Polyamide resin and polymerization method and application thereof
Polyamide resin polymerized with terephthalic acid and long carbon chain monomers solves the problems of uneven pipe diameter and low surface gloss of polyamide materials in new energy vehicles, achieving excellent performance in the range of 180-190°C Molding properties and high surface gloss, suitable for new energy vehicle piping systems.
Patent Information
- Application Number
- PCT/CN2024/082159
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-28
- Filing Date
- 2024-03-18
- Publication Date
- 2024-10-31
AI Technical Summary
When polyamide materials are melt-extruded and processed into pipes, the cooling rate is fast, resulting in uneven pipe diameters and low surface gloss. The added tougheners and plasticizers have a low decomposition temperature, which limits the material processing temperature and affects its performance. Application in new energy vehicle piping system.
By using semi-aromatic polyamide resin polymerized with terephthalic acid and long carbon chain monomers, its melting point is controlled at 180-190°C, and through specific polymerization methods and raw material ratios, the crystallization behavior and molecular chain structure are optimized to improve molding performance and surface gloss.
It achieves the excellent molding characteristics and high surface gloss of polyamide resin, meets the needs of new energy vehicle piping systems, and improves the practical application performance of the material.
Smart Images

Figure PCTCN2024082159-FTAPPB-I100001 
Figure PCTCN2024082159-FTAPPB-I100002 
Figure PCTCN2024082159-FTAPPB-I100003
Abstract
Description
A kind of polyamide resin and its polymerization method and application Technical Field The present invention relates to the technical field of polymer materials, in particular to a polyamide resin and a polymerization method and application thereof. Background Art The automobile industry is one of the important pillar industries of my country's national economy, especially new energy vehicles, which have achieved rapid development in recent years. According to statistics, the sales of new energy vehicles in 2021 exceeded 3.5 million units, an increase of 158% over 2020. Both the motors and batteries of new energy vehicles need to be cooled, so longer piping systems are required. With the vigorous development of new energy vehicles, the consumption of pipes has risen rapidly, but at the same time it has brought energy shortages and environmental pollution problems to society. Polyamide materials are considered to be the most likely to replace metal materials due to their excellent mechanical properties and solvent resistance, and become the mainstream alternative material for piping systems in new energy vehicles. However, polyamide is a semi-crystalline material with good crystallization performance. When it is melt-extruded and pulled into a pipe, the cooling rate is fast, which is prone to uneven pipe diameters, resulting in defects and affecting subsequent use. In addition, polyamide has good crystallization performance, which can easily lead to low surface gloss after the pipe is cooled, and the appearance is difficult to meet the requirements. At the same time, materials used in pipeline systems usually need to add toughening agents and plasticizers, but the decomposition temperature of these additives is low, so the material processing temperature is not easy to be too high, which requires that the melting point of the polyamide matrix resin cannot be too high (the melting point range is 180-190°C is most suitable). The above problems lead to defects in the actual application of polyamide materials, making it difficult to achieve large-scale promotion in new energy vehicles. Summary of the invention The object of the present invention is to provide a polyamide resin with good pipe forming performance, high surface gloss and a melting point of 180-190°C. The present invention is achieved through the following technical solutions: A polyamide resin, derived from the following units, in mole percent: Diacid units: terephthalic acid and straight-chain diacid, wherein the amount fraction of terephthalic acid in the diacid units is 2-10%; Diamine units: 1,10-decanediamine and / or 1,12-dodecanediamine; The straight-chain diacid is selected from at least one of 1,11-undecanedioic acid, 1,12-dodecanedioic acid, 1,13-tridecanedioic acid and 1,14-tetradecanedioic acid. Preferably, the amount of terephthalic acid in the diacid units is 6-8%. Preferably, the straight chain diacid is selected from 1,12-dodecanedioic acid. When the diamine units are 1,10-decanediamine and 1,12-dodecanediamine, the molar ratio range of 1,10-decanediamine to 1,12-dodecanediamine is 1:(0.01 - 99). The melting point range of the polyamide resin of the present invention is 180 - 190 °C, and at the same time, the range of (T melting point - T crystallization temperature) × half-peak width of the T crystallization peak of the polyamide resin is 160 - 220. The relative viscosity of the polyamide resin of the present invention is 2.0 - 3.0. The test method is as follows: Refer to GB12006.1 - 89, the method for determining the viscosity number of polyamide; the specific test method is: 98% concentrated sulfuric acid prepared according to the standard, add about 15 mL of 98% concentrated sulfuric acid to a 25 mL volumetric flask, then add 0.2500 + 0.0005 g of the sample accurately weighed, dried, crushed, and sieved, place it in a constant temperature shaking water bath at 55 ± 5 °C until completely dissolved, and then measure the relative viscosity ηr of the polyamide at 25 ± 0.01 °C. The polymerization method of the polyamide resin of the present invention includes the following steps: Add reaction monomers, benzoic acid, sodium hypophosphite, and deionized water to