Method for manufacturing semiconductor device

The method of forming a photosensitive resin layer on semiconductor wafers using light irradiation and development in plasma dicing addresses debris-related reliability concerns in hybrid bonding, ensuring improved chip manufacturing quality and equipment protection.

WO2024204615A1PCT designated stage expired Publication Date: 2024-10-03RESONAC CORP

Patent Information

Application Number
PCT/JP2024/012830
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

In semiconductor device manufacturing, plasma dicing methods often result in debris scattering during laser processing, which can adhere to chips and compromise the reliability and connectivity of hybrid-bonded semiconductor devices.

Method used

A method involving the formation of a photosensitive resin layer on a semiconductor wafer, where openings are created through light irradiation and development, eliminating the need for laser processing and thereby reducing debris impact on hybrid bonding, using a developer with a pH of 11 or less to minimize damage to manufacturing components.

Benefits of technology

This approach effectively reduces debris-related issues in semiconductor chip manufacturing, enhancing the reliability of hybrid bonding by eliminating the need for laser processing and protecting manufacturing equipment from damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024012830_03102024_PF_FP_ABST
    Figure JP2024012830_03102024_PF_FP_ABST
Patent Text Reader

Abstract

This method for manufacturing a semiconductor device is provided with the steps of: forming a photosensitive resin layer on one principal surface of a semiconductor wafer; forming an opening, which exposes the semiconductor wafer, by removing a portion of the photosensitive resin layer by light irradiation and development using a developing solution; forming a semiconductor chip, which has a first principal surface and a second principal surface on the opposite side of the first principal surface and is provided with a photosensitive resin layer on the first principal surface, by dividing the semiconductor wafer by plasma dicing along the opening; removing the photosensitive resin layer on the semiconductor chip; and hybrid-joining the semiconductor chip and another semiconductor member so that the first principal surface of the semiconductor chip is in contact with the semiconductor member.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor device manufacturing method

[0001] The present disclosure relates to a method for manufacturing a semiconductor device.

[0002] In the manufacturing process of semiconductor devices, semiconductor wafers are sometimes diced into semiconductor chips by plasma dicing. In plasma dicing, for example, a mask is formed on the semiconductor wafer to partially cover the semiconductor wafer, and then plasma is irradiated from above the mask to selectively etch the portions of the semiconductor wafer that are not covered by the mask, thereby dividing the semiconductor wafer.

[0003] One method for forming such a mask involves forming a layer that covers the entire surface of a semiconductor wafer and then removing a portion of the layer by laser processing. However, laser processing can cause debris (processing chips) to scatter around the processed area and adhere to the semiconductor chip being fabricated. If a semiconductor chip with debris attached is used in a semiconductor device, it may result in a decrease in reliability, etc. Therefore, methods have been studied to suppress the residue of debris that occurs during laser processing on semiconductor chips when fabricating semiconductor chips (e.g., Patent Document 1).

[0004] Japanese Patent Application Laid-Open No. 2019-50237

[0005] Hybrid bonding is a technique for bonding semiconductor chips to other semiconductor components (semiconductor chips, semiconductor wafers, etc.). In hybrid bonding, the semiconductor chip and the other semiconductor component each have a bonding surface composed of an electrode and an insulating film, and these bonding surfaces are directly bonded to each other. Therefore, when manufacturing a semiconductor device using hybrid bonding, even a small amount of debris adhering to the surface of the semiconductor chip is particularly susceptible to the effects, and there is a possibility that problems such as connectivity may occur.

[0006] The present disclosure relates to a method for manufacturing a semiconductor device by plasma dicing while reducing the influence of debris and the like on hybrid bonding.

[0007] One aspect of the present disclosure relates to a method for manufacturing a semiconductor device, comprising the steps of: forming a photosensitive resin layer on one main surface of a semiconductor wafer; removing a portion of the photosensitive resin layer by light irradiation and development using a developer to form an opening that exposes the semiconductor wafer; dividing the semiconductor wafer along the opening by plasma dicing to form a semiconductor chip having a first main surface and a second main surface opposite the first main surface, with the photosensitive resin layer provided on the first main surface; removing the photosensitive resin layer on the semiconductor chip; and hybrid-bonding the semiconductor chip and another semiconductor member so that the first main surface of the semiconductor chip is in contact with the semiconductor member.

[0008] In the above manufacturing method, the photosensitive resin layer with the openings formed therein is used as a mask for plasma dicing. The openings can be formed in the photosensitive resin layer by light irradiation and development using a developer, rather than by laser processing. In this way, the above manufacturing method does not require laser processing, which can generate debris, to form the mask for plasma dicing, thereby reducing the impact of debris on hybrid bonding.

[0009] In the above manufacturing method, the developer may be a developer containing water. The pH of the developer may be 11 or less. In these cases, deterioration of components (such as dicing tape and dicing ring) used in manufacturing the semiconductor device can be suppressed.

[0010] In the above manufacturing method, the photosensitive resin layer may be a positive photosensitive resin layer. When the photosensitive resin layer is a positive photosensitive resin layer, after plasma dicing, the photosensitive resin layer on the semiconductor chip can be easily removed by light irradiation and dissolution in a cleaning solution.

[0011] The manufacturing method may further include a step of irradiating the photosensitive resin layer on the semiconductor chip with light. The photosensitive resin layer on the semiconductor chip may be removed by dissolving in a cleaning solution. In this case, the cleaning solution may be a cleaning solution containing water. The cleaning solution may have a pH of 11 or less.

[0012] In the above-described manufacturing method, the photosensitive resin layer may contain a reaction product of a polythiol compound having a disulfide bond and a cyclic ether compound having a polyether chain and two or more cyclic ether groups, and a photoradical generator.

[0013] According to one aspect of the present disclosure, there is provided a method for manufacturing a semiconductor device by plasma dicing while reducing the influence of debris and the like on hybrid bonding.

