Cell culturing container

The cell culture container with a specific resin composition and surface characteristics effectively suppresses protein denaturation, enhancing cell adhesion and proliferation by maintaining a β-sheet structure, addressing the limitations of conventional polymer supports.

WO2024203650A1PCT designated stage expired Publication Date: 2024-10-03ZEON CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/010834
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-19
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Conventional cell culture containers made of polymer supports face issues with protein denaturation on the culture surface, which affects cell adhesion and proliferation.

Method used

A cell culture container with a culture surface made from a resin composition that has an infrared absorption spectrum with a specific band area ratio of 10% or more in the amide I region, and an X-ray photoelectron spectroscopy spectrum with a particular abundance ratio of oxygen-containing functional groups, which suppresses protein denaturation.

Benefits of technology

The solution effectively reduces protein denaturation on the culture surface, enhancing cell adhesion and proliferation by maintaining a structure rich in β-sheet structure, thereby improving protein adsorption and cell culture conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JPOXMLDOC01-APPB-T000001
    Figure JPOXMLDOC01-APPB-T000001
  • Figure JPOXMLDOC01-APPB-T000002
    Figure JPOXMLDOC01-APPB-T000002
Patent Text Reader

Abstract

The purpose of the present invention is to provide a cell culturing container that can suppress denaturing of protein attached to a culturing surface. A cell culturing container according to the present invention is provided with a culturing surface formed by using a resin composition containing a resin. In an infrared absorption spectrum of a recombinant human fibronectin fragment attached to the culturing surface, the area of a band having a peak at a vibration frequency of 1680 cm-1 obtained through band decomposition performed for a vibration frequency range of 1600-1700 cm-1 <sp / > is 10% or more when the total area of all bands obtained through the band decomposition is defined as 100%.
Need to check novelty before this filing date? Find Prior Art

Description

cell culture container

[0001] The present invention relates to a cell culture vessel.

[0002] In the field of life sciences, research using animal somatic cells such as iPS cells is actively conducted. Cells are placed in cell culture containers such as dishes or well plates along with culture medium (a liquid for culturing cells that contains nutrients necessary for the cells, such as serum), and cultured at approximately 37°C for a period of several days to several weeks.

[0003] Cultured cells are broadly divided into adherent cells and suspension cells. Adherent cells grow attached to the surface of the cell culture vessel via binding between integrins present on the cell membrane surface and extracellular matrix proteins such as fibronectin attached to the surface of the cell culture vessel.

[0004] Therefore, in recent years, attempts have been made to improve the polymer materials used in cell culture vessels in order to improve the cell adhesion of the vessels. For example, Patent Document 1 discloses a polymer support comprising a contact surface and an interior, the contact surface having a roughness quantified by a predetermined parameter. According to Patent Document 1, the contact surface of the polymer support exhibits improved cell adhesion, cell proliferation, and cell recovery rate.

[0005] Special table 2018-537556 publication

[0006] However, the inventors' investigations have revealed that cell culture vessels made of the above-mentioned conventional polymer supports have the problem that proteins attached to the culture surface of the cell culture vessel are easily denatured.

[0007] Therefore, an object of the present invention is to provide a cell culture vessel that can suppress the denaturation of proteins attached to the culture surface.

[0008] The present inventors have conducted extensive research to solve the above-mentioned problems. As a result, the present inventors have discovered a method for producing a culture surface made of a resin composition, which is characterized by an infrared absorption spectrum of a recombinant human fibronectin fragment in the amide I region (1600 cm) of the infrared absorption spectrum. -1 ~1700cm-1 ) is decomposed into bands, the total area of ​​all bands is 1680 cm -1 The present inventors have newly discovered that the denaturation of proteins attached to the culture surface can be effectively suppressed by using a cell culture vessel in which the ratio of the area of ​​the band having a peak at or above a predetermined value, and have completed the present invention.

[0009] That is, the present invention has an object to advantageously solve the above-mentioned problems, and provides the following cell culture vessels (1) to (4) according to the present invention.

[0010] (1) A cell culture vessel having a culture surface made of a resin composition containing a resin, wherein the recombinant human fibronectin fragment attached to the culture surface has an infrared absorption spectrum of a frequency of 1600 cm -1 More than 1700cm -1 The vibration frequency 1680 cm obtained by band decomposition in the following region -1 The cell culture vessel has a culture surface made of a resin composition containing a resin, and the area of ​​a band having a peak at a frequency of 1600 cm in the infrared absorption spectrum of a recombinant human fibronectin fragment attached to the culture surface is 10% or more, where the total area of ​​all bands obtained by the band resolution is 100%. -1 More than 1700cm -1 When the following region is decomposed into bands, 1680 cm -1 The ratio of the area of ​​the band having a peak at 1680 cm -1The cell culture vessel having a band area ratio (ratio of band area to total area of ​​the culture vessel) equal to or greater than the above value can effectively suppress the denaturation of proteins attached to the culture surface. In the present invention, the "culture surface" refers to the surface of the cell culture vessel with which cells are in contact during culture. In the present invention, the "recombinant human fibronectin fragment" refers to a recombinant protein (recombinant human fibronectin CH-296) containing three functional domains of human fibronectin: the cell adhesion domain (C-domain), the heparin-binding domain (H-domain), and the CS-1 site. "Recombinant human fibronectin CH-296" is commercially available as Rectronectin (registered trademark, manufactured by Takara Bio Inc.), and its amino acid sequence is disclosed as SEQ ID NO: 18 in WO 2018 / 021543. In the present invention, the "infrared absorption spectrum of the recombinant human fibronectin fragment attached to the culture surface" can be measured using the method described in the Examples of this specification. Furthermore, in the present invention, "1680 cm -1 The "band area ratio" can be calculated according to the method described in the Examples of this specification.

