Electrode manufacturing device and electrode manufacturing method
The electrode manufacturing device addresses foreign matter-related defects by integrating a foreign matter removal and inspection system within the manufacturing process, ensuring clean conditions for laser cutting, thus enhancing the accuracy and efficiency of electrode tab production.
Patent Information
- Application Number
- PCT/KR2024/006563
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-16
- Filing Date
- 2024-05-14
- Publication Date
- 2024-11-21
AI Technical Summary
Conventional electrode manufacturing devices face issues with foreign matter accumulation, leading to defects such as uncut electrode tabs and decreased productivity due to interference with laser cutting processes.
An electrode manufacturing device equipped with a laser cutting unit, a jig part for forming patterns, a foreign matter removal unit, and an inspection unit that detects and removes foreign matter, ensuring the jig part is clean before cutting, thereby preventing defects and maintaining productivity.
The solution effectively reduces defect rates and prevents productivity losses by ensuring accurate cutting and removing foreign matter from the jig part, improving the overall manufacturing process.
Smart Images

Figure KR2024006563_21112024_PF_FP_ABST
Abstract
Description
Electrode manufacturing device and electrode manufacturing method
[0001] Cross-citation with related application(s)
[0002] This application claims the benefit of priority to Korean Patent Application No. 10-2023-0063049, filed May 16, 2023, the entire contents of which are incorporated herein by reference.
[0003] The present invention relates to an electrode manufacturing device and an electrode manufacturing method, and more particularly, to an electrode manufacturing device and an electrode manufacturing method that improve the defect rate due to non-cutting of electrodes and prevent a decrease in productivity due to electrode breakage.
[0004] As technological developments and demand for mobile devices increase, the demand for secondary batteries as an energy source is rapidly increasing. In particular, secondary batteries are attracting significant attention as an energy source not only for mobile devices such as cell phones, digital cameras, laptops, and wearable devices, but also for powertrains such as electric bicycles, electric cars, and hybrid electric vehicles.
[0005] These secondary batteries are classified into cylindrical and prismatic batteries, in which the electrode assembly is housed in a cylindrical or prismatic metal can, and pouch-type batteries, in which the electrode assembly is housed in a pouch-type case made of aluminum laminate sheet, depending on the shape of the battery case. Here, the electrode assembly housed in the battery case is a power plant capable of charging and discharging, consisting of a positive electrode, a negative electrode, and a separator structure interposed between the positive electrode and the negative electrode, and is classified into a jelly-roll type in which a separator is interposed between long sheet-shaped positive and negative electrodes coated with an active material and wound, and a stack type in which a plurality of positive electrodes and negative electrodes are sequentially stacked while interposing the separator between them.
[0006] Among these, pouch-type batteries, which have a structure in which a stack-type or stack / folding-type electrode assembly is built into a pouch-type battery case made of aluminum laminate sheet, are gradually increasing in usage due to reasons such as low manufacturing cost, small weight, and easy deformation.
[0007] In particular, electrodes included in secondary batteries are manufactured by applying electrode active materials onto electrode current collectors, and some of the manufactured electrodes are notched to process (cut) electrode tabs, thereby manufacturing electrode tabs in a desired shape. Conventional electrode manufacturing devices include a jig unit having a predetermined pattern or shape and a laser cutting unit, thereby facilitating the processing of electrode tabs based on the pattern or shape of the jig unit.
[0008] However, in conventional electrode manufacturing devices, foreign substances may accumulate inside the pattern or shape of the jig part due to the processing (cutting) process or the external environment. The foreign substances accumulated inside the pattern or shape of the jig part interfere with the cutting of the laser, so there is a problem that the electrode tab is not processed into the desired pattern or shape. Such uncut portions of the electrode tab may cause defects such as breakage or tab folding of the electrode tab, and there is a problem that productivity is reduced by increasing the loss and downtime of the process.
[0009] Accordingly, there is a need to develop an electrode manufacturing device and electrode manufacturing method that improve the defect rate due to electrode miscutting and prevent a decrease in productivity due to electrode breakage.
[0010] The problem to be solved by the present invention is to provide an electrode manufacturing device and an electrode manufacturing method that improve the defect rate due to non-cutting of electrodes and prevent a decrease in productivity due to electrode breakage.
