Light detecting element, method for manufacturing light detecting element, and image sensor

The integration of a graphene layer with III-V semiconductor quantum dots and specific ligands in the photodetection element addresses the limitations of conventional infrared sensitivity and cost in existing technologies, enhancing photoresponsiveness and compliance with environmental regulations.

WO2024219263A1PCT designated stage expired Publication Date: 2024-10-24FUJIFILM CORP +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014198
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-20
Filing Date
2024-04-08
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Conventional photodetection elements, such as silicon photodiodes and InGaAs-based semiconductors, have limited sensitivity in the infrared region and high production costs, while graphene-PbS quantum dot photodetectors exhibit insufficient photoresponsiveness and lead content concerns under RoHS regulations.

Method used

A photodetection element is developed using a graphene layer with a photoelectric conversion layer containing III-V semiconductor quantum dots, specifically InSb quantum dots, and a ligand system including inorganic halides and polydentate ligands, which enhances photoresponsiveness through charge trapping and photocurrent amplification.

Benefits of technology

The solution provides a photodetection element with improved sensitivity in the infrared region and reduced production costs, while being RoHS compliant by avoiding lead-based materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024014198_24102024_PF_FP_ABST
    Figure JP2024014198_24102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a light detecting element having: a substrate (101); a graphene layer (102) provided on the substrate (101); electrodes (103, 104) which are electrically connected to the graphene layer (102) and read current or voltage; and a photoelectric conversion layer (105) electrically connected to the graphene layer (102), wherein the photoelectric conversion layer (105) has an aggregate of semiconductor quantum dots and a ligand coordinated to the semiconductor quantum dots. The semiconductor quantum dots include group III-V semiconductor quantum dots. The ligand includes at least one selected from among an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C). Also provided are a method for manufacturing the light detecting element, and an image sensor including aforementioned light detecting element.
Need to check novelty before this filing date? Find Prior Art

Description

Photodetection element, method of manufacturing photodetection element, and image sensor

[0001] The present invention relates to a photodetector element using semiconductor quantum dots and a method for manufacturing the same, and also to an image sensor.

[0002] In recent years, photodetectors capable of detecting light in the infrared region have been attracting attention in the fields of smartphones, surveillance cameras, in-vehicle cameras, and the like.

[0003] Conventionally, silicon photodiodes, which use silicon wafers as the material for the photoelectric conversion layer, have been used as photodetectors for image sensors, etc. However, silicon photodiodes have low sensitivity in the infrared region with wavelengths of 900 nm or more.

[0004] Furthermore, InGaAs-based semiconductor materials, which are known as near-infrared light receiving elements, have the problem of requiring very costly processes, such as epitaxial growth and substrate bonding processes, to achieve high quantum efficiency, and this has prevented them from becoming widely used.

[0005] Non-Patent Document 1 reports a photodetector in which graphene and a PbS quantum dot film are formed on a Si readout circuit.

[0006] S. Goossens et al. “Broadband image sensor array based on graphene-CMOS integration” Nature Photonics 11, 367-371 (2017)

[0007] According to the investigations of the present inventors, it has been found that the photodetector disclosed in Non-Patent Document 1 has insufficient light response and there is room for further improvement.

[0008] Furthermore, in Non-Patent Document 1, PbS quantum dots are used as quantum dots. In other words, since they contain lead, there are concerns about future restrictions on the use of certain hazardous substances (RoHS).

[0009] SUMMARY OF THE INVENTION It is therefore an object of the present invention to provide a photodetector element having excellent photoresponsiveness, a method for manufacturing the photodetector element, and an image sensor.

[0010] The present invention provides the following: <1> A photodetector element comprising: a substrate; a graphene layer provided on the substrate; an electrode for reading out a current or a voltage, electrically connected to the graphene layer; and a photoelectric conversion layer electrically connected to the graphene layer, wherein the photoelectric conversion layer comprises an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, the semiconductor quantum dots include III-V group semiconductor quantum dots, and the ligands comprise at least one selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C); In formula (A), X A1 and X A2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; X A1 and X A2 When one of L is a thiol group, the other is an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group, A1 represents a hydrocarbon group; B1 and X B2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; B3 represents S, O or NH; L B1 and L B2 each independently represents a hydrocarbon group; C1 ~X C3 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; C4 represents N, and L C1 ~L C3each independently represents a hydrocarbon group. <2> The photodetector according to <1>, wherein the semiconductor quantum dots are semiconductor quantum dots containing elemental indium. <3> The photodetector according to <1>, wherein the semiconductor quantum dots are InSb quantum dots. <4> The photodetector according to any one of <1> to <3>, wherein a charge transport layer is provided between the photoelectric conversion layer and the graphene layer. <5> The photodetector according to any one of <1> to <4>, wherein the photodetector is a field-effect transistor type photodetector. <6> The photodetector according to any one of <1> to <5>, wherein the photodetector has an insulating layer in contact with the graphene layer and a conductive layer in contact with the insulating layer. <7> The photodetector according to any one of <1> to <5>, wherein the substrate is a conductive substrate and wherein an insulating layer is provided between the substrate and the graphene layer. <8> A method for manufacturing a photodetector according to any one of <1> to <7>, comprising: forming an electrode for reading out a current or a voltage on a graphene layer provided on a substrate; and forming a photoelectric conversion layer on the graphene layer, the photoelectric conversion layer having an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, the semiconductor quantum dots including III-V group semiconductor quantum dots, and the ligands including at least one selected from the group consisting of an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C); In formula (A), X A1 and X A2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; X A1 and X A2 When one of L is a thiol group, the other is an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group, A1 represents a hydrocarbon group; B1 and X B2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; B3represents S, O or NH; L B1 and L B2 each independently represents a hydrocarbon group; C1 ~X C3 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; C4 represents N, and L C1 ~L C3 <9> The method for producing a photodetector according to <8>, wherein the step of forming the photoelectric conversion layer includes a step of applying, onto the substrate, a dispersion liquid containing III-V group semiconductor quantum dots, a ligand, and a solvent, wherein the ligand is at least one ligand selected from the group consisting of an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C). <10> The method for manufacturing the photodetector according to <8>, wherein the step of forming the photoelectric conversion layer comprises: a semiconductor quantum dot assembly forming step of applying a dispersion liquid containing III-V semiconductor quantum dots and a solvent to form a film of an assembly of III-V semiconductor quantum dots; and a ligand exchange step of applying a ligand solution containing at least one ligand selected from the group consisting of an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C), and a solvent to the film of the assembly of III-V semiconductor quantum dots formed in the semiconductor quantum dot assembly forming step, to coordinate the ligand to the III-V semiconductor quantum dots. <11> An image sensor comprising the photodetector according to any one of <1> to <8>.

[0011] According to the present invention, it is possible to provide a photodetector element having excellent photoresponsiveness, a method for manufacturing a photodetector element, and an image sensor.

[0012] 1 is a diagram showing a first embodiment of a photodetector element; 2 is a diagram showing a second embodiment of a photodetector element; 3 is a diagram showing a third embodiment of a photodetector element; 4 is a diagram showing a fourth embodiment of a photodetector element; 5 is a diagram showing a fifth embodiment of a photodetector element;

[0013] The present invention will be described in detail below. In this specification, the term "to" is used to mean that the numerical values ​​before and after it are included as the lower and upper limits. In the notation of groups (atomic groups) in this specification, notations that do not specify substituted or unsubstituted include groups (atomic groups) that have a substituent as well as groups (atomic groups) that have no substituent. For example, the term "alkyl group" includes not only alkyl groups that have no substituent (unsubstituted alkyl groups) but also alkyl groups that have a substituent (substituted alkyl groups). In this specification, the thickness of each layer can be measured by observing the cross section of the photodetector using a scanning electron microscope (SEM) or the like.

[0014] <Photodetector> The photodetector of the present invention comprises: a substrate; a graphene layer provided on the substrate; an electrode for reading out a current or a voltage, electrically connected to the graphene layer; and a photoelectric conversion layer electrically connected to the graphene layer, wherein the photoelectric conversion layer comprises an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, the semiconductor quantum dots include III-V group semiconductor quantum dots, and the ligands include at least one selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C).

[0015] The photodetector of the present invention includes an electrode for reading out current or voltage, a photoelectric conversion layer containing semiconductor quantum dots and ligands coordinated thereto, and a graphene layer, wherein the electrode for reading out current or voltage and the photoelectric conversion layer are electrically connected to the graphene layer. In this photodetector, when light is irradiated onto the photodetector, the photoelectric conversion layer absorbs the light and generates electron-hole pairs. It is presumed that one of the electron-hole pairs generated in the photoelectric conversion layer flows into the graphene layer, causing the photoelectric conversion layer to become charged due to charge trapping. Furthermore, the photoelectric conversion layer of the photodetector of the present invention uses III-V semiconductor quantum dots as the semiconductor quantum dots and the above-described specific ligand as the ligand coordinated to the III-V semiconductor quantum dots. It is presumed that, by using these specific ligands as the ligands coordinated to the III-V semiconductor quantum dots, a high photocurrent amplification effect can be achieved in the graphene layer while charge trapping occurs in the photoelectric conversion layer. Therefore, the photodetector of the present invention has excellent photoresponsiveness.

[0016] The photodetector of the present invention is preferably a field-effect transistor-type photodetector. Here, a field-effect transistor refers to a transistor that controls the density of electrons or holes by an electric field generated in a channel region by applying a voltage to a gate electrode, thereby controlling the current between the source and drain electrodes. Examples of field-effect transistor-type photodetectors include photodetectors having a structure including a source electrode, a drain electrode, and a gate electrode. Examples include photodetectors having the structure shown in Figures 2 and 3.

[0017] Each component of the photodetector element of the present invention will be described.

[0018] The substrate is not particularly limited, and examples thereof include glass substrates, quartz substrates, synthetic quartz substrates, resin substrates, ceramic substrates, silicon substrates, and other semiconductor substrates.