[0011] (2) The X-ray photoelectron spectroscopy spectrum of the culture surface is π-π * The cell culture vessel according to (1) above, wherein the ratio of the total amount of C═O groups and O—C═O groups to the amount of C—O groups on the culture surface, as determined based on the X-ray photoelectron spectroscopy spectrum, is 0.45 or less. The X-ray photoelectron spectroscopy spectrum (hereinafter sometimes abbreviated as "XPS spectrum") on the culture surface is π-π * A cell culture vessel that does not have a peak derived from bonding and in which the ratio of the total amount of C=O groups and O-C=O groups to the amount of C-O groups on the culture surface (hereinafter sometimes abbreviated as "abundance ratio of oxygen-containing functional groups") is equal to or less than the above value can further suppress denaturation of proteins attached to the culture surface. In the present invention, the "XPS spectrum of the culture surface" can be measured using the method described in the Examples of this specification. In addition, in the present invention, the "π-π *The "peak derived from the bond" is observed in the vicinity of 291 eV in the XPS spectrum (π-π * In the present invention, the "abundance ratio of oxygen-containing functional groups" can be calculated according to the method described in the examples of this specification.

[0012] (3) The cell culture vessel according to (1) or (2) above, wherein the ratio of the amount of oxygen element to the amount of carbon element on the culture surface is 2.0% or more, as determined based on an X-ray photoelectron spectroscopy spectrum. A cell culture vessel having a ratio of the amount of oxygen element to the amount of carbon element on the culture surface equal to or greater than this value can enhance the adsorption of proteins to the culture surface. In the present invention, the "ratio of the amount of oxygen element to the amount of carbon element on the culture surface" can be measured according to the method described in the Examples of this specification.

[0013] (4) The cell culture vessel according to any one of (1) to (3), wherein the resin contains a ring-opening polymer hydrogenated product of a norbornene-based monomer. A cell culture vessel having a culture surface made of a resin composition containing a ring-opening polymer hydrogenated product of a norbornene-based monomer can further suppress denaturation of proteins attached to the culture surface.

[0014] According to the present invention, it is possible to provide a cell culture vessel capable of suppressing the denaturation of proteins attached to the culture surface.

[0015] Hereinafter, embodiments of the present invention will be described in detail. Here, the cell culture vessel of the present invention is not particularly limited as long as it is intended to culture cells therein. Specific examples of the cell culture vessel of the present invention include dishes, plates, microchannel chips, bags, tubes, scaffolds, cups, jar fermenters, etc.

[0016] The cells contained in the cell culture vessel are not particularly limited and can be selected arbitrarily depending on the purpose. Specific examples include adherent cells such as CHO cells, VERO cells, NIH3T3 cells, HEK293 cells, nerve cells differentiated from human iPS cells, cardiomyocytes, and liver cells. One type of cell may be used alone, or two or more types may be used in combination at any ratio.

[0017] (Cell Culture Vessel) In the cell culture vessel of the present invention, at least the culture surface is formed using a resin composition containing a resin. For example, when the cell culture vessel of the present invention is a multi-well plate, it is sufficient that the portion of the well inner wall surface that comes into contact with the cells being cultured is formed using the resin composition. Furthermore, when the cell culture vessel of the present invention is a bag having a laminated structure made of multiple films, it is sufficient that the innermost film (the inner surface of the bag) is formed using the resin composition. Alternatively, the entire cell culture vessel may be formed using the resin composition. Here, the cell culture vessel of the present invention is a cell culture vessel that is formed using the resin composition at 1680 cm in the infrared absorption spectrum of a recombinant human fibronectin fragment attached to the culture surface. -1 The band area ratio is 10% or more.

[0018] The cell culture vessel of the present invention has a 1680 cm of recombinant human fibronectin fragment attached to the culture surface. -1 Since the area ratio of the bands is 10% or more, the denaturation of proteins attached to the culture surface is suppressed. Although the reason why the above effects are obtained by using such a cell culture vessel of the present invention is not clear, it is presumed to be as follows.

[0019] First, the cell culture vessel of the present invention has a frequency of 1600 cm in the infrared absorption spectrum of the recombinant human fibronectin fragment attached to the culture surface. -1 More than 1700cm -1 When the following region is decomposed into bands, the frequency for the total area of ​​all bands is 1680 cm -1 The ratio of the area of ​​the band having a peak at 1680 cm -1In the infrared absorption spectrum of a protein, the band area ratio (area ratio of the band) is 10% or more. -1 This region is called the amide I region and is known to reflect the secondary structure of the protein. In the infrared absorption spectrum of the recombinant human fibronectin fragment, -1 The present inventors have newly discovered through their investigation that the band having a peak at 1680 cm is assigned to a β-sheet structure. -1 The "band area ratio" can be considered as a value related to the β-sheet content (%) in the recombinant human fibronectin fragment molecule. -1 When the band area ratio is 10% or more, it can be said that the recombinant human fibronectin fragment attached to the culture surface maintains a structure rich in β-sheet structure, i.e., a structure close to the native state. In other words, the cell culture vessel of the present invention maintains the 1680 cm -1 Since the area ratio of the band is 10% or more, it is considered that the denaturation of proteins attached to the culture surface is sufficiently suppressed. Therefore, by using the cell culture vessel of the present invention, the denaturation of proteins attached to the culture surface can be suppressed.

[0020] <Resin Composition> The resin composition used to form the culture surface of the cell culture vessel of the present invention contains a resin, and optionally further contains components other than the resin (other components).

[0021] <<Resin>> Here, the resin contained in the resin composition is not particularly limited, and examples thereof include cycloolefin polymers, polyethylene terephthalate (PET), polystyrene (PS), acrylic resins, polycarbonates, and hydrogenated styrene-conjugated diene block copolymers. These resins may be used alone or in combination of two or more in any ratio. Among the above-mentioned resins, it is preferable to use cycloolefin polymers, and it is more preferable to use both cycloolefin polymers and hydrogenated styrene-conjugated diene block copolymers, from the viewpoint of further suppressing denaturation of proteins attached to the culture surface.

