Solar cell and photovoltaic module thereof

By combining a light-trapping textured surface and a tower-based structure on the silicon substrate side surface of the solar cell, the problem of poor etching of the coating was solved, improving light-harvesting efficiency and film integrity, and enhancing the electrical performance and stability of the solar cell.

WO2026233348A1PCT designated stage Publication Date: 2026-11-12TONGWEI SOLAR ENERGY (CHENGDU) CO LID
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2026/095137
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-09
Filing Date
2026-05-07
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

During the etching process of the coating layer of solar cells, poor etching is prone to occur, which may lead to leakage or reduce the power generation area of ​​the PN junction, affecting energy conversion efficiency and long-term stability.

Method used

By setting a combination of a light-trapping textured surface structure and a tower base structure on the side surface of a silicon substrate, and controlling the ratio of the height of the first region to the height of the side surface to be between 10% ≤ h1/H ≤ 99%, only the wrap-around coating of the first region is removed while the wrap-around coating of the second region is retained, thus forming a light-trapping textured surface structure and a tower base structure.

Benefits of technology

It improves the efficiency of light capture and utilization, enhances the light trapping effect of solar cells, protects the integrity of functional film layers, reduces the risk of leakage, and improves the energy conversion efficiency and long-term reliability of solar cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2026095137_12112026_PF_FP_ABST
    Figure CN2026095137_12112026_PF_FP_ABST
Patent Text Reader

Abstract

Disclosed in the present invention are a solar cell and a photovoltaic module thereof. The solar cell comprises a silicon substrate and a functional film layer arranged on a surface of the silicon substrate; the silicon substrate comprises a light-receiving surface, a back surface located on a side facing away from the light-receiving surface, and a side surface arranged between the light-receiving surface and the back surface; the side surface comprises a first region close to the light-receiving surface and a second region close to the back surface, wherein the light-receiving surface and the first region have light-trapping textured structures, and the second region has a pyramid-base structure; the functional film layer is arranged on a side of the back surface. The present invention can better solve the problem that is prone to occur during etching of a wrap-around coating, thereby improving the electrical performance of the solar cell.
Need to check novelty before this filing date? Find Prior Art

Description

A solar cell and its photovoltaic module Technical Field

[0001] This invention relates to the field of solar cells, and more particularly to a solar cell and its photovoltaic module. Background Technology

[0002] Currently, during the etching process to remove the coating layer from the surface of the silicon substrate in solar cells, there are often cases of poor etching, such as over-etching or no etching in some areas. This can lead to leakage or a reduction in the PN junction power generation area of ​​the solar cell after texturing, which has an adverse effect on the energy conversion efficiency and long-term stability of the solar cell. Summary of the Invention

[0003] To better address the etching defects that are prone to occur during the etching process around the coating, this invention provides a solar cell and its photovoltaic module.

[0004] In a first aspect, embodiments of the present invention provide a solar cell.

[0005] A solar cell includes a silicon substrate and a functional film layer disposed on the surface of the silicon substrate. The silicon substrate includes a light-receiving surface, a backlighting surface located on the opposite side of the light-receiving surface, and a side surface disposed between the light-receiving surface and the backlighting surface. The side surface includes a first region near the light-receiving surface and a second region near the backlighting surface. The light-receiving surface and the first region have a light-trapping textured surface structure, and the second region has a tower base structure. The functional film layer is disposed on the backlighting surface.

[0006] As an optional implementation, in an embodiment of the present invention, along the height direction of the silicon substrate, the height of the first region is h1, the height of the side surface is H, and the ratio of h1 to H is 10% ≤ h1 / H ≤ 99%.

[0007] As an optional implementation, in the embodiments of the present invention, the light-trapping velvet structure is pyramidal, pyramid-like, or wormhole-like.

[0008] As an optional implementation, in an embodiment of the present invention, the direction perpendicular to the height direction is taken as the horizontal direction, and in the horizontal direction, the surface of the first region is lower than the surface of the second region.

[0009] As an optional implementation, in an embodiment of the present invention, the depth difference D between the second region and the first region in the horizontal direction is 1 μm. <D≤8μm。

[0010] As an optional implementation, in an embodiment of the present invention, along the height direction, the first region includes a third region adjacent to the second region; the third region is a mixture of a light-trapping textured surface structure and a tower base structure.

[0011] As an optional implementation, in an embodiment of the present invention, the height of the second region is h2, and the ratio of h2 to the height H of the side surface is 1% ≤ h2 / H ≤ 90%.

[0012] As an optional implementation, in an embodiment of the present invention, the height of the third region is h3, and the ratio of h3 to the height H of the side surface is 1% ≤ h3 / H ≤ 40%.

[0013] As an optional implementation, in an embodiment of the present invention, the functional film layer includes an N-type conductive film layer and a P-type conductive film layer, which are distributed in an interdigitated manner on the surface of the silicon substrate.

[0014] As an optional implementation, in an embodiment of the present invention, a first dielectric layer is further disposed between the P-type conductive film layer and the silicon substrate, and a second dielectric layer is further disposed between the N-type conductive film layer and the silicon substrate.

[0015] As an optional implementation, in an embodiment of the present invention, the solar cell further includes a first electrode and a second electrode, wherein the second electrode forms an ohmic contact with the N-type conductive film layer, and the first electrode forms an ohmic contact with the P-type conductive film layer.

[0016] As an optional implementation, in an embodiment of the present invention, the solar cell further includes a first passivation film layer, which is disposed on the side of the functional film layer away from the silicon substrate. The first passivation film layer includes one or more of a first aluminum oxide layer, a first silicon nitride layer, and a first silicon oxide layer.

[0017] As an optional implementation, in an embodiment of the present invention, the solar cell further includes a second passivation film layer, which is disposed on the light-receiving side of the silicon substrate. The second passivation film layer includes one or more of a second aluminum oxide layer, a second silicon nitride layer, and a second silicon oxide layer.

