Method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas
The method addresses the inefficiencies in NOx denitrification by converting nitrogen dioxide from cement exhaust gas into ammonium nitrate using water and magnetite, achieving efficient denitrification and reducing environmental impact through waste heat utilization and recycling.
Patent Information
- Application Number
- PCT/JP2024/010413
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-28
- Filing Date
- 2024-03-18
- Publication Date
- 2024-10-03
AI Technical Summary
Conventional methods for denitrification of nitrogen oxides (NOx) in cement factory exhaust gases are limited by high-temperature requirements, complexity, and inefficiency, making it difficult to effectively recover and reuse NOx, which results in environmental pollution and increased costs.
A method that recovers nitrogen dioxide from cement exhaust gas by contacting it with water, followed by a reduction reaction with reduced iron and magnetite under acidic conditions to produce ammonia, which is then vaporized using waste heat, and subsequently converted into ammonium nitrate, reducing environmental impact and catalyst production burdens.
This method efficiently denitrifies nitrogen dioxide in cement factory exhaust gases, reduces environmental burden, and creates a recycling cycle that utilizes waste heat and residues, producing high-purity ammonium nitrate suitable for cement production.
Smart Images

Figure JP2024010413_03102024_PF_FP_ABST
Abstract
Description
A method for producing ammonium nitrate using nitrogen dioxide in cement waste gas
[0001] The present invention relates to a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, and in particular to a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, which can highly efficiently recover nitrogen dioxide generated in cement plants, thereby simply and effectively reducing the environmental load and also suppressing the environmental load of the preparation of a catalyst used in the process of preparing the ammonium nitrate.
[0002] In general, in cement production, exhaust gas generated by burning coal, heavy oil, or recycled fuel is used to dry the cement raw materials, and then the contained dust is recovered in a dust collection process and discharged outside the system. The exhaust gas discharged outside the system contains not only carbon dioxide and trace amounts of chlorides, but also large amounts of nitrogen oxides (hereinafter referred to as "NOx") resulting from fuel combustion, etc. NOx causes environmental loads such as acid rain and has adverse effects on the human body, including the respiratory system.
[0003] In light of these problems, cement plants have proposed reducing NOx emissions by selecting fuels with low nitrogen content and by using denitrifiers to regulate NOx emissions.
[0004] Japanese Patent No. 5100432 (Patent Document 1) proposes an SCR method using urea or alcohol as a NOx denitrification technology for use in cement plants. Specifically, the proposed method is an exhaust gas treatment method in which a denitrification agent is brought into contact with exhaust gas containing nitrogen oxides to denitrify the exhaust gas. The denitrification agent is a mixture of urea and one or more types of waste liquid selected from the group consisting of water-soluble waste liquid containing oil, waste liquid produced by washing ash with water, waste liquid containing alcohols, and waste liquid produced in cement or concrete plants. The type of waste liquid and the mass ratio of the waste liquid to urea are determined so as to satisfy specific conditions.
[0005] However, in this method, the optimum temperature for the denitration reaction is set at 800°C or higher, and the hot gas that passes through the urea spray area is not denitrified, so it can be assumed that approximately 400 ppm of NOx is emitted into the atmosphere.
[0006] Furthermore, Japanese Patent Laid-Open Publication No. 2003-175315 (Patent Document 2) proposes a nitrogen oxide absorbent that absorbs nitrogen oxides in a high-temperature gas containing oxygen and nitrogen oxides, the nitrogen oxide absorbent comprising a mixture of an oxide or hydroxide of an alkaline earth element and an oxide of a transition element, the alkaline earth element being barium (Ba) and / or strontium (Sr), and the transition element being copper (Cu) and / or iron (Fe).
[0007] Furthermore, Japanese Patent No. 5963405 (Patent Document 3) discloses a method for denitrifying a gas containing NOx to be treated, in which NOx, a component of the gas to be treated, is oxidized by ozone, and the NOx components in the gas to be treated after this ozone oxidation produce nitrous acid through mixing and contact with an absorption liquid, and the NOx generated by the conversion of the nitrous acid is released into the gas phase, which is suppressed or prevented by ozone added in advance to the absorption liquid.The molar ratio of ozone supplied to the gas to be treated to the gas to the components to be treated is set to be in the range of 0.1 to 2, and ozone of 1 ppm or more but not more than a saturated concentration is added in advance to the absorption liquid that absorbs the gas components to be treated, and the mixing and contact of the gas to which the ozone has been supplied and the absorption liquid to which the ozone has been added is carried out in a fibrous porous body having a gas-liquid separation function, and the gas-liquid separation is carried out below the porous body.