[0022] [Cycloolefin Polymer] Here, a cycloolefin polymer is a resin having an alicyclic structure in the main chain and / or side chain. Examples of the alicyclic structure of a cycloolefin polymer include a saturated cyclic hydrocarbon (cycloalkane) structure and an unsaturated cyclic hydrocarbon (cycloalkene) structure. Specific examples of cycloolefin polymers include norbornene polymers, monocyclic olefin polymers, cyclic conjugated diene polymers, vinyl alicyclic hydrocarbon polymers, and hydrogenated versions of these. Among these, norbornene polymers and hydrogenated versions thereof are preferred from the viewpoint of further suppressing denaturation of proteins attached to the culture surface.

[0023] —Norbornene-Based Polymer— Examples of norbornene-based polymers include ring-opening polymers of monomers having a norbornene structure, or ring-opening polymers of a monomer having a norbornene structure and an arbitrary monomer, or hydrogenated products thereof; addition polymers of monomers having a norbornene structure, or addition polymers of a monomer having a norbornene structure and an arbitrary monomer, or hydrogenated products thereof; and the like.

[0024] Here, the norbornene-based polymer is a polymer containing monomer units having a norbornene skeleton in an amount of 50% by mass or more, preferably 60% by mass or more, based on the total monomer units constituting the norbornene-based polymer. More specifically, norbornene-based polymers are obtained by polymerizing norbornene-based monomers, which are monomers having a norbornene skeleton, and are roughly classified into those obtained by ring-opening polymerization and those obtained by addition polymerization.

[0025] Examples of products obtained by ring-opening polymerization include ring-opening polymers of norbornene-based monomers, ring-opening polymers of norbornene-based monomers and other monomers copolymerizable therewith, and hydrogenated products thereof. Examples of products obtained by addition polymerization include addition polymers of norbornene-based monomers and addition polymers of norbornene-based monomers and other monomers copolymerizable therewith. Among these, hydrogenated ring-opening polymers of norbornene-based monomers are preferred from the viewpoint of further suppressing denaturation of proteins attached to the culture surface.

[0026] Norbornene-based monomers that can be used to synthesize norbornene-based polymers include bicyclo[2.2.1]hept-2-ene (commonly known as norbornene), 5-methyl-bicyclo[2.2.1]hept-2-ene, 5,5-dimethyl-bicyclo[2.2.1]hept-2-ene, 5-ethyl-bicyclo[2.2.1]hept-2-ene, 5-ethylidene-bicyclo[2.2.1]hept-2-ene, and 5-methyl-bicyclo[2.2.1]hept-2-ene. Bicyclic monomers such as hept-2-ene, 5-vinyl-bicyclo[2.2.1]hept-2-ene, 5-propenylbicyclo[2.2.1]hept-2-ene, 5-methoxycarbonyl-bicyclo[2.2.1]hept-2-ene, 5-cyanobicyclo[2.2.1]hept-2-ene, 5-methyl-5-methoxycarbonyl-bicyclo[2.2.1]hept-2-ene; tricyclo[4.3.0]hept-2-ene; 1,6 .1 2,5 ] tricyclic monomers such as deca-3,7-diene (commonly known as dicyclopentadiene), 2-methyldicyclopentadiene, 2,3-dimethyldicyclopentadiene, and 2,3-dihydroxydicyclopentadiene; tetracyclo[4.4.0.1 2,5 .1 7,10]-3-dodecene (tetracyclododecene), tetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8-methyltetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8-ethyltetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8-ethylidenetetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8,9-dimethyltetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8-ethyl-9-methyltetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8-ethylidene-9-methyltetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 8-methyl-8-carboxymethyltetracyclo[4.4.0.1 2,5 .1 7,10 ]-3-dodecene, 7,8-benzotricyclo[4.3.0.1 2,5 ] tetracyclic monomers such as dec-3-ene (commonly known as methanotetrahydrofluorene; also known as 1,4-methano-1,4,4a,9a-tetrahydrofluorene), 1,4-methano-8-methyl-1,4,4a,9a-tetrahydrofluorene, 1,4-methano-8-chloro-1,4,4a,9a-tetrahydrofluorene, and 1,4-methano-8-bromo-1,4,4a,9a-tetrahydrofluorene; and the like.

[0027] Other monomers capable of ring-opening copolymerization with norbornene-based monomers include monocyclic cycloolefin-based monomers such as cyclohexene, cycloheptene, cyclooctene, 1,4-cyclohexadiene, 1,5-cyclooctadiene, 1,5-cyclodecadiene, 1,5,9-cyclododecatriene, and 1,5,9,13-cyclohexadecatetraene. These monomers may have one or more substituents. Examples of the substituents include alkyl groups, alkylene groups, aryl groups, silyl groups, alkoxycarbonyl groups, and alkylidene groups.

[0028] Other monomers that can be addition copolymerized with norbornene-based monomers include α-olefin-based monomers having 2 to 20 carbon atoms, such as ethylene, propylene, 1-butene, 1-pentene, and 1-hexene; cyclobutene, cyclopentene, cyclohexene, cyclooctene, tetracyclo[9.2.1.0] 2,10 .0 3,8 ] Cycloolefin-based monomers such as tetradeca-3,5,7,12-tetraene (also called 3a,5,6,7a-tetrahydro-4,7-methano-1H-indene); non-conjugated diene-based monomers such as 1,4-hexadiene, 4-methyl-1,4-hexadiene, 5-methyl-1,4-hexadiene, and 1,7-octadiene; and the like.

[0029] Among these, the other monomer capable of addition copolymerization with the norbornene monomer is preferably an α-olefin monomer, and more preferably ethylene. These monomers may have one or more substituents. Examples of the substituents include an alkyl group, an alkylene group, an aryl group, a silyl group, an alkoxycarbonyl group, and an alkylidene group.

[0030] Ring-opening polymers of norbornene-based monomers, or ring-opening polymers of norbornene-based monomers and other monomers copolymerizable therewith, can be obtained by polymerizing the monomer components in the presence of a known ring-opening polymerization catalyst. Examples of ring-opening polymerization catalysts that can be used include catalysts comprising a halide of a metal such as ruthenium or osmium, a nitrate or an acetylacetone compound, and a reducing agent, or catalysts comprising a halide or acetylacetone compound of a metal such as titanium, zirconium, tungsten, or molybdenum, and an organoaluminum compound. Hydrogenated ring-opening polymers of norbornene-based monomers can usually be obtained by adding a known hydrogenation catalyst containing a transition metal such as nickel or palladium to a polymerization solution of the ring-opening polymer and hydrogenating the carbon-carbon unsaturated bonds.

