Development method and substrate processing system
The developing method employing a cleaning solution with 0.25 to 50% pure water and a substrate processing system effectively reduces residues on metal-containing coating films, addressing the issue of pattern defects by selectively dissolving intermediate polymers and maintaining the resist pattern's integrity.
Patent Information
- Application Number
- PCT/JP2024/017599
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-25
- Filing Date
- 2024-05-13
- Publication Date
- 2024-11-28
AI Technical Summary
During the development of metal-containing coating films in semiconductor manufacturing, residues such as resist scum are left on the substrate due to intermediate polymers formed near the boundaries of exposed and unexposed areas, leading to pattern defects, and existing methods are inadequate in fully removing these residues without dissolving the pattern.
A developing method that uses a developer with an organic solvent and a subsequent cleaning solution containing 0.25 to 50% pure water, which has a lower solubility than the developer, to dissolve and remove residues without affecting the pattern, utilizing a substrate processing system with specific devices for developer and cleaning liquid supply, ultraviolet irradiation, and heat treatment.
Effectively reduces the amount of residue on the substrate surface, maintaining the integrity of the resist pattern by selectively dissolving intermediate polymers without dissolving the pattern, thereby improving the quality of the developed substrate.
Smart Images

Figure JP2024017599_28112024_PF_FP_ABST
Abstract
Description
Development method and substrate processing system
[0001] The present disclosure relates to a development method and a substrate processing system.
[0002] Patent Document 1 discloses a developing method including the steps of supplying a developer containing an organic solvent to a substrate having a metal-containing coating film exposed to light in a predetermined pattern, and supplying a cleaning liquid containing an organic solvent to the substrate to which the developer has been supplied. In the cleaning liquid supplying step of this developing method, a cleaning liquid that has a lower solubility for the metal-containing coating film than the developer is used.
[0003] Japanese Patent Application Publication No. 2022-096081
[0004] The technology according to the present disclosure reduces the amount of residues on the substrate surface that are generated during development of a metal-containing coating film.
[0005] One aspect of the present disclosure is a development method for developing a substrate, the method comprising the steps of: supplying a developer containing an organic solvent to the substrate on which a metal-containing coating film has been exposed to a predetermined pattern; and supplying a first cleaning liquid containing an organic solvent to the substrate to which the developer has been supplied, the first cleaning liquid having a lower solubility for the metal-containing coating film than the developer, and containing 0.25 to 50 volume % pure water.
[0006] According to the present disclosure, it is possible to reduce the amount of residues on the substrate surface that are generated during the development process of a metal-containing coating film.
[0007] FIG. 1 is a plan view showing an outline of the internal configuration of a substrate processing system according to an embodiment. FIG. 2 is a view showing an outline of the internal configuration of the front side of the substrate processing system of FIG. 1. FIG. 3 is a view showing an outline of the internal configuration of the back side of the substrate processing system of FIG. 1. FIG. 4 is a longitudinal sectional view showing an outline of the configuration of a developer supply device according to an embodiment. FIG. 5 is a longitudinal sectional view showing an outline of the configuration of a cleaning liquid supply device according to an embodiment. FIG. 6 is a longitudinal sectional view showing an outline of the configuration of a heat treatment device according to an embodiment. FIG. 7 is a longitudinal sectional view showing an outline of the configuration of an ultraviolet irradiation device according to an embodiment. FIG. 8 is an explanatory view showing the state of a resist film on a wafer in each step of a developing method according to an embodiment. FIG. 9 is an explanatory view for explaining exposed and unexposed portions of a metal-containing resist film.
[0008] In the manufacturing process of semiconductor devices and the like, there is a photolithography process in which a resist film is formed by applying a resist to a semiconductor wafer (hereinafter referred to as "wafer"), exposing the resist film, and developing the exposed resist film to form a resist pattern. In this photolithography process, it is known that a metal-containing resist film is formed on the wafer using a resist solution containing a metal in order to form a finer resist pattern.
[0009] When a metal-containing resist film is exposed to light, a polymerization reaction between metal atoms and oxygen atoms proceeds in the exposed areas, while no such polymerization reaction occurs in the unexposed areas. Since the polymerized areas are hardly soluble in a developer, during the development process after exposure, only the unexposed areas are dissolved by supplying a developer to the wafer, and a predetermined pattern is formed on the wafer.
[0010] Although the unexposed area is basically a region where no polymerization reaction occurs, in the region near the boundary with the exposed area, an intermediate polymer that is hardly soluble in a developer may be formed due to low exposure. In the unexposed area where such an intermediate polymer has formed, when a developer is supplied during development, part of the intermediate polymer does not dissolve in the developer, and a residue such as resist scum remains on the wafer.
[0011] Since residues on a wafer cause pattern defects, it is desirable to reduce the amount of residues. In the development method described in Patent Document 1, an attempt is made to dissolve the residues without dissolving the pattern by supplying a cleaning solution to the wafer that has a lower solubility for the metal-containing resist film than the developer, but there is room for improvement in terms of reducing the amount of residues.
[0012] The technology according to the present disclosure reduces the amount of residues on the substrate surface that are generated during development of a metal-containing coating film.
[0013] Hereinafter, a developing method according to the present embodiment and a substrate processing system in which the developing method is performed will be described with reference to the drawings. In this specification and the drawings, elements having substantially the same functional configurations are designated by the same reference numerals, and redundant description will be omitted.
[0014] (Substrate Processing System) First, a substrate processing system in which a developing method described later is performed will be described. Fig. 1 is a plan view showing an outline of the internal configuration of the substrate processing system according to this embodiment. Figs. 2 and 3 are diagrams showing an outline of the internal configuration on the front side and rear side, respectively, of the substrate processing system shown in Fig. 1.