[0018] As an optional implementation, in an embodiment of the present invention, the solar cell further includes a coating layer disposed in the second region.

[0019] In a second aspect, embodiments of the present invention provide a photovoltaic module, including the solar cell as described in the first aspect.

[0020] Compared with related technologies, the beneficial effects of the present invention are as follows:

[0021] This invention provides a solar cell that further improves energy conversion efficiency and long-term reliability by structurally configuring the side surface of the silicon substrate. Specifically, the side surface of the silicon substrate includes two regions: a first region is close to the light-receiving surface and is given a light-trapping textured structure along with the light-receiving surface, while the second region is close to the back-lighting surface and retains its original tower-based structure. From the surface structure characteristics of the aforementioned regions of the silicon substrate's side surface, it can be seen that when removing the wrap-around coating, only the wrap-around coating in the first region is removed, while the wrap-around coating in the second region is retained to a certain extent. This allows the first region to form a light-trapping textured structure, while the second region retains its tower-based structure.

[0022] Because this invention, based on the light-trapping textured surface structure on the light-receiving surface, also forms a light-trapping textured surface structure in the first region of the side surface, this further enhances the light-trapping effect of the solar cell, thereby improving the light capture and utilization efficiency. More importantly, the height h1 of the first region has a significant impact on the leakage characteristics and photoelectric conversion efficiency of the solar cell. Therefore, this application also controls the ratio between the height h1 of the first region and the height H of the side surface to be between 10% ≤ h1 / H ≤ 99%. This ratio control not only ensures that the coating on the surface of the first region is fully removed, allowing the first region to form a light-trapping textured surface structure during the texturing process after decoating, but also allows the coating on the second region to be partially retained. This effectively maintains the integrity of the functional film layer, prevents damage or deformation of the functional film layer in subsequent processes, and ensures the long-term reliability of the cell. During the texturing process, the coating on the surface of the second region reacts with the solution, achieving partial or complete removal, effectively reducing its thickness and retaining the original tower base structure, further reducing leakage problems that may be caused by the coating, thereby further improving the electrical performance of the solar cell. Attached Figure Description

[0023] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0024] Figure 1 is a schematic diagram of the structure of the solar cell disclosed in an embodiment of the present invention;

[0025] Figure 2 is a schematic diagram of the surface structure of the silicon substrate disclosed in an embodiment of the present invention;

[0026] Figure 3 is a SEM image of the side surface of the silicon substrate disclosed in an embodiment of the present invention;

[0027] Figure 4 is a schematic diagram of the structure of another solar cell disclosed in an embodiment of the present invention;

[0028] Figure 5 is a SEM image of the side surface of the polished silicon substrate disclosed in an embodiment of the present invention;

[0029] Figure 6 is a schematic diagram of the solar cell structure after the functional film layer is prepared, as disclosed in an embodiment of the present invention.

[0030] Figure 7 is a schematic diagram of the solar cell structure after laser patterning, as disclosed in an embodiment of the present invention.

[0031] Figure 8 is a schematic diagram of the solar cell structure after decoating, as disclosed in an embodiment of the present invention.

[0032] Figure 9 is a schematic diagram of the structure of a solar cell after texturing, as disclosed in an embodiment of the present invention.

[0033] Icons: 1. Silicon substrate; 11. Light-receiving surface; 12. Backlight-receiving surface; 13. Side surface; 131. First region; 1311. Third region; 132. Second region; 2. Functional film layer; 21. P-type conductive film layer; 22. N-type conductive film layer; 31. First dielectric layer; 32. Second dielectric layer; 4. First passivation film layer; 5. Second passivation film layer; 61. First electrode; 62. Second electrode; 7. Wrap-around plating layer; 71a. P-type conductive wrap-around plating layer; 71b. First dielectric wrap-around plating layer; 71c. First mask wrap-around plating layer; 72a. N-type conductive wrap-around plating layer; 72b. Second dielectric wrap-around plating layer; 72c. Second mask wrap-around plating layer; 81. First mask layer; 82. Second mask layer. Detailed Implementation

[0034] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0035] In this invention, the terms "upper," "lower," "left," "right," "front," "rear," "top," "bottom," "inner," "outer," "middle," "vertical," "horizontal," "lateral," and "longitudinal" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. These terms are primarily for the purpose of better describing the invention and its embodiments, and are not intended to limit the indicated devices, elements, or components to having a specific orientation, or to be constructed and operated in a specific orientation.

[0036] Furthermore, in addition to indicating direction or positional relationship, some of the aforementioned terms may also have other meanings. For example, the term "above" may also be used in certain situations to indicate a dependency or connection. Those skilled in the art can understand the specific meaning of these terms in this invention based on the specific circumstances.

[0037] Furthermore, the terms "installation," "setup," "equipped with," "connection," and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral structure; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium, or an internal connection between two devices, components, or parts. Those skilled in the art can understand the specific meaning of these terms in this invention based on the specific circumstances.

[0038] Furthermore, the terms "first," "second," etc., are primarily used to distinguish different devices, elements, or components (which may be the same or different in specific type and construction), and are not intended to indicate or imply the relative importance or quantity of the indicated devices, elements, or components. Unless otherwise stated, "a plurality of" means two or more.

[0039] Etching with etching solutions is an important method for removing the coating layer on the surface of a silicon substrate. During the etching process, the silicon substrate is laid flat on a roller immersed in the etching solution, with the light-receiving side of the silicon substrate facing down and in contact with the etching solution for etching. The back side of the silicon substrate is usually covered with a mask layer, and a water film is covered on the mask layer (the water film is uniformly covered by the surface tension of water) as a protective layer.

