A method for preparing hexahydrophthalide using tetrahydrophthalic anhydride
By using tetrahydrophthalic anhydride as a raw material and employing an eggshell-type catalyst in a fixed-bed reactor to catalytically hydrogenate hexahydrophthalide, the problem of high price of hexahydrophthalide monomer is solved, achieving low-cost, high-efficiency preparation with fewer side reactions, making it suitable for industrial applications.
Patent Information
- Application Number
- CN202410469059.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-18
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2044-04-18
AI Technical Summary
The high price of hexahydrophthalide monomers, complex preparation methods, high energy consumption, numerous side reactions, and high investment costs in existing technologies limit their widespread application.
Hexahydrophthalide was prepared by catalytic hydrogenation of a mixture of tetrahydrophthalic anhydride and solvent in a fixed-bed reactor using an eggshell-type catalyst. The catalyst used palladium, ruthenium, copper and other metals as active components, and γ-Al2O3, SiO2 and ZrO2 as supports. The reaction conditions were mild and the catalyst was regenerable.
This method enables the low-cost and efficient preparation of hexahydrophthalide, reduces side reactions, and features a catalyst with good stability and long lifespan. The byproducts have high added value and are suitable for industrial applications.
Smart Images

Figure CN118344317B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of fine chemical synthesis technology, and particularly relates to a method for preparing hexahydrophthalide using tetrahydrophthalic anhydride. Background Technology
[0002] The invention and use of plastics have greatly improved our daily lives, making them an indispensable material in modern life. However, the improper use and non-degradability of plastics have led to serious global environmental pollution. Currently, the main methods for handling waste plastics include landfill, incineration, and recycling. Besides focusing on the chemical recycling of waste plastics, many experts and scholars believe that designing and developing easily degradable and recyclable polymer materials is the best strategy to solve the plastic pollution problem. After use, polymer materials can generate repolymerizable monomers through depolymerization reactions. By constructing a monomer-polymer-monomer recycling chain, not only can plastic waste be effectively reduced, but resources can also be maximized. In recent years, significant progress has been made in designing monomer structures to construct closed-loop recyclable polymers, which has attracted widespread attention from the academic community.
[0003] Hexahydrophthalide, also known as hexahydroisobenzofuran-1-one, has the molecular formula C8H10. 12 O2, molecular weight: 140.2, slightly soluble in water, readily soluble in organic solvents such as 1,4-dioxane, tetrahydrofuran, γ-butyrolactone, toluene, and diethyl ether. It is a biomass derivative based on γ-butyrolactone, exhibiting ring-opening polymerization properties similar to γ-butyrolactone, and has attracted considerable attention from researchers in recent years as a recyclable and biodegradable plastic monomer.
[0004] Among them, poly(γ-butyrolactone) synthesized from the ring-opening polymerization of γ-butyrolactone is a renewable resource with good biocompatibility and biodegradability. The process of obtaining poly(γ-butyrolactone) through bio-fermentation is relatively mature. However, the chemical synthesis of poly(γ-butyrolactone) has always been a challenge, with problems such as high energy consumption in the polymerization reaction, low molecular weight of the obtained polymer, and low Tm. In 2018, Chen et al. (Science 2018, 360:398–403) proposed to improve the ring strain by using a ring-fusion strategy while retaining the core structure of γ-butyrolactone, and designed a ring-opening polymerization reaction using a hexahydrophthalide monomer containing the γ-butyrolactone structure. This reaction uses hexahydrophthalide as a monomer and employs La[N(TMS)2]3, Y-1, or Zn-1 catalysts for efficient polymerization at room temperature and without solvents. The resulting polymer can be pyrolyzed at high temperature or by adding a metal salt catalyst at 120°C to return it to the original monomer hexahydrophthalide. Repeated experiments have verified that the monomer obtained after pyrolysis can be repolymerized with high efficiency, realizing a closed-loop cycle of monomer-polymer-monomer polymerization-depolymerization, which can effectively promote the research progress of polymer materials.
[0005] Subsequently, in 2019, Haritz Sardon et al. (NATURE COMMUNICATIONS, 2019.10) conducted a copolymerization reaction by mixing γ-butyrolactone and hexahydrophthalide in different proportions to obtain polymers with better performance and improve the extensibility of copolymers. The resulting copolymers showed extensibility and barrier properties suitable for different application materials. Depolymerization experiments were conducted on the formed copolymer films, and the comonomers were completely recycled, demonstrating complete chemical recyclability.
