Spot size converter
The spot size converter addresses the challenge of vertical adjustment by incorporating a high refractive index region within the core layer, enhancing light coupling efficiency and simplifying manufacturing, thus improving the vertical spot size adjustment and device performance.
Patent Information
- Application Number
- PCT/JP2023/019327
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-24
- Publication Date
- 2024-11-28
AI Technical Summary
Conventional spot size converters for semiconductor lasers face challenges in efficiently adjusting the spot size in the vertical direction, leading to decreased light coupling efficiency and complex manufacturing processes, especially when increasing the thickness of the core layer.
A spot size converter design that includes a core layer with a high refractive index region, surrounded by a cladding layer with a lower refractive index, allowing for vertical adjustment of the spot size without increasing the thickness of the cladding layer, thereby simplifying the manufacturing process and maintaining device performance.
The design effectively enlarges the spot size in the vertical direction, improving light coupling efficiency and reducing manufacturing complexity by utilizing a high refractive index region within the core layer to spread light, while maintaining the performance of the optical device.
Smart Images

Figure JP2023019327_28112024_PF_FP_ABST
Abstract
Description
Spot Size Converter
[0001] The present disclosure relates to spot size converters.
[0002] Conventionally, spot size converters used in semiconductor lasers are used to convert the spot size of light propagating through an optical waveguide. When waveguides with different spot sizes are joined together, the light coupling efficiency decreases. By arranging a spot size converter between the joined optical waveguides to match the spot size, light can be propagated efficiently. To improve the light coupling efficiency, the spot size can be adjusted in the vertical direction by changing the thickness of the core layer of the spot size converter. For example, a spot size converter disclosed in Japanese Patent Laid-Open Publication No. 2015-206969 (Patent Document 1) includes a cladding layer and a core layer.
[0003] Japanese Patent Application Laid-Open No. 2015-206969
[0004] However, increasing the thickness of the core layer to adjust the spot size in the vertical direction complicates the manufacturing process, and therefore there is room for improvement in spot size converters with respect to adjusting the spot size in the vertical direction.
[0005] The present disclosure has been made to solve the above-mentioned problems, and an object of the present disclosure is to provide a spot size converter that can control the spot size in the vertical direction.
[0006] A spot size converter according to the present disclosure includes a core layer and a cladding layer. The cladding layer surrounds the core layer. The core layer includes a first core layer. The cladding layer has a refractive index lower than that of the first core layer. The core layer includes a high refractive index region. The high refractive index region has a refractive index higher than that of the first core layer.
[0007] According to the above, it is possible to obtain a spot size converter capable of controlling the spot size in the vertical direction.
[0008] 13. A perspective view of the spot size converter according to the first embodiment. A plan view of the spot size converter according to the first embodiment. A cross-sectional view of the spot size converter shown along line III-III in FIG. 2. A cross-sectional view of the spot size converter shown along line IV-IV in FIG. 2. A flowchart of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A plan view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view of the spot size converter shown along line XIV-XIV in FIG. 13. A plan view showing one step of a method for manufacturing the spot size converter according to the first embodiment. A cross-sectional view of the spot size converter shown along line XVI-XVI in FIG. 15. A plan view showing one step of a method for manufacturing the spot size converter according to the first embodiment. 24 is a cross-sectional view of the spot size converter shown along line XVIII-XVIII in FIG. 17. FIG. 25 is a plan view showing one step of a manufacturing method of the spot size converter according to the first embodiment. FIG. 26 is a cross-sectional view of the spot size converter shown along line XX-XX in FIG. 19. FIG. 27 is a perspective view of the spot size converter according to comparative example 1. FIG. 28 is a distribution diagram showing the intensity of light in the vertical direction. FIG. 29 is a perspective view of the spot size converter according to the second embodiment. FIG. 29 is a plan view of the spot size converter according to the second embodiment. FIG. 29 is a cross-sectional view of the spot size converter shown along line XXV-XXV in FIG. 24. FIG. 29 is a cross-sectional view of the spot size converter shown along line XXVI-XXVI in FIG. 24. FIG. 29 is a flowchart of the manufacturing method of the spot size converter according to the second embodiment. FIG. 29 is a cross-sectional view showing one step of a ...36A and 36B are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36B are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36C are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36D are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36E are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36F are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36F are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36C are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36F are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36F are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36C are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. FIG. 36F are cross-sectional views showing a step of a manufacturing method of the spot size converter according to the second embodiment. 50. A cross-sectional view of the spot size converter shown in line XLV-XLV of Figure 44. A cross-sectional view of the spot size converter shown in line XLVI-XLVI of Figure 44. A cross-sectional view showing a step of a manufacturing method of the spot size converter according to embodiment 2. A plan view showing a step of a manufacturing method of the spot size converter according to embodiment 2. A cross-sectional view of the spot size converter shown in line XLIX-XLIX of Figure 48. A plan view showing a step of a manufacturing method of the spot size converter according to embodiment 2. A cross-sectional view of the spot size converter shown in line LI-LI of Figure 50. A plan view showing a step of a manufacturing method of the spot size converter according to embodiment 2. A cross-sectional view of the spot size converter shown in line LIII-LIII of Figure 52. A perspective view of a spot size converter according to comparative example 2. A distribution diagram showing the intensity of light in the vertical direction.
[0009] Hereinafter, embodiments of the present disclosure will be described. Unless otherwise specified, the same or corresponding parts in the following drawings will be denoted by the same reference numerals, and the description thereof will not be repeated.
[0010] First Embodiment <Configuration of Spot Size Converter> Fig. 1 is a perspective view of a spot size converter 100 according to the first embodiment. Fig. 2 is a plan view of the spot size converter 100 according to the first embodiment. Fig. 3 is a cross-sectional view of the spot size converter 100 shown along the line III-III in Fig. 2. Fig. 4 is a cross-sectional view of the spot size converter 100 shown along the line IV-IV in Fig. 2. Note that in Figs. 1 and 2, the boundary between the high refractive index region 131 and the core layer 120 is indicated by a dotted line.
[0011] The spot size converter 100 shown in FIGS. 1 to 4 is used, for example, in a semiconductor laser, and mainly includes a substrate 101, a cladding layer 110, and a core layer 120. The core layer 120, which propagates light, includes a first core layer 121. As described below, the refractive index n1a of the first core layer 121 is higher than the refractive index n2a of the cladding layer 110. The cladding layer 110 and the core layer 120 function as an optical waveguide. The cladding layer 110 is connected to the substrate 101. The cladding layer 110 surrounds the core layer 120. The core layer 120 propagates light. As shown in FIG. 1 , the direction in which the core layer 120 is arranged as viewed from the substrate 101 is defined as a first direction X. The direction in which light propagates in the core layer 120 is defined as a second direction Y. The second direction Y is perpendicular to the first direction X. A direction perpendicular to the first direction X and the second direction Y is defined as a third direction Z.
[0012] As shown in FIG. 1 , the core layer 120 has a rectangular prism extending in the second direction Y. That is, the cross-sectional shape of the core layer 120 in a cross section perpendicular to the second direction Y is a rectangle. The core layer 120 has a first end face 121s1, a second end face 121s2, and a side face 121s3. The first end face 121s1 is, for example, an emission face. The emission face is an end face from which light can be emitted. The second end face 121s2 is, for example, an incident face. The incident face is an end face into which light can be incident. The first end face 121s1 is the face opposite the second end face 121s2. The side face 121s3 is a face connecting the second end face 121s2 and the first end face 121s1. That is, the side face 121s3 is a face other than the first end face 121s1 and the second end face 121s2.
[0013] The cladding layer 110 surrounds the core layer 120. The only surface of the cladding layer 110 that is connected to the core layer 120 is the side surface 121s3. In other words, the cladding layer 110 is not connected to the second end surface 121s2 or the first end surface 121s1. Specifically, the cladding layer 110 includes a first upper cladding layer 113, a first lower cladding layer 111, and a pair of first side cladding layers 112. The first lower cladding layer 111 is connected to the substrate 101, the core layer 120, and the first side cladding layers 112. The first lower cladding layer 111 is disposed so as to be sandwiched between the core layer 120 and the substrate 101 in the first direction X.
