Optical component, optical module comprising optical component, and production method for optical component

The optical component's innovative structure of a metal member, high melting point glass, low melting point glass, and light-transmitting member, with a plating layer, addresses the inefficiencies in conventional sealing methods by eliminating oxide film removal and enhancing bonding and airtightness, thus simplifying the manufacturing process and improving durability.

WO2024204573A1PCT designated stage expired Publication Date: 2024-10-03KYOCERA CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/012714
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Conventional methods for sealing a light-transmitting window to a metal cap body are inefficient due to the need to remove oxide films before applying corrosion-resistant plating, increasing the manufacturing process time.

Method used

An optical component comprising a metal member, a high melting point glass material, a low melting point glass material, and a light-transmitting member, where the high melting point glass is bonded to the metal member, and the low melting point glass is applied on top, allowing for direct bonding without forming an oxide film, and a plating layer surrounds the high melting point glass to prevent corrosion.

Benefits of technology

This configuration simplifies the manufacturing process by eliminating the need for oxide film removal and enhances bonding strength, while the low melting point glass provides superior airtightness and heat radiation properties, improving the sealing and durability of the optical component.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024012714_03102024_PF_FP_ABST
    Figure JP2024012714_03102024_PF_FP_ABST
Patent Text Reader

Abstract

An optical component (100) comprises a metal member (3), a first glass material (1), a second glass material (2), and a light-transmitting member (5). The metal member (3) has a first surface (31s), a second surface (32s), and a through hole (30). The second surface (32s) is positioned on the opposite side from the first surface (31s). The through hole (30) passes from the first surface (31s) to the second surface (32s). The first glass material (1) is positioned on the first surface (31s) and surrounds the through hole (30) as seen in plan view. The second glass material (2) is positioned on the first glass material (1) and surrounds the through hole (30) as seen in plan view. The light-transmitting member (5) is positioned on the second glass material (2) and overlaps the through hole (30) as seen in plan view. The light-transmitting member (5) is translucent. The softening temperature t1 of the first glass material (1) is higher than the softening temperature t2 of the second glass material (2).
Need to check novelty before this filing date? Find Prior Art

Description

Optical component, optical module including optical component, and method for manufacturing optical component

[0001] Optical component, optical module including optical component, and method for manufacturing optical component.

[0002] A conventional cap for a semiconductor device is described in, for example, Japanese Patent Application Laid-Open No. 2003-222999.

[0003] Japanese Patent Application Laid-Open No. 2006-73776

[0004] In one embodiment (1), the optical component includes a metal member, a first glass material, a second glass material, and a translucent member. The metal member has a first surface, a second surface, and a through hole. The second surface is located on the opposite side of the first surface. The through hole penetrates from the first surface to the second surface. The first glass material is located on the first surface and surrounds the through hole in a planar view. The second glass material is located on the first glass material and surrounds the through hole in a planar view. The translucent member is located on the second glass material and overlaps with the through hole in a planar view. The translucent member has translucency. A softening temperature t1 of the first glass material is higher than a softening temperature t2 of the second glass material.

[0005] In one embodiment (2), the optical component includes a metal member, a first glass material, a second glass material, and a translucent member. The metal member has a first surface, a second surface, and a through hole. The second surface is located opposite the first surface. The through hole penetrates from the first surface to the second surface. The first glass material is located on the first surface and surrounds the through hole in a plan view. The second glass material is located on the first glass material and surrounds the through hole in a plan view. The translucent member is located on the second glass material and overlaps with the through hole in a plan view. The translucent member is translucent. The mass percent concentration of the first metal oxide material in the first glass material is lower than the mass percent concentration of the first metal oxide material in the second glass material.

[0006] (3) In the optical component of (2) above, the first metal oxide material includes at least one of vanadium oxide (VO), ruthenium oxide (RuO), diphosphorus pentoxide (PO), arsenic trioxide (AsO), boron oxide (BO), tellurium oxide (TeO), bismuth oxide (BiO), zinc oxide (ZnO), tin oxide (SnO), and lead oxide (PbO).

[0007] (4) In the optical component according to any one of (1) to (3), the light-transmitting member has a side surface located on a plane intersecting the first surface, and the second glass material is in contact with at least a portion of the side surface.

[0008] (5) In the optical component according to any one of (1) to (4) above, a plating layer is located on the metal member, and the plating layer surrounds the first glass material.

[0009] (6) In the optical component of (5) above, the plating layer is in contact with the first glass material.

[0010] (7) In the optical component of (5) or (6) above, the material of the plating layer contains gold (Au).

[0011] (8) In the optical component according to any one of (5) to (7) above, when the portion where the metal member and the first glass material contact is defined as the first portion, the first portion is surrounded by the plating layer in plan view.

[0012] (9) In the optical component according to any one of (1) to (8) above, the softening temperature t0 of the light-transmitting member is lower than the softening temperature t1 of the first glass material and higher than the softening temperature t2 of the second glass material.

[0013] (10) In the optical component according to any one of (1) to (9) above, a reflection reducing layer is located on at least a portion of the surface of the light-transmitting member.

[0014] (11) In the optical component of (10) above, the reflection-reducing layer is located between the light-transmitting member and the second glass material.

[0015] (12) In the optical component according to any one of (1) to (11) above, the contact area between the first glass material and the metal member is larger than the contact area between the first glass material and the second glass material in a plan view.

[0016] (13) In the optical component according to any one of (1) to (12) above, the thickness of the first glass material is greater than the thickness of the second glass material.