[0006] While some progress has been made in the ring-opening polymerization of hexahydrophthalide, the high price of hexahydrophthalide monomers has slowed research progress and hindered widespread adoption. Developing practical and inexpensive hexahydrophthalide monomers is a key research focus. Currently, three main methods for preparing hexahydrophthalide are known. One method involves the catalytic hydrogenation of phthalic anhydride in a high-pressure reactor. The water produced during hydrogenation promotes the hydrolysis of phthalic anhydride, increasing side reactions, and there are currently no reports of reactions in a fixed-bed reactor. The other two methods use phthalide and hexahydrophthalic anhydride as raw materials for hydrogenation reactions, respectively. These methods are simple and yield hexahydrophthalide with high selectivity, but the raw materials required for these methods are expensive, making them unsuitable for widespread application.
[0007] Therefore, in order to solve one of the above problems, it is necessary to develop a method for preparing hexahydrophthalide that has a wide range of raw material sources, is simple to operate, has mild conditions, few side reactions, and low investment costs. Summary of the Invention
[0008] In view of the shortcomings of the prior art, the technical problem to be solved by the present invention is to provide a method for preparing hexahydrophthalide using tetrahydrophthalic anhydride, so as to solve the problems of high raw material price, high energy consumption, many side reactions and high investment cost in the existing technology.
[0009] The method for preparing hexahydrophthalide using tetrahydrophthalic anhydride according to the present invention comprises the following steps:
[0010] S1: Raw material preparation: Tetrahydrophthalic anhydride is mixed with a solvent to make the concentration of tetrahydrophthalic anhydride 1-30%, and the resulting solution is the raw material;
[0011] S2: Catalytic hydrogenation reaction: Eggshell-shaped catalyst is loaded into a fixed-bed reactor. After hydrogen is introduced, the temperature is raised to 400℃ and maintained at this temperature for 6 hours to reduce the catalyst. When the temperature drops to 150-180℃, the raw material obtained in S1 is added to the fixed-bed reactor to carry out the catalytic hydrogenation reaction. The hydrogenation reaction temperature is 50-180℃, the hydrogen pressure is 0-5 MPa, and the space velocity is 0.1-2 h⁻¹. -1 The hydrogen-to-oil volume ratio is (100-800):1, and the final product is hexahydrophthalide.
[0012] Preferably, the eggshell-shaped catalyst is prepared by spraying.
[0013] Preferably, in the eggshell-shaped catalyst, the active component of the hydrogen metal element is one or more of palladium, ruthenium, and copper.
[0014] Preferably, the eggshell-shaped catalyst is supported by one of γ-Al2O3, SiO2, and ZrO2, the content of the hydrogenation metal element in the catalyst is 0.5-2%, and the content of the support is 98-99.5%.
[0015] Preferably, the solvent is one or more of 1,4-dioxane, tetrahydrofuran, and γ-butyrolactone.
[0016] Preferably, the tetrahydrophthalic anhydride is cis-1,2,3,6-tetrahydrophthalic anhydride or 3,4,5,6-tetrahydrophthalic anhydride, and the product hexahydrophthalide is cis-hexahydrophthalide or a mixture of cis-hexahydrophthalide and trans-hexahydrophthalide.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] (1) This invention innovatively uses a mixture of tetrahydrophthalic anhydride and solvent as raw material to directly prepare hexahydrophthalide by hydrogenation. The preparation process is simple, green and environmentally friendly, with mild reaction conditions and low reaction cost.
[0019] (2) The eggshell-type catalyst synthesized in this invention has excellent hydrogenation activity and selectivity. There is no precedent for using eggshell-type catalysts to prepare hexahydrophthalide. The synthesized eggshell-type catalyst effectively reduces the amount of precious metal active components, reduces costs, has good stability, long lifespan, can be recycled after regeneration, and the catalyst activity does not decrease significantly.
[0020] (3) The raw materials used in this invention can be completely converted, and the by-products cyclohexanecarboxylic acid and o-methylcyclohexanecarboxylic acid also have high added value. They are easy to separate from hexahydrophthalide in the future, which can improve economic benefits and has good industrial application value. Attached Figure Description
[0021] To more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the accompanying drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. In all the drawings, similar elements or parts are generally identified by similar reference numerals. In the drawings, the elements or parts are not necessarily drawn to scale.