[0014] The pair of first side cladding layers 112 are spaced apart from each other in the third direction Z. The pair of first side cladding layers 112 are arranged to sandwich the core layer 120 and the first upper cladding layer 113. The shape of the first side cladding layer 112 as viewed from the second direction Y is L-shaped. Specifically, the first side cladding layer 112 has a protruding portion 112a. The protruding portion 112a is connected to the first lower cladding layer 111. When viewed from the surface where the first side cladding layer 112 is connected to the core layer 120, the protruding portion 112a is arranged on the opposite side to the region where the core layer 120 is arranged.
[0015] The first upper cladding layer 113 is connected to the upper surface of the core layer 120. That is, in the first direction X, the core layer 120 is sandwiched between the first lower cladding layer 111 and the first upper cladding layer 113. In the third direction Z, the core layer 120 is sandwiched between the pair of first side cladding layers 112. In this way, the cladding layer 110 surrounds the core layer 120. Note that the width of the first upper cladding layer 113 in the third direction Z is the same as the width of the core layer 120 in the third direction Z. The width of the first lower cladding layer 111 in the third direction Z is larger than the width of the core layer 120 in the third direction Z. Thus, as shown in FIGS. 1 and 3 , the spot size converter 100 according to the first embodiment has a striped mesa structure.
[0016] Here, the refractive index of the core layer 120 is n1a. Specifically, the refractive index of the first core layer 121 is n1a. The refractive index of the cladding layer 110 is n2a. The refractive index n1a of the core layer 120 is greater than the refractive index n2a of the cladding layer 110. Note that, when the cladding layer 110 is composed of multiple components, the refractive index n2a of the cladding layer 110 corresponds to the largest refractive index among the multiple components. When light travels from a medium with a high refractive index to a medium with a low refractive index, if the angle of incidence of the light on the medium with a low refractive index exceeds the critical angle, the light does not travel to the medium with a low refractive index. In other words, if the angle of incidence of the light on the medium with a low refractive index exceeds the critical angle, total reflection occurs, in which all of the light is reflected back to the medium with a high refractive index. In this way, light can be propagated by surrounding the core layer 120 with the cladding layer 110.
[0017] Here, we will explain the problems with the conventional spot size converter 100. The second end face 121s2 is connected to another optical device (e.g., a semiconductor modulator, a silicon optical waveguide, an optical fiber, etc.). Coupling optical waveguides with different spot sizes reduces the optical coupling efficiency. In particular, a small spot size requires high-precision mounting of the optical device. In other words, a small spot size requires advanced mounting technology, which ultimately increases manufacturing costs. Therefore, a large spot size is preferable. The spot size converter 100 adjusts the spot size of light incident from the second end face 121s2 to match the spot size of the optical device to which it is coupled. Specifically, the spot size converter 100 can increase the spot size of light emitted from the first end face 121s1.
[0018] The spot size is determined by the thickness and width of the core layer 120. That is, the spot size can be adjusted by changing the thickness and width of the core layer 120. Alternatively, light can be made to seep into the cladding layer 110 by reducing the difference between the refractive index of the core layer 120 and the refractive index of the cladding layer 110. The width of the core layer 120 in the third direction Z can be adjusted relatively easily using common lithography and dry processing techniques.
[0019] On the other hand, increasing the thickness of the core layer 120 in the first direction X poses a problem of complicating the manufacturing process. Specifically, when a semiconductor device manufacturing process is applied to the manufacturing process of the spot size converter 100, the crystal film that will become the core layer 120 is thickened by epitaxial growth. Dry etching, such as RIE (Reactive Ion Etching), is then performed. The depth of the dry etching must be precisely controlled. To precisely control the depth of the dry etching, it is necessary to form an Etch-Stop Layer (ESL) in advance within the optical device. Therefore, increasing the thickness of the core layer 120 in the first direction X complicates the manufacturing process.
[0020] The spot size converter 100 is not used alone. The spot size converter 100 is used monolithically integrated with an optical device such as a semiconductor laser. Therefore, when the optical device to which it is coupled is a semiconductor laser, increasing the thickness of the core layer 120 requires increasing the thickness of the upper cladding layer of the coupled optical device. Increasing the thickness of the upper cladding layer increases the device resistance of the semiconductor laser. As a result, the characteristics of the semiconductor laser deteriorate. It is also possible to thicken only the cladding layer 110 of the spot size converter 100 using selective growth technology. However, this requires advanced selective growth technology. In other words, increasing the thickness of the core layer 120 may impose limitations on the characteristics. For the reasons described above, there is room for improvement in the spot size converter 100 in terms of adjusting the spot size in the vertical direction.
[0021] Here, as shown in FIGS. 1 to 4 , the spot size converter 100 according to this embodiment is characterized in that the core layer 120 includes a high-refractive-index region 131. The refractive index of the high-refractive-index region 131 is defined as n3a. The refractive index n3a is greater than the refractive index n1a of the first core layer 121. In the first direction X, the high-refractive-index region 131 may be disposed closer to the first upper cladding layer 113 than the center of the thickness of the core layer 120 in the first direction X, but is preferably disposed closer to the substrate 101. In this manner, light propagating within the core layer 120 spreads in the direction in which the high-refractive-index region 131 is disposed. In particular, since the high-refractive-index region 131 is disposed closer to the substrate 101, the light spreads toward the first lower cladding layer 111 shown in FIG. 1 to the substrate 101. As a result, the spot size can be enlarged along the first direction X while maintaining the performance of the optical device to be coupled, without increasing the thickness of the cladding layer of the optical device.
[0022] As shown in FIG. 2 , the shape of the high refractive index region 131 may be, for example, triangular in plan view from the first direction X. The width of the high refractive index region 131 in the third direction Z at the first end face 121s1 is the same as the width of the core layer 120 in the third direction Z. The width of the high refractive index region 131 in the third direction Z narrows toward the second end face 121s2. From a different perspective, the high refractive index region 131 includes a first high refractive index region 131a and a second high refractive index region 131b. In the second direction Y, the first high refractive index region 131a is located farther from the second end face 121s2 than the second high refractive index region 131b. The width of the second high refractive index region 131b in the third direction Z is smaller than the width of the first high refractive index region 131a in the third direction Z. That is, in a plan view, the high-refractive-index region 131 has a tip 131t where two side surfaces of the high-refractive-index region 131 intersect at an acute angle. In a plan view, the tip 131t of the high-refractive-index region 131 is the portion of the high-refractive-index region 131 that is located closest to the second end face 121s2. The base of the high-refractive-index region 131 is located on the first end face 121s1. In this way, the width of the high-refractive-index region 131 in the third direction Z increases from the second end face 121s2 toward the first end face 121s1, and thus the spot size adiabatically expands along the light propagation direction.
[0023] Note that, in a planar view, the shape of the high refractive index region 131 does not necessarily have to be triangular. In a planar view, the shape of the high refractive index region 131 may be any shape. For example, in a planar view, the periphery of the high refractive index region 131 may be curved. Specifically, the sides connecting both ends of the high refractive index region 131 at the first end face 121s1 to the tip end 131t may be curved. For example, in a planar view, the shape of the high refractive index region 131 may be quadrangular. Specifically, the width of the high refractive index region 131 in the third direction Z may be uniformly the same as the width of the core layer 120 from the first end face 121s1 to the second end face 121s2. In this way, in a planar view, the shape of the high refractive index region 131 may be polygonal.
[0024] <Method of Manufacturing Spot Size Converter> Fig. 5 is a flowchart of a method of manufacturing the spot size converter 100 according to the first embodiment. As shown in Figs. 5 and 6, the method of manufacturing the spot size converter 100 according to the present embodiment first performs a step (S1a) of preparing a substrate 101. The substrate 101 may be, for example, an InP (indium phosphide) substrate 101. The conductivity type of the substrate 101 may be p-type. The conductivity type of the substrate 101 may be n-type. The substrate 101 may also be a semi-insulating substrate.
[0025] Next, a step (S2a) of forming a cladding layer 110 is performed. In this step (S2a), as shown in FIG. 7 , a first lower cladding layer 111 is formed on the substrate 101. The first lower cladding layer 111 is formed by a crystal growth method such as metal organic chemical vapor deposition (MOCVD). The first lower cladding layer 111 is made of a material having a refractive index n2a that is lower than the refractive index n1a of the core layer 120, which will be described later. The material constituting the first lower cladding layer 111 may be any material that is lattice-matched to the core layer 120, and may be, for example, InP or InGaAsP.