[0014] 1A and 1B are schematic diagrams illustrating an example of a method for manufacturing a semiconductor device.

[0015] The present invention is not limited to the following examples.

[0016] 1 and 2 are schematic diagrams showing an example of a method for manufacturing a semiconductor device. The method shown in Fig. 1 and Fig. 2 includes a step of forming a photosensitive resin layer 30 on one main surface of a semiconductor wafer 10 (hereinafter also referred to as "step (a)"), a step of removing a part of the photosensitive resin layer 30 by light irradiation and development using a developer (hereinafter also referred to as "step (b)"), and a step of dividing the semiconductor wafer 10 along the opening 30a by plasma dicing, thereby forming a first main surface 20a. and a second main surface 20b on the opposite side thereof, and a step of forming a semiconductor chip 20 having a photosensitive resin layer 30 on the first main surface 20a (hereinafter also referred to as "step (c)"), a step of removing the photosensitive resin layer 30 on the semiconductor chip 20 as shown in (d) (hereinafter also referred to as "step (d)"), and a step of hybrid-bonding the semiconductor chip 20 and another semiconductor member 70 as shown in (e) so that the first main surface 20a of the semiconductor chip 20 is in contact with the semiconductor member 70 (hereinafter also referred to as "step (e)").

[0017] In step (a), a photosensitive resin layer 30 is formed on one main surface of a semiconductor wafer 10. The semiconductor wafer 10 may be, for example, a silicon wafer. An integrated circuit may be formed on one main surface of the semiconductor wafer 10. The thickness of the semiconductor wafer 10 may be, for example, 10 μm or more and 1000 μm or less. Such a semiconductor wafer 10 can be produced, for example, by forming an integrated circuit on one main surface of the semiconductor wafer 10 and then grinding the back surface of the surface on which the integrated circuit is formed.

[0018] An example of the semiconductor wafer 10 may include a wafer body and an electrode and an insulating film provided on one main surface of the wafer body, and one main surface of the semiconductor wafer 10 facing the photosensitive resin layer 30 may be configured with an insulating film having an opening and an electrode provided in the opening of the insulating film. By dividing such a semiconductor wafer 10 in step (c) described below, it is possible to form semiconductor chips 20 each having a first main surface 20a configured with an electrode and an insulating film. The electrode provided on the semiconductor wafer 10 may include a through electrode that penetrates the wafer body.

[0019] As shown in FIG. 1A, the semiconductor wafer 10 may be fixed on a dicing tape 50. A dicing ring may be attached to the dicing tape 50. Examples of materials for the dicing tape 50 include acrylic adhesives, unsaturated polyester adhesives, rubber adhesives, and urethane adhesives. Examples of materials for the dicing ring include SUS, aluminum, ABS resin, and PSS resin.

[0020] The photosensitive resin layer 30 may be formed to cover the entirety of one main surface of the semiconductor wafer 10, or may be formed to cover a portion of it. The photosensitive resin layer 30 may be formed to cover the entire portion of the semiconductor wafer 10 where the integrated circuits are formed. The photosensitive resin layer 30 may be a positive photosensitive resin layer or a negative photosensitive resin layer. When the photosensitive resin layer 30 is a positive photosensitive resin layer, the photosensitive resin layer 30 on the semiconductor chip 20 can be easily removed by light irradiation and dissolution in a cleaning solution in the step of removing the photosensitive resin layer on the semiconductor chip 20 described below.

[0021] In step (b), a portion of the photosensitive resin layer 30 is removed by light irradiation and development using a developer. As a result, an opening 30a is formed in the photosensitive resin layer 30, and the semiconductor wafer 10 is exposed in the opening 30a. If the photosensitive resin layer 30 is a positive photosensitive resin layer, the portion of the photosensitive resin layer 30 corresponding to the opening 30a is irradiated with light, and that portion is removed by dissolving in the developer.

[0022] The light source used for light irradiation may be, for example, an LED lamp, a mercury lamp (e.g., a low-pressure mercury lamp, a medium-pressure mercury lamp, or a high-pressure mercury lamp), a metal halide lamp, an excimer lamp, or a xenon lamp. Light irradiation may be performed directly on the photosensitive resin layer 30 or may be performed through glass or the like. Examples of the light to be irradiated include visible light and ultraviolet light. The light to be irradiated may be, for example, light containing light with a wavelength of 365 nm. The wavelength of the light to be irradiated may be, for example, 150 to 550 nm.

[0023] The exposure dose of light irradiation is, for example, 1000 mJ / cm 2 or more, and 2000 mJ / cm 2 In this specification, the exposure dose is defined as the illuminance (mW / cm 2 ) and the irradiation time (seconds).

[0024] The developer used for development may be, for example, a developer containing water. Examples of water include tap water, natural water, purified water, distilled water, ion-exchanged water, pure water, and ultrapure water (such as Milli-Q water). Milli-Q water refers to ultrapure water obtained using a Milli-Q water production system from Merck Millipore (Merck). Since the water has reduced impurities, it may be purified water, distilled water, ion-exchanged water, pure water, or ultrapure water. The proportion of water contained in the developer may be, for example, 80% by mass or more based on the total amount of the developer.

[0025] The pH of the developer may be 14 or less, 12 or less, 11 or less, 10 or less, or 8 or less, or may be 1 or more, 2 or more, 4 or more, or 6 or more. When the developer is neutral or close to neutral, deterioration of parts such as dicing tape and dicing ring can be suppressed.

[0026] The developer may contain a hydrophilic organic solvent. Examples of the hydrophilic organic solvent include alcohols such as methanol, ethanol, 2-propanol, and 1,2-propanediol, and glycol ethers such as ethylene glycol monomethyl ether, propylene glycol monomethyl ether, ethyl cellosolve, propylene glycol monopropyl ether, propylene glycol monoisopropyl ether, butyl cellosolve, ethylene glycol monoisobutyl ether, propylene glycol monobutyl ether, diethylene glycol dimethyl ether, diethylene glycol diethyl ether, and dipropylene glycol monomethyl ether.

