High-layer, fast drying polyurethane-based elastomeric coating and method of preparing and using the corresponding elastomeric coating
A solvent-free, high-layer polyurethane-based elastomeric coating composition addresses the limitations of conventional coatings by enabling rapid drying and high resistance in a single layer, suitable for industrial applications on concrete and metal surfaces, offering improved durability and environmental benefits.
Patent Information
- Application Number
- PCT/BR2024/050208
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-22
- Filing Date
- 2024-05-22
- Publication Date
- 2024-11-28
AI Technical Summary
Conventional polyurethane-based coatings face challenges with poor spreadability, high toxicity due to solvent use, limited thickness to avoid cracking, and long drying times, making them unsuitable for high-layer applications requiring rapid drying and high resistance to corrosion, abrasion, and chemicals.
A high-layer, fast-drying polyurethane-based elastomeric coating composition is developed, comprising a mixture of polyols and isocyanates with additives like zeolites, polysiloxane antifoam, polyamides, and fillers, applied in a solvent-free form using a 4:1 to 2:1 mixing ratio, allowing for single-layer application up to 10000 pm thickness without preheating or thermal curing.
The coating achieves rapid drying in under 1 hour, providing high mechanical and chemical resistance, low toxicity, and quick work area release, suitable for large-scale industrial applications on concrete and metal surfaces with improved durability and environmental sustainability.
Smart Images

Figure BR2024050208_28112024_PF_FP_ABST
Abstract
Description
HIGH-LAYER, FAST DRYING POLYURETHANE-BASED ELASTOMERIC COATING AND METHOD OF PREPARING AND USING THE CORRESPONDING ELASTOMERIC COATINGField of application
[0001] The invention is related to the field of coating, paint, and varnish compositions, more specifically, polyurethane-based coating compositions involving the reaction between an isocyanate component and a polyol component. As well as a method of preparing and using the corresponding elastomeric coating.Introduction
[0002] The invention relates to polyurethane-based elastomeric coating compositions, in particular, a two-component elastomeric coating composition for forming a fast-drying, low-toxicity, high-resistance to corrosion, abrasion, and chemicals waterproof coating. And also, a method of preparing and applying the coating in high layers on concrete or metal floors and walls, as well as in systems in contact with water and sewage, such as reservoirs, pipes, and tunnels.Background of the Invention
[0003] The manufacture of polyurethane elastomers generally involves the reaction of an isocyanate and a polyol, but it is possible to define them more broadly and include systems based on reactions of polyisocyanates and a polyol, a polyamine, or water, in the presence or absence of catalysts. In some cases, the catalytic activity onset must be delayed, and the polymerization reaction rate adjusted to obtain the desired processing and complete cure of the elastomer. Once started, however, the polymerization reaction must be fast and sustainable to complete the manufacture of polyurethane elastomers, resulting in a wide variety of coatings depending on the nature of the reagents and additives used.
[0004] Polyurethane-based coatings are well known for their use in applications where durability is an essential characteristic, with particular advantages in coating substrates for protection from adverse weather conditions, heat, chemicals, and / or abrasives, being capable of withstanding particularly severe environmental conditions, enabling the use of such coatings outdoors, as well as for the protection of equipment and parts.
[0005] However, some disadvantages are associated with the use of conventional polyurethane-based coatings. For example, due to the poor spreadability of these compositions it may be necessary to preheat the coating composition prior to application and / or to add low viscosity solvents to enable the use of standard coating equipment. And, although the use of such solvents results in a generally lower viscosity, many of them are highly toxic and pose environmental hazards and need to be removed afterwards, usually by heating, resulting in additional processing steps and increased work time.
[0006] In addition, polyurethane-based coatings are typically applied in thin layers, below 100 pm, to avoid the cracking typically associated with thicker layers of cured polyurethane material. The use of thinner coating layers provides lower mechanical resistance. For coatings with greater resistance, it is necessary to apply a greater number of coating layers, increasing the drying time and the cost of the process.