[0017] (14) In the optical component according to any one of (1) to (13) above, the first glass material and the second glass material are cemented together.

[0018] (15) In the optical components of (1) to (14) above, when viewed in a cross section perpendicular to the first surface, the first point is the point on the surface of the first glass material that is farthest from the first surface, and the second point is the point on the surface of the second glass material that is farthest from the first surface, the distance from the first surface to the second point is equal to or greater than the distance from the first surface to the first point.

[0019] (16) The optical component according to any one of (1) to (13) above further includes a frame-shaped member. The frame-shaped member is positioned between the first glass material and the second glass material and surrounds the through-hole in a plan view.

[0020] (17) In the optical component of (16) above, the light-transmitting member is inclined with respect to the first surface.

[0021] (18) In the optical component of (16) or (17), the frame member is made of ceramic.

[0022] (19) In one embodiment, an optical module includes a substrate, an electronic component, and the optical component described above in (1) to (18). The electronic component is located on the substrate. The optical component is located on the substrate.

[0023] (20) In one embodiment, a method for manufacturing an optical component includes preparing a first member by applying a first glass material to a predetermined position on a metal member. Then, the first member is metal-plated. Then, a second glass material having a softening temperature lower than that of the first glass material is applied onto the first glass material. Then, a light-transmitting member is bonded to the second glass material.

[0024] FIG. 1 is a perspective view of an optical component according to an embodiment. FIG. 2 is an exploded perspective view of the optical component shown in FIG. 1. FIG. 3 is a plan view of the optical component shown in FIG. 1. FIG. 4 is a cross-sectional view of the optical component shown in FIG. 3 taken along line IV-IV. FIG. 5 is an enlarged view of a main part A shown in FIG. 4. FIG. 5 is an enlarged view of a main part B shown in FIG. 4. FIG. 6 is a perspective view of an optical component according to another embodiment. FIG. 7 is a plan view of the optical component shown in FIG. 7. FIG. 8 is a cross-sectional view of the optical component shown in FIG. 8 taken along line IX-IX. FIG. 9 is an exploded perspective view of an optical module according to an embodiment. FIG. 10 is a flowchart showing a method for manufacturing an optical component according to an embodiment. FIG. 11 is an exploded perspective view of an optical component according to another embodiment.

[0025] As in the invention described in Patent Document 1, a known method for sealing a light-transmitting window to a metal cap body involves heating the cap body to form an oxide film on the surface of the cap body, and then using this oxide film to seal the light-transmitting window with low-melting-point glass. In this method, in order to apply a corrosion-resistant plating such as nickel plating to the surface of the cap body, it is necessary to remove the unnecessary oxide film from the surface of the cap body before applying the plating to the cap body, which increases the number of manufacturing steps.

[0026] <Configuration of Optical Components> Several exemplary embodiments will be described below with reference to the drawings. For the sake of convenience, a Cartesian coordinate system xyz is defined for optical components. In this disclosure, planar view is a concept that includes planar perspective. Below, numerical ranges expressed using "to" include the numerical values ​​before and after the range as the lower and upper limits, respectively.

[0027] As shown in FIGS. 1 to 6, in one embodiment, the optical component 100 includes a metal member 3 , a first glass member 1 , a second glass member 2 , and a light-transmitting member 5 .

[0028] The metal member 3 has a first surface 31s, a second surface 32s, and a through hole 30. The second surface 32s is located on the opposite side of the first surface 31s. The through hole 30 penetrates from the first surface 31s to the second surface 32s. While either side of the metal member 3 may be defined as the first surface 31s, the surface on which the first glass material 1 is located may be defined as the first surface 31s. Alternatively, the surface opposite a first light-transmitting surface 51s of the light-transmitting member 5 (described later) in the z direction may be defined as the first surface 31s.

[0029] The metal member 3 may have a protruding portion that protrudes annularly around the through hole 30, and in this case, the first surface 31s may be located on the protruding portion.

[0030] The material of the metal member 3 may be, for example, a metal material such as iron, copper, nickel, chromium, cobalt, molybdenum, or tungsten, or may be an alloy material that combines two or more of the above-mentioned metal materials, such as an iron-nickel alloy or an iron-cobalt-nickel alloy.

[0031] 2, the metal member 3 may be a box-shaped member having a concave cross section with a space continuous with the through-hole 30, or may be a flat plate-shaped member, or may be an annular member. The metal member 3 is, for example, a cube or rectangular parallelepiped, and is 0.1 mm x 0.1 mm x 0.1 mm to 50 mm x 50 mm x 50 mm. When the metal member 3 is a box-shaped member, the first surface 31s may be the inner surface of the box-shaped member. In other words, in this case, the translucent member 5, which will be described later, is located inside the box-shaped member.

[0032] The through hole 30 may have a square shape, a circular shape including an ellipse, or a rectangular shape with rounded corners in a plan view. The through hole 30 can be formed by subjecting the metal member 3 to a known drilling process such as drilling, blasting, or laser processing.

[0033] As shown in Fig. 3 , the first glass material 1 is located on the first surface 31s and surrounds the through hole 30 in a plan view. In one embodiment, the first glass material 1 surrounds the entire outer edge of the through hole 30, but the first glass material 1 does not need to surround the entire outer edge of the through hole 30. In other words, the first glass material 1 does not need to be completely annular, and may have a portion that is interrupted. The first glass material 1 may be in contact with the outer edge of the through hole 30 in a plan view, or may be separated from it.