[0040] Currently, solar cells are prone to significant leakage or impaired electrical performance after etching. This is because if the coating layer on the silicon substrate side surface is not completely removed during the etching process, this coating layer can easily become a recombination center for photogenerated carriers, manifesting as blackening at the edges of the solar cell in EL testing. Conversely, if the coating layer on the silicon substrate side surface is excessively removed, it can damage the functional film layer on the back side, compromising its integrity and reducing the area available for forming the effective power generation region, thereby lowering the solar cell's photoelectric conversion efficiency. Therefore, effectively addressing the problems caused by the coating layer is a challenge for improving the energy conversion efficiency of solar cells.

[0041] To address the aforementioned challenges in the removal of the coating process, this invention provides a solar cell and its photovoltaic module.

[0042] The technical solution of the present invention will be further described below with reference to the embodiments and accompanying drawings.

[0043] In a first aspect, embodiments of the present invention provide a solar cell.

[0044] Referring to Figures 1 and 2, Figure 1 is a schematic diagram of the structure of a solar cell disclosed in an embodiment of the present invention, and Figure 2 is a schematic diagram of the surface structure of a silicon substrate disclosed in an embodiment of the present invention. An embodiment of the present invention discloses a solar cell comprising a silicon substrate 1 and a functional film layer 2 disposed on the surface of the silicon substrate 1. The silicon substrate 1 includes a light-receiving surface 11, a backlighting surface 12 located on the opposite side of the light-receiving surface 11, and a side surface 13 disposed between the light-receiving surface 11 and the backlighting surface 12.

[0045] The side surface 13 includes a first region 131 near the light-receiving surface 11 and a second region 132 near the backlight surface 12, wherein the light-receiving surface 11 and the first region 131 have a light-trapping textured surface structure, the second region 132 has a tower base structure, and the functional film layer 2 is disposed on one side of the backlight surface 12.

[0046] Along the height direction of the silicon substrate 1 (i.e., the X direction shown in Figure 1), the height of the first region 131 is h1, and the height of the side surface 13 is H, with the ratio of h1 to H being 10% ≤ h1 / H ≤ 99%.

[0047] This invention achieves further improvement in the energy conversion efficiency and long-term reliability of solar cells by structurally configuring the side surface 13 of the silicon substrate 1. Specifically, the side surface 13 of the silicon substrate 1 includes two regions: a first region 131 is close to the light-receiving surface 11 and is given a light-trapping textured structure together with the light-receiving surface 11, while the second region 132 is close to the back-lighting surface 12 and retains its original tower base structure. As can be seen from the surface structure characteristics of the above-mentioned regions of the side surface 13 of the silicon substrate 1, when the wrap-around coating 7 is removed, only the wrap-around coating 7 of the first region 131 is removed, while the wrap-around coating 7 of the second region 132 is retained to a certain extent. This allows the first region 131 to form a light-trapping textured structure, while the second region 132 can maintain its tower base structure.

[0048] Since the present invention has a light-trapping textured surface structure on the light-receiving surface 11, and the first region 131 of the side surface 13 also forms a light-trapping textured surface structure, this further enhances the light-trapping effect of the solar cell, thereby improving the light capture and utilization efficiency. More importantly, the height h1 of the first region 131 has a significant impact on the leakage characteristics and photoelectric conversion efficiency of the solar cell. Therefore, preferably, this application controls the ratio between the height h1 of the first region 131 and the height H of the side surface 13 to be between 10% ≤ h1 / H ≤ 99%. This proportional control not only ensures that the coating 7 on the surface of the first region 131 is fully removed, so that the first region 131 forms a light-trapping textured surface structure in the texturing process after the coating removal, but also allows the coating 7 on the second region 132 to be partially retained. This can effectively maintain the integrity of the functional film layer 2 on the backlight surface, prevent damage or deformation of the functional film layer 2 in subsequent processes, and ensure the long-term reliability of the battery. In addition, it can also ensure the maximization of the area of ​​the functional film layer 2 on the backlight surface, thereby maximizing the effective functional film layer area for generating photogenerated carriers in the solar cell and improving the conversion efficiency of the solar cell.

[0049] For example, the ratio of h1 to H is 50%, 60%, 75%, 82%, 87%, or 90%. Preferably, the value of h1 / H is between 30% ≤ h1 / H ≤ 80%. This height ratio allows for larger process operation errors, has lower requirements for equipment precision, and helps to reduce process costs.

[0050] It should be noted that H is the arithmetic mean of the heights of the four side surfaces 13 (front, back, left, and right) of the silicon substrate 1 at their midpoints. Figure 3 is a SEM image of the side surfaces of the silicon substrate disclosed in an embodiment of the present invention. As shown in Figure 3, one of the side surfaces 13 of the silicon substrate 1 is shown, and the height of this side surface 13 is marked as H.

[0051] The second region 132 is the area on the side surface 13 with continuous tower base structural features. The extent of the second region 132 is defined as follows: geometric midlines parallel to the height direction are selected as observation reference lines on the four side surfaces 13 (front, back, left, and right) of the silicon substrate 1. As shown in Figure 3, the observation reference line of the side surface 13 is the dashed line A;

[0052] Visually inspect along the observation baseline from the shaded side 12 to the illuminated side 11. When the continuity of the tower base structure is first interrupted and a light-trapping textured area (such as wormhole-like or pyramid-like) appears, mark the location with a dashed line a1 perpendicular to the dashed line A. Record the height of the dashed line a1 relative to the shaded side and define the arithmetic mean of the heights of the second region 132 measured from the side surfaces 13 in the four directions as h2.

[0053] The first region 131 is a region with a light-trapping textured surface, which is the region on the side surface 13 other than the second region 132. Subtracting H from h2 gives the height of h1.

[0054] As shown in Figure 3, unlike the light-trapping textured surface structure formed on the surface of the first region 131, the tower base structure on the surface of the second region 132 has higher flatness, and its morphological characteristics are consistent with the tower base structure of the backlight surface of the silicon substrate. For example, the tower base structure is a block tower base with a square groove structure or a near-square groove structure.