[0031] The addition polymer of a norbornene-based monomer or an addition polymer of a norbornene-based monomer and another monomer copolymerizable therewith can be obtained by polymerizing the monomer components in the presence of a known addition polymerization catalyst, such as a catalyst comprising a titanium, zirconium, or vanadium compound and an organoaluminum compound.

[0032] -Monocyclic olefin polymer- As the monocyclic olefin polymer, for example, an addition polymer of a monocyclic olefin monomer such as cyclohexene, cycloheptene, or cyclooctene can be used.

[0033] -Cyclic Conjugated Diene Polymer- Examples of the cyclic conjugated diene polymer that can be used include polymers obtained by 1,2- or 1,4-addition polymerization of cyclic conjugated diene monomers such as cyclopentadiene and cyclohexadiene, and hydrogenated products thereof.

[0034] —Vinyl alicyclic hydrocarbon polymer— Examples of vinyl alicyclic hydrocarbon polymers include polymers of vinyl alicyclic hydrocarbon monomers such as vinylcyclohexene and vinylcyclohexane, and hydrogenated products thereof. The vinyl alicyclic hydrocarbon polymer may also be a copolymer of these monomers with other copolymerizable monomers. In the present invention, a “hydrogenated styrene-conjugated diene block copolymer” is not included in the “vinyl alicyclic hydrocarbon polymer.”

[0035] There are no particular restrictions on the molecular weight of the cycloolefin polymer, but the weight average molecular weight, calculated as polyisoprene, measured by gel permeation chromatography of a cyclohexane solution (or a toluene solution if the polymer is not soluble) is usually 5,000 or more, preferably 5,000 to 500,000, more preferably 8,000 to 200,000, and even more preferably 10,000 to 100,000. When the weight average molecular weight is within this range, a high level of balance between mechanical strength and moldability is achieved, which is preferable.

[0036] The content of the cycloolefin polymer in the resin is preferably 99.50 parts by mass or more, more preferably 99.70 parts by mass or more, and even more preferably 99.80 parts by mass or more, and is preferably 99.99 parts by mass or less, and more preferably 99.98 parts by mass or less, relative to 100 parts by mass of the total amount of the resin. If the content of the cycloolefin polymer is within the above range relative to 100 parts by mass of the resin, denaturation of proteins attached to the culture surface can be further suppressed, and the adsorption of proteins to the culture surface can be increased.

[0037] [Hydrogenated Styrene-Conjugated Diene Block Copolymer] The hydrogenated styrene-conjugated diene block copolymer is a hydrogenated styrene block-conjugated diene block copolymer having a styrene block mainly composed of repeating units derived from a styrene-based monomer and a diene block mainly composed of repeating units derived from a conjugated diene monomer.

[0038] Here, as the hydrogenated styrene-conjugated diene block copolymer, for example, a commercially available product can be used. Alternatively, the hydrogenated styrene-conjugated diene block copolymer may be obtained by obtaining a styrene-conjugated diene block copolymer according to a known method, and then hydrogenating the carbon-carbon unsaturated bonds in the main chain and side chain of the conjugated diene block of the obtained styrene-conjugated diene block copolymer. The method for hydrogenating the unsaturated bonds and the reaction form are not particularly limited, and may be performed according to a known method.

[0039] The content of the hydrogenated styrene-conjugated diene block copolymer in the resin is preferably 0.01 parts by mass or more, more preferably 0.02 parts by mass or more, and preferably 0.5 parts by mass or less, more preferably 0.3 parts by mass or less, and even more preferably 0.2 parts by mass or less, relative to 100 parts by mass of the total amount of the resin. When the content of the hydrogenated styrene-conjugated diene block copolymer is within the above range relative to 100 parts by mass of the resin, denaturation of proteins attached to the culture surface can be further suppressed, and the adsorption of proteins to the culture surface can be increased.

[0040] <<Other Components>> The resin composition used to form the culture surface of the cell culture vessel of the present invention can further contain components other than the resins described above (other components). Examples of other components include compounding agents commonly used in thermoplastic resin materials, such as soft polymers, antioxidants, ultraviolet absorbers, light stabilizers, near-infrared absorbers, release agents, colorants such as dyes and pigments, plasticizers, antistatic agents, and fluorescent brighteners. Note that the other components may be used alone or in combination of two or more in any ratio.

[0041] Examples of antioxidants include phenol-based antioxidants, organic phosphite-based antioxidants, and sulfur-based antioxidants. Examples of ultraviolet absorbers include benzophenone-based ultraviolet absorbers and benzotriazole-based ultraviolet absorbers. Examples of light stabilizers include hindered amine-based stabilizers. Among these, from the viewpoints of further suppressing denaturation of proteins attached to the culture surface and increasing the adsorption of proteins to the culture surface, it is preferable that the resin composition contains an antioxidant.

[0042] The content of the antioxidant in the resin composition is preferably 0.05 parts by mass or more, more preferably 0.1 parts by mass or more, and preferably 2 parts by mass or less, more preferably 1 part by mass or less, and even more preferably 0.5 parts by mass or less, per 100 parts by mass of resin. If the content of the antioxidant is within the above range per 100 parts by mass of resin, denaturation of proteins attached to the culture surface can be further suppressed and the adsorption of proteins to the culture surface can be increased.

[0043] The glass transition temperature of the resin composition may be appropriately selected depending on the intended use, but is usually 50 to 300°C, preferably 80 to 280°C, more preferably 90 to 250°C, and even more preferably 90 to 200°C. When the glass transition temperature is within this range, heat resistance and moldability are well balanced, which is preferable. In the present invention, the glass transition temperature of the resin composition is measured in accordance with JIS K 7121.

