Method for manufacturing semiconductor device
The semiconductor manufacturing method forms a pattern on a semiconductor wafer using a photomeltable resin to facilitate plasma dicing, eliminating debris and improving chip quality by avoiding laser grooving, thus addressing the issue of debris generation in existing plasma dicing processes.
Patent Information
- Application Number
- PCT/JP2024/012843
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-28
- Publication Date
- 2024-10-03
AI Technical Summary
The existing semiconductor manufacturing methods using plasma dicing generate debris during the laser grooving process, which can reduce the quality of semiconductor chips.
A method involving the formation of a positive photosensitive resin film on a semiconductor wafer, exposure to create a pattern, and subsequent plasma dicing without laser grooving, using a photomeltable resin that becomes low molecular weight upon irradiation, allowing for pattern formation and chip separation with reduced debris generation.
This method enables the formation of semiconductor chips with improved quality by eliminating the need for laser grooving, thereby minimizing debris and enhancing chip quality.
Smart Images

Figure JP2024012843_03102024_PF_FP_ABST
Abstract
Description
Semiconductor device manufacturing method
[0001] The present disclosure relates to a method for manufacturing a semiconductor device.
[0002] A semiconductor device is generally manufactured through the following steps: First, a semiconductor wafer is attached to a dicing tape, and then the semiconductor wafer is divided into semiconductor chips (dicing step). Then, steps such as a pick-up step for picking up the semiconductor chips and a semiconductor chip bonding step for bonding the picked-up semiconductor chips to a support member or the like by thermocompression bonding via an adhesive (die bonding film) or the like are performed, thereby producing a semiconductor device.
[0003] One known dicing method in the dicing process involves plasma etching (dry etching) along the cutting lines of the semiconductor wafer to cut it. This dicing process for processing the semiconductor wafer is called plasma dicing.
[0004] In plasma dicing, a protective film is typically formed on the surface of a semiconductor wafer, and a laser is irradiated along a planned cutting line to remove a portion of the protective film by burning it off (laser grooving), thereby forming a pattern (mask) from the protective film. Laser grooving generates fine cutting material (debris) derived from the protective film, semiconductor wafer, etc., and the debris may remain on the side surfaces of the resulting semiconductor chips, thereby degrading the quality of the semiconductor chips. Patent Document 1 discusses how to suppress the residue of debris during plasma dicing.
[0005] Japanese Patent Application Laid-Open No. 2019-050237
[0006] An object of the present disclosure is to provide a novel method for manufacturing a semiconductor device that includes a step of performing plasma dicing.
[0007] The present disclosure provides a method for manufacturing a semiconductor device according to [1] to [3]. [1] A method for manufacturing a semiconductor device, comprising: forming a positive photosensitive resin film on a surface of a semiconductor wafer; exposing a portion of the positive photosensitive resin film to light to provide an exposed portion in the positive photosensitive resin film; developing the positive photosensitive resin film using a developer and removing the exposed portion to form a pattern; performing plasma dicing using the pattern as a mask to separate the semiconductor wafer into individual patterned semiconductor chips; exposing the pattern of the patterned semiconductor chip; and removing the exposed pattern using a remover to obtain a semiconductor chip from which the pattern has been removed. [2] The method for manufacturing a semiconductor device according to [1], wherein the positive photosensitive resin composition contains a resin that is depolymerized by irradiation with light. [3] The method for manufacturing a semiconductor device according to [2], wherein the developer and the remover are aqueous solvents having a pH of 11 or less.
[0008] According to the present disclosure, a novel method for manufacturing a semiconductor device is provided, which includes a step of performing plasma dicing. The method for manufacturing a semiconductor device according to the present disclosure allows a pattern (mask) to be formed without performing laser grooving, thereby making it possible to suppress the generation of debris itself.
[0009] Fig. 1 is a schematic cross-sectional view for explaining one embodiment of a method for manufacturing a semiconductor device, and Fig. 1(a), Fig. 1(b), Fig. 1(c), and Fig. 1(d) are views showing each step. Fig. 2 is a schematic cross-sectional view for explaining one embodiment of a method for manufacturing a semiconductor device, and Fig. 2(a), Fig. 2(b), Fig. 2(c), Fig. 2(d), and Fig. 2(e) are views showing each step.
[0010] The present embodiment will be described in detail below with reference to the drawings. However, the present disclosure is not limited to the following embodiments. In the following embodiments, the components (including steps, etc.) are not essential unless otherwise specified. The same or equivalent parts are given the same reference numerals, and duplicate explanations will be omitted. Furthermore, unless otherwise specified, positional relationships such as up, down, left, and right will be based on the positional relationships shown in the drawings. The sizes of the components in each figure are conceptual, and the relative size relationships between the components are not limited to those shown in each figure.
[0011] The same applies to the numerical values and ranges in the present disclosure, and do not limit the present disclosure. In this specification, a numerical range indicated using "to" indicates a range that includes the numerical values before and after "to" as the minimum and maximum values, respectively. In the numerical ranges described in stages in this specification, the upper or lower limit value described in one numerical range may be replaced with the upper or lower limit value of another numerical range described in stages. Furthermore, in the numerical ranges described in this specification, the upper or lower limit value of that numerical range may be replaced with a value shown in an example.
[0012] In this specification, the term "layer" includes not only a structure having a shape formed over the entire surface when observed in a plan view, but also a structure having a shape formed on a portion thereof. In this specification, the term "process" includes not only an independent process, but also a process that cannot be clearly distinguished from other processes as long as the intended effect of the process is achieved.
[0013] In this specification, (meth)acrylate means an acrylate or the corresponding methacrylate, and the same applies to other similar expressions such as (meth)acrylic copolymer.