the autoclave; the amount of benzoic acid is 1 - 3% of the total amount of diamine and diacid, the weight of sodium hypophosphite is 0.05 - 0.15% of the total weight of other feedstocks except deionized water, and the weight of deionized water is 20 - 40% of the total feedstock weight; evacuate and fill with an inert gas as a protective gas, heat up to 190 - 210 °C within 1.5 - 2.5 hours, and then react at 190 - 210 °C for 0.5 - 1.5 hours; then continue to react at 260 - 280 °C and a pressure of 3.0 - 3.4 MPa for 1 - 3 hours, remove the water formed during the reaction process, reduce the pressure to atmospheric pressure after the reaction is completed, discharge, and obtain the polyamide resin. The application of the polyamide resin of the present invention is used for preparing a pipeline system for new energy vehicles. The present invention has the following beneficial effects: The crystallization behavior is closely related to the crystal melting behavior and the structural characteristics of the molecular chain. The present invention discovers that (T melting point - T crystallization temperature) × half-peak width of the T crystallization peak actually reflects the crystallization behavior of semi-aromatic polyamides polymerized from terephthalic acid and long carbon chain monomers. Specifically, it reflects the overall crystallization rate of the material: T melting point - T crystallization temperature reflects at what temperature below the melting point crystallization starts when the material cools down; the half-peak width of the T crystallization peak reflects within what short temperature range the material can complete crystallization. The present invention's research finds that when the thermal performance parameters of semi-aromatic polyamides polymerized from terephthalic acid and long carbon chain monomers simultaneously satisfy: 180 °C < T melting point < 190 °C (the higher within this temperature range, the better), and the range of (T melting point - T crystallization temperature) × half-peak width of the T crystallization peak is 160 - 200, the polyamide resin has the optimal molding characteristics and can achieve good surface gloss. DETAILED DESCRIPTION The present invention is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the present invention, but are not intended to limit the present invention in any form. It should be noted that, for those of ordinary skill in the art, several variations and improvements may be made without departing from the concept of the present invention. These all belong to the protection scope of the present invention. The sources of raw materials used in the present invention are as follows: Terephthalic acid: purity 99%, P108506, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; Linear diamines: 1,6-Hexanediamine: purity 99%, H103910, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,9-nonanediamine: purity 95%, D185781, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,10-Decanediamine: purity 97%, D100615, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,12-Dodecyldiamine: purity 98%, D106441, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; Straight chain diacids: 1,6-Hexanedioic acid: purity 99.5%, A108264, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,9-Azelaic acid: purity 99%, A108439, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,10-Decanedioic acid: purity 99%, S108453, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,11-Undecane dioic acid: purity 97%, U107255, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,12-Dodecane diacid: purity 99%, D109484, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,13-Tridecyl diacid: purity 98%, T283675, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,14-Tetradecanoic acid: purity 98%, T113585, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; 1,15-Pentadecanedioic acid: purity 97%, P121593, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.; Benzoic acid: purity 99.5%, 242381, purchased from Sigma-Aldrich; Sodium hypophosphite: purity 98%, S475696, purchased from Shanghai Aladdin Biochemical Technology Co., Ltd. Embodiment and comparative example Polyamide resin polymerization method: in the pressure autoclave equipped with magnetic coupling stirring, condenser, gas phase port, feed port, pressure explosion-proof port, add reaction raw materials (diamine, diacid) according to the proportion in the table; then add benzoic acid, sodium hypophosphite (catalyst) and deionized water; the amount of benzoic acid substance is 2.5% of the total amount of diamine and diacid, the weight of sodium hypophosphite is 0.1% of the weight of other feed materials except deionized water, and the weight of deionized water is 30% of the total feed weight; vacuumize and fill with high-purity nitrogen as protective gas, raise the temperature to 200°C within 2 hours under stirring, stir the reaction mixture at 200°C for 1 hour, and then raise the temperature of the reactants to 270°C under stirring; the reaction is continued at a constant temperature of 270°C and a pressure of 3.2MPa for 2 hours, the pressure is kept constant by removing the formed water, and then the pressure is gradually reduced to normal pressure. After the reaction is completed, the material is discharged to obtain polyamide. Various test methods: (1) Relative viscosity test: refer to GB12006.1-89, polyamide viscosity determination method; the specific test method is: measure the relative viscosity ηr of polyamide with a concentration of 0.25 g / dl in 98% concentrated sulfuric acid at 25±0.01°C. (2) Test of thermal performance parameters of polyamide resin: refer to ASTM D3418-2003, Standard Test Method for Transition Temperatures of Polymers By Differential Scanning Calorimetry; the specific test method is: use Perkin Elmer Dimond DSC analyzer to test the melting point