[0027] The developer may contain a pH adjuster. Examples of pH adjusters include inorganic acids, inorganic bases, organic acids, and organic bases. Examples of inorganic acids include nitric acid, sulfuric acid, hydrochloric acid, phosphoric acid, and boric acid. Examples of inorganic bases include sodium hydroxide, potassium hydroxide, and calcium hydroxide. Examples of organic acids include formic acid, acetic acid, propionic acid, butyric acid, acrylic acid, benzoic acid, and picolinic acid. Examples of organic bases include primary amines, secondary amines, tertiary amines, tetramethylammonium hydroxide, tetraethylammonium hydroxide, and imidazole-based compounds.

[0028] A positive-type photosensitive resin layer that can be developed with a water-containing, neutral or nearly neutral developer can be, for example, a layer containing a polymer having a chemical bond (e.g., a disulfide bond) that is cleaved by light irradiation and a hydrophilic group. One example of such a positive-type photosensitive resin layer contains a reaction product (polymer) of a polythiol compound having a disulfide bond (hereinafter also referred to as "compound (A)") and a cyclic ether compound having a polyether chain as a hydrophilic group and two or more cyclic ether groups (hereinafter also referred to as "compound (B)"), and a photoradical generator. In this case, the photosensitive resin layer has the property of melting upon light irradiation. When a photosensitive resin layer containing the reaction product of compound (A) and compound (B) and the photoradical generator is irradiated with light, the photoradical generator cleaves the disulfide bond (-S-S-) in the reaction product of compound (A) and compound (B). As a result, the reaction product of the compound (A) and the compound (B) can be reduced in molecular weight and become a liquid (liquid state).

[0029] The resin component generated by the reaction product of the compound (A) and the compound (B) having a low molecular weight has many polyether chains or hydroxyl groups and tends to be hydrophilic, and therefore the resin component dissolves in a developer containing water. Therefore, when such a photosensitive resin layer is used, it can be removed by development using a developer containing water.

[0030] Specifically, the reaction product of compound (A) and compound (B) may be a product of a curing reaction between compound (A) and compound (B). The photosensitive resin layer 30 containing the reaction product of compound (A) and compound (B) and a photoradical generator can be formed, for example, by a method including preparing a thermosetting composition containing compound (A), compound (B), a curing accelerator, and a photoradical generator, and curing the thermosetting composition by heating. In this case, it can be said that the photosensitive resin layer 30 includes a cured product of the thermosetting composition.

[0031] The thermosetting composition containing the compound (A), the compound (B), a curing accelerator, and a photoradical generator can be prepared, for example, by mixing the compound (A), the compound (B), the curing accelerator, and the photoradical generator.

[0032] Compound (A) is a compound having a disulfide bond (-S-S-) and two or more thiol groups (-SH). The upper limit of the number of thiol groups in compound (A) may be, for example, five or less. Compound (A) may be, for example, a dithiol compound, which is a compound having two thiol groups (-SH). Compound (A) may be a high-molecular-weight component of a polymer or oligomer. A compound having two thiol groups (-SH) can be considered to be a compound consisting of two thiol groups and a group (first linking group) that contains a disulfide bond and links the two thiol groups.

[0033] The molecular weight or number average molecular weight of compound (A) may be, for example, 100 to 10,000,000, 200 to 3,000,000, 300 to 1,000,000, 400 to 10,000, or 500 to 5,000. The number average molecular weight is a polystyrene-equivalent value determined by gel permeation chromatography (GPC) using a calibration curve with standard polystyrene.

[0034] Compound (A) has one or more (two or more) disulfide bonds in the molecule. The number of disulfide bonds in compound (A) may be, for example, 1 to 1000, or 4 to 50.

[0035] The compound (A) may be a compound (e.g., a polymer or oligomer) having a linear or branched molecular chain and a terminal group, with a disulfide bond in the molecular chain. In this case, the terminal group in the compound (A) may be a thiol group. When the compound (A) is such a compound, it tends to be easier to form a cured product with excellent photo-melting properties. The molecular chain in the compound (A) may contain a disulfide bond and a polyether chain, or may be composed of a disulfide bond and a polyether chain.

[0036] Compound (A) is, for example, a compound represented by formula (1): HS-(X-S-S) n1 In the formula, X represents a polyether chain. Multiple X's may be the same or different. n1 represents an integer of 1 or more. For example, n1 may be 1 or more, or 4 or more, or 1000 or less. When compound (A) is a compound represented by formula (1), -(X-S-S) n1 The group represented by -X- is a first linking group. The compound obtained by chain extension of compound (1) may be, for example, a Michael adduct of compound (1) or a thiourethanized product of compound (1).

[0037] The polyether chain represented by X may be, for example, a polyoxyalkylene chain. 1 -O-X 2 -O-X 3 X may be a group represented by the formula: 1 ~X 3 may each independently be an alkylene group, and may be an alkylene group having 1 to 2 carbon atoms (for example, a methylene group or an ethylene group). Examples of the polyether chain represented by X include -CH 2 CH 2 -O-CH 2 -O-CH 2 CH 2 - are some examples.

[0038] Examples of commercially available products of compound (A) include the Thiokol LP series (dithiols having a disulfide bond, manufactured by Toray Fine Chemicals Co., Ltd.). Compound (A) can also be obtained by converting the reactive functional group of a compound having a terminal reactive functional group (e.g., a carboxy group or a hydroxy group) and a disulfide bond to a thiol group. Examples of compounds having a terminal reactive functional group and a disulfide bond include 3,3'-dithiodipropionic acid (manufactured by Tokyo Chemical Industry Co., Ltd.), dithiodiethanol, and cystamine.