[0022] Appendix Figure 1 The reaction pathway diagram for the catalytic hydrogenation of tetrahydrophthalic anhydride to prepare hexahydrophthalide. Detailed Implementation
[0023] The present invention will now be further described with reference to the accompanying drawings:
[0024] The present invention will be further illustrated by specific embodiments below, but it is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
[0025] Example 1:
[0026] (1) Catalyst preparation: Weigh 0.83g PdCl2 and dissolve it in hydrochloric acid and distilled water. Adjust the pH value to 3-5 to obtain chloropalladic acid solution. Take 100g γ-Al2O3 and calcine it in a muffle furnace at 450℃ for 3h. Set the spraying speed to 10ml / h, the sugar pellet machine speed to 700rpm, and the temperature to 70℃. Spray the chloropalladic acid solution evenly on the surface of alumina pellets. After spraying, calcine it at 450℃ for 3h. After cooling, obtain 0.5% Pd@Al2O3 metal oxidation catalyst. Spray 0.5% Ru@Al2O3, 0.5% Ru3Pd@Al2O3, and 0.5% Pd3Cu@Al2O3 in the same way. The bimetallic catalyst is prepared with the content of the two metals in a molar ratio of 3:1.
[0027] (2) Preparation of hexahydrophthalide: The catalyst was loaded into a fixed-bed reactor, hydrogen gas was introduced, and the temperature was raised to 400℃ and maintained for 6 hours for reduction reaction. When the temperature dropped to 180℃, the raw material was introduced. The raw material was prepared at a mass concentration of 1% (1g cis-1,2,3,6-tetrahydrophthalic anhydride + 99g 1,4-dioxane). The reaction was carried out at a reaction temperature of 180℃, a hydrogen pressure of 3MPa, and a space velocity of 0.5h. -1 Catalytic hydrogenation was carried out under a hydrogen-to-oil ratio of 500:1, and the resulting products were analyzed by gas chromatography. The results are shown in Table 1 below.
[0028] Table 1
[0029]
[0030] Example 2:
[0031] (1) Catalyst preparation: Weigh 0.22g PdCl2 and dissolve it in hydrochloric acid and distilled water to obtain chloropalladic acid solution. Weigh 0.76g RuCl3·3H2O and dissolve it in distilled water. Add chloropalladic acid and stir evenly. Adjust the pH value to 3-5 to obtain bimetallic spraying liquid. Take 100g SiO2 and calcine it in a muffle furnace at 450℃ for 3h. Set the spraying speed to 10ml / h, the sugar pellet machine speed to 700rpm, and the temperature to 70℃. Spray the bimetallic spraying liquid evenly on the surface of silica microspheres. After spraying, calcine it at 450℃ for 3h. After cooling, obtain 0.5% Ru3Pd@SiO2 metal oxidation catalyst. Replace the SiO2 support with 100g ZrO2 according to the same method to prepare 0.5% Ru3Pd@ZrO2.
[0032] (2) Preparation of hexahydrophthalide: The catalyst was loaded into a fixed-bed reactor, hydrogen gas was introduced, and the temperature was raised to 400℃ and held for 6 hours for reduction reaction. When the temperature dropped to 180℃, the raw material was introduced. The raw material was prepared at a mass concentration of 1% (1g cis-1,2,3,6-tetrahydrophthalic anhydride + 99g 1,4-dioxane). The reaction was carried out at a reaction temperature of 180℃, a hydrogen pressure of 3MPa, and a space velocity of 0.5h. -1 Catalytic hydrogenation was carried out under a hydrogen-to-oil ratio of 500:1, and the resulting products were analyzed by gas chromatography. The results are shown in Table 2 below.
