Semiconductor device and method for manufacturing same

The method of forming a first block layer on the p-type semiconductor layer with attached Si-based residue and a second block layer between it and the active layer in semiconductor device manufacturing addresses the leak path issue, enhancing current efficiency and device characteristics by preventing direct contact and simplifying the process.

WO2024236689A1PCT designated stage expired Publication Date: 2024-11-21MITSUBISHI ELECTRIC CORP
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/018092
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-15
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

In semiconductor device manufacturing, the conventional method of forming current blocking layers on both sides of a ridge leads to a leak path due to the first layer contacting the active layer, resulting in increased leakage current and deteriorated device characteristics.

Method used

A method where a first block layer is formed on the p-type semiconductor layer while Si-based residue from dry etching remains attached to the ridge side surfaces, and a second block layer is formed between the first block layer and the active layer after residue removal, preventing direct contact and reducing lateral leakage current.

Benefits of technology

This approach improves current efficiency and device characteristics by reducing lateral leakage current and allowing for stable growth of the first block layer without increasing the leak path width, while also simplifying the manufacturing process by avoiding the need to re-grow masks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023018092_21112024_PF_FP_ABST
    Figure JP2023018092_21112024_PF_FP_ABST
Patent Text Reader

Abstract

According to the present invention, an active layer (2) and an n-type semiconductor layer (3) are sequentially formed on a p-type semiconductor layer (1). The n-type semiconductor layer (3) and the active layer (2) are dry etched using a pattern (4) of an insulating film as a mask so as to form a ridge (5). A first block layer (7), which is composed of an n-type semiconductor, is formed directly on the p-type semiconductor layer (1) on both sides of the ridge (5), while a residue (6) of the dry etching remains adhered to the side surface of the ridge (5). After the first block layer (7) is formed, the residue (6) is removed. After the residue (6) is removed, a second block layer (8), which is composed of a semiconductor other than the n-type semiconductor, is formed between the first block layer (7) and the active layer (2).
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor device and manufacturing method thereof

[0001] The present disclosure relates to a semiconductor device and a manufacturing method thereof.

[0002] In the manufacture of buried laser elements, the insulating film pattern is used as a mask to form SiCl 4 When a ridge is formed by dry etching a semiconductor layer with a gas, Si-based residues are formed on the surface of the ridge. Conventionally, the Si-based residues are removed using an oxidizing agent and diluted BHF, and then a current blocking layer is formed on both sides of the ridge (see, for example, Patent Document 1).

[0003] Japanese Patent Publication No. 2013-172059

[0004] However, the first layer of the current blocking layer formed on the sidewalls of the ridge acts as a leakage path. If the first layer is made thicker to ensure stable growth, the width of the leakage path will increase. This increases the leakage current, deteriorating the device characteristics.

[0005] The present disclosure has been made to solve the above-mentioned problems, and its object is to provide a semiconductor device and a manufacturing method thereof that can improve element characteristics.

[0006] A method for manufacturing a semiconductor device according to the present disclosure is characterized by comprising the steps of: forming an active layer and an n-type semiconductor layer in this order on a p-type semiconductor layer; dry-etching the n-type semiconductor layer and the active layer with a gas containing a Si compound to form a ridge; forming first block layers made of an n-type or undoped semiconductor directly on the p-type semiconductor layer on both sides of the ridge while leaving residues of the Si compound produced by the dry etching attached to the side surfaces of the ridge; removing the residues after forming the first block layer; and forming a second block layer made of a semiconductor other than n-type between the first block layer and the active layer after removing the residues.

[0007] In the present disclosure, the first blocking layer is selectively formed while the residue of the Si compound produced by dry etching remains attached to the side surfaces of the ridge, thereby separating the first blocking layer from the active layer. Since the first blocking layer, which is the first layer of the current blocking layer, does not contact the active layer, leakage current lateral to the active layer can be reduced. As a result, current efficiency is improved, leading to improved device characteristics.

[0008] Fig. 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to an embodiment. Fig. 2 is a cross-sectional view showing a manufacturing process of a semiconductor device according to an embodiment. Fig. 3 is a cross-sectional view showing a manufacturing process of a semiconductor device according to an embodiment. Fig. 4 is a cross-sectional view showing a manufacturing process of a semiconductor device according to an embodiment. Fig. 5 is a cross-sectional view showing a manufacturing process of a semiconductor device according to an embodiment. Fig. 6 is a cross-sectional view showing a manufacturing process of a semiconductor device according to an embodiment. Fig. 7 is a cross-sectional view showing a semiconductor device according to a comparative example. Fig. 8 is a cross-sectional view showing a semiconductor device according to an embodiment.

[0009] 1 to 6 are cross-sectional views showing the manufacturing process of a semiconductor device according to an embodiment of the present invention, which is a buried type laser element.

[0010] First, as shown in Figure 1, an active layer 2 and an n-type semiconductor layer 3 are formed in this order on a p-type semiconductor layer 1. The p-type semiconductor layer 1 is a p-InP substrate and a p-InP regrowth layer epitaxially grown thereon, or a p-Inp substrate. The active layer 2 is made of AlInGaAs, AlInGaAsP, InGaAsP, or the like. An insulating film is formed on the n-type semiconductor layer 3, and the insulating film is patterned to form a pattern 4.

[0011] Next, as shown in FIG. 2, the insulating film pattern 4 is used as a mask, and SiCl 4 The n-type semiconductor layer 3, the active layer 2, and a portion of the p-type semiconductor layer 1 are dry-etched using a gas containing a Si compound, such as a gas, to form a ridge 5. Residues 6 of the Si compound produced by the dry etching adhere to the side surfaces of the ridge 5. The residues 6 are Si compounds such as Si, SiO, and SiClx.