[0034] An annular buffer member may be located between the first glass material 1 and the metal member 3. The buffer member may be made of a metal material, for example, the same metal material as the metal member 3 or a different metal material. The presence of the buffer member reduces the possibility of damage to the optical component 100 due to differences in the thermal expansion coefficients of the metal member 3 and the first glass material 1 or the second glass material 2.

[0035] The material of the first glass material 1 is, for example, silica glass containing silicon dioxide (SiO2) as the main component. Here, the term "main component" refers to a mass percent concentration of 50% or more. The first glass material 1 may also be a so-called high-melting-point glass.

[0036] When forming the first glass material 1 on the first surface 31s of the metal member 3, the first glass material 1 and the metal member 3 may react with each other to form an oxide film partially at the contact points between the first glass material 1 and the metal member 3. This improves the bonding strength between the first glass material 1 and the metal member 3. Furthermore, the step of forming an oxide film on the metal member 3 can be omitted.

[0037] As shown in FIG. 3 , the second glass material 2 is positioned on the first glass material 1 and surrounds the through hole 30 in a plan view. In one embodiment, the second glass material 2 surrounds the entire outer edge of the through hole 30; however, the second glass material 2 does not need to surround the entire outer edge of the through hole 30. The material of the second glass material 2 may include, for example, vanadium pentoxide (VO), tellurium dioxide (TeO), barium oxide (BaO), zinc oxide (ZnO), and zirconium phosphate (OPZr). Alternatively, the material of the second glass material 2 may be silica glass doped with impurities such as phosphorus or boron.

[0038] The second glass material 2 may also be so-called low-melting-point glass. Specifically, low-melting-point glass is amorphous or crystalline glass that softens, deforms, and flows at temperatures between 200°C and 600°C. Crystallizable glass refers to a composite of amorphous glass and crystalline glass. Examples of low-melting-point glass include borosilicate glass, barium borosilicate glass, zinc borate glass, barium borate glass, high-silicic glass, aluminophosphate glass, phosphate glass, zinc phosphate glass, alkali glass, bismuth silicate glass, bismuth borosilicate glass, bismuth zinc borate glass, lead borosilicate glass, lead borate glass, potassium lead glass, and crystalline lead glass. Low-melting-point glass has superior airtightness compared to resin-based adhesives.

[0039] Pb (lead)-free low-melting-point glass may be used as the material for the second glass material 2. Pb-free means that the lead content is 0.1 mass % or less (RoHS (Restriction of the use of certain hazardous substances in electrical and electronic equipment) regulation). Examples of Pb-free low-melting-point glass that can be used include borosilicate glass, barium borosilicate glass, zinc borate glass, barium borate glass, high-silica glass, aluminophosphate glass, phosphate glass, zinc phosphate glass, alkali glass, bismuth silicate glass, bismuth borosilicate glass, and bismuth zinc borate glass.

[0040] The light-transmitting member 5 is located on the second glass member 2 and overlaps with the through hole 30 in a plan view. The light-transmitting member 5 is light-transmitting. When the optical component 100 is used in an optical module 10, the light emitted from an electronic component 9 (e.g., a semiconductor laser) located inside the optical module 10 can be emitted to the outside of the optical module 10. When the electronic component 9 is a light-receiving element (e.g., a photodiode or a CMOS sensor), the light that has passed through the light-transmitting member 5 can be received by the electronic component 9.

[0041] The light-transmitting member 5 may be a flat plate as shown in FIG. 2 , a curved plate, or a sphere. The material of the light-transmitting member 5 may be resin or glass. More specifically, the material of the light-transmitting member 5 may be sapphire glass or borosilicate glass. Sapphire glass has superior strength and transmittance compared to borosilicate glass. Furthermore, borosilicate glass is easier to process and manufacture compared to sapphire glass. The light-transmitting member 5 may also have a structure in which transparent members are stacked in multiple layers. When the light-transmitting member 5 is made of glass, when the optical component 100 is used in the optical module 10, the electronic components 9 inside the optical module 10 can be more airtightly sealed. In one embodiment, the light-transmitting member 5 may be a lens. Here, the thickness of the light-transmitting member 5 (i.e., the dimension in the z direction) is, for example, 0.1 mm to 1 mm.

[0042] The light-transmitting member 5 does not necessarily overlap the entire through hole 30 in a plan view, and may overlap only a portion of the through hole 30. The light-transmitting member 5 may overlap the entire through hole 30 in a plan view. More specifically, as shown in FIG. 3 , the area of ​​the light-transmitting member 5 may be larger than the area of ​​the through hole 30. In this case, the possibility of the light-transmitting member 5 falling into the through hole 30 can be reduced, making it easier to stably position the light-transmitting member 5 on the first glass material 1 and the second glass material 2.

[0043] The softening temperature t1 of the first glass material 1 is higher than the softening temperature t2 of the second glass material 2. This configuration reduces the possibility that the first glass material 1 will soften or deform due to the temperature of the second glass material 2 when the second glass material 2 is heated and positioned on the first glass material 1. This allows the light-transmitting member 5 to be stably bonded onto the second glass material 2. This facilitates assembly of the optical component 100. Furthermore, because the first glass material 1 and the second glass material 2 are positioned in layers, when the optical component 100 is used in the optical module 10, heat generated by the electronic component 9 located inside the optical module 10 can be efficiently dissipated.

[0044] More specifically, the above-described configuration can be rephrased as follows: high-melting point glass (first glass material 1) is located on the metal member 3, and low-melting point glass (second glass material 2) is located on the high-melting point glass (first glass material 1).

