A power frequency reactor based on the principle of flux shunting and a hybrid magnetic circuit core.

By employing the principle of magnetic flux shunting in power frequency reactors, and connecting silicon steel and iron-silicon soft magnetic composite materials in parallel, the permeability and magnetic flux density are controlled, thus solving the problems of high loss and high noise in power frequency reactors and optimizing inductance and loss.

CN117352275BActive Publication Date: 2026-11-10ANHUI RUIDE MAGNETOELECTRIC TECH CO LTD +4
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311528875.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-16
Publication Date
2026-11-10
Estimated Expiration
2043-11-16

AI Technical Summary

Technical Problem

Under power frequency conditions, dry-type iron-core reactors suffer from high losses and high vibration and noise. Using only iron-silicon soft magnetic composite materials will result in too low initial inductance, while using silicon steel will easily lead to magnetization saturation. Existing technologies cannot effectively reduce losses and noise while ensuring inductance.

Method used

By adopting the principle of magnetic flux shunting, silicon steel and iron-silicon soft magnetic composite material are connected in parallel to form the core column of the reactor. By adjusting the volume ratio of the silicon steel and iron-silicon soft magnetic composite material regions and the size of the air gap, the effective magnetic permeability and magnetic flux density are controlled, and the total air gap is reduced to reduce leakage flux and vibration noise.

Benefits of technology

While meeting the inductance design requirements, it reduces reactor losses and noise by 9dB and losses by about 15%. Furthermore, by flexibly adjusting the inductance and losses, the core's anti-saturation capability is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117352275B_ABST
    Figure CN117352275B_ABST
Patent Text Reader

Abstract

This invention relates to a power frequency reactor with a hybrid magnetic circuit core based on the principle of magnetic flux shunting, belonging to the field of reactor technology. It includes an upper yoke, a lower yoke, and three core columns, with copper coils wound on the three core columns. The upper and lower yokes are both made of silicon steel. Each core column is composed of an iron-silicon soft magnetic column and a silicon steel tube. The iron-silicon soft magnetic column is made of an iron-silicon soft magnetic composite material with a permeability of 26–90 μm. The silicon steel tube is made of non-oriented silicon steel, encasing the iron-silicon soft magnetic column, and both the iron-silicon soft magnetic column and the silicon steel tube are insulated, forming a parallel structure. Each iron-silicon soft magnetic column is divided into three segments along its length. Air gaps are provided between adjacent iron-silicon soft magnetic column segments and between the upper and lower yokes and the three core columns. Under the conditions of a rated voltage of 220V and a rated reactance of 14.5Ω, the power frequency reactor has a noise level of 55–61 dB and a loss of 118–123 W. This invention achieves flexible adjustment of the inductance and loss of the reactor by combining two materials and adjusting the thickness of the air gap.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of reactor technology, specifically relating to a power frequency reactor with a hybrid magnetic circuit core based on the principle of magnetic flux shunting. Background Technology

[0002] The common structure of dry-type iron-core reactors is a three-phase, three-column design, consisting of an upper yoke, a lower yoke, and core columns. Each core column comprises two side columns and one middle column. Currently, the upper yoke, lower yoke, and core columns of dry-type iron-core reactors used in power grids are all made of silicon steel. Because silicon steel has high permeability and is easily magnetized to saturation, relatively large air gaps are typically placed at different locations within the core columns and between the upper and lower yokes and the core columns to improve the anti-saturation capability of the silicon steel core. However, leakage flux at the air gaps generates additional losses, and the electromagnetic force at both ends of the air gap causes core vibration, producing significant noise. To reduce reactor losses and vibration noise, the air gap can be reduced. However, simply reducing the air gap reduces magnetic reluctance, potentially leading to an excessively high initial inductance and an excessively low load inductance.

[0003] Ferrosilicon soft magnetic composites possess high saturation magnetic flux density and significantly higher resistivity and anti-saturation capability than silicon steel. They have replaced silicon steel as reactor cores in high-frequency, high-power applications, substantially reducing the air gap and lowering leakage flux and vibration noise. However, under power frequency conditions, the permeability of ferrosilicon soft magnetic composites is relatively low, typically reaching only 90 μF. Therefore, using this material alone to replace silicon steel in reactor core fabrication results in excessively low initial inductance and significantly higher hysteresis losses at the same magnetic flux density compared to silicon steel. Thus, effectively reducing core losses and vibration noise while ensuring the inductance meets design requirements remains a challenge for power frequency reactors, and researchers have yet to find a satisfactory solution. Summary of the Invention

[0004] To address the issues of high noise and high loss in power frequency reactors to some extent, this invention provides a power frequency reactor with a hybrid magnetic circuit core based on the principle of magnetic flux shunting.