[0007] The challenge, therefore, lies in manufacturing polyurethane-based coatings that, when applied in high layers, provide corrosion, abrasion, and chemical resistance properties associated with fast drying times, thus allowing the rapid release of the work area for labor and traffic, and that are also easy to handle and apply.Prior Art
[0008] There are several solutions in the state of the art for obtaining both impermeable and corrosion-resistant polyurethane-based coatings. An example of a solution known from the prior art is patent document US 9,221,998 B2 which discloses and describes a polyurethane-based coating composition composed of a polyol component having a hydroxyl group and an isocyanate component for use as a coating agent in rotor blades, vehicles, vessels, or pipelines. However, the coating in question is applied at a preferred thickness of less than 600 pm and dried for 7 days at room temperature or through thermal curing at temperatures of up to 60 °C, which is not advantageous for large-scale applications.
[0009] Patent document US 11,279,846 B2, in turn, refers to a composition including a component based on polycaprolactone polyol or polycarbonate polyol and a pre-polymer hardener component with isocyanate function, generating a coating with a layer thickness of 400 pm, cured for 2 weeks at room temperature. Although the disclosed coating was used as a protective coating, presenting the expected properties of corrosion and weather resistance, especially in the protection of rotor blades edges, the low thickness and long drying time are disadvantages for use in industrial environments.
[0010] Other patent documents disclose two-component coating compositions with corrosion resistance properties, such as the patent document BR 112016030677-5 Bl, which describes a coating composition based on a paint base component containing at least a polycarbonate diol and a diamine, and a hardener component containing at least one polyisocyanate-modified polyester used for coating substrates in aircraft construction. Furthermore, the ability to protect against chemical damage and the toxicity of the coating compositions described in the documents cited above are not disclosed.[Oil] As can be inferred from the above, there is space and demand for a polyurethane-based coating composition solution applied in high layers capable of maintaining its mechanical and chemical resistance properties overcoming, therefore, the disadvantages of the prior art. There is also the need for a fastdrying composition, which makes the method viable for large-scale applications.Objects of the Invention
[0012] One of the objects of the present invention is, therefore, to provide a high-layer, fast drying polyurethane-based elastomeric coating, according to the characteristics of claim 1 of the appended set of claims.
[0013] Another object of the present invention is to provide a method of preparing the elastomeric coating herein according to the characteristics of claim 6 of the appended set of claims.
[0014] Still another object of the present invention is to provide a use of the elastomeric coating herein according to the characteristics of claim 9 of the appended set of claims.
[0015] Additional features and details thereof are presented in the dependent claims.Brief description of the drawings
[0016] Figure 1: Application of the polyurethane-based elastomeric coating according to the invention in floor painting with (a) smooth and (b) non-slip appearance.Detailed description of the invention
[0017] The present invention relates to polyurethane-based elastomeric coating compositions and a method of preparing and using the same. These coatings comprise the product of a reaction between a mixture of a component (A) of polyols and a component (B) of isocyanate. The resulting material can beused to coat a surface or substrate and protect it from mechanical and chemical damage.
[0018] Component (A) of the coating according to the present invention comprises at least one crosslinking agent, preferably a urethane crosslinking agent based on polyols including, but not limited to, acrylic polyols, polyether polyols, polyester polyols, polybutadiene diol, polypropylene glycol, polytetramethylene ether diol, polycarbonate polyol, and biopolyols; at least one moisture absorbing additive including, but not limited to, synthetic silica and alumina zeolites and other desiccant additives with different chemical compositions, preferably a moisture absorbing additive based on zeolites; at least one antifoam additive, preferably a polysiloxane-based antifoam additive including, but not limited to, polysiloxanes associated or modified with polymeric groups, such as polyethers and fluoroalkyls; at least one rheological additive including, but not limited to, inorganic compositions such as fumed silica, silica dispersions and organoclays, and / or organic compositions such as polyamides, cellulose ethers, functionalized acrylic polymers, modified urethane resins, and organo-titanates, preferably a rheological additive based on polyamides; at least one adhesion promoting additive including, but not limited to, functionalized or epoxy, acrylic and amino-linked silanes, preferably functionalized or epoxy-linked silanes; and fillers and pigments comprising micro to nanoscale particles of organic or inorganic origin in a natural, synthetic and / or functionalized state including, but not limited to, metal oxides of aluminum, iron, titanium, zinc, barium, copper, and silicon, salts of sulfates, carbonates, silicates, titanates, chromates, and phosphates, and organic compounds with azo group, phthalocyanine, and carbon black.
