A chelating plugging remover and preparation method thereof

By using neutral chelating plug-removing agents in oilfield water injection production, the problems of excessive acidification and equipment corrosion in acidification plug-removing technology are solved, effective plug-removing effects are achieved in low-permeability formations and high-temperature deep wells, and environmental protection is reduced. Influence.

CN116731694BActive Publication Date: 2024-10-29QINGDAO HUIZHI PETROLEUM TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310710898.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-15
Publication Date
2024-10-29
Estimated Expiration
2043-06-15

AI Technical Summary

Technical Problem

Existing acidification and plugging removal technology has problems such as excessive acidification, corrosion inhibitor failure and equipment corrosion in oilfield water injection production. It is particularly ineffective in low-permeability formations and high-temperature deep wells, leading to oil production well blockage and equipment scrapping.

Method used

A neutral chelating deblocking agent is used, which contains chelating solubilizer, chelating dispersant, clay hydration expansion inhibitor, corrosion inhibitor and dispersant. It is composed of biodegradable materials and is suitable for deep deblocking and reducing Base fluid viscosity, enhances permeability and stability, and avoids equipment corrosion.

Benefits of technology

It achieves effective plugging removal in low-permeability formations and high-temperature deep wells, reduces well site operation waste liquid, improves plugging removal effect and equipment safety, meets environmental protection requirements, is easy to biodegrade, and does not affect sewage treatment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116731694B_ABST
    Figure CN116731694B_ABST
Patent Text Reader

Abstract

The present invention relates to a chelating unblocking agent and a preparation method thereof. The chelating unblocking agent comprises the following components in percentage by mass: 10-25% of a chelating solubilizing agent, 5-15% of a chelating dispersant, 0.5-1% of a clay hydration swelling inhibitor, 0.3-1.0% of a corrosion inhibitor, 0.5-1.0% of a dispersant, and the remainder is water. The method comprises: (1) mixing the chelating dispersant with water to obtain a mixed liquid; (2) sequentially adding a chelating solubilizing agent, a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant to the mixed liquid and mixing them to obtain a chelating unblocking agent. The chelating unblocking agent in the present invention is a neutral unblocking material, the main component of the residual liquid is easily biodegradable, does not affect the technical indicators of sewage treatment in a downstream treatment plant, is suitable for deep reservoir unblocking, and has a good unblocking effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of oil and water well blockage removal, and in particular relates to a chelating blockage remover and a preparation method thereof. Background Art

[0002] Many oil fields at home and abroad are troubled by scaling damage to varying degrees during water injection production, especially in the middle and late stages of production. As the water content of oil increases, scaling problems become more common and serious. Due to the scaling of oil field water, oil formation damage occurs, and the wellbore of oil production wells, water injection wells, and oil pumps and equipment systems are blocked, which leads to the premature scrapping of oil wells, oil pumps and equipment. These problems have greatly increased the cost of oil production and seriously affected the normal production of oil and gas. In order to better solve the scaling problem of oil field formations and oil pumps and equipment, and solve the technical problem of scaling damage in oil field water injection production, it is necessary to use unblocking agent products.

[0003] At present, oil fields use acidification, biological and solvent methods to remove plugging, and mainly use acidification to remove plugging. Acidification removes plugging by means of inorganic acids (hydrochloric acid, hydrofluoric acid, and sulfuric acid), or organic acids (formic acid, acetic acid, etc.) can also be used to chemically dissolve formation rocks and blockages, as well as the hydraulic effect of acidification pressure to improve formation permeability and achieve oil well production and water well injection. In order to achieve the goal of acidification engineering, in addition to the main acid, corrosion inhibitors, iron ion stabilizers, etc. need to be added to the acidizing fluid. However, the hydrochloric acid and soil acid used in acidification are strong acids, especially hydrochloric acid reacts very quickly with carbonates, which can easily lead to excessive acidification of the formation near the wellbore, while the deep part cannot be fully acidified. This phenomenon has a greater impact on high-temperature deep wells in low-permeability formations and is the main reason for the failure of acidification. During the acidizing process, the acidizing corrosion inhibitor is easily affected by the formation temperature, pressure and iron ions and becomes ineffective. Once the acidizing corrosion inhibitor fails, it will cause serious corrosion to the oil wells, oil pumps and oil transportation equipment. Therefore, there is a huge potential risk in acidizing and unblocking. Summary of the invention

[0004] In order to solve one or more technical problems existing in the prior art, the present invention provides a chelating plugging remover and a preparation method thereof. The chelating plugging remover in the present invention is a neutral plugging remover material, the main component of the residual liquid is easily biodegradable, does not affect the technical indicators of sewage treatment in the downstream treatment plant, is suitable for deep reservoir plugging removal, and has a good plugging removal effect.