[0005] This invention is based on the principle of magnetic flux shunting. It connects silicon steel and iron-silicon soft magnetic composite material in parallel to form the core column of the reactor. By adjusting the volume ratio and air gap size of the silicon steel and iron-silicon soft magnetic composite material region, the effective permeability and magnetic flux density of the silicon steel and iron-silicon soft magnetic composite material region are controlled and the total air gap of the core is reduced. Thus, while meeting the inductance design requirements, the purpose of reducing reactor loss and noise is achieved at the same time.

[0006] A power frequency reactor with a hybrid magnetic circuit core includes an upper yoke, a lower yoke, and three core columns evenly distributed between the upper and lower yokes. The three core columns are a middle core column and two side core columns, and have the same cross-sectional area. Copper coils are wound on the three core columns respectively. The upper and lower yokes are both made of silicon steel. Each core column consists of an iron-silicon soft magnetic column and a silicon steel tube. The iron-silicon soft magnetic column is made of iron-silicon soft magnetic composite material. The silicon steel tube is sleeved on the iron-silicon soft magnetic column and fixed and bonded by epoxy resin. Both the iron-silicon soft magnetic column and the silicon steel tube are insulated, so that the iron-silicon soft magnetic column and the silicon steel tube form a parallel structure. Each iron-silicon soft magnetic column is divided into three iron-silicon soft magnetic column segments along its length. Air gaps are provided between adjacent iron-silicon soft magnetic column segments. Air gaps are also provided between the upper yoke, lower yoke and the connection ends of the three iron-silicon soft magnetic columns, and all are fixed and bonded by epoxy resin adhesive.

[0007] The further defined technical solution is as follows: The cross-sectional area of ​​the iron-silicon soft magnetic pillar is 20-40% of the total cross-sectional area of ​​the core pillar.

[0008] The thickness of the air gap between adjacent iron-silicon soft magnetic column segments is 0.4–0.8 mm.

[0009] The thickness of the air gap between the iron-silicon soft magnetic pillars at both ends of the core pillar and the upper and lower yokes is 1-2 mm.

[0010] The area of ​​the air gap is smaller than the cross-sectional area of ​​the core column.

[0011] The copper coils are respectively centered on the middle core post and the two side core posts.

[0012] The permeability of the iron-silicon soft magnetic composite material is 26–90 μ.

[0013] The silicon steel pipe is made of non-oriented silicon steel of grade 35WW300.

[0014] The power frequency reactor, under the conditions of rated voltage 220V and rated reactance 14.5Ω, tested according to GB / T1094.10—2003, has a noise level of 55~61dB and a loss of 118~123W.

[0015] The beneficial technical effects of this invention are reflected in the following aspects: (1) This invention creatively adopts the principle of magnetic flux shunting, and connects silicon steel and iron-silicon soft magnetic composite material in parallel in the core magnetic circuit. On the one hand, the high anti-saturation ability of iron-silicon soft magnetic composite material is used to make up for the defect of easy magnetization and saturation of silicon steel, and improve the overall anti-saturation ability of the core, so as to reduce the total air gap in the core, thereby laying the foundation for reducing reactor vibration noise and reducing leakage flux. On the other hand, the high permeability and low hysteresis loss of silicon steel are used to make up for the defect of low permeability and high hysteresis loss of iron-silicon soft magnetic composite material. By adjusting the thickness of the air gap plate, the effective permeability of the silicon steel region and the iron-silicon soft magnetic composite material region of the core column can be flexibly adjusted, and the inductance of the reactor and the magnetic flux shared by the core column in the two material regions can be reasonably controlled. More magnetic lines of force are appropriately shunted into the silicon steel region with high saturation magnetic flux density, thereby reducing the working magnetic flux density of the iron-silicon soft magnetic composite material region, and thus effectively reducing the hysteresis loss of the iron-silicon soft magnetic composite material region, laying the foundation for reducing the total loss of the core under the premise of meeting the design requirements of reactor inductance.

[0016] (2) The hybrid magnetic circuit core column of the present invention is made of silicon steel wrapped with iron-silicon soft magnetic composite material and air gap sheet. This combination is simple and easy to operate, and can combine the two core materials very compactly. The effective permeability and working magnetic flux density of the two material regions can be flexibly adjusted by adjusting the thickness of the air gap sheet, thereby flexibly adjusting the inductance and loss of the reactor.