[0055] Furthermore, the ratio of h2 to H is 1% ≤ h2 / H ≤ 90%.

[0056] By controlling the height h2 of the second region 132, the integrity of the functional film layer 2 can be better guaranteed, further reducing the risk of over-etching during the removal of the coating layer 7.

[0057] For example, the ratio of h2 to H is 2%, 8%, 15%, 26%, 35%, or 48%. Preferably, the value of h2 / H is between 20% ≤ h2 / H ≤ 45%.

[0058] By further adjusting the values ​​of h1 / H and h2 / H within the above-mentioned preferred range, it is possible to better remove the coating layer 7, enhance the light trapping effect, reduce the possibility of leakage, and more effectively ensure the structural integrity of the functional film layer 2 on the backlight surface. This ensures the maximization of the area of ​​the functional film layer 2 on the backlight surface, thereby maximizing the effective functional film layer area used to generate photogenerated carriers in the solar cell and maximizing the conversion efficiency of the solar cell.

[0059] In some embodiments, the light-trapping textured surface is pyramidal, pyramid-like, or wormhole-like.

[0060] After texturing in the fabrication of solar cells, the light-receiving surface 11 and the first region 131 are prone to forming light-trapping textured structures such as pyramids, pyramid-like structures, or wormholes. These light-trapping textured structures can better improve the light-trapping effect and increase the utilization rate of light.

[0061] Referring to Figures 1 and 2, in some embodiments, the horizontal direction is defined as the direction perpendicular to the height direction (i.e., the Y direction shown in Figure 1), and in the horizontal direction, the surface of the first region 131 is lower than the surface of the second region 132.

[0062] During the removal of the coating 7, after the coating 7 in the first region 131 is removed, the coating 7 in the second region 132 is not yet removed. This step results in a height difference between the second region 132 and the first region 131, with the first region 131 being lower than the second region 132. This height difference is retained after the solar cell fabrication is completed.

[0063] Referring to Figure 2, in some embodiments, the depth difference D between the second region 132 and the first region 131 in the depth direction is 1 μm. <D≤8μm。

[0064] By controlling the depth difference D between the second region 132 and the first region 131 to less than or equal to 8 μm, the etching effect of the side surface 13 is effectively optimized. This prevents leakage problems caused by insufficient etching depth and avoids performance loss of the silicon substrate 1 due to excessive etching. By precisely controlling the etching depth within a reasonable range, the yield of the finished battery is significantly improved.

[0065] It should be noted that the surface of the first region 131 has a pyramidal textured surface with varying heights, as shown in Figure 2. The depth difference D between the second region 132 and the first region 131 is the difference in height from the bottom of the pyramid in the first region 131 to the surface of the second region 132 in the horizontal direction. In order to reduce the influence of fluctuations in the test data, the depth difference can be measured at a location near the midpoint of the first region 131.

[0066] Referring to FIG2, in some embodiments, along the height direction, the first region 131 includes a third region 1311 adjacent to the second region 132;

[0067] The third region 1311 contains a mixture of light-trapping velvet structures and tower base structures.

[0068] The first region 131 consists of a velvet region and a transitional third region 1311. The velvet region is a region with a continuous light-trapping velvet structure. The extent of this velvet region is defined as follows:

[0069] Referring to Figure 3, visually inspect along the dashed line A from the light-receiving surface 11 to the backlight surface 12. When the continuity of the light-trapping textured surface structure is first interrupted and a tower base structure area appears, draw a dashed line a2 perpendicular to the dashed line A along that location to mark the position. Record the position height of the dashed line a2 relative to the light-receiving surface, which is the height h2 of the textured surface sub-region.

[0070] The third region 1311 is a region that combines a light-trapping textured surface structure and a tower-based structure. From the light-receiving surface 11 to the backlighting surface 12, the third region 1311 exhibits a mixed morphology transitioning from the textured surface structure to the tower-based structure. In some embodiments, the height of the third region 1311 along the height direction is h3. The height h3 of the third region is obtained by subtracting the heights h1 and h2 from H, and the ratio of h3 to H is 1% ≤ h3 / H ≤ 40%.

[0071] Due to errors such as silicon wafer wobble that may occur during the etching process, the height of the third region 1311 fluctuates within a certain range. Controlling the height of the third region 1311 within this range can better reduce the impact of errors caused by factors such as silicon wafer wobble and improve the energy conversion efficiency of solar cells.

[0072] For example, the ratio of h3 to H is 2%, 8%, 15%, 26%, 35%, or 40%. Preferably, the value of h3 / H is between 1% ≤ h3 / H ≤ 40%.

[0073] Referring back to Figure 1, in some embodiments, the functional film layer 2 includes a P-type conductive film layer 21 and an N-type conductive film layer 22, which are distributed in an interdigitated manner on the back surface 12 of the silicon substrate 1.

[0074] On the back surface 12 of the silicon substrate 1, N-type conductive film layer 22 and P-type conductive film layer 21 are specifically distributed, and electrodes are correspondingly disposed on the back surface 12 and connected to the corresponding N-type conductive film layer 22 and P-type conductive film layer 21, respectively. This design allows the light-receiving surface 11 of the solar cell to be fully exposed without being blocked by the electrodes, thereby greatly improving the light utilization efficiency. However, during the fabrication process, the overlay phenomenon of N-type conductive film layer 22 and P-type conductive film layer 21 will form a relatively thick overlay layer 7 on the light-receiving surface 11 and the side surface 13. The removal effect of this overlay layer 7 has a significant impact on the performance of the solar cell.