[0005] The present invention provides a chelating plugging remover in a first aspect, which comprises the following components in percentage by mass: 10-25% of a chelating solubilizer, 5-15% of a chelating dispersant, 0.5-1% of a clay hydration swelling inhibitor, 0.5-1% of a corrosion inhibitor, 0.3-1% of a dispersant, and the balance is water.

[0006] Preferably, the chelating solubilizing agent is one or more of sodium polyaspartate, sodium citrate, and aminotriacetic acid.

[0007] Preferably, the chelating dispersant is one or more of tetrasodium iminodisuccinate, trisodium methylglycine diacetate, and tetrasodium glutamate diacetate.

[0008] Preferably, the clay hydration swelling inhibitor is one or more of a quaternary ammonium salt surfactant and potassium chloride; preferably, the quaternary ammonium salt surfactant is one or more of octadecyltrimethylammonium bromide, octadecyltrimethylammonium chloride, heptadecyltrimethylammonium bromide, heptadecyltrimethylammonium chloride, hexadecyltrimethylammonium bromide, hexadecyltrimethylammonium chloride, tetradecyltrimethylammonium bromide, tetradecyltrimethylammonium chloride, dodecyltrimethylammonium chloride, dodecyltrimethylammonium bromide, and dodecyltrimethylammonium chloride.

[0009] Preferably, the corrosion inhibitor is one or more of imidazoline quaternary ammonium salt, rhodin, and Lan-826.

[0010] Preferably, the dispersant is one or more of emulsifier MOA-4, emulsifier OP-10, and emulsifier SP-80.

[0011] Preferably, the chelating plugging remover further comprises 0.5-1% by mass of an adsorption carrier; the adsorption carrier is cellulose and / or gelatin microspheres.

[0012] Preferably, the preparation of the gelatin microspheres comprises the following steps:

[0013] (a) mixing gelatin powder with water to obtain a gelatin aqueous solution; preferably, the gelatin content in the gelatin aqueous solution is 1 to 5% by weight;

[0014] (b) heat treating the gelatin aqueous solution at 50 to 60° C. for 0.5 to 3 h;

[0015] (c) adding the gelatin aqueous solution treated in step (b) dropwise into a coolant to obtain spherical particles; preferably, the coolant is an organic solvent and / or saline; more preferably, the organic solvent is ethanol and / or acetone, and the saline is a sodium chloride aqueous solution and / or a calcium chloride aqueous solution;

[0016] (d) placing the obtained spherical particles in a glutaraldehyde aqueous solution for cross-linking treatment, and then washing and drying to obtain gelatin microspheres.

[0017] The present invention provides in a second aspect a method for preparing the chelating blocking remover according to the first aspect of the present invention, the method comprising the following steps:

[0018] (1) mixing the chelating dispersant with water to obtain a mixed solution;

[0019] (2) Adding a chelating solubilizing agent, a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant to the mixed solution in sequence and mixing them evenly to obtain a chelating plugging remover.

[0020] Preferably, step (1) is: mixing the chelating dispersant and the adsorption carrier evenly with water to obtain a mixed solution.

[0021] Compared with the prior art, the present invention has at least the following beneficial effects:

[0022] (1) The chelating plugging remover of the present invention has a relatively low base liquid viscosity, which can be controlled below 30 mPa·s. The low viscosity provides convenience for mechanical injection during injection and can eliminate equipment hazards and construction difficulties caused by injection difficulties, thereby reducing operational difficulties in use.

[0023] (2) The chelating dispersant contained in the chelating plugging remover of the present invention is one or more of tetrasodium iminodisuccinate, trisodium methylglycine diacetate, and tetrasodium glutamate diacetate, which can form complexes with metal ions such as calcium, magnesium, and iron, so that they lose their binding force on sediments and blockages, thereby promoting their dissolution and dispersion. In addition, adding the chelating dispersant of the present invention to the chelating plugging remover also helps to maintain the uniformity and stability of the chelating plugging remover; the chelating solubilizing agent contained in the chelating plugging remover of the present invention is one or more of sodium polyaspartate, sodium citrate, and aminotriacetic acid, which can form a stronger chelating effect with the metal ions in the sediments and blockages, thereby enhancing the effect of the chelating plugging remover, and can also improve the permeability of the chelating plugging remover, making it easier to penetrate into the sediments and blockages, thereby more effectively removing them; the chelating dispersant used in the present invention matches the chelating solubilizing agent, and can play a synergistic role in the chelating plugging remover, promote the dispersion and dissolution of sediments and blockages, enhance the chelating effect, and improve the permeability of the chelating plugging remover, thereby improving the blockage removal effect.