[0008] The conventional method of Patent Document 2 is carried out under high-temperature gas conditions (300 to 600°C), and application to cement plants is difficult because the cement combustion exhaust gas contains collected dust. Also, the conventional method of Patent Document 3 recovers NOx with water at room temperature, but requires the recovered nitrous acid to be oxidized using ozone or the like, which makes the process complicated and expensive, making it difficult to introduce into actual cement plants.
[0009] As described above, in the conventional methods, denitrification of NOx in exhaust gases generated in cement plants can only be performed within a limited temperature range, and the process is complicated, making it impossible to effectively reuse the recovered NOx. Furthermore, there is a need for a method for producing ammonium nitrate that utilizes NOx in exhaust gases and achieves a sufficient reduction in environmental impact.
[0010] Japanese Patent No. 5100432 Japanese Patent Laid-Open No. 2003-175315 Japanese Patent No. 5963405
[0011] An object of the present invention is to solve the above problems and to provide a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, which can simply and efficiently denitrify nitrogen dioxide in waste gas generated during cement production in a cement factory, thereby suppressing emissions into the atmosphere and reducing the environmental load.
[0012] Another object of the present invention is to provide a circulation cycle that is suitable for cement plants and has excellent environmental impact reduction properties, in which nitrogen dioxide in cement exhaust gas is converted into ammonium nitrate by utilizing waste heat gas emitted in the cement manufacturing process, and the catalyst used in the process of manufacturing ammonium nitrate is also manufactured, thereby reducing the environmental impact, and the resulting residue can be effectively used in cement manufacturing.
[0013] (I) The method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas of the present invention comprises: a nitrogen dioxide recovery step (1) of contacting nitrogen dioxide in cement exhaust gas with water to absorb the nitrogen dioxide into the water and recovering the nitrogen dioxide as a nitrate-nitrite nitrogen-containing liquid; a reduction reaction step (2) of contacting reduced iron and magnetite with all or a part of the nitrate-nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) under acidic conditions to produce iron hydroxide and ammonia; an ammonia recovery step (3) of distilling and vaporizing the ammonia produced in the reduction reaction step (2) using waste heat gas from the cement production process to recover it; and a solid-liquid separation step (4) of separating the remainder after recovering ammonia in the ammonia recovery step (3) and separating the iron hydroxide from the reduction reaction step (2) that has undergone the ammonia recovery step (3) and the unused remainder nitrate-nitrite nitrogen. a neutralization step (5) in which the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4) and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) are brought into contact with ammonia vaporized and recovered in the ammonia recovery step (3) to prepare ammonium nitrate; and a catalyst production step (7) in which the magnetite used in the reduction reaction step (2) is prepared by reacting iron sulfate with an aqueous sodium hydroxide solution to produce magnetite and an aqueous sodium sulfate solution, subjecting the resulting aqueous sodium sulfate solution to solid-liquid separation, separating the sodium hydroxide and sodium hydroxide by electrodialysis, and recycling the resulting sodium hydroxide for use in preparing magnetite to be reacted with the iron sulfate.
[0014] (II) Preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in cement exhaust gas according to the present invention described in (I) above, the sulfuric acid obtained in the catalyst production step (7) is used to create acidic conditions in the reduction reaction step (2) and / or is reacted with unreacted sodium hydroxide after magnetite preparation to produce sodium sulfate, which is recycled for use in the electrodialysis together with the aqueous sodium sulfate solution obtained by solid-liquid separation in the catalyst production step (7).
[0015] (III) More preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in exhaust gas from cement production according to the present invention described in (I) or (II) above, the hydrogen generated during the preparation of magnetite in the catalyst production step (7) is recycled and reused as a combustion raw material during cement production.
[0016] (IV) More preferably, the method for producing ammonium nitrate utilizing nitrogen dioxide in cement exhaust gas according to the present invention described in (I) or (II) above further comprises a granulation step (6) of granulating the ammonium nitrate prepared in the neutralization step (5).
