Quad flat no-lead (QFN) packaging process with wettable flanks with exposed pins
By adopting a wettable flank process with exposed pins in the QFN package, the problem of welding defects in the QFN package in the existing technology is solved, the welding quality and device performance are improved, and it is suitable for miniaturized, high-performance electronic products.
Patent Information
- Application Number
- CN202410730549.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-06
- Publication Date
- 2024-10-11
AI Technical Summary
Existing QFN packaging technology has welding defects in ultra-fine pitch pins, high-density assembly and high-speed signal transmission, such as signal pad bridging, heat dissipation pad voids and insufficient tin crawl height of side solder joints, which affects the electrical performance and performance of the device. reliability.
The wettable flank QFN packaging process with exposed pins is adopted, including micro lead frame copper substrate packaging, electroplating treatment, tin plating layer addition, optimized PCB pad and solder paste printing template design, reflow soldering process and quality control. Monitor weld quality via X-ray and automated optical inspection.
Significantly improves the solderability of side pins, reduces tin failure, ensures solder joint integrity and electrical connection stability, optimizes heat dissipation efficiency and signal performance, reduces rework rate, improves production efficiency, and meets high-end requirements reliability requirements.
Smart Images

Figure CN118763003A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of QFN packaging, and in particular relates to a QFN packaging process with wettable flanks and exposed pins. Background Art
[0002] In the existing QFN packaging technology, QFN devices are widely used in various electronic devices due to their miniaturization, light weight and excellent electrical performance. However, as electronic devices develop towards higher performance and smaller size, the process requirements for QFN packaging are becoming increasingly higher. Traditional QFN packaging is prone to various defects during the assembly process, such as signal pad bridging, heat dissipation pad voids, insufficient side solder joint creep height, etc. These problems seriously affect the electrical performance and reliability of the device.
[0003] QFN devices are usually packaged in a micro lead frame copper substrate, with a large heat sink pad in the center of the bottom, and signal pads arranged around the heat sink pad matrix. In the ultra-fine pitch pin design, the control accuracy of solder paste printing is extremely high to avoid welding defects such as bridging. In addition, the void problem of the heat sink pad is also one of the key factors affecting device performance. Since the solvent in the solder paste is difficult to completely volatilize during the welding process, it is easy to form voids in the solder joints, affecting the heat dissipation efficiency and signal transmission performance. Summary of the invention
[0004] In view of the shortcomings of the prior art, the present invention provides a wettable flank QFN packaging process with exposed pins, aiming to overcome the defects of the existing QFN packaging in ultra-fine pitch pins, high-density assembly and high-speed signal transmission through innovative design and process flow, and improve the welding quality and the overall performance of the device.
[0005] In order to achieve the above object, the following technical solution is adopted: The present invention provides a wettable flank QFN packaging process with exposed pins, comprising the following steps:
[0006] S1. Package design: The package adopts the micro lead frame copper substrate package. The lead frame is directly exposed at the bottom of the package as a soldering terminal. A large exposed heat dissipation pad is designed in the center of the bottom of the package. Small pads arranged in a matrix are surrounded by the large heat dissipation soldering terminal.
[0007] S2. Exposed pin processing: Design exposed pins on the side of the package, and electroplate these pins to ensure their solderability. Use cutting and separation packaging to ensure that the pin cuts are not electroplated to avoid oxidation during storage;
[0008] S3, Wettable Flank Process: Adds a tin plating layer to the flank of the package to protect the copper and improve soldering performance. This process allows visual inspection to ensure good lap soldering and stable electrical connections.
[0009] S4. Design of PCB pads: When designing PCB pads, they should be slightly larger than the pin ends of QFN devices to ensure that the toes of the signal pad pins are filled, and a gap of 0.2mm is reserved between the heat dissipation pad and the surrounding signal pads to prevent bridging;
[0010] S5. Solder paste printing template design: When designing the template, the area ratio and thickness-width ratio requirements should be met. The template opening and PCB pad size should be 1:1. For fine-pitch pins, the template opening should be appropriately reduced to prevent bridging of adjacent pins.
[0011] S6, reflow soldering: after the preheating stage, thermal activation stage, thermal activation stage and cooling stage, the volatilization of the solvent in the solder paste is controlled to reduce the formation of voids, and nitrogen protection is used to remove the oxide layer of the side pins to improve their solderability;
[0012] S7. Quality control: Monitor the welding quality through X-ray inspection and automatic optical inspection to ensure that there are no bridges or voids in the solder joints, and that the tin climbing height of the side solder joints meets the requirements.
[0013] Furthermore, the thickness of the electroplating layer of the exposed pins should be controlled within 5-15 μm.
[0014] Furthermore, the thickness of the tin-plated layer should be controlled within 5-10 μm.
[0015] Furthermore, the area ratio of the template openings is greater than 0.66, and the thickness-to-width ratio is greater than 1.5.