[0045] In this disclosure, the softening temperature refers to the temperature at which each component begins to deform. When the first glass material 1 contains, by mass percent, 60% to 70% silicon dioxide (SiO2) and 20% to 30% boron oxide (BO3), the softening temperature t1 of the first glass material 1 is, for example, 650°C to 800°C. When the second glass material 2 contains, by mass percent, 30% to 35% vanadium oxide (VO5), 30% to 50% tellurium oxide (TeO2), and 15% to 35% zirconium phosphate (O16P4Zr3), the softening temperature t2 of the second glass material 2 is, for example, 300°C to 500°C.

[0046] 4 and 5 , a diffusion layer 12 may be located between the first glass material 1 and the second glass material 2. The diffusion layer 12 may be a portion where the first glass material 1 and the second glass material 2 are melted and mixed together. The presence of the diffusion layer 12 between the first glass material 1 and the second glass material 2 can improve the bonding strength between the first glass material 1 and the second glass material 2. Therefore, when the optical component 100 is used in an optical module 10, the electronic component 9 inside the optical module 10 can be more airtightly sealed.

[0047] A frame-shaped member 6 shaped to surround the through-hole 30 or a light-transmitting filter may be positioned between the first glass material 1 and the second glass material 2. FIG. 12 shows an exploded perspective view of the optical component 100 when the frame-shaped member 6 is positioned between the first glass material 1 and the second glass material 2. The frame-shaped member 6 may be made of a ceramic material such as alumina. When the frame-shaped member 6 made of a ceramic material is positioned between the first glass material 1 and the second glass material 2, the difference in thermal expansion between the first glass material 1 and the second glass material 2 can be alleviated. This reduces residual stress when the optical component 100 is assembled. Furthermore, alumina has higher rigidity than the metal material used for the metal member 3. This reduces the possibility of deformation or breakage of the light-transmitting member 5 due to thermal deformation, for example, when seam-welding the optical component 100 to the substrate 8 (described later). The filter may be, for example, a color filter or an IR (Infrared Rays) cut filter.

[0048] Here, when the frame member 6 is positioned between the first glass member 1 and the second glass member 2, the light-transmitting member 5 may be tilted with respect to the first surface 31s. More specifically, the first light-transmitting surface 51s and / or the second light-transmitting surface 52s of the light-transmitting member 5 may be tilted by approximately 3° to 15° with respect to the first surface 31s. This configuration reduces the possibility that light emitted from the electronic component 9 is reflected by the first surface 31s when passing through the light-transmitting member 5 and the reflected light strikes the electronic component 9. This reduces the possibility that the electronic component 9 will be deteriorated by the reflected light. As shown in FIG. 12 , the light-transmitting member 5 can be tilted with respect to the first surface 31s by tilting the surface of the frame member 6 facing the light-transmitting member 5.

[0049] More specifically, the first glass material 1 and the second glass material 2 are said to be bonded together when the above-mentioned frame-shaped member or translucent filter is not located between the first glass material 1 and the second glass material 2. Note that the term "bonded together" as used herein also refers to a state in which a diffusion layer 12 is located between the first glass material 1 and the second glass material 2.

[0050] The mass percent concentration (wt %) of the first metal oxide material in the first glass material 1 is lower than the mass percent concentration (wt %) of the first metal oxide material in the second glass material 2. Here, "low mass percent concentration" includes cases where the mass percent concentration of the first metal oxide material in the first glass material 1 is zero. The ionization tendency of the metal contained in the first metal oxide material is greater than the ionization tendency of gold (Au). Therefore, the first glass material 1, which has a lower mass percent concentration of the first metal oxide material than the second glass material 2, is less likely to dissolve in a plating solution during metal plating (e.g., gold plating or nickel-gold plating), allowing for stable metal plating to be formed on the metal member 3 on which the first glass material 1 is placed. This configuration eliminates the need for a process for forming an oxide film over the entire metal member 3 and / or a process for removing the formed oxide film. The second glass material 2 may be positioned on the first glass material 1 after metal plating, as in the manufacturing method of the optical component 100 described below.

[0051] The first metal oxide material may include at least one of vanadium oxide (VO), ruthenium oxide (RuO), diphosphorus pentoxide (PO), arsenic trioxide (AsO), boron oxide (BO), tellurium oxide (TeO), bismuth oxide (BiO), zinc oxide (ZnO), tin oxide (SnO), and lead oxide (PbO). Since the first metal oxide material includes the above-described materials and the mass percent concentration of the first metal oxide material in the second glass material 2 is lower than the mass percent concentration of the first metal oxide material in the first glass material 1, the softening temperature t2 of the second glass material 2 can be lower than the softening temperature t1 of the first glass material 1. Therefore, the second glass material 2 is easier to process than the first glass material 1.

[0052] The translucent member 5 may have a side surface 5s located on a plane intersecting the first surface 31s. The side surface 5s is connected to a first translucent surface 51s and a second translucent surface 52s, which will be described later. The second glass material 2 may be in direct or indirect contact with the first translucent surface 51s. Here, "the second glass material 2 and the first translucent surface 51s are in indirect contact" refers to a state in which a first reflection-reducing layer 511, which will be described later, is located between the second glass material 2 and the first translucent surface 51s. Furthermore, the second glass material 2 may be in direct or indirect contact with the second translucent surface 52s. Here, "the second glass material 2 and the second translucent surface 52s are in indirect contact" refers to a state in which a second reflection-reducing layer 522, which will be described later, is located between the second glass material 2 and the second translucent surface 52s. The translucent member 5 may be in contact with the first glass material 1. In this case, the light-transmitting member 5 and the first glass member 1 do not need to be joined together.