[0024] (3) The chelating plugging remover in the present invention is a neutral plugging remover material. No backflow is required after the plugging removal construction, which reduces the waste liquid from the well site operation. The components such as tetrasodium iminodisuccinate, trisodium methylglycine diacetate, tetrasodium glutamate diacetate, sodium polyaspartate, sodium citrate or aminotriacetic acid contained in the chelating plugging remover of the present invention are easily degraded by various microorganisms. The main components of the residual liquid are easily biodegradable. Under certain conditions, the degradation rate reaches more than 80% in 48 hours, which does not affect the technical indicators of sewage treatment in the downstream treatment plant, does not cause the COD and total nitrogen values ​​of the terminal water treatment system to increase, does not affect the discharge of sewage treatment, has no impact on the production process, and meets the current environmental protection requirements. The chelating plugging remover in the present invention has a good plugging removal effect and is particularly suitable for unblocking deep water injection wells in reservoirs. It is a new neutral plugging removal material that is easily biodegradable.

[0025] (4) The dispersant contained in the chelating plugging remover of the present invention can effectively increase the solubility of the chelating reactant in water, and has the effect of penetrating and stripping the scale samples of pipelines and tanks, thereby effectively increasing the effect of descaling and unblocking.

[0026] (5) The clay hydration expansion inhibitor contained in the chelating plugging remover of the present invention avoids reservoir damage caused by particle migration and clay expansion during construction; the corrosion inhibitor contained in the chelating plugging remover of the present invention is a temperature-resistant and efficient corrosion inhibitor, which will not cause corrosion to pumping equipment and pipelines during high-temperature construction.

[0027] (6) The chelating plugging remover of the present invention does not need to be removed from the pipe column during the plugging removal construction. The agent and water can be injected at the same time during the whole process without stopping the injection, and the operation process is simple. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a curve diagram showing the relationship between the scaling rate and concentration of calcium carbonate of the chelating plugging remover obtained in Example 1 of the present invention. DETAILED DESCRIPTION

[0029] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0030] In a first aspect, the present invention provides a chelating plugging remover, which comprises the following components in percentage by mass: 10-25% (e.g., 10%, 10.5%, 11%, 11.5%, 12%, 12.5%, 13%, 13.5%, 14%, 14.5%, 15%, 15.5%, 16%, 16.5%, 17%, 17.5%, 18%, 18.5%, 19%, 19.5%, 20%, 20.5%, 21.5%, 22%, 22.5%, 23%, 23.5%, 24%, 24.5% or 25%) of a chelating dispersant, 5-15% (e.g., 5%, 5.5%, 6%, 6.5%, 7%) of a chelating dispersant. , 7.5%, 8%, 8.5%, 9%, 9.5%, 10%, 10.5%, 11%, 11.5%, 12%, 12.5%, 13%, 13.5%, 14%, 14.5% or 15%), clay hydration swelling inhibitor 0.5-1% (for example, 0.5%, 0.6%, 0.7%, 0.8%, 0.9% or 1%), corrosion inhibitor 0.5-1% (for example, 0.5%, 0.6%, 0.7%, 0.8%, 0.9% or 1%), dispersant 0.3-1% (for example, 0.3%, 0.4%, 0.5%, 0.6%, 0.7%, 0.8%, 0.9% or 1%), and the balance is water; in the present invention, the water is, for example, deionized water.

[0031] According to some preferred embodiments, the chelating solubilizing agent is one or more of sodium polyaspartate, sodium citrate, and aminotriacetic acid; in the present invention, the CAS number of the sodium polyaspartate is, for example, 181828-06-8.

[0032] According to some preferred embodiments, the chelating dispersant is one or more of tetrasodium iminodisuccinate, trisodium methylglycine diacetate, and tetrasodium glutamate diacetate; the present invention does not specifically limit the sources of sodium polyaspartate, sodium citrate, aminotriacetic acid, tetrasodium iminodisuccinate, trisodium methylglycine diacetate, and tetrasodium glutamate diacetate, for example, they can be products directly purchased on the market or products synthesized by existing methods.