[0014] Unless otherwise specified, each of the components and materials exemplified in this specification may be used alone or in combination of two or more.
[0015] [Method for Manufacturing a Semiconductor Device] The method for manufacturing a semiconductor device according to the present embodiment includes the steps of forming a positive photosensitive resin film on the surface of a semiconductor wafer (hereinafter sometimes referred to as "step (A)"), exposing a portion of the positive photosensitive resin film to light to form an exposed portion in the positive photosensitive resin film (hereinafter sometimes referred to as "step (B)"), developing the positive photosensitive resin film using a developer and removing the exposed portion to form a pattern (hereinafter sometimes referred to as "step (C)"), performing plasma dicing using the pattern as a mask to separate the semiconductor wafer into individual patterned semiconductor chips (hereinafter sometimes referred to as "step (D)"), exposing the pattern of the patterned semiconductor chip (hereinafter sometimes referred to as "step (E)"), and removing the exposed pattern using a remover to obtain a semiconductor chip from which the pattern has been removed (hereinafter sometimes referred to as "step (F)"). FIGS. 1 and 2 are schematic cross-sectional views illustrating one embodiment of the method for manufacturing a semiconductor device.
[0016] <Step (A)> In this step, a positive photosensitive resin film 4 is formed on the surface of a semiconductor wafer 1 .
[0017] The positive photosensitive resin film 4 is a resin film in which exposed portions with increased solubility are removed and unexposed portions remain by treating with a developer. The positive photosensitive resin film 4 may contain, for example, a known positive photoresist material.
[0018] The positive photosensitive resin film 4 may contain a resin that is degraded by irradiation with light (hereinafter, sometimes referred to as a "photofusible resin"). The photofusible resin may be a resin that is degraded by irradiation with light, and has properties such as a decrease in elastic modulus and an increase in loss tangent (tan δ). The photofusible resin may be a water-insoluble resin that is degraded by irradiation with light, and has the property of forming a water-soluble gel or liquid substance (increasing solubility in aqueous solvents).
[0019] In one embodiment, the photo-fusible resin may be a reaction product of a compound A having a disulfide bond and two or more thiol groups, and a compound B having two or more functional groups reactive with thiol groups. The positive photosensitive resin film 4 may further contain a photoradical generator in addition to the photo-fusible resin. The positive photosensitive resin film 4 may further contain a curing accelerator or the like that accelerates the reaction between the compound A and the compound B.
[0020] The mechanism by which the photo-fusible resin is degraded (melted) is not entirely clear, but the following mechanisms are considered. However, the mechanism is not limited to these. The photo-fusible resin contains a compound having a disulfide bond (a reaction product of compound A and compound B). When the photo-fusible resin contained in the positive photosensitive resin film 4 is irradiated with light, the disulfide bond in the photo-fusible resin is decomposed (cleaved), generating thiyl radicals. If a photo-radical generator (intramolecular cleavage-type photo-radical generator) is present at this time, the thiyl radical reacts with the photo-radical generator, and the thiyl radical is capped by the photo-radical generator. It is believed that this degrading the molecular weight of the compound having a disulfide bond causes the cured product to photosoften (photo-melt). Another possible mechanism is that photoinduced radicals generated by a photoradical generator (intramolecular cleavage-type photoradical generator) react directly with disulfide bonds, forming a photoinduced radical-thioether bond and generating a thiyl radical, which then reacts with another photoinduced radical, lowering the molecular weight of the compound containing the disulfide bond and softening the photocured material. The reaction in which a disulfide bond is cleaved can be said to be an irreversible reaction.
[0021] The positive photosensitive resin film 4 containing a photo-fusible resin can be formed, for example, by disposing a curable composition containing compound A, compound B, a photoradical generator, and, if necessary, a curing accelerator on the surface of the semiconductor wafer 1, and curing the curable composition by heating or light irradiation (reacting compound A and compound B). In this case, the positive photosensitive resin film 4 can be said to contain a cured product of the curable composition. The cured product of the curable composition can be said to contain a reaction product of compound A and compound B and a photoradical generator. The curable composition may be a thermosetting composition that cures by heating, or a photocurable composition that cures by light irradiation, with a thermosetting composition being preferred. The components of the curable composition are described below.
[0022] (Compound A) Compound A is a compound having a disulfide bond (-S-S-) and two or more thiol groups (-SH). The upper limit of the number of thiol groups in compound A may be, for example, 10 or less, 8 or less, 6 or less, or 4 or less. Component (A) may be, for example, a dithiol compound, which is a compound having two thiol groups (-SH). Component (A) may be a high-molecular-weight component of a polymer or oligomer. A compound having two thiol groups (-SH) can be considered to be a compound consisting of two thiol groups and a group (first linking group) that contains a disulfide bond and links the two thiol groups.
[0023] The molecular weight or number average molecular weight of compound A may be, for example, 100 to 10,000,000, 200 to 3,000,000, 300 to 1,000,000, 400 to 10,000, or 500 to 5,000. The number average molecular weight is a polystyrene-equivalent value obtained by gel permeation chromatography (GPC) using a calibration curve with standard polystyrene.
[0024] Compound A has one or more (two or more) disulfide bonds in the molecule. The number of disulfide bonds in Compound A may be, for example, 1 to 1,000 or 4 to 50.
[0025] Compound A may be a compound (e.g., a polymer or oligomer) having a linear or branched molecular chain and an end group, with a disulfide bond in the molecular chain. In this case, the end group in compound A may be a thiol group. When the curable composition contains such a compound as compound A, the photo-melting property of the photo-meltable resin (the reaction product of compound A and compound B) tends to be further improved. The molecular chain in compound A may contain a disulfide bond and a polyether chain, or may be composed of a disulfide bond and a polyether chain.