[0053] As shown in Fig. 4, the second glass material 2 may be in contact with at least a portion of the side surface 5s. More specifically, the second glass material 2 may be bonded to the side surface 5s. This configuration increases the contact area between the second glass material 2 and the light-transmitting member 5, thereby improving the bonding strength between the second glass material 2 and the light-transmitting member 5. Furthermore, since at least a portion of the side surface 5s is in contact with the second glass material 2, the light-transmitting member 5 can be protected from external impacts. The second glass material 2 may be in contact with the entire side surface 5s.

[0054] A plating layer 4 may be located on the metal member 3. The plating layer 4 may surround the first glass material 1. In other words, the surface of the metal member 3 may be covered with the plating layer 4. This configuration reduces the possibility of corrosion of the metal member 3. For example, when the optical module 10 including the optical component 100 is used in an information display device such as VR goggles or AR glasses, the optical module 10 may be located near or in contact with the human body, and the possibility of corrosion of the metal member 3 due to sweat or tears from the human body can be reduced. Furthermore, the plating layer 4 may also be located on the inner circumferential surface of the through hole 30.

[0055] The material for plating layer 4 can be a highly corrosion-resistant metal material such as gold, nickel, tin, copper, zinc, chromium, copper, or palladium. The material for plating layer 4 may also be an alloy of the aforementioned metal materials (e.g., nickel-gold, nickel-palladium-gold). When the material for plating layer 4 contains gold (Au), gold has excellent corrosion resistance, especially since gold has a low tendency to become ionized.

[0056] Furthermore, the plating layer 4 may be in contact with the first glass material 1. More specifically, the plating layer 4 may be in contact with the first glass material 1 without any gaps. This configuration reduces the possibility of moisture entering between the first glass material 1 and the plating layer 4, which could cause corrosion of the metal member 3. Here, the thickness of the plating layer 4 (i.e., the dimension in the z direction) is, for example, 0.5 μm to 10 μm.

[0057] When the portion where the metal member 3 and the first glass material 1 contact each other is defined as first portion 301, first portion 301 may be surrounded by plating layer 4 in a plan view. More specifically, plating layer 4 does not have to be located on first portion 301. The absence of plating layer 4 on first portion 301 makes it easier to form an oxide film on first portion 301. Therefore, an oxide film formed by oxidizing a portion of the metal member 3 may be located only in first portion 301. The presence of an oxide film only in first portion 301 allows the oxide film to react with the first glass material 1, thereby improving the bonding strength between the first glass material 1 and the metal member 3.

[0058] Furthermore, the surface roughness of first portion 301 may be rougher than the surface roughness of the surface of metal member 3 other than first portion 301. More specifically, as shown in FIG. 6 , metal member 3 may have one or more protrusions 315 and / or depressions 316 in first portion 301. Protrusions 315 may extend into first glass material 1, or first glass material 1 may extend into depressions 316. This increases the bonding strength between metal member 3 and first glass material 1. Protrusions 315 or depressions 316 may be formed in first portion 301 of metal member 3 under predetermined conditions. Sandblasting and etching can be used as methods for forming protrusions 315 or depressions 316.

[0059] The softening temperature t0 of the light-transmitting member 5 may be lower than the softening temperature t1 of the first glass material 1. Alternatively, the softening temperature t0 of the light-transmitting member 5 may be higher than the softening temperature t2 of the second glass material 2. Because the softening temperature t0 of the light-transmitting member 5 is higher than the softening temperature t2 of the second glass material 2, it is possible to reduce the possibility that the light-transmitting member 5 will be softened and deformed due to the temperature of the second glass material 2 when bonding the light-transmitting member 5 to the second glass material 2.

[0060] Reflection reduction layers 511, 522 may be located on at least a portion of the surface of the light-transmitting member 5. By including the reflection reduction layers 511, 522 in the light-transmitting member 5, it is possible to reduce the reflection of light in the light-transmitting member 5 and adjust the refractive index of the light-transmitting member 5. The reflection reduction layers 511, 522 may be, for example, an AR (Anti-Reflective) coating. The AR coating can be formed by vacuum deposition of, for example, magnesium fluoride. The thickness of the reflection reduction layers 511, 522 is, for example, 50 nm to 500 nm.

[0061] The reflection reduction layers 511, 522 may include a first reflection reduction layer 511 located on the first light-transmitting surface 51s and a second reflection reduction layer 522 located on the second light-transmitting surface 52s. The first light-transmitting surface 51s is a surface facing the first surface 31s of the metal member 3 in the z-direction, and the second light-transmitting surface 52s is located on the opposite side of the first light-transmitting surface 51s. In other words, of the two surfaces of the light-transmitting member 5 facing the first surface 31s, the one closer to the first surface 31s can be defined as the first light-transmitting surface 51s, and the one farther from the first surface 31s can be defined as the second light-transmitting surface 52s. The reflection reduction layers 511, 522 do not need to be located on the side surfaces 5s of the light-transmitting member 5.

[0062] The reflection-reducing layers 511, 522 may be located between the light-transmitting member 5 and the second glass material 2. More specifically, the first reflection-reducing layer 511 may be located between the light-transmitting member 5 and the second glass material 2. With this configuration, the first reflection-reducing layer 511 and the second glass material 2 react with each other and are bonded together, thereby improving the bonding strength between the light-transmitting member 5 and the second glass material 2.