[0015] 1 to 3, the substrate processing system 1 includes a cassette station 10 into which a cassette C containing a plurality of wafers W as substrates is loaded and unloaded, and a processing station 11 equipped with a plurality of various processing devices that perform predetermined processing on the wafers W. The substrate processing system 1 is configured to integrally connect the cassette station 10, the processing station 11, and an interface station 13 that transfers the wafers W between the processing station 11 and an exposure device 12 adjacent to the processing station 11.
[0016] The cassette station 10 is provided with a cassette placement table 20. The cassette placement table 20 is provided with a plurality of cassette placement plates 21 on which the cassettes C are placed when the cassettes C are transported in and out of the substrate processing system 1.
[0017] The cassette station 10 is provided with a wafer transfer device 23 that is movable on a transfer path 22 extending in the X direction in Fig. 1. The wafer transfer device 23 is also movable in the vertical direction and around the vertical axis (the θ direction), and can transfer wafers W between the cassettes C on each cassette mounting plate 21 and a transfer device in the third block G3 of the processing station 11, which will be described later.
[0018] The processing station 11 is provided with multiple blocks, for example, four blocks G1, G2, G3, and G4, each equipped with various devices. For example, a first block G1 is provided on the front side of the processing station 11 (the negative side in the X direction in FIG. 1 ), and a second block G2 is provided on the rear side of the processing station 11 (the positive side in the X direction in FIG. 1 ). A third block G3 is provided on the cassette station 10 side of the processing station 11 (the negative side in the Y direction in FIG. 1 ), and a fourth block G4 is provided on the interface station 13 side of the processing station 11 (the positive side in the Y direction in FIG. 1 ).
[0019] 2, the first block G1 is provided with liquid processing devices such as a developer supply device 30, a resist coating device 31, and a cleaning liquid supply device 32. The liquid processing devices 30 to 32 are arranged side by side in the horizontal direction at different heights.
[0020] The developer supplying device 30 supplies a developer to the wafer W to perform a development process. The resist coating device 31 supplies a resist solution containing a metal (e.g., Sn) as a metal-containing coating solution to the wafer, and forms a metal-containing resist film on the wafer as a metal-containing coating film. The resist coating device 31 ejects the resist solution onto the wafer W from a nozzle and rotates the wafer W to spread the resist solution over the surface of the wafer W. The cleaning solution supplying device 32 supplies a first cleaning solution containing an organic solvent to the wafer to clean the wafer. The number and arrangement of the developer supplying devices 30, resist coating devices 31, and cleaning solution supplying devices 32 can be selected as desired.
[0021] In these developing solution supplying device 30, resist coating device 31, and cleaning solution supplying device 32, for example, spin coating using a predetermined processing solution or coating solution is performed on the wafer W. In spin coating, for example, the processing solution or coating solution is ejected onto the wafer W from a nozzle, and the wafer W is rotated to spread the processing solution or coating solution over the surface of the wafer W.
[0022] 3, the second block G2 is provided with a heat treatment device 40, a peripheral exposure device 41, and an ultraviolet irradiation device 42, which are arranged vertically and horizontally. The heat treatment device 40 performs heat treatment such as heating and cooling of the wafer W. The peripheral exposure device 41 exposes the peripheral portion of the wafer W to light. The ultraviolet irradiation device 42 irradiates the wafer W with ultraviolet light. The number and arrangement of the heat treatment devices 40, peripheral exposure devices 41, and ultraviolet irradiation devices 42 can be selected arbitrarily.
[0023] In the third block G3, a plurality of transfer devices 50, 51, 52, 53, 54, 55, and 56 are provided in this order from the bottom up. In addition, in the fourth block G4, a plurality of transfer devices 60, 61, and 62 are provided in this order from the bottom up.
[0024] 1 and 3, the area surrounded by the first block G1 to the fourth block G4 forms a wafer transfer area D. In the wafer transfer area D, a wafer transfer device 70 is disposed.
[0025] Each wafer transfer device 70 has a transfer arm 70a that can move freely in, for example, the X direction, Y direction, θ direction, and up and down direction. A plurality of wafer transfer devices 70 are arranged one above the other, and each wafer transfer device 70 moves within the wafer transfer region D and can transfer the wafer W to a predetermined device at approximately the same height in each of blocks G1 to G4, for example.
[0026] In addition, the wafer transfer region D is provided with a shuttle transfer device 80 that transfers the wafer W linearly between the third block G3 and the fourth block G4.
[0027] The shuttle transfer device 80 is configured to be linearly movable, for example, in the Y direction in Fig. 3. By moving in the Y direction while supporting a wafer, the shuttle transfer device 80 can transfer the wafer between the delivery device 52 in the third block G3 and the delivery device 62 in the fourth block G4.
[0028] 1, a wafer transfer device 90 is provided adjacent to the third block G3 on the positive side in the X direction. The wafer transfer device 90 has a transfer arm 90a that is movable in, for example, the X direction, the θ direction, and the up-and-down direction. The wafer transfer device 90 moves up and down while supporting a wafer W, and can transfer the wafer W to each of the delivery devices 50 to 56 in the third block G3.
[0029] The interface station 13 is provided with a wafer transfer device 100 and a transfer device 101. The wafer transfer device 100 has a transfer arm 100a that is movable, for example, in the Y direction, the θ direction, and the up and down direction. The wafer transfer device 100 supports a wafer W on, for example, the transfer arm 100a, and transfers the wafer W between each of the transfer devices 60 to 62 in the fourth block G4, the transfer device 101 in the interface station 13, and the exposure device 12.