[0011] The problems to be solved by the present invention are not limited to the problems described above, and problems not mentioned can be clearly understood by a person having ordinary skill in the art to which the present invention pertains from this specification and the attached drawings.
[0012] An electrode manufacturing device according to one embodiment of the present invention includes a laser cutting unit for cutting at least a portion of an electrode; a jig unit for forming a predetermined pattern on at least a portion of the electrode when the laser cutting unit cuts; a foreign matter removal unit for removing foreign matters from the jig unit; and an inspection unit for inspecting whether there is a foreign matter in the jig unit, wherein the jig unit moves to a position corresponding to the laser cutting unit when the inspection unit does not detect a foreign matter in the jig unit, and moves to a position corresponding to the foreign matter removal unit when the inspection unit detects a foreign matter in the jig unit.
[0013] When the foreign matter in the jig part is removed in the foreign matter removal unit, the jig part is re-moved to a position corresponding to the inspection unit, and the inspection unit can check whether the foreign matter in the jig part has been removed.
[0014] The above jig part can be moved to a position corresponding to the laser cutting part if the foreign matter in the jig part is not reconfirmed in the inspection part, and the jig part can be detached if the foreign matter in the jig part is reconfirmed in the inspection part.
[0015] The inspection unit may determine that the foreign matter is not confirmed in the jig part if the area where the foreign matter is not formed is 90% or more but less than 100% of the total area of the pattern formed in the jig part, and may determine that the foreign matter is confirmed if the area where the foreign matter is not formed is 0% or more but less than 90% of the total area of the pattern formed in the jig part.
[0016] The above inspection unit is a vision camera, and the inspection unit can check for foreign substances in the jig unit based on an image acquired by the vision camera.
[0017] The above jig section can be rotated to a position corresponding to the laser cutting section, the foreign matter removal section, and the inspection section.
[0018] The jig part further includes a main body part positioned inside, and the jig part can rotate as the main body part rotates.
[0019] The laser cutting section, the foreign matter removal section, and the inspection section may each be positioned on the outer surface of the main body.
[0020] The above main body may have a drum structure formed in a cylindrical shape.
[0021] The inspection unit and the foreign matter removal unit are positioned spaced apart from each other in a direction facing each other, and the laser cutting unit can be positioned between the inspection unit and the foreign matter removal unit.
[0022] The above jig part includes a jig body part and a jig pattern part located at the center of the jig body part, and the inspection part can check for foreign matter in the jig pattern part.
[0023] A method for manufacturing an electrode using the above-described electrode manufacturing device, comprising: a jig part foreign matter checking step in which the jig part is moved to a position corresponding to the inspection part, and the inspection part checks whether there is a foreign matter in the jig part; a jig part moving step in which the jig part is moved to a position corresponding to the laser cutting part or the foreign matter removal part depending on whether there is a foreign matter in the jig part; and a foreign matter removal step in which the foreign matter removal part removes the foreign matter in the jig part when the jig part is moved to a position corresponding to the foreign matter removal part, and in the jig part moving step, when no foreign matter is found in the jig part, the jig part is moved to a position corresponding to the laser cutting part, and when a foreign matter is found in the jig part, the jig part is moved to a position corresponding to the foreign matter removal part.
[0024] In the above foreign matter removal step, after the foreign matter removal unit removes the foreign matter from the jig part, the jig part may further include a jig part re-movement step in which the jig part is re-moved to a position corresponding to the inspection unit; and the inspection unit may further include a jig part foreign matter re-confirmation step in which the jig part is checked to confirm whether the foreign matter has been removed.
[0025] If the foreign matter in the jig section is not reconfirmed in the inspection section, a step of moving to a position corresponding to the laser cutting section may be further included.
[0026] If the inspection unit reconfirms the foreign matter in the jig part, the jig part may further include a step of being detached, and the detached jig part may be replaced with another jig part or the user may directly remove the foreign matter in the jig part.
[0027] According to embodiments, the electrode manufacturing device and electrode manufacturing method of the present invention can improve the non-cutting of electrodes and the resulting defect rate caused by foreign matter formed in the jig part by having the inspection unit reconfirm whether the foreign matter has been removed after the foreign matter has been removed from the jig part by the foreign matter removal unit, and can prevent a decrease in productivity caused by electrode breakage.