[0033] The chelating plugging remover in the present invention is a chelating plugging remover for water injection well unblocking and injection enhancement. The chelating dispersant contained in the present invention is one or more of tetrasodium iminodisuccinate, trisodium methylglycine diacetate, and tetrasodium glutamate diacetate, which can form complexes with metal ions such as calcium, magnesium, and iron, so that they lose their binding force on sediments and blockages, thereby promoting their dissolution and dispersion. In addition, adding the chelating dispersant of the present invention to the chelating plugging remover can also help maintain the uniformity and stability of the chelating plugging remover; the chelating solubilizing agent contained in the present invention is sodium polyaspartate One or more of sodium citrate and aminotriacetic acid can form a stronger chelating effect with the metal ions in the sediments and blockages, thereby enhancing the effect of the chelating blockage remover, and can also improve the permeability of the chelating blockage remover, making it easier to penetrate into the sediments and blockages, thereby more effectively removing them; the chelating dispersant used in the present invention is matched with the chelating solubilizing agent, and can play a synergistic promoting role in the chelating blockage remover, promote the dispersion and dissolution of sediments and blockages, enhance the chelating effect, and improve the permeability of the chelating blockage remover, thereby improving the blockage removal effect. The chelating plugging remover in the present invention is a neutral plugging remover material. No backflow is required after plugging removal construction, thereby reducing waste liquid from well site operations. The components such as tetrasodium iminodisuccinate, trisodium methylglycine diacetate, tetrasodium glutamate diacetate, sodium polyaspartate, sodium citrate or aminotriacetic acid contained in the chelating plugging remover in the present invention are easily degraded by various microorganisms. The main components of the residual liquid are easily biodegradable. Under certain conditions, the degradation rate reaches more than 80% in 48 hours, does not affect the technical indicators of sewage treatment in the downstream treatment plant, does not cause the COD and total nitrogen values ​​of the terminal water treatment system to increase, does not affect the discharge of sewage treatment, has no impact on the production process, and meets the current environmental protection requirements. The chelating plugging remover in the present invention has good plugging removal effect, is particularly suitable for deep reservoir plugging removal, and is a new neutral plugging removal material that is easily biodegradable.

[0034] According to some preferred embodiments, the clay hydration and swelling inhibitor is one or more of a quaternary ammonium salt surfactant and potassium chloride; preferably, the quaternary ammonium salt surfactant is one or more of octadecyltrimethylammonium bromide, octadecyltrimethylammonium chloride, heptadecyltrimethylammonium bromide, heptadecyltrimethylammonium chloride, hexadecyltrimethylammonium bromide, hexadecyltrimethylammonium chloride, tetradecyltrimethylammonium bromide, tetradecyltrimethylammonium chloride, dodecyltrimethylammonium chloride, dodecyltrimethylammonium bromide, dodecyltrimethylammonium bromide, and dodecyltrimethylammonium chloride; the clay hydration and swelling inhibitor contained in the chelating plugging remover of the present invention avoids reservoir damage caused by particle migration and clay swelling during construction.

[0035] According to some preferred embodiments, the corrosion inhibitor is one or more of imidazoline quaternary ammonium salt, rhodin, and Lan-826; the present invention does not specifically limit the sources of imidazoline quaternary ammonium salt, rhodin, and Lan-826, for example, they can be products that can be directly purchased on the market or products synthesized by existing methods, for example, the imidazoline quaternary ammonium salt can be imidazoline quaternary ammonium salt CT2-12 and / or benzyl chloride quaternized imidazoline quaternary ammonium salt; the corrosion inhibitor contained in the chelating deblocking agent of the present invention is a temperature-resistant and efficient corrosion inhibitor, which will not cause corrosion to pumping equipment and pipelines during high-temperature construction.

[0036] According to some preferred embodiments, the dispersant is one or more of emulsifier MOA-4, emulsifier OP-10, and emulsifier SP-80; the dispersant contained in the chelating deblocking agent of the present invention can effectively increase the solubility of the chelating reactant in water, has the effect of penetrating and stripping the scale samples of pipelines and tanks, and effectively increases the effect of descaling and deblocking.

[0037] According to some preferred embodiments, the chelating unblocking agent further comprises 0.5-1% (e.g., 0.5%, 0.6%, 0.7%, 0.8%, 0.9% or 1%) of an adsorption carrier in percentage by mass; the adsorption carrier is cellulose and / or gelatin microspheres; in the present invention, the cellulose may be, for example, cellulose nanocrystals; the present invention preferably further adds cellulose and / or gelatin microspheres as adsorption carriers to the chelating unblocking agent, and the cellulose or gelatin microspheres have a large specific surface area and a void structure, which can increase the adsorption capacity of the chelating dispersant and the chelating solubilizing agent, and improve the adsorption and removal effect of the chelating unblocking agent on harmful substances. The present invention uses cellulose or gelatin microspheres as adsorption carriers, which can help fix and stabilize the chelating unblocking agent, prevent the problem of uneven dispersion of the active ingredients in the chelating unblocking agent and reducing the unblocking agent, and is beneficial to improving the unblocking effect and the continuity of unblocking. At the same time, it can also be biodegraded after use, which can ensure the environmental friendliness of the chelating unblocking agent and effectively avoid the pollution of the environment by the chelating unblocking agent.

[0038] The gelatin microspheres in the present invention may be known products in the prior art, but preferably, the gelatin microspheres are obtained through the following steps (a) to (d).