[0026] Compound A is, for example, a compound represented by formula (1): HS-(X-S-S) n1 In the formula, X represents a polyether chain. Multiple Xs may be the same or different. n1 represents an integer of 1 or greater. n1 may be, for example, 1 or greater, or 4 or greater, or 1000 or less. When component (A) is a compound represented by formula (1), -(X-S-S) n1 The group represented by -X- is a first linking group. The compound obtained by chain extension of compound (1) may be, for example, a Michael adduct of compound (1) or a thiourethanized product of compound (1).
[0027] The polyether chain represented by X may be, for example, a polyoxyalkylene chain. 1 -O-X 2 -O-X 3 X may be a group represented by the formula: 1 ~X 3 may each independently be an alkylene group, and may be an alkylene group having 1 to 2 carbon atoms (for example, a methylene group or an ethylene group). Examples of the polyether chain represented by X include -CH 2 CH 2 -O-CH 2 -O-CH 2 CH 2 - etc.
[0028] Examples of commercially available products of Compound A include the Thiokol LP series (dithiols having a disulfide bond, manufactured by Toray Fine Chemicals Co., Ltd.). Compound A can also be obtained by converting the reactive functional group of a compound having a terminal reactive functional group (e.g., a carboxy group or a hydroxy group) and a disulfide bond to a thiol group. Examples of compounds having a terminal reactive functional group and a disulfide bond include 3,3'-dithiodipropionic acid (manufactured by Tokyo Chemical Industry Co., Ltd.), dithiodiethanol, and cystamine.
[0029] The content of compound A may be 15% by mass or more, 25% by mass or more, or 35% by mass or more, and may be 80% by mass or less, 70% by mass or less, or 60% by mass or less, based on the total amount of the curable composition (solid content excluding the solvent).
[0030] (Compound B) Compound B is a compound having two or more functional groups capable of reacting with a thiol group. Examples of the functional group capable of reacting with a thiol group include cyclic ether groups (oxirane groups (oxiranyl groups, epoxy groups), oxetane groups (oxetanyl groups), tetrahydrofuryl groups, tetrahydropyranyl groups, etc.); isocyanate groups; and ethylenically unsaturated groups (C=C). The upper limit of the number of functional groups in Compound B may be, for example, 10 or less, 8 or less, 6 or less, or 4 or less.
[0031] Compound B may be compound B1 having a polyether chain and two or more cyclic ether groups. When the curable composition contains compound B1 as compound B, low-molecular-weight components generated by irradiating the photo-fusible resin with light tend to have many polyether chains or hydroxyl groups and exhibit water solubility, making it possible to remove the low-molecular-weight components with an aqueous solvent.
[0032] The cyclic ether group may be an oxirane group from the viewpoints of reactivity and availability. That is, compound B1 is an oxirane compound (epoxy compound) having a polyether chain and two or more oxirane groups (oxiranyl groups, epoxy groups). In this specification, the cyclic ether group includes a group having a cyclic ether structure (a structure containing a cyclic ether group). For example, the oxirane group includes a group having an oxirane structure (a structure containing an oxirane group (oxiranyl group, epoxy group)), such as a glycidyl group, a glycidyl ether group, or an epoxycyclohexyl group.
[0033] The molecular weight or number average molecular weight of compound B1 may be, for example, 100 to 1,000,000, 100 to 500,000, 100 to 10,000, 150 to 5,000, or 200 to 2,000. The number average molecular weight is a polystyrene-equivalent value obtained by gel permeation chromatography (GPC) using a calibration curve with standard polystyrene.
[0034] When the cyclic ether group of compound B1 is an oxirane group (oxiranyl group, epoxy group), the epoxy equivalent of component (B) may be 50 to 2000 g / eq, 80 to 1500 g / eq, or 100 to 1000 g / eq.
[0035] Compound B1 may be compound B1a having two cyclic ether groups or compound B1b having three or more cyclic ether groups. Compound B1a may be a compound (e.g., a polymer or oligomer) having a linear molecular chain and terminal groups, with a polyether chain in the molecular chain. In this case, the terminal group in compound B1a may be a cyclic ether group. Compound B1a can be considered a compound consisting of two cyclic ether groups and a group (second linking group) containing a polyether chain and connecting the two cyclic ether groups. Compound B1b may be compound B1a having one or more cyclic ether groups as a side chain or substituent of the second linking group. Compound B1 may contain both compound B1a and compound B1b, as this can further shorten the curing time and further improve photomeltability and water solubility.
[0036] Compound B1a may be a compound (e.g., a polymer or oligomer) having a linear molecular chain and an end group, and having a polyether chain in the molecular chain. In this case, the end group in compound B1a may be a cyclic ether group. When compound B is compound B1a, low molecular weight components generated by irradiating the photo-fusible resin with light tend to be easily removed with an aqueous solvent. The polyether chain as a molecular chain may have a substituent such as a hydroxyl group or an alkyl group optionally having a hydroxyl group. The molecular chain in compound B1a may contain a polyether chain or may consist of a polyether chain.
[0037] Compound B1a can be, for example, a compound represented by formula (2): Z-(Y) n2 In the formula, Y represents a polyether chain, and Z represents a cyclic ether group. A plurality of Z's may be the same or different. n2 represents an integer of 1 or more. n2 may be, for example, 1 or more, or 2 or more, or 1000 or less. When compound B1a is compound (2), -(Y) n2 The group represented by - is the second linking group.
