Method for forming protective film on outer peripheral part including bevel part of substrate

The method of using shielding structures to separate plasma generation and non-generation areas during substrate processing improves film uniformity and adhesion, addressing the issues of incomplete film formation and peeling in existing technologies.

WO2024247446A1PCT designated stage expired Publication Date: 2024-12-05EBARA CORP +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/010493
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-01
Filing Date
2024-03-18
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Existing methods for forming protective films on the outer periphery of substrates during semiconductor manufacturing often result in incomplete film formation and adhesion issues due to unclear boundaries between plasma generation and non-generation regions, leading to thinner film thickness and decreased adhesion at the inner boundary, which can cause peeling and particle generation.

Method used

A method involving a substrate processing apparatus where the substrate is placed on a stage smaller than itself with the outer periphery protruding, and shielding structures are used to separate the outer periphery from the inner region, allowing for uniform film formation by supplying film-forming gas between the substrate and electrode, ensuring clear separation between plasma generation and non-generation areas.

Benefits of technology

This approach improves the uniformity and adhesion of the protective film at the inner boundary, preventing peeling and particle generation, and enhancing the overall quality of the protective film.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024010493_05122024_PF_FP_ABST
    Figure JP2024010493_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention aims to improve the quality of a protective film for protecting an outer peripheral part of a substrate. The present invention provides a method for forming, with use of a plasma, a protective film on an outer peripheral part, including a bevel part, of a substrate, the method comprising: a step in which a second surface of the substrate, which has a first surface and the second surface opposite to each other, is placed on a stage that is smaller than the size of the substrate, in such a manner that the outer peripheral part of the substrate protrudes from the outer edge of the stage; a step in which at least a part of the outer peripheral part of the substrate in the circumferential direction is caused to face an electrode; a step in which a first shielding structure is brought into contact with the first surface of the substrate, the first shielding structure separating the outer peripheral part and the region inside the outer peripheral part from each other, and / or a second shielding structure is brought into contact with the second surface of the substrate, the second shielding structure separating the outer peripheral part and the region inside the outer peripheral part from each other; and a step in which a protective film is formed on the outer peripheral part of the substrate by supplying a film forming gas between the outer peripheral part of the substrate and the electrode.
Need to check novelty before this filing date? Find Prior Art

Description

A method for forming a protective film on the outer periphery of a substrate, including the bevel portion

[0001] The present invention relates to a substrate processing method, and more particularly to a method for forming a protective film on the outer periphery of a substrate, including a bevel portion.

[0002] As described in Japanese Patent No. 3949941 (Patent Document 1), during a semiconductor manufacturing process, the outer periphery (edge ​​and bevel) of a substrate may be eroded during etching of the substrate. This may cause damage to the outer periphery of the substrate during substrate transfer or substrate processing. Furthermore, particles may be trapped in the eroded portion, which may adversely affect the substrate processing in subsequent steps, resulting in a decrease in yield.

[0003] As described in Japanese Patent No. 5,982,383 (Patent Document 2), a solution is proposed in which a protective film is formed on the outer periphery (edge ​​and bevel) of the substrate to protect it from etching. According to this technology, plasma is maintained only on the outer periphery of the substrate, while the electrode gap is set to a predetermined distance in the central portion of the substrate, and the pressure is adjusted to prevent plasma formation, thereby forming a protective film only on the outer periphery of the substrate. Furthermore, Japanese Patent Laid-Open No. 2020-021931 (Patent Document 3) proposes performing plasma processing on the outer periphery of the substrate by placing an electrode only on a portion of the outer periphery of the substrate and rotating the substrate. In both patent document technologies, gas is introduced from the center of the substrate and electrodes are placed on the outer periphery of the substrate.

[0004] Patent No. 3949941 Patent No. 5982383 JP 2020-021931 A

[0005] However, in the above-mentioned method, the boundary between the space where plasma is maintained and the space where plasma generation is prevented is not clearly defined because the boundary between the gas pressure and the space where plasma generation is prevented changes continuously. As a result, when a protective film is formed on the outer periphery of a substrate using a plasma process, the inner boundary of the protective film may be incompletely formed. In other words, the thickness of the inner boundary of the protective film may be thin, or the adhesion of the protective film may be reduced. As a result, peeling of the protective film or generation of particles may occur in processes after the protective film formation.

[0006] It is also possible to improve the uniformity of the film thickness at the boundary by forming a resist film on the substrate except for the outer periphery, then forming a protective film on the outer periphery of the substrate, and then removing the resist. However, this is expected to have the disadvantage of being costly due to the resist application, baking, and removal processes.

[0007] SUMMARY OF THE INVENTION It is an object of the present invention to solve at least some of the above problems, and one of the objects of the present invention is to improve the quality of a protective film for protecting the outer periphery of a substrate.

[0008] According to one aspect of the present invention, there is provided a method for forming a protective film on an outer periphery, including a bevel portion, of a substrate using plasma, the method comprising: placing a second surface of a substrate having opposing first and second surfaces on a stage smaller than the dimensions of the substrate so that the outer periphery of the substrate protrudes from the outer edge of the stage; arranging at least a portion of the circumferential direction of the outer periphery of the substrate opposite an electrode; contacting the first surface of the substrate with a first shielding structure that separates the outer periphery from an area inside it, and / or contacting the second surface of the substrate with a second shielding structure that separates the outer periphery from an area inside it; and supplying a film formation gas between the outer periphery of the substrate and the electrode to form a protective film on the outer periphery of the substrate.

[0009] 1 is a schematic diagram showing an example of the configuration of a substrate processing apparatus according to an embodiment; FIG. 1 is a schematic diagram showing an example of the configuration of a substrate processing apparatus according to an embodiment; FIG. 2 is a cross-sectional view showing an example of the configuration for supplying a film formation gas; FIG. 3 is a bottom view of a top cover; FIG. 4 is a cross-sectional view showing an example of the configuration for supplying a film formation gas; FIG. 5 is a bottom view of the top cover; FIG. 6 is a cross-sectional view showing an example of the configuration for supplying a film formation gas; FIG. 7 is a cross-sectional view showing an example of the configuration for supplying a film formation gas; FIG. 8 is a cross-sectional view showing an example of the configuration for an electrode; FIG. 9 is a plan view showing an example of the configuration for an electrode; FIG. 10 is a cross-sectional view showing an example of the configuration for an electrode divided into upper and lower parts when opened; FIG. 11 is a cross-sectional view showing an example of the configuration for an electrode divided into upper and lower parts when closed; FIG. 12 is a schematic diagram showing an example of a connection for connecting a substrate to a negative bias; FIG. 13 is a schematic diagram showing an example of a connection for connecting a substrate to a negative bias; FIG. 14 is a schematic diagram showing an example of a connection for biasing the top cover and the bottom cover; FIG. 15 is an explanatory diagram for explaining a method for centering a substrate; FIG. 16 is an explanatory diagram for explaining a method for centering a substrate; FIG. 17 is an explanatory diagram for explaining the formation of a protective film according to an embodiment; FIG. 18 is an explanatory diagram for explaining the formation of a protective film according to a comparative example; FIG. 19 is a schematic diagram showing a substrate (substrate with a protective film) on which a protective film according to an embodiment has been formed. FIG. 1 is a schematic diagram showing a substrate (substrate with protective film) on which a protective film according to one embodiment has been formed. FIG. 2 is a schematic diagram showing a substrate (substrate with protective film) on which a protective film according to one embodiment has been formed. FIG. 3 is a schematic diagram showing a substrate (substrate with protective film) on which a protective film according to one embodiment has been formed. FIG. 4 is a flowchart of a semiconductor manufacturing process. FIG. 5 is a flowchart of a semiconductor manufacturing process. FIG. 6 is a flowchart of a semiconductor manufacturing process.

[0010] An embodiment of the present invention will be described below with reference to the drawings. In the following embodiments, identical or corresponding components are designated by the same reference numerals, and redundant description will be omitted. Furthermore, expressions such as "upper," "lower," "left," and "right" are used in this specification, but these are for the sake of convenience and indicate positions and directions on the paper surface of the illustrative drawings, and may differ in actual placement when the device is in use, etc.

[0011] FIG. 1 is a schematic diagram showing an example of the configuration of a substrate processing apparatus 100 according to an embodiment. The substrate processing apparatus 100 forms a protective film 90 ( FIG. 12A ) on the outer periphery (edge ​​and bevel portions) of a substrate W using localized plasma. The substrate processing apparatus 100 may be a substrate processing apparatus that uses capacitively coupled plasma, inductively coupled plasma, microwave plasma, or other plasmas. In this embodiment, a plasma film forming apparatus is used as the substrate processing apparatus 100, but the substrate processing apparatus 100 may also be a plasma etching apparatus or other plasma substrate processing apparatus. In this specification, as shown in FIG. 12A , the outer periphery 200 of the substrate W includes an edge portion 201 and a bevel portion 202. The bevel portion 202 is a chamfered side portion of the substrate W, and the edge portion 201 is a flat portion inside the bevel portion 202 in the outer periphery 200 of the substrate W. In this embodiment, the region (range) inside the outer periphery 200 of the substrate W is referred to as a central portion 300. In this embodiment, the central portion 300 of the front surface and the back surface (top surface and bottom surface in FIG. 1 ) of the substrate W is the device formation region. In other embodiments, the substrate W may have device formation regions on both the front surface and the back surface. The outer peripheral portion 200 can be defined as the region outside the device formation region. For example, if the substrate W has a device formation region on its front surface, the regions on the front and back surfaces of the substrate W corresponding to the device formation region can be defined as the central portion 300, and the regions outside the central portion 300 on the front and back surfaces of the substrate W can be defined as the outer peripheral portion 200.