[0039] The content of compound (A) in the thermosetting composition may be 15 mass% or more, 25 mass% or more, or 35 mass% or more, and may be 80 mass% or less, 70 mass% or less, or 60 mass% or less, based on the total amount of the thermosetting composition.

[0040] Compound (B) is a compound having a polyether chain and two or more cyclic ether groups. When a photosensitive resin layer 30 containing a cured product of a thermosetting composition containing compound (B) (specifically, a reaction product of compound (A) and compound (B)) is irradiated with light, the reaction product of compound (A) and compound (B) is reduced in molecular weight, resulting in the generation of a resin component having a structure derived from compound (B). Here, since compound (B) is a compound having a polyether chain and two or more cyclic ether groups, a large amount of resin component having a large number of polyether chains or hydroxyl groups (derived from the cyclic ether groups) and tending to exhibit hydrophilicity is generated. Therefore, by using such compound (B), it is possible to remove the photosensitive resin layer 30 using a developer or cleaning solution containing water in steps (b) and (d). Compound (B) may be a high-molecular-weight component of a polymer or oligomer.

[0041] The cyclic ether group of compound (B) may be a group obtained by removing one hydrogen atom from a cyclic ether compound. Specific examples of the cyclic ether group of compound (B) include oxirane groups (e.g., oxiranyl groups and epoxy groups), oxetane groups (e.g., oxetanyl groups), tetrahydrofuryl groups, and tetrahydropyranyl groups. Among these, the cyclic ether group may be an oxirane group from the viewpoint of reactivity and ease of availability. That is, compound (B) may be an oxirane compound (epoxy compound) having a polyether chain and two or more oxirane groups (e.g., oxiranyl groups or epoxy groups). In this specification, the cyclic ether group includes a group having a cyclic ether structure (a structure containing a cyclic ether group). For example, the cyclic ether group includes a group having an oxirane structure (a structure containing an oxirane group (e.g., an oxiranyl group or an epoxy group)), such as a glycidyl group, a glycidyl ether group, or an epoxycyclohexyl group.

[0042] The molecular weight or number average molecular weight of compound (B) may be, for example, 100 to 1,000,000, 100 to 500,000, 100 to 10,000, 150 to 5,000, or 200 to 2,000. The number average molecular weight is a polystyrene-equivalent value determined by gel permeation chromatography (GPC) using a calibration curve with standard polystyrene.

[0043] When the cyclic ether group of compound (B) is an oxirane group (for example, an oxiranyl group or an epoxy group), the epoxy equivalent of compound (B) may be 50 to 2000 g / eq, 80 to 1500 g / eq, or 100 to 1000 g / eq.

[0044] Compound (B) may be a compound having two cyclic ether groups (hereinafter also referred to as "compound (B1)") or a compound having three or more cyclic ether groups (hereinafter also referred to as "compound (B2)"). Compound (B1) can be considered a compound consisting of two cyclic ether groups and a group (second linking group) containing a polyether chain and linking the two cyclic ether groups. Compound (B2) may be a compound of compound (B1) having one or more cyclic ether groups as a side chain or substituent of the second linking group. Compound (B) may contain both compound (B1) and compound (B2) because this can further shorten the curing time of the thermosetting composition and further improve the photomeltability of the photosensitive resin layer 30 and the solubility in a developing solution or cleaning solution containing water.

[0045] Compound (B1) may be a compound (e.g., a polymer or oligomer) having a linear molecular chain and a terminal group, and having a polyether chain in the molecular chain. In this case, the terminal group in compound (B1) may be a cyclic ether group. When compound (B) is compound (B1), resin components generated by irradiating the photosensitive resin layer 30 with light tend to be easily removed with a developer or cleaning solution containing water. The polyether chain as a molecular chain may have a substituent such as a hydroxyl group or an alkyl group optionally having a hydroxyl group. The molecular chain in compound (B1) may contain a polyether chain or may consist of a polyether chain.

[0046] The compound (B1) is, for example, a compound represented by the formula (2): Z-(Y) n2 In the formula, Y represents a polyether chain, and Z represents a cyclic ether group. A plurality of Z's may be the same or different. n2 represents an integer of 1 or more. n2 may be, for example, 1 or more, or 2 or more, and may be 1000 or less. When compound (B1) is a compound represented by formula (2), -(Y) n2 The group represented by - is the second linking group.

[0047] The polyether chain represented by Y may be, for example, a polyoxyalkylene chain.1 -O-Y 2 -O-Y 3 Y may be a group represented by -. 1 ~Y 3 may each independently be an alkylene group, and may be an alkylene group having 1 to 3 carbon atoms (for example, a methylene group, an ethylene group, or a propylene group). Examples of the polyether chain represented by Y include -CH 2 CH 2 -O-CH 2 -CH 2 -O-CH 2 CH 2 - are some examples.

[0048] Commercially available products of compound (B1) include, for example, the Denacol EX series (EX-850, EX-851, EX-821, EX-830, EX-832, EX-841, EX-861, and EX-920, manufactured by Nagase ChemteX Corporation).

[0049] The compound (B2) may be a compound (B1) having one or more cyclic ether groups as side chains of the second linking group (polyether chain as Y).

[0050] Examples of commercially available products of compound (B2) include the Denacol EX series (EX-614B, EX-313, EX-512, and EX-521, manufactured by Nagase ChemteX Corporation).

[0051] The content of compound (B) (total of compound (B1) and compound (B2)) in the thermosetting composition may be 15 mass% or more, 25 mass% or more, or 35 mass% or more, and may be 80 mass% or less, 70 mass% or less, or 60 mass% or less, based on the total amount of the thermosetting composition.