[0019] The substrate may be a conductive substrate made of a conductive material. Examples of the conductive material include the materials listed as conductive materials used to form electrodes for reading current or voltage, which will be described later, p-type semiconductors (p-type Si such as B-doped Si), and n-type semiconductors (n-type Si such as P-doped Si). When a conductive substrate is used as the substrate, it is preferable that an insulating layer be provided between the substrate and the graphene layer.

[0020] A conductive layer may be provided on the surface of the substrate. Examples of the conductive layer include layers made of the materials listed below as conductive materials used to form electrodes for reading current or voltage, p-type semiconductors (p-type Si such as B-doped Si), or n-type semiconductors (n-type Si such as P-doped Si). The thickness of the conductive layer is preferably 1 to 1000 nm. The upper limit is preferably 500 nm or less, and more preferably 300 nm or less. The lower limit is preferably 10 nm or more, and more preferably 20 nm or more. When a substrate having a conductive layer provided on its surface is used as the substrate, it is preferable that an insulating layer be provided on the surface of the conductive layer.

[0021] The insulating layer formed on the surface of the conductive substrate or the conductive layer may be an inorganic film or an organic film. From the viewpoint of insulating properties, an inorganic film is preferable. As the insulating layer of an inorganic film, silicon oxide (SiO 2 ), silicon nitride (Si 3 N 4 ), silicon oxynitride (SiON), magnesium fluoride (MgF 2 ) and sodium aluminum fluoride (Na 3 AlF 6 ), aluminum oxide (Al 2 O 3 ), yttrium oxide (Y 2 O 3 ), tantalum oxide (Ta 2 O 5 ), hafnium oxide (HfO 2 ), zirconium oxide (ZrO 2The insulating layer preferably has a high transmittance for light in the wavelength range of 400 to 4000 nm, more preferably 70% or more, even more preferably 80% or more, still more preferably 90% or more, and particularly preferably 95% or more.

[0022] The conductive substrate or the conductive layer provided on the surface of the substrate can be used as a gate electrode.

[0023] A graphene layer is provided on the substrate. The graphene layer is a layer made of graphene. Graphene is a layered material made of graphite crystals with one atomic layer or more and several atomic layers or less. The graphene layer may be turbostratic graphene, in which upper and lower layers do not have a graphite-like crystalline alignment but are made up of stacked graphene layers with different orientations.

[0024] Graphene layers can be formed, for example, by mechanically exfoliating the layered material graphite, or by growing graphene on a substrate by chemical vapor deposition (CVD).

[0025] The thickness of the graphene layer is preferably 0.3 to 50 nm. The upper limit is preferably 5 nm or less, and more preferably 1 nm or less. The lower limit of the thickness of the graphene layer is the film thickness of a single-layer graphene, which is approximately 0.3 nm. The graphene layer is preferably a single-layer graphene.

[0026] The photodetector element of the present invention has an electrode for reading out a current or a voltage (hereinafter referred to as a readout electrode) electrically connected to the graphene layer.

[0027] The read electrode is preferably made of a conductive material such as a metal material or an oxide semiconductor. Examples of the metal material include materials containing at least one atom selected from gold (Au), platinum (Pt), iridium (Ir), palladium (Pd), copper (Cu), lead (Pb), titanium (Ti), strontium (Sr), tungsten (W), molybdenum (Mo), tantalum (Ta), germanium (Ge), nickel (Ni), chromium (Cr), indium (In), zinc (Zn), tin (Sn), and cerium (Ce). The metal material may be a single metal, an alloy, or a compound containing the above atoms. Examples of oxide semiconductors include tin oxide, zinc oxide, indium oxide, indium zinc oxide, tin (Sn)-doped indium oxide (indium tin oxide; ITO), tungsten (W)-doped indium oxide, antimony (Sb)-doped tin oxide (antimony-doped tin oxide; ATO), yttrium (Y)-doped strontium titanate, fluorine-doped tin oxide (fluorine-doped tin oxide; FTO), aluminum (Al)-doped zinc oxide, gallium (Ga)-doped zinc oxide, niobium (Nb)-doped titanium oxide, indium tungsten oxide, and indium zinc oxide. The read electrode may be a laminate of two or more layers.

[0028] The photodetector element may have two or more readout electrodes. For example, when the photodetector element has two readout electrodes, one of the electrodes can be used as a source electrode and the other as a drain electrode.

[0029] The thickness of the readout electrode is preferably 5 to 1000 nm, the upper limit is preferably 500 nm or less, more preferably 300 nm or less, and the lower limit is preferably 10 nm or more, more preferably 20 nm or more.

[0030] The readout electrode may be disposed so as to be electrically connected to the graphene layer, and a charge transport layer, such as a hole transport layer or an electron transport layer, may be disposed between the readout electrode and the graphene layer.

[0031] The electron transport layer is a layer that transports electrons generated in the photoelectric conversion layer to the readout electrode. The electron transport layer is also called a hole blocking layer. The electron transport layer is formed from an electron transport material that can perform this function.

[0032] As the electron transport material, [6,6]-Phenyl-C 61 Examples of the electron transport material include fullerene compounds such as butylic acid methyl ester (PC61BM), perylene compounds such as perylene tetracarboxydiimide, tetracyanoquinodimethane, titanium oxide, tin oxide, zinc oxide, indium oxide, indium tungsten oxide, indium zinc oxide, indium tin oxide, fluorine-doped tin oxide, etc. The electron transport material may be in the form of particles.

[0033] The electron transport layer is also preferably composed of zinc oxide doped with metal atoms other than Zn. Hereinafter, zinc oxide doped with metal atoms other than Zn will also be referred to as doped zinc oxide.

[0034] The metal atoms other than Zn in the doped zinc oxide are preferably monovalent to trivalent metal atoms, more preferably at least one selected from Li, Mg, Al, and Ga, further preferably Li, Mg, Al, or Ga, and particularly preferably Li or Mg.

[0035] In the doped zinc oxide, the ratio of metal atoms other than Zn to the total of Zn and metal atoms other than Zn is preferably 1 atomic % or more, more preferably 2 atomic % or more, and even more preferably 4 atomic % or more. From the viewpoint of suppressing an increase in crystal defects, the upper limit is preferably 20 atomic % or less, more preferably 15 atomic % or less, and even more preferably 12 atomic % or less. The ratio of metal atoms other than Zn in the doped zinc oxide can be measured by a high-frequency inductively coupled plasma (ICP) method.

[0036] The electron transport layer may be a single layer film or a laminated film of two or more layers. The thickness of the electron transport layer is preferably 10 to 1000 nm. The upper limit is preferably 800 nm or less. The lower limit is preferably 20 nm or more, and more preferably 50 nm or more.

[0037] The hole transport layer is a layer that transports holes generated in the photoelectric conversion layer to the readout electrode. The hole transport layer is also called an electron blocking layer.

[0038] The hole transport layer is formed from a hole transport material that can perform this function. Examples of hole transport materials include PEDOT:PSS (poly(3,4-ethylenedioxythiophene):poly(4-styrenesulfonic acid)), PTB7 (poly{4,8-bis[(2-ethylhexyl)oxy]benzo[1,2-b:4,5-b']dithiophene-2,6-diyl-lt-alt-3-fluoro-2-[(2-ethylhexyl)carbonyl]thieno[3,4-b]thiophene-4,6-diyl}), PTB7-Th (poly([2,6'-4,8-di(5-ethylhexylthienyl)benzo[1,2-b;3,3-b]dithiophene]{3-fluoro-2[(2-ethylhexyl)carbonyl]thieno[3,4-b]thiophenediyl})), PC71BM ([6,6]-phenyl-C71-methyl butyrate), and MoO 3 and the like. Also, organic hole transport materials and the like described in paragraphs 0209 to 0212 of JP-A-2001-291534 can be used. Also, quantum dots can be used as the hole transport material. Examples of quantum dot materials constituting quantum dots include nanoparticles (particles with a size of 0.5 nm or more and less than 100 nm) of common semiconductor crystals [a) Group IV semiconductors, b) Group IV-IV, III-V, or II-VI compound semiconductors, and c) compound semiconductors consisting of a combination of three or more of Group II, III, IV, V, and VI elements]. Specific examples include PbS, PbSe, PbSeS, InN, Ge, InAs, InGaAs, CuInS, CuInSe, CuInGaSe, InSb, HgTe, HgCdTe, Ag 2 S, Ag 2 Se, Ag2 Examples of such semiconductor materials include Te, SnS, SnSe, SnTe, Si, InP, etc. Ligands may be coordinated to the surface of the quantum dots.

[0039] The thickness of the hole transport layer is preferably 5 to 200 nm, with the lower limit being preferably 10 nm or more, and the upper limit being preferably 100 nm or less, more preferably 50 nm or less.

[0040] The photodetector element of the present invention has a photoelectric conversion layer electrically connected to a graphene layer. The photoelectric conversion layer has an aggregate of semiconductor quantum dots and ligands that coordinate to the semiconductor quantum dots. The aggregate of semiconductor quantum dots is a large number (for example, 1 μm 2 In this specification, the term "semiconductor" refers to a semiconductor having a resistivity of 10 -2 Ωcm or more 10 8 This refers to a substance with a resistivity of Ωcm or less.

[0041] The semiconductor quantum dots include III-V semiconductor quantum dots. III-V semiconductor quantum dots are quantum dots made of compound semiconductors using group III and group V elements. Compound semiconductors are semiconductors composed of two or more elements. Examples of group III elements include aluminum (Al), gallium (Ga), and indium (In). Examples of group V elements include nitrogen (N), phosphorus (P), arsenic (As), and antimony (Sb). III-V semiconductor quantum dots may further include elements other than group III and group V elements. Examples of additional elements include boron (B), thallium (Tl), bismuth (Bi), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), zinc (Zn), cadmium (Cd), and mercury (Hg).

[0042] The III-V group semiconductor quantum dots are preferably semiconductor quantum dots containing indium. Specific examples of III-V group semiconductor quantum dots include InSb quantum dots, InAs quantum dots, and InGaAs quantum dots, and InSb quantum dots are preferred.