[0012] In this embodiment, the substrate W is a circular wafer on which, for example, semiconductor devices, optical elements, MEMS, etc. are formed. Note that the substrate W may also be a substrate on which other types of devices are formed, or may be a substrate of any shape other than a circle, such as a polygon (e.g., a rectangle). The substrate W may also be a silicon substrate (including a substrate made of silicon and a composite substrate such as an SOI substrate whose surface is silicon), a compound semiconductor substrate, or a substrate made of any other material.

[0013] In this embodiment, the protective film 90 may be an insulating film, a dielectric film, a conductor film, an organic film, or any other film used in semiconductor manufacturing. The protective film 90 is preferably a film that is etch-resistant and has high hardness. For example, an amorphous carbon or DLC (diamond-like carbon) film can be used as such a protective film 90.

[0014] The substrate processing apparatus 100 mainly comprises a housing 10 that constitutes a plasma chamber 11 , a stage 20 disposed within the housing 10 , an electrode 60 , a top cover 40 , and a bottom cover 50 .

[0015] The stage 20 has a support surface on which the substrate W is placed and a chuck function for fixing the substrate W. The stage 20 may also have a heater function for heating the substrate W. The stage 20 can be rotated by a driving device such as a motor (not shown). The substrate W on which the protective film 90 is to be formed is placed on the support surface (the upper surface in FIG. 1 ) of the stage 20. The diameter of the substrate W is larger than the diameter of the support surface of the stage 20. In other words, the diameter of the support surface of the stage 200 is smaller than the diameter of the substrate W. Therefore, the outer periphery 200 (edge ​​portion 201 and bevel portion 202) of the substrate W is not supported by the stage 20. In this example, the stage 20 is connected to a ground potential, and the substrate W is connected to the ground potential via the stage 20. The housing 10 is also connected to a ground potential, and the stage 20 is connected to the ground potential via the housing 100.

[0016] The electrode 60 is located outside the stage 20 and has a shape that faces the outer periphery of the substrate W and covers the outer periphery 200 of the substrate W from the side, and has, for example, an arc-shaped cross-sectional shape. The electrode 60 is made of a conductive material, for example, a metal. The electrode 60 is connected to, for example, an RF power supply 110 that applies high-frequency power to the electrode 60. In this embodiment, high-frequency power is supplied from the electrode 60 to the film formation gas 70 to ionize the film formation gas 70 and generate plasma. Alternatively, a DC power supply may be connected to the electrode 60, and DC power may be supplied from the electrode 60 to the film formation gas 70 to ionize the film formation gas 70 and generate plasma. The electrode 60 is positioned so that the distance between the electrode 60 and the outer periphery 200 of the substrate W (edge ​​portion 201, bevel portion 202) is constant in the film formation region or plasma generation region 71, thereby ensuring a uniform flow of the film formation gas 70 between the electrode 60 and the outer periphery 200 of the substrate W. The plasma generation region 71 is a three-dimensional space and is also referred to as a plasma generation space. The electrodes 60 are provided so as to be arranged continuously or intermittently (discretely) around the entire circumference of the substrate W, as shown in Fig. 1. Alternatively, the electrodes 60 may be arranged at a portion of the circumference of the substrate W, as shown in Fig. 7B.

[0017] When the electrode 60 is provided continuously around the entire circumference of the substrate W, it is preferable to divide the electrode 60 into an upper electrode 60A and a lower electrode 60B, as shown in Figures 8A and 8B, to facilitate installation and removal of the substrate W. When the electrode 60 is provided discretely around the entire circumference of the substrate W, it is preferable to move the individual electrodes 60 toward or away from the substrate W along the substrate radial direction, for example, by an actuator (not shown), to facilitate installation and removal of the substrate W. When the electrode 60 is disposed on a portion of the circumference of the substrate W, for example, the substrate W is rotated so that the electrodes 60 sequentially face the entire circumference of the substrate W, and a protective film 90 is formed around the entire circumference of the substrate W (Figure 7B). Even when the electrode 60 is disposed on a portion of the circumference of the substrate W, it is possible to move the electrode 60 toward or away from the substrate W along the substrate radial direction by an actuator (not shown), to facilitate installation and removal of the substrate W.

[0018] The top cover 40 is a shielding structure for shielding the central portion 300 of the substrate W (the region inside the outer peripheral portion 200) from plasma. The top cover 40 has a hollow portion therein, and this hollow portion accommodates the central portion 300 of the substrate W (in FIG. 1 , the central portion 300 of the upper surface of the substrate W). The hollow portion within the top cover 40, the central portion 300 of the substrate W, is a non-plasma generation region 72 that is shielded from plasma. The central portion 300 of the upper surface of the substrate W is a device formation region, and the top cover 40 is positioned so that the top cover 40 does not directly contact the device formation region. The pressure within the hollow portion of the top cover 40 may be lower, higher, or the same as the vacuum pressure around the outer peripheral portion 200 of the substrate W, and may be atmospheric pressure, for example. The top cover 40 may be formed of a plasma-resistant material, such as polyimide, yttria-coated metal, or other material.

[0019] The top cover 40 includes, for example, a cylindrical tubular portion 42 having a contact portion at one end that contacts the substrate W, and a disk-shaped lid portion 41 provided at the other end of the tubular portion 42. In the example shown in the figure, the outer periphery of the lid portion 41 forms a flange portion 41A that extends to the outside of the tubular portion 42. On the outside of the tubular portion 42 (the flange portion 41A), the lid portion 41 is provided with a plurality of gas supply holes 43 along the circumferential direction ( FIG. 3B ). The plurality of gas supply holes 43 are configured to generate a uniform downflow of the film formation gas 70 along the circumferential direction. The plurality of gas supply holes 43 are oriented to supply the film formation gas 43 along the tubular portion 42 and in the vertical direction (perpendicular to the substrate W) to a region (plasma generation region 71) surrounded by the top cover 40, the bottom cover 50, and the electrode 60. A buffer chamber 30 is provided on the upper surface of the lid 41 so that the film formation gas 70 supplied to the outer peripheral portion 200 of the substrate W is uniform in the entire circumferential direction (around the entire circumference). The buffer chamber 30 may be configured, for example, in an annular or donut shape with an open center, as shown in FIG. 1 . The internal space of the buffer chamber 30 is fluidly connected to a plurality of gas supply holes 43. The buffer chamber 30 is provided with supply ports 31 fluidly connected to the internal space. The film formation gas is supplied into the buffer chamber 30 through the supply ports 31 and distributed from the buffer chamber 30 to each gas supply hole 43. With this configuration, the film formation gas can be uniformly supplied in the circumferential direction through the plurality of gas supply holes 43 to the area surrounded by the top cover 40, the bottom cover 50, and the electrode 60.

[0020] A drive shaft 13 of an actuator 12 is fixed to the upper surface of the top cover 40. The actuator 12 is located outside the plasma chamber 11, and the drive shaft 13 of the actuator 12 penetrates the wall of the housing 10 and is connected to the top cover 40. A magnetic fluid seal 14 seals the gap between the drive shaft 13 and the housing 10. The drive shaft 13 is configured to be movable up and down by the power of the actuator 12. The drive shaft 13 is also attached to the actuator body so that it can rotate together with the top cover 40 when the substrate W rotates with the top cover 40 pressed against it. When the substrate W is carried into the chamber 11 and placed on the stage 20, the actuator 12 moves the top cover 40 to a retracted position above the stage 20. After the substrate W is placed on the stage 20, the actuator 12 lowers the top cover 40 so that the top cover 40 comes into contact with and is pressed against the substrate W. This allows the top cover 40 to physically separate the plasma generation region 71 from the non-plasma generation region 72.

[0021] In this embodiment, the substrate W is rotated so that the flow of the film formation gas 70 is uniform in the circumferential direction of the substrate W. This makes it easier to form the protective film 90 uniformly around the entire outer periphery of the substrate W. Note that in other embodiments, the substrate W does not need to be rotated. For example, when the electrodes 60 are arranged continuously around the entire periphery of the substrate W, if the protective film 90 can be formed around the entire periphery of the substrate W with an acceptable level of uniformity, the substrate W does not need to be rotated. For example, when the electrodes 60 are arranged intermittently (discretely) around the entire periphery of the substrate W, if the electrode pieces are sufficiently close to each other so that the protective film 90 can be formed around the entire periphery of the substrate W with an acceptable level of uniformity, the substrate W does not need to be rotated.

