Method for preparing polyethylene glycol derivative

Through the reslurry washing method and the control of solvent ratio and temperature, the problems of increasing thermal history and low production efficiency in the purification of polyethylene glycol derivatives were solved, and high efficiency, high purity and uniform preparation of polyethylene glycol derivatives were achieved. Suitable for industrial applications.

CN118922470APending Publication Date: 2024-11-08NOF CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380028239.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-17
Filing Date
2023-03-14
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the prior art, when purifying polyethylene glycol derivatives, repeated reprecipitation processes lead to an increase in thermal history, resulting in an increase in polydispersity, a decrease in production efficiency, and it is difficult to carry out on a large scale in industrial scale.

Method used

Using the reslurry washing method, the washing is performed using a specific proportion of organic solvent mix to avoid heating and dissolution steps. By controlling the solvent ratio and temperature, the reslurry washing is repeated to remove impurities, and reprecipitation is carried out under appropriate conditions to obtain high purity. Polyethylene glycol derivatives.

Benefits of technology

Effectively remove impurities, reduce heat history, shorten production time, and achieve efficient, high-purity and uniform quality preparation of polyethylene glycol derivatives. It is suitable for industrial production, without the need for carriers or ion exchange resins, improving productivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005046701920000081
    Figure BDA0005046701920000081
  • Figure BDA0005046701920000121
    Figure BDA0005046701920000121
  • Figure BDA0005046701920000131
    Figure BDA0005046701920000131
Patent Text Reader

Abstract

A crude polyethylene glycol derivative comprising a polyethylene glycol derivative and impurities is mixed with a mixed organic solvent comprising an organic solvent A and an organic solvent B to form a slurry, the slurry is re-washed, and the polyethylene glycol derivative is subsequently recovered from the mixed organic solvent, the polyethylene glycol derivative has, at its terminal, at least one selected from the group consisting of a functional group capable of reacting with a biologically relevant substance, a functional group serving as a precursor of the functional group, and a protecting group of the functional group, and the polyethylene glycol derivative is dissolved in a good solvent and then returned to the collection of the polyethylene glycol derivative. If (mass of organic solvent A / (mass of organic solvent A + mass of organic solvent B) is Y, and the temperature during repulping washing is T (DEG C), Y and T satisfy the following relationship: 0.5 < = Y * T < = 30.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for preparing purified polyethylene glycol derivatives. Background Art

[0002] When a drug using biologically related substances such as hormones, cytokines and enzymes is administered to a normal living body, it is rapidly excreted from the organism through glomerular filtration of the kidneys and uptake by macrophages of the liver or spleen. Therefore, the half-life of the drug in the blood is short, and sufficient pharmacological effects may not be obtained. In order to solve this problem, drugs have been developed in which biologically related substances are chemically modified with water-soluble polymers such as polyethylene glycol or albumin. By increasing the molecular weight of the chemically modified biologically related substance and forming a hydration layer, its half-life in the blood can be extended.

[0003] Polyethylene glycol is the most commonly used modifying agent used to improve the properties of bio-related substances, and currently, there are several polyethylene glycol-modified drugs on the market and used in medical settings around the world.

[0004] From the perspective of drug performance and safety, the polyethylene glycol derivatives used as drug raw materials or drug additives need few impurities and high homogeneity. The impurities contained in the polyethylene glycol derivatives can be divided into high molecular weight compounds and low molecular weight compounds, and between these two impurities, the low molecular weight compounds used when the low molecular weight compound impurities are derived from the derivatization polyethylene glycol end. The impurities derived from low molecular weight compounds usually have reactive functional groups, which can cause unexpected side reactions when chemically modifying biological related substances, causing impurities to be produced in the drug, and therefore, it is expected that the impurity content is low. Due to the requirement that the drug quality in each production batch remains consistent, the polyethylene glycol derivatives used as drug raw materials or drug additives also require that the impurity content in each production batch remains consistent.

[0005] Generally, when removing low molecular weight compounds as impurities from amphiphilic high molecular weight compounds such as polyethylene glycol, purification methods such as dialysis, ultrafiltration, ion exchange chromatography, extraction and reprecipitation utilizing differences in molecular weight and physicochemical properties as shown in Non-Patent Document 1 can be used.

[0006] First, dialysis and ultrafiltration are separation methods that utilize molecular weight differences, and techniques such as ion exchange chromatography are separation methods that utilize electrostatic interaction differences. In order to utilize these purification methods, the low molecular weight compounds to be separated must be water soluble. Therefore, when the low molecular weight impurities are hydrophobic compounds, it is difficult to effectively purify the low molecular weight impurities using these methods.