[0043] The band gap of the semiconductor quantum dots is preferably 1.2 eV or less, more preferably 1.0 eV or less. The lower limit of the band gap of the semiconductor quantum dots is not particularly limited, but is preferably 0.3 eV or more, more preferably 0.5 eV or more.

[0044] The average particle size of the semiconductor quantum dots is preferably 3 to 20 nm. The lower limit of the average particle size of the semiconductor quantum dots is preferably 4 nm or more, more preferably 5 nm or more. The upper limit of the average particle size of the semiconductor quantum dots is preferably 15 nm or less, more preferably 10 nm or less. If the average particle size of the semiconductor quantum dots is within the above range, a photodetector element can be obtained that has high external quantum efficiency for light with wavelengths in the infrared region. Note that, in this specification, the value of the average particle size of the semiconductor quantum dots is the average value of the particle sizes of 10 arbitrarily selected semiconductor quantum dots. The particle size of the semiconductor quantum dots can be measured using a transmission electron microscope.

[0045] The photoelectric conversion layer contains a ligand that coordinates with the semiconductor quantum dots. The ligand includes an inorganic halide and at least one selected from the group consisting of the multidentate ligands shown below. The photoelectric conversion layer may contain two or more types of ligands. That is, the photoelectric conversion layer may contain two or more types of inorganic halides, two or more types of multidentate ligands shown below, or one or more types of inorganic halide and one or more types of multidentate ligands shown below.

[0046] The inorganic halide used as a ligand is preferably a compound containing at least one element selected from indium, lead, cadmium, potassium, sodium, zinc, copper, silver, and gallium, and a halogen element, and more preferably a compound containing indium and a halogen element. Examples of the halogen element include fluorine, chlorine, bromine, and iodine, and bromine or iodine is preferred.

[0047] Specific examples of inorganic halides include zinc iodide, zinc bromide, zinc chloride, indium iodide, indium bromide, indium chloride, cadmium iodide, cadmium bromide, cadmium chloride, gallium iodide, gallium bromide, and gallium chloride, with indium bromide being preferred.

[0048] In inorganic halides, halogen ions may dissociate and be coordinated to the surface of semiconductor quantum dots. Furthermore, moieties other than halogen elements may also be coordinated to the surface of semiconductor quantum dots. To give a specific example, in the case of indium bromide, indium bromide may be coordinated to the surface of semiconductor quantum dots, or bromine ions or indium ions may be coordinated to the surface of semiconductor quantum dots.

[0049] The polydentate ligand is at least one compound selected from the group consisting of compounds represented by formula (A), compounds represented by formula (B), and compounds represented by formula (C).

[0050] In formula (A), X A1 and X A2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; X A1 and X A2 When one of L is a thiol group, the other is an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group, A1 represents a hydrocarbon group; B1 and X B2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; B3 represents S, O or NH; L B1 and L B2 each independently represents a hydrocarbon group; C1 ~X C3 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group; C4represents N, and L C1 ~L C3 each independently represents a hydrocarbon group.

[0051] X A1 , X A2 , X B1 , X B2 , X C1 , X C2 and X C3 The amino group represented by is -NH 2 The amino group is not limited to the above, and also includes a substituted amino group and a cyclic amino group. Examples of the substituted amino group include a monoalkylamino group, a dialkylamino group, a monoarylamino group, a diarylamino group, and an alkylarylamino group. The amino group includes -NH 2 , a monoalkylamino group, or a dialkylamino group is preferred, and —NH 2 It is more preferable that:

[0052] L A1 , L B1 , L B2 , L C1 , L C2 and L C3 The hydrocarbon group represented by is preferably an aliphatic hydrocarbon group or a group containing an aromatic ring, and more preferably an aliphatic hydrocarbon group. The aliphatic hydrocarbon group may be a saturated aliphatic hydrocarbon group or an unsaturated aliphatic hydrocarbon group. The hydrocarbon group preferably has 1 to 20 carbon atoms. The upper limit of the carbon number is preferably 10 or less, more preferably 6 or less, and even more preferably 3 or less. Specific examples of the hydrocarbon group include an alkylene group, an alkenylene group, an alkynylene group, and an arylene group.

[0053] Examples of the alkylene group include a linear alkylene group, a branched alkylene group, and a cyclic alkylene group, and are preferably a linear alkylene group or a branched alkylene group, and more preferably a linear alkylene group. Examples of the alkenylene group include a linear alkenylene group, a branched alkenylene group, and a cyclic alkenylene group, and are preferably a linear alkenylene group or a branched alkenylene group, and more preferably a linear alkenylene group. Examples of the alkynylene group include a linear alkynylene group and a branched alkynylene group, and are preferably a linear alkynylene group. The arylene group may be monocyclic or polycyclic. A monocyclic arylene group is preferred. Specific examples of the arylene group include a phenylene group and a naphthylene group, and are preferably a phenylene group. The alkylene group, alkenylene group, alkynylene group, and arylene group may further have a substituent. The substituent is preferably a group having 1 to 10 atoms. Specific preferred examples of the group having 1 to 10 atoms include alkyl groups having 1 to 3 carbon atoms [methyl, ethyl, propyl, and isopropyl], alkenyl groups having 2 to 3 carbon atoms [ethenyl and propenyl], alkynyl groups having 2 to 4 carbon atoms [ethynyl, propynyl, etc.], cyclopropyl groups, alkoxy groups having 1 to 2 carbon atoms [methoxy and ethoxy], acyl groups having 2 to 3 carbon atoms [acetyl and propionyl], alkoxycarbonyl groups having 2 to 3 carbon atoms [methoxycarbonyl and ethoxycarbonyl], acyloxy groups having 2 carbon atoms [acetyloxy], Examples of such an alkyl group include an acylamino group (acetylamino group), a hydroxyalkyl group having 1 to 3 carbon atoms (hydroxymethyl group, hydroxyethyl group, hydroxypropyl group), an aldehyde group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, a carbamoyl group, a cyano group, an isocyanate group, a thiol group, a nitro group, a nitroxy group, an isothiocyanate group, a cyanate group, a thiocyanate group, an acetoxy group, an acetamido group, a formyl group, a formyloxy group, a formamido group, a sulfamino group, a sulfino group, a sulfamoyl group, a phosphono group, an acetyl group, a halogen atom, and an alkali metal atom.

[0054] In formula (A), X A1and X A2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group. A1 and X A2 When one of X is a thiol group, the other is an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group. A1 and X A2 In the formula (A), when one of X is a thiol group, the other is preferably a carboxy group, an amino group, or a hydroxy group. A1 and X A2 It is also preferable that X are different groups. A1 and X A2 Preferred combinations of X A1 and X A2 a combination in which one of the groups is a thiol group and the other is a carboxyl group, A1 and X A2 a combination in which one of the groups is a thiol group and the other is an amino group; A1 and X A2 and a combination in which one of the groups is a thiol group and the other is a hydroxy group.

[0055] In formula (A), X A1 and X A2 Is L A1 Preferably, they are separated by 1 to 10 atoms, more preferably by 1 to 6 atoms, even more preferably by 1 to 4 atoms, even more preferably by 1 to 3 atoms, and particularly preferably by 1 or 2 atoms.

[0056] In formula (B), X B1 and X B2 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group. B1 and X B2 may be the same group or different groups.

[0057] In formula (B), X B1 and X B3Is L B1 Preferably, they are separated by 1 to 10 atoms, more preferably 1 to 6 atoms, even more preferably 1 to 4 atoms, still more preferably 1 to 3 atoms, and particularly preferably 1 or 2 atoms. B2 and X B3 Is L B2 Preferably, they are separated by 1 to 10 atoms, more preferably by 1 to 6 atoms, even more preferably by 1 to 4 atoms, even more preferably by 1 to 3 atoms, and particularly preferably by 1 or 2 atoms.

[0058] In formula (C), X C1 ~X C3 each independently represents a thiol group, an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group. C1 ~X C3 may be the same group or different groups.

[0059] In formula (C), X C1 and X C4 Is L C1 Preferably, they are separated by 1 to 10 atoms, more preferably 1 to 6 atoms, even more preferably 1 to 4 atoms, still more preferably 1 to 3 atoms, and particularly preferably 1 or 2 atoms. C2 and X C4 Is L C2 Preferably, they are separated by 1 to 10 atoms, more preferably 1 to 6 atoms, even more preferably 1 to 4 atoms, still more preferably 1 to 3 atoms, and particularly preferably 1 or 2 atoms. C3 and X C4 Is L C3Preferably, they are separated by 1 to 10 atoms, more preferably by 1 to 6 atoms, even more preferably by 1 to 4 atoms, even more preferably by 1 to 3 atoms, and particularly preferably by 1 or 2 atoms.

[0060] In addition, X A1 and X A2 Is L A1 The term "separated by 1 to 10 atoms" means that X A1 and X A2 This means that the number of atoms constituting the molecular chain with the shortest distance connecting X is 1 to 10. For example, in the case of the following formula (A1), X A1 and X A2 and are separated by two atoms, and in the case of the following formula (A2) and formula (A3), X A1 and X A2 The numbers in the following structural formulas represent X A1 and X A2 It represents the order of the arrangement of atoms that make up the shortest molecular chain connecting the

[0061] To explain this by taking a specific compound, 3-mercaptopropionic acid is X A1 The site corresponding to X is a carboxyl group. A2 The site corresponding to is a thiol group, and L A1 In 3-mercaptopropionic acid, the site corresponding to X is an ethylene group (compound with the following structure). A1 (carboxy group) and X A2 (thiol group) and L A1 (ethylene group) separates them by two atoms.

[0062] X B1 and X B3 Is L B1 are separated by 1 to 10 atoms, B2 and X B3 Is L B2 are separated by 1 to 10 atoms, C1 and X C4 Is L C1 are separated by 1 to 10 atoms,C2 and X C4 Is L C2 are separated by 1 to 10 atoms, C3 and X C4 Is L C3 The meaning of being separated by 1 to 10 atoms is the same as above.