[0022] In this embodiment, the drive shaft 13 of the actuator 12 is fixed to the upper surface of the top cover 40, but if the buffer chamber 30 is disc-shaped rather than annular, the drive shaft 13 of the actuator 12 may be fixed to the upper surface of the buffer chamber 30.

[0023] The bottom cover 50 is disposed on the outer side of the stage 20 and is configured as a cylindrical tubular portion that surrounds the entire periphery of the stage 20. The bottom cover 50 is electrically insulated from the stage 20. The bottom cover 50 can be formed of a plasma-resistant material, such as polyimide, yttria-coated metal, or other materials. The top surface of the bottom cover 50 is flush with the top surface (mounting surface) of the stage 20. The bottom cover 50 reliably contacts the substrate W by utilizing the force generated when the top cover 40 contacts the substrate W, thereby physically isolating the plasma generation region 71. The bottom cover 50 is disposed at a predetermined distance from the outer peripheral surface of the stage 20. However, the distance is set to a level that prevents plasma from penetrating through the gap between the bottom cover 50 and the outer peripheral surface of the stage 20 and forming a film on the underside of the substrate W.

[0024] In this substrate processing apparatus 100, the region surrounded by the top cover 40, the bottom cover 50, and the electrode 60 is the plasma generation region 71. Furthermore, the outer peripheral portion 200 and the central portion 300 of the substrate W are physically separated by the top cover 40 and the bottom cover 50, thereby clearly defining the boundary between the plasma generation region 71 and the non-plasma generation region 72. Therefore, as shown in FIG. 12A , the protective film 90 is formed with a consistent thickness at its inner boundary (improving film thickness uniformity), thereby improving the adhesion of the protective film 90. On the other hand, in the comparative example shown in FIG. 12B , the plasma generation region 71 and the non-plasma generation region 72 are non-physically separated by pressurizing the central portion 300 of the substrate W and / or introducing a purge gas. Therefore, the boundary between the two regions is unclear, resulting in incomplete deposition at the inner boundary of the protective film 90. As a result, the thickness of the protective film 90 becomes thinner at its inner boundary, reducing the adhesion of the protective film 90.

[0025] FIG. 2 is a schematic diagram showing another example of the configuration of a substrate processing apparatus 100 according to an embodiment. The substrate processing apparatus 100 shown in FIG. 2 differs from the substrate processing apparatus 100 shown in FIG. 1 in that it does not include a bottom cover 50. Furthermore, the dimensions of the stage 20 have been expanded so that the mounting surface of the stage 20 is roughly flush with the outer peripheral surface of the cylindrical portion 42 of the top cover 40. Other configurations are similar to those shown in FIG. 1 , and therefore detailed descriptions are omitted. In this substrate processing apparatus 100, the plasma generation region 71 is partitioned by the stage 20 instead of the bottom cover 50. That is, the plasma generation region 71 is partitioned by the top cover 40, the stage 20, and the electrode 60. This configuration can achieve the same effects as the configuration shown in FIG. 1 . Furthermore, since the stage 20 is also used as a shielding structure, the bottom cover 50 can be omitted, which has the advantage of simplifying the apparatus configuration.

[0026] FIG. 3A is a cross-sectional view showing an example of a configuration for supplying a film formation gas. FIG. 3B is a bottom view of the top cover. In this configuration, a plurality of gas supply holes 43, which are through-holes, are provided along the circumferential direction of the lid portion 41 on the outer side (flange portion 41A) of the cylindrical portion 42. To uniformly supply the film formation gas to the plasma generation region 71 along the circumferential direction, the plurality of gas supply holes 43 are preferably provided at equal intervals along the circumferential direction. In this configuration, the film formation gas 70 is supplied from the buffer chamber 70 to the plurality of gas supply holes 43, and the film formation gas 70 is supplied from each gas supply hole 43 to the plasma generation region 71 (the region surrounded by the top cover 40, the stage 20 (or the bottom cover 50), and the electrode 60). After being used to form a film on the outer peripheral portion 200 of the substrate W in the plasma generation region 71, the film formation gas 70 flows downward through the gap between the stage 20 (or the bottom cover 50) and the electrode 60. Although FIG. 3A shows an example in which the bottom cover 50 is omitted (FIG. 2), the same applies to an example in which the bottom cover 50 is provided (FIG. 1).

[0027] FIG. 4A is a cross-sectional view showing another example of a configuration for supplying a film formation gas. FIG. 4B is a bottom view of the top cover. In this configuration, an annular porous body 44 is provided on the lid portion 41 at the outer side (flange portion 41A) of the cylindrical portion 42. The porous body 44 is provided so as to penetrate between the upper and lower surfaces of the lid portion 41. Here, an example in which the porous body 44 is provided continuously around the entire circumference is shown, but the porous body 44 may also be provided intermittently or discretely in the circumferential direction. In order to uniformly supply the film formation gas to the plasma generation region 71 around the circumference, the intermittently or discretely provided porous bodies 44 are preferably provided at equal intervals around the circumference. In this configuration, the film formation gas 70 is supplied from the buffer chamber 70 to the porous body 44, and then the film formation gas 70 is supplied from the porous body 44 to the plasma generation region 71 (the region surrounded by the top cover 40, the stage 20 (or the bottom cover 50), and the electrode 60). After being used to form a film on the outer periphery of the substrate W in the plasma generation region 71, the film formation gas 70 flows downward through between the stage 20 (or the bottom cover 50) and the electrode 60. Note that, although Fig. 4A shows an example in which the bottom cover 50 is omitted (Fig. 2), the same applies to the example in which the bottom cover 50 is provided (Fig. 1).

[0028] FIG. 5 is a cross-sectional view showing another example of a configuration for supplying a film formation gas. In this configuration, a plurality of nozzles 81 arranged along the circumferential direction of the substrate W supply the film formation gas 70 horizontally into the gap between the lid portion 41 (flange portion 41A) on the outer side of the cylindrical portion 42 and the electrode 60. To uniformly supply the film formation gas 70 circumferentially to the plasma generation region 71, the plurality of nozzles 81 are preferably arranged at equal intervals along the circumferential direction. In this configuration, the film formation gas 70 is supplied horizontally from the nozzles 81 into the gap between the lid portion 41 and the electrode 60, then turns vertically downward upon hitting the cylindrical portion 42, and is supplied to the plasma generation region 71 (the region surrounded by the top cover 40, the stage 20 (or the bottom cover 50), and the electrode 60). After being used to form a film on the outer periphery of the substrate W in the plasma generation region 71, the film formation gas 70 flows downward through the gap between the stage 20 (or the bottom cover 50) and the electrode 60. In this configuration, the deposition gas 70 is caused to flow perpendicular to the cylindrical portion 42 of the top cover 40 and is made to hit the cylindrical portion 42 once, thereby improving the uniformity of the deposition gas 70. Note that, although Fig. 5 shows an example in which the bottom cover 50 is omitted (Fig. 2), the same applies to the example in which the bottom cover 50 is provided (Fig. 1).

[0029] FIG. 6 is a cross-sectional view showing another example of a configuration for supplying a film formation gas. While FIG. 6 shows an example in which the bottom cover 50 is omitted (FIG. 2), the same applies to the example in which the bottom cover 50 is provided (FIG. 1). In this configuration, one or more gas supply holes 61 are provided in the electrode 60, and the film formation gas 70 is supplied to the plasma generation region 71 in a flow parallel to the surface of the substrate W. When the electrode 60 is provided continuously or intermittently around the entire circumference of the substrate W, multiple gas supply holes 61 are provided in the electrode 60 around the circumference of the substrate W. To uniformly supply the film formation gas to the plasma generation region 71 around the circumference, the multiple gas supply holes 61 are preferably provided at equal intervals around the circumference. A buffer chamber 82 is provided in an annular shape around the entire circumference of the electrode 60 on the outer circumferential surface of the electrode 60, and the buffer chamber 82 is fluidly connected to the multiple gas supply holes 61. The film formation gas 70 is supplied to the buffer chamber 82 through one or more gas supply pipes 83. By supplying the film formation gas 70 to each gas supply hole 61 through the buffer chamber 82, the film formation gas 70 can be supplied at a uniform flow rate to each gas supply hole 61. In this configuration, the film formation gas 70 is supplied from the gas supply pipe 83 to the buffer chamber 82 and then supplied from the buffer chamber 82 to the plasma generation region 71 (the region surrounded by the top cover 40, the stage 20 (or the bottom cover 50), and the electrode 60) through each gas supply hole 61. The film formation gas 70 supplied to the plasma generation region 71 is divided into upper and lower flows, and the film formation gas 70 flowing upward flows out through the gap between the top cover 40 and the electrode 60, while the film formation gas 70 flowing downward flows out through the gap between the top cover 40 and the electrode 60.