[0063] In a plan view, the contact area between the first glass material 1 and the metal member 3 may be larger than the contact area between the first glass material 1 and the second glass material 2. This configuration reduces the possibility of the second glass material 2 coming into contact with the metal member 3 and / or the plating layer 4. If the second glass material 2 comes into contact with the metal member 3 and / or the plating layer 4, the bonding strength at the contact points between the second glass material 2 and the metal member 3 and / or the plating layer 4 may be insufficient. Therefore, when the optical component 100 is deformed, for example, by heat from the electronic component 9, the contact points between the second glass material 2 and the metal member 3 and / or the plating layer 4 may be damaged, making it difficult to maintain airtightness within the optical module 10. However, the above-described configuration reduces the possibility of the second glass material 2 coming into contact with the metal member 3 and / or the plating layer 4, thereby reducing the possibility of the optical component 100 being damaged.

[0064] 4 , in a plan view or a cross-sectional view, the width W1 of the first glass member 1 may be larger than the width W2 of the second glass member 2. This configuration reduces the possibility that the second glass member 2 will come into contact with the metal member 3, even if the second glass member 2 sags. Note that the width here refers to the maximum dimension in the y direction or the x direction.

[0065] The thickness T1 of the first glass material 1 may be greater than the thickness T2 of the second glass material 2. This configuration reduces the possibility that the second glass material 2 will come into contact with the metal member 3 and / or the plating layer 4. Note that the "thickness" referred to here refers to the dimension in the z direction. The thickness T1 of the first glass material 1 may be rephrased as the distance from the first surface 31s to a first point P1 (described later) in a cross-sectional view perpendicular to the first surface 31s. The thickness T2 of the second glass material 2 may be rephrased as the distance from the first point P1 to a second point P2 in a cross-sectional view perpendicular to the first surface 31s.

[0066] 7 to 9, other embodiments of the optical component 100 will be described. In the other embodiments, only the parts that differ from the configuration in the embodiment will be described, and the other configurations will be assigned the same reference numerals as in the embodiment, and descriptions thereof will be omitted.

[0067] Other embodiments differ from the above-described embodiments in that the metal member 3 has a recess 33. The recess 33 has an inner wall surface 331. The first surface 31s may be connected to the inner wall surface 331. In this case, as shown in FIG. 9 , the first surface 31s is located on the bottom surface of the recess 33. The through hole 30 is located on the bottom surface of the recess 33. Even in this case, the surface facing the first light-transmitting surface 51s of the light-transmitting member 5 in the z direction can be defined as the first surface 31s. Note that, as shown in FIG. 8 , in a plan view, the area of ​​the light-transmitting member 5 is larger than the area of ​​the through hole 30 and smaller than the area of ​​the recess 33 (i.e., the area of ​​the portion surrounded by the inner wall surface 331).

[0068] Since the metal member 3 has the recess 33 as described above, the light-transmitting member 5 is positioned within the recess 33, and therefore the light-transmitting member 5 can be protected from external impacts. Note that a portion of the light-transmitting member 5 may be in contact with the inner wall surface 331. In this case, by bringing the light-transmitting member 5 into contact with the inner wall surface 331, the positioning of the light-transmitting member 5 can be easily performed.

[0069] 9 , the first glass material 1 may be in contact with the inner wall surface 331. Alternatively, the first glass material 1 may be bonded to the inner wall surface 331. More specifically, an oxide film formed by oxidizing a portion of the metal member 3 may be located on the inner wall surface 331. In this case, the oxide film reacts with the first glass material 1, thereby improving the bonding strength between the first glass material 1 and the metal member 3.

[0070] In a cross-sectional view perpendicular to the first surface 31s, the point on the surface of the first glass material 1 farthest from the first surface 31s is defined as a first point P1, and the point on the surface of the second glass material 2 farthest from the first surface 31s is defined as a second point P2. The distance T3 from the first surface 31s to the second point P2 may be equal to or greater than the distance T1 from the first surface 31s to the first point P1. More specifically, the end of the second glass material 2 on the inner wall surface 331 side may be covered with the first glass material 1. In this case, the contact area between the first glass material 1 and the second glass material 2 is increased, thereby improving the bonding strength between the first glass material 1 and the second glass material 2. Therefore, a highly reliable optical component 100 can be provided.

[0071] <Configuration of Optical Module> An optical module 10 according to one embodiment will be described with reference to Fig. 10. The optical module 10 includes a substrate 8, an electronic component 9, and an optical component 100. The electronic component 9 is located on the substrate 8. The optical component 100 is located on the substrate 8.

[0072] The substrate 8 is, for example, rectangular in plan view, with dimensions of 10 mm x 10 mm to 50 mm x 50 mm and a thickness of 0.5 mm to 20 mm. Examples of materials for the substrate 8 include metal materials such as copper, iron, tungsten, molybdenum, nickel, and cobalt, as well as alloys containing these metal materials. In this case, the substrate 8 may be a single metal plate or a laminate of multiple metal plates.

[0073] The material of the substrate 8 is an insulating material, and may be, for example, an aluminum oxide sintered body, a mullite sintered body, a silicon carbide sintered body, an aluminum nitride sintered body, a silicon nitride sintered body, or a ceramic material such as glass ceramics. In this case, a metal layer 81, a terminal portion 82, and a pedestal portion 83 may be positioned on the substrate 8. The metal layer 81 and the terminal portion 82 may each be formed by sintering a metal paste, or may be formed using a thin film formation technique such as a vapor deposition method or a sputtering method.