[0044] <<Method for Preparing Resin Composition>> The mixing method for obtaining a resin composition containing the above-mentioned resin and optionally other components is not particularly limited, and can be performed using, for example, a known melt kneader such as a single-screw extruder, a twin-screw extruder, a Banbury mixer, a kneader, a feeder rudder, etc. After mixing, the mixture can be extruded into a rod shape according to a conventional method and cut to an appropriate length with a strand cutter to form pellets.

[0045] <1680cm -1 The cell culture vessel of the present invention has an infrared absorption spectrum of the recombinant human fibronectin fragment attached to the culture surface at a frequency of 1600 cm -1 More than 1700cm -1 When the following region is decomposed into bands, the frequency for the total area of ​​all bands is 1680 cm -1 The ratio of the area of ​​the band having a peak at 1680 cm -1 The band area ratio must be 10% or more, and 1680 cm -1 The area ratio of the band is preferably 11% or more, more preferably 12% or more, and even more preferably 13% or more. -1 If the band area ratio is less than 10%, the degree of denaturation of the protein attached to the culture surface increases. -1 The upper limit of the area ratio of the band is not particularly limited, and can be, for example, 30% or less, or 25% or less. -1 The area ratio of the bands can be adjusted by, for example, changing the type of resin in the resin composition used to form the culture surface, whether or not the culture surface is subjected to a surface treatment, the type and conditions of the surface treatment, etc. Specifically, by not performing a surface treatment, or by shortening the treatment time when a heat treatment is performed as the surface treatment, the area ratio of the bands can be adjusted by, for example, changing the type of resin in the resin composition used to form the culture surface, whether or not the culture surface is subjected to a surface treatment, etc. -1 The area ratio of the band can be increased.

[0046] <π-π * Peaks derived from binding> In order to further suppress the denaturation of proteins attached to the culture surface, the cell culture vessel of the present invention has an XPS spectrum of π-π *It is preferable that there is no peak due to bonding. * The presence or absence of a peak due to bonding can be adjusted, for example, by changing the type of resin in the resin composition used to form the culture surface. Specifically, by using a resin that does not have an aromatic ring, * An XPS spectrum can be obtained that does not have peaks derived from bonds.

[0047] <Ratio of Oxygen-Containing Functional Groups> Furthermore, in the cell culture vessel of the present invention, the ratio of the total amount of C═O groups and O—C═O groups to the amount of C—O groups on the culture surface (ratio of oxygen-containing functional groups) is preferably 0.45 or less, more preferably 0.40 or less, even more preferably 0.35 or less, and particularly preferably 0.33 or less. When the ratio of oxygen-containing functional groups on the culture surface is 0.45 or less, denaturation of proteins attached to the culture surface can be further suppressed. The lower limit of the ratio of oxygen-containing functional groups on the culture surface is not particularly limited and can be, for example, 0.05 or more, or 0.10 or more. The ratio of oxygen-containing functional groups on the culture surface can be adjusted by, for example, changing the type of resin in the resin composition used to form the culture surface, the molding conditions when forming the culture surface from the resin composition, whether or not the culture surface is surface-treated, and the type and conditions of the surface treatment. Specifically, the ratio of oxygen-containing functional groups on the culture surface can be reduced by not performing a surface treatment, or by shortening the treatment time if heat treatment is performed as the surface treatment.

[0048] <Ratio of Oxygen Element Amount to Carbon Element Amount> In the cell culture vessel of the present invention, the ratio of oxygen element amount to carbon element amount on the culture surface is preferably 2.0% or more, more preferably 2.5% or more, even more preferably 3.0% or more, preferably 10.0% or less, more preferably 7.5% or less, even more preferably 5.0% or less, even more preferably 3.9% or less, and particularly preferably 2.6% or less. When the ratio of oxygen element amount to carbon element amount on the culture surface is 2.0% or more, the adsorption of proteins to the culture surface can be enhanced. On the other hand, when the ratio of oxygen element amount to carbon element amount on the culture surface is 10.0% or less, the denaturation of proteins attached to the culture surface can be further suppressed. The ratio of oxygen element amount to carbon element amount on the culture surface can be adjusted by, for example, changing the type of resin in the resin composition used to form the culture surface, the molding conditions when forming the culture surface from the resin composition, whether or not the culture surface is subjected to a surface treatment, and the type and conditions of the surface treatment. Specifically, the ratio of the amount of oxygen element to the amount of carbon element on the culture surface can be reduced by not performing surface treatment, or by shortening the treatment time if heat treatment is used as the surface treatment.

[0049] <Protein Adsorption Rate> The cell culture vessel of the present invention preferably has a protein adsorption rate of 60% or more on the culture surface, more preferably 65% ​​or more, and even more preferably 70% or more. A protein adsorption rate of 60% or more on the culture surface ensures good protein adsorption on the culture surface. The upper limit of the protein adsorption rate on the culture surface is not particularly limited, and can be, for example, 100% or less, or 90% or less. In the present invention, the protein adsorption rate on the culture surface can be measured using the method described in the Examples section of the present specification. The protein adsorption rate on the culture surface can be adjusted, for example, by changing the type of resin in the resin composition used to form the culture surface, the molding conditions when forming the culture surface from the resin composition, whether or not the culture surface is subjected to a surface treatment, and the type and conditions of the surface treatment.

[0050] <Method for manufacturing cell culture vessel> The method for manufacturing the cell culture vessel of the present invention is not particularly limited. For example, the cell culture vessel of the present invention can be manufactured through a step of molding a resin composition containing the above-mentioned resin and, optionally, other components, to obtain a culture surface (molding step), and a step of optionally performing a surface treatment on the culture surface (surface treatment step).

[0051] <<Molding Step>> Here, the method for molding the resin composition is not particularly limited and can be appropriately selected from known molding methods depending on the desired shape of the culture surface. Examples of such known molding methods include extrusion molding, injection molding, inflation molding, blow molding, extrusion blow molding, injection blow molding, press molding, vacuum molding, powder slush molding, calendar molding, foam molding, thermoforming, etc. Among these, injection molding is preferably used as the molding method.