[0007] Next, extraction is illustrated as a separation method utilizing the solubility difference in water and organic solvents. In extraction, the necessary condition is that the solubility of the target substance and the impurity in water or organic solvent is significantly different. Amphiphilic polyethylene glycol has an extremely unique property, that is, in a two-phase system, by using appropriate conditions, polyethylene glycol can be selectively distributed to any one of the organic layer or the aqueous layer during extraction. Therefore, when the impurity is a water-soluble compound, it is possible to purify by distributing polyethylene glycol into the organic layer and distributing the impurity into the aqueous layer. When the impurity is a hydrophobic compound, it is possible to purify by distributing polyethylene glycol into the aqueous layer and distributing the impurity into the organic layer. However, depending on the polyethylene glycol derivative, the reactive functional group used to modify the drug may be hydrolyzed, resulting in quality degradation, and therefore applicable polyethylene glycol derivatives are limited.

[0008] Similar to extraction, reprecipitation is a separation method that utilizes the difference in solubility between a target substance and impurities in a solvent, and is a method of removing impurities by only reducing the solubility of the target substance in a solution, precipitating the target substance, and then separating the precipitate from the solution containing impurities. There are several reprecipitation techniques, such as a method of cooling a solution to reduce the solubility of a target substance and a method of adding a poor solvent to reduce the solubility of a target substance, and generally, by repeating reprecipitation multiple times, a high-purity polyethylene glycol derivative with a low impurity content required for a pharmaceutical raw material or a pharmaceutical additive can be obtained. This is because polyethylene glycol has the property that its polymer chains entangle with each other and embrace impurities and solvents to precipitate, and it is difficult to completely separate the precipitate from the solution containing impurities, and therefore, it is necessary to gradually reduce the impurity concentration in the system by repeating reprecipitation multiple times. Patent document 1 describes reprecipitation by adding hexane as a poor solvent to a polyethylene glycol derivative dissolved in heated ethyl acetate.

[0009] Repulp washing is also a separation method that utilizes the difference in solubility between a high molecular weight compound and impurities in a solvent. Repulp washing is a washing treatment using a solvent that dissolves only impurities but not the target substance, and can remove impurities by separating a solution containing the target substance and impurities after this repulp washing.

[0010] Prior art documents

[0011] Non-patent literature

[0012] Non-patent document 1: Harris, JM Poly (Ethylene Glycol) Chemistry; Plenum Press: New York, 1992

[0013] Non-patent literature 2: Green's Protective Groups in Organic Synthesis Fifth Edition, Peter GMWuts

[0014] Non-patent document 3: Gross, Hans; Bilk, L. Tetrahedron (1968), 24 (24), 6935-9

[0015] Patent Literature

[0016] Patent Document 1: JP2004-197077A Summary of the invention

[0017] Problems to be solved by the present invention

[0018] Since the organic solvent is used as both a good solvent and a poor solvent in the reprecipitation, the risk of hydrolysis is low even for a polyethylene glycol derivative having a reactive functional group sensitive to water, and hydrophobic compounds can be removed. By repeating the reprecipitation multiple times, a high-purity and high-quality polyethylene glycol derivative with a low impurity content required for a pharmaceutical raw material or a pharmaceutical additive can be obtained, and thus the reprecipitation can be used as a method for removing impurities from a polyethylene glycol derivative and purifying the polyethylene glycol derivative.

[0019] However, repeated purification of polyethylene glycol derivatives by reprecipitation may result in a decrease in quality. This is because heating is required when the precipitate of the polyethylene glycol derivative is dissolved in a good solvent, and repeated heating and dissolving steps increase the thermal history, which leads to an increase in polydispersity due to oxidative decomposition of the polyethylene glycol chain. An increase in the number of reprecipitations also leads to an increase in the number of production steps, i.e., an extension of the production time, and thus a decrease in production efficiency.

[0020] Therefore, although polyethylene glycol derivatives are important materials for medical applications, polyethylene glycol derivatives have not yet been obtained through a simple industrial preparation method.

[0021] The object of the present invention is to provide an industrially feasible method for purifying polyethylene glycol, which can provide polyethylene glycol derivatives with high efficiency, high purity and uniform quality, and can prevent the increase of polydispersity due to increased thermal history.

[0022] Solutions to the problem

[0023] That is, the present invention is as follows.