of the sample; nitrogen atmosphere, flow rate is 50mL / min; during the test, first heat up to 350℃ at 20℃ / min, keep at 350℃ for 2min, remove the thermal history of the resin, then cool to 50℃ at 20℃ / min, keep at 50℃ for 2min, then heat up to 350℃ at 20℃ / min, set the endothermic peak temperature at this time as Tmelting point, then keep at 350℃ for 2min, then cool to 50℃ at 20℃ / min, set the exothermic peak temperature at this time as Tcrystallization temperature, and set the peak width at half the height of the exothermic peak as Tcrystallization peak half-peak width. (3) Pipe diameter uniformity test: Use precision PA manufactured by Dongguan Songhu Plastic Machinery Co., Ltd. The tube extruder is used to test the extrusion of polyamide materials. The equipment includes a single screw extruder main unit SH-50 / 28T, a precision tube extrusion die SHMJ-1, a three-dimensional precision vacuum water tank SHSC-6000, and a haul-off machine SHQD-600. The extruded tube has a diameter of 12mm and a set wall thickness of 1mm. After the polyamide material is extruded into the tube, the actual wall thickness is measured, and the difference between the thickest and thinnest positions is used to characterize the uniformity of the tube diameter. (4) Surface gloss test: The surface gloss is tested in accordance with GB8807-1988 "Plastic Mirror Gloss Test Method", with a test angle of 60 degrees and a test piece size of 100 mm × 100 mm × 3.2 mm. Table 1: Examples 1-7 Polyamide resin unit content (mol%) and test results From Examples 1-7 and Comparative Examples 1-4, it can be seen that when the molar fraction of terephthalic acid in the diacid unit is 2-10 mol%, (melting point - crystallization temperature) × half-width of crystallization peak is greater than 160, and the melting point is 180-190°C, the thickness difference of the polyamide resin is small and the surface gloss is high. Preferably, when the molar fraction of terephthalic acid in the diacid unit is 6-8 mol%, the melting point, thickness difference and surface gloss of the polyamide resin are better. Table 2: Unit contents (mol%) and test results of polyamide resins in Examples 8-12 It can be seen from Examples 2 / 8-12 that when the straight-chain diacid is selected from 1,12-dodecanedioic acid, the melting point, thickness difference and surface glossiness are better. Table 3: Comparative Examples 1-6 Polyamide resin unit content (mol%) and test results It can be seen from Comparative Examples 5-9 that the technical effects of the present invention cannot be achieved by using other types of diamines or diacids. Table 4: Comparative Examples 7-10 Polyamide resin unit content (mol%) and test results It can be seen from the above embodiments that the wall thickness difference of the polyamide resin of this patent is less than 0.17 mm, and the surface glossiness is greater than or equal to 90%.
Claims
1. A polyamide resin, It is characterized in that In mole percent, derived from units including: Diacid units: terephthalic acid and straight-chain diacid, wherein the amount fraction of terephthalic acid in the diacid units is 2-10%; Diamine units: 1,10-decanediamine and / or 1,12-dodecanediamine; The straight-chain diacid is selected from at least one of 1,11-undecanedioic acid, 1,12-dodecanedioic acid, 1,13-tridecanedioic acid and 1,14-tetradecanedioic acid.
2. The polyamide resin according to claim 1, It is characterized in that The amount of terephthalic acid in the diacid units is 6-8%.
3. The polyamide resin according to claim 1, It is characterized in that The straight chain diacid is selected from 1,12-dodecanedioic acid.
4. The polyamide resin according to claim 1, It is characterized in that When the diamine units are 1,10-decanediamine and 1,12-dodecanediamine, the molar ratio of 1,10-decanediamine to 1,12-dodecanediamine is in the range of 1:(0.01-99).
5. The polyamide resin according to claim 1, It is characterized in that The melting point range of the polyamide resin is 180-190° C., and the range of (T melting point-T crystallization temperature)×T crystallization peak half-peak width of the polyamide resin is 160-220.
6. A method for polymerizing a polyamide resin according to any one of claims 1 to 5, It is characterized in that The following steps are involved: Add reaction monomers, benzoic acid, sodium hypophosphite and deionized water into a pressure autoclave; the amount of benzoic acid is 1-3% of the total amount of diamine and diacid, the weight of sodium hypophosphite is 0.05-0.15% of the total weight of other materials except deionized water, and the weight of deionized water is 20-40% of the total weight of the materials; evacuate and fill with inert gas protection gas, heat to 190-210° C. within 1.5-2.5 hours, and then react at 190-210° C. for 0.5-1.5 hours; then continue to react at 260-280° C. and 3.0-3.4 MPa for 1-3 hours, and remove the water formed during the reaction; after the reaction is completed, reduce the pressure to normal pressure and discharge the material to obtain a polyamide resin.
7. Use of the polyamide resin according to any one of claims 1 to 5, It is characterized in that Used to prepare new energy vehicle pipeline systems.
Citation Information
Patent Citations
Semi-aromatic and aliphatic polyamide block copolymer and preparation method thereof
CN103360599A
Polyamide resin and polyamide composition formed by same
CN104017204A
Semi-aromatic copolyamide resin and copolyamide molded composition consisting of same
CN106117549A
Semi-aromatic transparent copolymer polyamide material and preparing method thereof
CN108047444A
Semi-aromatic polyamide as well as preparation method and application thereof
CN114409895A
Cited By
Liquid crystal polyester-amide-imide based on bio-based diamine as well as preparation and application of liquid crystal polyester-amide-imide
CN119570021A