[0017] (V) More preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in cement exhaust gas according to the present invention described in (I) or (II) above, the iron hydroxide separated in the solid-liquid separation step (4) is converted into iron hydroxide oxide by exposure to air, and the iron hydroxide oxide is used as a cement raw material.
[0018] (VI) Preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in cement exhaust gas according to the present invention described in (I) above, the ammonium nitrate prepared in the neutralization step (5) is contained in a liquid containing ammonium nitrate and nitrate / nitrite nitrogen, and the liquid is heated and distilled at 170 to 180°C using waste heat gas to concentrate ammonium nitrate, and the remaining nitrate / nitrite nitrogen is vaporized and circulated to the neutralization step (5), and a portion of the ammonia vaporized in the ammonia recovery step (3) is added to the concentrated ammonium nitrate to react with unreacted nitrate / nitrite nitrogen mixed in the concentrated ammonium nitrate, thereby improving the purity of the ammonium nitrate, and the method is cooled to obtain crystallized ammonium nitrate.
[0019] The method for producing ammonium nitrate of the present invention makes it possible to highly efficiently denitrify nitrogen dioxide contained in exhaust gases emitted from cement plants, which is environmentally friendly. Furthermore, the recovered nitrate and nitrite nitrogen can be reduced without any special oxidation treatment, and the ammonium nitrate obtained as the final product can be effectively used as a blasting agent in limestone mines, which is a raw material for cement production. This makes it possible to create an environmentally friendly recycling cycle.
[0020] Furthermore, the waste heat gas emitted in the cement manufacturing process can be used as a heat source for producing magnetite, a reducing catalyst, and for vaporizing ammonia, making it possible to effectively utilize the waste heat gas in the cement manufacturing process. Furthermore, the environmental impact can be reduced in the manufacture of the reducing catalyst used in the process of manufacturing ammonium nitrate, and the resulting residue can be effectively used in cement manufacturing, making it possible to form a circulation cycle that is excellent in reducing the environmental impact and is suitable for cement factories, etc.
[0021] 1 is a flow chart showing an example of an outline of a method for producing ammonium nitrate using nitrogen dioxide in a cement exhaust gas according to the present invention.
[0022] The present invention will be described below by way of preferred examples with reference to FIGS. 1 and 2, but is not limited thereto.
[0023] The method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas of the present invention comprises: a nitrogen dioxide recovery step (1) of contacting nitrogen dioxide in the cement exhaust gas with water to absorb the nitrogen dioxide into the water and recover the nitrogen dioxide as a nitrate / nitrite nitrogen-containing liquid; a reduction reaction step (2) of contacting reduced iron and magnetite with all or a part of the nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) under acidic conditions to produce iron hydroxide and ammonia; an ammonia recovery step (3) of distilling and vaporizing the ammonia produced in the reduction reaction step (2) using waste heat gas from the cement production process to recover it; and a solid-liquid separation step (4) of separating the remainder after recovering ammonia in the ammonia recovery step (3) and separating the iron hydroxide from the reduction reaction step (2) that has undergone the ammonia recovery step (3) and the remaining unused nitrate / nitrite nitrogen. The method for producing ammonium nitrate utilizing nitrogen dioxide in cement exhaust gas includes: a neutralization step (5) in which the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4) and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) are brought into contact with ammonia vaporized and recovered in the ammonia recovery step (3) to prepare ammonium nitrate; and a catalyst production step (7) in which the magnetite used in the reduction reaction step (2) is prepared by reacting iron sulfate with an aqueous sodium hydroxide solution to produce magnetite and an aqueous sodium sulfate solution, subjecting the resulting sodium sulfate solution to solid-liquid separation, separating the sodium hydroxide and sodium hydroxide by electrodialysis, and recycling the resulting sodium hydroxide for use in preparing magnetite to be reacted with the iron sulfate.
[0024] As shown in Figure 1, cement is generally produced in a cement factory through a raw material crushing process in which raw materials are crushed, a clinker burning process in which the crushed raw materials are burned to produce cement clinker, and a cement finishing process in which the cement clinker is crushed and mixed with gypsum.