[0063] Specific examples of the polydentate ligand include 3-mercaptopropionic acid, thioglycolic acid, 2-aminoethanol, 2-aminoethanethiol, 2-mercaptoethanol, glycolic acid, ethylene glycol, ethylenediamine, aminosulfonic acid, glycine, aminomethylphosphate, guanidine, diethylenetriamine, tris(2-aminoethyl)amine, 4-mercaptobutanoic acid, 3-aminopropanol, 3-mercaptopropanol, N-(3-aminopropyl)-1,3-propanediamine, 3-(bis(3-aminopropyl)amino)propan-1-ol, 1-thioglycerol, dimercaprol, 1-mercapto-2-butanol, 1-mercapto-2-pentanol, 3-mercapto-1-propanol, 2,3-dimercapto-1-propanol, diethanolamine, 2-(2 2-[(2-aminoethyl)amino]ethanethiol, bis(2-mercaptoethyl)amine, 2-aminoethane-1-thiol, 1-amino-2-butanol, 1-amino-2-pentanol, L-cysteine, D-cysteine, 3-amino-1-propanol, L-homoserine, D-homoserine, aminohydroxyacetic acid, L-lactic acid, D-lactic acid, L-malic acid, D-malic acid, glyceric acid, 2-hydroxybutyric acid, L-tartaric acid, D-tartaric acid, tartronic acid, 1,2-benzenedithiol, 1,3-benzenedithiol, 1,4-benzenedithiol, 2-mercaptobenzoic acid, 3-mercaptobenzoic acid, 4-mercaptobenzoic acid, and derivatives thereof.

[0064] The thickness of the photoelectric conversion layer is preferably 10 to 1000 nm. The lower limit of the thickness is preferably 20 nm or more, and more preferably 30 nm or more. The upper limit of the thickness is preferably 600 nm or less, more preferably 550 nm or less, even more preferably 500 nm or less, and particularly preferably 450 nm or less. The refractive index of the photoelectric conversion layer for light of the target wavelength to be detected by the photodetector element can be 1.5 to 5.0.

[0065] The photoelectric conversion layer may be a single layer or a laminate of two or more layers.

[0066] The photoelectric conversion layer may be disposed so as to be electrically connected to the graphene layer, and a charge transport layer or the like may be disposed between the photoelectric conversion layer and the graphene layer. Examples of the charge transport layer include a hole transport layer and an electron transport layer. These include those described above.

[0067] When a charge transport layer is provided between the photoelectric conversion layer and the graphene layer and between the readout electrode and the graphene layer, it is preferable that either the charge transport layer provided between the photoelectric conversion layer and the graphene layer or the charge transport layer provided between the readout electrode and the graphene layer is a hole transport layer, and the other is an electron transport layer.

[0068] In the light-detecting element of the present invention, the photoelectric conversion layer and the readout electrode may be arranged so as to be in contact with each other, or may be provided at a distance from each other. The photoelectric conversion layer and the readout electrode may be provided on the same surface of the graphene layer, or the photoelectric conversion layer and the readout electrode may be provided on different surfaces of the graphene layer. That is, the readout electrode may be provided on the surface of the graphene layer opposite to the surface on which the photoelectric conversion layer is provided. However, when the photoelectric conversion layer and the readout electrode are provided on different surfaces of the graphene layer, the photoelectric conversion layer is provided on the light irradiation side.

[0069] In the photodetector element of the present invention, a conductive layer may be provided on the surface of the photoelectric conversion layer opposite to the graphene layer. The conductive layer may be provided directly on the surface of the photoelectric conversion layer, or an insulating layer may be provided between the conductive layer and the photoelectric conversion layer, and the conductive layer may be provided on the insulating layer. Such a conductive layer can be used as a gate electrode. Examples of the insulating layer include those described above.

[0070] The conductive layer formed on the surface of the photoelectric conversion layer is preferably a transparent conductive layer formed of a conductive material that is substantially transparent to the wavelength of light to be detected by the photodetector. In this specification, "substantially transparent" means that the light transmittance is 50% or more, preferably 60% or more, and more preferably 80% or more. Examples of materials for the conductive layer include conductive metal oxides. Specific examples include tin oxide, zinc oxide, indium oxide, indium tungsten oxide, indium zinc oxide (IZO), indium tin oxide (ITO), and fluorine-doped tin oxide (FTO).

[0071] The thickness of the conductive layer is preferably 1 to 1000 nm. The upper limit is preferably 500 nm or less, and more preferably 300 nm or less. The lower limit is preferably 10 nm or more, and more preferably 20 nm or more. The thickness of the insulating layer is preferably 1 to 1000 nm. The upper limit is preferably 600 nm or less, and more preferably 400 nm or less. The lower limit is preferably 10 nm or more, and more preferably 20 nm or more.

[0072] Specific embodiments of the photodetector of the present invention will be described below with reference to the drawings.

[0073] 1 is a diagram showing a first embodiment of a photodetector element of the present invention. In this photodetector element 1, a graphene layer 102 is provided on a substrate 101. An electrode 103, an electrode 104, and a photoelectric conversion layer 105 are provided on the graphene layer 102. As shown in FIG. 1, the electrode 103 and the electrode 104 are provided on the graphene layer 102 with a certain distance between them. The photoelectric conversion layer 105 is provided between the electrode 103 and the electrode 104.

[0074] 1, the substrate 101 is made of an insulating substrate, such as a glass substrate, a quartz substrate, a synthetic quartz substrate, a resin substrate, a ceramic substrate, a silicon substrate, or another semiconductor substrate.

[0075] 1, the electrodes 103 and 104 are readout electrodes. One of the electrodes 103 and 104 is used as a source electrode, and the other is used as a drain electrode.

[0076] In FIG. 1 , the electrode 103 and the electrode 104 are provided directly on the surface of the graphene layer 102, but a layer such as a charge transport layer may be provided between the electrode 103 and the graphene layer 102 and between the electrode 104 and the graphene layer 102.

[0077] 1, the photoelectric conversion layer 105 is provided directly on the surface of the graphene layer 102, but a layer such as a charge transport layer may be provided between the photoelectric conversion layer 105 and the graphene layer 102. In addition, although the electrode 103, the electrode 104, and the photoelectric conversion layer 105 are each a single layer in FIG. 1, they may be a laminate of two or more layers.

[0078] 1, photoelectric conversion layer 105 is in contact with electrode 103 and electrode 104, but photoelectric conversion layer 105 is not in contact with electrode 103 and electrode 104, that is, photoelectric conversion layer 105 may be spaced apart from electrode 103 and electrode 104. Also, in FIG. 1, electrode 103, electrode 104, and photoelectric conversion layer 105 have the same thickness, but these thicknesses may be different.

[0079] In FIG. 1, the electrode 103, the electrode 104, and the photoelectric conversion layer 105 are provided on the same surface of the graphene layer 102, but the electrode 103 and the electrode 104 may be provided on the surface of the graphene layer 102 facing the substrate 101.

[0080] 2 is a diagram showing a second embodiment of a photodetector element of the present invention. In this photodetector element 2, an insulating layer 206 is provided on a substrate 201, and a graphene layer 202 is provided on the insulating layer 206. An electrode 203, an electrode 204, and a photoelectric conversion layer 205 are provided on the graphene layer 202. As shown in FIG. 2, the electrode 203 and the electrode 204 are provided on the graphene layer 202 with a certain distance between them. The photoelectric conversion layer 205 is provided between the electrode 203 and the electrode 204.

[0081] In the photodetector element shown in FIG. 2 , a conductive substrate or a substrate having a conductive layer formed on its surface is used as the substrate 201. Examples of conductive substrates and conductive layers formed on the substrate surface include those described above. The present embodiment is similar to the first embodiment except that an insulating layer 206 is provided between the substrate 201 and the graphene layer 202 (or, in the case of using a substrate having a conductive layer formed on its surface, between the conductive layer formed on the substrate surface and the graphene layer 202). The modified example is also similar to the content described in the first embodiment. The insulating layer 206 preferably has a high transmittance for light in the wavelength band of 400 to 4000 nm, more preferably 70% or more, even more preferably 80% or more, even more preferably 90% or more, and particularly preferably 95% or more. Examples of such insulating layers include those described above.

[0082] In the photodetector shown in Figure 2, electrodes 203 and 204 are readout electrodes. One of electrodes 203 and 204 is used as a source electrode, and the other is used as a drain electrode. When a conductive substrate is used as substrate 201, substrate 201 is used as a gate electrode. When a substrate having a conductive layer on its surface is used as substrate 201, this conductive layer is used as the gate electrode. The photodetector shown in Figure 2 can be used as a field-effect transistor-type photodetector.

[0083] 3 is a diagram showing a third embodiment of a photodetector element of the present invention. In this photodetector element 3, an insulating layer 306 is provided on a substrate 301, and a graphene layer 302 is provided on the insulating layer 306. An electrode 303, an electrode 304, and a photoelectric conversion layer 305 are provided on the graphene layer 302. As shown in FIG. 3, the electrode 303 and the electrode 304 are provided on the graphene layer 302 at a certain distance from each other. The photoelectric conversion layer 305 is provided between the electrode 303 and the electrode 304. An insulating layer 307 is provided on the photoelectric conversion layer 305. A conductive layer 308 is provided on the insulating layer 307.

[0084] 3 is the same as that of the second embodiment except that an insulating layer 307 is provided on a photoelectric conversion layer 305 and a conductive layer 308 is provided on this insulating layer 307. The modified example is also the same as that described in the first embodiment.

[0085] 3, the insulating layer 307 preferably has a high transmittance for light in the wavelength band of 400 to 4000 nm, more preferably 70% or more, even more preferably 80% or more, still more preferably 90% or more, and particularly preferably 95% or more. Examples of such an insulating layer include those described above.

[0086] 3, the conductive layer 308 is preferably a transparent conductive layer formed of a conductive material that is substantially transparent to the wavelength of light to be detected by the photodetector. Examples of the transparent conductive layer include those described above.