[0033] Table 2
[0034]
[0035] Example 3:
[0036] (1) Catalyst preparation: Weigh 0.22g PdCl2 and dissolve it in hydrochloric acid and distilled water to obtain chloropalladic acid solution. Weigh 0.76g RuCl3·3H2O and dissolve it in distilled water. Add chloropalladic acid and stir evenly. Adjust the pH value to 3-5 to obtain bimetallic spraying liquid. Take 100g γ-Al2O3 and calcine it in a muffle furnace at 450℃ for 3h. Set the spraying speed to 10ml / h, the sugar pellet machine speed to 700rpm, and the temperature to 70℃. Spray the bimetallic spraying liquid evenly on the surface of alumina microspheres. After spraying, calcine it at 450℃ for 3h. After cooling, obtain 0.5% Ru3Pd@Al2O3 metal oxidation catalyst.
[0037] (2) Preparation of hexahydrophthalide: The catalyst was loaded into a fixed-bed reactor, hydrogen was introduced, and the temperature was raised to 400℃ and maintained for 6 hours for reduction reaction. When the temperature dropped to 180℃, the raw material was introduced. The raw material was prepared at a mass concentration of 1% (1g cis-1,2,3,6-tetrahydrophthalic anhydride + 99g tetrahydrofuran). The reaction was carried out at a reaction temperature of 180℃, a hydrogen pressure of 3MPa, and a space velocity of 0.5h. -1Catalytic hydrogenation was carried out under a hydrogen-to-oil ratio of 500:1, and the resulting product was analyzed by gas chromatography. The results are shown in Table 3 below. A raw material with a mass concentration of 1% (1g cis-1,2,3,6-tetrahydrophthalic anhydride + 99g γ-butyrolactone) was prepared according to the above method, and the reaction was carried out under the same conditions. The resulting product was analyzed by gas chromatography. The results are shown in Table 3 below.
[0038] Table 3
[0039]
[0040] Example 4:
[0041] (1) Catalyst preparation: Weigh 0.22g PdCl2 and dissolve it in hydrochloric acid and distilled water to obtain chloropalladic acid solution. Weigh 0.76g RuCl3·3H2O and dissolve it in distilled water. Add chloropalladic acid and stir evenly. Adjust the pH value to 3-5 to obtain bimetallic spraying liquid. Take 100g γ-Al2O3 and calcine it in a muffle furnace at 450℃ for 3h. Set the spraying speed to 10ml / h, the sugar pellet machine speed to 700rpm, and the temperature to 70℃. Spray the bimetallic spraying liquid evenly on the surface of alumina microspheres. After spraying, calcine it at 450℃ for 3h. After cooling, obtain 0.5% Ru3Pd@Al2O3 metal oxidation catalyst.
[0042] (2) Preparation of hexahydrophthalide: The catalyst was loaded into a fixed-bed reactor, hydrogen gas was introduced, and the temperature was raised to 400℃ and maintained for 6 hours for reduction reaction. When the temperature dropped to 150℃, the raw material was introduced. The raw material was prepared at a mass concentration of 1% (1g cis-1,2,3,6-tetrahydrophthalic anhydride + 99g 1,4-dioxane). The reaction was carried out at a reaction temperature of 150℃, a hydrogen pressure of 3MPa, and a space velocity of 0.5h. -1 Catalytic hydrogenation was carried out under a hydrogen-to-oil ratio of 500:1. The resulting product was analyzed by gas chromatography, and the results are shown in Table 4 below. A raw material with a mass concentration of 1% (1g 3,4,5,6-tetrahydrophthalic anhydride + 99g 1,4-dioxane) was prepared according to the above method, and the reaction was carried out under the same conditions. The resulting product was analyzed by gas chromatography, and the results are shown in Table 4 below.
[0043] Table 4
[0044]
[0045] Example 5:
[0046] (1) Catalyst preparation: Weigh 0.22g PdCl2 and dissolve it in hydrochloric acid and distilled water to obtain chloropalladic acid solution. Weigh 0.76g RuCl3·3H2O and dissolve it in distilled water. Add chloropalladic acid and stir evenly. Adjust the pH value to 3-5 to obtain bimetallic spraying liquid. Take 100g γ-Al2O3 and calcine it in a muffle furnace at 450℃ for 3h. Set the spraying speed to 10ml / h, the sugar pellet machine speed to 700rpm, and the temperature to 70℃. Spray the bimetallic spraying liquid evenly on the surface of alumina microspheres. After spraying, calcine it at 450℃ for 3h. After cooling, obtain 0.5% Ru3Pd@Al2O3 metal oxidation catalyst.