[0030] It is preferable that the flow resistances of the upward and downward flow paths be approximately equal so that the film formation gas 70 entering the plasma generation region 71 through the gas supply holes 61 is divided into vertically uniform flow rates. For this reason, in the example of FIG. 6 , the gas supply holes 61 are provided at the same height as the substrate W (or the height of the center of the substrate W in the vertical direction). When the electrode 60 is vertically symmetrical, the gas supply holes 61 are provided at the center of the electrode 60 in the vertical direction. Also, in the example of FIG. 6 , an extension or flange 21 is provided on the stage 20 so as to correspond to the flange 41A of the lid 41 of the top cover 40, so that the flow resistances of the upward and downward flow paths are approximately equal. However, instead of providing the flange 21 on the stage 20, a flange may be provided on the bottom cover 50 so as to correspond to the flange 41A of the lid 41 of the top cover 40.

[0031] When the electrode 60 is provided so as to face a part of the circumferential direction of the outer circumferential portion 200 of the substrate W (see FIGS. 7A and 7B ), one gas supply hole 61 may be provided in the electrode 60. Furthermore, the buffer chamber 82 may be omitted.

[0032] FIG. 7A is a cross-sectional view showing an example of the configuration of the electrode 60. FIG. 7B is a plan view showing an example of the configuration of the electrode 60. As shown in these figures, the electrode 60 may be provided so as to face a portion of the circumferential direction of the outer peripheral portion 200 of the substrate W. In this configuration, for example, by rotating the substrate W using the stage 20, the electrode 60 and the plasma generation region 71 inside the electrode 60 face the entire circumference of the outer peripheral portion of the substrate W. That is, by disposing the electrode 60 with dimensions corresponding to a portion of the circumferential direction of the outer peripheral portion of the substrate W and rotating the substrate W, the protective film 90 is formed around the entire circumference of the outer peripheral portion 200 of the substrate W. Reference numeral 25 indicates the direction of rotation of the substrate W. The rotation direction may be reversed or is arbitrary. Note that while FIG. 7A shows an example in which a bottom cover 50 is provided ( FIG. 1 ), the same applies to an example in which the bottom cover 50 is omitted ( FIG. 2 ).

[0033] 8A is a cross-sectional view showing an example of the configuration of the electrode 60 divided into upper and lower parts when it is open. FIG. 8B is a cross-sectional view showing an example of the configuration of the electrode 60 divided into upper and lower parts when it is closed. When the electrode 60 is arranged in a circular ring shape around the entire circumference of the substrate W, the electrode 60 may be divided into an upper electrode 60A and a lower electrode 60B to facilitate installation of the substrate W on the stage 20. In this case, the upper electrode 60A can be fixed to, for example, the flange portion 41A of the lid portion 41 of the top cover 40, and configured to move up and down together with the movement of the top cover 40 by the actuator 12. 8A , when the substrate W is to be placed on the stage 20, the top cover 40 and the upper electrode 60A are moved upward and retracted, and after the substrate W is placed on the stage 20, the top cover 40 and the upper electrode 60A are moved downward so that the top cover 40 comes into contact with the substrate W, and the upper electrode 60A and the lower electrode 60B are joined together to form a plasma generation region 71 (a region surrounded by the top cover 40, the stage 20 (or the bottom cover 50), and the electrode 60). Note that, although a configuration in which the stage 20 defines the plasma generation region 71 (corresponding to FIG. 2 ) is given as an example here, the same applies to a configuration in which the bottom cover 50 is disposed to define the plasma generation region 71 (corresponding to FIG. 1 ).

[0034] FIG. 9A is a schematic diagram showing an example of connecting a substrate to a negative bias. In the above-described embodiment, the stage 20 and substrate W are connected to ground potential. However, the stage 20 and substrate W may be connected to the low-potential side of the DC power supply 111 and biased to a negative DC voltage (negative bias voltage). The DC power supply 111 is preferably a power supply capable of adjusting the negative bias voltage. Applying a negative bias voltage to the substrate W accumulates negative charges only in the outer peripheral portion 200 of the substrate W facing the electrode 60, thereby promoting plasma generation. The central portion 300 of the substrate W does not face the electrode 60, and therefore does not accumulate charges. Note that FIG. 9A shows an example in which the lid portion 41 of the top cover 40 does not have a flange, and film formation gas is supplied downward from between the top cover 40 and the electrode 60. However, this also applies to the configuration of the above-described embodiment. As shown in FIG. 9A, when the electrode 60 is fixed to the inner wall of the housing 10, an insulator 62 may be disposed between the electrode 60 and the housing 10 to electrically insulate the electrode 60 from the housing 10.

[0035] 9B is a schematic diagram showing another example of connection for connecting a substrate to a negative bias. As shown in the figure, a conductor 22, which is a component that contacts the substrate W and applies a negative bias voltage, is arranged on the stage 20 at a position close to the outer periphery 200 of the substrate W. The conductor 22 may be an annular (ring-shaped) component that corresponds to the inner side of the outer periphery 200 of the substrate W. The conductor 22 may be provided continuously or intermittently around the entire circumference of the outer periphery 200 of the substrate W. The conductor 22 is connected to the low-potential side of the DC power supply 111, is arranged on the outer periphery of the stage 20, contacts the substrate W, and applies a negative bias voltage to the substrate W. The conductor 22 is electrically insulated from other parts of the stage 20 by an insulator or the like (not shown), or the stage 20 is made of an insulator. The conductor 22 is provided so as to penetrate the outer periphery of the stage 20, with the upper surface of the conductor 22 being flush with the mounting surface of the stage 20 (either completely flush or slightly protruding from the mounting surface), and the lower surface of the conductor 22 being exposed to the lower surface of the stage 20. With this configuration, the necessary negative bias voltage can be efficiently applied to the outer periphery 200 of the substrate W from a position close to the outer periphery 200 of the substrate W. Note that although an example is given here in which the negative bias voltage is applied to the substrate W by the DC power supply 111, the negative bias voltage may also be applied to the substrate W by a pulsed power supply. While FIG. 9B shows an example in which a bottom cover 50 is provided (corresponding to FIG. 1 ), the bottom cover 50 may be omitted and the stage 20 may be extended to the position of the bottom cover 50. In this case, the conductor 22 may come into contact with the outer periphery 200 of the substrate W.

[0036] 10A and 10B are schematic diagrams showing examples of connections for biasing the top cover 40 and the bottom cover 50. As shown in FIG. 10A , the top cover 40 and the bottom cover 50 that contact the substrate W may be formed of a conductor, and the top cover 40 and the bottom cover 50 may be connected to the low-potential side of the DC power supply 111, biasing the outer periphery of the substrate W to a negative DC voltage. The stage 20 may be connected to a ground potential. The top cover 40 and the bottom cover 50 may be entirely formed of a conductor, or at least the portions of the top cover 40 and the bottom cover 50 that contact the substrate W may be formed of a conductor. Furthermore, as shown in FIG. 10B , the portions of the top cover 40 and the bottom cover 50 exposed to the plasma generation region 71 may be covered with insulators (insulators 42A and 50A). This configuration can suppress or prevent the top cover 40 and the bottom cover 50 from being deteriorated by plasma. The outer periphery of the substrate W may be biased to a negative DC voltage using either the top cover 40 or the bottom cover 50 .

[0037] The bias is not limited to a DC voltage, but may be a pulse or a high frequency voltage. A negative bias makes it easier to attract positive ions, but when attracting negative ions, a positive bias is applied.

[0038] In this embodiment, when DLC is used as the protective film 90, for example, the substrate bias voltage is −500 V to −50 V, the film forming pressure is 0.1 to 1 Pa, and the material gas is CH 4 , C 2 H 2 A gas containing carbon such as CO is used.

[0039] 11A and 11B are explanatory diagrams illustrating a method for centering a substrate W. As shown in FIG. 11A , a line sensor 120 is installed at a position of θ=180° on the outer periphery of a substrate W placed on a stage 20, and the substrate W is rotated by the stage 20. The distance at which an irradiation area 121 is blocked is measured at positions θ=θ1 and θ=θ1+180° on the outer periphery of the substrate W. The origin θ=0 can be set to any position, and in the example of FIG. 11A , the origin θ=0 is set to the position of an electrode 60 arranged in a part of the outer periphery 200 of the substrate W. The line sensor 120 has a pair of a light-emitting element 120A and a light-receiving element 120B. The light-emitting element 120A irradiates light in a line toward the light-receiving element 120B to form an irradiation area 121, and the distance or position at which the substrate W blocks the irradiation area 121 is measured. As shown in FIG. 11B , the distance over which the substrate W blocks the irradiation area 121 of the line sensor 120 at θ=θ1+180° is longer by a distance D than the distance over which the substrate W blocks the irradiation area 121 of the line sensor 120 at θ=θ1. In this case, since the center of the substrate W is displaced by a distance D / 2 from the position of θ=θ1 toward the position of θ=θ1+180° relative to the center of rotation of the stage 20, the substrate W is moved in the opposite direction, that is, by a distance D / 2 from the position of θ=θ1+180° toward the position of θ=θ1. In this manner, the substrate W can be aligned (centered) with respect to the center of rotation of the stage 20. This makes it easy to make the distance between the outer periphery 200 of the substrate W and the electrode 60 uniform over the entire circumference. When the substrate W is rotated relative to the electrode 60 located at a portion of the outer periphery 200 of the substrate W as shown in FIG. 11A , the outer periphery 200 of the substrate W can be made to face the electrode 60 at a uniform distance over the entire circumference.