[0052] When the culture surface is formed by injection molding, the temperature of the mold used for injection molding (hereinafter sometimes simply referred to as "mold temperature") is preferably (Tg-40)°C or higher and preferably (Tg-20)°C or lower, where Tg (°C) is the glass transition temperature of the resin composition. If the mold temperature is within the above-mentioned range, denaturation of proteins attached to the culture surface can be further suppressed and the adsorption of proteins to the culture surface can be increased. Furthermore, when the culture surface is formed by injection molding, the temperature of the cylinder provided in the injection molding machine (hereinafter sometimes simply referred to as "cylinder temperature") is preferably (Tg+120)°C or higher and preferably (Tg+170)°C or lower, where Tg (°C) is the glass transition temperature of the resin composition. If the cylinder temperature is within the above-mentioned range, denaturation of proteins attached to the culture surface can be further suppressed and the adsorption of proteins to the culture surface can be increased.

[0053] <<Surface Treatment Step>> The type of surface treatment applied to the culture surface is not particularly limited and can be appropriately selected from known surface treatment methods. Such known surface treatment methods include heat treatment, plasma treatment, vacuum ultraviolet treatment, corona treatment, ozone treatment, etc. Among these, heat treatment is preferred from the viewpoint of further suppressing denaturation of proteins attached to the culture surface.

[0054] Here, from the viewpoint of further suppressing denaturation of proteins attached to the culture surface, the treatment temperature in the heat treatment is preferably (Tg-10)°C or lower, and more preferably (Tg-15)°C or lower, where Tg (°C) is the glass transition temperature of the resin composition. The lower limit of the treatment temperature in the heat treatment is not particularly limited, and can be, for example, (Tg-40)°C or higher, or (Tg-30)°C or higher.

[0055] The treatment time for the heat treatment may be appropriately set depending on the treatment temperature. From the viewpoint of further suppressing the denaturation of proteins attached to the culture surface, the treatment time for the heat treatment is preferably 50 hours or less, more preferably 40 hours or less. The lower limit of the treatment time for the heat treatment is not particularly limited, and may be, for example, 10 hours or more, or 20 hours or more.

[0056] <<Other Steps>> The cell culture vessel of the present invention may be produced optionally through steps (other steps) other than the molding step and the surface treatment step described above. Examples of other steps include a step of pre-drying the resin composition prior to the molding step (pre-drying step), a step of assembling the cell culture vessel by combining the culture surface with other members (assembly step), a step of sterilizing the cell culture vessel (sterilization step), etc.

[0057] The present invention will be specifically described below based on examples, but the present invention is not limited to these examples. In the following description, "%" and "parts" that represent amounts are based on mass unless otherwise specified. In the examples and comparative examples, the ratio of the amount of oxygen element to the amount of carbon element, the abundance ratio of oxygen-containing functional groups, and π-π * The presence or absence of a peak due to binding, and the 1680 cm of the recombinant human fibronectin fragment attached to the culture surface -1 The band area ratio and protein adsorption rate were evaluated by the following method.