[0016] Furthermore, the temperature in the preheating stage is controlled at 120-150° C. and the duration is 30-60 seconds.
[0017] Furthermore, the temperature of the thermal activation stage is controlled at 180-200° C. and the duration is 60-90 seconds.
[0018] Furthermore, the peak temperature of the thermal activation stage is controlled at 235-255° C., and the duration is 20-30 seconds.
[0019] Furthermore, the cooling rate in the cooling stage is 20-30°C / min.
[0020] The beneficial effects of the present invention are as follows: the present invention significantly improves the solderability of the side pins through the wettable flank process, reduces the situation of tinning failure, ensures the integrity of the solder joints and the stability of the electrical connections, optimizes the heat dissipation pad design and the application of heat dissipation vias, improves the heat dissipation efficiency of the device, ensures the performance of high-speed and radio frequency signals, and the precise PCB pad design and solder paste printing template design reduce the formation of signal pad bridging and heat dissipation pad voids, thereby improving the reliability of the product. Through the optimized packaging design and welding process, the defects in the assembly process are reduced, the rework rate is reduced, and the production efficiency is improved. The packaging process scheme meets the requirements of electronic products for high reliability and is suitable for application scenarios with strict requirements for miniaturization, thinness, and high performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 FIG. 4 is a process flow diagram for a wettable flank QFN package process with exposed leads.
[0022] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention. DETAILED DESCRIPTION
[0023] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0024] Unless otherwise defined, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. In addition, any methods and materials similar or equivalent to those described herein may be applied to the present invention. The preferred implementation methods and materials described herein are for demonstration purposes only and are not intended to limit the content of this application.
[0025] The experimental methods in the following examples are conventional methods unless otherwise specified, and the experimental materials used in the following examples are purchased from commercial channels unless otherwise specified.
[0026] Example
[0027] A wettable flank QFN packaging process with exposed leads
[0028] The packaging process comprises the following steps:
[0029] S1. Package design: The package form of micro lead frame copper substrate is adopted. The copper substrate has good electrical and thermal conductivity. At the same time, the processability of copper is also conducive to the realization of complex package design. The lead frame is directly exposed at the bottom of the package as a welding end. A large area of exposed heat dissipation pad is designed in the center of the bottom of the package. Small pads arranged in a matrix are surrounded by the large heat dissipation welding end.
[0030] S2. Exposed pin processing: Design exposed pins on the side of the package, and electroplate these pins to ensure their solderability. Use cutting and separation packaging to ensure that the pin cuts are not electroplated to avoid oxidation during storage;
[0031] The electroplating treatment of the exposed pins is to enhance their solderability and corrosion resistance. The electroplating layer is usually composed of tin or tin alloy, because tin has a low melting point and good wettability, which helps to form a uniform and strong solder joint during the soldering process. During the electroplating process, the pin cutout is not electroplated to prevent the copper material at the cutout from oxidizing during storage. Copper oxide will reduce the soldering quality;
[0032] S3, Wettable Flank Process: Adds a tin plating layer to the flank of the package to protect the copper and improve soldering performance. This process allows visual inspection to ensure good lap soldering and stable electrical connections.
[0033] The wettable flank process improves soldering performance by adding a tin layer on the package flank. The tin layer not only protects the copper from oxidation, but also forms good wettability during the soldering process, which helps the solder spread evenly on the flank to form a stable electrical connection. In addition, the tin layer can also reflect the heat generated during the soldering process, reducing the impact of heat on the inside of the package.
[0034] S4. Design of PCB pads: When designing PCB pads, they should be slightly larger than the pin ends of QFN devices to ensure that the toes of the signal pad pins are filled, and a gap of 0.2mm is reserved between the heat dissipation pad and the surrounding signal pads to prevent bridging;
[0035] The design of the PCB pad needs to take into account the matching with the pin solder end of the QFN device. The pad is slightly larger than the pin solder end to ensure that the solder can form sufficient filling around the pin and enhance the mechanical strength of the solder joint. The 0.2mm gap is reserved to prevent solder bridging during the soldering process, which may cause a short circuit and affect the normal operation of the device.
[0036] S5. Solder paste printing template design: When designing the template, the area ratio and thickness-width ratio requirements should be met. The template opening and PCB pad size should be 1:1. For fine-pitch pins, the template opening should be appropriately reduced to prevent bridging of adjacent pins.
[0037] The design of the solder paste printing template needs to meet the requirements of area ratio and thickness-width ratio to ensure uniform distribution of solder paste and proper solder joint formation. The 1:1 ratio of the template opening to the PCB pad size is to ensure that the solder paste can be accurately printed on the pad to avoid soldering problems caused by too much or too little solder paste. For fine-pitch pins, the template opening is reduced to reduce the risk of solder bridging between adjacent pins.