[0038] The polyether chain represented by Y may be, for example, a polyoxyalkylene chain. 1 -O-Y 2 -O-Y 3 Y may be a group represented by -. 1 ~Y 3 may each independently be an alkylene group, and may be an alkylene group having 1 to 3 carbon atoms (for example, a methylene group, an ethylene group, or a propylene group). Examples of the polyether chain represented by Y include -CH 2 CH 2 -O-CH 2 -CH 2 -O-CH 2 CH 2 - etc.
[0039] Commercially available products of compound B1a include, for example, Denacol EX series (EX-850, EX-851, EX-821, EX-830, EX-832, EX-841, EX-861, EX-920, manufactured by Nagase ChemteX Corporation).
[0040] Compound B1b can be a compound having one or more cyclic ether groups as side chains of the second linking group (polyether chain as Y) in compound B1a.
[0041] Commercially available products of compound B1b include, for example, Denacol EX series (EX-614B, EX-313, EX-512, EX-521, manufactured by Nagase ChemteX Corporation).
[0042] The mass ratio of the content of compound B1b to the total content of compound B1a and compound B1b (content (mass) of compound B1b / total content (mass) of compound B1a and compound B1b) may be 0.01 to 0.40. When this mass ratio is 0.01 or more, the curing time of the curable composition tends to be further shortened, and when this mass ratio is 0.40 or less, the photomeltability and water solubility tend to be further improved. This mass ratio may be 0.02 or more or 0.03 or more, or may be 0.35 or less, 0.30 or less, 0.25 or less, 0.20 or less, 0.15 or less, or 0.10 or less.
[0043] The content of compound B may be 10% by mass or more, 20% by mass or more, or 30% by mass or more, and may be 60% by mass or less, 50% by mass or less, or 40% by mass or less, based on the total amount of the curable composition (solid content excluding the solvent).
[0044] The ratio of the total number of moles of thiol groups in compound A to the total number of moles of functional groups in compound B may be, for example, 0.90 or more or 0.95 or more, and may be 1.10 or less or 1.05 or less.
[0045] (Photoradical generator) The photoradical generator is a component that generates radicals when irradiated with light. For example, a component used as a photopolymerization initiator can be used as the photoradical generator. Examples of the photoradical generator include an intramolecular cleavage-type photoradical polymerization initiator that photocleaves the photoradical generator itself when irradiated with light to generate two radicals.
[0046] Examples of the intramolecular cleavage type photoradical generator include a benzyl ketal-based photoradical generator, an α-aminoalkylphenone-based photoradical generator, an α-hydroxyalkylphenone-based photoradical generator, an α-hydroxyacetophenone-based photoradical generator, and an acylphosphine oxide-based photoradical generator.
[0047] Examples of benzyl ketal photoradical generators include 2,2-dimethoxy-1,2-diphenylethan-1-one (Omnirad 651).
[0048] Examples of α-aminoalkylphenone photoradical generators include 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butanone-1 (Omnirad369), 2-methyl-1-[4-(methylthio)phenyl]-2-morpholinopropan-1-one (Omnirad907), and 2-dimethylamino-2-(4-methyl-benzyl)-1-(4-morpholin-4-yl-phenyl)-butan-1-one (Omnirad379EG).
[0049] Examples of the α-hydroxyalkylphenone-based photoradical generator include 1-hydroxy-cyclohexyl-phenyl-ketone (Omnirad 184).
[0050] Examples of the α-hydroxyacetophenone-based photoradical generator include 2-hydroxy-1-{4-[4-(2-hydroxy-2-methyl-propionyl)-benzyl]-phenyl}-2-methyl-propan-1-one (Omnirad 127) and 2-hydroxy-2-methyl-1-phenyl-propan-1-one (Omnirad 1173).
[0051] Examples of acylphosphine oxide photoradical generators include 2,4,6-trimethylbenzoyl-diphenyl-phosphine oxide (OmniradTPO 3 H), bis(2,4,6-trimethylbenzoyl)-phenylphosphine oxide (Omnirad 819), and the like.
[0052] The content of the photoradical generator may be 1 mass % or more, 3 mass % or more, or 5 mass % or more, and may be 30 mass % or less, 20 mass % or less, or 15 mass % or less, based on the total amount of the curable composition (solid content excluding the solvent).
[0053] The ratio of the number of moles of the photoradical generator to the number of moles of compound A (number of moles of photoradical generator / number of moles of compound A) may be 0.1 or more, 0.2 or more, or 0.3 or more, since this further improves the photosoftening property.
[0054] (Curing Accelerator) The curing accelerator is a component for accelerating the reaction between Compound A and Compound B, and includes a component (catalytic curing agent) that functions as a catalyst for the curing reaction. Examples of the curing accelerator include amine compounds, imidazole derivatives, quaternary ammonium salts, organic metal salts, and phosphorus compounds.
[0055] Examples of the amine compound include dicyandiamide, trimethylamine, triethylamine, tripropylamine, tributylamine, tri-n-octylamine, dimethylethylamine, dimethylpropylamine, dimethylbutylamine, dimethyl-n-octylamine, 1,4-diazabicyclo[2.2.2]octane, 1,8-diazabicyclo[5.4.0]undec-7-ene, benzyldimethylamine, 4-methyl-N,N-dimethylbenzylamine, 2,4,6-tris(dimethylaminomethyl)phenol, and 4-dimethylaminopyridine.
[0056] Examples of the imidazole derivatives include 1-(1-cyanomethyl)-2-ethyl-4-methyl-1H-imidazole, 2-ethyl-4-methylimidazole, 2-methylimidazole, 2-phenylimidazole, 1-cyanoethyl-2-phenylimidazole, 2-phenyl-4,5-dihydroxymethylimidazole, 2-phenyl-4-methyl-5-hydroxymethylimidazole, 2,4,5-triphenylimidazole, 1-benzyl-2-imidazole, 1,2-dimethylimidazole, and 1-benzyl-2-phenylimidazole.