[0017] (3) The power frequency reactor of the present invention and the conventional silicon steel core reactor were compared in terms of noise (according to GB / T 1094.10—2003) and loss under the conditions of rated voltage 220V and rated reactance 14.5Ω. The comparison test data are shown in Table 1. Among them, reactor No. 1 is a silicon steel core reactor of grade 35WW300, and reactor No. 2 is a hybrid magnetic circuit core reactor made by the method of the present invention. It can be seen that when the upper yoke, lower yoke and coil of the reactor are exactly the same, the power frequency reactor made by the present invention has lower noise and loss than the silicon steel core reactor. The noise is reduced by 9dB and the loss is reduced by about 15%, as detailed in Example 2. Attached Figure Description

[0018] Figure 1 This is a schematic diagram of the structure of a power frequency reactor.

[0019] Figure 2 This is a schematic diagram of the cross-sectional structure of the core column of the hybrid magnetic circuit of a power frequency reactor.

[0020] Figure 3 This is a schematic diagram of the core and air gap of a power frequency reactor.

[0021] Figure 4This is a schematic diagram of the magnetic flux density distribution of the simulated cross section of the power frequency reactor with a hybrid magnetic circuit core in Example 1.

[0022] Figure 1 The sequence numbers are: upper yoke 1, lower yoke 2, middle core column 3, side core column 4, copper coil 5, silicon steel tube 6, iron-silicon soft magnetic column 7. Detailed Implementation

[0023] The present invention will be further described below with reference to the accompanying drawings and embodiments.

[0024] Example 1 See Figure 1 A power frequency reactor with a hybrid magnetic circuit core based on the principle of magnetic flux shunting includes an upper yoke 1, a lower yoke 2, and three core columns evenly distributed between the upper yoke 1 and the lower yoke 2. The three core columns are a middle core column 3 and two side core columns 4, and the three core columns have the same cross-sectional area. Copper coils 5 are wound on the three core columns. The upper yoke 1 and the lower yoke 2 are both made of non-oriented silicon steel 35WW300, and their dimensions are both 300mm×80mm×60mm.

[0025] See Figure 2 Each core post consists of an iron-silicon soft magnetic pillar and a silicon steel tube. The iron-silicon soft magnetic pillar is made of iron-silicon soft magnetic composite material with a permeability of 26μm, while the silicon steel tube is made of non-oriented silicon steel 35WW300. The silicon steel tube encloses the iron-silicon soft magnetic pillar and is fixed and bonded with epoxy resin. Both the iron-silicon soft magnetic pillar and the silicon steel tube are insulated, forming a parallel structure. The single-segment dimensions of each core post are 80mm × 60mm × 80mm, and the total cross-sectional area of ​​the core post is 4800mm².

[0026] See Figure 3 Each iron-silicon soft magnetic column is divided into three iron-silicon soft magnetic column segments along its length. Air gaps are provided between adjacent iron-silicon soft magnetic column segments. Air gaps are also provided between the upper yoke 1, the lower yoke 2 and the connection ends of the three iron-silicon soft magnetic columns, and all are fixed and bonded by epoxy resin adhesive.

[0027] See Figure 2 Each segment of the iron-silicon soft magnetic column measures 32mm × 30mm × 80mm, with a total of 3 segments and a cross-sectional area of ​​960mm², accounting for 20% of the total cross-sectional area of ​​the core column; the remainder is the cross-sectional area of ​​a silicon steel tube. The air gap between adjacent iron-silicon soft magnetic column segments measures 75mm × 55mm × 0.4mm. The air gap between the two ends of the core column and the upper yoke 1 and lower yoke 2 measures 75mm × 55mm × 1mm. The 224-turn copper coil 5 is centered on the middle core column 3 and the two side core columns 4.

[0028] See Figure 4The power frequency reactor modeled using ANSYS software was simulated. The magnetic flux density distribution of the simulated cross section of the power frequency reactor with a hybrid magnetic circuit core was clearly visible, and the magnetic flux shunting effect was obvious.

[0029] The power frequency reactor in this embodiment 1 was tested for noise (according to GB / T 1094.10—2003) and loss under the conditions of rated voltage 220V and rated reactance 14.5Ω. The test noise was 58dB and the loss was 130W.

[0030] Example 2 The difference from Example 1 is that: The permeability of the material for the iron-silicon soft magnetic pillar is 60 μ.