[0074] The metal layer 81 has the same shape as or a similar shape to the outer shape of the metal member 3 in a plan view, and is located below the metal member 3 when the optical module 10 is assembled. The metal member 3 and the metal layer 81 may be directly bonded together, or a seal ring may be located between the metal layer 81 and the metal member 3. The optical component 100 may be bonded to the metal member 3 and / or the substrate 8 by welding, or may be bonded with an adhesive such as solder, brazing material, glass, or resin adhesive.

[0075] The terminal portion 82 can be electrically connected to the electronic component 9 by conductive wiring formed inside the substrate 8. A flexible printed circuit (FPC) or a printed circuit board (PCB) on which an electronic circuit is formed may be connected to the terminal portion 82, or a lead terminal and / or a metal wire such as a bonding wire may be mounted on the terminal portion 82.

[0076] The base 83 may be integrally formed with the substrate 8, or may be a separate member from the substrate 8. An electrode 85 may be located on the base 83. The electrode 85 may be formed, for example, using the same material and method as the terminal 82. The electrode 85 can be electrically connected to the electronic component 9. Furthermore, a submount 84 for mounting the electronic component 9 may be located on the base 83.

[0077] The electronic component 9 is located on a base portion 83 on the substrate 8. The electronic component 9 may also be located on a submount 84. A plurality of electronic components 9 may be located within the optical module 10.

[0078] The electronic component 9 may be, for example, an optical semiconductor element such as a semiconductor laser (LD) or a photodiode (PD), a semiconductor integrated circuit element, a sensor element such as an optical sensor, or a power amplifier IC. The electronic component 9 may be formed from a semiconductor material such as gallium arsenide or gallium nitride. More specifically, the electronic component 9 may be three light-emitting elements 9A-9C, each emitting red (R), green (G), and blue (B) light, respectively. In this case, the optical module 10 may be an RGB laser light source module and may be used in information display devices such as VR goggles and AR glasses.

[0079] It should be noted that various combinations of the embodiments are not limited to the examples of the embodiments described above, and combinations of the embodiments with each other are also possible.

[0080] <Method of Manufacturing Optical Component> Here, a method of manufacturing optical component 100 will be described with reference to Fig. 11. In the description of this manufacturing method, the same reference numerals as in the above-described embodiment will be used to designate the configuration of optical component 100, and the description thereof may be omitted.

[0081] (1) First, a first member is prepared by applying the first glass material 1 to a predetermined position on the metal member 3. This step is referred to as the first member preparation step S1. The first glass material 1 may be applied by first forming the first glass material 1 into a predetermined shape, hardening it, and then partially heating and pressing it to a predetermined position on the metal member 3. Alternatively, the first glass material 1 may be placed on the metal member 3, and then the metal member 3 itself may be heated to melt and bond the first glass material 1 by the heat. Alternatively, the unhardened first glass material 1 may be applied to a predetermined position on the metal member 3, and then the first glass material 1 may be cooled and hardened.

[0082] By performing step S1 before subsequent steps S2 to S4, when the first glass material 1 is formed on the first surface 31s of the metal member 3, the first glass material 1 heated to a high temperature reacts with the metal member 3, and an oxide film can be partially formed at the contact point between the first glass material 1 and the metal member 3. This improves the bonding strength between the first glass material 1 and the metal member 3. Furthermore, step S1 makes it possible to omit the step of heating the metal member 3 to form an oxide film. The step of forming the through hole 30 in the metal member 3 may be performed between steps S3 and S4 described below, or the through hole 30 may be formed in the metal member 3 in advance before step S1.

[0083] (2) Subsequently, the first member is metal-plated. By the metal plating, a plating layer 4 is formed on the surface of the metal member 3. This step is referred to as a plating step S2. The metal plating in step S2 may be electroless plating or electrolytic plating.

[0084] (3) Then, a second glass material 2 (softening temperature t2) having a softening temperature lower than the softening temperature t1 of the first glass material 1 is applied onto the first glass material 1. This step is referred to as a glass material application step S3. The second glass material 2 may be applied by forming a predetermined shape, hardening it, and then partially heating and pressing it onto the first glass material 1. Alternatively, the unhardened second glass material 2 may be applied to a predetermined position on the first glass material 1, and then the second glass material 2 may be cooled and hardened.

[0085] (4) Finally, a light-transmitting member 5 having translucency is bonded to the second glass material 2. This step is referred to as a bonding step S4. The light-transmitting member 5 may be bonded to the second glass material 2 by pressing the light-transmitting member 5 against the second glass material 2 before the applied second glass material 2 hardens in step S3. Alternatively, the hardened second glass material 2 may be partially heated to soften it, and then the light-transmitting member 5 may be pressed against the second glass material 2 to bond it.

[0086] Since the second glass material 2 has a lower softening temperature than the first glass material 1 and therefore contains impurities, it is more likely to dissolve in a plating solution, but because the first glass material 1 is made of a material that is less soluble in a plating solution, the above-described manufacturing method makes it possible to form the plating layer 4 on the surface of the metal member 3 other than the portion where the first glass material 1 is located (i.e., first portion 301). Furthermore, because the plating layer 4 can be in contact with the first glass material 1, it is possible to effectively reduce the possibility of moisture penetrating between the plating layer 4 and the first glass material 1 and corroding the metal member 3.

