reduced brightness. Therefore, by heating and cooling the red light-emitting layer 24REM containing the matrix MR containing the metal halide MHa and the quantum dots QD, the metal halide MHa melts and recrystallizes, thereby allowing the crystal growth of the metal halide MHa to resume using the crystalline structure on the surface of the quantum dots QD as a base. This allows the reduced brightness to be restored. The heating means may be heating using the heating unit 33, which is an external heat source as described above, induction heating using electromagnetic waves, or Joule heat generated by current driving of the light-emitting element.

[0149] In addition, when considering the process of melting the metal halide MHa contained in the light-emitting layer provided in the light-emitting element as described above, the metal halide MHa contained in the light-emitting layer is preferably composed of different types of metal halides, and may be composed of, for example, copper (I) iodide (CuI) and silver (I) iodide (AgI). In this case, the matrix containing the metal halide MHa becomes a CuI-AgI mixed crystal, and the melting point is lowered, so that the temperature in the process of melting the metal halide MHa contained in the light-emitting layer can be lowered.

[0150] According to a method for restoring the light-emitting characteristics of a light-emitting element, which includes a step of melting metal halide MHa contained in a light-emitting layer provided in the light-emitting element, the light-emitting characteristics of the light-emitting element can be restored and the long-term reliability of the light-emitting element can be improved.

[0151] [Additional Notes] The present disclosure is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present disclosure. Furthermore, new technical features can be formed by combining the technical means disclosed in each embodiment.

[0152] The present disclosure can be utilized in a light-emitting device, a display device, a method for manufacturing a light-emitting device, and a method for restoring the light-emitting characteristics of a light-emitting device.

[0153] REFERENCE SIGNS LIST 1, 1a Display device 3 Barrier layer 4 Thin film transistor layer 5R, 5R', 5R'' Red light emitting element (light emitting element) 5G Green light emitting element (light emitting element) 5B Blue light emitting element (light emitting element) 12 Substrate 22 Anode 24R, 24R', 24R'' Functional layer including red light emitting layer 24G Functional layer including green light emitting layer 24B Functional layer including blue light emitting layer 24REM Red light emitting layer (light emitting layer) 24HT, 24HT' Hole transport layer 24REM, 24REM' Red light emitting layer (light emitting layer) 24ET Electron transport layer 24EB Electron blocking layer 25 Cathode 30 Display panel 31, 31a Scanning side drive circuit 32, 32a Data side drive circuit 33 Heating unit PIX Pixel RSUB Red subpixel GSUB Green subpixel BSUB Blue subpixel DA Display area NDA Frame area QD Quantum dot CO Core of quantum dot SH Shell of quantum dot MR Matrix containing metal halide MHa, MHa1, MHa2 Metal halide Bg Band gap CBM Bottom of conduction band VBM Top of valence band

Claims

1. A light-emitting element comprising: an anode; a cathode; and a light-emitting layer provided between the anode and the cathode, wherein the light-emitting layer includes a plurality of quantum dots and a matrix containing a metal halide composed of a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more, provided at least partially between each of the plurality of quantum dots.

2. The light-emitting device according to claim 1, wherein in the light-emitting layer, spaces between each of the plurality of quantum dots are filled with the matrix.

3. The light-emitting element according to claim 1 or 2, wherein the crystal system of the crystal structure of the metal halide is a cubic system.

4. The light-emitting element according to any one of claims 1 to 3, wherein the quantum dot has a core and a shell, and the crystal system of the crystal structure of the shell is the same as the crystal system of the crystal structure of the metal halide.

5. The light-emitting device according to claim 4, wherein the shell is made of a metal sulfide.

6. The light-emitting element according to claim 5, wherein the metal sulfide is composed of zinc (Zn) and sulfur (S), and a crystal system of the crystal structure of the metal halide and a crystal system of the crystal structure of the metal sulfide composed of the zinc (Zn) and the sulfur (S) are cubic zinc blende structures.

7. The light-emitting element according to any one of claims 1 to 3, wherein the quantum dot has a core, and the crystal system of the crystal structure of the core is the same as the crystal system of the crystal structure of the metal halide.

8. The light-emitting element according to any one of claims 1 to 7, wherein the metal halide comprises one type of metal element and one type of halogen element.

9. The light-emitting element according to any one of claims 1 to 7, wherein the metal halide comprises two or more kinds of metal elements and one or more kinds of halogen elements.

10. A light-emitting device according to any one of claims 1 to 9, wherein the quantum dot has a core, and the band gap of the metal halide is equal to or greater than the band gap of the core of the quantum dot.

11. A light-emitting element described in any one of claims 1 to 10, wherein a hole functional layer is provided between the anode and the light-emitting layer, the hole functional layer has at least one of a hole transport layer and a hole injection layer, and at least one of the hole transport layer and the hole injection layer contains a metal halide composed of a metal element and a halogen element whose difference in electronegativity is 0.7 or more.