[0030] The substrate processing system 1 described above is provided with at least one controller 200, as shown in FIG. 1 . The controller 200 processes computer-executable instructions that cause the substrate processing system 1 to perform the various processes described herein. The controller 200 may be configured to control each element of the substrate processing system 1 to perform the various processes described herein. In one embodiment, part or all of the controller 200 may be included in the substrate processing system 1. The controller 200 may include a processor, a storage unit, and a communication interface. The controller 200 is implemented, for example, by a computer. The processor may be configured to read from the storage unit a program that provides logic or routines that enable the various control operations to be performed, and to execute the read program to perform the various control operations. This program may be stored in the storage unit in advance or may be acquired via a medium when needed. The acquired program is stored in the storage unit and read from the storage unit by the processor for execution. The medium may be a computer-readable storage medium H or a communication line connected to the communication interface. The storage medium H may be temporary or non-temporary. The processing unit may be a CPU (Central Processing Unit) or one or more circuits. The storage unit may include a RAM (Random Access Memory), a ROM (Read Only Memory), a HDD (Hard Disk Drive), an SSD (Solid State Drive), or a combination thereof. The communication interface may communicate with the substrate processing system 1 via a communication line such as a LAN (Local Area Network).
[0031] The above has described the outline of the configuration of the substrate processing system 1. Next, the outline of the configuration of each of the devices, namely, the developing solution supply device 30, the cleaning solution supply device 32, the heat treatment device 40, and the ultraviolet irradiation device 42, provided in the substrate processing system 1 according to this embodiment will be described in order.
[0032] 4 is a longitudinal cross-sectional view showing an outline of the configuration of a developer supplying apparatus 30 according to this embodiment. The developer supplying apparatus 30 has a processing vessel 110, and a loading / unloading port (not shown) for a wafer W serving as a substrate is formed on the side of the processing vessel 110. The processing vessel 110 contains a spin chuck 111 serving as a substrate holder. The spin chuck 111 holds the wafer W horizontally and is connected to a rotating unit 112 that can be raised and lowered. The rotating unit 112 is connected to a rotation driving unit 113 formed by a motor or the like, and the wafer W held by the spin chuck 111 is rotated by driving the rotation driving unit 113.
[0033] A filter device 114 is provided on the ceiling of the processing vessel 110. Air purified by the filter device 114 is supplied into the processing vessel 110 via an air supply unit 115, and a downflow is formed within the processing vessel 110.
[0034] A cup 116 is provided around the spin chuck 111 to receive and recover liquid that splashes or drops from the wafer W. A drain pipe 117 and an exhaust pipe 118 are provided at the bottom of the cup 116. The exhaust pipe 118 is connected to an exhaust device 119 such as an exhaust pump.
[0035] A developer nozzle 120 is disposed in the processing vessel 110 as a developer supply unit that discharges a developer toward the surface of the wafer W. The developer nozzle 120 is attached to a nozzle support 121, such as an arm. The nozzle support 121 can be raised and lowered by a drive mechanism (not shown) along the reciprocating arrow A indicated by a dashed line in the figure, and can also be moved horizontally along the reciprocating arrow B indicated by a dashed line. The developer nozzle 120 is connected to a developer supply source 123 via a supply pipe 122.
[0036] Also disposed within the processing vessel 110 is a first cleaning liquid nozzle 130 serving as a first cleaning liquid supply unit that discharges a first cleaning liquid toward the surface of the wafer W. The first cleaning liquid nozzle 130 is mounted on a nozzle support 131, such as an arm. The nozzle support 131 can be raised and lowered by a drive mechanism (not shown) along the reciprocating arrow C indicated by the dashed line in the figure, and can also be moved horizontally along the reciprocating arrow D indicated by the dashed line. The first cleaning liquid nozzle 130 is connected to a supply source 133 of the first cleaning liquid via a supply pipe 132.
[0037] According to the developer supplying device 30 of this embodiment, the developer or first cleaning liquid is supplied to the center of the wafer W while rotating the wafer W, so that the developer or first cleaning liquid is spread over the entire wafer W.
[0038] The method for supplying the developer or the first cleaning liquid is not particularly limited as long as it is possible to supply the developer or the first cleaning liquid to the surface of the wafer W. In other words, the configuration of the developer supply device 30 is appropriately changed depending on the development method to be adopted, such as puddle development or spray development. Also, for example, a first cleaning liquid nozzle 130 may be provided in the cleaning liquid supply device 32 described below, and the wafer W may be transported to the cleaning liquid supply device 32 after the development process to supply the first cleaning liquid to the wafer W.
[0039] <Cleaning Liquid Supply Apparatus> Fig. 5 is a longitudinal cross-sectional view showing an outline of the configuration of the cleaning liquid supply apparatus 32 according to this embodiment. The cleaning liquid supply apparatus 32 has a housing 140, and a loading / unloading port (not shown) for the wafer W is formed on a side surface of the housing 140. A spin chuck 141 serving as a substrate holder is provided within the housing 140. The spin chuck 141 holds the wafer W horizontally and is connected to a rotating unit 142 that can be raised and lowered. The rotating unit 142 is connected to a rotation drive unit 143 formed by a motor or the like, and the wafer W held by the spin chuck 141 is rotated by driving the rotation drive unit 143.
[0040] A filter device 144 is provided on the ceiling of the housing 140. Air purified by the filter device 144 is supplied into the housing 140 via an air supply section 145, and a downflow is formed within the housing 140.
[0041] A cup 146 is provided around the spin chuck 141 to receive and recover liquid scattered or dropped from the wafer W. A drain pipe 147 and an exhaust pipe 148 are provided at the bottom of the cup 146. The exhaust pipe 148 is connected to an exhaust device 149 such as an exhaust pump.
[0042] A second cleaning liquid nozzle 150 serving as a second cleaning liquid supply unit that discharges the second cleaning liquid toward the surface of the wafer W is disposed within the housing 140. The second cleaning liquid nozzle 150 is attached to a nozzle support unit 151, such as an arm. The nozzle support unit 151 can be raised and lowered by a drive mechanism (not shown) along the reciprocating arrow E indicated by the dashed line in the figure, and can also be moved horizontally along the reciprocating arrow F indicated by the dashed line. The second cleaning liquid nozzle 150 is connected to a supply source 153 of the second cleaning liquid via a supply pipe 152.