[0028] The effects of the present invention are not limited to the effects described above, and effects not mentioned can be clearly understood by a person having ordinary skill in the art to which the present invention pertains from this specification and the attached drawings.
[0029] FIG. 1 is a drawing showing an electrode manufacturing device according to one embodiment of the present invention.
[0030] Fig. 2 is an enlarged view of a portion of the electrode manufacturing device of Fig. 1.
[0031] Fig. 3 is a drawing showing a cross-section of the jig section of Fig. 2.
[0032] Fig. 4 is a flowchart explaining the operating sequence of the electrode manufacturing device of Fig. 2.
[0033] Hereinafter, various embodiments of the present invention will be described in detail with reference to the attached drawings so that those skilled in the art can easily implement the invention. The present invention may be implemented in various different forms and is not limited to the embodiments described herein.
[0034] In order to clearly explain the present invention, parts that are not related to the description are omitted, and the same reference numerals are used for identical or similar components throughout the specification.
[0035] Furthermore, the sizes and thicknesses of each component shown in the drawings are arbitrarily indicated for convenience of explanation, and thus the present invention is not necessarily limited to the illustrated components. In the drawings, the thicknesses are enlarged to clearly represent various layers and regions. Furthermore, in the drawings, the thicknesses of some layers and regions are exaggerated for convenience of explanation.
[0036] Additionally, throughout the specification, whenever a part is said to “include” a component, this does not mean that it excludes other components, but rather that it may include other components, unless otherwise specifically stated.
[0037] Additionally, throughout the specification, when we say "in plan", we mean when the target portion is viewed from above, and when we say "in cross section", we mean when the target portion is viewed from the side in a cross-section cut vertically.
[0038] Hereinafter, an electrode manufacturing device according to one embodiment of the present invention will be described.
[0039] Fig. 1 is a drawing showing an electrode manufacturing device according to one embodiment of the present invention. Fig. 2 is an enlarged drawing showing a portion of the electrode manufacturing device of Fig. 1. Fig. 3 is a drawing showing a cross-section of a jig portion of Fig. 2.
[0040] Referring to FIGS. 1 and 2, an electrode manufacturing device (1000) according to one embodiment of the present invention includes a laser cutting unit (100) for cutting at least a portion of an electrode; a jig unit (300) for forming a predetermined pattern on at least a portion of the electrode when the laser cutting unit (100) cuts; a foreign matter removal unit (400) for removing foreign matters from the jig unit (300); and an inspection unit (500) for inspecting whether there are foreign matters in the jig unit (300).
[0041] Although not shown in detail in the drawing, the wound electrode is transported while being unwound, and the laser cutting unit (100) can irradiate a laser onto the transported electrode to cut at least a portion of the electrode. For example, the electrode has an electrode active material applied to an electrode current collector, and the laser cutting unit (100) can cut an electrode tab portion on which the electrode active material is not applied to the electrode current collector. Here, the laser cutting unit (100) can adjust the laser irradiation amount and speed based on conditions such as the thickness of the electrode current collector or the thickness of the electrode active material applied.
[0042] Although not depicted in detail in the drawing, the jig portion (300) can support the transported electrode and at the same time, the laser cutting portion (100) facing the electrode can provide a shape or pattern for cutting the electrode. Referring to FIG. 3, the jig portion (300) includes a jig body portion (310) and a jig pattern portion (350) located at the center of the jig body portion (310). Here, the shape or pattern of the jig pattern portion (350) is not limited to FIG. 3, and various shapes or patterns can be applied depending on the cutting conditions of the electrode.
[0043] Accordingly, in the electrode manufacturing device (1000) according to the present embodiment, the laser irradiated from the laser cutting unit (100) passes through the jig pattern unit (350) of the jig unit (300), and the electrode can be cut along the shape or pattern of the jig pattern unit (350).