[0057] Examples of quaternary ammonium salts include tetramethylammonium chloride, tetraethylammonium chloride, tetrabutylammonium chloride, benzyltrimethylammonium chloride, benzyltriethylammonium chloride, benzyltributylammonium chloride, tetramethylammonium bromide, tetraethylammonium bromide, tetrabutylammonium bromide, benzyltrimethylammonium bromide, benzyltriethylammonium bromide, tetramethylammonium iodide, tetraethylammonium iodide, tetrabutylammonium iodide, and benzyltributylammonium iodide.
[0058] Examples of the organic metal salt include zinc(II) bis(2,4-pentanedionato), zinc octylate, zinc naphthenate, cobalt naphthenate, copper naphthenate, iron acetylacetonate, nickel octylate, and manganese octylate.
[0059] Examples of the phosphorus compound include tetraphenylphosphonium tetra-p-tolylborate, tetraphenylphosphonium tetraphenylborate, triphenylphosphine, tri-p-tolylphosphine, tris(4-chlorophenyl)phosphine, tris(4-methoxyphenyl)phosphine, tris(2,6-dimethoxyphenyl)phosphine, triphenylphosphine triphenylborane, tetraphenylphosphonium dicyanamide, and tetraphenylphosphonium tetra(4-methylphenyl)borate.
[0060] The content of the curing accelerator may be 0.01 mass % or more, 0.1 mass % or more, or 0.5 mass % or more, and may be 10 mass % or less, 5 mass % or less, or 2 mass % or less, based on the total amount of the curable composition (solid content excluding the solvent).
[0061] The curable composition may further contain components (other components) that do not fall under the category of compound A, compound B, photoradical generator, or curing accelerator. Examples of other components include additives such as plasticizers; tackifiers (e.g., tackifiers); antioxidants; leuco dyes; sensitizers; adhesion improvers (e.g., coupling agents); polymerization inhibitors; light stabilizers; antifoaming agents; fillers; chain transfer agents; thixotropy-imparting agents; flame retardants; mold release agents; surfactants; lubricants; and antistatic agents. Known additives can be used as these additives. When the curable composition contains other components, the total content of the other components may be 0 to 95% by mass, 0.01 to 50% by mass, or 0.1 to 10% by mass, based on the total amount of the curable composition.
[0062] The curable composition may be used as a varnish of the curable composition diluted with a solvent. Examples of the solvent include aromatic hydrocarbons such as toluene, xylene, mesitylene, cumene, and p-cymene; aliphatic hydrocarbons such as hexane and heptane; cyclic alkanes such as methylcyclohexane; cyclic ethers such as tetrahydrofuran and 1,4-dioxane; ketones such as acetone, methyl ethyl ketone, methyl isobutyl ketone, cyclohexanone, and 4-hydroxy-4-methyl-2-pentanone; esters such as methyl acetate, ethyl acetate, butyl acetate, methyl lactate, ethyl lactate, and γ-butyrolactone; carbonates such as ethylene carbonate and propylene carbonate; and amides such as N,N-dimethylformamide, N,N-dimethylacetamide, and N-methyl-2-pyrrolidone (NMP). The solid content of the varnish, that is, the content of the varnish other than the solvent, may be 10 to 95 mass %, 15 to 70 mass %, or 20 to 50 mass % based on the total mass of the varnish.
[0063] Step (A) includes, for example, a step of preparing a laminate 10 including a dicing tape 2 (dicing film) and a semiconductor wafer 1 provided on the dicing tape 2 (see FIG. 1(a)), and a step of disposing a positive photoresist material on the surface of the semiconductor wafer 1 to form a positive photosensitive resin film 4 (see FIG. 1(b)).
[0064] When the positive photosensitive resin film 4 contains a photo-fusible resin, the step (A) includes, for example, a step of preparing a laminate 10 (see FIG. 1( a)), a step of disposing a curable composition on the surface of the semiconductor wafer 1, and a step of curing the curable composition to form a positive photosensitive resin film 4 containing a cured product of the curable composition (see FIG. 1( b)).
[0065] Examples of the semiconductor wafer 1 include single crystal silicon, polycrystalline silicon, various ceramics, and compound semiconductors such as gallium arsenide. The semiconductor wafer 1 may have electrodes such as through electrodes.
[0066] The thickness of the semiconductor wafer 1 may be, for example, 10 to 1000 μm, 20 to 900 μm, or 30 to 800 μm.
[0067] Examples of the dicing tape 2 (dicing film) include plastic films such as polytetrafluoroethylene film, polyethylene terephthalate film, polyethylene film, polypropylene film, polymethylpentene film, and polyimide film. Furthermore, the dicing tape may be subjected to surface treatments such as primer application, UV treatment, corona discharge treatment, polishing treatment, and etching treatment, as needed. The dicing tape may be adhesive. Such a dicing tape may be the above-mentioned plastic film to which adhesive properties have been imparted, or may be the above-mentioned plastic film to which an adhesive layer has been provided on one side. The adhesive layer may be made of an ultraviolet-curable adhesive or a non-ultraviolet-curable adhesive. The ultraviolet-curable adhesive or non-ultraviolet-curable adhesive is not particularly limited as long as it has sufficient adhesive strength to prevent the semiconductor chips from scattering during the dicing process, and conventionally known adhesives can be used.
[0068] The thickness of the dicing tape 2 may be, for example, 10 to 1000 μm, 30 to 500 μm, or 50 to 300 μm.