[0024] (1) A method for preparing a polyethylene glycol derivative, the method comprising:

[0025] (A) a step of preparing a crude polyethylene glycol derivative, the crude polyethylene glycol derivative comprising a polyethylene glycol derivative and impurities, the polyethylene glycol derivative having at its terminal at least one member selected from the group consisting of a functional group capable of reacting with a bio-related substance, a functional group serving as a precursor of the functional group, and a protective group for the functional group;

[0026] (B) mixing the crude polyethylene glycol derivative with a mixed organic solvent comprising an organic solvent A and an organic solvent B to form a slurry, subjecting the slurry to re-slurry washing, and then recovering the polyethylene glycol derivative from the mixed organic solvent; and

[0027] (C) dissolving the polyethylene glycol derivative obtained in step (B) in a good solvent, and then recovering the polyethylene glycol derivative from the good solvent, wherein

[0028] The organic solvent A is selected from the group consisting of xylene, toluene, benzene, methyl acetate, ethyl acetate, butyl acetate, acetonitrile, acetone, N,N-dimethylformamide (DMF), dimethyl sulfoxide (DMSO), chloroform, dichloromethane and combinations thereof,

[0029] The organic solvent B is selected from the group consisting of pentane, hexane, heptane, diethyl ether, methyl tert-butyl ether (MTBE) and combinations thereof, and

[0030] Assuming that the mass ratio of organic solvent A to the total value of the mass of organic solvent A and the mass of organic solvent B (mass of organic solvent A / (mass of organic solvent A+mass of organic solvent B)) is Y, and the temperature during repulp washing is T (° C.), Y and T satisfy the following relationship.

[0031] 0.5≤Y×T≤30

[0032] (2) The method according to (1), wherein step (B) is repeated multiple times.

[0033] (3) The method according to (1) or (2), wherein the organic solvent A is ethyl acetate or a mixed solvent of ethyl acetate and acetonitrile, and the organic solvent B is hexane.

[0034] (4) The method according to any one of (1) to (3), wherein the mass of the organic solvent A and the mass of the organic solvent B are each 1 to 50 times the mass of the polyethylene glycol derivative, and the temperature during the reslurry washing is 1° C. to 33° C.

[0035] Effects of the Invention

[0036] Reslurry washing is an operation of washing the polyethylene glycol derivative still in a slurry state with an organic solvent, and since purification can be performed without heating and dissolving the polyethylene glycol derivative, it is expected to reduce thermal history and prevent increase in polydispersity. However, there are no reports on the type of solvent and temperature suitable for reslurry washing of polyethylene glycol derivatives.

[0037] Therefore, the inventors of the present invention specifically studied re-pulping and washing of polyethylene glycol derivatives containing impurities, and found that by performing re-pulping and washing using two or more organic solvents mixed in a specific weight ratio, impurities can be effectively removed while preventing quality deterioration due to increased thermal history and significantly shortening production time.

[0038] In addition, it was revealed that although re-slurry washing can effectively remove impurities, it is insufficient in terms of the homogenization ability required for pharmaceutical raw materials, and it was found that by performing reprecipitation (a step of dissolving a polyethylene glycol derivative in a good solvent and then recovering the polyethylene glycol derivative) after re-slurry washing, a target substance with uniform quality can be obtained.

[0039] The purification method of the present invention can be achieved by controlling the weight ratio of two or more organic solvents used in the reslurry washing and the temperature during the reslurry washing within an appropriate range. Unlike other purification methods, no carrier / adsorbent such as a resin or a gel for purification is required, nor is an ultrafiltration membrane required, and thus the purification method of the present invention can be carried out industrially on a large scale.

[0040] Thus, the present invention is a novel purification method for obtaining a polyethylene glycol derivative as a pharmaceutical raw material or a pharmaceutical additive with high efficiency, high purity and uniform quality. The present purification method utilizes the unique solubility of the polyethylene glycol derivative, can effectively separate and remove impurities, and in addition, can obtain a polyethylene glycol derivative with high purity and uniform quality required for a pharmaceutical raw material or a pharmaceutical additive. The present purification method can be easily carried out industrially, has excellent productivity, and can be carried out at a high yield through a step that does not generate waste materials such as an adsorbent or an ion exchange resin. DETAILED DESCRIPTION

[0041] The number average molecular weight of the polyethylene glycol derivative of the present invention is a value obtained by gel permeation chromatography (GPC) analysis, and is a number average molecular weight calculated based on a calibration curve made using polyethylene glycols of various known molecular weights. The number average molecular weight of the polyethylene glycol derivative is not particularly limited, and is preferably 2000 to 160000, more preferably 2000 to 120000, and even more preferably 2000 to 80000. Note that the polyethylene glycol derivative having a number average molecular weight less than 2000 may be liquid at room temperature, and in this case, it is difficult to form a slurry using a mixed organic solvent, which makes the present invention difficult to implement.

[0042] The polyethylene glycol derivative of the present invention has at its terminal one or more of a functional group capable of reacting with a bio-related substance, a functional group serving as a precursor of the functional group, and the protective group.