[0039] According to some preferred embodiments, the preparation of the gelatin microspheres comprises the following steps:

[0040] (a) mixing gelatin powder with water to obtain a gelatin aqueous solution; preferably, the gelatin aqueous solution has a mass percentage of 1 to 5% (e.g., 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, 4%, 4.5% or 5%); specifically, for example, adding gelatin powder to an appropriate amount of deionized water, heating to 50 to 60° C. and stirring to fully dissolve the gelatin;

[0041] (b) heat treating the gelatin aqueous solution at 50 to 60° C. (e.g., 50° C., 55° C., or 60° C.) for 0.5 to 3 h (e.g., 0.5, 1, 1.5, 2, 2.5, or 3 h); in the present invention, the heat treatment is carried out under stirring;

[0042] (c) dripping the gelatin aqueous solution treated in step (b) into a coolant to obtain spherical particles; preferably, the coolant is an organic solvent and / or saline; more preferably, the organic solvent is ethanol and / or acetone, and the saline is a sodium chloride aqueous solution and / or a calcium chloride aqueous solution. Preferably, the mass fraction of sodium chloride contained in the sodium chloride aqueous solution is 2-8%, and / or the mass fraction of calcium chloride contained in the calcium chloride aqueous solution is 2-8%; in the present invention, the temperature of the coolant is, for example, 5-10° C., and the dripping speed is, for example, 1-5 drops / second; dripping the heat-treated gelatin aqueous solution into an organic solvent, such as ethanol, acetone, etc., due to the volatility and low surface tension of the organic solvent, the gelatin molecules can be rapidly solidified into spherical particles; dripping the heat-treated gelatin aqueous solution into an aqueous solution (saline) containing salts, such as NaCl, CaCl2, etc., the saline can cause an osmotic pressure difference in water, so that the gelatin molecules can be rapidly solidified into spherical particles;

[0043] (d) placing the obtained spherical particles in a glutaraldehyde aqueous solution for cross-linking treatment, and then washing and drying to obtain gelatin microspheres; in the present invention, the spherical particles are cross-linked with the glutaraldehyde aqueous solution as a cross-linking agent to enhance the stability and heat resistance of the gelatin microspheres, the mass fraction of glutaraldehyde contained in the glutaraldehyde aqueous solution can be, for example, 5-15%, the temperature of the cross-linking treatment can be, for example, 40-60°C, the time of the cross-linking treatment can be, for example, 3-24h, and the mass ratio of the spherical particles to the glutaraldehyde aqueous solution can be, for example, (1-2):100; after the cross-linking treatment, for example, washing can be performed with an organic solvent and / or brine to remove excess cross-linking agent and impurities, and then low-temperature drying is performed in vacuum, for example, vacuum drying at 40°C for 5-24h to obtain the gelatin microspheres.

[0044] The present invention provides in a second aspect a method for preparing the chelating blocking remover according to the first aspect of the present invention, the method comprising the following steps:

[0045] (1) mixing the chelating dispersant with water to obtain a mixed solution;

[0046] (2) Adding a chelating solubilizing agent, a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant to the mixed solution in sequence and mixing them evenly to obtain a chelating plugging remover.

[0047] According to some specific embodiments, the chelating unblocking agent is prepared as follows: at room temperature of 15 to 35° C., a formulated amount of chelating dispersant is uniformly stirred in a formulated amount of water, and then a formulated amount of chelating solubilizing agent is sequentially added while stirring, and finally a formulated amount of clay hydration swelling inhibitor, corrosion inhibitor and dispersant are sequentially added while stirring, and then fully stirred, for example, for 30 to 60 minutes, to obtain the chelating unblocking agent; the present invention does not specifically limit the stirring speed, and those skilled in the art can select it according to needs, for example, it can be 100 to 800 r / min.

[0048] According to some preferred embodiments, step (1) is: mixing the chelating dispersant and the adsorption carrier with water to obtain a mixed solution; for example, stirring the formulated amount of the chelating dispersant and the adsorption carrier in the formulated amount of water at a temperature of 40 to 60° C. The present invention does not specifically limit the stirring time, and those skilled in the art can select it as needed. The stirring time can be, for example, 1 to 8 hours.

[0049] The present invention will be further described below by way of examples, but the protection scope of the present invention is not limited to these embodiments. The present invention may also have other various embodiments, and those skilled in the art may make various corresponding changes and deformations according to the present invention without departing from the spirit and essence of the present invention, but these corresponding changes and deformations shall all belong to the protection scope of the claims attached to the present invention.

[0050] Example 1

[0051] The present embodiment provides a chelating plugging remover and a preparation method thereof. The chelating plugging remover is composed of the following components in percentage by mass: 20% chelating solubilizer, 12% chelating dispersant, 1% clay hydration swelling inhibitor, 1% corrosion inhibitor, 0.3% dispersant, and 65.7% deionized water; the chelating solubilizer is sodium polyaspartate, the chelating dispersant is trisodium methylglycine diacetate, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is rhodin, and the dispersant is emulsifier OP-10.