[0038] S6, reflow soldering: after the preheating stage, thermal activation stage, thermal activation stage and cooling stage, the volatilization of the solvent in the solder paste is controlled to reduce the formation of voids, and nitrogen protection is used to remove the oxide layer of the side pins to improve their solderability;
[0039] S7. Quality control: Monitor the welding quality through X-ray inspection and automatic optical inspection to ensure that there are no bridges or voids in the solder joints, and that the tin climbing height of the side solder joints meets the requirements.
[0040] The thickness of the electroplating layer of the exposed pins should be controlled within 10 μm.
[0041] The thickness of the tin-plated layer should be controlled at 6 μm.
[0042] The area ratio of the template openings is greater than 0.66, and the thickness-to-width ratio is greater than 1.5.
[0043] The temperature in the preheating stage is controlled at 1250° C. and lasts for 50 seconds. The preheating stage temperature is used to activate the flux in the solder paste.
[0044] The temperature of the thermal activation stage is controlled at 190°C for 80 seconds to remove moisture and volatile substances in the solder paste.
[0045] The peak temperature of the thermal activation stage is controlled at 235-255°C and lasts for 20-30 seconds. The melting and welding process of the solder is completed through the thermal activation stage.
[0046] The cooling rate of the cooling stage is 15° C. / min, and the solder joint is quickly cooled to room temperature during the cooling stage to lock the solder joint morphology and prevent the solder joint from collapsing.
[0047] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
[0048] The present invention and its implementation methods are described above, which is not restrictive. The drawings are only one of the implementation methods of the present invention, and the actual application is not limited thereto. In short, if ordinary technicians in the field are inspired by it and design methods and embodiments similar to the technical solution without creativity without departing from the purpose of the invention, they should all fall within the protection scope of the present invention.
Claims
1. A wettable flank QFN packaging process with exposed leads, characterized in that: The steps include: S1. Package design: The package adopts the micro lead frame copper substrate package. The lead frame is directly exposed at the bottom of the package as a soldering terminal. A large exposed heat dissipation pad is designed in the center of the bottom of the package. Small pads arranged in a matrix are surrounded by the large heat dissipation soldering terminal. S2. Exposed pin processing: Design exposed pins on the side of the package, and electroplate these pins to ensure their solderability. Use cutting and separation packaging to ensure that the pin cuts are not electroplated to avoid oxidation during storage; S3, Wettable Flank Process: Adds a tin plating layer to the flank of the package to protect the copper and improve soldering performance. This process allows visual inspection to ensure good lap soldering and stable electrical connections. S4. Design of PCB pads: When designing PCB pads, they should be slightly larger than the pin ends of QFN devices to ensure that the toes of the signal pad pins are filled, and a gap of 0.2mm is reserved between the heat dissipation pad and the surrounding signal pads to prevent bridging; S5. Solder paste printing template design: When designing the template, the area ratio and thickness-width ratio requirements should be met. The template opening and PCB pad size should be 1:
1. For fine-pitch pins, the template opening should be appropriately reduced to prevent bridging of adjacent pins. S6, reflow soldering: after the preheating stage, thermal activation stage, thermal activation stage and cooling stage, the volatilization of the solvent in the solder paste is controlled to reduce the formation of voids, and nitrogen protection is used to remove the oxide layer of the side pins to improve their solderability; S7. Quality control: Monitor the welding quality through X-ray inspection and automatic optical inspection to ensure that there are no bridges or voids in the solder joints, and that the tin climbing height of the side solder joints meets the requirements.
2. A wettable flank QFN packaging process with exposed pins according to claim 1, characterized in that: The thickness of the electroplating layer of the exposed pins should be controlled within 5-15 μm.
3. A wettable flank QFN packaging process with exposed pins according to claim 2, characterized in that: The thickness of the tin-plated layer should be controlled at 5-10 μm.
4. A wettable flank QFN packaging process with exposed pins according to claim 3, characterized in that: The area ratio of the template openings is greater than 0.66, and the thickness-to-width ratio is greater than 1.
5.
5. A wettable flank QFN packaging process with exposed pins according to claim 4, characterized in that: The temperature in the preheating stage is controlled at 120-150°C and lasts for 30-60 seconds.
6. A wettable flank QFN packaging process with exposed pins according to claim 5, characterized in that: The temperature of the thermal activation stage is controlled at 180-200° C. and the duration is 60-90 seconds.
7. A wettable flank QFN packaging process with exposed pins according to claim 6, characterized in that: The peak temperature of the thermal activation stage is controlled at 235-255° C. and lasts for 20-30 seconds.
8. A wettable flank QFN packaging process with exposed pins according to claim 7, characterized in that: The cooling rate in the cooling stage is 20-30°C / min.
Citation Information
Cited By
WF process and application thereof in DFN packaging
CN120109031A
Welding defect intelligent detection method of AOI equipment and AOI equipment