[0075] The present invention forms a light-trapping textured surface structure in the first region 131 without the surrounding coating 7, further enhancing the capture and utilization rate of incident light in the first region 131 of the side surface 13. Simultaneously, the present invention forms a base structure identical to that of the backlight surface 12 in the second region 132, ensuring that the texturing solution avoids adverse corrosion to the film structure on the backlight surface 12 during the formation of the light-trapping textured surface structure on the light-receiving surface 11. In other words, the second region 132 provides a buffer protection for the film structure on the backlight surface during wet etching with the texturing solution, ensuring the structural integrity of the N-type conductive film layer 22 and the P-type conductive film layer 21 on the backlight surface 12, and reducing the adverse effects on the solar cell caused by structural damage to the N-type conductive film layer 22 and the P-type conductive film layer 21. Therefore, the present invention is particularly suitable for solar cell structure designs where the N-type conductive film layer 22 and the P-type conductive film layer 21 are distributed in an interdigital pattern on the backlight surface 12 of the silicon substrate 1.

[0076] For example, the P-type conductive film layer 21 is a P-type doped polysilicon layer, and the N-type conductive film layer 22 is an N-type doped polysilicon layer.

[0077] Referring to Figure 4, in some embodiments, a first dielectric layer 31 is further disposed between the P-type conductive film layer 21 and the silicon substrate 1, and a second dielectric layer 32 is further disposed between the N-type conductive film layer 22 and the silicon substrate 1; and / or,

[0078] The solar cell also includes a first electrode 61 and a second electrode 62. The second electrode 62 forms an ohmic contact with the N-type conductive film layer 22, and the first electrode 61 forms an ohmic contact with the P-type conductive film layer 21.

[0079] The solar cell also includes a first passivation film layer 4, which is disposed on the side of the functional film layer 2 away from the silicon substrate 1. The first passivation film layer 4 includes one or more of a first silicon nitride layer, a first silicon oxynitride layer, and a first silicon oxide layer.

[0080] The solar cell also includes a second passivation film layer 5, which is disposed on the light-receiving surface 11 side of the silicon substrate 1. The second passivation film layer 5 includes one or more of a second aluminum oxide layer, a second silicon nitride layer, a second silicon oxynitride layer, and a second silicon oxide layer.

[0081] The materials of the first dielectric layer 31 and the second dielectric layer 32 may include at least one of various dielectric materials, such as silicon oxide, magnesium fluoride, amorphous silicon, polycrystalline silicon, silicon carbide, silicon nitride, silicon oxynitride, aluminum oxide, or titanium oxide. Specifically, the first dielectric layer 31 and the second dielectric layer 32 may be composed of a silicon oxide layer containing silicon oxide. This is because the silicon oxide layer has excellent passivation properties, which can minimize the recombination loss of minority carriers on the surface of the silicon substrate 1, and is a thin film with excellent durability for subsequent high-temperature processes.

[0082] To better provide interface passivation for the silicon substrate 1, the thickness of the first dielectric layer 31 and the second dielectric layer 32 can be 0.5 nm to 3 nm. For example, the thickness of the dielectric layer can be 0.5 nm, 0.8 nm, 1 nm, 1.5 nm, 2 nm, 3 nm, etc. However, the present invention is not limited to this, and the thickness of the first dielectric layer 31 and the second dielectric layer 32 can be various values.

[0083] Preferably, the first passivation film layer 4 is a first aluminum oxide layer, a first silicon nitride layer, a first silicon oxynitride layer and a first silicon oxide layer stacked sequentially, wherein the thickness of the first aluminum oxide layer is 2nm to 8nm, the thickness of the first silicon nitride layer is 10nm to 60nm, the thickness of the first silicon oxynitride layer is 10nm to 60nm, and the thickness of the first silicon oxide layer is 10nm to 60nm.

[0084] Preferably, the second passivation film layer 5 is a second aluminum oxide layer, a second silicon nitride layer, a second silicon oxynitride layer and a second silicon oxide layer stacked sequentially, wherein the thickness of the second aluminum oxide layer is 2nm to 8nm, the thickness of the second silicon nitride layer is 10nm to 60nm, the thickness of the second silicon oxynitride layer is 10nm to 60nm, and the thickness of the second silicon oxide layer is 10nm to 60nm.

[0085] Secondly, embodiments of the present invention provide a method for preparing a solar cell.

[0086] A method for fabricating a solar cell, as mentioned in the first aspect, includes the following steps:

[0087] Polishing: The silicon substrate 1 is polished on both sides to form a blocky tower base structure on the side surface 13. The morphology of the side surface 13 after polishing is shown in Figure 5.

[0088] Preparation of functional film layer 2: Functional film layer 2 is prepared on the back light surface 12 of silicon substrate 1, and functional film layer 2 forms a coating layer 7 on the side surface 13 and the light-receiving surface 11 of silicon substrate 1. The structure of functional film layer 2 after preparation is shown in Figures 6 and 7. The preparation of functional film layer 2 will be further explained later.

[0089] De-coating: Etch the coating layer 7 to remove the coating layer 7 located on the light-receiving surface 11 and the first region 131, and retain the coating layer 7 located in the second region 132. The structure after the de-coating process is shown in Figure 8.

[0090] Texturing process: The silicon substrate 1 after de-coating is texturized so that the light-receiving surface 11 and the first region 131 have a light-trapping textured surface structure, and the second region 132 has a tower base structure. The structure after texturing process is shown in Figure 9.

[0091] In the decoating stage, the light-receiving surface 11 of the silicon substrate 1 with the functional film layer 2 is oriented towards the etching solution and etched in contact with the etching solution. The etching solution removes the coating layer 7 from the light-receiving surface 11 and the first region 131 of the silicon substrate 1, while the coating layer 7 remains on the surface of the second region 132. In the texturing stage, the light-receiving surface 11 and the silicon substrate 1 in the first region 131 react with the texturing solution to form a light-trapping textured surface structure that facilitates light capture. At the same time, the texturing solution also reacts with the coating layer 7 retained in the second region 132 to partially or completely remove the coating layer 7 in the second region 132, thereby forming a tower-based structure on the surface of the second region 132.