[0052] The chelating plugging remover is prepared as follows: at room temperature of 25° C., a formulated amount of chelating dispersant is dissolved in a formulated amount of deionized water and stirred evenly, then a formulated amount of chelating solubilizing agent is sequentially added while stirring, and finally a formulated amount of clay hydration swelling inhibitor, corrosion inhibitor and dispersant are sequentially added while stirring and stirred for 30 minutes to obtain the chelating plugging remover.

[0053] Example 2

[0054] Embodiment 2 is substantially the same as Embodiment 1, except that:

[0055] In this embodiment, the chelating solubilizing agent is sodium citrate, the chelating dispersant is tetrasodium iminodisuccinate, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is imidazoline quaternary ammonium salt, and the dispersant is emulsifier MOA-4.

[0056] Example 3

[0057] Embodiment 3 is substantially the same as Embodiment 1, except that:

[0058] In this embodiment, the chelating solubilizing agent is aminotriacetic acid, the chelating dispersant is tetrasodium glutamate diacetate, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is Lan-826, and the dispersant is emulsifier SP-80.

[0059] Example 4

[0060] The present embodiment provides a chelating plugging remover and a preparation method thereof. The chelating plugging remover is composed of components measured by mass percentage: 20% chelating solubilizer, 12% chelating dispersant, 1% adsorption carrier, 1% clay hydration swelling inhibitor, 1% corrosion inhibitor, 0.3% dispersant, and 64.7% deionized water; the chelating solubilizer is sodium polyaspartate, the chelating dispersant is trisodium methylglycine diacetate, the adsorption carrier is cellulose nanocrystals, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is rhodin, and the dispersant is emulsifier OP-10.

[0061] The chelating plugging remover is prepared as follows: at a temperature of 60° C., a formulated amount of a chelating dispersant and an adsorption carrier (cellulose nanocrystal) are uniformly stirred in a formulated amount of deionized water, and then a formulated amount of a chelating solubilizing agent is sequentially added while stirring, and finally, a formulated amount of a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant are sequentially added while stirring and fully stirred for 30 minutes to obtain the chelating plugging remover.

[0062] Example 5

[0063] The present embodiment provides a chelating plugging remover and a preparation method thereof. The chelating plugging remover is composed of components measured by mass percentage: 20% chelating solubilizer, 12% chelating dispersant, 1% adsorption carrier, 1% clay hydration swelling inhibitor, 1% corrosion inhibitor, 0.3% dispersant, and 64.7% deionized water; the chelating solubilizer is sodium polyaspartate, the chelating dispersant is trisodium methylglycine diacetate, the adsorption carrier is gelatin microspheres, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is rhodin, and the dispersant is emulsifier OP-10.

[0064] The chelating plugging remover is prepared as follows: at a temperature of 50° C., a chelating dispersant and an adsorption carrier (gelatin microspheres) in a formula amount of deionized water are stirred uniformly, and then a chelating solubilizing agent in a formula amount is sequentially added while stirring, and finally, a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant in a formula amount are sequentially added while stirring, and the mixture is fully stirred for 30 minutes to obtain the chelating plugging remover;

[0065] The preparation of gelatin microspheres in this example is as follows:

[0066] (a) stirring and mixing gelatin powder with deionized water at 50° C. to obtain a gelatin aqueous solution; the gelatin aqueous solution has a gelatin content of 2% by mass; and the stirring speed is 200 r / min;

[0067] (b) heat treating the gelatin aqueous solution at 50° C. for 1.5 h with stirring at a speed of 200 r / min;

[0068] (c) adding the gelatin aqueous solution treated in step (b) dropwise into ethanol at a temperature of 10° C. to obtain spherical particles at a rate of 1 drop / second;

[0069] (d) placing the obtained spherical particles in a glutaraldehyde aqueous solution at 40°C for cross-linking treatment for 5 hours, washing them with ethanol for multiple times after the cross-linking treatment, and then vacuum drying them at 40°C for 8 hours to obtain gelatin microspheres; the mass fraction of glutaraldehyde contained in the glutaraldehyde aqueous solution is 8%, and the mass ratio of the spherical particles to the glutaraldehyde aqueous solution is 2:100.

[0070] Comparative Example 1

[0071] The comparative example provides a chelating plugging remover and a preparation method thereof. The chelating plugging remover is composed of the following components in percentage by mass: 32% chelating solubilizer, 1% clay hydration swelling inhibitor, 1% corrosion inhibitor, 0.3% dispersant, and 65.7% deionized water; the chelating solubilizer is sodium polyaspartate, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is rhodin, and the dispersant is emulsifier OP-10.