[0052] The mass ratio of the content of compound (B2) to the content of compound (B) (the sum of compound (B1) and compound (B2)) in the thermosetting composition (the content (mass) of compound (B2) / the content (mass) of compound (B) (the sum of compound (B1) and compound (B2)))) may be 0.01 to 0.40. When this mass ratio is 0.01 or more, the curing time of the thermosetting composition tends to be further shortened, and when this mass ratio is 0.40 or less, the photo-meltability of the photosensitive resin layer 30 and the solubility of the resin components generated by light irradiation of the photosensitive resin layer 30 in a developer or cleaning solution containing water tend to be further improved. This mass ratio may be 0.02 or more or 0.03 or more, or may be 0.35 or less, 0.30 or less, 0.25 or less, 0.20 or less, 0.15 or less, 0.10 or less, or 0.05 or less.

[0053] The equivalent ratio of the cyclic ether group of compound (B) to the thiol group of compound (A) (cyclic ether group of compound (B) / thiol group of compound (A)) may be, for example, 0.5 to 2.5. When the equivalent ratio is 0.5 or more, the solubility of the resin component generated by light irradiation of the photosensitive resin layer 30 in a developer or cleaning solution containing water tends to be further improved, and when the equivalent ratio is 2.5 or less, the photomeltability of the photosensitive resin layer 30 tends to be further improved. The equivalent ratio may be 0.8 or more, 1.0 or more, 1.2 or more, or 1.5 or more, or may be 2.2 or less, or 2.0 or less.

[0054] The curing accelerator is a component for accelerating the (curing) reaction of the compound (A) and the compound (B), and includes a component (catalytic curing agent) that functions as a catalyst for the curing reaction. Examples of the curing accelerator include amine compounds, imidazole derivatives, quaternary ammonium salts, organic metal salts, and phosphorus compounds.

[0055] Examples of the amine compound include dicyandiamide, trimethylamine, triethylamine, tripropylamine, tributylamine, tri-n-octylamine, dimethylethylamine, dimethylpropylamine, dimethylbutylamine, dimethyl-n-octylamine, 1,4-diazabicyclo[2.2.2]octane, 1,8-diazabicyclo[5.4.0]undec-7-ene, benzyldimethylamine, 4-methyl-N,N-dimethylbenzylamine, 2,4,6-tris(dimethylaminomethyl)phenol, and 4-dimethylaminopyridine.

[0056] Examples of imidazole derivatives include 1-(1-cyanomethyl)-2-ethyl-4-methyl-1H-imidazole, 2-ethyl-4-methylimidazole, 2-methylimidazole, 2-phenylimidazole, 1-cyanoethyl-2-phenylimidazole, 2-phenyl-4,5-dihydroxymethylimidazole, 2-phenyl-4-methyl-5-hydroxymethylimidazole, 2,4,5-triphenylimidazole, 1-benzyl-2-imidazole, 1,2-dimethylimidazole, and 1-benzyl-2-phenylimidazole.

[0057] Examples of quaternary ammonium salts include tetramethylammonium chloride, tetraethylammonium chloride, tetrabutylammonium chloride, benzyltrimethylammonium chloride, benzyltriethylammonium chloride, benzyltributylammonium chloride, tetramethylammonium bromide, tetraethylammonium bromide, tetrabutylammonium bromide, benzyltrimethylammonium bromide, benzyltriethylammonium bromide, tetramethylammonium iodide, tetraethylammonium iodide, tetrabutylammonium iodide, and benzyltributylammonium iodide.

[0058] Examples of the organic metal salt include zinc(II) bis(2,4-pentanedionato), zinc octylate, zinc naphthenate, cobalt naphthenate, copper naphthenate, iron acetylacetonate, nickel octylate, and manganese octylate.

[0059] Examples of phosphorus compounds include tetraphenylphosphonium tetra-p-tolylborate, tetraphenylphosphonium tetraphenylborate, triphenylphosphine, tri-p-tolylphosphine, tris(4-chlorophenyl)phosphine, tris(4-methoxyphenyl)phosphine, tris(2,6-dimethoxyphenyl)phosphine, triphenylphosphinetriphenylborane, tetraphenylphosphonium dicyanamide, and tetraphenylphosphonium tetra(4-methylphenyl)borate.

[0060] The content of the curing accelerator may be 0.01 mass % or more, 0.1 mass % or more, or 0.5 mass % or more, and may be 10 mass % or less, 5 mass % or less, or 2 mass % or less, based on the total amount of the thermosetting composition.

[0061] The photoradical generator is a component that generates radicals upon light irradiation. Examples of the photoradical generator include a hydrogen abstraction type photoradical polymerization initiator that generates radicals by abstracting hydrogen from other molecules upon light irradiation, and an intramolecular cleavage type photoradical polymerization initiator that photocleaves itself upon light irradiation to generate two radicals. The photoradical generator may be an intramolecular cleavage type photoradical polymerization initiator from the viewpoint of facilitating the progress of the (photomelting) reaction of the photosensitive resin layer 30.

[0062] Examples of hydrogen abstraction type photoradical generators include hexaarylbisimidazole (HABI) compounds, benzophenone compounds, thioxanthone compounds, fluorenone compounds, and α-diketone compounds.

[0063] Examples of HABI compounds include 2,2'-bis(o-chlorophenyl)-4,4',5,5'-tetraphenylbiimidazole (e.g., 2,2'-bis(2-chlorophenyl)-4,4',5,5'-tetraphenyl-1,2'-biimidazole), 2,2'-bis(o-bromophenyl)-4,4',5,5'-tetraphenylbiimidazole, 2,2'-bis(o,p-dichlorophenyl)-4,4',5,5'-tetraphenylbiimidazole, and the like. biimidazole, 2,2'-bis(o-chlorophenyl)-4,4',5,5'-tetra(m-methoxyphenyl)biimidazole, 2,2'-bis(o,o'-dichlorophenyl)-4,4',5,5'-tetraphenylbiimidazole, 2,2'-bis(o-nitrophenyl)-4,4',5,5'-tetraphenylbiimidazole, and 2,2'-bis(o-methylphenyl)-4,4',5,5'-tetraphenylbiimidazole.