[0092] This invention controls the height ratio of the first region 131 within a specific range, which not only ensures that the coating 7 of the first region 131 is fully removed during the removal of the coating, so that the first region 131 forms a light-trapping textured surface structure, which better enhances the light-trapping effect and improves the light utilization rate; but also ensures that the area of ​​the functional film layer 2 on the backlight surface is maximized, thereby maximizing the area of ​​the effective functional film layer used to generate photogenerated carriers in the solar cell, and maximizing the conversion efficiency of the solar cell.

[0093] Furthermore, when the height ratio of the first region 131 increases to a certain range, it indicates that the area ratio control of the light-trapping textured structure of the side surface 13 and the textured area of ​​the light-receiving surface 11 plays a crucial role in suppressing leakage current and improving the conversion efficiency of solar cells. Since the light-receiving surface 11 of the silicon wafer (i.e., the silicon substrate 1) faces the etching solution and is transported by rollers carrying the solution, wet etching of the light-receiving surface of the silicon wafer is achieved during the transport process. However, the power for roller transport is mechanical equipment. For silicon wafers with a thickness of only 100μm to 150μm, the wet etching of its side surface by rollers carrying the solution will inevitably be limited by the transport accuracy of the mechanical equipment. The transmission of the silicon wafer causes slight mechanical vibrations, which in turn affects the proportion of the height h1 of the first region 131 to the height H of the side surface 13. Therefore, this application reduces the impact of the roller mechanical transmission device by controlling the ratio of h1 to H to be 10% ≤ h1 / H ≤ 99%. The light-trapping textured structure in the first region 131 provides short-circuit current gain, and the tower base structure in the second region 132 ensures that the area of ​​the functional film layer 2 on the back side is maximized, thereby maximizing the conversion efficiency of the solar cell. This achieves the best industrialization balance between the first region 131 with the light-trapping textured structure and the second region 132 with the tower base structure.

[0094] Furthermore, after forming the structure shown in Figure 9, the first passivation film layer 4, the second passivation film layer 5, the first electrode 61 and the first electrode 61 are prepared, and a solar cell as shown in Figure 1 or Figure 4 is obtained.

[0095] Referring to FIG6, in some embodiments, the functional film layer 2 includes an N-type conductive film layer 22 and a P-type conductive film layer 21;

[0096] The winding coating 7 includes an N-type conductive winding sub-layer 72a formed by preparing an N-type conductive film layer 22 and a P-type conductive winding sub-layer 71a formed by preparing a P-type conductive film layer 21. The N-type conductive winding sub-layer 72a and the P-type conductive winding sub-layer 71a are stacked.

[0097] For example, the N-type conductive film layer 22 can be an N-type phosphorus-doped polycrystalline silicon layer, and the P-type conductive film layer 21 can be a P-type boron-doped polycrystalline silicon layer.

[0098] Referring to FIG6, in some embodiments, a first dielectric layer 31 is further disposed between the P-type conductive film layer 21 and the silicon substrate 1, and a second dielectric layer 32 is further disposed between the N-type conductive film layer 22 and the silicon substrate 1.

[0099] The coating 7 further includes a first dielectric layer 71b formed by preparing the first dielectric layer 31 and a second dielectric layer 72b formed by preparing the second dielectric layer 32. The first dielectric layer 71b is located on the surface of the P-type conductive layer 71a near the silicon substrate 1, and the second dielectric layer 72b is located on the surface of the N-type conductive layer 72a near the silicon substrate 1; and / or,

[0100] A first mask layer 81 is also prepared on the surface of the P-type conductive film layer 21 away from the silicon substrate 1, and a second mask layer 82 is also prepared on the surface of the N-type conductive film layer 22 away from the silicon substrate 1.

[0101] The coating layer 7 also includes a first mask-around coating layer 71c formed by preparing a first mask layer 81 and a second mask-around coating layer 72c formed by preparing a second mask layer 82. The first mask-around coating layer 71c is located on the surface of the P-type conductive coating layer 71a away from the silicon substrate 1, and the second mask-around coating layer 72c is located on the surface of the N-type conductive coating layer 72a away from the silicon substrate 1.

[0102] For example, when the P-type conductive film layer 21 is prepared first and the N-type conductive film layer 22 is prepared later, the surrounding plating layer 7 sequentially includes a first dielectric surrounding plating layer 71b, a P-type conductive surrounding plating layer 71a, a first mask surrounding plating layer 71c, a second dielectric surrounding plating layer 72b, an N-type conductive surrounding plating layer 72a, and a first mask surrounding plating layer 72c. After the N-type conductive film layer 22 is deposited, the structure shown in FIG. 6 is sequentially formed on the back surface 12 of the silicon substrate 1. Before removing the surrounding plating layer 7, laser patterning is performed to remove part of the second mask layer 82, forming the structure shown in FIG. 7.

[0103] In some embodiments, the etching solution includes at least HF and HNO3, with the concentration of HF being 2.5 wt% to 25 wt% and the concentration of HNO3 being 5 wt% to 35 wt%.

[0104] By controlling the concentration of the etching solution, the surface tension of the etching solution can be altered, thereby affecting its spreading behavior on the side surface 13 of the silicon substrate 1. The etching solution with the aforementioned concentration ratio can spread uniformly on the first region 131, which requires precise control, avoiding over-etching or under-etching, thus achieving precise height control of the first region 131. This not only optimizes the etching effect around the coating layer 7 but also enhances the protection of the functional film layer 2, ensuring that the functional film layer 2 is not damaged during the etching process.

[0105] To control the spread of the etching solution on the side surface 13 of the silicon substrate 1, ensuring that the second region 132 and the first region 131 are within an appropriate range and preventing leakage, two methods can be adopted: one is to adjust the concentration of the etching solution, and the other is to control the pump power. These two strategies can be implemented independently or in combination. Through precise control, the etching process can be effectively managed to achieve better processing results. The following is a detailed explanation of these two methods.

[0106] In some embodiments, the etching solution also includes H2SO4, with a concentration of 2wt% to 30wt%.