[0019] In one embodiment of the present invention, the coating composition of the present invention includes a component (A) comprising from50 to 65% by weight of a urethane crosslinker agent based on polyols, from 5 to 15% by weight of a moisture based on zeolite, from 0.5 to 2% by weight of an antifoam additive based on polysiloxanes, from 1 to 3% by weight of a rheological additive based on polyamide, from 1 to 5% by weight of an adhesion promoting additive based on functionalized silanes, and from 12 to 50% by weight of fillers and pigments. In the context of the present invention, "% by weight" refers to the percentage by weight based on the total weight of component (A) of the coating composition described herein.
[0020] The preparation method for component (A) is similar to the traditional process of producing liquid paints, through which the ingredients of the corresponding formulation are mixed and homogenized.
[0021] Component (B) of the coating according to the present invention comprises an isocyanate selected from aromatic or aliphatic isocyanates including, but not limited to, hexamethylene diisocyanate, diphenylmethane diisocyanate, dicyclohexylmethane diisocyanate, isophorone diisocyanate, metatetramethylxylene diisocyanate, polymethylene polyphenyl polyisocyanate, phenylene diisocyanate, preferably a modified polymeric isocyanate based on diphenylmethane diisocyanate or hexamethylene diisocyanate.
[0022] The polyurethane-based elastomeric coating compositions of the present invention may also comprise the addition of additives and auxiliaries other than those described above. The additives and auxiliaries used depend on the intended purpose of the product, including the use of, but not limited to, flame retardants, leveling agents, dispersants, antioxidants, and viscosity reducers, which are preferably added to component (A). Optionally, component (A) may also have organic and inorganic fillers and pigments, added, to assign color and / or coverage capacity.
[0023] Furthermore, in order to obtain a coating with an anti-slip appearance for use on concrete floors, as shown in Figure IB, abrasive raw materials can also be added to component (A) of the composition herein, such as high granulometry silicon dioxide and sintered bauxite. The coating surface may also be sprayed with particulates, in this case, being preferably applied over a geotextile fabric in order to increase its mechanical resistance.
[0024] Optionally, solvents may also be added for viscosity adjustment, however, it is particularly preferred to produce the coating composition of the present invention in a solvent-free form. In the context of the present invention, "solvent-free" refers to a composition containing less than 10% by weight of solvents, which are typically derived from the manufacturing processes of the constituents, additives, and auxiliaries used in the composition, preferably less than 1% by weight of solvents. The solids content of the coating composition herein is greater than 90%, preferably greater than 95%, more preferably 98% to 100% by weight.
[0025] The present invention also relates to a method of preparing the elastomeric coating herein, which can be produced using customary mixing methods. Thus, the elastomeric coating is formed from a bicomponent composition by mixing components (A) and (B) in a mixing ratio of 4:1 to 2:1, preferably 3.4:1 or 2:1, depending on the chosen application equipment.
[0026] The method of preparing an elastomeric coating comprises applying the coating composition to a substrate. The application of the elastomeric coating of the invention can be carried out via spraying with an airless spray gun, roller coating, brushes, and other hand application methods. The elastomeric coating is preferably applied via spraying, with the use a two-component airless spray gun.
[0027] The coating application according to the present invention can be carried out in multiple layers, being preferably carried out in a single layer, reaching a dry film layer of 500 pm to 10000 pm, depending on the surface and area to be coated. As previously mentioned, a corrosion, abrasion, and chemical resistant polyurethane-based elastomeric coating can be obtained and applied without the need for further dilution or addition of solvents.
[0028] In order to produce a cured coating, the composition is dried at room temperature after application, without the need for high temperatures and the use of furnaces, thus facilitating its application in large environments and on an industrial scale. An advantage of the present invention is that even when applied in multiple layers and at a high thickness, between 500 pm and 10000 pm, the elastomeric coating composition herein is fast drying, in less than 1 hour, providing complete release of the work area for labor and traffic in up to 3 hours from the application.
[0029] The present invention further discloses the use of a polyurethane- based elastomeric coating on a variety of concrete or metal surfaces and substrates.
[0030] The coating is preferably suitable for coating floors and walls made of new or used concrete or metal, such as iron, steel, and alloys, providing a smooth or rough, when used as an anti-slip, finish without presenting defects such as cracks, chalking, pin-holing, and peeling, as shown in Figure 1. The coating is preferably semi-glossy or glossy, with gloss adjustments that can be performed during the composition preparation in order to obtain a glossy or matte coating.