[0040] FIG. 12A is a diagram illustrating the formation of a protective film according to one embodiment. FIG. 12B is a diagram illustrating the formation of a protective film according to a comparative example. According to the substrate processing apparatus 100 according to the embodiment, as shown in FIG. 12A , the region surrounded by the top cover 40, stage 20 (or bottom cover 50), and electrode 60 is the plasma generation region 71. Furthermore, the outer peripheral portion 200 and the central portion 300 of the substrate W are physically separated by the top cover 40 and stage 20 (or bottom cover 50), thereby clearly defining the boundary between the plasma generation region 71 and the non-plasma generation region 72. Therefore, the protective film 90 is formed with a consistent thickness at its inner boundary (improving film thickness uniformity), thereby improving adhesion of the protective film 90. While FIG. 12A illustrates an example in which the underside of the substrate W is separated by the stage 20 ( FIG. 2 ), the same applies to the case in which the underside of the substrate W is separated by the bottom cover 50 ( FIG. 1 ). 12B, which is shown as a comparative example, non-physically separates the plasma generation region 71 and the non-plasma generation region 72 by pressurizing the central portion 300 of the substrate W and / or introducing a purge gas, and the boundary between the two regions is not clearly defined. When the two regions are separated non-physically in this manner, a stable film cannot be formed at the inner boundary of the protective film 90, and the film thickness at the inner boundary of the protective film 90 becomes thin, resulting in a decrease in adhesion of the protective film 90.

[0041] (Modifications) (1) In the above embodiment, an example in which a top cover and a bottom cover are provided ( FIG. 1 ) and an example in which only a top cover is provided ( FIG. 2 ) have been described, but a configuration in which only a bottom cover is provided may also be used. In this case, the bottom cover can suppress or prevent a decrease in the film thickness and a decrease in adhesion at the inner boundary of the protective film at least on the underside of the substrate W, thereby improving the quality of the protective film. Furthermore, on the upper surface of the substrate, other shielding methods such as a resist film may be used to prevent the formation of film material in the central portion of the upper surface of the substrate. (2) While the above describes a plasma film formation apparatus, the structure of the above embodiment (shielding structure using a top cover and / or bottom cover) can also be applied to plasma etching apparatuses and other plasma substrate processing apparatuses.

[0042] 13A to 13E are schematic diagrams showing substrates W (substrates with protective films) on which various types of protective films are formed. The protective film 90 can be formed on both or one side of the substrate W, covering part or all of the radial direction of the outer periphery 200 of the substrate W (e.g., at least one of the edge portion 201 and the bevel portion 202). For example, the protective film 90 can be formed on the edge portion 201 and the bevel portion 202 on both or one side of the substrate W. The protective film 90 can also be formed only on the bevel portion 202 on both or one side of the substrate W. The protective film 90 can also be formed only on the edge portion 201 on both or one side of the substrate W. The protective film 90 may also be composed of multiple layers. When a protective film is formed on one side of the substrate W, it is preferable to form the protective film on part or all of the radial direction of the outer periphery of the surface including the device formation region (e.g., at least one of the edge portion 201 and the bevel portion 202). The area where the protective film 90 is formed (the edge portion 201 and / or the bevel portion 202 on both sides or one side of the substrate W) can be an area on the outer periphery of the substrate that needs to be particularly protected, or an area on the outer periphery of the substrate where protection is sufficient.

[0043] 13A shows an example in which a protective film 90 made of amorphous carbon or DLC is formed on the edge portion 201 and the bevel portion 202 on both sides of the substrate W. FIG. 13B shows an example in which a protective film 90 made of amorphous carbon or DLC is formed only on the bevel portion 202 on both sides of the substrate W. The areas on which the protective film 90 is not formed may be protected by a combination of one or more of the top cover 40, bottom cover 50, stage 20, and resist film described above. When the protective film 90 is formed only on the bevel portion 202, for example, the top cover 40 described above can be used to shield the center portion 300 and the edge portion 201 from plasma.

[0044] FIG. 13C illustrates a case where a protective film 90 consisting of multiple layers, including an amorphous carbon or DLC film, is formed on the edge portion 201 and the bevel portion 202 of both sides of the substrate. In this example, the protective film 90 includes a first layer 90A formed on the substrate W and a second layer 90B formed on the first layer 90A. As an example of each layer, the first layer 90A may be a SiC film, and the second layer 90B may be an amorphous carbon or DLC film. For example, if the material of the substrate W or the surface of the substrate W is silicon (Si), a SiC layer may be formed on the silicon as the first layer 90A, and then an amorphous carbon or DLC film may be formed as the second layer 90B. This SiC layer can be formed by methods such as chemical vapor deposition (CVD) or epitaxial growth. The amorphous carbon or DLC film can be formed, for example, by the plasma deposition method described above. The areas where the protective film 90 is not formed may be protected by a combination of one or more of the top cover 40, bottom cover 50, stage 20, and resist film described above. The protective film 90 may be composed of three or more layers. When the protective film 90 is composed of multiple layers, it is preferable that at least the outermost layer be formed of a film that is resistant to etching and has high hardness, such as an amorphous carbon or DLC film. The protective film in any of the embodiments may be composed of multiple layers, and in this case, it is preferable that at least the outermost layer be formed of a film that is resistant to etching and has high hardness, such as an amorphous carbon or DLC film.

[0045] 13D shows an example in which a protective film 90 including an amorphous carbon or DLC film is formed on the edge portion 201 and bevel portion 202 on one side of the substrate W. In this example, the protective film 90 is formed on the upper surface of the substrate W. Note that the boundary between the upper and lower surfaces of the substrate W in the bevel portion 202 can be, for example, half the thickness of the substrate W. In this example, the protective film 90 may also be formed from multiple layers, as in FIG. 13C. The areas on which the protective film 90 is not formed may be protected by a combination of one or more of the top cover 40, bottom cover 50, stage 20, and resist film formation described above.

[0046] 13E shows an example in which a protective film 90 including an amorphous carbon or DLC film is formed only on the bevel portion 202 on one surface of the substrate W. In this example, the protective film 90 may be formed of multiple layers, as in the case of FIG. 13C. The area on which the protective film 90 is not formed may be protected by a combination of one or more of the top cover 40, bottom cover 50, stage 20, and resist film described above.

[0047] The substrate W having a protective film containing amorphous carbon or DLC film formed on the outer periphery of the substrate in this manner can prevent erosion of the outer periphery of the substrate W that may occur during processing steps in the semiconductor manufacturing process. Therefore, by starting the semiconductor manufacturing process using a substrate having a protective film containing amorphous carbon or DLC film on the outer periphery of the substrate, it is possible to protect the outer periphery of the substrate from erosion throughout all steps of the semiconductor manufacturing process.

[0048] The protective film on the outer periphery of the substrate may be peeled off before the substrate dicing step in the semiconductor manufacturing process. Alternatively, the dicing step may be performed without peeling off the protective film on the outer periphery of the substrate. In this case, the protective film peeling step can be omitted.

[0049] The protective film may be formed on the outer periphery of the substrate before a process that requires protection of the outer periphery of the substrate, for example, before an etching process that may erode the outer periphery of the substrate.

[0050] FIG. 14A shows a flowchart of an example of a semiconductor manufacturing process. In this example, a protective film is formed on the outer periphery of the substrate in the first step of the semiconductor manufacturing process, and then subsequent semiconductor manufacturing processes are carried out. First, a protective film 90 including an amorphous carbon or DLC film is formed on part or all of the outer periphery of the substrate in the radial direction (step S11). The protective film 90 includes one or more layers, and it is preferable that at least the outermost layer is an amorphous carbon or DLC film. After a transistor formation step (step S12) and a wiring layer formation step (step S13) are performed on the device formation region of the substrate W, the protective film 90 is peeled off from the substrate W by chemical etching, dry etching, or other methods (step S14). Next, multiple semiconductor devices (semiconductor chips) W are removed from the substrate W by dicing or the like. device The semiconductor manufacturing process (pre-process) is completed by performing processes such as dicing the substrate into individual pieces (step S15). Note that a substrate with a protective film formed on the outer periphery of the substrate (substrate with protective film) may be prepared / purchased, and the semiconductor manufacturing process may be performed on the substrate with protective film.

[0051] FIG. 14B shows a flowchart of another example of a semiconductor manufacturing process. In this example, a protective film is formed on the outer periphery of the substrate in the first step of the semiconductor manufacturing process, and then the subsequent semiconductor manufacturing process is performed. The dicing process is also performed without removing the protective film from the outer periphery of the substrate. A protective film 90 including an amorphous carbon or DLC film is formed on part or all of the outer periphery of the substrate in the radial direction (step S21). The protective film 90 includes one or more layers, and preferably, at least the outermost layer is an amorphous carbon or DLC film. After performing a transistor formation process (step S22) and a wiring layer formation process (step S23) on the device formation region of the substrate W, a dicing process is performed to separate multiple semiconductor devices (semiconductor chips) from the substrate W, completing the semiconductor manufacturing process (pre-process) (steps S24 and S25). In this case, the protective film removal process can be omitted. Alternatively, a substrate with a protective film formed on the outer periphery (protective film-coated substrate) may be prepared / purchased and the semiconductor manufacturing process may be performed on the protective film-coated substrate.