[0043] According to the cleaning liquid supply device 32 of this embodiment, the second cleaning liquid is supplied to the center of the wafer W while rotating the wafer W, thereby spreading the second cleaning liquid over the entire wafer W. The method of supplying the cleaning liquid is not particularly limited as long as it is possible to supply the second cleaning liquid to the surface of the wafer W. In other words, the configuration of the cleaning liquid supply device 32 is not limited to the configuration described in this embodiment.
[0044] <Heat Treatment Apparatus> Fig. 6 is a longitudinal cross-sectional view showing an outline of the configuration of a heat treatment apparatus 40 according to this embodiment. The heat treatment apparatus 40 has a processing vessel 160, and a loading / unloading port (not shown) for a wafer W is formed on a side surface of the processing vessel 160. A mounting table 161 serving as a substrate holder for mounting the wafer W is provided within the processing vessel 160. The mounting table 161 incorporates a heater 162 serving as a heating unit for heating the wafer W. The mounting table 161 also has a plurality of through holes 163 formed therein, and lift pins 164a that move up and down within these through holes 163 are fixed to lift pin supports 164. The lift pin supports 164 are raised and lowered by a lift mechanism 165.
[0045] The heat treatment apparatus 40 is not limited to the configuration described in this embodiment, but may have any configuration capable of heating the wafer W.
[0046] <Ultraviolet Irradiation Apparatus> Fig. 7 is a longitudinal cross-sectional view showing an outline of the configuration of an ultraviolet irradiation apparatus 42 according to this embodiment. The ultraviolet irradiation apparatus 42 has a housing 170, and a loading / unloading port (not shown) for a wafer W is formed on a side of the housing 170. A mounting table 171 is provided within the housing 170 as a substrate holder for placing the wafer W thereon. The mounting table 171 has through holes 172 formed in multiple locations, and lift pins 173a that move up and down within these through holes 172 are fixed to lift pin supports 173. The lift pin supports 173 are raised and lowered by a lift mechanism 174.
[0047] Above the mounting table 171, a UV lamp 175 is disposed as an ultraviolet irradiator that irradiates ultraviolet rays onto the surface of the wafer W mounted on the mounting table 171. The UV lamp 175 radially irradiates ultraviolet rays having a wavelength of 190 to 400 nm. Note that, although a KrF exposure device that irradiates ultraviolet rays having a wavelength of 248 nm is used as the ultraviolet irradiator 42, the ultraviolet irradiator 42 is not particularly limited as long as it is configured to irradiate ultraviolet rays having a wavelength of 190 to 400 nm.
[0048] The substrate processing system 1 according to this embodiment has been described above.
[0049] (Developing Method) Next, a description will be given of a developing method for a wafer W using the substrate processing system 1. Fig. 8 is an explanatory diagram showing the state of a resist film on a wafer in each step of the developing method according to this embodiment.
[0050] First, as shown in FIG. 8A, when a wafer W is subjected to a development process, a metal-containing resist film R is formed on the surface of the wafer W by a resist coating device.
[0051] Thereafter, the wafer W is subjected to edge exposure processing by the edge exposure device 41, exposure processing by the exposure device 12, and PEB processing by the heat treatment device 40. As a result, as shown in FIG. 8B, the resist film formed on the surface of the wafer W becomes a mixture of unexposed resist film (hereinafter referred to as "unexposed resist film R1") and exposed resist film (hereinafter referred to as "exposed resist film R2"), and is exposed to a predetermined pattern. The predetermined pattern is set appropriately according to the specifications of the semiconductor product.
[0052] 9, due to the characteristics of the exposure machine, exposure is performed under conditions in which the exposure intensity changes periodically. Therefore, in the central region of the unexposed resist film R1, which is sufficiently far from the boundary with the exposed resist film R2, the exposure intensity is low enough to prevent the polymerization reaction from proceeding, but the exposure intensity near the boundary with the exposed resist film R2 is higher than that in the central region of the unexposed resist film R1.
[0053] Therefore, no polymerization reaction occurs in the central region of the unexposed resist film R1, but a slight polymerization reaction progresses in the unexposed resist film R1 near the boundary with the exposed resist film R2, resulting in the formation of an intermediate polymer. In the following explanation, the region of the unexposed resist film R1 where the intermediate polymer is formed will be referred to as "region A1."
[0054] On the other hand, since the exposure intensity changes periodically as described above, the exposed resist film R2 is exposed to an exposure intensity at which the polymerization reaction proceeds sufficiently in the central region thereof, which is sufficiently distant from the boundary with the unexposed resist film R1. However, the exposure intensity in the vicinity of the boundary with the unexposed resist film R2 is lower than that in the central region of the exposed resist film R2.
[0055] As a result, the polymerization reaction proceeds sufficiently in the central region of the exposed resist film R2, but is insufficient near the boundary between the exposed resist film R2 and the unexposed resist film R1, resulting in the formation of an intermediate polymer. In the following explanation, the region of the exposed resist film R2 where the intermediate polymer is formed will be referred to as "region A2."
[0056] 8(c), the wafer W exposed to a predetermined pattern is transferred to a developer supplying device 30, where a developer containing an organic solvent is supplied to the surface of the wafer W. As a result, the unexposed resist film R1 formed on the surface of the wafer W is dissolved.
[0057] The type of organic solvent contained in the developer is not particularly limited as long as it dissolves the unexposed resist film R1 but does not dissolve the exposed resist film R2. The developer may also be a mixture of two or more organic solvents, and for example, a mixture of PGMEA (propylene glycol monomethyl ether acetate) and acetic acid may be used as the developer.