[0031] The elastomeric coating of the present invention is particularly effective for use in systems that require high resistance to corrosion, abrasion, and contact with chemicals, such as oils, solvents, acids, and bases. The obtainedcoating materials have an abrasion resistance (ASTM D4060) of a maximum loss of 50 mg, an impact resistance > 20 J, a Shore D hardness (ASTM D2240) greater than 35 kgf, a tensile strength (ASTM D412) above 15 MPa, an elongation (ASTM D638) above 50% and a corrosion resistance above 3000 hours in neutral saltspray test (ISO 9227), without corrosion and blistering.
[0032] Another particular use disclosed in the present invention comprises providing low toxicity coating compositions for use in systems in contact with water and sewage, such as reservoirs, pipes, and tunnels, due to the absence of further organic solvents in the composition, which confers less environmental impact and low toxicity to the coating and to its high impermeability, with a water absorption rate (ASTM D471) of less than 2%.
[0033] Surfaces and substrates suitable for use with the elastomeric coating of the present invention are preferably prepared by removing possible surface contaminants, such as dirt, oils, greases, chemicals, and other forms of contamination prior to application. The coating of the present invention can be applied over well-adhered aged paint, moderate flash rust, a sandblasted or mechanically / manually treated surface, after previous degreasing.
[0034] The elastomeric coating application according to the present invention can also be carried out over primers and substrate adhesion promoters. In addition, finishing paints can also be used without altering the corrosion, abrasion, and chemical resistance properties of the coating presented herein.Conclusion
[0035] It will be easily understood by one skilled in the art that modifications can be made to the present invention without departing from the concepts set out in the description above. Such modifications should be considered as comprised by the scope of the present invention. Consequently,the particular embodiments previously described in detail are merely illustrative and exemplary, and not limitative in terms of the scope of the present invention, to which the full extent of the accompanying set of claims should be given, in addition to all and any equivalents thereof.
Claims
CLAIMS1. High-layer, fast drying polyurethane-based elastomeric coating, characterized in that it comprises:- a component (A) of polyols comprising at least one crosslinking agent, at least one moisture absorbing additive, at least one antifoam additive; at least one rheological additive, at least one adhesion promoting additive, fillers and pigments, and- a component (B) comprising an isocyanate.
2. High-layer, fast drying polyurethane-based elastomeric coating, according to claim 1, characterized in that component (A) comprises, in relation to the component weight,- from 50 to 65% by weight of a crosslinking agent based on polyols,- from 5 to 15% by weight of a moisture absorbing additive based on zeolites,- from 0.5 to 2% by weight of an antifoam additive based on polysiloxanes,- from 1 to 3% by weight of a rheological additive based on polyamides,- from 1 to 5% by weight of an adhesion promoting additive based on functionalized silanes, and- from 12 to 50% by weight of fillers and pigments.
3. High-layer, fast drying polyurethane-based elastomeric coating according to claims 1 and 2, characterized in that component (A) comprises at least one crosslinking agent based on polyols.
4. High-layer, fast drying polyurethane-based elastomeric coating according to claims 1 and 2, characterized in that component (B) comprises amodified polymeric isocyanate based on diphenylmethane diisocyanate or hexamethylene diisocyanate.
5. High-layer, fast drying polyurethane-based elastomeric coating according to claims 1 and 2, characterized in that it optionally comprises additional additives and auxiliaries.
6. Method of preparing the elastomeric coating, characterized in that it comprises mixing component (A) with component (B) and, optionally, homogenizing these components.
7. Method of preparing the elastomeric coating according to claim 6, characterized in that the mixing ratio between components (A) and (B) is from 4:1 to 2:1, preferably 3.4:1 or 2:1.
8. Method of preparing the elastomeric coating according to claims 6 and 7, characterized in that it comprises curing the coating on the substrate at room temperature.
9. Use of an elastomeric coating, characterized in that it comprises applying an elastomeric coating as defined in claims 1 to 8 to a substrate.
10. Use of an elastomeric coating according to claim 9, characterized in that the substrate is a concrete and / or metal floor and wall surface.
11. Use of an elastomeric coating according to claim 9, characterized in that the substrate is a system in contact with water and sewage, such as reservoirs, pipes, and tunnels.