[0087] In the method for manufacturing optical component 100 according to one embodiment, steps S1 to S4 may be performed in the order described above, and steps different from S1 to S4 may be present between the steps. For example, if optical component 100 includes frame member 6 between first glass material 1 and second glass material 2, the step of bonding frame member 6 to first glass material 1 may be performed between steps S1 and S2, or between steps S2 and S3.

[0088] The present disclosure can be used as an optical component, an optical module including the optical component, and a method for manufacturing the optical component.

[0089] REFERENCE SIGNS LIST 1 First glass material 12 Diffusion layer 2 Second glass material 3 Metal member 30 Through hole 31s First surface 32s Second surface 301 First portion 315 Protrusion 316 Depression 33 Concave portion 331 Inner wall surface 4 Plating layer 5 Light-transmitting member 5s Side surface 51s First light-transmitting surface 52s Second light-transmitting surface 511 First reflection reduction layer 522 Second reflection reduction layer 6 Frame-shaped member T1 Thickness of first glass material (distance from first surface to first point) T2 Thickness of second glass material (distance from first point to second point) T3 Distance from first surface to second point W1 Width of first glass material W2 Width of second glass material P1 First point P2 Second point 8 Substrate 81 Metal layer 82 Terminal portion 83 Base portion 84 Submount 85 Electrode 9 Electronic component 9A to 9C Light emitting element 10 Optical module 100 Optical component

Claims

1. An optical component comprising: a metal member having a first surface, a second surface opposite the first surface, and a through hole penetrating from the first surface to the second surface; a first glass material located on the first surface and surrounding the through hole in a planar view; a second glass material located on the first glass material and surrounding the through hole in a planar view; and a translucent member located on the second glass material, overlapping with the through hole in a planar view and having translucency, wherein a softening temperature t1 of the first glass material is higher than a softening temperature t2 of the second glass material.

2. An optical component comprising: a metal member having a first surface, a second surface opposite the first surface, and a through hole penetrating from the first surface to the second surface; a first glass material located on the first surface and surrounding the through hole in a planar view; a second glass material located on the first glass material and surrounding the through hole in a planar view; and a translucent material located on the second glass material, overlapping with the through hole in a planar view and having translucency, wherein a mass percent concentration of a first metal oxide material in the first glass material is lower than a mass percent concentration of the first metal oxide material in the second glass material.

3. The optical component of claim 2, wherein the first metal oxide material includes at least one of vanadium oxide (V2O5), ruthenium oxide (RuO2), phosphorus pentoxide (P2O5), arsenic trioxide (As2O3), boron oxide (B2O3), tellurium oxide (TeO2), bismuth oxide (Bi2O3), zinc oxide (ZnO), tin oxide (SnO2), and lead oxide (PbO).

4. An optical component according to any one of claims 1 to 3, wherein the light-transmitting member has a side surface located on a plane intersecting the first surface, and the second glass material is in contact with at least a portion of the side surface.

5. The optical component according to any one of claims 1 to 4, wherein a plating layer is located on the metal member, and the plating layer surrounds the first glass material.

6. The optical component according to claim 5, wherein the plating layer is in contact with the first glass material.

7. The optical component according to claim 5 or 6, wherein the material of the plating layer includes gold (Au).

8. An optical component according to any one of claims 5 to 7, wherein, when a portion where the metal member and the first glass material contact is defined as a first portion, the first portion is surrounded by the plating layer in a plan view.

9. The optical component according to any one of claims 1 to 8, wherein the softening temperature t0 of the light-transmitting member is lower than the softening temperature t1 of the first glass material and higher than the softening temperature t2 of the second glass material.

10. The optical component according to any one of claims 1 to 9, wherein a reflection reducing layer is located on at least a portion of the surface of the light-transmitting member.

11. The optical component according to claim 10, wherein the reflection reduction layer is located between the light-transmitting member and the second glass material.

12. The optical component according to any one of claims 1 to 11, wherein, in a plan view, the contact area between the first glass material and the metal member is larger than the contact area between the first glass material and the second glass material.

13. The optical component according to any one of claims 1 to 12, wherein the thickness of the first glass material is greater than the thickness of the second glass material.

14. The optical component according to any one of claims 1 to 13, wherein the first glass material and the second glass material are bonded together.

15. An optical component described in any one of claims 1 to 14, wherein, in a cross-sectional view perpendicular to the first surface, when a point on the surface of the first glass material that is farthest from the first surface is defined as a first point, and a point on the surface of the second glass material that is farthest from the first surface is defined as a second point, the distance from the first surface to the second point is equal to or greater than the distance from the first surface to the first point.

16. The optical component according to any one of claims 1 to 13, further comprising a frame-shaped member located between the first glass material and the second glass material and surrounding the through hole in a plan view.

17. The optical component according to claim 16, wherein the light-transmitting member is inclined with respect to the first surface.

18. The optical component according to claim 16 or 17, wherein the material of the frame-shaped member is ceramic.

19. An optical module comprising: a substrate; an electronic component located on said substrate; and an optical component according to any one of claims 1 to 18 located on said substrate.

20. A method for manufacturing an optical component, comprising the steps of: preparing a first member having a first glass material applied to a predetermined position of a metal member; metal plating the first member; applying a second glass material having a softening temperature lower than that of the first glass material onto the first glass material; and bonding a translucent member having translucency to the second glass material.

Citation Information

Patent Citations

  • Window cap and manufacture of the same

    JP1987202565A

  • Cap for semiconductor laser, and optical module

    JP2007086472A

  • Electronic device mounting package and electronic device

    JP2022116383A

  • Airtight package

    WO2020071047A1