[0064] Examples of benzophenone compounds include 4,4'-bis(dimethylamino)benzophenone and 4,4'-bis(diethylamino)benzophenone.

[0065] Examples of thioxanthone compounds include thioxanthone, 2-isopropylthioxanthone, 2-dodecylthioxanthone, 2-cyclohexylthioxanthone, 2,4-diethylthioxanthone, 2,4-dimethylthioxanthone, 1-phenoxythioxanthone, 1-methoxycarbonylthioxanthone, 2-ethoxycarbonylthioxanthone, 3-(2-methoxyethoxycarbonyl)-thioxanthone, 4-butoxycarbonylthioxanthone, 3-butoxycarbonyl-7-methylthioxanthone, 3,4-di-[2-(2-methoxyethoxy)-ethoxycarbonyl]-thioxanthone, 2-chlorothioxanthone, and 1-ethoxycarbonyl thioxanthone-2-carboxylic acid polyethylene glycol esters.

[0066] Examples of fluorenone compounds include 9-fluorenone, 3,4-benzo-9-fluorenone, 2-dimethylamino-9-fluorenone, 2-methoxy-9-fluorenone, 2-chloro-9-fluorenone, 2,7-dichloro-9-fluorenone, 2-bromo-9-fluorenone, 2,7-dibromo-9-fluorenone, 2-nitro-9-fluorenone, and 2-acetoxy-9-fluorenone.

[0067] An example of an α-diketone compound is benzil (a compound also known as diphenylethanedione or dibenzoyl).

[0068] Examples of the intramolecular cleavage type photoradical generator include benzyl ketal-based photoradical generators, α-aminoalkylphenone-based photoradical generators, α-hydroxyalkylphenone-based photoradical generators, α-hydroxyacetophenone-based photoradical generators, and acylphosphine oxide-based photoradical generators.

[0069] An example of a benzyl ketal-based photoradical generator is 2,2-dimethoxy-1,2-diphenylethan-1-one (Omnirad 651).

[0070] Examples of α-aminoalkylphenone photoradical generators include 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butanone-1 (Omnirad 369), 2-methyl-1-[4-(methylthio)phenyl]-2-morpholinopropan-1-one (Omnirad 907), and 2-dimethylamino-2-(4-methyl-benzyl)-1-(4-morpholin-4-yl-phenyl)-butan-1-one (Omnirad 379EG).

[0071] An example of an α-hydroxyalkylphenone-based photoradical generator is 1-hydroxy-cyclohexyl-phenyl-ketone (Omnirad 184).

[0072] Examples of α-hydroxyacetophenone-based photoradical generators include 2-hydroxy-1-{4-[4-(2-hydroxy-2-methyl-propionyl)-benzyl]-phenyl}-2-methyl-propan-1-one (Omnirad 127) and 2-hydroxy-2-methyl-1-phenyl-propan-1-one (Omnirad 1173).

[0073] Examples of acylphosphine oxide photoradical generators include 2,4,6-trimethylbenzoyl-diphenyl-phosphine oxide (OmniradTPO H) and bis(2,4,6-trimethylbenzoyl)-phenylphosphine oxide (Omnirad819).

[0074] The content of the photoradical generator in the thermosetting composition may be 1 mass % or more, 5 mass % or more, or 10 mass % or more, and may be 30 mass % or less, 20 mass % or less, or 15 mass % or less, based on the total amount of the thermosetting composition.

[0075] The thermosetting composition may further contain other components in addition to compound (A), compound (B), the curing accelerator, and the photoradical generator. Examples of other components include additives such as plasticizers, tackifiers, adhesion improvers such as antioxidants, leuco dyes, sensitizers, and coupling agents, polymerization inhibitors, light stabilizers, antifoaming agents, fillers, chain transfer agents, thixotropy-imparting agents, flame retardants, mold release agents, surfactants, lubricants, and antistatic agents. Known additives can be used. The content of other components in the thermosetting composition may be 0 to 95% by mass, 0.01 to 50% by mass, or 0.1 to 10% by mass, based on the total amount of the thermosetting composition.

[0076] By heating the thermosetting composition described above, a (curing) reaction between compound (A) and compound (B) (e.g., a compound having a glycidyl ether group as a cyclic ether group) proceeds, and a cured product of the thermosetting composition is produced. Here, the cured product of the thermosetting composition contains the reaction product of compound (A) and compound (B) and a photoradical generator. The reaction product of compound (A) and compound (B) can be, for example, a compound (polymer) containing a structure represented by the following formula:

[0077] In the formula, X represents a first linking group containing a disulfide bond, and Y represents a second linking group containing a polyether chain. m represents an integer of 1 or more. m may be, for example, 50 or more, 100 or more, 500 or more, or 1000 or more. * represents a bond.

[0078] The heating temperature of the thermosetting composition may be, for example, 0 to 200° C., 30 to 150° C., or 60 to 100° C. The heating time of the thermosetting composition may be, for example, 0.1 to 168 hours, and may be 72 hours or less, 24 hours or less, 12 hours or less, 6 hours or less, 4 hours or less, 3 hours or less, or 2 hours or less.

[0079] The method for forming the photosensitive resin layer 30 containing the reaction product of the compound (A) and the compound (B) and the photoradical generator described above may further include a step of disposing the thermosetting composition on one main surface of the semiconductor wafer 10. In this case, after the thermosetting composition is disposed on one main surface of the semiconductor wafer 10, the thermosetting composition is heated.