[0058] Furthermore, when the developer contains pure water, the content of pure water in the developer is preferably less than 0.25%. When the content of pure water in the developer is less than 0.25%, it is possible to prevent the resist pattern from becoming thinner. When the content of pure water in the developer is 0.25% or more, the solubility of the exposed resist film R2 in the developer increases, which may result in the resist pattern becoming thinner, and measures such as increasing the exposure intensity of the exposure machine in the exposure process before development may be necessary.
[0059] As described above, the unexposed resist film R1 includes a region A1 where an intermediate polymer is formed, and the intermediate polymer in this region A1 is less soluble in a developer than the central region of the unexposed resist film R1. Therefore, in the step of supplying a developer to the wafer W shown in Figure 8(c), some of the intermediate polymer in region A1 may not dissolve in the developer, and residues such as resist scum may remain on the surface of the wafer W.
[0060] In order to remove the residue, in the next step, a first cleaning liquid is supplied to the surface of the wafer W. The first cleaning liquid supplied here is a processing liquid containing an organic solvent and 0.25 to 50 volume % of pure water, and having a lower solubility for the metal-containing resist film than the developer in order to avoid dissolution of the resist pattern.
[0061] "Solubility of a metal-containing resist film" is an index showing the ease with which a metal-containing resist film dissolves in a processing liquid such as a developer or a first cleaning liquid. For example, when evaluating the solubility of two processing liquids, the two processing liquids are each supplied in equal amounts to a metal-containing resist film of the same composition, and the amount of dissolution of the resist film per unit time (amount of volume reduction) is compared. Then, of the two processing liquids, the processing liquid that dissolves the lesser amount of resist film per unit time is the processing liquid that dissolves the metal-containing resist film less than the other processing liquid.
[0062] The developer has a solubility that does not dissolve the exposed resist film R2. However, if a processing liquid with a higher solubility than the developer is used as the first cleaning liquid, the exposed resist film R2 may dissolve, possibly causing the pattern shape to collapse.
[0063] Furthermore, in the aforementioned region A2 present in the exposed resist film R2, the polymerization reaction has not progressed as much as in the central region of the exposed resist film R2. Therefore, region A2 is more easily dissolved in an organic solvent than the central region of the exposed resist film R2. Therefore, if the solubility of the metal-containing resist film in the first cleaning solution is the same as that of the developer, there is a concern that the exposed resist film R2 in region A2 will be slightly dissolved, resulting in the collapse of the pattern shape.
[0064] Therefore, by using a processing liquid having a lower solubility for the metal-containing resist film than the developer as the first cleaning liquid, it is possible to dissolve the residues remaining on the surface of the wafer W without dissolving the exposed resist film R2, as shown in Fig. 8(d) . In other words, it is possible to reduce the amount of residues on the surface of the wafer W without destroying the pattern.
[0065] The type of organic solvent contained in the first cleaning liquid is not particularly limited as long as it is a processing liquid that has lower solubility in the metal-containing resist film than the developer. For example, when the organic solvent contained in the developer is 2-heptanone, the organic solvent contained in the first cleaning liquid may be MIBC (methyl isobutyl carbinol) or PGMEA (propylene glycol monomethyl ether acetate), which has lower solubility in the metal-containing resist film than 2-heptanone.
[0066] Furthermore, when the organic solvent contained in the developer is a mixed solution of PGMEA (propylene glycol monomethyl ether acetate) and acetic acid, the organic solvent contained in the first cleaning liquid may be, for example, one or a mixed solution of two or more selected from the group consisting of 2-heptanone, IPA (isopropyl alcohol), PGME (propylene glycol monomethyl ether), PGMEA (propylene glycol monomethyl ether acetate), nBA (n-butyl acetate), cyclohexanone, MIBC (methyl isobutyl carbinol), and ethyl lactate.
[0067] The pure water contained in the first cleaning liquid is a highly polar solvent, and therefore easily dissolves residues, which are highly polar substances. Therefore, by supplying the first cleaning liquid containing 0.25 to 50 volume % pure water to the wafer W, the amount of residues on the surface of the wafer W can be reduced compared to when a cleaning liquid containing no pure water is supplied.
[0068] If the pure water content in the first cleaning solution is less than 0.25% by volume, the first cleaning solution will not be able to dissolve the residues sufficiently.
[0069] On the other hand, when the pure water content in the first cleaning liquid is 50% by volume or more, the properties of the pure water become dominant in the wettability characteristics of the first cleaning liquid, and the contact angle of the first cleaning liquid with the wafer W and the exposed resist film R2 increases. As a result, droplets are likely to form on the surface of the wafer W and the surface of the exposed resist film R2 after the first cleaning liquid is supplied, and liquid splashes occur as the wafer W rotates, which makes it easier for the inside of the module to be contaminated.
[0070] Furthermore, on the surface of the wafer W, there are regions with different wettability due to the presence of exposed and unexposed regions, and when the contact angle of the first cleaning liquid increases because the first cleaning liquid contains 50% by volume or more of pure water, the difference in contact angle increases at the regions with different wettability as described above. Because the liquid in the region with a small contact angle has difficulty flowing to the region with a relatively large contact angle, when the pure water content in the first cleaning liquid is 50% by volume or more, the first cleaning liquid is difficult to remove even when the wafer W is rotated.
[0071] For the above reasons, the content of pure water in the first cleaning solution is limited to 0.25 to 50% by volume.
[0072] Among organic solvents that can be used as the first cleaning liquid, for example, IPA and PGME are highly hydrophilic and easily mix with pure water, whereas organic solvents such as 2-heptanone, PGMEA, and nBA are less hydrophilic than IPA and PGME and are easily separated from pure water.