[0087] In the photodetector element shown in FIG. 3, the electrodes 303 and 304 are readout electrodes. One of the electrodes 303 and 304 is used as a source electrode, and the other is used as a drain electrode. When a conductive substrate is used as the substrate 301, the substrate 301 is used as a gate electrode. When a substrate having a conductive layer provided on its surface is used as the substrate 301, this conductive layer is used as the gate electrode. Furthermore, the conductive layer 308 provided on the photoelectric conversion layer 305 is used as the gate electrode. The photodetector element shown in FIG. 3 can be used as a field-effect transistor type photodetector element.

[0088] 4 is a diagram showing a fourth embodiment of a photodetector element of the present invention. This photodetector element 4 has an insulating layer 406 provided on a substrate 401, and a graphene layer 402 provided on the insulating layer 406. An electrode 403 and a photoelectric conversion layer 405 are provided on the graphene layer 402. The insulating layer 406 preferably has a high transmittance for light in the wavelength band of 400 to 4000 nm, more preferably 70% or more, even more preferably 80% or more, even more preferably 90% or more, and particularly preferably 95% or more. Examples of such an insulating layer include those described above.

[0089] 4, a conductive substrate or a substrate having a conductive layer formed on its surface is used as the substrate 401. Examples of the conductive substrate and the conductive layer formed on the substrate surface include those described above.

[0090] 4, the electrode 403 is a readout electrode. When a conductive substrate is used as the substrate 401, the substrate 401 is used as a gate electrode. When a substrate having a conductive layer on its surface is used as the substrate 401, this conductive layer is used as the gate electrode.

[0091] In FIG. 4, the electrode 403 is provided directly on the surface of the graphene layer 402, but a layer such as a charge transport layer may be provided between the electrode 403 and the graphene layer 402.

[0092] 4, the photoelectric conversion layer 405 is provided directly on the surface of the graphene layer 402, but a layer such as a charge transport layer may be provided between the photoelectric conversion layer 405 and the graphene layer 402. Furthermore, although the electrode 403 and the photoelectric conversion layer 405 are each a single layer in FIG. 4, they may be a laminate of two or more layers.

[0093] 4, the photoelectric conversion layer 405 is in contact with the electrode 403, but the photoelectric conversion layer 405 may not be in contact with the electrode 403, that is, the photoelectric conversion layer 405 may be spaced apart from the electrode 403. Also, in FIG. 4, the electrode 403 and the photoelectric conversion layer 405 have the same thickness, but the thicknesses may be different.

[0094] In FIG. 4, the electrode 403 and the photoelectric conversion layer 405 are provided on the same surface of the graphene layer 402, but the electrode 403 may be provided on the surface of the graphene layer 402 facing the substrate 401.

[0095] 5 is a diagram showing a fifth embodiment of a photodetector element of the present invention. In this photodetector element 5, an insulating layer 506 is provided on a substrate 501, and a graphene layer 502 is provided on the insulating layer 506. An electrode 503 and a photoelectric conversion layer 505 are provided on the graphene layer 502. An insulating layer 507 is provided on the photoelectric conversion layer 505. A conductive layer 508 is provided on the insulating layer 507.

[0096] 5 is the same as that of the fourth embodiment except that an insulating layer 507 is provided on a photoelectric conversion layer 505 and a conductive layer 508 is provided on this insulating layer 507. The modified example is also the same as that shown in the fourth embodiment.

[0097] 5, the insulating layer 507 preferably has a high transmittance for light in the wavelength band of 400 to 4000 nm, more preferably 70% or more, even more preferably 80% or more, still more preferably 90% or more, and particularly preferably 95% or more. Examples of such an insulating layer include those described above.

[0098] 5, the conductive layer 508 is preferably a transparent conductive layer formed of a conductive material that is substantially transparent to the wavelength of light to be detected by the photodetector. Examples of the transparent conductive layer include those described above.

[0099] 5, the electrode 503 is a readout electrode. When a conductive substrate is used as the substrate 501, the substrate 501 is used as a gate electrode. When a substrate having a conductive layer on its surface is used as the substrate 501, this conductive layer is used as the gate electrode. When a conductive layer 508 is provided on the photoelectric conversion layer 505, the conductive layer 508 is used as the gate electrode.

[0100] <Method for manufacturing photodetector> The method for manufacturing a photodetector of the present invention is the method for manufacturing a photodetector described above, characterized by comprising the steps of: forming an electrode for reading out current or voltage on a graphene layer on a substrate on which the graphene layer is provided; and forming a photoelectric conversion layer on the graphene layer, the photoelectric conversion layer having an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, wherein the semiconductor quantum dots include III-V group semiconductor quantum dots, and the ligands include at least one selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C).

[0101] In the substrate on which a graphene layer is provided, an insulating layer may be provided between the graphene layer and the substrate. Alternatively, an insulating layer and a conductive layer may be provided between the graphene layer and the substrate, with the insulating layer being in contact with the graphene layer and the conductive layer being in contact with the insulating layer. That is, the conductive layer, the insulating layer, and the graphene layer may be provided in this order on the substrate.

[0102] The electrode for reading out the current or voltage can be formed by a method such as a vacuum deposition method such as ion plating or ion beam, a physical vapor deposition method (PVD method) such as sputtering, or a chemical vapor deposition method (CVD method).

[0103] In the step of forming the photoelectric conversion layer, a photoelectric conversion layer is formed on the graphene layer, the photoelectric conversion layer having an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, the semiconductor quantum dots including III-V group semiconductor quantum dots, and the ligands including at least one selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C).

[0104] Specific examples of the step of forming the photoelectric conversion layer include the first embodiment and the second embodiment shown below.

[0105] A first aspect of the step of forming a photoelectric conversion layer is an aspect that includes a step of applying, onto a substrate, a dispersion liquid containing III-V group semiconductor quantum dots, a ligand, and a solvent, wherein the ligand is at least one ligand selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C).

[0106] A second aspect of the step of forming a photoelectric conversion layer includes a semiconductor quantum dot assembly forming step of applying a dispersion containing III-V semiconductor quantum dots and a solvent to form a film of an assembly of III-V semiconductor quantum dots, and a ligand exchange step of applying a ligand solution containing at least one ligand selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C), and a solvent to the film of an assembly of III-V semiconductor quantum dots formed in the semiconductor quantum dot assembly forming step, thereby coordinating the ligand to the III-V semiconductor quantum dots.

[0107] (Regarding the First Aspect) In the first aspect, the dispersion liquid used to form the photoelectric conversion layer contains III-V group semiconductor quantum dots, a ligand, and a solvent, and the ligand contains at least one ligand selected from the group consisting of an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C).

[0108] Examples of III-V semiconductor quantum dots include those mentioned above. The content of III-V semiconductor quantum dots in the dispersion is preferably 1 to 500 mg / mL, more preferably 10 to 200 mg / mL, and even more preferably 20 to 100 mg / mL.

[0109] Examples of the inorganic halide, the compound represented by formula (A), the compound represented by formula (B) and the compound represented by formula (C) used as the ligand include those described above.

[0110] The ligand contained in the dispersion may further include a ligand other than an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C) (hereinafter also referred to as "other ligands"). The other ligands not only function as ligands that coordinate to the III-V semiconductor quantum dots, but also preferably have a molecular structure that easily forms steric hindrance or charge repulsion, and also serve as a dispersant that disperses the III-V semiconductor quantum dots in the solvent. When the solvent is a polar solvent, the ligand is preferably one that forms charge repulsion. Specifically, halogen compounds, low-molecular-weight thiols, alcohols, carboxylic acids, chalcogens, and chalcogen compounds are preferred. When the solvent is a nonpolar solvent, the ligand is preferably one that forms steric hindrance. Specifically, the ligand preferably has a main chain with at least 6 carbon atoms, and more preferably has a main chain with 10 or more carbon atoms. The ligand may be either a saturated compound or an unsaturated compound. Specific examples include decanoic acid, lauric acid, myristic acid, palmitic acid, stearic acid, behenic acid, oleic acid, erucic acid, oleylamine, stearylamine, 1-aminodecane, dodecylamine, aniline, dodecanethiol, 1,2-hexadecanethiol, tributylphosphine, trihexylphosphine, trioctylphosphine, tributylphosphine oxide, trioctylphosphine oxide, and cetrimonium bromide.

[0111] The content of the ligand in the dispersion is preferably 0.1 mmol / L to 500 mmol / L, and more preferably 0.5 mmol / L to 100 mmol / L.

[0112] The solvent used in the dispersion is not particularly limited, but is preferably a solvent that hardly dissolves the III-V semiconductor quantum dots and easily dissolves the ligands. An organic solvent is preferred. The organic solvent may be either a polar solvent or a non-polar solvent. Specific examples of polar solvents include ethanol, acetone, methanol, acetonitrile, dimethylformamide, dimethyl sulfoxide, butanol, and propanol. Specific examples of non-polar solvents include alkanes (n-hexane, n-octane, and the like), alkenes (octadecene, and the like), benzene, and toluene. The dispersion may contain only one solvent, or a mixed solvent containing two or more solvents.

[0113] The content of the solvent in the dispersion is preferably from 50 to 99% by mass, more preferably from 70 to 99% by mass, and even more preferably from 90 to 98% by mass.

[0114] The dispersion may further contain other components to the extent that the effects of the present invention are not impaired.

[0115] The method for applying the dispersion onto the substrate is not particularly limited, and examples thereof include coating methods such as spin coating, dipping, inkjet printing, dispenser printing, screen printing, letterpress printing, intaglio printing, and spray coating.

[0116] The thickness of the film of the semiconductor quantum dot aggregate formed by applying the dispersion is preferably 10 to 1000 nm or more. The lower limit is more preferably 20 nm or more, and more preferably 30 nm or more. The upper limit is preferably 600 nm or less, and more preferably 400 nm or less.

[0117] After forming a film of an aggregate of semiconductor quantum dots, a ligand exchange step may be further carried out to exchange the ligands coordinated to the III-V semiconductor quantum dots for other ligands.

[0118] The ligand contained in the ligand solution preferably contains at least one selected from inorganic halides, compounds represented by formula (A), compounds represented by formula (B), and compounds represented by formula (C). Details of these are as described above. The ligand contained in the ligand solution may be the same as or different from the ligand contained in the dispersion. The ligand solution may contain only one type of ligand, or may contain two or more types. Furthermore, two or more types of ligand solutions may be used in the step of applying the ligand solution.