[0025] Cement clinker is produced by calcining fuel at a calcination temperature of approximately 1300 to 1500°C in a cement kiln, where cement raw materials are calcined. From the perspective of effective waste utilization, waste materials such as household garbage, sewage sludge, waste acid and alkali, waste plastics, dried sludge, waste clay, wood chips, recycled oil, ASR, and PKS are burned as fuel, and the resulting heat source is used as the heat source for the cement clinker calcination process. Nitrogen-containing waste materials, such as coal ash, general incineration ash, construction soil, cinders, sludge, foundry sand, steelmaking dust, and slowly cooled slag, can also be used as cement raw materials.
[0026] Here, the exhaust gas refers to the exhaust gas discharged when these waste materials are burned, and includes, for example, dust such as cement dust used in the clinker burning process and CO 2 The term "NOx recovery process" refers to a gas containing a large amount of NOx, etc. Exhaust gas contains various types of dust, and the dust in the exhaust gas is recovered, for example, by an electrostatic precipitator, and the exhaust gas is cooled, for example, to about 30°C. The amount of NOx in the cooled exhaust gas is, for example, 300 to 400 ppm. In the present invention, by recovering NOx in the exhaust gas in the NOx recovery process (1) described below, for example, if the amount of NOx contained in the exhaust gas before the NOx recovery process is 350 ppm, it is possible to reduce the amount of NOx contained in the exhaust after the application of the NOx recovery process (1) to 28 ppm.
[0027] The exhaust gas, such as combustion gas emitted from a cement manufacturing process, is cooled after dust has been collected, for example, cooled to 40°C or less, and is introduced into a NOx (nitrogen dioxide, etc.) recovery step (1) where it is brought into contact with water. The NOx recovery step (1) is a recovery step that utilizes a NOx absorption and removal process using water.
[0028] Specifically, the exhaust gas cooled after dust recovery is brought into contact with water, and NOx contained in the exhaust gas is absorbed by the water, and the NOx is recovered as a nitrate / nitrite nitrogen-containing liquid. For example, heat can be indirectly recovered using a heat exchanger, and NOx can be reacted with water to convert NOx into nitrate / nitrite nitrogen.
[0029] The NOx in the cement exhaust gas to be recovered has an equilibrium relationship as shown in the following formula (A): 2NO → 2NO 2 ←→N 2 O 4 ...(A) Also, as shown in the following reaction formula (B), NO 2 When it comes into contact with water, it produces nitrate and nitrite nitrogen. 2 +H 2 O → HNO 3 +HNO 2 ... (I) (N 2 O 4 +H 2 O → HNO 3 +HNO 2 )
[0030] The ((HNO 3 +HNO 2 The NOx absorption liquid / NOx-containing liquid volume ratio is not particularly limited, but may be, for example, 0.01 to 0.15, and preferably 0.01 to 0.08. As described above, the NOx recovery process uses water as the NOx absorption liquid and does not use chemicals such as chemicals, so that costs can be kept low and the NOx-containing liquid can be recovered and reused as a nitric acid solution.
[0031] Furthermore, in the present invention, there is no need to provide a separate step for oxidizing nitrous acid to nitric acid, such as a step of converting nitrous acid to nitric acid using ozone or the like, and both nitrous acid and nitric acid can be reduced in the subsequent reduction step (2), which can lead to a shortening of the reaction process.
[0032] Next, all or a portion of the nitrate / nitrite nitrogen-containing liquid produced in the NOx recovery step (1) is introduced into the subsequent reduction reaction step (2) (arrows in the main production step in FIG. 1 ) for treatment. The nitrate / nitrite nitrogen-containing liquid introduced into the reduction reaction step (2) can be all or a portion of the nitrate / nitrite nitrogen-containing liquid produced in the NOx recovery step (1). If only a portion of the nitrate / nitrite nitrogen-containing liquid is introduced, the remaining nitrate / nitrite nitrogen-containing liquid can be introduced into the neutralization step (5) described below. As an example, of the nitrate / nitrite nitrogen-containing liquid produced in the NOx recovery step (1), about 40 vol%, preferably 38 vol%, and more preferably 35 vol% of the nitrate / nitrite nitrogen-containing liquid can be separated and introduced into the neutralization step (5) described below without being introduced into the subsequent reduction reaction step (2).
[0033] The reduction reaction step (2) is a step in which a catalyst having a reducing action is brought into contact with a nitrate / nitrite nitrogen-containing liquid under acidic conditions, for example, by adding sulfuric acid produced by bipolar membrane electrodialysis in the catalyst production step (7) described below, to cause a reaction, thereby converting the nitrate / nitrite nitrogen in the nitrate / nitrite nitrogen-containing liquid into ammonia.