[0012] 3, first block layers 7 made of n-type semiconductor are selectively formed directly on the p-type semiconductor layer 1 on both sides of the ridge 5 while the residues 6 remain attached to the side surfaces of the ridge 5. At this time, the first block layers 7 are not formed on the side surfaces of the ridge 5 to which the residues 6 have attached.

[0013] Next, as shown in FIG. 4 , the residue 6 is removed by wet processing using an oxidizing agent and diluted BHF. Next, a second block layer 8 is formed between the first block layer 7 and the active layer 2. The second block layer 8 is in direct contact with the side surfaces of the first block layer 7 and the active layer 2. The second block layer 8 is an undoped InP layer. The second block layer 8 may be made of any semiconductor other than n-type, such as undoped, lightly p-type doped, or semi-insulating. A third block layer 9 made of p-InP and a fourth block layer 10 made of n-InP are sequentially formed on the second block layer 8. The first to fourth block layers 7 to 10 of the current block layer are formed by epitaxial growth. The material of the first to fourth block layers 7 to 10 is not limited to InP, and other compound semiconductors may also be used.

[0014] Next, as shown in FIG. 5, the pattern 4 is removed, and a contact layer 11 made of n-InP is formed on the n-type semiconductor layer 3 of the ridge 5 and the fourth blocking layer 10 of the current blocking layer.

[0015] 6, the contact layer 11, the first to fourth block layers 7 to 10, and a portion of the p-type semiconductor layer 1 are etched to form a mesa structure. Insulating films 12 and 13 are formed on the side surfaces of the mesa structure. An opening is formed in the insulating film 13 on the top surface of the mesa structure. A front surface electrode 14 is formed so as to be connected to the contact layer 11 through this opening. A back surface electrode 15 is formed on the back surface of the p-type semiconductor layer 1. The semiconductor device according to this embodiment is manufactured through the above steps.

[0016] Next, the effects of this embodiment will be described in comparison with a comparative example. Figure 7 is a cross-sectional view showing a semiconductor device according to the comparative example. In the comparative example, a first layer of the current blocking layer is formed on the side surface of the active layer 2. If n-InP were formed as the first layer, the current flowing through the active layer 2 would decrease, so a p-InP blocking layer 16 is formed as the first layer. However, this p-InP blocking layer 16 on the side of the active layer 2 becomes a leak path, resulting in increased leak current and current consumption.

[0017] FIG. 8 is a cross-sectional view showing a semiconductor device according to an embodiment. In this embodiment, the first blocking layer 7 is selectively formed while the residue 6 remains attached to the side surfaces of the ridge 5, thereby separating the first blocking layer 7 from the active layer 2. Because the first blocking layer 7, which is the first layer of the current blocking layer, does not contact the active layer 2, the lateral leakage current of the active layer 2 can be reduced. As a result, current efficiency is improved, leading to improved device characteristics. Although leakage current occurs when the p-type semiconductor layer 1 and the p-type second blocking layer 8 are slightly in contact with each other, the leakage current is less than in the comparative example. Furthermore, the use of the residue 6 eliminates the need to re-grow a mask covering the side surfaces of the ridge 5, thereby reducing the number of processes.

[0018] Furthermore, to prevent the first block layer 7 from contacting the active layer 2, the lower surface of the first block layer 7 is made lower than the lower surface of the active layer 2. However, if the thickness of the first block layer 7 is constant, it is necessary to deeply etch the p-type semiconductor layer 1 during the formation of the ridge 5 so that the first block layer 7 does not contact the active layer 2, which increases the current injection resistance of the p-type semiconductor layer 1. In contrast, in this embodiment, the first block layer 7 is epitaxially grown while the residue 6 remains attached to the side surfaces of the ridge 5, so the thickness of the first block layer 7 decreases as it approaches the ridge 5. This prevents the first block layer 7 from contacting the active layer 2 even if the etching depth of the p-type semiconductor layer 1 is shallow. Because the first block layer 7 can be made thick, the first block layer 7 can be stably grown without relying on film thickness controllability.

[0019] 1 p-type semiconductor layer, 2 active layer, 3 n-type semiconductor layer, 4 pattern, 5 ridge, 6 residue, 7 first block layer, 8 second block layer

Claims

1. A method for manufacturing a semiconductor device comprising the steps of: forming an active layer and an n-type semiconductor layer in that order on a p-type semiconductor layer; dry etching the n-type semiconductor layer and the active layer with a gas containing a Si compound to form a ridge; forming a first block layer made of an n-type or undoped semiconductor directly on the p-type semiconductor layer on both sides of the ridge while leaving residue of the Si compound produced by the dry etching adhering to the side surfaces of the ridge; removing the residue after forming the first block layer; and forming a second block layer made of a semiconductor other than n-type between the first block layer and the active layer after removing the residue.

2. A semiconductor device comprising: a p-type semiconductor layer; a ridge having an active layer formed on the p-type semiconductor layer and an n-type semiconductor layer formed on the active layer; first block layers formed directly on the p-type semiconductor layer on both sides of the ridge and made of an n-type or undoped semiconductor with a thickness decreasing toward the ridge; and a second block layer formed between the first block layer and the active layer and made of a semiconductor other than n-type, wherein the first block layer is not in contact with the active layer.

3. The semiconductor device according to claim 2, wherein the lower surface of said first blocking layer is located below the lower surface of said active layer.

Citation Information

Patent Citations

  • Semiconductor laser element and its production

    JP1993226774A

  • Semiconductor laser and manufacture thereof

    JP1995022691A

  • Method of manufacturing compound semiconductor device

    JP2002057142A

  • Method of manufacturing semiconductor light-emitting element

    JP2009260189A

  • Semiconductor element manufacturing method

    JP2013172059A