[0043] The functional group capable of reacting with a bio-related substance is not particularly limited as long as it is a functional group capable of chemically bonding to a functional group of a bio-related substance such as an amino group, a thiol group, an aldehyde group, a carboxyl group, an unsaturated bond or an azide group. Specifically, examples thereof include an active ester group, an active carbonate group, an aldehyde group, an isocyanate group, an isothiocyanate group, an epoxy group, a carboxyl group, a mercapto group, a maleimide group, a substituted maleimide group, a hydrazide group, a dithiopyridyl group, a substituted sulfonate group, a vinylsulfonyl group, an amino group, an oxyamino group (H2N-O- group), an iodoacetamide group, an alkylcarbonyl group, an alkenyl group (e.g., an allyl group, a vinyl group), an alkynyl group, a substituted alkynyl group (e.g., an alkynyl group substituted with a hydrocarbon group having 1 to 5 carbon atoms described below), an azido group, an acrylic group, a sulfonyloxy group (e.g., an alkylsulfonyloxy group) and an α-halogenated hexadecyl group, and preferred examples thereof include an active ester group, an active carbonate group, an aldehyde group, an isocyanate group, an isothiocyanate group, an epoxy group , maleimide group, substituted maleimide group, vinylsulfonyl group, acrylic group, sulfonyloxy group (e.g., alkyl-sulfonyloxy group having 1 to 5 carbon atoms), substituted sulfonic acid group, carboxyl group, mercapto group, pyridyldisulfide group, α-halohexadecyl group, alkynyl group, substituted alkynyl group (e.g., alkynyl group having 2 to 5 carbon atoms substituted by hydrocarbon group having 1 to five carbon atoms as described below), allyl group, vinyl group, amino group, oxyamino group, hydrazide group and azido group, and more preferred examples include active ester group, active carbonate group, aldehyde group, maleimide group, carboxyl group, mercapto group, oxyamino group and amino group, and particularly preferred examples include active ester group, active carbonate group, maleimide group, carboxyl group, mercapto group and oxyamino group.

[0044] Specifically, the functional groups capable of reacting with bio-related substances can be divided into the following groups (I), (II), (III), (IV), (V), and (VI).

[0045] Group (I): Functional groups that can react with the amino groups of biologically relevant substances

[0046] Examples thereof include functional groups represented by the following (a), (b), (c), (d), (e), (f), (g), (j), and (k).

[0047] Group (II): Functional groups that can react with sulfhydryl groups of biologically relevant substances

[0048] Examples thereof include functional groups represented by the following (a), (b), (c), (d), (e), (f), (g), (h), (i), (j), (k), and (l).

[0049] Group (III): Functional groups that can react with aldehyde groups of biologically relevant substances

[0050] Examples thereof include functional groups represented by the following (h), (m), (n), and (p).

[0051] Group (IV): Functional groups that can react with the carboxyl groups of biologically relevant substances

[0052] Examples thereof include functional groups represented by the following (h), (m), (n), and (p).

[0053] Group (V): Functional groups that can react with unsaturated bonds of biologically relevant substances

[0054] Examples thereof include functional groups represented by the following (h), (m) and (o).

[0055] Group (VI): Functional groups capable of reacting with the azide group of biologically relevant substances

[0056] Examples thereof include functional groups represented by the following (1).

[0057]

[0058] In the functional group (j), U1 in the formula represents a halogen atom such as a chlorine atom (Cl), a bromine atom (Br) or an iodine atom (I), and is preferably Br or I, and more preferably I.

[0059] In the functional group (e) and the functional group (l), Y in the formula 1 , Y 3 Each independently represents a hydrogen atom or a hydrocarbon group having 1 to 5 carbon atoms. Specific examples of the hydrocarbon group having 1 to 5 carbon atoms include methyl, ethyl, propyl, isopropyl, butyl and tert-butyl. 1 , Y 3 Preferred is a hydrogen atom, a methyl group or an ethyl group.

[0060] In the functional group (k), Y 2 represents a hydrocarbon group having 1 to 10 carbon atoms which may contain a fluorine atom, specific examples of which include methyl, ethyl, propyl, isopropyl, butyl, tert-butyl, hexyl, nonyl, vinyl, phenyl, benzyl, 4-methylphenyl, trifluoromethyl, 2,2,2-trifluoroethyl and 4-(trifluoromethoxy)phenyl, and preferred examples thereof include methyl, vinyl, 4-methylphenyl and 2,2,2-trifluoroethyl.

[0061] The active ester group is an ester group of an alkoxy group having a high leaving ability. Examples of the alkoxy group having a high leaving ability include alkoxy groups derived from nitrophenol, N-hydroxysuccinimide, pentafluorophenol, etc. The active ester group is preferably an ester group having an alkoxy group derived from N-hydroxysuccinimide.

[0062] The active carbonate group is a carbonate group of an alkoxy group with high leaving ability. Examples of the alkoxy group with high leaving ability include alkoxy groups derived from nitrophenol, N-hydroxysuccinimide, pentafluorophenol, etc. The active carbonate group is preferably a carbonate group having an alkoxy group derived from nitrophenol or N-hydroxysuccinimide.