[0069] The laminate 10 can be obtained by laminating the semiconductor wafer 1 to the adhesive surface of the dicing tape 2 or the surface on which an adhesive layer is provided.
[0070] The laminate 10 may further include a dicing ring 3 disposed on the dicing tape 2 so as to surround the semiconductor wafer 1. The dicing ring 3 is a ring-shaped jig for fixing the semiconductor wafer 1 in the dicing process.
[0071] The curable composition can be prepared, for example, by a method including a step of mixing or kneading the above-mentioned components. The mixing and kneading can be carried out using an appropriate combination of dispersing machines such as a conventional mixer, a mortar and pestle, a triple-roll mill, a ball mill, or a bead mill.
[0072] The method for disposing the curable composition on the surface of the semiconductor wafer is not particularly limited, and examples thereof include a method of applying the curable composition to the surface of the semiconductor wafer 1 using a spin coater, a bar coater, or the like, and a method of forming the curable composition into a film and attaching (transferring) the formed curable composition film to the semiconductor wafer 1. The curable composition film may be in a semi-cured state (B-stage state) before bonding the curable composition film to the semiconductor wafer 1. The curable composition may be disposed, for example, on the circuit-forming surface of the semiconductor wafer 1.
[0073] A cured product of the curable composition can be obtained, for example, by heating the curable composition. By heating the curable composition, the reaction between compound A and compound B proceeds. At this time, a curing accelerator can accelerate the reaction. The reaction product (photo-fusible resin) of compound A and compound B can be, for example, a compound (polymer) including a structure represented by the following formula. On the other hand, the photo-radical generator is less involved in the reaction, and the cured product of the curable composition can include the reaction product (photo-fusible resin) of compound A and compound B and the photo-radical generator.
[0074]
[0075] In the formula, X represents a first linking group, and Y represents a second linking group. m represents an integer of 1 or more. m may be, for example, 50 or more, 100 or more, 500 or more, or 1000 or more. * represents a bond.
[0076] The heating temperature of the curable composition may be, for example, 0 to 200° C., 30 to 150° C., or 60 to 100° C. The heating time of the curable composition may be, for example, 0.1 to 168 hours, and may be 72 hours or less, 48 hours or less, or 24 hours or less.
[0077] The positive photosensitive resin film 4 may be in a (completely) cured state (C-stage state). The thickness of the positive photosensitive resin film 4 may be, for example, 10 to 1000 μm, 30 to 500 μm, or 50 to 200 μm.
[0078] In this manner, a positive photosensitive resin film 4 containing a photo-fusible resin can be formed on the surface of the semiconductor wafer 1 .
[0079] <Step (B)> In this step, a part of the positive photosensitive resin film 4 is exposed to light to provide an exposed portion 4 a in the positive photosensitive resin film 4 .
[0080] The exposure is performed on the positive photosensitive resin film 4, for example, along the planned cutting line of the semiconductor wafer 1. This makes it possible to provide the positive photosensitive resin film 4 with exposed portions 4a where exposure has been performed and unexposed portions 4b where exposure has not been performed (see FIG. 1(c)).
[0081] The irradiation device and irradiation light for performing the exposure are not particularly limited as long as they can provide the exposed portions 4 a and the unexposed portions 4 b. The exposure can be performed, for example, by irradiating laser light A using a laser irradiation device 5. By using the laser irradiation device 5, the laser light A can be selectively irradiated onto desired portions of the positive photosensitive resin film 4 along the planned cutting line of the semiconductor wafer 1, thereby providing the exposed portions 4 a and the unexposed portions 4 b.
[0082] The laser light A irradiated onto the positive photosensitive resin film 4 may be, for example, ultraviolet light or visible light. When the positive photosensitive resin film 4 contains a photo-fusible resin, the wavelength of the laser light A can be set arbitrarily depending on, for example, the type of photo-radical generator used. The wavelength of the laser light A may be, for example, 150 to 550 nm.
[0083] As the laser irradiation device 5, for example, a laser marking device, a laser scribing device, a spotlight type irradiation device, or the like can be used.
[0084] Other exposure methods include exposure through a photomask or reticle using an exposure device, as is done in conventional photolithography. Examples of the exposure device that can be used include contact aligners, mirror projection, and stepper exposure devices. Examples of the light source include low-pressure mercury lamps, high-pressure mercury lamps, ultra-high-pressure mercury lamps, and halogen lamps.
[0085] <Step (C)> In this step, the positive photosensitive resin film 4 is developed using a developer to remove the exposed portions 4 a, thereby forming a pattern 6 .
[0086] The developer used for development may be an aqueous solvent containing an alkaline compound such as sodium hydroxide, potassium hydroxide, sodium hydrogen carbonate, sodium carbonate, sodium silicate, tetramethylammonium hydroxide, or an organic amine.
[0087] Examples of the aqueous solvent include water and a mixed solvent of water and a hydrophilic organic solvent. In the mixed solvent of water and a hydrophilic organic solvent, the proportion of water can be, for example, 80% by mass or more. The aqueous solvent may contain additives such as a pH adjuster, a detergent, and a surfactant.
[0088] The aqueous solvent may be water. Examples of water include tap water, natural water, purified water, distilled water, ion-exchanged water, pure water, and ultrapure water (such as Milli-Q water). Milli-Q water refers to ultrapure water obtained using a Milli-Q water production system manufactured by Merck Millipore (Merck). Since the water has reduced impurities, it may be purified water, distilled water, ion-exchanged water, pure water, or ultrapure water.