[0107] Adding sulfuric acid to the etching solution can effectively increase its viscosity and promote the control of its spreading performance on the side surface 13 of the silicon substrate 1. By further adjusting the concentration of sulfuric acid based on the above-mentioned concentration ranges of HF (2.5wt% to 25wt%) and HNO3 (5wt% to 35wt%), the spreading performance of the etching solution in the first region 131 can be controlled more precisely. This not only improves the etching height accuracy of the first region 131, but also enhances the ability to control the etching depth, thereby optimizing the etching quality of the silicon substrate 1 surface and ensuring the high-precision etching requirements of the silicon substrate 1 surface. Specifically, the first mask-around plating layer 71c contains hydrophilic silicon oxide material. When wet etching is performed on the light-receiving surface of the silicon wafer, the hydroxide ions in the solution make the etching solution easier to spread on the surface of the silicon wafer. Therefore, it is necessary to control the composition of the wet etching solution so that a suitable surface tension is formed between the wet etching solution and the first mask-around plating layer 71c on the surface of the silicon wafer. Under the gravity of the water film on the back surface of the silicon wafer and under the action of a specific pump power, the effective components in the wet etching solution are etched only on a portion of the side surface.

[0108] In some embodiments, the decoupling process is performed in a chain acid etching machine, the maximum power of which is S. The pump power used for the decoupling process is 30% to 60% of S. Specifically, the pump power S is 1.5 kW.

[0109] By adjusting the pump power, the spreading height of the etching solution on the side surface 13 of the silicon substrate 1 can be controlled, thereby achieving effective control of the height of the second region 132 and the first region 131.

[0110] By combining the method of adjusting the concentration of the etching solution with the method of controlling the pump power, the height of the second region 132 and the first region 131 can be controlled more stably, significantly reducing the uncertainty and unexpected situations in the adjustment process.

[0111] It should be noted that the pump power output (30%S~60%S) directly affects the circulation efficiency and process stability of the etching solution. When the output power is within this range, the circulation exchange efficiency of the etching solution in the tank reaches 50%~90%. Under the corresponding output power conditions, the etching solution in the tank can be replaced once within 2min~8min, ensuring that the wet etching solution contains a certain amount of active etching components, achieving efficient etching of the coating 7 around the side surface. Under specific pump output power conditions, the fluctuation of the etching solution's spreading height on the side surface of the silicon substrate 1 is controlled within ±5%, thereby effectively avoiding local over-etching or residual defects caused by uneven liquid flow distribution. Furthermore, controlling the pump power output can effectively regulate the fluctuation of the spreading height of the etching solution on the side surface of the silicon substrate 1.

[0112] Thirdly, embodiments of the present invention provide a photovoltaic module.

[0113] A photovoltaic module includes a solar cell as mentioned in the first aspect or a solar cell prepared by the preparation method mentioned in the second aspect.

[0114] The technical solution of the present invention will be further described below with reference to more specific embodiments.

[0115] Example 1

[0116] This invention provides a solar cell, the preparation method of which includes the following steps:

[0117] Provide N-type silicon wafers and polish the backlight and light-receiving surfaces of the N-type silicon wafers;

[0118] A first dielectric layer, a P-type boron-doped polysilicon layer, and a first mask layer were prepared on the back surface of an N-type silicon wafer using low-pressure chemical vapor deposition (LPCVD). The N-type silicon wafer was loaded into an LCVD apparatus, and oxidation was performed at a pressure of 7600 mTorr, an oxygen flow rate of 20000 sccm, and a temperature of 610°C to deposit a first dielectric layer with a thickness of 1.5 nm on the back surface of the N-type silicon wafer.

[0119] Next, the pressure was controlled at 300 mTorr, the silane gas flow rate at 2000 sccm, and the temperature at 610 °C, and an intrinsic amorphous silicon layer with a thickness of 400 nm was deposited.

[0120] Using boron trichloride as the boron source, boron diffusion was carried out by introducing boron trichloride and oxygen at a flow ratio of 1:5 under an environment of 150 mBar and 610℃. Then, the mixture was pushed together at 950℃ to obtain a P-type boron-doped polycrystalline silicon layer with a thickness of 400 nm and a first mask layer with a thickness of 35 nm. After the preparation was completed, a first dielectric layer, a P-type conductive layer, and a first mask layer were sequentially formed on the side surface and the light-receiving surface of the N-type silicon wafer.

[0121] First graphical processing:

[0122] A first mask layer in a certain area is etched by laser to expose the P-type boron-doped polysilicon layer below the laser processing area. The exposed P-type boron-doped polysilicon layer and the N-type silicon wafer below it are etched by KOH solution with a volume fraction of 20% at 75°C, and a groove region with a recess depth of 0.1μm to 10μm is formed on the back surface of the N-type silicon wafer; wherein, the recess depth is the depth of the bottom of the groove relative to the surface of the silicon substrate.

[0123] A second dielectric layer, an N-type phosphorus-doped polycrystalline silicon layer, and a second mask layer were prepared using low-pressure chemical vapor deposition.

[0124] Oxidation was carried out at a controlled pressure of 7600 mTorr, an oxygen flow rate of 20000 sccm, and a temperature of 610°C to deposit a second dielectric layer with a thickness of 1.5 nm on the back surface of an N-type silicon wafer.

[0125] Next, the pressure was controlled at 300 mTorr, the silane gas flow rate at 1500 sccm, and the temperature at 610 °C, and an intrinsic amorphous silicon layer with a thickness of 400 nm was deposited.

[0126] Using phosphorus oxychloride as the phosphorus source, phosphorus oxychloride and oxygen with a flow ratio of 1:5 were introduced at a pressure of 150 mBar and a temperature of 610°C to carry out phosphorus diffusion. Then, the mixture was pushed together at 950°C to obtain an N-type phosphorus-doped polycrystalline silicon layer with a thickness of 400 nm and a second mask layer with a thickness of 35 nm. After the preparation was completed, a second dielectric layer, an N-type conductive layer, and a second mask layer were formed on the surface of the first mask layer.