[0044] The foreign matter removal unit (400) can automatically remove foreign matters from the jig unit (300). For example, the foreign matter removal unit (400) can include a brush member and / or a suction member. Here, the brush member can brush off foreign matters attached to the outer surface of the jig unit (300). In other words, the brush member can brush the outer surface of the jig unit (300). In addition, the suction member can remove foreign matters attached to the outer surface of the jig unit (300) and / or foreign matters dropped from the jig unit (300) by the brush member.
[0045] Accordingly, in the electrode manufacturing device (1000) according to the present embodiment, foreign matter can be automatically removed from the jig portion (300) through the foreign matter removal portion (400), thereby preventing electrode miscutting and tab folding defects due to foreign matter attached to the jig portion (300). In addition, in the electrode manufacturing device (1000) according to the present embodiment, there is no need for the user to separately separate the jig portion (300) to remove foreign matter, and productivity and production speed can be further improved.
[0046] The inspection unit (500) can check whether there is a foreign substance located inside the jig unit (300). More specifically, the inspection unit (500) can check whether there is a foreign substance located inside the jig pattern unit (350). For example, the inspection unit (500) may be a vision camera, and the inspection unit (500) can check for a foreign substance in the jig unit (300) based on an image acquired by the vision camera. More specifically, in the image acquired by the vision camera, the inspection unit (500) can compare the number of pixels containing the foreign substance in the jig unit (300) with the number of pixels constituting the jig pattern unit (350), thereby checking whether there is a foreign substance in the jig unit (300) and the degree of the foreign substance in the jig unit (300). As another example, the inspection unit (500) may include a deep learning model that is learned in advance based on an image acquired by the vision camera. Here, the deep learning model may be pre-trained to compare the number of pixels containing foreign substances in the jig portion (300) based on the number of pixels constituting the jig pattern portion (350) based on the image acquired by the vision camera. However, the present invention is not limited thereto, and any device capable of detecting foreign substances in the jig portion (300) may be included in the present embodiment.
[0047] More specifically, the inspection unit (500) may determine that the foreign matter in the jig unit (300) is not confirmed if the area where the foreign matter is not formed is 90% or more but less than 100% of the total area of the pattern formed in the jig pattern unit (350), and may determine that the foreign matter is confirmed if the area where the foreign matter is not formed is 0% or more but less than 90% of the total area of the pattern formed in the jig pattern unit (350). Here, the area may mean the sum of the areas of pixels included in the image acquired by the vision camera. However, the numerical range for whether or not the inspection unit (500) confirms the foreign matter is not limited thereto, and may be changed depending on the detailed settings of the inspection unit (500).
[0048] Accordingly, in the electrode manufacturing device (1000) according to the present embodiment, the inspection unit (500) checks whether there is foreign matter in the jig unit (300) based on the numerical range described above, so that even if some foreign matter is generated within the normal operating range of the electrode manufacturing device (1000), the device can operate without equipment movement.
[0049] In contrast, in the electrode manufacturing device (1000) according to the present embodiment, when the inspection unit (500) checks whether there is foreign matter in the jig unit (300) based on a numerical range that is outside the above-described numerical range, even if some foreign matter is generated within the normal operating range of the electrode manufacturing device (1000), there is a problem that equipment drift occurs, resulting in a decrease in productivity and production speed.
[0050] Referring to FIG. 3, FIG. 3(a) shows a case where the area where no foreign matter (390) is formed is 100% based on the total area of the pattern formed in the jig pattern portion (350), FIG. 3(b) shows a case where the area where no foreign matter (390) is formed is 92%, and FIG. 3(c) shows a case where the area where no foreign matter (390) is formed is 75%.
[0051] For example, in the case of the jig pattern portion (350) of FIGS. 3(a) and 3(b), the area where the foreign matter (390) is not formed is 90% or more and 100% or less based on the total area of the pattern formed in the jig pattern portion (350), and therefore, the inspection unit (500) can determine that the foreign matter (390) is not confirmed in the jig pattern portion (350) of FIGS. 3(a) and 3(b). In contrast, in the case of the jig pattern portion (350) of FIG. 3(c), the area where the foreign matter (390) is not formed is 0% or more and less than 90% based on the total area of the pattern formed in the jig pattern portion (350), and therefore, the inspection unit (500) can determine that the foreign matter (390) is confirmed in the jig pattern portion (350) of FIG. 3(c).