[0031] See Figure 2 Each segment of the iron-silicon soft magnetic column measures 40mm × 36mm × 80mm, with a cross-sectional area of ​​1440m², accounting for 30% of the total cross-sectional area of ​​the core column; the remainder is the cross-sectional area of ​​a silicon steel tube. The air gap between adjacent iron-silicon soft magnetic column segments measures 75mm × 55mm × 0.6mm. The air gap between the two ends of the core column and the upper yoke 1 and lower yoke 2 measures 75mm × 55mm × 1.5mm.

[0032] See Figure 4 The power frequency reactor modeled using ANSYS software was simulated. The magnetic flux density distribution of the simulated cross section of the power frequency reactor with a hybrid magnetic circuit core was clearly visible, and the magnetic flux shunting effect was obvious.

[0033] The power frequency reactor in this embodiment 2 was tested for noise (according to GB / T 1094.10—2003) and loss under the conditions of rated voltage 220V and rated reactance 14.5Ω. The test noise was 55dB and the loss was 118W.

[0034] Example 3 The difference from Example 1 is that: The permeability of the material for the iron-silicon soft magnetic pillar is 90 μ.

[0035] See Figure 2 Each segment of the iron-silicon soft magnetic column measures 48mm × 40mm × 80mm, with a cross-sectional area of ​​1920m², accounting for 40% of the total cross-sectional area of ​​the core column; the remainder is the cross-sectional area of ​​a silicon steel tube. The air gap between adjacent iron-silicon soft magnetic column segments measures 75mm × 55mm × 0.8mm. The air gap between the two ends of the core column and the upper yoke 1 and lower yoke 2 measures 75mm × 55mm × 2.0mm.

[0036] See Figure 4 The power frequency reactor modeled using ANSYS software was simulated. The magnetic flux density distribution of the simulated cross section of the power frequency reactor with a hybrid magnetic circuit core was clearly visible, and the magnetic flux shunting effect was obvious.

[0037] The power frequency reactor in this embodiment 3 was tested for noise (according to GB / T 1094.10—2003) and loss under the conditions of rated voltage 220V and rated reactance 14.5Ω. The test noise was 61dB and the loss was 123W.

[0038] Those skilled in the art will readily understand that the above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

Claims

1. A power frequency reactor with a hybrid magnetic circuit core, comprising an upper yoke, a lower yoke, and three core columns evenly distributed between the upper and lower yokes, wherein the three core columns are a middle core column and two side core columns, and have the same cross-sectional area; copper coils are wound on the three core columns respectively; the upper and lower yokes are both made of silicon steel, characterized in that: Each core column consists of an iron-silicon soft magnetic column and a silicon steel tube. The iron-silicon soft magnetic column is made of iron-silicon soft magnetic composite material. The silicon steel tube is sleeved on the iron-silicon soft magnetic column and fixed and bonded by epoxy resin. Both the iron-silicon soft magnetic column and the silicon steel tube are insulated, so that the iron-silicon soft magnetic column and the silicon steel tube form a parallel structure. Each iron-silicon soft magnetic column is divided into three iron-silicon soft magnetic column segments along its length. Air gaps are provided between adjacent iron-silicon soft magnetic column segments. Air gaps are also provided between the upper yoke, lower yoke and the connection ends of the three iron-silicon soft magnetic columns, and all are fixed and bonded by epoxy resin adhesive.

2. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The cross-sectional area of ​​the iron-silicon soft magnetic pillar is 20-40% of the total cross-sectional area of ​​the core pillar.

3. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The thickness of the air gap between adjacent iron-silicon soft magnetic column segments is 0.4–0.8 mm.

4. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The thickness of the air gap between the iron-silicon soft magnetic pillars at both ends of the core pillar and the upper and lower yokes is 1-2 mm.

5. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The area of ​​the air gap is smaller than the cross-sectional area of ​​the core column.

6. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The copper coils are respectively centered on the middle core post and the two side core posts.

7. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The permeability of the iron-silicon soft magnetic composite material is 26–90 μ.

8. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The silicon steel pipe is made of non-oriented silicon steel of grade 35WW300.

9. The power frequency reactor with a hybrid magnetic circuit core according to claim 1, characterized in that: The power frequency reactor, under the conditions of rated voltage 220V and rated reactance 14.5Ω, tested according to GB / T 1094.10—2003, has a noise level of 55~61dB and a loss of 118~123W.

Citation Information

Patent Citations

  • Three-phase and five-column electric reactor of new structure

    CN103680857A

  • Three-phase electric reactor

    CN104715899A