[0058] <X-ray photoelectron spectroscopy measurements> The bottom surfaces (culture surfaces) of the dishes prepared in the examples and comparative examples were used as the measurement targets. X-ray photoelectron spectroscopy (XPS) was used to measure soft X-rays in an ultra-vacuum, and photoelectrons emitted from the surface were detected with an analyzer to obtain elemental information on the culture surface from the binding energy of bound electrons in the material. The measurement conditions were as follows: Apparatus: ULVAC-PHI, product name "Quantera SXM" Excitation X-rays: Monochromated AlKα 12 X-ray diameter: 200 μm; Photoelectron detection angle: 45°; Horizontal axis correction: The C1s main peak was set to 284.6 eV. [Ratio of oxygen to carbon] The elemental species present on the culture surface were identified using XPS wide scan mode (measurement range: 0 eV to 1100 eV). The peak area of ​​each identified element was integrated and corrected by the elemental sensitivity coefficient, after which the ratio (%) of oxygen to carbon on the culture surface was calculated. [Ratio of oxygen-containing functional groups] The binding energy range in which the C1s main peak appears was scanned with high resolution using XPS narrow scan mode (measurement range: 275 eV to 300 eV). The obtained spectrum was peak-split, and the peaks corresponding to C-O, C=O, and O-C=O were identified based on the individual peak positions (binding energy values). Then, the area of ​​the peak corresponding to C-O was designated as S1, the area of ​​the peak corresponding to C=O as S2, and the area of ​​the peak corresponding to O-C=O as S3, and the ratio of the total amount of C=O groups and O-C=O groups to the amount of C-O groups on the culture surface (abundance ratio of oxygen-containing functional groups) was calculated using the following formula: Abundance ratio of oxygen-containing functional groups = (S2 + S3) / S1 [π - π * Presence or absence of peaks derived from bonds] Using the narrow scan mode of XPS, the binding energy range where the C1s main peak appears was scanned with high resolution (measurement range: 275 eV to 300 eV). In the obtained spectrum, a π-π peak was observed around 291 eV. * It was confirmed whether a peak derived from a bond was observed. -1Band Area Ratio> [1. Protein Treatment] RetroNectin (manufactured by Takara Bio Inc., model number "T100B") was dissolved in heavy water (DO, manufactured by Kanto Chemical Co., Ltd.) to a concentration of 10 μg / mL to obtain a protein solution. 2.5 mL of the protein solution was placed in a dish (35 mm diameter) prepared in the Examples and Comparative Examples and kept at 37°C for 45 minutes. Next, the protein solution in the dish was removed, and 3 mL of heavy water was added to wash the dish. Thereafter, the washing water in the dish was removed, and 3 mL of fresh heavy water was added for further washing. After performing the above washing procedure three times, the washing water was removed, and the dish was dried in an atmospheric environment until no liquid was visible. [2. FT-IR Measurement and Band Resolution] The bottom surface (culture surface) of the dish after the protein treatment was attached to the germanium prism of the ATR attachment of an FT-IR device (manufactured by Thermo Fisher Scientific, product name "Niclet 6700"), and infrared absorption spectrum measurement was performed. The software "OMNIC" manufactured by Thermo Fisher Scientific was used for measurement and analysis. The amide I region (1600-1700 cm) of the obtained measured spectrum was analyzed. -1 ) was second-derivatively obtained to obtain the second-derivative spectrum. Next, based on the position of the negative peak (valley) in the second-derivative spectrum, the amide I region (1600-1700 cm) of the measured spectrum was determined. -1 ) was subjected to band resolution. At this time, one of the bands used for band resolution was -1 The total area of ​​all bands obtained by band resolution was determined as SA, 1680 cm -1 The area of ​​the band having a peak at 1680 cm is defined as SB, and the area of ​​the band having a peak at 1680 cm is calculated by the following formula: -1 The band area ratio was calculated. -1 Band area ratio (%) = (SB / SA) x 100 The measurement and analysis conditions were as follows: Measurement method: ATR method Number of accumulations: 32 Resolution: 16 cm -1Background correction: before sample measurement; Spectral intensity: absorbance; Function (distribution function) representing band shape: Gaussian function; Peak detection sensitivity: low sensitivity; Noise level in peak fitting: 0.01; Baseline correction in peak fitting: linear (linear) interpolation. <Protein adsorption rate> [1. Protein treatment] RetroNectin (manufactured by Takara Bio Inc., model number "T100B") was dissolved in phosphate-buffered saline (PBS) solution (manufactured by Fujifilm Wako Pure Chemical Industries, Ltd., PBS(-)) to a concentration of 10 μg / mL to obtain a protein solution. 2.5 mL of the protein solution was placed in a dish (35 mm diameter) prepared in the Examples and Comparative Examples and maintained at 37°C for 45 minutes. Next, the protein solution in the dish was removed, and the dish was washed once with 3.0 mL of sterile water. 2 mL of colloidal gold solution (manufactured by Bio-Rad, model number "#1706527") was then added to the dish and maintained at 25°C for 45 minutes. Next, the gold colloid solution in the dish was removed, and 3 mL of sterile water was added to wash the dish. The washing water in the dish was then removed, and 3 mL of sterile water was added again to wash the dish. Finally, the washing water was removed, and the dish was dried in an air environment until no liquid was visible. [2. Ruthenium Staining Treatment] Ruthenium tetroxide and the dish after the protein treatment were placed in a glass desiccator, and ruthenium staining was performed for 30 minutes in a gas-phase environment. [3. SEM Photography] A field of view near the center of the bottom surface (culture surface) of the dish after the ruthenium staining treatment was observed at a magnification of 50,000 times using a field emission scanning electron microscope (FE-SEM) (manufactured by Hitachi High-Tech Corporation, product name "SU8220") under conditions of secondary electron imaging, accelerating voltage of 0.7 kV, and scanning electron microscope (SEM) observation images were obtained. [4. Image analysis] The SEM observation images were read using image processing software ImageJ (open source) and the image data was converted to 8-bit data. The ruthenium-stained areas (gray) and gold colloid areas (white) were designated as bright areas, and areas other than the ruthenium-stained areas and gold colloid areas (black) were designated as dark areas, and the proportion (%) of bright areas among all pixels in the SEM observation image was taken as the protein adsorption rate.A higher protein adsorption rate indicates a cell culture vessel with better protein adsorption. A protein adsorption rate of 60% or higher indicates that the protein adsorption capacity of the culture surface is sufficiently ensured.

[0059] Example 1 <Preparation of Cell Culture Vessel (Dish)> [Pre-drying and Molding] A resin composition having the following composition (glass transition temperature (Tg): 163°C, hereinafter referred to as "COP1") was vacuum dried (pre-drying) under conditions of an ambient temperature of (Tg-20)°C and a drying time of 4 hours. - Composition of COP1 - Cycloolefin polymer (hydrogenated ring-opening polymer of norbornene-based monomer, weight average molecular weight (Mw): 34,000) 99.9 parts Antioxidant 0.2 parts Hydrogenated styrene-conjugated diene block copolymer 0.1 parts This pre-dried COP1 was used to perform injection molding under the following conditions to prepare a dish (diameter 35 mm) as a cell culture vessel. - Injection molding conditions - Injection molding machine: FANUC, product name "Roboshot α-S50iA" Mold: Mold for dish (diameter 35 mm) Cylinder temperature: (Tg + 140) ° C Mold temperature: (Tg - 30) ° C Injection pressure: 70 MPa For the bottom surface (culture surface) of the obtained dish, the ratio of the amount of oxygen element to the amount of carbon element, the abundance ratio of oxygen-containing functional groups, and π-π * The presence or absence of a peak due to binding, the 1680 cm of the recombinant human fibronectin fragment -1 The band area ratio and protein adsorption rate were measured, and the results are shown in Table 1.

[0060] Example 2 <Preparation of cell culture vessel> [Preparation and molding] Preparation and molding were performed in the same manner as in Example 1 to prepare a dish (diameter 35 mm). [Heat treatment] The dish (diameter 35 mm) obtained as described above was subjected to heat treatment at 140°C for 24 hours. The bottom surface (culture surface) of the dish after heat treatment was then evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0061] (Example 3) A cell culture vessel was produced in the same manner as in Example 2, except that the heat treatment time was changed from 24 hours to 30 hours. Then, the bottom surface (culture surface) of the heat-treated dish was evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0062] Example 4 A cell culture vessel was produced in the same manner as in Example 1, except that a resin composition having the following composition (Tg: 136°C, hereinafter referred to as "COP2") was used instead of COP1. Evaluation was then carried out in the same manner as in Example 1. The results are shown in Table 1. - Composition of COP2 - Cycloolefin polymer (hydrogenated ring-opening polymer of norbornene-based monomer, Mw: 35,000) 99.9 parts Antioxidant 0.135 parts Hydrogenated styrene-conjugated diene block copolymer 0.1 parts