[0047] (2) Preparation of hexahydrophthalide: The catalyst was loaded into a fixed-bed reactor, hydrogen gas was introduced, and the temperature was raised to 400℃ and maintained for 6 hours for reduction reaction. When the temperature dropped to 180℃, the raw material was introduced. The raw material was prepared according to a mass concentration of 1% (1g cis-1,2,3,6-tetrahydrophthalic anhydride + 99g 1,4-dioxane). The reaction was carried out at a reaction temperature of 180℃ and a space velocity of 0.2h. -1 Under the condition of a hydrogen-to-oil ratio of 500:1, the effect of different pressure conditions on the catalytic hydrogenation reaction was investigated. The obtained products were analyzed by gas chromatography, and the results are shown in Table 5 below.
[0048] Table 5
[0049]
[0050] Example 6:
[0051] The service life of the catalyst was evaluated. The catalyst 0.5% Ru3Pd@Al2O3 was prepared according to the preparation method described in Example 3. The equipment was run continuously for 500 hours according to the preparation method of hexahydrophthalide in Example 3. The conversion rate and selectivity did not decrease significantly. The conversion rate of tetrahydrophthalic anhydride remained at 100%, and the selectivity of hexahydrophthalide remained above 89%, indicating that the catalyst performance was stable.
[0052] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection of the present invention is defined by the appended claims and their equivalents.
[0053] Any aspects of this invention not described in detail are well-known to those skilled in the art.
Claims
1. A method for preparing hexahydrophthalide using tetrahydrophthalic anhydride, characterized in that, The specific preparation steps are as follows: S1: Raw material preparation: Tetrahydrophthalic anhydride is mixed with a solvent to make the concentration of tetrahydrophthalic anhydride 1-30%, and the resulting solution is the raw material; S2: Catalytic hydrogenation reaction: Eggshell-shaped catalyst is loaded into a fixed-bed reactor. After hydrogen is introduced, the temperature is raised to 400℃ and maintained at this temperature for 6 hours to reduce the catalyst. When the temperature drops to 150-180℃, the raw material obtained in S1 is added to the fixed-bed reactor to carry out the catalytic hydrogenation reaction. The hydrogenation reaction temperature is 50-180℃, the hydrogen pressure is 0-5 MPa, and the space velocity is 0.1-2 h⁻¹. -1 The hydrogen-to-oil volume ratio is (100-800):1, and the final product is hexahydrophthalide; Catalyst preparation: 0.22g PdCl2 was weighed and dissolved in hydrochloric acid and distilled water to obtain a chloropalladium acid solution. 0.76g RuCl3·3H2O was weighed and dissolved in distilled water, and chloropalladium acid was added and stirred evenly. The pH value was adjusted to 3-5 to obtain a bimetallic spraying solution. 100g γ-Al2O3 was calcined in a muffle furnace at 450℃ for 3h. The spraying speed was set to 10ml / h, the sugar pellet machine speed was 700rpm, and the temperature was 70℃. The bimetallic spraying solution was evenly sprayed onto the surface of alumina microspheres. After spraying, it was calcined at 450℃ for 3h. After cooling, a metal oxidizing catalyst of 0.5% Ru3Pd@Al2O3 was obtained. The equipment was run continuously for 500h. The conversion rate and selectivity did not decrease significantly. The conversion rate of tetrahydrophthalic anhydride remained at 100%, and the selectivity of hexahydrophthalide remained above 89%, indicating that the catalyst performance was stable.
2. The method for preparing hexahydrophthalide using tetrahydrophthalic anhydride according to claim 1, characterized in that, The eggshell-shaped catalyst was prepared by spraying.
3. The method for preparing hexahydrophthalide using tetrahydrophthalic anhydride according to claim 1, characterized in that, The solvent is one or more of 1,4-dioxane, tetrahydrofuran, and γ-butyrolactone.
4. The method for preparing hexahydrophthalide using tetrahydrophthalic anhydride according to claim 1, characterized in that, The tetrahydrophthalic anhydride is cis-1,2,3,6-tetrahydrophthalic anhydride or 3,4,5,6-tetrahydrophthalic anhydride, and the product hexahydrophthalide is cis-hexahydrophthalide or a mixture of cis-hexahydrophthalide and trans-hexahydrophthalide.
Citation Information
Patent Citations
Preparation of lactone
JP1982091984A