[0089] Examples of the hydrophilic organic solvent include alcohols such as methanol, ethanol, 2-propanol, and 1,2-propanediol; and glycol ethers such as ethylene glycol monomethyl ether, propylene glycol monomethyl ether, ethyl cellosolve, propylene glycol monopropyl ether, propylene glycol monoisopropyl ether, butyl cellosolve, ethylene glycol monoisobutyl ether, propylene glycol monobutyl ether, diethylene glycol dimethyl ether, diethylene glycol diethyl ether, and dipropylene glycol monomethyl ether.
[0090] Examples of pH adjusters include inorganic acids, inorganic bases, organic acids, and organic bases. Examples of inorganic acids include nitric acid, sulfuric acid, hydrochloric acid, phosphoric acid, and boric acid. Examples of inorganic bases include sodium hydroxide, potassium hydroxide, and calcium hydroxide. Examples of organic acids include formic acid, acetic acid, propionic acid, butyric acid, acrylic acid, benzoic acid, and picolinic acid. Examples of organic bases include primary amines, secondary amines, tertiary amines, tetramethylammonium hydroxide, tetraethylammonium hydroxide, and imidazole-based compounds.
[0091] When the positive-type photosensitive resin film 4 contains a photofusible resin, the developer used for development may be an aqueous solvent with a pH of 11 or less. Note that pH refers to the hydrogen ion exponent. Low-molecular-weight components generated by irradiating the photofusible resin with light tend to have many polyether chains or hydroxyl groups and exhibit water solubility. Therefore, the low-molecular-weight components can be removed with a weakly alkaline aqueous solvent or an aqueous solvent that does not contain alkaline compounds. Furthermore, using an aqueous solvent with a pH of 11 or less as the developer can prevent problems such as chip scattering due to reduced adhesion of the dicing tape 2 to the semiconductor wafer 1, infiltration of the developer onto the backside of the chip, embrittlement of the dicing tape 2, defects in subsequent assembly steps due to swelling, and corrosion of the dicing ring 3. The pH of the aqueous solvent may be 10 or less, 9 or less, or 8 or less, or 4 or more, 5 or more, or 6 or more.
[0092] The positive photosensitive resin film 4 is developed using a developer (the exposed portions 4a are removed using the developer), leaving unexposed portions 4b on the semiconductor wafer 1, thereby forming a pattern 6. In this manner, a laminate 20 can be obtained that includes the dicing tape 2, the semiconductor wafer 1 provided on the dicing tape 2, and the pattern 6 formed on the semiconductor wafer 1 (see FIG. 1(d)).
[0093] <Step (D)> In this step, the semiconductor wafer 1 is divided into individual pieces by performing plasma dicing using the pattern 6 as a mask, thereby obtaining patterned semiconductor chips 8 .
[0094] The plasma used in plasma dicing is generated in a plasma generator 7 under conditions that etch the semiconductor wafer 1. The etching conditions can be appropriately selected depending on the material of the semiconductor wafer 1. When the semiconductor wafer 1 is made of silicon, the Bosch process can be used for etching. In the Bosch process, etching progresses in the depth direction in the portions S on the surface of the semiconductor wafer 1 that are not covered by the pattern 6 (mask) by sequentially repeating a protective film formation step, a protective film etching (anisotropic etching) step, and a Si etching (isotropic etching) step (see FIG. 2( a)).
[0095] In the protective film forming process, for example, C is used as a raw material gas in the plasma generating device 7. 4 F 8 While supplying the above, a medium vacuum (10 -1 ~10 2 The pressure is adjusted to 1 Pa (Pa) and plasma is generated. This makes it possible to form a protective film on the Si surface or the like.
[0096] The protective film etching process is carried out, for example, in a plasma generating device 7 using SF as a raw material gas. 6 While supplying the above, a medium vacuum (10 -1 ~10 2 The pressure is adjusted to 1 Pa (Pa) and plasma is generated, which allows etching of the protective film on the Si surface.
[0097] The Si etching process is carried out, for example, in a plasma generating device 7 using SF as a raw material gas. 6 While supplying the above, a medium vacuum (10 -1 ~10 2 The pressure is adjusted to 1 Pa (Pa) and plasma is generated, which allows etching of the Si surface.
[0098] In this way, a laminate 30 can be obtained which includes the dicing tape 2 and a plurality of patterned semiconductor chips 8 provided on the dicing tape 2, each having a semiconductor chip 1a and a pattern 6 (see FIG. 2(b)).
[0099] <Step (E)> In this step, the pattern 6 of the patterned semiconductor chip 8 is exposed to light.
[0100] The pattern 6 is exposed to light (see FIG. 2C), which increases the solubility of the pattern 6 in a remover solution, which will be described later.
[0101] The light B irradiated onto the pattern 6 may be, for example, ultraviolet light or visible light. When the positive photosensitive resin film 4 contains a photo-fusible resin, the wavelength of the light B can be appropriately selected depending on, for example, the type of photo-radical generator used. The wavelength of the light B may be, for example, 150 to 550 nm.
[0102] The light B is irradiated using, for example, a light irradiation device 9 at an irradiation dose of 1000 mJ / cm 2 The irradiation amount can be appropriately set depending on, for example, the wavelength of the light B. For example, the irradiation amount is 3000 mJ / cm 2 Above, 5000mJ / cm 2 or more, or 10,000 mJ / cm 2 or more, 100,000 mJ / cm 2 Below, 80000mJ / cm 2 or less, or 60,000 mJ / cm 2 It may be the following:
[0103] The irradiation amount means the product of illuminance and irradiation time (seconds). Examples of light sources for irradiating ultraviolet light or visible light include low-pressure mercury lamps, medium-pressure mercury lamps, high-pressure mercury lamps, metal halide lamps, and LED lamps.