[0034] As the catalyst having a reducing action used in the reduction reaction step (2), commercially available magnetic materials capable of reducing nitrate nitrogen to ammonia can be used, for example, spinel ferrite (R 1 -Fe 2 O 4 ), hexagonal ferrite (R 2 -Fe 12 O 19 ), garnet ferrite (R 3 -Fe 5 O 12 ), R 3 -MB, etc. In the above structural formula, R 1 , R 2 , R 3 , M can be exemplified as follows: 1 :Fe, Mn, Ni, Cu, Zn, R 2 :Ba, Sr, Pb, R 3:Sc, Y, La, Ce, Pr, Nd, Sm, Gd, Eu, Tb, Dy, Ho, Er, Tm, Yb, Lu, M: Fe, Fe-Co
[0035] In particular, as a catalyst having a reducing action, among magnetic materials, magnetite and / or reduced iron powder (e.g., JIP 300R, manufactured by JFE Steel Corporation) can be suitably used. Any commercially available magnetite or reduced iron powder can be used as the magnetite or reduced iron powder, or magnetite prepared by effectively utilizing waste heat gas discharged from a cement factory, for example. In the present invention, it is desirable to use magnetite prepared by utilizing exhaust gas from such a cement factory (catalyst production step (7)). Here, waste heat gas is different from exhaust gas and means hot gas such as air that does not contain cement dust, etc., heated outside the cement kiln in the cement production process.
[0036] Magnetite, the reducing catalyst used in the present invention, can be prepared by reacting iron sulfate with sodium hydroxide (reaction formulas (d) to (e)) and subjecting the resulting magnetite and aqueous sodium sulfate solution to solid-liquid separation (catalyst production step (7)). Commercially available iron sulfate can be used, and examples thereof include industrial ferrous iron monohydrate (manufactured by Sakai Chemical Industry Co., Ltd.). Commercially available sodium hydroxide can also be used, but in the present invention, for example, sodium hydroxide obtained by bipolar membrane electrodialysis (reaction formula (c)) described below is used. Sulfuric acid can be used in the reduction reaction step (2) as described above. Na 2 SO 4 +2H 2 O → 2NaOH + H 2 SO 4 ···(cormorant)
[0037] Bipolar membrane electrodialysis involves electrodialysis of an aqueous solution containing sodium sulfate (see reaction formula (C) above) to produce sulfuric acid and sodium hydroxide. The sodium sulfate produced in the magnetite preparation process, as shown in reaction formula (D) below, is circulated during bipolar membrane electrodialysis. The sulfuric acid obtained by bipolar membrane electrodialysis can be used to create acidic conditions in the reduction reaction step (2), and / or can be reacted with unreacted sodium hydroxide after magnetite preparation to produce sodium sulfate, which can then be recycled for use in the electrodialysis process together with the aqueous sodium sulfate solution obtained through solid-liquid separation in the catalyst production step (7). The sodium hydroxide obtained by bipolar membrane electrodialysis is used to prepare magnetite, which is reacted with iron sulfate as shown in reaction formula (D) below. Thus, sodium hydroxide can be recycled and utilized in the catalyst production step (7).
[0038] Magnetite is produced by the ferrite method shown in the following reaction formulas (d) to (e) using iron sulfate and sodium hydroxide produced by the above reaction formula (c). This production process involves using waste heat gas, for example, to react iron sulfate with sodium hydroxide at 200 to 250°C, for example, at a pH of 8 to 13. FeSO 4 +2NaOH→Fe(OH) 2 +Na 2 SO 4 ... (D) 3Fe(OH) 2 →Fe 3 O 4 +H 2 +2H 2 O (E) The obtained magnetite is used as a catalyst having a reducing action in the reduction reaction step (2).
[0039] Furthermore, when unreacted sodium hydroxide remains after magnetite is prepared by the above reaction formulas (d) to (e), sulfuric acid obtained by the above bipolar membrane electrodialysis (reaction formula (c)) is added to the unreacted sodium hydroxide to cause a reaction, thereby producing sodium sulfate, and the sodium sulfate can be subjected to bipolar membrane electrodialysis treatment together with the sodium sulfate produced by the above reaction formula (d).