[0080] An example of a method for disposing the thermosetting composition on one main surface of the semiconductor wafer 10 is a method in which a varnish of the thermosetting composition is prepared by diluting the thermosetting composition with a solvent, and the prepared varnish is applied to one main surface of the semiconductor wafer 10. Examples of solvents include aromatic hydrocarbons such as toluene, xylene, mesitylene, cumene, and p-cymene; aliphatic hydrocarbons such as hexane and heptane; cyclic alkanes such as methylcyclohexane; cyclic ethers such as tetrahydrofuran and 1,4-dioxane; ketones such as acetone, methyl ethyl ketone, methyl isobutyl ketone, cyclohexanone, and 4-hydroxy-4-methyl-2-pentanone; esters such as methyl acetate, ethyl acetate, butyl acetate, methyl lactate, ethyl lactate, and γ-butyrolactone; carbonates such as ethylene carbonate and propylene carbonate; and amides such as N,N-dimethylformamide, N,N-dimethylacetamide, and N-methyl-2-pyrrolidone (NMP). The solid content of the varnish, that is, the total content of the varnish other than the solvent, may be 10 to 95% by mass, or 15 to 70% by mass, or 20 to 50% by mass, based on the total amount of the varnish.

[0081] In another embodiment, the method for forming the photosensitive resin layer 30 containing the reaction product of the compound (A) and the compound (B) and the photoradical generator described above may further include a step of placing a cured product of the thermosetting composition on one main surface of the semiconductor wafer 10. In this case, after heating the thermosetting composition, the cured product of the thermosetting composition is placed on one main surface of the semiconductor wafer 10. The cured product of the thermosetting composition may be, for example, in the form of a film. The film-like cured product of the thermosetting composition can be produced, for example, by pouring the above-described thermosetting composition into a mold and heating it.

[0082] The photosensitive resin layer 30 is not limited to the above examples, and may be a positive or negative photosensitive resin layer containing any photosensitive material used for photolithography. For example, the photosensitive resin layer 30 may contain any of a positive or negative liquid photoresist, a photosensitive film, a photosensitive solder resist, and a photosensitive polyimide.

[0083] In step (c), the semiconductor wafer 10 is divided along the openings 30a by plasma dicing, thereby forming semiconductor chips 20 each having a first main surface 20a and a second main surface 20b opposite thereto, with the photosensitive resin layer 30 provided on the first main surface 20a.

[0084] Plasma dicing refers to dicing by plasma etching. The conditions for plasma dicing can be set appropriately depending on the type, thickness, etc. of the semiconductor wafer 10. For example, a dry etching device can be used for plasma dicing. For example, a C 4 F 6 Gas, C 4 F 8 Gas or the like can be used.

[0085] Plasma dicing may be performed, for example, by the BOSCH method, which allows cutting of the semiconductor wafer 10 by alternately generating plasma for forming a protective film and plasma for etching. The BOSCH method enables etching with a high aspect ratio.

[0086] In step (d), the photosensitive resin layer 30 on the semiconductor chip 20 is removed.

[0087] The photosensitive resin layer 30 on the semiconductor chip 20 may be removed by, for example, light irradiation and dissolution in a cleaning solution. In this case, the manufacturing method further includes a step of irradiating the photosensitive resin layer 30 on the semiconductor chip 20 with light.

[0088] The light source used for light irradiation can be any of the light sources described above as the light source used for light irradiation in step (b) without any particular limitations. Light irradiation may be performed simultaneously on the photosensitive resin layer 30 on multiple semiconductor chips 20 (e.g., all semiconductor chips 20 present on the same dicing tape 50). In this case, examples of light sources used for light irradiation include mercury lamps (low-pressure mercury lamps, medium-pressure mercury lamps, high-pressure mercury lamps), metal halide lamps, and LED lamps. Light irradiation may be performed directly on the photosensitive resin layer 30 or through glass or the like. Examples of the light to be irradiated include visible light and ultraviolet light. The irradiated light may be, for example, light containing light with a wavelength of 365 nm. The wavelength of the irradiated light may be, for example, 150 to 550 nm.

[0089] The exposure dose of the light irradiation may be within the numerical range described above as the exposure dose of the light irradiation in step (b).

[0090] The cleaning liquid may be any of the developer solutions described above for the step (b) without any particular limitations. The pH of the cleaning liquid may be within the range of the pH of the developer solution described above for the step (b).

[0091] In another embodiment, the photosensitive resin layer 30 on the semiconductor chip 20 may be removed by ashing. The ashing is performed, for example, by a method including irradiating the photosensitive resin layer 30 on the semiconductor chip 20 with plasma generated using oxygen gas.

[0092] In step (e), the semiconductor chip 20 and another semiconductor member 70 are hybrid-bonded so that the first main surface 20a of the semiconductor chip 20 contacts the semiconductor member 70. This results in the semiconductor device 100 shown in FIG.

[0093] The semiconductor chip 20 shown in FIG. 2(e) includes a main body 20A, an electrode 21 provided on one main surface of the main body 20A, and an insulating film 22. The first main surface 20a of the semiconductor chip 20 is a bonding surface for hybrid bonding formed by the electrode 21 and the insulating film 22. Here, the first main surface 20a of the semiconductor chip 20 corresponds to the surface on which the photosensitive resin layer 30 removed in step (d) was provided. The semiconductor member 70 also includes an electrode 71 and an insulating film 72, and the surface 70a of the semiconductor member 70 that contacts the first main surface 20a of the semiconductor chip 20 (hereinafter also referred to as the "first main surface of the semiconductor member 70") is a bonding surface formed by the electrode 71 and the insulating film 72. The semiconductor member 70 may be, for example, a semiconductor wafer or a semiconductor chip. The second main surface 20b of the semiconductor chip 20 may also be a bonding surface formed by an electrode and an insulating film. In this case, multiple semiconductor chips 20 may be stacked by hybrid bonding.