[0072] The chelating plugging remover is prepared as follows: at room temperature of 25° C., a formulated amount of chelating solubilizing agent is dissolved in a formulated amount of deionized water and stirred evenly, and then the formulated amounts of clay hydration swelling inhibitor, corrosion inhibitor and dispersant are added in sequence while stirring, and then stirred for 30 minutes to obtain the chelating plugging remover.

[0073] Comparative Example 2

[0074] The comparative example provides a chelating plugging remover and a preparation method thereof. The chelating plugging remover is composed of the following components in percentage by mass: 32% chelating dispersant, 1% clay hydration swelling inhibitor, 1% corrosion inhibitor, 0.3% dispersant, and 65.7% deionized water; the chelating dispersant is trisodium methylglycine diacetate, the clay hydration swelling inhibitor is hexadecyltrimethylammonium chloride, the corrosion inhibitor is rhodin, and the dispersant is emulsifier OP-10.

[0075] The chelating plugging remover is prepared as follows: at room temperature of 25° C., a formulated amount of chelating dispersant is dissolved in a formulated amount of deionized water and stirred evenly, and then the formulated amounts of clay hydration swelling inhibitor, corrosion inhibitor and dispersant are sequentially added while stirring, and then stirred for 30 minutes to obtain the chelating plugging remover.

[0076] Comparative Example 3

[0077] Comparative Example 3 is substantially the same as Example 1, except that:

[0078] The chelating dispersant in this comparative example is aminotri(methylenephosphonic acid).

[0079] Comparative Example 4

[0080] Comparative Example 4 is substantially the same as Example 1, except that:

[0081] The chelating solubilizing agent in Comparative Example 4 is sodium gluconate.

[0082] The present invention uses the chelating plugging removers in Examples 1 to 5 and Comparative Examples 1 to 4 to carry out dissolution tests on calcium carbonate and magnesium carbonate, respectively, and the scale dissolution rate results are shown in Table 1.

[0083] The method for the dissolution test of the present invention is: weigh a certain amount of chelating plugging remover and mix it evenly with distilled water to obtain a chelating plugging remover aqueous solution with a concentration of 5wt%, then add 2.0g of calcium carbonate or magnesium carbonate sample to 100mL of the chelating plugging remover aqueous solution and shake it at 60°C, then place it in a 60°C constant temperature incubator for 24h, take out the sample and filter it with medium-speed qualitative filter paper, then place it at 105°C for drying, and finally calculate the scale dissolution rate by the mass difference before and after the experiment. The present invention uses the same dissolution test method to measure the scale dissolution rate of calcium carbonate of the chelating plugging remover obtained in Example 1 of the present invention when it is prepared into a chelating plugging remover aqueous solution with a concentration of 1wt%, 2wt%, 3wt%, 4wt%, and 5wt%. The results are shown in Table 2, and the relationship curve between the scale dissolution rate and the concentration is shown in Table 2. Figure 1 shown.

[0084] Table 1

[0085]

[0086]

[0087] Table 2

[0088] Concentration, wt% 1 2 3 4 5 Scaling rate, % 15.2 23.4 34.2 63.5 75.1

[0089] The present invention also tests the biodegradability of sodium polyaspartate and trisodium methylglycine diacetate involved in the chelating plugging remover obtained in Example 1. First, a standard curve is drawn using different concentrations of sodium polyaspartate solutions by spectrophotometry, and the absorbance is tested at about 420 nm. In subsequent biodegradation experiments, the standard curve can be used to find the corresponding concentration of sodium polyaspartate to obtain the degradation rate of sodium polyaspartate; in the biodegradation experiment, the content change of trisodium methylglycine diacetate can be obtained by quantitative complexation reaction of trisodium methylglycine diacetate with a standard ferric chloride solution, thereby obtaining the degradation rate of trisodium methylglycine diacetate; the biodegradation experiment is to culture Bacillus subtilis: at 10 0mL of Bacillus subtilis culture medium was inoculated with Bacillus subtilis strain, and it was cultured at 37°C to the logarithmic growth phase to obtain Bacillus subtilis bacterial liquid; 100mL of Bacillus subtilis culture medium was prepared, 5g of a 40wt% sodium polyaspartate aqueous solution or 5g of a 40wt% trisodium methylglycine diacetate aqueous solution was evenly spread in the culture medium to obtain a culture medium containing sodium polyaspartate or trisodium methylglycine diacetate, respectively, 2mL of Bacillus subtilis bacterial liquid was inoculated into the culture medium, and it was cultured at 37°C for 48h. During the 48h culture process, the biodegradation rates of sodium polyaspartate and trisodium methylglycine diacetate at different time points were measured, and the results were shown in Table 3 and Table 4, respectively.

[0090] Table 3

[0091]

[0092] Table 4

[0093]

[0094] The present invention applies the chelating blocking remover of Example 1, specifically:

[0095] The production pipe of West 5-12-4 well is used for application. The inner diameter volume of the oil pipe of this well is: 4.5m 3 Annulus casing volume: 16m 3 .