[0040] The following can be given as an example of an outline of the manufacturing process of magnetite: Iron sulfate is added to an aqueous sodium hydroxide solution, and the precipitate produced by the above reaction formulas (d) to (e) is filtered using a filter press, and then the water is evaporated and the product is dried using waste heat gas from a cement factory, for example, at 70°C for about 30 minutes, and then the product is pulverized in a coarse pulverizer such as a hammer mill, recovered by magnetic separation, and sieved using a vibrating screen to reduce the particle size to 0.5 mm to 2 mm, thereby preparing pulverized magnetite.
[0041] The chemical composition of the obtained magnetite can be analyzed by component analysis using a fluorescent X-ray analyzer (PRIMUS IV, manufactured by Rigaku Corporation). For example, it is possible to prepare a pulverized magnetite product having the following composition: Fe: 68.3%, O: 28.6%, C: 1.2%, Mn: 1.1%, Al: 0.3%, S: 0.3%, Si: 0.2%.
[0042] In addition, the obtained magnetite pulverized product was further pulverized, and then a powder X-ray diffractometer (manufactured by PANalytical, X'Part Powder) was used, and the measurement conditions were: measurement range: 2θ = 10 to 70 °, step size: 0.017 °, scan speed: 0.1012 ° / s, voltage: 45 kV, current: 40 mA. X-ray diffraction measurement was performed to confirm that it was magnetite. Specifically, for the X-ray diffraction profile, it was confirmed that it was magnetite using crystal structure analysis software (manufactured by PANalytical, X'Part High Score Plus version 2.1b) provided in the powder X-ray diffractometer.
[0043] Furthermore, the hydrogen produced by the above reactions (d) to (e) can be recycled and reused as a heat source for the burner when preparing cement.
[0044] In the reduction reaction step (2), as described above, nitrate and nitrite nitrogen are reacted with a catalyst having a reducing effect, such as magnetite, produced in the catalyst production step (7) under acidic conditions to produce ammonia. For example, a catalyst having a reducing effect, such as magnetite, is added to the nitrate and nitrite nitrogen-containing liquid introduced from the NOx recovery step, and a reduction reaction is carried out under acidic conditions to convert all or part of the nitrate and nitrite nitrogen into ammonia. As an example, "part" refers to converting 90% by volume, preferably 93% by volume, of the nitrate and nitrite nitrogen to ammonia. In addition, to efficiently proceed with the reduction reaction, it is desirable to maintain an equilibrium state so that oxygen does not enter the nitrate and nitrite nitrogen-containing liquid. For example, the reduction reaction may be carried out in a sealed state or in an inert atmosphere.
[0045] As one example, for example, magnetite obtained in the catalyst production step (7) and reduced iron are added in a mass ratio of 2:1 to a nitrate / nitrite nitrogen-containing liquid introduced into the reduction reaction step, and the pH of the nitrate / nitrite nitrogen-containing liquid is adjusted to 1.0 to 6.0, preferably 1.0 to 4.0, more preferably 1.0 to 2.0, at room temperature under acidic conditions, and the reduction reaction is carried out with stirring for, for example, 1 to 10 hours, preferably 3 to 10 hours. The reduction reaction is represented by the following formulas (f) to (g): HNO 3 +4Fe+5H 2 O → NH 3 + 4Fe(OH) 2 ...(Ka) HNO 2 +3Fe+4H 2 O → NH 3 + 3Fe(OH) 2 ···(tree)
[0046] Any additive can be used as the additive for promoting the reduction reactions of the above reaction formulas (f) to (g) under acidic conditions, as long as it enables the pH of the aqueous solution to be adjusted to an acidic state and does not affect the treatment of the present invention. Examples of such additives include hydrochloric acid, sulfuric acid, and nitric acid. Nitric acid is preferably used, and sulfuric acid obtained by electrodialysis in the above catalyst production step (7) can be used, which is desirable from the viewpoint of recycling.
[0047] More preferably, during the reduction treatment, continuous measurement is carried out with an ORP electrode, and the ORP is adjusted to be −500 mV to −200 mV, preferably −500 mV to −400 mV, so that the reduction treatment progresses effectively.