[0127] Second graphical processing:

[0128] Laser is used to remove the second mask layer on the side of the P-type boron-doped polysilicon layer away from the N-type silicon wafer and a portion of the second mask layer near the side of the groove region, so that an isolation region can be formed between the P-type boron-doped polysilicon layer and the N-type phosphorus-doped polysilicon layer after subsequent texturing.

[0129] Remove the coating: Place the N-type silicon wafer that has undergone the second patterning process on the rollers of the chain acid etching equipment. The chain acid etching equipment is filled with etching solution. In the etching solution, the concentration of HF is 10wt% and the concentration of HNO3 is 20wt%. The light-receiving side of the N-type silicon wafer faces the etching solution downwards, and a layer of water film is laid on the back side. The water tension evenly covers the back side as a protective water film. The pump power is set to 30% of S, so that the etching solution covers the light-receiving side and part of the side surface. Etching takes 200 seconds.

[0130] Next, alkaline texturing is performed. The alkaline solution in the texturing tank reacts with the light-receiving surface of the N-type silicon wafer to form a textured surface. The temperature of the alkaline texturing treatment is 70℃ and the reaction time is 500s. After etching, a light-receiving surface with a pyramid-shaped light-trapping textured surface structure and a first region are formed. The second region forms a tower base structure, and the third region is a hybrid structure that combines the light-trapping textured surface structure and the tower base structure. The height h1 of the first region accounts for 52%, the height h2 of the second region accounts for 48%, and the height h3 of the third region accounts for 39%. A separation region is formed between the N-type phosphorus-doped polycrystalline silicon layer and the P-type boron-doped polycrystalline silicon layer.

[0131] A first electrode and a second electrode are prepared such that the second electrode forms an ohmic contact with an N-type phosphorus-doped polycrystalline silicon layer, and the first electrode forms an ohmic contact with a P-type boron-doped polycrystalline silicon layer.

[0132] The solar cells and photovoltaic modules disclosed in the embodiments of the present invention have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only for the purpose of helping to understand the solar cells and photovoltaic modules of the present invention and their core ideas. At the same time, for those skilled in the art, there will be changes in the specific implementation methods and application scope based on the ideas of the present invention. Therefore, the content of this specification should not be construed as a limitation of the present invention.

Claims

1. A solar cell, characterized in that, The invention includes a silicon substrate and a functional film layer disposed on the surface of the silicon substrate. The silicon substrate includes a light-receiving surface, a back-lighting surface located on the opposite side of the light-receiving surface, and a side surface disposed between the light-receiving surface and the back-lighting surface. The side surface includes a first region near the light-receiving surface and a second region near the backlighting surface, wherein the light-receiving surface and the first region have a light-trapping textured surface structure, the second region has a tower base structure, and the functional film layer is disposed on one side of the backlighting surface.

2. The solar cell according to claim 1, characterized in that, Along the height direction of the silicon substrate, the height of the first region is h1, the height of the side surface is H, and the ratio of h1 to H is 10% ≤ h1 / H ≤ 99%.

3. The solar cell according to any one of claims 1 to 2, characterized in that, The light-trapping velvet structure is pyramidal, pyramid-like, or wormhole-like.

4. The solar cell according to any one of claims 1 to 3, characterized in that, With the direction perpendicular to the height of the silicon substrate as the horizontal direction, the surface of the first region is lower than the surface of the second region in the horizontal direction.

5. The solar cell according to claim 4, characterized in that, In the horizontal direction, the depth difference D between the second region and the first region is 1 μm. <D≤8μm。 6. The solar cell according to any one of claims 1 to 5, characterized in that, Along the height direction of the silicon substrate, the first region includes a third region adjacent to the second region; The third region contains a mixture of the light-trapping velvet structure and the tower base structure.

7. The solar cell according to any one of claims 1 to 6, characterized in that, The height of the second region is h2, and the ratio of h2 to the height H of the side surface is 1% ≤ h2 / H ≤ 90%.

8. The solar cell according to any one of claims 1 to 6, characterized in that, The height of the third region is h3, and the ratio of h3 to the height H of the side surface is 1% ≤ h3 / H ≤ 40%.

9. The solar cell according to any one of claims 1-8, characterized in that, The functional film layer includes an N-type conductive film layer and a P-type conductive film layer, which are distributed in an interdigitated manner on the back surface of the silicon substrate.

10. The solar cell according to claim 9, characterized in that, A first dielectric layer is disposed between the P-type conductive film layer and the silicon substrate, and a second dielectric layer is disposed between the N-type conductive film layer and the silicon substrate.

11. The solar cell according to claim 9 or 10, characterized in that, The solar cell further includes a first electrode and a second electrode, wherein the second electrode forms an ohmic contact with the N-type conductive film layer, and the first electrode forms an ohmic contact with the P-type conductive film layer.

12. The solar cell according to any one of claims 1 to 11, characterized in that, The solar cell further includes a first passivation film layer, which is disposed on the side of the functional film layer away from the silicon substrate. The first passivation film layer includes one or more of a first aluminum oxide layer, a first silicon nitride layer, a first silicon oxynitride layer, and a first silicon oxide layer.

13. The solar cell according to any one of claims 1 to 11, characterized in that, The solar cell further includes a second passivation film layer, which is disposed on the light-receiving side of the silicon substrate. The second passivation film layer is one or more of the following: a second aluminum oxide layer, a second silicon nitride layer, a second silicon oxynitride layer, and a second silicon oxide layer.

14. The solar cell according to any one of claims 1 to 13, characterized in that, The solar cell also includes a wrap-around coating, which is disposed in the second region.

15. A photovoltaic module, characterized in that, Includes the solar cell as described in any one of claims 1 to 14.