[0096] According to the perforation data of the well, we can know that: formation thickness h: 5.9m; effective porosity φ: 31.77%; treatment radius r: 5m.

[0097] Dosage of formation plugging-removing agent: πr 2 ×h×φ+V=160m 3 , V represents the displacement fluid volume, which is 16m 3 -4.5m 3 =11.5m 3 .

[0098] The chelating plugging remover in Example 1 was used, and the daily liquid production of the well before plugging was 5.89m 3 , daily oil production 1.0m 3 ; After the well was unblocked, the daily liquid production was 12.50m 3 , daily oil production 3.98m 3 , valid for more than six months.

[0099] The parts of the present invention that are not described in detail are well-known technologies for those skilled in the art. Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit them; although the present invention is described in detail with reference to the above embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the above embodiments, or replace some of the technical features therein by equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A chelating plugging remover, characterized in that: The chelating plugging remover comprises the following components in percentage by mass: 10-25% of chelating solubilizer, 5-15% of chelating dispersant, 0.5-1% of clay hydration swelling inhibitor, 0.5-1% of corrosion inhibitor, 0.3-1% of dispersant, and the balance is water; The chelating solubilizing agent is one or more of sodium polyaspartate, sodium citrate, and aminotriacetic acid; The chelating dispersant is one or more of tetrasodium iminodisuccinate, trisodium methylglycine diacetate, and tetrasodium glutamate diacetate; The dispersant is one or more of emulsifier MOA-4, emulsifier OP-10, and emulsifier SP-80.

2. The chelating plugging remover according to claim 1, characterized in that: The clay hydration expansion inhibitor is one or more of a quaternary ammonium salt surfactant and potassium chloride.

3. The chelating plugging remover according to claim 2, characterized in that: The quaternary ammonium salt surfactant is one or more of octadecyltrimethylammonium bromide, octadecyltrimethylammonium chloride, heptadecyltrimethylammonium bromide, heptadecyltrimethylammonium chloride, hexadecyltrimethylammonium bromide, hexadecyltrimethylammonium chloride, tetradecyltrimethylammonium bromide, tetradecyltrimethylammonium chloride, dodecyltrimethylammonium chloride, dodecyltrimethylammonium bromide, and dodecyltrimethylammonium chloride.

4. The chelating plugging remover according to claim 1, characterized in that: The corrosion inhibitor is one or more of imidazoline quaternary ammonium salt, rhodin, and Lan-826.

5. The chelating plugging remover according to any one of claims 1 to 4, characterized in that: The chelating plugging remover further comprises 0.5-1% of an adsorption carrier in terms of mass percentage; The adsorption carrier is cellulose and / or gelatin microspheres.

6. The chelating plugging remover according to claim 5, characterized in that: The preparation of the gelatin microspheres comprises the following steps: (a) mixing gelatin powder with water to obtain a gelatin aqueous solution; (b) heat-treating the gelatin aqueous solution at 50-60° C. for 0.5-3 h; (c) adding the gelatin aqueous solution treated in step (b) to a coolant to obtain spherical particles; (d) placing the obtained spherical particles in a glutaraldehyde aqueous solution for cross-linking treatment, and then washing and drying to obtain gelatin microspheres.

7. The chelating plugging remover according to claim 6, characterized in that: In step (a), the mass percentage of gelatin in the gelatin aqueous solution is 1-5%.

8. The chelating plugging remover according to claim 6, characterized in that: In step (c), the coolant is an organic solvent and / or brine.

9. The chelating plugging remover according to claim 8, characterized in that: The organic solvent is ethanol and / or acetone, and the salt water is a sodium chloride aqueous solution and / or a calcium chloride aqueous solution.

10. The method for preparing a chelating blocking agent according to any one of claims 1 to 4, characterized in that: The method comprises the following steps: (1) mixing the chelating dispersant with water to obtain a mixed solution; (2) Add a chelating solubilizing agent, a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant to the mixed solution in sequence and mix them evenly to obtain a chelating plugging remover.

11. The method for preparing a chelating blocking remover according to any one of claims 5 to 9, characterized in that: The method comprises the following steps: (1) mixing the chelating dispersant and the adsorption carrier uniformly with water to obtain a mixed solution; (2) Add a chelating solubilizing agent, a clay hydration swelling inhibitor, a corrosion inhibitor and a dispersant to the mixed solution in sequence and mix them evenly to obtain a chelating plugging remover.

Citation Information

Patent Citations

  • Neutral blocking remover for ultra-low permeability reservoir water injection well and preparation method

    CN111117584A

  • Chelating type blocking remover and preparation method and application thereof

    CN112094633A