[0119] The solvent contained in the ligand solution is preferably selected appropriately depending on the type of ligand contained in the ligand solution, and is preferably a solvent that easily dissolves the ligand. Furthermore, the solvent contained in the ligand solution is preferably an organic solvent with a high dielectric constant. Specific examples include ethanol, acetone, methanol, acetonitrile, dimethylformamide, dimethyl sulfoxide, butanol, propanol, etc. Furthermore, the solvent contained in the ligand solution is preferably a solvent that is unlikely to remain in the photoelectric conversion layer. From the viewpoint of ease of drying and ease of removal by washing, low-boiling point alcohols, ketones, and nitriles are preferred, and methanol, ethanol, acetone, or acetonitrile are more preferred. The solvent contained in the ligand solution is preferably one that is immiscible with the solvent contained in the dispersion. As a preferred solvent combination, when the solvent contained in the dispersion is an alkane such as hexane or octane, or toluene, the solvent contained in the ligand solution is preferably a polar solvent such as methanol or acetone.

[0120] When performing the step of applying a ligand solution, a step of rinsing the film after applying the ligand solution by contacting it with a rinse liquid (rinsing step) may be performed. As the rinse liquid, an aprotic solvent is preferable because it is easy to more effectively remove excess ligands contained in the film and ligands detached from the quantum dots, and it is easy to maintain a uniform film surface by rearranging the semiconductor quantum dot surface. Specific examples of aprotic solvents include acetonitrile, acetone, methyl ethyl ketone, methyl isobutyl ketone, cyclopentanone, diethyl ether, tetrahydrofuran, cyclopentyl methyl ether, dioxane, ethyl acetate, butyl acetate, propylene glycol monomethyl ether acetate, hexane, octane, cyclohexane, benzene, toluene, chloroform, carbon tetrachloride, and dimethylformamide. Acetonitrile and tetrahydrofuran are preferred, and acetonitrile is more preferred.

[0121] The rinsing step may be performed multiple times using two or more rinse solutions with different polarities (dielectric constants). For example, it is preferable to first rinse using a rinse solution with a high dielectric constant (also referred to as a first rinse solution), and then rinse using a rinse solution with a lower dielectric constant than the first rinse solution (also referred to as a second rinse solution). The dielectric constant of the first rinse solution is preferably 15 to 50, more preferably 20 to 45, and even more preferably 25 to 40. The dielectric constant of the second rinse solution is preferably 1 to 15, more preferably 1 to 10, and even more preferably 1 to 5.

[0122] (Regarding the Second Aspect) In the second aspect, the dispersion liquid used to form the photoelectric conversion layer contains III-V semiconductor quantum dots and a solvent.

[0123] Examples of III-V semiconductor quantum dots include those mentioned above. The content of III-V semiconductor quantum dots in the dispersion is preferably 1 to 500 mg / mL, more preferably 10 to 200 mg / mL, and even more preferably 20 to 100 mg / mL.

[0124] The solvent used in the dispersion is not particularly limited, but is preferably a solvent that hardly dissolves III-V semiconductor quantum dots and easily dissolves ligands. Organic solvents are preferred. Specific examples include alkanes (n-hexane, n-octane, etc.), alkenes (octadecene, etc.), benzene, toluene, etc. The dispersion may contain only one solvent, or a mixed solvent containing two or more solvents. The content of the solvent in the dispersion is preferably 50 to 99% by mass, more preferably 70 to 99% by mass, and even more preferably 90 to 98% by mass.

[0125] The dispersion liquid may contain a ligand. From the viewpoint of improving the dispersibility of the III-V semiconductor quantum dots, the ligand preferably has at least 6 carbon atoms in its main chain, and more preferably has 10 or more carbon atoms in its main chain. The ligand contained in the dispersion liquid may be either a saturated compound or an unsaturated compound. Specific examples of ligands contained in the dispersion liquid include decanoic acid, lauric acid, myristic acid, palmitic acid, stearic acid, behenic acid, oleic acid, erucic acid, oleylamine, dodecylamine, dodecanethiol, 1,2-hexadecanethiol, trioctylphosphine oxide, and cetrimonium bromide, with oleic acid and oleylamine being preferred. The content of the ligand in the dispersion liquid is preferably 0.1 mmol / L to 500 mmol / L, and more preferably 0.5 mmol / L to 100 mmol / L.

[0126] The method for applying the dispersion onto the substrate is not particularly limited, and examples thereof include coating methods such as spin coating, dipping, inkjet printing, dispenser printing, screen printing, letterpress printing, intaglio printing, and spray coating.

[0127] The thickness of the film of the semiconductor quantum dot aggregate formed by applying the dispersion is preferably 10 to 1000 nm or more. The lower limit is more preferably 20 nm or more, and more preferably 30 nm or more. The upper limit is preferably 600 nm or less, and more preferably 400 nm or less.

[0128] In the ligand exchange step, a ligand solution containing at least one ligand selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C), and a solvent is applied to the film of the assembly of III-V semiconductor quantum dots formed in the semiconductor quantum dot assembly formation step, and the ligand is coordinated to the III-V semiconductor quantum dots.

[0129] The inorganic halide, the compound represented by formula (A), the compound represented by formula (B) and the compound represented by formula (C) used in the ligand solution are those described above.

[0130] The method for applying the ligand solution to the assembly of semiconductor quantum dots is the same as the method for applying the dispersion onto the substrate, and the preferred embodiments are also the same.

[0131] After the ligand exchange step, a step of rinsing the membrane by bringing it into contact with a rinse liquid (rinsing step) may be carried out. The rinsing step is the same as that described in the first embodiment.

[0132] The method for manufacturing a photodetector of the present invention may further include a step of forming a charge transport layer. Examples of the charge transport layer include a hole transport layer and an electron transport layer. The charge transport layer can be formed by a vacuum deposition method such as ion plating or ion beam, a physical vapor deposition method (PVD method) such as sputtering, or a chemical vapor deposition method (CVD method). Alternatively, the charge transport layer can be formed by applying a composition containing a charge transport material such as an electron transport material or a hole transport material.

[0133] When a charge transport layer is formed, it is preferable to form the charge transport layer on the graphene layer before forming the photoelectric conversion layer. That is, it is preferable to form the charge transport layer on the graphene layer and then form the photoelectric conversion layer on the charge transport layer.

[0134] The method for manufacturing a photodetector of the present invention may further include a step of forming an insulating layer on the photoelectric conversion layer and a step of forming a conductive layer on the insulating layer formed on the photoelectric conversion layer. Through these steps, a photodetector having the structure shown in Figures 3 and 5 can be manufactured.

[0135] The insulating layer can be formed by a method such as a vacuum deposition method such as ion plating or ion beam, a physical vapor deposition method (PVD method) such as sputtering, a chemical vapor deposition method (CVD method), etc. Alternatively, the insulating layer can be formed by applying a composition for forming an insulating layer, such as a resin composition, onto the photoelectric conversion layer.

[0136] The conductive layer can be formed by a method such as a vacuum deposition method such as ion plating or ion beam, a physical vapor deposition method (PVD method) such as sputtering, or a chemical vapor deposition method (CVD method).

[0137] <Image Sensor> The image sensor of the present invention includes the photodetector element of the present invention described above. Since the photodetector element of the present invention has excellent sensitivity to light with wavelengths in the infrared region, this image sensor can be particularly preferably used as an infrared sensor. Furthermore, the image sensor can be preferably used to sense light with a wavelength of 900 to 3000 nm, more preferably used to sense light with a wavelength of 900 to 2000 nm, and even more preferably used to sense light with a wavelength of 900 to 1600 nm.

[0138] The configuration of the image sensor is not particularly limited as long as it has a photodetector element and functions as an image sensor. Examples of the photodetector element include those described above.

[0139] The image sensor may include an infrared-transmitting filter layer, which preferably has low transmittance for light in the visible wavelength range, and more preferably has an average transmittance of 10% or less, even more preferably 7.5% or less, and particularly preferably 5% or less for light in the wavelength range of 400 to 650 nm.

[0140] The infrared transmission filter layer may be formed of a resin film containing a colorant. Examples of the colorant include chromatic colorants such as red, green, blue, yellow, purple, and orange, as well as black colorants. The colorant contained in the infrared transmission filter layer preferably comprises a combination of two or more chromatic colorants to form a black color, or a black colorant. Examples of combinations of chromatic colorants when a black color is formed by combining two or more chromatic colorants include the following (C1) to (C7): (C1) A configuration containing a red colorant and a blue colorant; (C2) A configuration containing a red colorant, a blue colorant, and a yellow colorant; (C3) A configuration containing a red colorant, a blue colorant, a yellow colorant, and a purple colorant; (C4) A configuration containing a red colorant, a blue colorant, a yellow colorant, a purple colorant, and a green colorant; and (C5) A configuration containing a red colorant, a blue colorant, a yellow colorant, and a green colorant. (C6) An embodiment containing a red color material, a blue color material, and a green color material. (C7) An embodiment containing a yellow color material and a purple color material.

[0141] The chromatic colorant may be a pigment or a dye. It may contain both a pigment and a dye. The black colorant is preferably an organic black colorant. Examples of organic black colorants include bisbenzofuranone compounds, azomethine compounds, perylene compounds, and azo compounds.

[0142] The infrared transmission filter layer may further contain an infrared absorber. By incorporating an infrared absorber into the infrared transmission filter layer, the wavelength of light to be transmitted can be shifted to a longer wavelength side. Examples of the infrared absorber include pyrrolopyrrole compounds, cyanine compounds, squarylium compounds, phthalocyanine compounds, naphthalocyanine compounds, quaterrylene compounds, merocyanine compounds, croconium compounds, oxonol compounds, iminium compounds, dithiol compounds, triarylmethane compounds, pyrromethene compounds, azomethine compounds, anthraquinone compounds, dibenzofuranone compounds, dithiolene metal complexes, metal oxides, and metal borides.