[0063] The substituted maleimide group is a maleimide group in which a hydrocarbon group is bonded to one carbon atom of the double bond of the maleimide group. Specific examples of the hydrocarbon group include methyl, ethyl, propyl, isopropyl, butyl and tert-butyl groups, and preferred examples thereof include methyl and ethyl groups.

[0064] The substituted sulfonic acid group is a sulfonic acid group in which the sulfur atom of the sulfonic acid group is bonded to a hydrocarbon group which may contain a fluorine atom. Specific examples of the hydrocarbon group which may contain a fluorine atom include methyl, ethyl, propyl, isopropyl, butyl, tert-butyl, hexyl, nonyl, vinyl, phenyl, benzyl, 4-methylphenyl, trifluoromethyl, 2,2,2-trifluoroethyl and 4-(trifluoromethoxy)phenyl, and preferred examples thereof include methyl, vinyl, 4-methylphenyl and 2,2,2-trifluoroethyl.

[0065] The functional group that is a precursor of a functional group that can react with a biologically related substance refers to a functional group that is in the previous stage of a chemical reaction that generates a functional group that can react with a biologically related substance. For example, since a cyano group can be hydrolyzed to provide a carboxyl group and reduced to provide an aldehyde group or an amino group, a cyano group can be exemplified as a precursor of a functional group. Since a hydroxyl group can be converted into a functional group that can react with a biologically related substance by a chemical reaction, a hydroxyl group can also be exemplified as a precursor.

[0066] The protective group of the functional group that can react with biological related substances is the part that stops or blocks the reaction of specific chemical reactive functional group under certain reaction conditions.The functional group protected by the protected group can be deprotected, that is, the reaction conditions suitable for each protective group are used to carry out chemical reaction, to regenerate the original functional group.The type of protective group is not particularly limited, and can depend on the type of the chemical reactive functional group to be protected, the use period condition and the existence of other functional groups or protective groups in the molecule and select from various types, and specific examples can be found in many common books (seeing above-mentioned non-patent literature 2).For example, the example of the protective group of hydroxyl includes benzyl, p-methoxyphenyl benzyl, methoxymethyl, tert-butyl, trimethylsilyl, triethylsilyl, tert-butyldimethylsilyl, acetyl, benzoyl and trityl.The example of the protective group of carboxyl includes methyl ester group, ethyl ester group, benzyl ester group and tert-butyl ester group. Examples of the protecting group of the amino group include tert-butyloxycarbonyl, benzyloxycarbonyl, 9-fluorenylmethyloxycarbonyl, 2,2,2-trichlorooxycarbonyl, allyloxycarbonyl, phthaloyl, p-toluenesulfonyl, and 2-nitrobenzenesulfonyl. Examples of the protecting group of the aldehyde group include a dimethylacetal group, a diethylacetal group, a cyclic acetal group, and a dithioacetal group. Examples of the protecting group of the mercapto group include the same ones as the protecting groups of the above-mentioned hydroxyl group.

[0067] The polyethylene glycol derivative of the present invention is a polyethylene glycol derivative having one or more of a functional group capable of reacting with a bio-related substance, a functional group serving as a precursor for modifying a functional group, or a protective group for the functional group.

[0068] (Step (A))

[0069] Step (A) is a step of preparing a crude polyethylene glycol derivative, which contains a polyethylene glycol derivative and impurities, wherein the polyethylene glycol derivative has one or more of a functional group capable of reacting with a bio-related substance, a functional group serving as a precursor of the functional group, or a protective group of the functional group.

[0070] In step (A), in the preparation of the polyethylene glycol derivative, after the reaction step or other treatment steps, the solution in which impurities and the polyethylene glycol derivative are dissolved is reprecipitated by adding an organic solvent as a poor solvent to the solution to precipitate the crude polyethylene glycol derivative. Then, by stirring at a specific temperature for a period of time, the crude polyethylene glycol derivative can be separated and recovered from the mixed organic solvent.

[0071] The crude polyethylene glycol derivative is a composition containing the polyethylene glycol derivative and impurities.

[0072] The impurities are impurities contained in the polyethylene glycol derivative, specifically, low molecular weight compounds used in the reaction for producing the polyethylene glycol derivative and by-products generated by using these compounds. Examples of such compounds include N-hydroxysuccinimide (NHS), N,N'-dicyclohexylcarbodiimide (DCC), N-succinimidyl-6-maleimidocaproic acid (SMH), N-succinimidyl-3-maleimidocaproic acid (SMP) and di(N-succinimidyl) carbonate (DSC), which are used in the derivatization reactions represented by formulas (1), (2), (3), (4) and (5), and examples of such by-products include di(N-succinimidyl) glutaric acid (Glu-diNHS) and N,N'-dicyclohexylurea (DCU) by-produced in a reaction using glutaric anhydride, NHS and DCC, and N-succinimidylcarbonyl-β-alanine-N-succinimidyl ester (β-Ala-diNHS) by-produced in a reaction using NHS and DCA. It is known that β-Ala-diNHS is produced by the mechanism represented by formula (6) (see the above-mentioned Non-Patent Document 3).