[0073] For this reason, when an organic solvent with low hydrophilicity such as 2-heptanone, PGMEA, or nBA is used as the organic solvent contained in the first cleaning liquid, it is preferable to mix in an organic solvent with high hydrophilicity such as IPA or PGME. This allows the highly hydrophilic organic solvent such as IPA or PGME to promote mixing of the low hydrophilic organic solvent such as 2-heptanone, PGMEA, or nBA with pure water, and makes it possible to configure a first cleaning liquid that is sufficiently mixed with pure water even when an organic solvent with low hydrophilicity is used.
[0074] The developing method according to this embodiment has been described above. According to this developing method, by carrying out the step of supplying a first cleaning liquid to the wafer W after supplying a developer to the wafer W, it is possible to form a predetermined resist pattern in a state in which the amount of residue remaining on the surface of the wafer W that is not dissolved in the developer is reduced.
[0075] (Cleaning with Second Cleaning Liquid) In order to further reduce the amount of residue remaining on the surface of the wafer W, the following steps are carried out as necessary after the step of supplying the first cleaning liquid to the wafer W.
[0076] First, the wafer W, which has been cleaned with a cleaning solution, is transferred to the ultraviolet irradiation device 42, where ultraviolet rays with a wavelength of 190 to 400 nm are irradiated onto the surface of the wafer W. In this process, for example, KrF exposure with a wavelength of 248 nm is performed. No mask is used during ultraviolet irradiation, and the entire wafer W is uniformly irradiated with ultraviolet rays. As a result, as shown in FIG. 8( e), the exposure reaction of the entire exposed resist film R2 progresses further, and the exposure reaction also progresses in a region A2 of the resist film R2 where the exposure reaction has relatively not progressed, similar to the other regions.
[0077] In addition, when the wavelength of the ultraviolet light is less than 190 nm, irradiation of the ultraviolet light causes a reaction in which the C—O bond of the resist film R2 is broken, but an exposure reaction of the resist film R2 does not occur. In addition, in this embodiment, irradiation of the ultraviolet light is performed by the ultraviolet irradiation device 42, but it may also be performed by, for example, the exposure device 12.
[0078] Next, the wafer W irradiated with ultraviolet light is transferred to the heat treatment device 40 and heated. As a result, as shown in FIG. 8( f), the polymerization reaction of the exposed resist film R2 is further accelerated, and the resist film R2 is hardened and transformed into a strong resist film R3.
[0079] In this embodiment, the wafer W is heated in the heat treatment device 40 after the ultraviolet irradiation, but the wafer W may be heated in the ultraviolet irradiation device if, for example, the ultraviolet irradiation device 42 has a heating mechanism for the wafer W. Furthermore, if the same module is capable of irradiating ultraviolet rays and heating the wafer W, the wafer W may be heated during ultraviolet irradiation or after ultraviolet irradiation.
[0080] Next, the heated wafer W is transferred to the cleaning liquid supply device 32, and a second cleaning liquid is supplied onto the surface of the wafer W. The second cleaning liquid contains an organic solvent, and as shown in FIG. 8( g), residues on the surface of the wafer W come into contact with the second cleaning liquid, dissolving the residues.
[0081] Since the resist film R3 hardened through ultraviolet irradiation and heat treatment is less soluble in organic solvents, a treatment liquid having a higher solubility for the resist film than the first cleaning liquid can be used as the second cleaning liquid, which dissolves the residues that were not sufficiently removed in the step of cleaning the wafer W with the first cleaning liquid shown in FIG.
[0082] The organic solvent contained in the second cleaning liquid is not particularly limited as long as it is a processing liquid that does not dissolve the cured resist film R3, and may be a processing liquid that is a mixture of two or more organic solvents. The organic solvent contained in the second cleaning liquid is, for example, an alkaline processing liquid containing TMAH (tetramethylammonium hydroxide) or a processing liquid containing an organic acid such as acetic acid, formic acid, or citric acid.
[0083] In this embodiment, the supply of the second cleaning liquid to the wafer W is performed by the cleaning liquid supply device 32, but if the developer supply device 30 has the function of supplying the second cleaning liquid, the supply of the second cleaning liquid may also be performed by the developer supply device 30.
[0084] The second cleaning liquid may be selected based on the difference in solubility due to the difference in polarity with the first cleaning liquid. For example, when the pure water concentration of the first cleaning liquid is low, a second cleaning liquid having a higher polarity than the first cleaning liquid may be used. By selecting the second cleaning liquid in this way, taking into account the difference in polarity with the first cleaning liquid, the solubility of the metal-containing resist film can be changed, thereby reducing the possibility of residue remaining on the surface of the wafer W.
[0085] After the wafer W has been cleaned with the second cleaning liquid, the wafer W is cleaned with pure water and dried, completing a series of development steps.
[0086] As described above, by irradiating the wafer W with ultraviolet light having a wavelength of 190 to 400 nm after supplying the developing solution, then heating the wafer W, and then supplying the second cleaning solution to the wafer W, it is possible to promote dissolution of residues on the wafer surface and further reduce the amount of residues.
[0087] In the embodiment described above, the organic solvent and pure water are mixed in advance in the supply source 133 shown in FIG. 4 , and the mixed liquid is supplied to the wafer W as the first cleaning liquid. However, the form of "supplying the first cleaning liquid containing the organic solvent and pure water to the wafer" in the present disclosure is not limited to the form shown in FIG. 4 .
[0088] For example, the "supply of a first cleaning liquid containing an organic solvent and pure water to a wafer" may be performed by adding pure water to a flow path (organic solvent flow path) from an organic solvent supply source to a nozzle outlet for discharging the organic solvent. In this case, for example, a pure water supply pipe (not shown) is connected to the organic solvent supply pipe, and pure water is supplied from the pure water supply pipe to mix the organic solvent and pure water to form the first cleaning liquid.