[0052] Referring to FIGS. 1 and 2, the jig unit (300) can rotate to a position corresponding to the laser cutting unit (100), the foreign matter removal unit (400), and the inspection unit (500). More specifically, the jig unit (300) further includes a main body unit (200) positioned therein, and the jig unit (300) can rotate as the main body unit (200) rotates. More specifically, the corresponding positions may mean that the corresponding components are positioned facing each other. Here, the laser cutting unit (100), the foreign matter removal unit (400), and the inspection unit (500) may be respectively positioned on the outer surface of the main body unit (200).
[0053] For example, the main body (200) may have a drum structure formed in a cylindrical shape. However, the present invention is not limited thereto, and if the jig section (300) has a structure that can move to a position corresponding to the laser cutting section (100), the foreign matter removal section (400), and the inspection section (500), it may be included in the present embodiment.
[0054] As shown in FIG. 2, the inspection unit (500) and the foreign matter removal unit (400) are positioned spaced apart from each other in a direction facing each other, and the laser cutting unit (100) can be positioned between the inspection unit (500) and the foreign matter removal unit (400). More specifically, the jig unit (300) can be rotated to positions a, b, c, and d of the main body unit (200), as shown in FIG. 2. Here, positions a, b, c, and d can have an angle of 90 degrees to each other. Here, the laser cutting unit (100) can be positioned at a position corresponding to position a of the main body unit (200), the foreign matter removal unit (400) can be positioned at a position corresponding to position b of the main body unit (200), and the inspection unit (500) can be positioned at a position corresponding to position d of the main body unit (200). Here, the jig unit (300) can wait at position c of the main body unit (200). However, the positions of the laser cutting section (100), foreign matter removal section (400), and inspection section (500) are not limited thereto, and the positions of the laser cutting section (100), foreign matter removal section (400), and inspection section (500) may be appropriately changed.
[0055] Accordingly, in the electrode manufacturing device (1000) according to the present embodiment, the jig part (300) can move to a position corresponding to the laser cutting part (100), the foreign matter removal part (400), and the inspection part (500), so that it is easy to check whether the foreign matter removal part (400) is foreign in the jig part (300), and there is an advantage in that it is easy to move to the laser cutting part (100) or the inspection part (500) depending on the confirmation of the foreign matter.
[0056] Fig. 4 is a flowchart explaining the operating sequence of the electrode manufacturing device of Fig. 2.
[0057] Referring to FIGS. 2 and 4, the jig unit (300) can be moved to a position (d) corresponding to the inspection unit (500) before cutting the electrode by the laser cutting unit (100). Here, if no foreign matter is detected in the jig unit (300) in the inspection unit (500), the jig unit (300) can be moved to a position (a) corresponding to the laser cutting unit (100), and if a foreign matter is detected in the jig unit (300) in the inspection unit (500), the jig unit (300) can be moved to a position (b) corresponding to the foreign matter removal unit (400).
[0058] However, although FIG. 2 illustrates that the jig part (300) rotates clockwise, the rotation direction of the jig part (300) is not limited thereto, and a case of rotation in a counterclockwise direction may also be included in this embodiment.
[0059] In addition, when the foreign matter of the jig part (300) is removed in the foreign matter removal part (400), the jig part (300) is moved again to a position (d) corresponding to the inspection part (500), and the inspection part (500) can reconfirm whether the foreign matter of the jig part (300) has been removed.
[0060] In addition, if foreign matter in the jig part (300) is not reconfirmed in the inspection part (500), the jig part (300) moves to a position (a) corresponding to the laser cutting part (100), and if foreign matter in the jig part (300) is reconfirmed in the inspection part (500), the jig part (300) can be detached.
[0061] In particular, if a foreign substance in the jig part (300) is reconfirmed in the inspection unit (500), the jig part (300) can be moved to the standby position (c). The jig part (300) located in the standby position (c) can be detached. The detached jig part (300) can be used by the user to check the status of the jig part (300), and if there is contamination in the jig part (300), the user can directly remove the contamination, and if there is damage to the jig part (300), it can be replaced with another jig part.