[0073]

[0074]

[0075]

[0076]

[0077]

[0078]

[0079] (Step (B))

[0080] Step (B) is a step of slurrying the crude polyethylene glycol derivative obtained in step (A) using a mixed organic solvent comprising organic solvent A and organic solvent B, reslurry washing the slurry (washing with a solvent that does not dissolve the target substance but only dissolves impurities), and then separating and recovering the polyethylene glycol derivative from the mixed organic solvent.

[0081] In the reslurry washing of the present invention, a mixed organic solvent prepared in advance is added to a crude polyethylene glycol derivative to form a slurry, which is then stirred and washed at a prescribed temperature (T)° C. for a prescribed time (stirring time).

[0082] First, a pre-prepared mixed organic solvent of organic solvent A and organic solvent B is added to the crude polyethylene glycol derivative containing impurities prepared in step (A) to perform re-slurry washing. Then, the slurry is stirred at a specific temperature for a period of time, and the polyethylene glycol derivative is recovered from the mixed organic solvent.

[0083] Compared with reprecipitation, this step does not require the operation of dissolving the polyethylene glycol derivative in a good solvent by heating and the operation of precipitating by adding a poor solvent, and has the advantage of reducing the number of steps compared with a purification method of repeating redissolution in a solvent and reprecipitation.

[0084] In the reprecipitation method, polyethylene glycol derivatives (especially polyethylene glycol with a number average molecular weight of 2000 or more) are hardly soluble in good solvents such as ethyl acetate and toluene used for reprecipitation at room temperature, and therefore require heating to dissolve. Reslurry washing of polyethylene glycol derivatives eliminates the need for heating and dissolving steps, thereby reducing thermal history compared to the reprecipitation method and preventing oxidative decomposition of PEG chains.

[0085] By repeating step (B), the content of impurities can be reduced. The number of times of repeating step (B) is not particularly limited, and preferably step (B) is repeated multiple times. Specifically, the number of repetitions of step (B) is preferably 1 to 20 times, more preferably 1 to 15 times, and even more preferably 2 to 10 times. However, from the perspective of productivity, the number of times of step (B) is preferably less than 10 times.

[0086] The organic solvent A used in the present invention is xylene, toluene, benzene, methyl acetate, ethyl acetate, butyl acetate, acetonitrile, acetone, N,N-dimethylformamide (DMF), dimethyl sulfoxide (DMSO), chloroform, dichloromethane, and a mixed solvent of a combination thereof.

[0087] However, when the organic solvent A is acetonitrile, acetone, N,N-dimethylformamide (DMF), dimethyl sulfoxide (DMSO), chloroform or dichloromethane, the use of the organic solvent A alone may change the properties of the precipitate during reslurry washing, which may reduce the operability when the polyethylene glycol derivative is separated and recovered from the organic solvent. Therefore, acetonitrile, acetone, N,N-dimethylformamide (DMF), dimethyl sulfoxide (DMSO), chloroform and dichloromethane are preferably used in combination with xylene, toluene, benzene, methyl acetate, ethyl acetate and butyl acetate.

[0088] The organic solvent B is selected from the group consisting of pentane, hexane, heptane, diethyl ether, methyl tert-butyl ether (MTBE), and combinations thereof.

[0089] In a particularly preferred embodiment, from the perspective of the efficiency of purifying the polyethylene glycol derivative as the object of the present invention, the organic solvent A is one or more solvents selected from the group consisting of xylene, toluene, benzene, methyl acetate, ethyl acetate, butyl acetate and acetonitrile, and the organic solvent B is hexane or heptane. More preferably, the organic solvent A is one or more solvents selected from the group consisting of toluene, ethyl acetate and acetonitrile, and the organic solvent B is one or two solvents selected from the group consisting of hexane and heptane. Still more preferably, the organic solvent A is ethyl acetate or a mixture of acetonitrile and ethyl acetate, and the organic solvent B is hexane.

[0090] The range of Y×T in the steps of the present invention is 0.5≤Y×T≤30. That is, Y and T satisfy the relationship of 0.5≤Y×T≤30.