[0089] Furthermore, for example, the embodiment of "supplying a first cleaning liquid containing an organic solvent and pure water to a wafer" may be an embodiment in which an organic solvent is supplied to the surface of the wafer W, and then pure water is supplied to mix with the organic solvent remaining on the surface of the wafer W. In this embodiment, for example, an organic solvent nozzle for discharging the organic solvent and a pure water nozzle for discharging pure water are separately provided, and the organic solvent is discharged from the organic solvent nozzle onto the wafer W, and then pure water is discharged from the pure water nozzle toward the wafer W, thereby mixing the organic solvent and pure water on the surface of the wafer W. As another example, pure water may be sprayed toward the wafer W from a shower head having multiple openings above the wafer W, thereby mixing the pure water with the organic solvent remaining on the surface of the wafer W. In such an embodiment in which pure water is supplied to the organic solvent remaining on the surface of the wafer W, the first cleaning liquid containing the organic solvent and pure water is present on the surface of the wafer W, and therefore, it can be considered that "a first cleaning liquid containing an organic solvent and pure water is supplied to the wafer W." In other words, the embodiment described in this paragraph also falls within the technical scope of the present disclosure.
[0090] The first cleaning solution in the present disclosure contains 0.25 to 50 volume percent pure water. However, according to the inventors' investigations, depending on the type of organic solvent, the higher the pure water concentration, the more likely it is that the metal-containing resist film will be altered due to a chemical reaction between the organic solvent and the pure water. Therefore, the pure water concentration in the first cleaning solution is preferably, for example, 0.25 to 10 volume percent. This can reduce the possibility of deterioration of process performance or the occurrence of defects due to the alteration of the metal-containing resist film.
[0091] Furthermore, when pure water is supplied to the wafer W in a sprayed state, the amount of pure water supplied relative to the supply time can be made very small compared to when pure water is ejected from a nozzle, making it easier to prepare a first cleaning liquid with a pure water concentration of 0.25 to 10% by volume. In addition, supplying pure water in a sprayed state makes it possible to prepare a first cleaning liquid in a short period of time that does not have a biased distribution of pure water concentration on the surface of the wafer W. The phrase "preparing a first cleaning liquid on the surface of the wafer" described here corresponds to supplying a first cleaning liquid containing an organic solvent and pure water to the wafer, since it is possible to achieve a state in which the first cleaning liquid containing an organic solvent and pure water is present on the surface of the wafer W.
[0092] Furthermore, "supplying a first cleaning liquid containing an organic solvent and pure water to the wafer W" may also include supplying pure water only to a partial region of the wafer W, including the center, after supplying a developer to the wafer W and completing development. In this embodiment, the supply of pure water is performed simultaneously with the timing at which the liquid remaining on the surface of the wafer W begins to be discharged outward by increasing the rotation speed of the wafer W, or before the timing at which the rotation speed of the wafer W is increased. Alternatively, pure water may be supplied to the organic solvent remaining on the surface of the wafer W to prepare a first cleaning liquid, and then further pure water may be supplied to the partial region. The "partial region" referred to here refers to a region radially inward from the periphery of the liquid remaining on the surface of the wafer W. In other words, by further supplying pure water to the "partial region" after preparing the first cleaning liquid, a region with a high contact angle can be formed inside the periphery of the liquid remaining on the surface of the wafer W. As a result, when the wafer W is subsequently rotated to discharge the liquid remaining on the surface of the wafer W outward, the liquid in the high contact angle region pushes out the liquid outside the region, allowing for efficient drainage of the liquid from the wafer surface.
[0093] The substrate developing method according to the present disclosure can also be applied to substrates to be processed other than semiconductor wafers, such as FPD (flat panel display) substrates.
[0094] The embodiments disclosed herein should be considered to be illustrative in all respects and not restrictive. The above-described embodiments may be omitted, substituted, or modified in various ways without departing from the scope of the appended claims, the configuration examples that fall within the technical scope of the present disclosure described below, and the spirit thereof. For example, the components of the above-described embodiments may be arbitrarily combined. Such an arbitrary combination naturally provides the functions and effects of each of the components involved in the combination, as well as other functions and effects that would be apparent to a person skilled in the art from the description of this specification.
[0095] Furthermore, the effects described herein are merely descriptive or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that are apparent to those skilled in the art from the description of this specification, in addition to or in place of the above-described effects.