[0062] Accordingly, in the electrode manufacturing device (1000) according to the present embodiment, the inspection unit (500) can re-check whether there is a foreign substance in the jig unit (300) after the foreign substance has been removed by the foreign substance removal unit (400), thereby quantitatively managing the level of foreign substances in the jig unit (300). In addition, by preventing the level of foreign substances in the jig unit (300) from worsening beyond a certain level, the non-cutting of the electrode and the resulting defect rate can be improved, and a decrease in productivity due to electrode breakage can be prevented.
[0063] Hereinafter, a method for manufacturing an electrode according to another embodiment of the present invention will be described.
[0064] Referring to FIGS. 2 and 4, an electrode manufacturing method according to another embodiment of the present invention is an electrode manufacturing method for manufacturing an electrode using the electrode manufacturing device (1000) described above, and includes a jig part foreign matter checking step (S100, S200) in which a jig part (300) moves to a position (d) corresponding to an inspection part (500) and the inspection part (500) checks whether there is a foreign matter in the jig part (300); a jig part moving step (S300, S400) in which the jig part (300) moves to a position (b) corresponding to a laser cutting part (100) or a foreign matter removal part (400) depending on whether there is a foreign matter in the jig part (300); and a foreign matter removal step (S400) in which, when the jig part (300) moves to a position (b) corresponding to a foreign matter removal part (400), the foreign matter removal part (400) removes the foreign matter in the jig part (300).
[0065] In the jig moving step (S300, S400), if no foreign matter is found in the jig (300), it moves to a position (a) corresponding to the laser cutting section (100) (S300), and if a foreign matter is found in the jig (300), it moves to a position (b) corresponding to the foreign matter removal section (400) (S400).
[0066] In the foreign matter removal step (S400), after the foreign matter removal unit (400) removes the foreign matter from the jig unit (300), the jig unit (300) is re-moved to a position (d) corresponding to the inspection unit (500) in the jig unit re-movement step (S500); and the inspection unit (500) may further include a jig unit foreign matter re-confirmation step (S600) for confirming whether the foreign matter from the jig unit (300) has been removed.
[0067] In the step of reconfirming the foreign matter in the jig part (S600), if the foreign matter in the jig part (300) is not reconfirmed by the inspection part (500), a step (S300) of moving to a position (a) corresponding to the laser cutting part (100) may be further included.
[0068] In the step (S600) of reconfirming foreign matter in the jig part (300), if the inspection unit (500) reconfirms foreign matter in the jig part (300), a step (S700) of detaching the jig part (300) is further included. Here, if the jig part (300) is detached, an NG decision is made, and the detached jig part (300) can be replaced with another jig part as described above, or the user can directly remove the foreign matter in the jig part (300).
[0069] Accordingly, in the electrode manufacturing method according to the present embodiment, the inspection unit (500) can recheck whether there is a foreign substance in the jig unit (300) after the foreign substance has been removed by the foreign substance removal unit (400), thereby quantitatively managing the level of foreign substances in the jig unit (300). In addition, by preventing the level of foreign substances in the jig unit (300) from worsening beyond a certain level, the non-cutting of the electrode and the resulting defect rate can be improved, and a decrease in productivity due to electrode breakage can be prevented.
[0070] Although the preferred embodiments of the present invention have been described in detail above, the scope of the present invention is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concept of the present invention defined in the following claims also fall within the scope of the present invention.
[0071] [Explanation of symbols]
[0072] 100: Laser cutting section
[0073] 200: Main body
[0074] 300: Zigbu
[0075] 310: Jig body
[0076] 350: Jig pattern section
[0077] 400: Foreign body removal unit
[0078] 500: Inspection Department
[0079] 1000: Electrode manufacturing device
Claims
1. A laser cutting section for cutting at least a portion of the electrode; A jig section that forms a predetermined pattern on at least a portion of the electrode when cutting the laser cutting section; A foreign matter removal unit for removing foreign matter from the above jig unit; and Including an inspection unit that inspects the presence of foreign matter in the above jig unit, The above jig part, If no foreign matter is found in the jig section in the above inspection section, it moves to a position corresponding to the laser cutting section, An electrode manufacturing device that moves to a position corresponding to the foreign matter removal unit when a foreign matter is confirmed in the jig unit in the above inspection unit.