[0094] The electrode 21 and the electrode 71 may each independently contain Cu as a constituent material. The insulating film 22 and the insulating film 72 may each independently contain SiO. 2 The insulating material may include inorganic insulators such as those mentioned above, or organic insulators (including dielectrics).

[0095] As shown in Figure 2 (e), hybrid bonding of the semiconductor chip 20 and another semiconductor member 70 can be performed by a method including the steps of picking up the semiconductor chip 20 from the dicing tape 50, aligning the semiconductor chip 20 and the semiconductor member 70 so that the first main surface 20a of the semiconductor chip 20 contacts the semiconductor member 70, and bonding the semiconductor chip 20 and the semiconductor member 70.

[0096] In the step of picking up the semiconductor chip 20 from the dicing tape 50, for example, a needle is pressed against the dicing tape 50 from below to bend the dicing tape 50, and a suction collet is used to pick up the semiconductor chip 20 from the dicing tape 50. If the dicing tape 50 is an ultraviolet-curing dicing tape whose adhesive strength is reduced by irradiation with ultraviolet light, the adhesive strength of the dicing tape 50 may be reduced by irradiating it with ultraviolet light before this step.

[0097] In the process of aligning the semiconductor chip 20 and the semiconductor member 70 so that the first main surface 20a of the semiconductor chip 20 contacts the semiconductor member 70, the first main surface 20a of the semiconductor chip 20 and the first main surface 70a of the semiconductor member 70 are arranged so that the electrodes 21 and 71, and the insulating films 22 and 72, face each other.

[0098] In the step of bonding the semiconductor chip 20 and the semiconductor member 70, the first main surface 20a of the semiconductor chip 20 is brought into contact with the first main surface 70a of the semiconductor member 70. More specifically, the electrodes 21 and 71, and the insulating films 22 and 72 are brought into contact with each other.

[0099] At least one of heating and pressurization may be performed in the step of bonding the semiconductor chip 20 and the semiconductor member 70. The heating temperature may be, for example, 20° C. or higher, or 200° C. or higher, and may be 500° C. or lower, or 400° C. or lower. The pressurization pressure may be, for example, 0.1 MPa or higher, and 1.0 MPa or lower.

[0100] The above manufacturing method may include a step of activating at least one of the bonding surfaces of the first main surface 20a of the semiconductor chip 20 and the first main surface 70a of the semiconductor member 70 before contacting the first main surface 20a of the semiconductor chip 20 with the first main surface 70a of the semiconductor member 70. When the step of activating the bonding surface is included, bonding between the semiconductor chip 20 and the semiconductor member 70 becomes easier.

[0101] Examples of methods for activating the bonding surfaces include methods for hydrophilizing the bonding surfaces and methods for removing non-active substances (oxide films, etc.) from the bonding surfaces. An example of a method for hydrophilizing the bonding surfaces is a method for irradiating the bonding surfaces with oxygen plasma. An example of a method for removing non-active substances from the bonding surfaces is a method for irradiating the bonding surfaces with an ion beam (e.g., an Ar ion beam) under high vacuum.

[0102] The step of activating the bonding surface may be performed, for example, after the step of removing the photosensitive resin layer 30 on the semiconductor chip 20. Furthermore, the step of activating the bonding surface may be performed before the step of picking up the semiconductor chip 20 from the dicing tape 50 in the step of bonding the semiconductor chip 20 and the semiconductor member 70 together.

[0103] 10...semiconductor wafer, 20...semiconductor chip, 20a...first main surface, 20b...second main surface, 20A...main body portion, 21...electrode, 22...insulating film, 30...photosensitive resin layer, 30a...opening, 50...dicing tape, 70...semiconductor member, 70a...first main surface, 71...electrode, 72...insulating film, 100...semiconductor device.

Claims

1. A method for manufacturing a semiconductor device, comprising the steps of: forming a photosensitive resin layer on one main surface of a semiconductor wafer; removing a portion of the photosensitive resin layer by light irradiation and development using a developer to form an opening exposing the semiconductor wafer; dividing the semiconductor wafer along the opening by plasma dicing to form a semiconductor chip having a first main surface and an opposite second main surface, the photosensitive resin layer being provided on the first main surface; removing the photosensitive resin layer on the semiconductor chip; and hybrid-bonding the semiconductor chip to another semiconductor member so that the first main surface of the semiconductor chip is in contact with the semiconductor member.

2. The method according to claim 1, wherein the developer is a developer containing water.

3. The method according to claim 2, wherein the developer has a pH of 11 or less.

4. The manufacturing method according to claim 1, wherein the photosensitive resin layer is a positive-type photosensitive resin layer.

5. The manufacturing method according to claim 4, further comprising the step of irradiating the photosensitive resin layer on the semiconductor chip with light, and the photosensitive resin layer on the semiconductor chip is removed by dissolving in a cleaning solution.

6. The manufacturing method according to claim 5, wherein the cleaning solution is a cleaning solution containing water.

7. The method according to claim 6, wherein the pH of the cleaning solution is 11 or less.

8. The method according to any one of claims 4 to 7, wherein the developer is a developer containing water.

9. The method according to claim 8, wherein the developer has a pH of 11 or less.

10. The manufacturing method described in claim 8, wherein the photosensitive resin layer contains a reaction product of a polythiol compound having a disulfide bond and a cyclic ether compound having a polyether chain and two or more cyclic ether groups, and a photoradical generator.

Citation Information

Patent Citations

  • Semiconductor device and method for manufacturing the same

    JP2004103738A

  • Method of manufacturing IC card

    JP2004119975A

  • Water soluble mask for substrate dicing by laser and plasma etch

    JP2015159296A

  • Method for manufacturing element chip

    JP2018200957A

  • Product ordering system and method having store addttion function

    KR102333464B1

Cited By

  • Thermosetting composition and cured product thereof, photo-meltable composition, and structural body production method

    EP4410859A4