[0096] The following configuration examples also fall within the technical scope of the present disclosure. (1) A developing method for developing a substrate, comprising: supplying a developer containing an organic solvent to the substrate on which a metal-containing coating film has been exposed to light in a predetermined pattern; and supplying a first cleaning liquid containing an organic solvent to the substrate to which the developer has been supplied, wherein the first cleaning liquid has a lower solubility for the metal-containing coating film than the developer and contains 0.25 to 50 volume % pure water. (2) The developing method according to (1), wherein the organic solvent contained in the first cleaning liquid is one or a mixture of two or more selected from the group consisting of 2-heptanone, isopropyl alcohol, propylene glycol monomethyl ether, propylene glycol monomethyl ether acetate, n-butyl acetate, cyclohexanone, methyl isobutyl carbinol, and ethyl lactate. (3) The developing method according to (1) or (2), wherein the developer is a mixture of propylene glycol monomethyl ether acetate and acetic acid. (4) The developing method according to any one of (1) to (3), wherein the developer contains less than 0.25% by volume of pure water. (5) The developing method according to any one of (1) to (4), further comprising the steps of: irradiating the substrate to which the first cleaning liquid has been supplied with ultraviolet light having a wavelength of 190 to 400 nm; heating the substrate during or after the ultraviolet light irradiation; and supplying the heated substrate with a second cleaning liquid containing an organic solvent. (6) The developing method according to (5), wherein the second cleaning liquid is an alkaline processing liquid or a processing liquid containing an organic acid. (7) A substrate processing system for performing a developing process on a substrate, comprising: a developer supply unit that supplies a developer containing an organic solvent to the substrate; a cleaning liquid supply unit that supplies a first cleaning liquid containing an organic solvent to the substrate; and a control unit that controls operations of the developer supply unit and the first cleaning liquid supply unit, wherein the control unit is configured to execute the steps of: supplying the developer to the substrate on which a metal-containing coating film has been exposed to a predetermined pattern; and supplying the first cleaning liquid to the substrate to which the developer has been supplied; and wherein the first cleaning liquid has a lower solubility for the metal-containing coating film than the developer, and contains 0.25 to 50 volume % of pure water.(8) The substrate processing system according to (7), wherein the organic solvent contained in the first cleaning liquid is one or a mixture of two or more selected from the group consisting of 2-heptanone, isopropyl alcohol, propylene glycol monomethyl ether, propylene glycol monomethyl ether acetate, n-butyl acetate, cyclohexanone, methyl isobutyl carbinol, and ethyl lactate. (9) The substrate processing system according to (7) or (8), wherein the developer is a mixture of propylene glycol monomethyl ether acetate and acetic acid. (10) The substrate processing system according to any one of (7) to (9), wherein the developer contains less than 0.25% by volume of pure water. (11) The substrate processing system according to any one of (7) to (10), comprising: an ultraviolet irradiation unit that irradiates the substrate with ultraviolet light having a wavelength of 190 to 400 nm, a heating unit that heats the substrate, and a second cleaning liquid supply unit that supplies a second cleaning liquid containing an organic solvent to the heated substrate, wherein the control unit is configured to execute the steps of: irradiating the substrate, to which the first cleaning liquid has been supplied, with ultraviolet light having a wavelength of 190 to 400 nm, heating the substrate during or after the ultraviolet light irradiation, and supplying the second cleaning liquid to the heated substrate. (12) The substrate processing system according to (11), wherein the second cleaning liquid is an alkaline processing liquid or a processing liquid containing an organic acid.
[0097] REFERENCE SIGNS LIST 1 substrate processing system 30 developer supply device 32 cleaning liquid supply device 200 control unit R metal-containing resist film W wafer
Claims
1. A developing method for performing a developing process on a substrate, comprising the steps of: supplying a developing solution containing an organic solvent to the substrate on which a metal-containing coating film has been exposed to a predetermined pattern; and supplying a first cleaning solution containing an organic solvent to the substrate to which the developing solution has been supplied, wherein the first cleaning solution has a lower solubility for the metal-containing coating film than the developing solution and contains 0.25 to 50 volume % pure water.
2. The developing method according to claim 1, wherein the organic solvent contained in the first cleaning solution is one or a mixture of two or more selected from the group consisting of 2-heptanone, isopropyl alcohol, propylene glycol monomethyl ether, propylene glycol monomethyl ether acetate, n-butyl acetate, cyclohexanone, methyl isobutyl carbinol, and ethyl lactate.
3. The developing method according to claim 2, wherein the developer is a mixture of propylene glycol monomethyl ether acetate and acetic acid.
4. The developing method according to any one of claims 1 to 3, wherein the developer contains less than 0.25% by volume of pure water.
5. The developing method according to any one of claims 1 to 3, further comprising the steps of: irradiating the substrate to which the first cleaning liquid has been supplied with ultraviolet light having a wavelength of 190 to 400 nm; heating the substrate during or after the irradiation with the ultraviolet light; and supplying a second cleaning liquid containing an organic solvent to the heated substrate.
6. The developing method according to claim 5, wherein the second cleaning liquid is an alkaline processing liquid or a processing liquid containing an organic acid.
7. A substrate processing system for performing a developing process on a substrate, comprising: a developing solution supply unit for supplying a developing solution containing an organic solvent to the substrate; a first cleaning solution supply unit for supplying a first cleaning solution containing an organic solvent to the substrate; and a control unit for controlling operation of the developing solution supply unit and the first cleaning solution supply unit, wherein the control unit is configured to execute a process of supplying the developing solution to the substrate having a metal-containing coating film exposed to a predetermined pattern; and supplying the first cleaning solution to the substrate to which the developing solution has been supplied, wherein the first cleaning solution has a lower solubility for the metal-containing coating film than the developing solution and contains 0.25 to 50 volume % pure water.
8. The substrate processing system according to claim 7, wherein the organic solvent contained in the first cleaning solution is one or a mixture of two or more selected from the group consisting of 2-heptanone, isopropyl alcohol, propylene glycol monomethyl ether, propylene glycol monomethyl ether acetate, n-butyl acetate, cyclohexanone, methyl isobutyl carbinol, and ethyl lactate.
9. The substrate processing system of claim 8, wherein the developer is a mixture of propylene glycol monomethyl ether acetate and acetic acid.
10. The substrate processing system according to any one of claims 7 to 9, wherein the developer contains less than 0.25% by volume of pure water.
11. A substrate processing system according to any one of claims 7 to 9, comprising: an ultraviolet irradiating unit that irradiates the substrate with ultraviolet light having a wavelength of 190 to 400 nm; a heating unit that heats the substrate; and a second cleaning liquid supply unit that supplies a second cleaning liquid containing an organic solvent to the heated substrate, wherein the control unit is configured to execute the steps of: irradiating the substrate to which the first cleaning liquid has been supplied with ultraviolet light having a wavelength of 190 to 400 nm; heating the substrate during or after the irradiation with ultraviolet light; and supplying the second cleaning liquid to the heated substrate.
12. The substrate processing system according to claim 11, wherein the second cleaning liquid is an alkaline processing liquid or a processing liquid containing an organic acid.
Citation Information
Patent Citations
Method for forming resist pattern and method for producing mold
JP2015053459A
Separating device and separating system
JP2015138954A
Film processing unit and substrate processing apparatus
JP2017092243A
Development unit, substrate processing apparatus, development method, and substrate processing method
JP2017147328A
Development method and substrate processing system
JP2022096081A