[0104] <Step (F)> In this step, the exposed pattern 6 is removed using a remover to obtain a semiconductor chip 1a from which the pattern 6 has been removed from the patterned semiconductor chip 8.
[0105] Examples of the remover used to remove the pattern 6 include the same as the developer. The remover may be an aqueous solvent containing an alkaline compound, and when the positive photosensitive resin film 4 contains a photo-fusible resin, the remover may be an aqueous solvent having a pH of 11 or less. The pH of the aqueous solvent may be 10 or less, 9 or less, or 8 or less, or may be 4 or more, 5 or more, or 6 or more.
[0106] In conventional semiconductor device manufacturing methods that include a plasma dicing process, processes such as high-pressure cleaning and ashing may be performed to remove the pattern (mask). The method for removing pattern 6 in this embodiment does not require processes such as high-pressure cleaning and ashing, and therefore can be said to be a simpler method than conventional methods. By removing pattern 6, a stacked body 40 including dicing tape 2 and multiple semiconductor chips 1a provided on dicing tape 2 can be obtained (see FIG. 2(d)).
[0107] The method for manufacturing a semiconductor device of this embodiment may further include a step of irradiating the adhesive layer of the dicing tape with ultraviolet light (hereinafter, sometimes referred to as "step (G)"), a step of picking up a semiconductor chip (hereinafter, sometimes referred to as "step (H)"), a step of thermocompressing the picked-up semiconductor chip and a support member via an adhesive layer (such as a die bonding film) (hereinafter, sometimes referred to as "step (I)"), and a heat curing step of heat curing the adhesive layer (hereinafter, sometimes referred to as "step (J)").
[0108] <Step (G)> When the adhesive layer of the dicing tape 2 is made of an ultraviolet-curable adhesive, the method for manufacturing a semiconductor device may include step (G). In this step, the adhesive layer is irradiated with ultraviolet light. The wavelength of the ultraviolet light may be 200 to 400 nm. The ultraviolet light irradiation conditions are an illuminance and an irradiation amount of 30 to 240 mW / cm. 2 and 50 to 500 mJ / cm 2 may be in the range of
[0109] <Step (H)> In this step, the individual semiconductor chips 1a are spaced apart from one another, and the semiconductor chips 1a pushed up by needles from the dicing tape 2 side are sucked by a suction collet and picked up from the dicing tape 2.
[0110] The ultraviolet irradiation step and the pick-up step may be carried out after step (E) and step (F), or may be carried out before step (E) and step (F).
[0111] <Step (I)> In this step, the picked-up semiconductor chip 1 a and the support member 11 are bonded by thermocompression via an adhesive layer 12 (such as a die bonding film). The die bonding film may be a die bonding film used in the relevant field. Multiple semiconductor chips 1 a may be bonded to the support member 11.
[0112] The heating temperature in the thermocompression bonding may be, for example, 80 to 160° C. The load in the thermocompression bonding may be, for example, 5 to 15 N. The heating time in the thermocompression bonding may be, for example, 0.5 to 20 seconds.
[0113] <Step (J)> In this step, the adhesive layer 12 is thermally cured. The heating temperature can be appropriately changed depending on the constituent components of the die bonding film. The heating temperature may be, for example, 60 to 200°C, 90 to 190°C, or 120 to 180°C. The heating time may be 30 minutes to 5 hours, 1 to 3 hours, or 2 to 3 hours. The temperature or pressure may be changed stepwise during the heating process.
[0114] In this way, a semiconductor device 100 (see Figure 2 (e)) can be manufactured, which includes a semiconductor chip 1a, a support member 11 on which the semiconductor chip 1a is mounted, and an adhesive layer 12 provided between the semiconductor chip 1a and the support member 11 and bonding the semiconductor chip 1a and the support member 11 together.
[0115] According to the present disclosure, a novel method for manufacturing a semiconductor device is provided, which includes a step of performing plasma dicing. The method for manufacturing a semiconductor device according to the present disclosure allows a pattern (mask) to be formed without performing laser grooving, thereby making it possible to suppress the generation of debris itself.
[0116] 1...semiconductor wafer, 1a...semiconductor chip, 2...dicing tape, 3...dicing ring, 4...positive photosensitive resin film, 4a...exposed portion, 4b...unexposed portion, 5...laser irradiation device, 6...pattern (mask), 7...plasma generation device, 8...patterned semiconductor chip, 9...light irradiation device, 10, 20, 30, 40...laminated body, 11...support member, 12...adhesive layer, 100...semiconductor device
Claims
1. A method for manufacturing a semiconductor device, comprising the steps of: forming a positive photosensitive resin film on a surface of a semiconductor wafer; exposing a portion of the positive photosensitive resin film to light to provide an exposed portion in the positive photosensitive resin film; developing the positive photosensitive resin film with a developer and removing the exposed portion to form a pattern; performing plasma dicing using the pattern as a mask to separate the semiconductor wafer and obtain patterned semiconductor chips; exposing the pattern of the patterned semiconductor chip; and removing the exposed pattern using a remover to obtain a semiconductor chip from which the pattern has been removed from the patterned semiconductor chip.
2. The method for manufacturing a semiconductor device according to claim 1, wherein the positive-type photosensitive resin film contains a resin that is depolymerized by irradiation with light.
3. The method for manufacturing a semiconductor device according to claim 2, wherein the developing solution and the removing solution are water-based solvents having a pH of 11 or less.
Citation Information
Patent Citations
Semiconductor device and method for manufacturing the same
JP2004103738A
Water soluble mask for substrate dicing by laser and plasma etch
JP2015159296A
Method for manufacturing element chip
JP2018200957A
Ester compound, method for synthesizing ester compound, and resin composition
WO2022080409A1