[0026] As will be described later, light propagating within the core layer 120 may seep into the first lower cladding layer 111. By making the difference between the refractive index of the first lower cladding layer 111 and the refractive index n1a of the core layer 120 smaller than the difference between the refractive index of the first upper cladding layer 113 or the first side cladding layer 112 and the refractive index n1a of the core layer 120, light propagating within the core layer 120 can seep into the first lower cladding layer 111.
[0027] Next, a step (S3a) of forming a core layer 120 is performed. In this step (S3a), as shown in FIG. 8 , the core layer 120 (first core layer 121) is formed on the first lower cladding layer 111. Similar to the method of forming the first lower cladding layer 111, the core layer 120 may be formed using metalorganic chemical vapor deposition. The material constituting the core layer 120 may be, for example, InP. From the viewpoint of light absorption rate, the core layer 120 made of InP is preferably undoped. The core layer 120 may be semi-insulating. The material of the core layer 120 may be InGaAsP, AlGaInAs, or InGaAs. The core layer 120 may be n-type InP or p-type InP. The core layer 120 may be composed of only a single material. The core layer 120 may also be composed of multiple materials each having a different refractive index.
[0028] Next, a step (S4a) of forming high refractive index region 131 is performed. In this step (S4a), as shown in FIG. 9 , high refractive index region 131 is formed on core layer 120. Similar to the method of forming first lower cladding layer 111, high refractive index region 131 may be formed using metalorganic vapor phase epitaxy. The material constituting high refractive index region 131 is a material having a refractive index n3a higher than the refractive index n1a of core layer 120. When core layer 120 is made of undoped InP, the material constituting high refractive index region 131 may be, for example, InGaAsP, AlGaInAs, or InGaAs. When core layer 120 is made of n-type InP, the material constituting high refractive index region 131 may be, for example, undoped InP, semi-insulating InP, or p-type InP. This allows utilization of the plasma effect. When core layer 120 is made of a plurality of materials each having a different refractive index, the materials must be selected so that the refractive index n3a of high refractive index region 131 is higher than the effective refractive index n1a of core layer 120. In this manner, first lower cladding layer 111, core layer 120, and high refractive index region 131 may be formed in this order on substrate 101 by metal organic chemical vapor deposition.
[0029] Next, an etching step (S5a) is performed. In this step (S5a), as shown in FIG. 10, a first processing mask 141 is formed on the high refractive index region 131. The first processing mask 141 is made of, for example, SiO 2 The film is either a SiO film or a SiN film. 2 The method for forming the SiN film or SiN film is, for example, chemical vapor deposition (CVD). The first processing mask 141 may be patterned into a desired shape using photolithography and etching. As shown in FIG. 11 , the shape of the first processing mask 141 may be triangular in plan view. In plan view, the shape of the first processing mask 141 does not necessarily have to be triangular. For example, in plan view, the sides connecting both ends of the first processing mask 141 on the first end face 121s1 to the tip portion on the second end face 121s2 side may be curved. For example, in plan view, the shape of the first processing mask 141 may be rectangular. Specifically, the width of the first processing mask 141 in the third direction Z may be the same from the first end face 121s1 to the second end face 121s2, and may be the same as the width of the core layer 120, for example.
[0030] Next, the high refractive index region 131 is dry-etched using the first processing mask 141 as a mask. Specifically, the high refractive index region 131 in the region where the first processing mask 141 is arranged in a planar view is not etched. On the other hand, the high refractive index region 131 in the region where the first processing mask 141 is not arranged in a planar view is etched. As a result, as shown in FIG. 12 , a portion of the high refractive index region 131 is etched so that a portion of the core layer 120 is exposed. At this time, a portion of the core layer 120 may be etched in the first direction X. The etching may be wet etching. After the high refractive index region 131 is etched, the first processing mask 141 is removed by wet etching. In this manner, the high refractive index region 131 having the desired shape is formed.
[0031] Next, a step (S6a) of forming core layer 120 is performed. In this step (S6a), core layer 120 is formed on high refractive index region 131 and on the exposed portion of core layer 120, as shown in Figures 13 and 14. Figure 14 is a cross-sectional view of spot size converter 100 shown along line XIV-XIV in Figure 13. Core layer 120 may be formed using metal organic chemical vapor deposition, similar to the method of forming first lower cladding layer 111.
[0032] The position of the high refractive index region 131 in the first direction X within the core layer 120 is determined by the thickness of the core layer 120 in the first direction X in the step (S3a) of forming the core layer 120 and the thickness of the core layer 120 in the first direction X in the step (S6a) of forming the core layer 120.
[0033] For example, in the step (S3a) of forming the core layer 120, the core layer 120 is formed to a thickness of 1 μm in the first direction X. In the step (S4a) of forming the high refractive index region 131, the high refractive index region 131 is formed to a thickness of 100 nm in the first direction X. In the step (S6a) of forming the core layer 120, the core layer 120 is formed to a thickness of 1 μm in the first direction X. In this case, the high refractive index region 131 is disposed at the center of the thickness of the core layer 120 in the first direction X.
[0034] For example, in the step (S3a) of forming the core layer 120, the core layer 120 is formed to a thickness of 500 nm in the first direction X. In the step (S4a) of forming the high refractive index region 131, the high refractive index region 131 is formed to a thickness of 100 nm in the first direction X. In the step (S6a) of forming the core layer 120, the core layer 120 is formed to a thickness of 1500 nm in the first direction X. In this case, in the first direction X, the high refractive index region 131 is positioned closer to the substrate 101 than the center of the thickness of the core layer 120 in the first direction X.
[0035] For example, the step (S3a) of forming the core layer 120 may not be performed. That is, the step (S4a) of forming the high refractive index region 131 may be performed after the step (S2a) of forming the cladding layer 110. In the step (S4a) of forming the high refractive index region 131, the high refractive index region 131 is formed to a thickness of 100 nm in the first direction X. In the step (S6a) of forming the core layer 120, the core layer 120 is formed to a thickness of 2 μm in the first direction X. In this case, the high refractive index region 131 is disposed in the core layer 120 at a position closest to the first lower cladding layer 111 in the first direction X.
[0036] In this way, the position of the high refractive index region 131 in the first direction X within the core layer 120 can be easily controlled.
[0037] Next, an etching step (S7a) is performed. In this step (S7a), a second processing mask 142 is formed on the core layer 120, as shown in FIGS. 15 and 16. FIG. 16 is a cross-sectional view of the spot size converter 100 shown along the line XVI-XVI in FIG. 15. The second processing mask 142 is made of, for example, SiO 2 The film is either a SiO film or a SiN film. 2 The method for forming the SiN film or SiN film is, for example, chemical vapor deposition. The second processing mask 142 may be patterned into a desired shape using photolithography and etching. As shown in FIG. 15 , the second processing mask 142 has a rectangular shape in plan view. The second processing mask 142 is formed to extend from the first end face 121s1 to the second end face 121s2. The second processing mask 142 is formed at the center of the width of the core layer 120 in the third direction Z so that the edge of the core layer 120 is exposed. In other words, the width of the second processing mask 142 in the third direction Z is uniformly smaller than the width of the core layer 120.
[0038] Next, the core layer 120 is dry-etched using the second processing mask 142 as a mask. Specifically, the core layer 120 is not etched in the region where the second processing mask 142 is disposed in a planar view. On the other hand, the core layer 120 is etched in the region where the second processing mask 142 is not disposed in a planar view. As a result, only the core layer 120 located on both sides of the second processing mask 142 in the third direction Z is etched. At this time, as shown in FIGS. 17 and 18 , the core layer 120 may be etched in the first direction X so as to expose a portion of the first lower cladding layer 111. It is also sufficient that the core layer 120 is etched in the first direction X to a depth below the high refractive index region 131. Therefore, for example, the etching may reach the substrate 101. The etching may be wet etching, but dry etching is preferable from the viewpoint of controlling the shape of the core layer 120. After etching the core layer 120, the second processing mask 142 is removed by wet etching. In this way, an optical waveguide having a mesa structure 151 of a desired shape is formed, as shown in FIG.