[0063] (Example 5) <Preparation of cell culture vessel> [Preparation and molding] Preparation and molding were performed in the same manner as in Example 4 to prepare a dish (diameter 35 mm). [Heat treatment] The dish (diameter 35 mm) obtained as described above was subjected to heat treatment at 115°C for 30 hours. The bottom surface (culture surface) of the dish after heat treatment was then evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0064] (Example 6) A cell culture vessel was produced in the same manner as in Example 1, except that a resin composition having the following composition (Tg: 100°C, hereinafter referred to as "COP3") was used instead of COP1. Evaluation was then carried out in the same manner as in Example 1. The results are shown in Table 1. - Composition of COP3 - Cycloolefin polymer (hydrogenated ring-opening polymer of norbornene-based monomer, Mw: 29,400) 99.98 parts Antioxidant 0.48 parts Hydrogenated styrene-conjugated diene block copolymer 0.02 parts

[0065] (Example 7) <Preparation of cell culture vessel> [Preparation and molding] Preparation and molding were performed in the same manner as in Example 6 to prepare a dish (diameter 35 mm). [Heat treatment] The dish (diameter 35 mm) obtained as described above was subjected to heat treatment at 80°C for 30 hours. The bottom surface (culture surface) of the dish after heat treatment was then evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0066] (Example 8) A cell culture vessel was produced in the same manner as in Example 1, except that a resin composition containing an addition copolymer of norbornene and ethylene (Tg: 138°C, hereinafter referred to as "COC1") was used instead of COP1. Evaluation was then carried out in the same manner as in Example 1. The results are shown in Table 2.

[0067] Example 9 <Preparation of Cell Culture Vessel> [Preparation and Molding] Preparation and molding were performed in the same manner as in Example 8 to prepare a dish (diameter 35 mm). [Heat Treatment] The dish (diameter 35 mm) obtained as described above was subjected to heat treatment at 115°C for 30 hours. The bottom surface (culture surface) of the dish after heat treatment was then evaluated in the same manner as in Example 1. The results are shown in Table 2.

[0068] Comparative Example 1 <Preparation of Cell Culture Vessel> [Preparation and Molding] Preparation and molding were performed in the same manner as in Example 1 to prepare a dish (diameter 35 mm). [Plasma Treatment] The dish (diameter 35 mm) obtained as described above was subjected to plasma treatment for 60 seconds at a voltage of 100 V and a vacuum of 200 Pa using a low-pressure plasma device (manufactured by Izumi Kogyo Co., Ltd.). The bottom surface (culture surface) of the dish after plasma treatment was then evaluated in the same manner as in Example 1. The results are shown in Table 2.

[0069] (Comparative Example 2) A cell culture vessel was produced in the same manner as in Example 7, except that the heat treatment time was changed from 30 hours to 96 hours. Then, the bottom surface (culture surface) of the heat-treated dish was evaluated in the same manner as in Example 1. The results are shown in Table 2.

[0070] (Comparative Example 3) A cell culture vessel was produced in the same manner as in Example 9, except that the heat treatment time was changed from 30 hours to 144 hours. Then, the bottom surface (culture surface) of the heat-treated dish was evaluated in the same manner as in Example 1. The results are shown in Table 2.

[0071] Comparative Example 4 <Preparation of Cell Culture Vessel> [Preparation and Molding] Preparation and molding were performed in the same manner as in Example 1, except that polystyrene (manufactured by Corning, product name "Falcon", Tg: 100°C) was used instead of COP1, to prepare a dish (diameter 35 mm). [Plasma Treatment] The dish (diameter 35 mm) obtained as described above was subjected to plasma treatment for 60 seconds using a low-pressure plasma device (manufactured by Izumi Kogyo Co., Ltd.) at a voltage of 100 V and a vacuum degree of 200 Pa. The bottom surface (culture surface) of the dish after plasma treatment was then evaluated in the same manner as in Example 1. The results are shown in Table 2.

[0072] In Tables 1 and 2 below, "PS" indicates polystyrene, "plasma" indicates plasma treatment, and "Tg" indicates glass transition temperature.

[0073]

[0074]

[0075] From Tables 1 and 2, the culture surface is made of a resin composition, and the 1680 cm -1 In Examples 1 to 9, which used cell culture vessels with band area ratios equal to or greater than a predetermined value, it can be seen that the denaturation of proteins attached to the culture surface was sufficiently suppressed. -1 It can be seen that in Comparative Examples 1 to 4, which used cell culture vessels in which the band area ratio was less than the predetermined value, the denaturation of proteins attached to the culture surface could not be sufficiently suppressed.

[0076] According to the present invention, it is possible to provide a cell culture vessel capable of suppressing the denaturation of proteins attached to the culture surface.

Claims

1. A cell culture vessel having a culture surface made of a resin composition containing a resin, wherein the recombinant human fibronectin fragment attached to the culture surface has an infrared absorption spectrum of a frequency of 1600 cm -1 More than 1700cm -1 The vibration frequency 1680 cm obtained by band decomposition in the following region -1 The area of ​​a band having a peak at is 10% or more, where the total area of ​​all bands obtained by the band resolution is 100%.

2. The X-ray photoelectron spectroscopy spectrum of the culture surface is π-π * The cell culture vessel according to claim 1, which has no peaks derived from bonds, and has a ratio of the total amount of C=O groups and O-C=O groups to the amount of C-O groups on the culture surface, based on the X-ray photoelectron spectroscopy spectrum, of 0.45 or less.

3. The cell culture vessel according to claim 1, wherein the ratio of the amount of oxygen element to the amount of carbon element on the culture surface, obtained based on an X-ray photoelectron spectroscopy spectrum, is 2.0% or more.

4. The cell culture vessel according to any one of claims 1 to 3, wherein the resin contains a ring-opening polymer hydride of a norbornene monomer.

Citation Information

Patent Citations

  • Method for promoting extracellular matrix production, method for culturing cells, and agent for promoting extracellular matrix production

    WO2017010533A1