[0091] Y is the mass ratio of organic solvent A to the total mass of organic solvent A and organic solvent B (organic solvent A / (mass of organic solvent A+mass of organic solvent B)). Organic solvent A is a good solvent for the above-mentioned polyethylene glycol derivative, and organic solvent B is a poor solvent for the above-mentioned polyethylene glycol derivative. The larger the value of Y is, the higher the proportion of good solvents is, and thus the solubility of polyethylene glycol derivatives and impurities is higher. The smaller the value of Y is, the higher the proportion of poor solvents is, and thus the solubility of polyethylene glycol derivatives and impurities is lower. The range of Y is appropriately between 0.5 and 0.9, preferably between 0.5 and 0.8, and more preferably between 0.5 and 0.7.

[0092] T is the temperature at which repulp washing is performed. The larger T is, the higher the solubility of the polyethylene glycol derivative and impurities is, and the smaller T is, the lower the solubility of the polyethylene glycol derivative and impurities is. The range of T is preferably between 1°C and 33°C, more preferably between 5°C and 30°C, and still more preferably between 10°C and 26°C.

[0093] In addition, when Y×T is large, the polyethylene glycol derivative will dissolve, which makes recovery difficult. When Y×T is small, the purification efficiency decreases. From this point of view, Y×T ranges from 0.1 to 30, preferably from 3 to 27, more preferably from 5 to 25, and even more preferably from 7 to 20.

[0094] The stirring time during the repulping washing is not particularly limited, and is preferably 5 minutes to 6 hours, more preferably 10 minutes to 3 hours, and still more preferably 15 minutes to 2 hours. The atmosphere in which the repulping washing operation is performed is not particularly limited, and is preferably performed in the presence of an inert gas, such as nitrogen or argon, to minimize oxidation. The apparatus for repulping washing is not particularly limited, and in view of the operation under nitrogen and in a sealed state where the polyethylene glycol derivative is less likely to undergo oxidative degradation, the repulping washing can be performed in a pressure-resistant container.

[0095] The mass (total value) of the organic solvent A and the mass (total value) of the organic solvent B used are each preferably 1 to 50 times the mass of the polyethylene glycol derivative, and more preferably 1 to 20 times.

[0096] (Step (C))

[0097] Step (C) is a step of dissolving the polyethylene glycol derivative obtained in step (B) in a good solvent and then recovering the polyethylene glycol derivative from the good solvent. Step (C) is a step for redissolving the polyethylene glycol derivative having uneven mass in step (B) to make the mass uniform.

[0098] The polyethylene glycol derivative obtained in step (B) is dissolved by adding a good solvent. The good solvent is preferably xylene, toluene, benzene, methyl acetate, ethyl acetate, butyl acetate, acetonitrile, acetone, N,N-dimethylformamide (DMF), dimethyl sulfoxide (DMSO), chloroform, dichloromethane and a combination thereof. Such a good solvent is preferably xylene, toluene, benzene, methyl acetate, ethyl acetate, butyl acetate or acetonitrile, more preferably ethyl acetate, toluene or acetonitrile, and even more preferably ethyl acetate or a mixed solvent of ethyl acetate and acetonitrile.

[0099] The recovery method is not particularly limited, and the following method is preferred.

[0100] A method of adding a poor solvent such as hexane or heptane to precipitate the polyethylene glycol derivative, and then recovering the polyethylene glycol derivative by filtration or decantation (including removing the supernatant)

[0101] ·Method for recovering polyethylene glycol derivatives by freeze drying

[0102] ·Method for recovering polyethylene glycol derivatives by evaporation and drying

[0103] The method of filtering the polyethylene glycol derivative from the good solvent is not particularly limited, and reduced pressure filtration, pressure filtration, and centrifugal filtration are preferred.

[0104] In steps (A) to (C), an antioxidant, such as butylated hydroxytoluene (BHT), can be added to the system to prevent oxidative degradation of the polyethylene glycol derivative.

[0105] Example

[0106] The present invention will be described in more detail with reference to Examples.

[0107] The molecular weight and polydispersity of the polyethylene glycol derivatives were measured using LC-10Avp (Shimadzu) as a GPC system under the following conditions.

[0108] GPC equipment: LC-10Avp (Shimadzu)

[0109] Developing solvent: DMF (10mM LiBr)

[0110] Flow rate: 0.7ml / min

[0111] Column: PL gel MIXED-D (Polymer Laboratory)

[0112] Column temperature: 65°C

[0113] Detector: RI

[0114] Sample concentration (injection volume): 30mg / 30mL (100μl)

[0115] The calibration curve was prepared using polyethylene glycol derivatives as standard substances.

[0116] (Method for Quantifying Impurities Contained in Crude Polyethylene Glycol Derivatives)

[0117] The content of β-Ala-diNHS in the polyethylene glycol derivative was measured using alliance (Waters) as an HPLC system under the following conditions.