[0143] The spectral characteristics of the infrared transmission filter layer can be appropriately selected depending on the application of the image sensor. Examples include filter layers satisfying any one of the following spectral characteristics (1) to (5): (1): A filter layer in which the maximum light transmittance in the thickness direction of the film in the wavelength range of 400 to 750 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum light transmittance in the thickness direction of the film in the wavelength range of 900 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (2): A filter layer in which the maximum light transmittance in the thickness direction of the film in the wavelength range of 400 to 830 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum light transmittance in the thickness direction of the film in the wavelength range of 1000 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (3): A filter layer in which the maximum light transmittance in the thickness direction of the film in the wavelength range of 400 to 950 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum light transmittance in the thickness direction of the film in the wavelength range of 1100 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (4): A filter layer in which the maximum light transmittance in the thickness direction of the film in the wavelength range of 400 to 1100 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum light transmittance in the wavelength range of 1400 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (5) A filter layer having a maximum light transmittance in the thickness direction of the film in the wavelength range of 400 to 1300 nm of 20% or less (preferably 15% or less, more preferably 10% or less), and a minimum light transmittance in the wavelength range of 1600 to 2000 nm of 70% or more (preferably 75% or more, more preferably 80% or more).Further, as the infrared transmission filter, films described in JP 2013-077009 A, JP 2014-130173 A, JP 2014-130338 A, WO 2015 / 166779 A, ​​WO 2016 / 178346 A, WO 2016 / 190162 A, WO 2018 / 016232 A, JP 2016-177079 A, ​​JP 2014-130332 A, and WO 2016 / 027798 can be used. The infrared transmission filter may be a combination of two or more filters, or a dual bandpass filter that transmits two or more specific wavelength regions with one filter may be used.

[0144] The image sensor may include an infrared shielding filter for the purpose of improving various performances such as noise reduction, etc. Specific examples of the infrared shielding filter include the filters described in International Publication No. 2016 / 186050, International Publication No. 2016 / 035695, Japanese Patent No. 6248945, International Publication No. 2019 / 021767, Japanese Patent Laid-Open No. 2017-067963, and Japanese Patent No. 6506529.

[0145] The image sensor may include a dielectric multilayer film. Examples of the dielectric multilayer film include a multilayer film in which a high refractive index dielectric thin film (high refractive index material layer) and a low refractive index dielectric thin film (low refractive index material layer) are alternately stacked. The number of dielectric thin films stacked in the dielectric multilayer film is not particularly limited, but is preferably 2 to 100 layers, more preferably 4 to 60 layers, and even more preferably 6 to 40 layers. A material with a refractive index of 1.7 to 2.5 is preferred as a material used to form the high refractive index material layer. Specific examples include Sb 2 O 3 , Sb 2 S 3 , Bi 2 O 3 , CeO 2 , CeF 3 , HfO 2 , La 2 O 3 , Nd 2 O 3 , Pr 6 O 11 , Sc 2 O3 , SiO, Ta 2 O 5 , TiO 2 , TlCl, Y 2 O 3 , ZnSe, ZnS, ZrO 2 The material used to form the low refractive index material layer is preferably a material having a refractive index of 1.2 to 1.6. 2 O 3 , BiF 3 , CaF 2 , LaF 3 , PbCl 2 , PbF 2 , LiF, MgF 2 , MgO, NdF 3 , SiO 2 , Si 2 O 3 , NaF, ThO 2 , ThF 4 , Na 3 AlF 6 and the like. The method for forming the dielectric multilayer film is not particularly limited, and examples thereof include vacuum deposition methods such as ion plating and ion beam, physical vapor deposition methods (PVD methods) such as sputtering, and chemical vapor deposition methods (CVD methods). The thickness of each of the high refractive index material layer and the low refractive index material layer is preferably 0.1λ to 0.5λ, where λ (nm) is the wavelength of the light to be blocked. Specific examples of the dielectric multilayer film that can be used include the films described in JP 2014-130344 A and JP 2018-010296 A.

[0146] The dielectric multilayer film preferably has a transmission wavelength band in the infrared region (preferably a wavelength region exceeding 700 nm, more preferably a wavelength region exceeding 800 nm, and even more preferably a wavelength region exceeding 900 nm). The maximum transmittance in the transmission wavelength band is preferably 70% or more, more preferably 80% or more, and even more preferably 90% or more. The maximum transmittance in the light-shielding wavelength band is preferably 20% or less, more preferably 10% or less, and even more preferably 5% or less. The average transmittance in the transmission wavelength band is preferably 60% or more, more preferably 70% or more, and even more preferably 80% or more. The wavelength range of the transmission wavelength band is determined by dividing the wavelength showing the maximum transmittance by the center wavelength λ t1 In this case, the central wavelength λ t1 ±100 nm, and the central wavelength λ t1 ±75 nm, and the central wavelength λ t1 It is more preferably ±50 nm.

[0147] The dielectric multilayer film may have only one transmission wavelength band (preferably a transmission wavelength band with a maximum transmittance of 90% or more), or may have a plurality of transmission wavelength bands.

[0148] The image sensor may include a color separation filter layer. Examples of the color separation filter layer include a filter layer containing colored pixels. Examples of the colored pixels include red, green, blue, yellow, cyan, and magenta pixels. The color separation filter layer may include colored pixels of two or more colors, or may include only one color. The filter layer may be appropriately selected depending on the application and purpose. For example, the filter described in International Publication No. 2019 / 039172 may be used.

[0149] Furthermore, when the color separation layer includes color pixels of two or more colors, the color pixels of each color may be adjacent to each other, and a partition wall may be provided between each color pixel. The material of the partition wall is not particularly limited. Examples include organic materials such as siloxane resin and fluororesin, and inorganic particles such as silica particles. The partition wall may also be made of a metal such as tungsten or aluminum.

[0150] When the image sensor includes an infrared transmission filter layer and a color separation layer, it is preferable that the color separation layer is provided on a different optical path from the infrared transmission filter layer. It is also preferable that the infrared transmission filter layer and the color separation layer are arranged two-dimensionally. The two-dimensional arrangement of the infrared transmission filter layer and the color separation layer means that at least a portion of each layer exists on the same plane.

[0151] The image sensor may include an intermediate layer such as a planarization layer, a base layer, or an adhesion layer, an anti-reflection film, and a lens. The anti-reflection film may be, for example, a film made from a composition described in International Publication No. 2019 / 017280. The lens may be, for example, a structure described in International Publication No. 2018 / 092600.

[0152] The present invention will be explained in more detail below with reference to examples. The materials, amounts used, ratios, processing details, processing procedures, etc. shown in the following examples can be changed as appropriate without departing from the spirit of the present invention. Therefore, the scope of the present invention is not limited to the specific examples shown below.

[0153] <Production of Quantum Dot Dispersion> (Quantum Dot Dispersion 1) Indium chloride was added to and dissolved in degassed oleylamine to prepare a 0.1 M indium chloride oleylamine solution (hereinafter referred to as the In precursor solution). Antimony (V) chloride was added to and dissolved in degassed oleylamine to prepare a 0.05 M antimony (V) chloride oleylamine solution (hereinafter referred to as the Sb precursor solution). Degassed dioctyl ether and a 1 M solution of lithium triethylborohydride (tetrahydrofuran (THF), manufactured by Aldirch) were mixed, and the THF was evaporated by vacuum heating to prepare a 1.33 M dioctyl ether solution of lithium triethylborohydride (hereinafter referred to as the Li-DOE solution). In a glove box, 15 mL of the In precursor solution, 15 mL of the Sb precursor solution, and 3 mL of oleylamine were added to a three-neck flask to obtain a solution. The three-neck flask was removed from the glove box, and after repeated evacuation and nitrogen purging, the flask was placed in a nitrogen flow state. 4.3 mL of Li-DOE solution was added to the solution, which was then heated to 285°C at a rate of 3°C / min. The temperature was then maintained at 285°C for 20 minutes. The solution was then cooled, and once the temperature reached 80°C, 18 mL of degassed oleic acid was added. The solution was then cooled to room temperature and placed in a glove box for purification. The purification process involved centrifuging the solution at 7,800 rpm for 5 minutes to precipitate the by-products purified during the reaction, and the supernatant was then recovered. A total of 60 mL of acetonitrile was then added to the supernatant, followed by centrifugation under the same conditions, and the supernatant was discarded. Approximately 9 mL of toluene was added to the precipitate, resulting in a toluene dispersion of InSb quantum dots (quantum dot dispersion 1). The band gap of the quantum dots was estimated to be about 0.95 eV from optical absorption measurements in the visible to infrared region using an ultraviolet-visible-near-infrared spectrophotometer (V-670, manufactured by JASCO Corporation).

[0154] (Quantum Dot Dispersion 2) 8 mL of quantum dot dispersion 1 and 0.8 mL of oleic acid were placed in a centrifuge tube and stirred. Then, 8 mL of acetonitrile was added, and the mixture was centrifuged at 10,000 rpm for 5 minutes at 20°C. The supernatant was then discarded. The precipitate was vacuum dried, and approximately 5 mL of octane was added for redispersion, yielding an octane dispersion of InSb quantum dots (hereinafter referred to as Dispersion A). A ligand exchange solution was prepared by adding 0.9 g of indium bromide, 0.115 g of ammonium acetate, and 25 mL of N,N-dimethylformamide to a separate vial. Approximately 7 mL of the ligand exchange solution was added to Dispersion A, and the resulting mixture was stirred. After removing the separated supernatant, approximately 5 mL of octane was added and stirred. After removing the separated supernatant, approximately 7 mL of the ligand exchange solution was added and the resulting mixture was stirred. After removing the separated supernatant, approximately 5 mL of octane was added and stirred. The separated supernatant was removed. Approximately 15 mL of toluene was added to the resulting solution, which was then centrifuged (10,000 rpm, 5 minutes, 25°C). After the supernatant was removed, the solution was dried in a vacuum. N,N-dimethylformamide was added in a nitrogen atmosphere to re-disperse the InSb quantum dots, yielding quantum dot dispersion 2, which was a dispersion of InSb quantum dots coordinated with indium bromide (concentration: approximately 50 mg / mL).