[0052] FIG. 15A shows a flowchart of another example of a semiconductor manufacturing process. In this example, a protective film including amorphous carbon or DLC is formed on the outer periphery of the substrate before the wiring layer formation process, thereby protecting the outer periphery of the substrate from erosion during the wiring layer formation process. Specifically, after the transistor formation process (step S31) in the semiconductor manufacturing process is completed, a protective film 90 including amorphous carbon or DLC is formed on part or all of the outer periphery of the substrate in the radial direction (step S32). The protective film 90 includes one or more layers, and preferably, at least the outermost layer is an amorphous carbon or DLC film. Next, the wiring layer formation process (step S33) is performed on the substrate W after the protective film formation, and the protective film 90 is then peeled off from the substrate W by chemical etching, dry etching, or other methods. The semiconductor manufacturing process (pre-process) is then completed by performing a dicing process to separate multiple semiconductor devices (semiconductor chips) from the substrate W (step S35).

[0053] FIG. 15B shows a flowchart of another example of a semiconductor manufacturing process. In this example, a protective film including amorphous carbon or DLC is formed on the outer periphery of the substrate before the silicon etching process, thereby protecting the outer periphery of the substrate from erosion during the silicon etching process. After completing the transistor formation process (step S41) during the semiconductor manufacturing process, a protective film 90 including amorphous carbon or DLC is formed on part or all of the outer periphery of the substrate in the radial direction (step S42). The protective film 90 includes one or more layers, and preferably, at least the outermost layer is an amorphous carbon or DLC film. Next, the substrate W after the protective film formation is subjected to a silicon etching process (step S43), and then the protective film 90 is peeled off from the substrate W by chemical etching, dry etching, or other methods (step S44). Subsequently, the substrate W is subjected to processes such as a wiring layer formation process (step S45).

[0054] In the examples of FIGS. 15A and 15B, a protective film including amorphous carbon or DLC film is formed on the outer periphery of the substrate before the wiring formation process or the silicon etching process. However, a protective film including amorphous carbon or DLC film may also be formed on the outer periphery of the substrate before other processes.

[0055] According to the above embodiment, by preparing (purchasing) a substrate on which a protective film is formed on part or all of the outer periphery in the radial direction of the substrate and carrying out the semiconductor manufacturing process, it is possible to prevent erosion of the outer periphery of the substrate W that may occur during the processing steps of the semiconductor manufacturing process. Furthermore, by forming a protective film on the outer periphery of the substrate before a process that requires protection of the outer periphery of the substrate, it is possible to prevent erosion of the outer periphery of the substrate W that may occur during that process.

[0056] At least the following technical ideas can be understood from the above embodiment.

[0057] [1] According to one aspect, there is provided a method for forming a protective film on an outer periphery of a substrate, including a bevel portion, using plasma, the method including: placing a substrate having a first surface and a second surface facing each other on a stage smaller than the substrate, the second surface of the substrate being such that the outer periphery of the substrate protrudes from an outer edge of the stage; arranging at least a portion of the circumferential direction of the outer periphery of the substrate facing an electrode; contacting the first surface of the substrate with a first shielding structure that separates the outer periphery from an area inside the first surface and / or contacting the second surface of the substrate with a second shielding structure that separates the outer periphery from an area inside the second surface; and supplying a film formation gas between the outer periphery of the substrate and the electrode to form a protective film on the outer periphery of the substrate. According to this aspect, a protective film can be formed on the outer periphery of the substrate while the first shielding structure and / or the second shielding structure physically shield the first and / or second surfaces of the substrate except for the outer periphery (central portion). Because a plasma generation region (periphery) and a non-plasma generation region (center) on the substrate are separated by a physical structure, a decrease in film thickness and a decrease in adhesion at the inner boundary of the protective film can be suppressed or prevented. For example, the region surrounded by a first shielding structure, an electrode, and a stage or a second shielding structure is defined as the plasma generation region, and a protective film can be formed on the outer periphery of the substrate while the first shielding structure and the stage or the second shielding structure shield the substrate except for the outer periphery (center). Because a plasma generation region (periphery) and a non-plasma generation region (center) on the substrate are separated by a physical structure, a decrease in film thickness and a decrease in adhesion at the inner boundary of the protective film can be suppressed or prevented. Alternatively, the first shielding structure on the first surface of the substrate may be omitted, and a second shielding structure may be provided only on the second surface of the substrate, thereby suppressing or preventing a decrease in film thickness and a decrease in adhesion at the inner boundary of the protective film on the second surface. In this case, it is possible to suppress or prevent a decrease in the film thickness and a decrease in adhesion at least at the inner boundary portion of the protective film on the second surface of the substrate, thereby improving the quality of the protective film.

[0058] [2] According to one embodiment, the method includes a step of bringing the first shielding structure into contact with the first surface of the substrate, wherein the first shielding structure has a contact portion that contacts the substrate and a hollow portion that is provided inside the contact portion and forms a shielded space together with the substrate, and the region inside the outer periphery of the substrate is accommodated within the hollow portion. According to this embodiment, since the inner portion (center portion) of the outer periphery of the substrate can be accommodated within the hollow portion, the device formation region of the substrate can be protected without contacting the first shielding structure, and deterioration of the device formation region can be suppressed or prevented.

[0059] [3] According to one embodiment, the first shielding structure has a cylindrical portion that contacts the substrate and a lid portion that closes one end of the cylindrical portion, and the other end of the cylindrical portion contacts the substrate. According to this embodiment, the first shielding structure can be formed with a simple configuration.

[0060] [4] According to one embodiment, the lid portion extends to the outside of the cylindrical portion, and the film formation gas is supplied between the outer periphery of the substrate and the electrode through a plurality of gas supply holes arranged in the lid portion outside the cylindrical portion along the outer periphery of the substrate. With this embodiment, the film formation gas can be uniformly supplied to a plasma generation region (a region surrounded by a first shielding structure, an electrode, and a stage or a second shielding structure) with a simple configuration.

[0061] [5] According to one embodiment, the film formation gas is supplied to the gas supply holes through a buffer chamber provided on the outside of the lid and communicating with the gas supply holes. By supplying the film formation gas to the gas supply holes through the buffer chamber, the gas can be supplied uniformly to each gas supply hole, thereby enabling the film formation gas to be supplied uniformly throughout the entire circumferential direction of the plasma generation region.

[0062] [6] According to one embodiment, the lid extends to the outside of the cylindrical portion, and the film formation gas is supplied between the outer periphery of the substrate and the electrode through a porous body arranged in a ring shape outside the cylindrical portion so as to penetrate the lid. With this embodiment, the film formation gas can be uniformly supplied to a plasma generation region (a region surrounded by a first shielding structure, an electrode, and a stage or a second shielding structure) with a simple configuration.

[0063] [7] According to one embodiment, the film formation gas is supplied to the porous body through a buffer chamber provided outside the lid and communicating with the porous body. By supplying the film formation gas to the annular porous body through the buffer chamber, the gas can be supplied uniformly over the entire circumferential direction of the annular porous body, thereby enabling the film formation gas to be supplied uniformly over the entire circumferential direction of the plasma generation region.

[0064] [8] According to one embodiment, the lid extends to the outside of the cylindrical portion, and the film formation gas is supplied between the lid and the electrode outside the cylindrical portion. After the film formation gas collides with the cylindrical portion, it is supplied between the outer periphery of the substrate and the electrode. According to this embodiment, the film formation gas flows perpendicular to the cylindrical portion of the first shielding structure and hits the cylindrical portion once, thereby improving the uniformity of the film formation gas. Furthermore, the film formation gas can be uniformly supplied to the plasma generation region (the region surrounded by the first shielding structure, the electrode, and the stage or the second shielding structure) without forming a gas supply hole or a porous flow path in the first shielding structure. This simplifies the structure of the first shielding structure.

[0065] [9] According to one embodiment, the film formation gas is supplied from the side of the substrate between the outer periphery of the substrate and the electrode through one or more gas supply holes provided in the electrode. According to this embodiment, by supplying the film formation gas to the plasma generation region from the lateral direction through the gas supply holes provided in the electrode, the film formation gas can be supplied uniformly throughout the plasma generation region. Furthermore, since the film formation gas can be supplied uniformly to the plasma generation region without forming gas supply holes or porous flow paths in the first shielding structure, the structure of the first shielding structure can be simplified.

[0066]

[10] According to one embodiment, the electrode is provided with a plurality of gas supply holes, and the film formation gas is supplied to the plurality of gas supply holes via a buffer chamber that is provided on the outside of the electrode and communicates with the plurality of gas supply holes. According to this embodiment, by supplying the film formation gas to the plurality of gas supply holes of the electrode via the buffer chamber, the gas can be supplied uniformly to each gas supply hole, thereby making it possible to supply the film formation gas uniformly over the entire circumferential direction of the plasma generation region.