12. A light-emitting element described in any one of claims 1 to 10, wherein a hole transport layer or a hole injection layer in contact with the light-emitting layer is provided between the anode and the light-emitting layer, the hole transport layer or the hole injection layer in contact with the light-emitting layer contains a metal halide composed of a metal element and a halogen element whose difference in electronegativity is 0.7 or more, and a crystal system of a crystal structure of the metal halide contained in the light-emitting layer is the same as a crystal system of a crystal structure of the metal halide contained in the hole transport layer or the hole injection layer.

13. The light-emitting element according to any one of claims 1 to 12, wherein an electronic functional layer is provided between the cathode and the light-emitting layer, and the electronic functional layer includes at least one of an electron transport layer and an electron injection layer.

14. The light-emitting element according to claim 13, further comprising an electron blocking layer provided between the light-emitting layer and the electronic functional layer, the electron blocking layer including a metal halide composed of a metal element and a halogen element having an electronegativity difference of 0.7 or more.

15. A light-emitting element described in any one of claims 1 to 12, wherein an electron blocking layer is provided between the cathode and the light-emitting layer and is in contact with the light-emitting layer, the electron blocking layer in contact with the light-emitting layer contains a metal halide composed of a metal element and a halogen element whose difference in electronegativity is 0.7 or more, and a crystal system of a crystal structure of the metal halide contained in the light-emitting layer and a crystal system of a crystal structure of the metal halide contained in the electron blocking layer are the same.

16. A display device comprising a light-emitting element according to any one of claims 1 to 15.

17. A method for manufacturing a light-emitting element, comprising the step of forming a light-emitting layer including a plurality of quantum dots and a matrix containing a metal halide composed of a metal element and a halogen element, the difference in electronegativity between which is 0.7 or more, provided at least in a portion between each of the plurality of quantum dots.

18. The method for manufacturing a light-emitting element according to claim 17, wherein in the step of forming the light-emitting layer, the light-emitting layer is formed using a quantum dot solution containing a solvent, the quantum dots, and the metal halide dispersed or dissolved in the solvent.

19. The method for manufacturing a light-emitting element according to claim 17, wherein the step of forming the light-emitting layer includes the steps of: forming a quantum dot layer containing the plurality of quantum dots on a substrate; and forming the matrix on the quantum dot layer using a metal halide solution containing a solvent and the metal halide dispersed or dissolved in the solvent.

20. A method for manufacturing a light-emitting element as described in claim 17, wherein the step of forming the light-emitting layer includes: a step of forming a quantum dot layer containing the plurality of quantum dots on a substrate; a first solution treatment step of treating the quantum dot layer with a first solution containing one of ions of the metal element and ions of the halogen element; and a second solution treatment step of treating the quantum dot layer with a second solution containing the other of the ions of the metal element and ions of the halogen element after the first solution treatment step.

21. A method for manufacturing a light-emitting element as described in claim 17, wherein the step of forming the light-emitting layer includes the steps of: forming a quantum dot layer containing the plurality of quantum dots on a substrate; immersing the substrate on which the quantum dot layer has been formed in a first solution containing one of the ions of the metal element and the ions of the halogen element; and dripping a second solution containing the other of the ions of the metal element and the ions of the halogen element while the substrate is immersed in the first solution.

22. The method for manufacturing a light-emitting element according to any one of claims 17 to 21, wherein the step of forming the light-emitting layer is carried out at a temperature of 25°C or higher and 100°C or lower.

23. A method for manufacturing a light-emitting element according to any one of claims 17 to 22, comprising a step of forming a hole functional layer containing a metal halide composed of a metal element and a halogen element, the difference between whose electronegativity is 0.7 or more, before or after the step of forming the light-emitting layer.

24. A method for producing a light-emitting element according to any one of claims 17 to 22, comprising a step of forming an electron blocking layer containing a metal halide composed of a metal element and a halogen element, the difference in electronegativity of which is 0.7 or more, before or after the step of forming the light-emitting layer.

25. A method for recovering the luminous characteristics of a light-emitting element manufactured by the method for manufacturing a light-emitting element according to any one of claims 17 to 24, comprising the step of melting the metal halide contained in the light-emitting layer.

Citation Information

Patent Citations

  • Heterojunction structure quantum dot and synthetic method and application thereof

    CN109119543A

  • Light-emitting film, production method thereof, and a light emitting device including the same

    EP3575379A1

  • Quantum dot structure and method of forming quantum dot structure, and wavelength conversion element, optical converter and photoelectric converter

    JP2012114419A

  • Electroluminescent device, and display device comprising same