[0048] Next, the ammonia and nitrate / nitrite nitrogen-containing liquid obtained in the reduction reaction step (2) is introduced into the ammonia recovery step (3) (arrows in the main production step in Figure 1). Next, the ammonia and nitrate / nitrite nitrogen-containing liquid is adjusted to pH 8.0 to 14.0, preferably pH 10.0 to 14.0, with a base, and then distilled using waste heat gas from a cement factory, and the ammonia is heated and vaporized and recovered (ammonia recovery step (3)). The waste heat gas used to heat and concentrate the ammonium nitrate prepared in the neutralization step (5) below to precipitate crystals can also be circulated and used to vaporize ammonia in the ammonia recovery step (3). To recover ammonia by heating and vaporizing it, for example, a stripping method is used, and the heating temperature is preferably 50 to 70°C.
[0049] A portion of the vaporized ammonia is introduced into the neutralization step (5) described below, and the remaining vaporized ammonia can be used to improve the purity of ammonium nitrate by reacting it with nitrate and nitrite nitrogen remaining in ammonium nitrate obtained by heating and concentrating the ammonium nitrate obtained in the neutralization step (5) described below.
[0050] Any basic agent can be used as the basic agent as long as it enables the pH of the aqueous solution to be adjusted to a basic state and does not affect the treatment of the present invention. Examples of the basic agent include sodium hydroxide, calcium hydroxide, potassium hydroxide, and magnesium hydroxide. Preferably, sodium hydroxide can be used. For example, sodium hydroxide obtained by electrodialysis in the catalyst production step (7) can be used, which is desirable from the viewpoint of recycling.
[0051] Furthermore, the iron hydroxide (II), which is the residue produced by the above reaction formulas (f) and (g), is introduced into the ammonia recovery step (3) together with ammonia and a nitrate / nitrite nitrogen-containing liquid. After passing through the ammonia recovery step (3), the residue is subjected to solid-liquid separation, and the iron hydroxide from the reduction reaction step (2) and the unused nitrate / nitrite nitrogen residue are separated (solid-liquid separation step (4)). The iron hydroxide separated in the solid-liquid separation step (4) becomes iron hydroxide oxide when exposed to air (reaction formula (h) below), and this iron hydroxide oxide can be reused as a cement raw material. 4Fe(OH) 2 +O 2 →4FeO(OH)+2H 2 O... (Q)
[0052] Next, a portion of the ammonia recovered by vaporization in the ammonia recovery step (3), the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4), and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) are introduced into a neutralization step (5) for catalytic reaction to produce ammonium nitrate (e.g., 78% purity). In the neutralization step (5), a solution containing the produced ammonium nitrate and excess nitrate / nitrite nitrogen not used in the production of ammonium nitrate is obtained. For example, the reaction between nitrate nitrogen and ammonia is represented by the following formula (I), and an ammonium nitrate solution with a concentration of, for example, about 78% can be produced. HNO 3 +NH 3 →NH 4 NO 3 ... (Ke)
[0053] The ammonium nitrate-containing liquid thus obtained is heated and distilled using waste heat gas as needed, for example, by adjusting the temperature to 170 to 180 ° C. to obtain a suspension (for example, 98% purity) in which ammonium nitrate is concentrated, and the remaining nitrate and nitrite nitrogen (HNO 3 +HNO 2 ) is evaporated. 3 and HNO 2 It is desirable to recycle the remaining ammonia gas that was not introduced into the neutralization step (5) to the concentrated ammonium nitrate-containing suspension. By adding such ammonia gas, the suspension (concentrated ammonium nitrate) becomes weakly alkaline, and the nitrate and nitrite nitrogen (HNO ) remaining in the concentrated ammonium nitrate is dissolved in the concentrated ammonium nitrate. 3 +HNO 2 The neutralization reaction with ammonium nitrate allows the purity of the ammonium nitrate to be increased (for example, to about 100%), and the ammonium nitrate crystals are precipitated and isolated by cooling. Preferably, this treatment is carried out before the granulation step (6) described below.
[0054] The waste heat gas can be used to concentrate and precipitate ammonium nitrate, and then to vaporize ammonia in the ammonia recovery step (3).
[0055] Next, after isolating the ammonium nitrate, granular ammonium nitrate is produced using any commercially available granulator (granulation step (6)). In the granulation step (6), solid ammonium nitrate is mixed with light oil or the like, and can be used to produce, for example, explosives, blasting materials, etc.