[0039] Next, the step (S8a) of forming cladding layer 110 is performed. In this step (S8a), as shown in FIGS. 19 and 20, cladding layer 110 is formed on core layer 120 and on exposed portions of first lower cladding layer 111. FIG. 20 is a cross-sectional view of spot size converter 100 shown along line XX-XX in FIG. 19. Specifically, as shown in FIG. 20, first upper cladding layer 113 is formed on core layer 120. A pair of first side cladding layers 112 are formed on first lower cladding layer 111 so as to sandwich core layer 120. The material constituting first upper cladding layer 113 and first side cladding layer 112 may be a material having a refractive index n2a lower than the refractive index n1a of core layer 120. When core layer 120 is made of InP, the material constituting first upper cladding layer 113 and first side cladding layer 112 may be, for example, SiO 2 The film may be at least one of a SiO film and a SiN film. 2The SiN film or the SiN film may be formed by, for example, chemical vapor deposition. When the core layer 120 is made of at least one of InGaAsP and AlGaInAs, the first upper cladding layer 113 and the first side cladding layer 112 may be made of InP. The InP film may be formed by, for example, metalorganic vapor phase deposition.
[0040] The core layer 120 only needs to be in contact with a medium having a refractive index lower than the refractive index n1a of the core layer 120. Therefore, at least one of the first upper cladding layer 113 and the first side cladding layer 112 may be air. In other words, the side surface 121s3 of the core layer 120 may be exposed. In this case, after the etching step (S7a) is performed, a SiO 2 film is formed as a protective film for the mesa structure 151. 2 A film may be formed, but nothing may be formed.
[0041] The refractive index n2a of the first upper cladding layer 113 and the first side cladding layer 112 may be smaller than the refractive index of the first lower cladding layer 111. This allows light propagating through the core layer 120 to seep into the substrate 101 without seeping into the first upper cladding layer 113 and the first side cladding layer 112. In this way, the material forming the first upper cladding layer 113 and the first side cladding layer 112 may be different from the material forming the first lower cladding layer 111.
[0042] In this way, a spot size converter 100 with vertically controllable spot size can be obtained, as shown in FIGS.
[0043] <Operation> Next, the operation of the spot size converter 100 will be described.
[0044] The spot size converter 100 is connected to an optical device such as a light source or a modulator. For example, assume that the spot size converter 100 is connected to a semiconductor laser, which is a light source. The spot size converter 100 is connected to the semiconductor laser at the second end face 121s2. Light propagates from the semiconductor laser. The light enters the core layer 120. As described above, the core layer 120 is surrounded by the cladding layer 110, which has a refractive index lower than that of the core layer 120. Therefore, the light is confined within the core layer 120. The light propagates within the core layer 120 along the second direction Y. The light spreads in the direction in which the high-refractive-index region 131 is disposed. In particular, since the high-refractive-index region 131 is disposed on the substrate 101 side, the light spreads in the vertical direction (the first direction X shown in FIG. 1 ). The light exits from the first end face 121s1. In this manner, the light is emitted to the outside of the semiconductor device including the spot size converter 100.
[0045] <Effects> The spot size converter 100 according to the present disclosure includes a core layer 120 and a cladding layer 110. The cladding layer 110 surrounds the core layer 120. The core layer 120 includes a first core layer 121. The refractive index of the cladding layer 110 is lower than the refractive index of the first core layer 121. The core layer 120 includes a high refractive index region 131. The high refractive index region 131 has a refractive index higher than the refractive index of the first core layer 121.
[0046] In this way, light propagating within the core layer 120 spreads in the direction in which the high refractive index regions 131 are arranged. In particular, by appropriately changing the locations in which the high refractive index regions 131 are arranged in the first direction X, the spot size can be adjusted in the vertical direction (the first direction X shown in FIG. 1 ).
[0047] The spot size converter 100 further includes a substrate 101. The substrate 101 is connected to the cladding layer 110. A direction in which the core layer 120 is viewed from the substrate 101 is defined as a first direction X. The high refractive index region 131 is disposed closer to the substrate 101 than the center of the thickness of the core layer 120 in the first direction X. This allows light to spread in the vertical direction. The light spread in the vertical direction can seep out toward the substrate 101.
[0048] In the spot size converter 100, the high refractive index region 131 includes a first high refractive index region 131a and a second high refractive index region 131b. In the second direction Y, the first high refractive index region 131a is farther from the second end face 121s2 than the second high refractive index region 131b. The width of the second high refractive index region 131b in a direction perpendicular to the second direction Y (third direction Z) is smaller than the width of the first high refractive index region 131a. In this way, the spot size expands adiabatically along the light propagation direction. As a result, the spot size is expanded efficiently.
[0049] FIG. 21 is a perspective view of a spot size converter 300 according to Comparative Example 1. FIG. 21 corresponds to FIG. 1. The spot size converter 300 shown in FIG. 21 basically has the same configuration as the spot size converter 300 shown in FIGS. 1 to 4, but differs in that the core layer 120 does not include a high refractive index region 131. FIG. 22 is a distribution diagram showing the light intensity in the vertical direction at the first end face 121s1. The distribution diagram shows the light intensity distribution in a near-field pattern (NFP). The solid line in FIG. 22 shows the light intensity distribution in Example 1. Example 1 basically has the same configuration as the spot size converter 100 according to the first embodiment. In FIG. 22, the dotted line shows the light intensity distribution in Comparative Example 1. In FIG. 22, the horizontal axis indicates the height of the core layer in the vertical direction, specifically the distance (unit: μm) from the first lower cladding layer 111. In FIG. 22, the vertical axis indicates the relative light intensity (unit: -) in the vertical direction. 22, the plane where the first lower cladding layer 111 is connected to the core layer 120 is used as the reference (=0 μm). The direction toward the first upper cladding layer 113 as viewed from the first lower cladding layer 111 is the positive direction on the horizontal axis. On the other hand, the direction toward the substrate 101 as viewed from the first lower cladding layer 111 is the negative direction on the horizontal axis. The distribution diagram shown in FIG. 22 is normalized by the maximum value of the light intensity in the first direction X (vertical direction).
[0050] As can be seen from Figure 22, there are two distances from the first lower cladding layer 111 where the light intensity is 0.5. The difference between the distances from the first lower cladding layer 111 at these two points is the half-width. The half-width in Comparative Example 1 is 1.87 µm. The half-width in Example 1 is 2.13 µm. In other words, the half-width in Example 1 is larger than the half-width in Comparative Example 1. From the above results, it can be seen that the core layer 120 includes the high refractive index region 131, which increases the spot size in the first direction X.
[0051] Second Embodiment <Structure of Spot Size Converter> Fig. 23 is a perspective view of spot size converter 200 according to the second embodiment. Fig. 23 corresponds to Fig. 1. Fig. 24 is a plan view of spot size converter 200 according to the second embodiment. Fig. 24 corresponds to Fig. 2. Fig. 25 is a cross-sectional view of spot size converter 200 shown along line XXV-XXV in Fig. 24. Fig. 25 corresponds to Fig. 3. Fig. 26 is a cross-sectional view of spot size converter 200 shown along line XXVI-XXVI in Fig. 24. Fig. 26 corresponds to Fig. 4. Note that in Figs. 23 and 24, the boundary between high refractive index region 231 and second core layer 241 is indicated by a dotted line.
[0052] The spot size converter 200 shown in Figures 23 to 26 basically has the same configuration as the spot size converter 100 shown in Figures 1 to 4, but differs in that the core layer 220 includes a region having a higher refractive index than the other regions of the core layer 220, in addition to the high refractive index region 231. Specifically, the core layer 220 includes a first core layer 221 and a second core layer 241. The first core layer 221 corresponds to the core layer 220 of the first embodiment. The refractive index n2b of the second core layer 241 is higher than the refractive index n1b of the first core layer 221. In this way, light propagates through the second core layer 241 with low loss.
[0053] In particular, it is more preferable that the refractive index n2b of the second core layer 241 is higher than the refractive index n3b of the high refractive index region 231. The refractive index of the first core layer 221 is set to n1b. The refractive index of the second core layer 241 is set to n2b. The refractive index of the high refractive index region 231 is set to n3b. The refractive index of the cladding layer 250 is set to n4b. The spot size converter 200 satisfies the relationship n2b > n3b > n1b > n4b. In this way, light can be efficiently propagated from the second core layer 241 to the first core layer 221.