[0067]

[11] According to one embodiment, the region surrounded by the first shielding structure, the stage, and the electrode is defined as a plasma generation region. According to this embodiment, the stage is used as part of the structure that separates the plasma generation region, so that the shielding structure can be omitted on one side of the substrate. That is, the second shielding structure can be omitted on the second side of the substrate.

[0068]

[12] According to one embodiment, a region surrounded by the first shielding structure, the second shielding structure, and the electrode is defined as a plasma generation region. This embodiment allows for more flexible design of structures that separate the plasma generation region on each surface of the substrate.

[0069]

[13] According to one embodiment, the electrode is divided into an upper electrode and a lower electrode, and the substrate is placed on the stage with the upper electrode and the lower electrode separated from each other, and after the substrate is placed, the upper electrode and the lower electrode are brought together. According to this embodiment, when an electrode is provided around the entire periphery of the substrate, the substrate can be easily installed and removed.

[0070]

[14] In one embodiment, the stage is connected to a ground potential, a negative potential, or a positive potential. This configuration applies a ground potential, a negative potential, or a positive potential to the outer periphery of the substrate on which the protective film is formed, allowing negative / positive charges to accumulate on the outer periphery of the substrate, making it easier to attract positive / negative ions in the film-forming gas. This facilitates the formation of the protective film.

[0071]

[15] According to one aspect, a first conductor disposed on the outer periphery of the stage so as to be in electrical contact with the outer periphery of the substrate or the inside of the outer periphery is connected to a ground potential, a negative potential, or a positive potential. With this aspect, the ground potential, a negative potential, or a positive potential can be efficiently applied to the outer periphery of the substrate on which the protective film is formed.

[0072]

[16] According to one embodiment, at least a portion of the first shielding structure and / or the second shielding structure that contacts the substrate is a conductor, and the conductor portion of the first shielding structure and / or the second shielding structure is connected to a ground potential, a negative potential, or a positive potential. According to this embodiment, the first shielding structure and / or the second shielding structure that contacts the boundary between the periphery and the center of the substrate can be used to efficiently apply a ground potential, a negative potential, or a positive potential to the periphery of the substrate on which a protective film is formed. There is no need to provide a separate conductor for applying a potential to the periphery of the substrate.

[0073]

[17] According to one aspect, the method includes a step of bringing the second shielding structure into contact with the second surface of the substrate, the second shielding structure being in contact with the second surface of the substrate outside the stage. This aspect allows for more flexible design of a structure that separates a plasma generation region on the second surface of the substrate.

[0074]

[18] According to one embodiment, a protective film is formed on the outer periphery of the substrate while the substrate is being rotated. This embodiment allows a film formation gas to be supplied more uniformly along the entire circumferential direction of the plasma generation region, and allows the film formation gas and plasma to come into contact with the outer periphery of the substrate more uniformly along the entire circumferential direction. This allows a protective film to be formed more uniformly along the entire periphery of the substrate.

[0075]

[19] According to one embodiment, in a cross section along the radial direction of the substrate, the electrode has a shape and arrangement such that the distance between the outer periphery of the substrate and the electrode is constant throughout the film formation region of the substrate. The electrode has, for example, an arc-shaped cross-sectional shape. According to this embodiment, since the distance between the electrode and the outer periphery of the substrate is constant throughout the film formation region, a protective film with a uniform thickness can be formed throughout the entire outer periphery of the substrate.

[0076]

[20] According to one embodiment, the electrodes are disposed continuously or intermittently around the entire periphery of the outer periphery of the substrate. According to this embodiment, since the electrodes are disposed around the entire circumferential direction of the outer periphery of the substrate, a constant distance can be stably maintained between the electrodes and the outer periphery of the substrate, thereby further improving the uniformity of the film thickness of the protective film.

[0077]

[21] According to one embodiment, the electrode is disposed on a portion of the outer periphery of the substrate in the circumferential direction, and the protective film is formed on the entire outer periphery of the substrate in the circumferential direction by rotating the substrate. According to this embodiment, since the electrode is disposed on a portion of the outer periphery of the substrate in the circumferential direction, the electrode configuration is easy.

[0078]

[22] According to one aspect, the protective film includes at least one of an insulating film, a dielectric film, a conductor film, and an organic film. The protective film may include a plurality of layers of different types. According to this aspect, it is possible to form a variety of protective films suitable for protecting the outer periphery of the substrate in substrate processing after the protective film formation.

[0079]

[23] According to one embodiment, the protective film includes a layer made of amorphous carbon or diamond-like carbon. According to this embodiment, amorphous carbon or DLC (diamond-like carbon), which is favorable in terms of etching resistance and hardness, is used for the protective film (or at least the outermost layer in the case of a multi-layer structure), thereby making it possible to adequately protect the outer periphery of the substrate in substrate processing after the protective film is formed.

[0080]

[24] According to one aspect, there is provided a substrate processing apparatus for depositing a protective film on an outer periphery of a substrate, including a bevel portion, using plasma, the substrate processing apparatus comprising: a stage smaller than the dimensions of the substrate, on which the second of first and second opposing surfaces of the substrate is placed so that the outer periphery of the substrate protrudes from an outer edge of the stage; an electrode disposed on the outer periphery of the substrate, the electrode facing at least a portion of the circumferential direction of the outer periphery of the substrate; a first shielding structure in contact with the first surface of the substrate and separating the outer periphery of the substrate from an inner region thereof, and / or a second shielding structure in contact with the second surface of the substrate and separating the outer periphery of the substrate from an inner region thereof; and a gas supply device for supplying a film formation gas between the outer periphery of the substrate and the electrode. According to this aspect, a protective film can be formed on the outer periphery of the substrate while the first shielding structure and / or the second shielding structure physically shield the first and / or second surfaces of the substrate other than the outer periphery (central portion). Because a plasma generation region (periphery) and a non-plasma generation region (center) on the substrate are separated by a physical structure, a decrease in film thickness and a decrease in adhesion at the inner boundary of the protective film can be suppressed or prevented. For example, the region surrounded by a first shielding structure, an electrode, and a stage or a second shielding structure is defined as the plasma generation region, and a protective film can be formed on the outer periphery of the substrate while the first shielding structure and the stage or the second shielding structure shield the substrate except for the outer periphery (center). Because a plasma generation region (periphery) and a non-plasma generation region (center) on the substrate are separated by a physical structure, a decrease in film thickness and a decrease in adhesion at the inner boundary of the protective film can be suppressed or prevented. Alternatively, the first shielding structure on the first surface of the substrate may be omitted, and a second shielding structure may be provided only on the second surface of the substrate, thereby suppressing or preventing a decrease in film thickness and a decrease in adhesion at the inner boundary of the protective film on the second surface. In this case, it is possible to suppress or prevent a decrease in the film thickness and a decrease in adhesion at least at the inner boundary portion of the protective film on the second surface of the substrate, thereby improving the quality of the protective film.

[0081]

[25] According to one embodiment, a substrate is provided in which a protective film is formed on the outer periphery of the substrate, the protective film having one or more layers, and at least the outermost layer of the one or more layers is an amorphous carbon or diamond-like carbon (DLC) film. When the protective film is a single layer, the entire protective film is the outermost layer and is an amorphous carbon or DLC film. A portion of the outer periphery in the substrate radial direction, i.e., at least one of the edge portion and the bevel portion, may be covered with the protective film. According to this embodiment, by covering the outer periphery of the substrate with an amorphous carbon or DLC film that is etch-resistant and highly hard, the outer periphery of the substrate can be protected from erosion during semiconductor manufacturing processes.

[0082]

[26] According to one embodiment, the protective film includes a plurality of layers, and at least the outermost layer of the plurality of layers is an amorphous carbon or DLC film. According to this embodiment, by forming the protective film from a plurality of layers, for example, by forming one or more base films on the substrate and then forming the amorphous carbon or DLC film thereon, it is possible to improve the adhesion of the amorphous carbon or DLC film to the substrate.

[0083]

[27] According to one embodiment, the protective film includes a first layer and a second layer formed on the first layer, and the second layer is an amorphous carbon or DLC film. According to this embodiment, the protective film is configured with two layers, and the second layer, which is the outermost layer, is an amorphous carbon or DLC film, thereby achieving the above-mentioned effects.

[0084]

[28] According to one embodiment, the substrate is a silicon substrate, and the first layer is a SiC film. By forming a SiC film on the silicon substrate as a base film, it is possible to improve adhesion of the amorphous carbon or DLC film to the substrate.

[0085]

[29] According to one embodiment, the protective film is formed only on the bevel portion of the substrate. According to this embodiment, when it is particularly necessary to protect the bevel portion of the substrate, or when it is sufficient to protect the bevel portion, it is possible to reduce the area where the protective film is formed.