[0056] The treatment method of the present invention makes it possible to convert nitrogen dioxide contained in cement exhaust gas into ammonium nitrate and utilize it, thereby sufficiently reducing the nitrogen dioxide content in the cement exhaust gas and effectively carrying out denitration. It also reduces the environmental burden in the production of reducing catalysts used in the process of producing ammonium nitrate, makes it possible to utilize waste heat gas during cement production, and allows the residue obtained by the treatment method of the present invention to be effectively used in cement production, thereby forming an environmentally friendly circulation cycle.
[0057] The nitrogen dioxide in the waste gas discharged from a cement factory can be denitrified with high efficiency, forming an environmentally friendly circulation cycle, and therefore the treatment method of the present invention can be effectively applied to cement factories producing cement.
Claims
1. A nitrogen dioxide recovery process (1) in which nitrogen dioxide in a cement exhaust gas is brought into contact with water to absorb the nitrogen dioxide into the water and recover the nitrogen dioxide as a nitrate / nitrite nitrogen-containing liquid; a reduction reaction process (2) in which reduced iron and magnetite are brought into contact with all or a part of the nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery process (1) under acidic conditions to produce iron hydroxide and ammonia; an ammonia recovery process (3) in which the ammonia produced in the reduction reaction process (2) is distilled and vaporized using waste heat gas from a cement manufacturing process and recovered; and a solid-liquid separation process (4) in which the remainder after the ammonia recovery in the ammonia recovery process (3) is subjected to solid-liquid separation to separate the iron hydroxide from the reduction reaction process (2) that has been subjected to the ammonia recovery process (3) and the unused remainder nitrate / nitrite nitrogen. A neutralization step (5) of preparing ammonium nitrate by contacting the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4) and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) with ammonia vaporized and recovered in the ammonia recovery step (3); and a catalyst production step (7) of preparing magnetite to be used in the reduction reaction step (2) by solid-liquid separation of magnetite and an aqueous sodium sulfate solution produced by reacting iron sulfate with an aqueous sodium hydroxide solution, separating the aqueous sodium sulfate solution into sodium hydroxide and sulfuric acid by electrodialysis, and circulating the obtained sodium hydroxide for use in preparing magnetite to be reacted with the iron sulfate.
2. A method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, as described in claim 1, characterized in that the sulfuric acid obtained in the catalyst production process (7) is used to make the reduction reaction process (2) acidic, and / or is reacted with unreacted sodium hydroxide remaining after the preparation of magnetite to produce sodium sulfate, which is recycled for electrodialysis together with the aqueous sodium sulfate solution obtained by solid-liquid separation in the catalyst production process (7).
3. A method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas as claimed in claim 1 or 2, characterized in that the hydrogen generated during the preparation of magnetite in the catalyst production process (7) is recycled and reused as a combustion raw material during the production of cement.
4. A method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, comprising the steps of: (1) preparing ammonium nitrate in the neutralization step (5); and (2) producing ammonium nitrate in the form of ammonium nitrate.
5. A method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, as set forth in claim 1 or 2, characterized in that the iron hydroxide separated in the solid-liquid separation step (4) is converted into iron oxide hydroxide by exposure to air, and the iron oxide hydroxide is used as a cement raw material.
6. A method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas as described in claim 1, characterized in that the ammonium nitrate prepared in the neutralization step (5) is contained in a liquid containing ammonium nitrate and nitrate / nitrite nitrogen, the liquid is heated and distilled at 170-180°C using waste heat gas to concentrate ammonium nitrate, and the remaining nitrate / nitrite nitrogen is vaporized and circulated to the neutralization step (5), a portion of the ammonia vaporized in the ammonia recovery step (3) is added to the concentrated ammonium nitrate to react with unreacted nitrate / nitrite nitrogen mixed in the concentrated ammonium nitrate to improve the purity of ammonium nitrate, and crystallized ammonium nitrate is obtained by cooling.
Citation Information
Patent Citations
Nitrogen oxide absorbent, regeneration method therefor and nitrogen oxide recovery method
JP2003175315A
Exhaust gas treatment methods
JP5100432B2
JP1973022396B1
Process and device for detoxifying ammonia
JP1998165766A
Recovery system for nitric acid and carbon dioxide