2. In paragraph 1, When the foreign matter in the jig part is removed in the foreign matter removal part, the jig part is re-moved to a position corresponding to the inspection part, The above inspection unit is an electrode manufacturing device that reconfirms whether foreign substances have been removed from the jig unit.
3. In paragraph 2, The above jig part, If the foreign matter in the jig section is not reconfirmed in the above inspection section, it moves to a position corresponding to the laser cutting section, An electrode manufacturing device in which the jig part is detached when a foreign substance in the jig part is reconfirmed in the inspection section.
4. In paragraph 3, The above inspection department, If the area where foreign matter is not formed is 90% or more but less than 100% of the total area of the pattern formed on the jig, it is determined that foreign matter is not confirmed on the jig. An electrode manufacturing device that determines that a foreign substance has been confirmed when the area where no foreign substance is formed is 0% or more and less than 90% of the total area of the pattern formed on the above jig.
5. In paragraph 1, The above inspection unit is a vision camera, The above inspection unit is an electrode manufacturing device that checks for foreign substances in the jig unit based on an image acquired by the vision camera.
6. In paragraph 1, An electrode manufacturing device in which the above jig section rotates to a position corresponding to the laser cutting section, the foreign matter removal section, and the inspection section.
7. In paragraph 6, The above jig portion further includes a main body portion located inside, An electrode manufacturing device in which the jig part rotates as the main body part rotates.
8. In paragraph 7, An electrode manufacturing device in which the laser cutting section, the foreign matter removal section, and the inspection section are each located on the outer surface of the main body.
9. In paragraph 8, The above main body is an electrode manufacturing device having a drum structure formed in a cylindrical shape.
10. In paragraph 8, The above inspection unit and the foreign matter removal unit are positioned apart from each other in a direction facing each other, An electrode manufacturing device in which the laser cutting section is located between the inspection section and the foreign matter removal section.
11. In paragraph 1, The above jig part includes a jig body part and a jig pattern part located at the center of the jig body part, The above inspection unit is an electrode manufacturing device that checks whether there is any foreign matter in the above jig pattern unit.
12. An electrode manufacturing method for manufacturing an electrode using the electrode manufacturing device of paragraph 1, A jig part foreign matter confirmation step in which the jig part moves to a position corresponding to the inspection part and the inspection part checks whether there is a foreign matter in the jig part; A jig part moving step in which the jig part moves to a position corresponding to the laser cutting part or the foreign matter removal part depending on whether the jig part contains foreign matter; When the jig part moves to a position corresponding to the foreign matter removal part, the foreign matter removal part includes a foreign matter removal step in which the foreign matter removal part removes the foreign matter from the jig part, An electrode manufacturing method in which, in the above jig section moving step, if no foreign matter is found in the jig section, the jig section moves to a position corresponding to the laser cutting section, and if a foreign matter is found in the jig section, the jig section moves to a position corresponding to the foreign matter removal section.
13. In paragraph 12, In the above foreign matter removal step, after the foreign matter removal unit removes the foreign matter from the jig unit, A jig re-movement step in which the jig part is re-moved to a position corresponding to the inspection part; and An electrode manufacturing method further comprising a jig part foreign matter re-confirmation step for checking whether the inspection part has removed foreign matter from the jig part.
14. In paragraph 13, An electrode manufacturing method further comprising a step of moving to a position corresponding to the laser cutting unit when, in the step of reconfirming the foreign matter in the jig unit, the foreign matter in the jig unit is not reconfirmed by the inspection unit.
15. In paragraph 14, In the step of reconfirming the foreign matter in the jig part, if the foreign matter in the jig part is reconfirmed by the inspection unit, the step of detaching the jig part is further included. An electrode manufacturing method in which the detached jig part is replaced with another jig part or a user directly removes foreign matter from the jig part.
Citation Information
Patent Citations
Electrode manufacturing device and electrode manufacturing method
JP2018018681A
Removal method of foreign matter, inspection method, exposure method, removal apparatus of foreign matter, inspection apparatus, and exposure apparatus
JP2020046491A
Application for mental care and wearable apparatus for mental care
KR1020210116888A
Light emitting diode illumination device
KR1020240015521A
KR20210147658A