[0054] 24 , a region in the second direction Y where the high refractive index region 231 is not arranged in a plan view is referred to as a first region 281. Specifically, the first region 281 is a region in the second direction Y from the first end face 221s1 to the tip end 231t of the high refractive index region 231. On the other hand, a region in the second direction Y where the high refractive index region 231 is arranged is referred to as a second region 282. Specifically, the second region 282 is a region in the second direction Y from the first end face 221s1 to the tip end 231t of the high refractive index region 231.
[0055] As shown in FIGS. 23 and 24 , the second core layer 241 is disposed at the center of the core layer 220 in the third direction Z. The second core layer 241 also extends in the second direction Y from the second end face 221s2 to a region overlapping with the high refractive index region 231. Specifically, as shown in FIG. 24 , in a plan view, the second core layer 241 extends from the second end face 221s2 to the second region 282. In this way, a portion of the second core layer 241 is disposed in the region in the second direction Y where the high refractive index region 231 is disposed. In a plan view, the shape of the second core layer 241 in the first region 281 is quadrangular. Specifically, in the first region 281, the width of the second core layer 241 in the third direction Z is uniform. In the first region 281, the width of the second core layer 241 in the third direction Z is smaller than the width of the first core layer 221 in the second region 282 in the third direction Z.
[0056] In a plan view, the shape of the second core layer 241 in the second region 282 is triangular. In the second region 282, the width of the second core layer 241 in the third direction Z gradually decreases toward the first end face 221s1. Specifically, the second core layer 241 includes a first core region 241a and a second core region 241b. In the second direction Y, the second core region 241b is farther from the second end face 221s2 than the first core region 241a. In the third direction Z, the width of the second core region 241b is smaller than the width of the first core region 241a. In the second region 282, the second core layer 241 has a tip portion 241t. In the second core layer 241, the tip portion 241t is located at a position closest to the first end face 221s1 in the second direction Y. In the second region 282, the base of the second core layer 241 is located at the boundary 283 between the first region 281 and the second region 282. The sides connecting both ends of the base of the second core layer 241 to the tip end 241t are straight lines. Thus, in a plan view, the shape of the second core layer 241 is a pentagon that combines a rectangle and a triangle.
[0057] By doing so, as the light propagating through the second core layer 241 approaches the first end face 221s1, the second core layer 241 is no longer able to confine the light. The light gradually seeps out from the second core layer 241 into the first core layer 221. When the width of the second core layer 241 in the third direction Z becomes sufficiently small, all of the light moves from the second core layer 241 to the first core layer 221.
[0058] In plan view, the shape of the second core layer 241 does not necessarily have to be a pentagon. In plan view, the shape of the second core layer 241 may be any shape. The shape of the second core layer 241 may be a polygon such as a triangle or a rectangle. For example, in plan view, the sides connecting both ends of the base of the second core layer 241 and the tip end 241t may be curved.
[0059] 25 , the high refractive index region 231 may be disposed at a position closer to the substrate 201 in the first direction X than the second core layer 241. Specifically, in the first direction X, the second core layer 241 may be disposed at a position sandwiched between the high refractive index region 231 and the first upper cladding layer 251. In this way, light leaking out from the second core layer 241 spreads in the vertical direction (the first direction X shown in FIG. 25 ).
[0060] In plan view, the high-refractive-index region 231 may have any shape. As shown in FIG. 24 , the shape of the high-refractive-index region 231 in the spot size converter 200 according to the second embodiment is a combination of a rectangle and two triangles. Specifically, the high-refractive-index region 231 extends from the first end face 221s1 to the boundary 283 between the first region 281 and the second region 282. In plan view, the rectangle portion of the high-refractive-index region 231 is disposed on the first end face 221s1 side in the second direction Y. In the second direction Y, the rectangle portion of the high-refractive-index region 231 is disposed between the first end face 221s1 and the triangular portion of the high-refractive-index region 231. The width of the rectangle portion of the high-refractive-index region 231 in the third direction Z is uniform from the first end face 221s1 to the region where the triangular portion of the high-refractive-index region 231 is disposed. The width in the third direction Z of the quadrangular portion of the high refractive index region 231 is the same as the width in the third direction Z of the first core layer 221 .
[0061] The triangular portion of the high refractive index region 231 is disposed between a boundary 283 between the first region 281 and the second region 282 and the rectangular portion of the high refractive index region 231. The width of the triangular portion of the high refractive index region 231 in the third direction Z gradually decreases from the rectangular portion of the high refractive index region 231 toward the second end face 221s2. Specifically, the triangular portion of the high refractive index region 231 includes a first high refractive index region 231a and a second high refractive index region 231b. In the second direction Y, the first high refractive index region 231a is farther from the second end face 221s2 than the second high refractive index region 231b. The width of the second high refractive index region 231b in the third direction Z is smaller than the width of the first high refractive index region 231a. 24 , when two triangular portions in the high refractive index region 231 are arranged side by side in the third direction Z, the width of the high refractive index region 231 is the sum of the widths of the two triangular portions in the third direction Z. The triangular portion in the high refractive index region 231 has a tip 231t. The tip 231t is located at the boundary 283 between the first region 281 and the second region 282. The triangular portion in the high refractive index region 231 and the square portion in the high refractive index region 231 are connected at the base of the triangular portion in the high refractive index region 231. The sides connecting both ends of the base of the triangular portion in the high refractive index region 231 and the tip 231t are straight lines. The sides connecting both ends of the base of the triangular portion in the high refractive index region 231 and the tip 231t may be curved lines.
[0062] 24 , in a plan view, the tip portion 241t of the second core layer 241 is located at the same position as point p1 where the two triangular portions in the high refractive index region 231 are connected. Specifically, the two triangular portions in the high refractive index region 231 are spaced apart from each other by the same distance from the center of the width of the first core layer 221 in the third direction Z. In other words, point p1 is located at the center of the width of the first core layer 221 in the third direction Z. The tip portion 241t of the second core layer 241 is located at the center of the width of the first core layer 221 in the third direction Z. In the second direction Y, the tip portion 241t of the second core layer 241 is located at a position where the base of the triangular portion in the high refractive index region 231 is located.
[0063] The function of the core layer 220 in the first region 281 is different from the function of the core layer 220 in the second region 282. The refractive index n2b of the second core layer 241 is higher than the refractive index n1b of the first core layer 221. Therefore, in the first region 281, the first core layer 221 connected to the second core layer 241 functions as a cladding layer for the second core layer 241.
[0064] <Method of Manufacturing Spot Size Converter> FIG. 27 is a flowchart of a method of manufacturing the spot size converter 200 according to the second embodiment. FIGS. 28 to 53 are cross-sectional views or plan views for explaining the method of manufacturing the spot size converter 200 according to the second embodiment shown in FIG. 27. As shown in FIGS. 27 and 28, the method of manufacturing the spot size converter 200 according to the second embodiment first performs a step (S1b) of preparing a substrate 201. The substrate 201 may be, for example, an InP (indium phosphide) substrate 201. The conductivity type of the substrate 201 may be p-type. The conductivity type of the substrate 201 may be n-type. The substrate 201 may be a semi-insulating substrate.
[0065] Next, a step (S2b) of forming a cladding layer 250 is performed. In this step (S2b), as shown in FIG. 29 , a first lower cladding layer 253 is formed on the substrate 201. The first lower cladding layer 253 is formed by a crystal growth method such as metal organic chemical vapor deposition. As will be described later, the material constituting the first lower cladding layer 253 is a material having a refractive index lower than the refractive index n1b of the first core layer 221. The material constituting the first lower cladding layer 253 may be any material that is lattice-matched with the core layer 220, and may be, for example, InP or InGaAsP.
[0066] As will be described later, light propagating within the first core layer 221 may seep into the first lower cladding layer 253. In this case, by making the difference between the refractive index of the first lower cladding layer 253 and the refractive index n1b of the first core layer 221 smaller than the difference between the refractive index of the first upper cladding layer 251 or the first side cladding layer 252 and the refractive index n1b of the core layer 220, the light propagating within the core layer 220 can seep into the first lower cladding layer 221.