[0086]

[30] According to one embodiment, the protective film is formed only on the bevel portion on one side of the substrate. This embodiment allows the area where the protective film is formed to be reduced when it is necessary to particularly protect the bevel portion on one side of the substrate (e.g., the side on which a device formation region is located) or when it is sufficient to protect the bevel portion on one side of the substrate.

[0087] Although embodiments of the present invention have been described above based on several examples, the above-described embodiments of the invention are intended to facilitate understanding of the present invention and are not intended to limit the present invention. The present invention may be modified and improved without departing from its spirit, and of course, the present invention includes equivalents thereof. Furthermore, any combination or omission of the components described in the claims and specification is possible to the extent that at least part of the above-described problems can be solved or at least part of the effects can be achieved. This application claims priority based on Japanese Patent Application No. 2023-090817, filed June 1, 2023. The entire disclosure of Japanese Patent Application No. 2023-090817, filed June 1, 2023, including the specification, claims, drawings, and abstract, is incorporated herein by reference in its entirety. The entire disclosures of Japanese Patent No. 3949941 (Patent Document 1), Japanese Patent No. 5982383 (Patent Document 2), and Japanese Patent Laid-Open Publication No. 2020-021931 (Patent Document 3), including the specifications, claims, drawings, and abstracts, are incorporated herein by reference.

[0088] REFERENCE SIGNS LIST 10 Housing 11 Plasma chamber 12 Actuator 13 Drive shaft 14 Magnetic fluid seal 20 Stage 22 Conductor 30 Buffer chamber 31 Supply port 40 Top cover 41 Lid portion 41A Flange portion 42 Cylindrical portion 42A Insulator 43 Gas supply hole 44 Porous body 50 Bottom cover 50A Insulator 60 Electrode 60A Upper electrode 60B Lower electrode 61 Gas supply hole 62 Insulator 70 Film formation gas 71 Plasma generation region 72 Non-plasma generation region 81 Nozzle 82 Buffer chamber 83 Gas supply pipe 90 Protective film 90A First layer 90B Second layer 100 Substrate processing apparatus 110 RF power supply 111 DC power supply 120 Line sensor 121 Irradiation region 200 Outer periphery 201 Edge portion 202 Bevel portion 300 Center portion

Claims

1. A method for forming a protective film on an outer periphery including a bevel portion of a substrate using plasma, comprising: placing a second surface of a substrate having first and second surfaces opposing each other on a stage smaller than the dimensions of the substrate such that the outer periphery of the substrate protrudes from the outer edge of the stage; bringing at least a portion of the circumferential direction of the outer periphery of the substrate into opposition with an electrode; contacting the first surface of the substrate with a first shielding structure that separates the outer periphery from an area inside it, and / or contacting the second surface of the substrate with a second shielding structure that separates the outer periphery from an area inside it; and supplying a film formation gas between the outer periphery of the substrate and the electrode to form a protective film on the outer periphery of the substrate.

2. A method according to claim 1, comprising a step of contacting the first shielding structure with the first surface of the substrate, the first shielding structure having a contact portion that contacts the substrate and a hollow portion that is provided inside the contact portion and forms a shielded space together with the substrate, and the area inside the outer periphery of the substrate is accommodated within the hollow portion.

3. A method according to claim 2, wherein the first shielding structure has a cylindrical portion that contacts the substrate and a lid portion that closes one end of the cylindrical portion, and the other end of the cylindrical portion is brought into contact with the substrate.

4. A method according to claim 3, wherein the lid portion extends to the outside of the cylindrical portion, and the film forming gas is supplied between the outer periphery of the substrate and the electrode through a plurality of gas supply holes arranged in the lid portion outside the cylindrical portion along the outer periphery of the substrate.

5. The method according to claim 4, wherein the film forming gas is supplied to the plurality of gas supply holes via a buffer chamber communicating with the plurality of gas supply holes provided on the outside of the lid portion.

6. A method according to claim 3, wherein the lid portion extends to the outside of the cylindrical portion, and the film forming gas is supplied between the outer periphery of the substrate and the electrode through a porous body arranged in a ring shape so as to penetrate the lid portion outside the cylindrical portion.

7. The method according to claim 6, wherein the film forming gas is supplied to the porous body through a buffer chamber provided on the outside of the lid portion and communicating with the porous body.

8. A method according to claim 3, wherein the lid portion extends to the outside of the cylindrical portion, and the film-forming gas is supplied between the lid portion and the electrode outside the cylindrical portion, and the film-forming gas is supplied between the outer periphery of the substrate and the electrode after colliding with the cylindrical portion.

9. A method according to claim 1, wherein the film forming gas is supplied between the outer periphery of the substrate and the electrode from the side of the substrate through one or more gas supply holes provided in the electrode.

10. A method according to claim 9, wherein the electrode is provided with a plurality of gas supply holes, and the film forming gas is supplied to the plurality of gas supply holes via a buffer chamber communicating with the plurality of gas supply holes provided on the outside of the electrode.

11. The method according to any one of claims 1 to 10, wherein a region surrounded by the first shielding structure, the stage, and the electrode is a plasma generation region.

12. The method according to any one of claims 1 to 10, wherein a region surrounded by the first shielding structure, the second shielding structure, and the electrode is a plasma generation region.

13. A method according to any one of claims 1 to 10, wherein the electrode is divided into an upper electrode and a lower electrode, the substrate is placed on the stage with the upper electrode and the lower electrode separated from each other, and after the substrate is placed, the upper electrode and the lower electrode are aligned.

14. A method according to any one of claims 1 to 10, wherein the stage is connected to ground potential, negative potential or positive potential.

15. A method according to any one of claims 1 to 10, further comprising connecting a first conductor arranged at the outer periphery of the stage so as to be in electrical contact with the outer periphery of the substrate or the inside of the outer periphery to a ground potential, a negative potential or a positive potential.

16. A method according to any one of claims 1 to 10, wherein at least a portion of the first shielding structure and / or the second shielding structure that contacts the substrate is conductive, and the conductive portion of the first shielding structure and / or the second shielding structure is connected to ground potential, negative potential or positive potential.

17. A method according to any one of claims 1 to 10, comprising the step of contacting the second surface of the substrate with the second shielding structure, the second shielding structure contacting the second surface of the substrate outside the stage.

18. The method according to any one of claims 1 to 10, wherein a protective film is formed on the outer periphery of the substrate while rotating the substrate.

19. A method according to any one of claims 1 to 10, wherein, in a cross section along the radial direction of the substrate, the electrode has a shape and arrangement such that the distance between the outer periphery of the substrate and the electrode is constant over the entire deposition area of ​​the substrate.

20. The method according to any one of claims 1 to 10, wherein the electrodes are disposed continuously or intermittently around the entire periphery of the outer periphery of the substrate.

21. A method according to any one of claims 1 to 10, wherein the electrode is disposed on a portion of the circumferential direction of the outer periphery of the substrate, and the protective film is formed on the entire circumferential direction of the outer periphery of the substrate by rotating the substrate.

22. The method according to any one of claims 1 to 10, wherein the protective film includes at least one of an insulating film, a dielectric film, a conductor film, or an organic film.

23. The method of claim 22, wherein the protective film comprises a layer of amorphous carbon or diamond-like carbon.

24. A substrate processing apparatus for depositing a protective film on an outer periphery including a bevel portion of a substrate using plasma, comprising: a stage smaller than the dimensions of the substrate, on which the second surface of a first and second opposing surfaces of the substrate is placed such that the outer periphery of the substrate protrudes from an outer edge of the stage; an electrode disposed on the outer periphery of the substrate, the electrode facing at least a portion of the circumferential direction of the outer periphery of the substrate; a first shielding structure in contact with the first surface of the substrate and separating the outer periphery of the substrate from an inner region thereof, and / or a second shielding structure in contact with the second surface of the substrate and separating the outer periphery of the substrate from an inner region thereof; and a gas supply device for supplying a film formation gas between the outer periphery of the substrate and the electrode.

25. A substrate, comprising a protective film formed on an outer periphery of the substrate, the protective film having one or more layers, and at least the outermost layer of the one or more layers being an amorphous carbon or diamond-like carbon (DLC) film.

26. The substrate according to claim 25, wherein the protective film includes a plurality of layers, and at least the outermost layer of the plurality of layers is an amorphous carbon or DLC film.

27. The substrate according to claim 26, wherein the protective film includes a first layer and a second layer formed on the first layer, the second layer being an amorphous carbon or DLC film.

28. The substrate of claim 27, wherein the substrate is a silicon substrate and the first layer is a SiC film.

29. The substrate according to any one of claims 25 to 28, wherein the protective film is formed only on the bevel portion of the substrate.

30. The substrate according to claim 29, wherein the protective film is formed only on a bevel portion on one side of the substrate.

Citation Information

Patent Citations

  • Semiconductor production device and semiconductor device

    JP1994283500A

  • Method and Apparatus for Forming Thin Films in Near Edge Regions of Semiconductor Substrates During Processing

    JP2005524235A

  • Method and apparatus for manufacturing semiconductor

    JP2007115834A

  • Method for producing curved crystal and curved crystal

    JP2014009131A

  • Bevel protective film deposition method

    JP2014503986A