[0155] (Quantum Dot Dispersion 3) Quantum dot dispersion 3, which is a dispersion of InSb quantum dots coordinated with 3-mercaptopropionic acid (concentration: approximately 50 mg / mL), was obtained in the same manner as quantum dot dispersion 2, except that a ligand exchange liquid produced using 3-mercaptopropionic acid was used instead of indium bromide.

[0156] (Quantum dot dispersion c1) A quantum dot dispersion c1, which is a dispersion of InSb quantum dots coordinated with ethanedithiol (concentration: approximately 50 mg / mL), was obtained in the same manner as in quantum dot dispersion 2, except that a ligand exchange liquid produced using ethanedithiol instead of indium bromide was used as the ligand exchange liquid.

[0157] <Production of Photodetector Element> (Production of Graphene Element) SiO 2A graphene device was fabricated using a substrate on which a 300-nm thermal oxide film (C1000) was formed and single-layer graphene was formed thereon. First, a resist (manufactured by Clariant) was applied to the graphene, followed by baking, pattern exposure, reverse exposure, and development to form a resist pattern on the graphene. Next, the graphene was irradiated with oxygen plasma to remove all graphene except for areas where the resist pattern was not formed. The resist pattern was then removed with a solvent to obtain a graphene fine line pattern. Next, a resist (manufactured by Clariant) was applied to the substrate, followed by baking, pattern exposure, and development to form a resist perforation pattern on the graphene to serve as an electrode portion. Next, 10-nm Ni and 30-nm Au were vapor-deposited onto the substrate. Next, all metal thin films on the resist were removed by lift-off, and a 40-nm-thick electrode (a laminated film of 10-nm Ni and 30-nm Au) was formed only in the perforation pattern portion. The resulting graphene device was annealed in a vacuum chamber at 200°C for 10 hours. In this way, a graphene element (the channel length of the graphene portion between the electrodes was 50 μm and the channel width was 5 μm) was produced.

[0158] (Production of Photodetector) Examples 1 and 2, Comparative Example 1 A quantum dot dispersion liquid shown in the table below was spin-coated onto a graphene element at 2500 rpm, and then heated at 60°C for 5 minutes in a glove box and dried at room temperature for 10 hours to form a photoelectric conversion film with a thickness of approximately 80 nm in which the ligands shown in the table below were coordinated to InSb quantum dots, thereby producing a field-effect transistor-type photodetector element having the structure shown in FIG. 2 .

[0159]

[0160] Examples 3 to 6: The following steps (a) to (d) were repeated four times on a graphene element, followed by heating at 60°C for 5 minutes in a glove box and drying at room temperature for 10 hours. This formed a photoelectric conversion film with a thickness of approximately 80 nm, in which the ligands listed in the table below were coordinated to InSb quantum dots. This produced a field-effect transistor-type photodetector element with the structure shown in FIG. 2 . (a) Quantum dot dispersion 1, adjusted to a concentration of approximately 50 mg / mL, was spin-coated onto the graphene element at 2500 rpm to form a coating film. (b) A ligand solution listed in the table below was dropped onto the coating film, allowed to stand for 30 seconds, and then spin-dried. (c) Acetonitrile was dropped onto the coating film, allowed to stand for 10 seconds, and then spin-dried for 10 seconds. (d) Acetonitrile was dropped onto the coating film, allowed to stand for 10 seconds, and then spin-dried for 20 seconds.

[0161]

[0162] Ligand solution 1: 3-mercaptopropionic acid in methanol (0.02 v / v%) Ligand solution 2: InI 3 Ligand solution 3: methanol solution of diethylenetriamine (0.02 v / v%) Ligand solution 4: methanol solution of tris(2-aminoethyl)amine (0.02 v / v%)

[0163] <Evaluation of photoresponsiveness> The photoresponsiveness of the fabricated photodetector element was evaluated using a semiconductor parameter analyzer (C4155, Agilent). First, the current-voltage characteristics (IV characteristics) were measured while sweeping the gate voltage from -40 V to +40 V in a state where no light was irradiated, and the dark current value was evaluated. Here, the dark current value was taken as the value at a source-drain voltage of 5 V. Next, a mounted light-emitting diode (emission wavelength 1550 nm (irradiation intensity 0.024 mW / cm) manufactured by Thoulabs) was used. 2 ) or emission wavelength 1300 nm (irradiation intensity 0.16 mW / cm 2)) was collimated using an optical lens and irradiated onto the photodetector element to measure the IV characteristics. The photocurrent value was calculated by subtracting the dark current value from the obtained IV characteristics. The photocurrent value was divided by the channel region area of ​​the photodetector element to calculate the value (A / W), and this value was used as an index of photoresponsiveness. A larger value indicates a higher photoresponsiveness.

[0164]

[0165] As shown in the above table, the photodetector element of the example exhibited high responsiveness.

[0166] In Examples 1 to 6, even when the InSb quantum dots were replaced with InAs quantum dots, high photoresponse similar to that of each Example was exhibited.

[0167] 1 to 5: Photodetector elements 101, 201, 301, 401, 501: Substrate 102, 202, 302, 402, 502: Graphene layer 103, 104, 203, 204, 303, 304, 403, 503: Electrode 105, 205, 305, 405, 505: Photoelectric conversion layer 206, 306, 307, 406, 506, 507: Insulating layer 308, 508: Conductive layer

Claims

1. A photodetector comprising: a substrate; a graphene layer provided on the substrate; an electrode for reading out a current or a voltage, electrically connected to the graphene layer; and a photoelectric conversion layer, electrically connected to the graphene layer, wherein the photoelectric conversion layer comprises an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, the semiconductor quantum dots include III-V group semiconductor quantum dots, and the ligands comprise at least one selected from the group consisting of an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C); In formula (A), X A1 and X A2 each independently represents a thiol group, an amino group, a hydroxyl group, a carboxyl group, a sulfo group, a phospho group, or a phosphonic acid group; X A1 and X A2 When one of L is a thiol group, the other is an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group, A1 represents a hydrocarbon group; B1 and X B2 each independently represents a thiol group, an amino group, a hydroxyl group, a carboxyl group, a sulfo group, a phospho group, or a phosphonic acid group; B3 represents S, O or NH; L B1 and L B2 each independently represents a hydrocarbon group; C1 ~X C3 each independently represents a thiol group, an amino group, a hydroxyl group, a carboxyl group, a sulfo group, a phospho group, or a phosphonic acid group; C4 represents N; L C1 ~L C3 each independently represents a hydrocarbon group.

2. The photodetector element according to claim 1, wherein the semiconductor quantum dots are semiconductor quantum dots containing indium element.

3. The photodetector element according to claim 1, wherein the semiconductor quantum dots are InSb quantum dots.

4. The photodetector according to any one of claims 1 to 3, further comprising a charge transport layer between the photoelectric conversion layer and the graphene layer.

5. The photodetector according to any one of claims 1 to 3, wherein the photodetector is a field effect transistor type photodetector.

6. The photodetection element according to any one of claims 1 to 3, comprising an insulating layer in contact with the graphene layer, and a conductive layer in contact with the insulating layer.

7. The photodetector element according to any one of claims 1 to 3, wherein the substrate is a conductive substrate and has an insulating layer between the substrate and the graphene layer.

8. A method for producing a photodetector according to claim 1 or 2, comprising the steps of: forming an electrode for reading out a current or voltage on a graphene layer provided on a substrate on which the graphene layer is provided; and forming a photoelectric conversion layer on the graphene layer, the photoelectric conversion layer having an aggregate of semiconductor quantum dots and ligands coordinated to the semiconductor quantum dots, the semiconductor quantum dots including III-V group semiconductor quantum dots, and the ligands including at least one selected from an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C); In formula (A), X A1 and X A2 each independently represents a thiol group, an amino group, a hydroxyl group, a carboxyl group, a sulfo group, a phospho group, or a phosphonic acid group; X A1 and X A2 When one of L is a thiol group, the other is an amino group, a hydroxy group, a carboxy group, a sulfo group, a phospho group, or a phosphonic acid group, A1 represents a hydrocarbon group; B1 and X B2 each independently represents a thiol group, an amino group, a hydroxyl group, a carboxyl group, a sulfo group, a phospho group, or a phosphonic acid group; B3 represents S, O or NH; L B1 and L B2 each independently represents a hydrocarbon group; C1~X C3 each independently represents a thiol group, an amino group, a hydroxyl group, a carboxyl group, a sulfo group, a phospho group, or a phosphonic acid group; C4 represents N; L C1 ~L C3 each independently represents a hydrocarbon group.

9. The method for producing a light-detecting element according to claim 8, wherein the step of forming the photoelectric conversion layer comprises a step of applying onto the substrate a dispersion liquid containing III-V group semiconductor quantum dots, a ligand, and a solvent, wherein the ligand is at least one ligand selected from the group consisting of an inorganic halide, a compound represented by formula (A), a compound represented by formula (B), and a compound represented by formula (C).

10. The method for manufacturing a photodetector according to claim 8, wherein the step of forming the photoelectric conversion layer comprises: a semiconductor quantum dot assembly forming step of applying a dispersion liquid containing III-V semiconductor quantum dots and a solvent to form a film of an assembly of III-V semiconductor quantum dots; and a ligand exchange step of applying a ligand solution containing at least one ligand selected from an inorganic halide, the compound represented by formula (A), the compound represented by formula (B), and the compound represented by formula (C), and a solvent to the film of the assembly of III-V semiconductor quantum dots formed by the semiconductor quantum dot assembly forming step, so as to coordinate the ligand to the III-V semiconductor quantum dots.

11. An image sensor comprising a photodetection element according to claim 1 or 2.

Citation Information

Patent Citations

  • Phototransistor having carbon-based conductor and quantum dots

    JP2014522117A

  • Optical sensor

    JP2022031994A

  • Method to modify the surface of quantum dots and a method to prepare a dispersion of surface modified quantum dots

    WO2022079198A1