[0067] Next, a step (S3b) of forming a core layer 220 is performed. In this step (S3b), as shown in FIG. 30 , a first core layer 221 constituting the core layer 220 is formed on the first lower cladding layer 253. Similar to the method of forming the first lower cladding layer 253, the first core layer 221 may be formed using metalorganic chemical vapor deposition. The material constituting the first core layer 221 may be, for example, InP. From the viewpoint of light absorption, the first core layer 221 composed of InP is preferably undoped. The first core layer 221 may be semi-insulating. The material of the first core layer 221 may be InGaAsP, AlGaInAs, or InGaAs. The material constituting the first core layer 221 may be n-type InP or p-type InP. The first core layer 221 may be composed of only a single material. The first core layer 221 may also be composed of multiple materials each having a different refractive index. The first lower cladding layer 253 and the first core layer 221 may be made of the same material. That is, the first lower cladding layer 253 and the first core layer 221 may be formed simultaneously by metal organic chemical vapor deposition. However, the first core layer 221 in the first region 281 has a different function from the first core layer 221 in the second region 282. That is, the first core layer 221 in the first region 281 functions as a cladding layer for the second core layer 241 (see FIG. 23 ). The first core layer 221 in the second region 282 functions as a core layer that propagates light leaking from the second core layer 241.
[0068] Next, a step (S4b) of forming a high refractive index region 231 is performed. In this step (S4b), as shown in FIG. 31 , the high refractive index region 231 is formed on the first core layer 221. Similar to the method of forming the first lower cladding layer 253, the high refractive index region 231 may be formed using a metal-organic chemical vapor deposition method. The material constituting the high refractive index region 231 is a material having a refractive index n3b higher than the refractive index n1b of the first core layer 221. When the material constituting the first core layer 221 is undoped InP, the material constituting the high refractive index region 231 may be, for example, InGaAsP, AlGaInAs, or InGaAs. When the material constituting the first core layer 221 is n-type InP, the material constituting the high refractive index region 231 may be, for example, undoped InP, semi-insulating InP, or p-type InP. This allows the plasma effect to be utilized. When first core layer 221 is made of a plurality of materials each having a different refractive index, it is necessary to select the materials so that refractive index n3b of high refractive index region 231 is higher than effective refractive index n1a of first core layer 221. In this manner, first lower cladding layer 253, first core layer 221, and high refractive index region 231 may be formed in this order on substrate 201 by metal organic chemical vapor deposition.
[0069] Next, an etching step (S5b) is performed. In this step (S5b), as shown in FIG. 32, a first processing mask 261 is formed on the high refractive index region 231. The first processing mask 261 is made of, for example, SiO 2 The film is either a SiO film or a SiN film. 2The method for forming the SiN film or SiN film is, for example, chemical vapor deposition. As shown in FIG. 33 , the first processing mask 261 may be patterned into a desired shape using photolithography and etching. As shown in FIG. 33 , in a plan view, the shape of the first processing mask 261 may be a combination of a triangle and a rectangle. In a plan view, the sides connecting both ends of the base of the triangular portion of the first processing mask 261 to the tip may be curved. For example, in a plan view, the shape of the first processing mask 261 may be a rectangle. Specifically, the width of the first processing mask 261 in the third direction Z may be uniformly the same as the width of the first core layer 221 from the first end face 221s1 (see FIG. 24 ) to the second end face 221s2 (see FIG. 24 ).
[0070] Next, the high refractive index region 231 is dry-etched using the first processing mask 261 as a mask. Specifically, the high refractive index region 231 in the region where the first processing mask 261 is arranged in a planar view is not etched. On the other hand, the high refractive index region 231 in the region where the first processing mask 261 is not arranged in a planar view is etched. As a result, as shown in FIGS. 34 and 35 , only the high refractive index region 231 is etched so that a portion of the first core layer 221 is exposed. At this time, a portion of the first core layer 221 may be etched in the first direction X. The etching may be wet etching. After the high refractive index region 231 is etched, the first processing mask 261 is removed by wet etching. In this manner, the high refractive index region 231 having the desired shape is formed.
[0071] Next, a step (S6b) of forming core layer 220 is carried out. In this step (S6b), first core layer 221 is formed on high refractive index region 231 and a part of first core layer 221, as shown in Figures 36 and 37. Figure 37 is a cross-sectional view of spot size converter 200 shown along line segment XXXVII-XXXVII in Figure 36. Similar to the method of forming first lower cladding layer 253, first core layer 221 may be formed using metal organic chemical vapor deposition.
[0072] Next, as shown in FIG. 38 , the second core layer 241 is formed on the first core layer 221. The material constituting the second core layer 241 is a material having a refractive index n2b higher than the refractive index n1b of the first core layer 221. The material constituting the second core layer 241 is preferably a material having a refractive index n2b higher than the refractive index n3b of the high refractive index region 231. When the second core layer 241 is composed of multiple materials each having a different refractive index, the multiple materials are preferably selected so that the effective refractive index n2b of the second core layer 241 is higher than the effective refractive indices of the first core layer 221 and the high refractive index region 231. The material constituting the second core layer 241 may be, for example, InGaAsP or AlGaInAs.
[0073] 39 , the first core layer 221 is formed on the second core layer 241. The first core layer 221 may be formed by metal organic chemical vapor deposition, similar to the method for forming the first lower cladding layer 253. At this time, the first core layer 221 in the first region 281 is formed as the second upper cladding layer 213.
[0074] Next, an etching step (S7b) is performed. In this step (S7b), as shown in FIG. 40, a second processing mask 262 is formed on the first core layer 221. The second processing mask 262 is made of, for example, SiO 2 The film is either a SiO film or a SiN film. 2 The method for forming the SiN film or the SiN film is, for example, chemical vapor deposition. The second processing mask 262 is patterned into a desired shape using photolithography and etching. As shown in FIG. 40 , the second processing mask 262 has, for example, a pentagonal shape in plan view. The second processing mask 262 is formed to extend from the second end face 221s2 to the second region 282. The second processing mask 262 is formed at the center of the width of the first core layer 221 in the third direction Z. The width of the second processing mask 262 in the third direction Z is smaller than the width of the core layer 220.
[0075] Next, the first core layer 221 and the second core layer 241 are dry-etched. Specifically, the first core layer 221 and the second core layer 241 are not etched in a region where the second processing mask 262 is arranged in a planar view. On the other hand, the first core layer 221 and the second core layer 241 are etched in a region where the second processing mask 262 is not arranged in a planar view. In this dry-etching process, the first core layer 221 is etched to a position between the second core layer 241 and the high refractive index region 231 in the first direction X. That is, as shown in FIGS. 41 and 42 , the first core layer 221 may be etched in the first direction X so as to expose a portion of the first core layer 221 (the first core layer 221 in the second region 282 and the portion of the first core layer 221 functioning as the second lower cladding layer 211 in the first region 281). Figure 42 is a cross-sectional view of the spot size converter 200 shown along line XLII-XLII in Figure 41. As shown in Figure 42, the side surfaces of the second core layer 241 are exposed. The high refractive index region 231 is not exposed and is surrounded by the first core layer 221. Although wet etching may be used, dry etching is preferable from the viewpoint of controlling the shape of the core layer 220. In this way, an optical waveguide with a ridge structure having a desired shape is formed, as shown in Figure 43.
[0076] Next, a step (S8b) of forming a core layer 220 is performed. In this step (S8b), as shown in FIG. 44 , the core layer 220 is formed on the second lower cladding layer 211 and the first core layer 221. FIG. 45 is a cross-sectional view of the spot size converter 200 shown along the line segment XLV-XLV in FIG. 44 . FIG. 46 is a cross-sectional view of the spot size converter 200 shown along the line segment XLVI-XLVI in FIG. 44 . As shown in FIG. 45 , the first core layer 221 is formed up to the position of the lower surface of the second processing mask 262 in the first direction X. In other words, the first core layer 221 is formed so as to cover the second core layer 241. The second processing mask 262 is exposed. Similar to the method of forming the first lower cladding layer 253, the first core layer 221 may be formed using metalorganic chemical vapor deposition. 44, the first core layer 221 in the first region 281 is formed as the second side cladding layer 212. After the first core layer 221 is formed, the second processing mask 262 is removed by wet etching.
[0077] Considering that the second side cladding layer 212 in the first region 281 is connected to an optical device such as a semiconductor laser, it is preferable that the second side cladding layer 212 have a current confinement function. Therefore, the second side cladding layer 212 may have a three-layer structure, for example, in which a p-type InP layer, an n-type InP layer, and a p-type InP layer are stacked in this order. The second side cladding layer 212 may have a three-layer structure, for example, in which a p-type InP layer, a semi-insulating InP layer, and an n-type InP layer are stacked in this order. The second side cladding layer 212 may have a two-layer structure, for example, in which a semi-insulating InP layer and an n-type InP layer are stacked in this order. The second side cladding layer 212 may have a structure other than the above combination as long as it has a current confinement function.
[0078] Next, a step (S9b) of forming a core layer 220 is performed. In this step (S9b), as shown in Fig. 47 , a first core layer 221 is formed on the second upper cladding layer 213, the second side cladding layer 212, and the first core layer 221. Similar to the method of forming the first lower cladding layer 253, the first core layer 221 may be formed using metal organic chemical vapor deposition. At this time, as shown in Fig. 47 , the first core layer 221 in the first region 281 is formed as the second upper cladding layer 213.
[0079] Considering that the second upper cladding layer 213 in the first region 281 is coupled to an optical device such as a semiconductor laser, the upper surface of the first core layer 221 formed in this step (S9b) may serve as a low-resistance contact layer for ohmic contact with the second upper cladding layer 213 and the electrode. A material with a high absorption coefficient, such as InGaAs, is used to form the contact layer. Therefore, the presence of the contact layer on the waveguide results in a loss of propagating light. After forming the contact layer, only the contact layer of the spot size converter 200 may be selectively etched. When InGaAs is used as the material for the contact layer, the contact layer can be selectively removed by wet etching using, for example, a mixed solution containing tartaric acid. The mixed solution may include, for example, tartaric acid, hydrogen peroxide, and water.
[0080] The position of the high refractive index region 231 in the first direction X within the core layer 220 is determined by the thickness of the first core layer 221 in the first direction X in the step (S3b) of forming the core layer 220, the thickness of the first core layer 221 in the first direction X in the step (S6b) of forming the core layer 220, the thickness of the first core layer 221 in the first direction X in the step (S8b) of forming the core layer 220, and the thickness of the first core layer 221 in the first direction X in the step (S9b) of forming the core layer 220.
[0081] For example, in the step (S3b) of forming the core layer 220, the first core layer 221 is formed to a thickness of 1 μm in the first direction X. In the step (S4b) of forming the high refractive index region 231, the high refractive index region 231 is formed to a thickness of 100 nm in the first direction X. In the step (S6b) of forming the core layer 220, the first core layer 221 is formed to a thickness of 1 μm in the first direction X. In the step (S8b) of forming the core layer 220, the first core layer 221 is formed to a thickness of 500 nm in the first direction X. In the step (S9b) of forming the core layer 220, the first core layer 221 is formed to a thickness of 2 μm in the first direction X. In this case, the thickness of the core layer 220 in the first direction X is 4 μm. The high refractive index region 231 is disposed at a position 1 μm away from the first lower cladding layer 253 in the first direction X. In this way, in the first direction X, the high refractive index region 231 is disposed closer to the substrate 201 than the center of the thickness of the core layer 220 in the first direction X.
[0082] In this way, the position of the high refractive index region 231 in the first direction X within the core layer 220 can be easily controlled.
[0083] Next, an etching step (S10b) is performed. In this step (S10b), as shown in Figures 48 and 49, a third processing mask 263 is formed on first core layer 221. Figure 49 is a cross-sectional view of spot size converter 200 shown on line segment XLIX-XLIX in Figure 48. Third processing mask 263 is made of, for example, SiO 2 The film is either a SiO film or a SiN film. 2 The method for forming the SiN film or the SiN film is, for example, chemical vapor deposition. The third processing mask 263 may be patterned into a desired shape using photolithography and etching. As shown in FIG. 48 , the third processing mask 263 has a rectangular shape in plan view. The third processing mask 263 is formed to extend from the first end face 221s1 to the second end face 221s2. The third processing mask 263 is formed at the center of the width of the first core layer 221 in the third direction Z so that the edge of the first core layer 221 is exposed. In other words, the width of the third processing mask 263 in the third direction Z is uniformly smaller than the width of the first core layer 221.
[0084] Next, the core layer 220 is dry-etched. Specifically, the first core layer 221 is not etched in the region where the third processing mask 263 is arranged in a plan view. On the other hand, the first core layer 221 is etched in the region where the third processing mask 263 is not arranged in a plan view. As a result, only the edge portion of the first core layer 221 in the third direction Z is etched. At this time, as shown in FIGS. 50 and 51 , the first core layer 221 may be etched in the first direction X so as to expose a portion of the first lower cladding layer 253. Alternatively, the first core layer 221 and the first lower cladding layer 253 may be etched in the first direction X so as to expose a portion of the substrate 201. Although wet etching may be used for the etching, dry etching is preferable from the viewpoint of controlling the shape of the core layer 220. After etching the core layer 220, the third processing mask 263 is removed by wet etching. In this manner, an optical waveguide having a desired shape, i.e., a mesa structure 254, is formed, as shown in FIG. 51 .
[0085] Next, a step (S11b) of forming a cladding layer 250 is performed. In this step (S11b), as shown in FIGS. 52 and 53 , the cladding layer 250 (see FIG. 23 ) is formed on the core layer 220 and on the exposed portion of the first lower cladding layer 253. Specifically, as shown in FIG. 53 , a first upper cladding layer 251 is formed on the first core layer 221. A pair of first side cladding layers 252 is formed on the first lower cladding layer 253. The pair of first side cladding layers 252 are arranged to sandwich the core layer 220. The material constituting the first upper cladding layer 251 and the first side cladding layer 252, which are components of the cladding layer 250, may be a material having a refractive index n4b that is lower than the refractive indices n1b and n2b of the core layer 220. When the material constituting the core layer 220 is InP, the material constituting the first upper cladding layer 251 and the first side cladding layer 252 is, for example, SiO 2 The film may be at least one of a SiO film and a SiN film. 2The SiN film or the SiN film may be formed by, for example, chemical vapor deposition. When the core layer 220 is made of at least one of InGaAsP and AlGaInAs, the first upper cladding layer 251 and the first side cladding layer 252 may be made of InP. The InP film may be formed by, for example, metalorganic vapor phase deposition.
[0086] The core layer 220 only needs to be in contact with a medium having a refractive index lower than that of the core layer 220. Therefore, at least one of the first upper cladding layer 251 and the first side cladding layer 252 may be air. In other words, the side surface 221s3 of the core layer 220 may be exposed. In this case, after the etching step (S7a) is performed, a SiO 2 film is formed as a protective film for the mesa structure 254. 2 A film may be formed, but nothing may be formed.
[0087] The refractive index of the first upper cladding layer 251 and the first side cladding layer 252 may be smaller than the refractive index of the first lower cladding layer 253. This allows light propagating through the core layer 220 to seep into the substrate 201 without seeping into the first upper cladding layer 251 and the second side cladding layer 212. In this way, the material forming the first upper cladding layer 251 and the first side cladding layer 252 may be different from the material forming the first lower cladding layer 253.
[0088] In this way, a spot size converter 200 capable of controlling the spot size in the vertical direction can be obtained, as shown in FIGS.
[0089] <Operation> Next, the operation of the spot size converter 200 will be described.
[0090] The spot size converter 200 is connected to an optical device such as a light source or a modulator. Here, it is assumed that the spot size converter 200 is connected to a semiconductor laser, which is the light source. The semiconductor laser has, for example, a buried heterostructure. A buried heterostructure is a structure in which the active layer (core layer) of the semiconductor laser is sandwiched between materials with different bandgaps from above and below, and the active layer of the semiconductor laser is sandwiched between layers with different bandgaps and current confinement functions from the side. The spot size converter 200 is connected to the semiconductor laser at the second end face 221s2. Light propagates from the semiconductor laser. The light is incident on the second core layer 241. The second core layer 241 has a buried heterostructure, similar to that of a semiconductor laser. Therefore, the light propagating from the semiconductor laser propagates into the second core layer 241 with minimal change in propagation mode. As a result, the light propagates into the second core layer 241 with low loss. The second core layer 241 is surrounded by the second upper cladding layer 213, the second side cladding layer 212, and the second lower cladding layer 211 (corresponding to the first core layer 221), which have a refractive index n1b lower than the refractive index n2b of the second core layer 241. Therefore, light is confined in the second core layer 241 in the first region 281.
[0091] Within the second core layer 241, the light reaches the second region 282. Within the second region 282, the width of the second core layer 241 in the third direction Z gradually decreases toward the first end face 221s1. Therefore, as the light propagating within the second core layer 241 approaches the first end face 221s1, the second core layer 241 is no longer able to confine the light. The light gradually seeps out from the second core layer 241 into the first core layer 221. When the width of the second core layer 241 in the third direction Z becomes sufficiently small, all of the light transfers from the second core layer 241 to the first core layer 221.
[0092] Light propagates through the first core layer 221 along the second direction Y. The light spreads in the direction in which the high refractive index region 231 is arranged. In particular, since the high refractive index region 231 is arranged on the substrate 201 side, the light spreads in the vertical direction (first direction X shown in FIG. 23 ). The light is emitted from the first end face 221s1. In this way, the light is emitted to the outside of the semiconductor device including the spot size converter 200.
[0093] <Operation and Effect> In the spot size converter 200, the core layer 220 includes the second core layer 241. The refractive index n2b of the second core layer 241 is higher than the refractive index n1b of the first core layer 221. In this way, light propagates through the second core layer 241 with low loss and without changing its propagation mode.
[0094] In the spot size converter 200, the high refractive index region 231 is disposed at a position closer to the substrate 201 in the first direction X than the second core layer 241. In this way, the light leaking out from the second core layer 241 spreads in the vertical direction (first direction X).
[0095] In the spot size converter 200, the core layer 220 has a first end face 221s1 and a second end face 221s2. The direction when viewing the first end face 221s1 from the second end face 221s2 is defined as a second direction Y. A portion of the second core layer 241 is disposed in a region in the second direction Y in which the high refractive index region 231 is disposed. The second core layer 241 includes a first core region 241a and a second core region 241b. In the second direction Y, the second core region 241b is farther from the second end face 221s2 than the first core region 241a. The width of the second core region 241b in a direction perpendicular to the second direction Y is smaller than the width of the first core region 241a.
[0096] In this way, as the light propagating through the second core layer 241 approaches the first end face 221s1, the second core layer 241 is no longer able to confine the light. The light can gradually seep out from the second core layer 241 into the first core layer 221. When the width of the second core layer 241 in the third direction Z becomes sufficiently small, all of the light can transfer from the second core layer 241 to the first core layer 221.
[0097] In the spot size converter 200, the refractive index of the first core layer 221 is defined as n1b. The refractive index of the second core layer 241 is defined as n2b. The refractive index of the high refractive index region 231 is defined as n3b. The refractive index of the cladding layer 250 is defined as n4b. The spot size converter 200 satisfies the relationship n2b > n3b > n1b > n4b. In this way, light can be efficiently propagated from the second core layer 241 to the first core layer 221.
[0098] FIG. 54 is a perspective view of a spot size converter 400 according to Comparative Example 2. FIG. 54 corresponds to FIG. 23 . The spot size converter 400 shown in FIG. 54 basically has the same configuration as the spot size converter 200 shown in FIGS. 23 to 26 , but differs in that the core layer 220 does not include the high refractive index region 231. FIG. 55 is a distribution diagram showing the light intensity in the vertical direction at the first end face 221s1. FIG. 55 corresponds to FIG. 22 . In FIG. 55 , the solid line indicates the light intensity distribution in Example 2. Example 2 basically has the same configuration as the spot size converter 200 according to the second embodiment. In FIG. 55 , the dotted line indicates the light intensity distribution in Comparative Example 2. In FIG. 55 , the horizontal axis indicates the height of the core layer in the vertical direction, specifically the distance from the first lower cladding layer 253 (unit: μm). In FIG. 55 , the vertical axis indicates the relative light intensity in the vertical direction (unit: −). In addition, the horizontal axis of Fig. 55 uses the plane where the first lower cladding layer 253 is connected to the first core layer 221 as the reference (=0 µm). The direction in which the first core layer 221 is located as viewed from the first lower cladding layer 253 is the positive direction of the horizontal axis. On the other hand, the direction in which the substrate 201 is located as viewed from the first lower cladding layer 253 is the negative direction of the horizontal axis. The distribution diagram shown in Fig. 55 is normalized by the maximum value of the light intensity in the first direction X (vertical direction).
[0099] 55, the half width in Comparative Example 2 is 2.67 μm. The half width in Example 2 is 3.37 μm. In other words, the half width in Example 2 is larger than the half width in Comparative Example 2. From the above results, it can be seen that the spot size is increased by including the high refractive index region 231 in the core layer 220.
[0100] The embodiments disclosed herein should be considered to be illustrative in all respects and not restrictive. Unless there is a contradiction, at least two of the embodiments disclosed herein may be combined. The basic scope of the present disclosure is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims.
[0101] 100, 200, 300, 400 Spot size converter, 101, 201 Substrate, 110, 250 Cladding layer, 111, 253 First lower cladding layer, 112, 252 First side cladding layer, 112a Protrusion, 113, 251 First upper cladding layer, 120, 220 Core layer, 121, 221 First core layer, 121s2, 221s2 Second end surface, 121s1, 221s1 First end surface, 121s3, 221s3 Side surface, 131, 231 High refractive index region, 131a, 231a First high refractive index region, 131b, 231b Second high refractive index region, 131t, 231t, 241t Tip portion, 141, 261 First processing mask, 142, 262 Second processing mask, 151, 254 Mesa structure, 211 Second lower cladding layer, 212 Second side cladding layer, 213 Second upper cladding layer, 241 Second core layer, 241a First core region, 241b Second core region, 263 Third processing mask, 281 First region, 282 Second region, 283 Boundary, X First direction, Y Second direction, Z Third direction, n1a, n1b, n2a, n2b, n3b, n3a, n4b Refractive index, p1 Point.
Claims
1. A spot size converter comprising: a core layer; and a clad layer surrounding the core layer, the core layer including a first core layer, the refractive index of the clad layer being lower than the refractive index of the first core layer, and the core layer including a high refractive index region having a refractive index higher than the refractive index of the first core layer.
2. A spot size converter as described in claim 1, further comprising a substrate, the substrate being connected to the cladding layer, and when a direction in which the core layer is viewed from the substrate is defined as a first direction, the high refractive index region is positioned on the substrate side relative to the center of the thickness of the core layer in the first direction.
3. The spot size converter of claim 2, wherein the core layer includes a second core layer, and the refractive index of the second core layer is higher than the refractive index of the first core layer.
4. The spot size converter according to claim 3, wherein the high refractive index region is disposed at a position closer to the substrate side than the second core layer in the first direction.
5. A spot size converter as claimed in claim 3 or 4, wherein the core layer has a first end face and a second end face, and when a direction in which the first end face is viewed from the second end face is defined as a second direction, a part of the second core layer is arranged in a region in the second direction in which the high refractive index region is arranged, the second core layer includes a first core region and a second core region, the second core region is farther from the second end face than the first core region in the second direction, and a width of the second core region in a direction perpendicular to the second direction is smaller than a width of the first core region.
6. A spot size converter described in any one of claims 3 to 5, wherein the refractive index of the first core layer is n1b, the refractive index of the second core layer is n2b, the refractive index of the high refractive index region is n3b, and the refractive index of the cladding layer is n4b, satisfying the relationship n2b > n3b > n1b > n4b.
7. The spot size converter of claim 5, wherein the high refractive index region includes a first high refractive index region and a second high refractive index region, the first high refractive index region is farther from the second end face in the second direction than the second high refractive index region, and a width of the second high refractive index region in a direction perpendicular to the second direction is smaller than a width of the first high refractive index region.
Citation Information
Patent Citations
Optical coupler and its manufacturing method
JP2003207684A
Spot-size converter element, its manufacture method and waveguide-embedding optical circuit using spot-size converter element
JP2004258610A
Spot size converter, manufacturing method thereof and optical integrated circuit device
JP2014191301A
Optical waveguide coupling structure and manufacturing method of optical waveguide coupling structure