[0118] HPLC device: alliance(Waters)

[0119] Flow rate: 1.0ml / min

[0120] Column: ODS column Inertsil ODS-3 (GL Sciences)

[0121] Column temperature: 40°C

[0122] Detector: UV (194nm)

[0123] Injection volume: 10μl (100mg / mL)

[0124] Analysis time: 40 minutes

[0125] Mobile phase: Mobile phase A (water / acetonitrile = 7 / 3, 0.02% phosphoric acid)

[0126] Mobile phase B (water / acetonitrile = 2 / 8, 0.02% phosphoric acid)

[0127] Gradient conditions

[0128] Time %A %B

[0129] 0 points 100% 0%

[0130] 15 points 100% 0%

[0131] 19 points 0% 100%

[0132] 23 points 100% 0%

[0133] 40 points 100% 0%

[0134] Use under the following conditions 1 H-NMR was used to measure the content of NHS, SMP and DSC in the polyethylene glycol derivatives.

[0135] NMR equipment: JNM-ECP400 (JEOL-NMR) or JNM-ECA600 (JEOL-NMR)

[0136] Temperature: 25℃

[0137] Cumulative times: 128 or 512

[0138] Sample concentration: 20mg / 0.7mL

[0139] The content of DCU in the polyethylene glycol derivative was measured using alliance (Waters) as the HPLC system under the following conditions.

[0140] HPLC device: alliance(Waters)

[0141] Flow rate: 1.0ml / min

[0142] Column: ODS column Inertsil ODS-3 (GL Sciences)

[0143] Column temperature: 30°C

[0144] Detector: UV (201nm)

[0145] Injection volume: 100 μl (10 mg / mL)

[0146] Analysis time: 35 minutes

[0147] Mobile phase: Mobile phase C (water / acetonitrile = (5 / 5)

[0148] Mobile phase D (water / acetonitrile = 0 / 10)

[0149] Gradient conditions

[0150] Time %C %D

[0151] 0 points 100% 0%

[0152] 15 points 100% 0%

[0153] 20 points 0% 100%

[0154] The content of SMH in the polyethylene glycol derivative was measured using alliance (Waters) as the HPLC system under the following conditions.

[0155] HPLC device: alliance(Waters)

[0156] Flow rate: 1.0ml / min

[0157] Column: ODS column Inertsil ODS-3 (GL Sciences)

[0158] Column temperature: 40°C

[0159] Detector: UV (220nm)

[0160] Injection volume: 10μl (20mg / mL)

[0161] Analysis time: 300 minutes

[0162] Mobile phase: Mobile phase E (water / acetonitrile = 55 / 45, 0.1% acetic acid)

[0163] Mobile phase F (water / acetonitrile = 2 / 8, 0.1% acetic acid)

[0164] Gradient conditions

[0165] Time %E %F

[0166] 0 points 100% 0%

[0167] 15 points 100% 0%

[0168] 19 points 0% 100%

[0169] 23 points 100% 0%

[0170] 40 points 100% 0%

[0171] The content of Glu-diNHS in the polyethylene glycol derivative was measured using alliance (Waters) as the HPLC system under the following conditions.

[0172] HPLC device: alliance(Waters)

[0173] Flow rate: 1.0ml / min

[0174] Column: ODS column Inertsil ODS-3 (GL Sciences)

[0175] Column temperature: 40°C

[0176] Detector: UV (194nm)

[0177] Injection volume: 10μl (20mg / mL)

[0178] Analysis time: 40 minutes

[0179] Mobile phase: Mobile phase G (water / acetonitrile = 7 / 3, 0.1% acetic acid)

[0180] Mobile phase H (water / acetonitrile = 2 / 8, 0.1% acetic acid)

[0181] Gradient conditions

[0182] Time %G %H

[0183] 0 points 100% 0%

[0184] 15 points 100% 0%

[0185] 19 points 0% 100%

[0186] 23 points 100% 0%

[0187] 40 points 100% 0%

[0188] The content of DTT in the polyethylene glycol derivative was measured using alliance (Waters) as the HPLC system under the following conditions.

[0189] HPLC device: alliance(Waters)

[0190] Flow rate: 1.0ml / min

[0191] Column: ODS column Inertsil ODS-3 (GL Sciences)

[0192] Column temperature: 30°C

[0193] Detector: UV (197nm)

[0194] Injection volume: 100 μl (10 mg / mL)

[0195] Analysis time: 20 minutes

[0196] Mobile phase: Mobile phase I (10mmol / L phosphate buffer / acetonitrile = 9 / 1)

[0197] (Example 1)

[0198] 37 g of α-(5-carboxypentyl)-ω-methoxypoly(ethylene oxide) (molecular weight: 20,000) and 111 g of toluene were added to a 300 mL four-necked flask equipped with a mechanical stirrer, a Dey condenser, a thermometer and a nitrogen inlet tube, and dissolved at 45° C. with stirring under nitrogen. Then, 427 mg of N-hydroxysuccinimide and 840 mg of dicyclohexylcarbodiimide were added and reacted at 42° C. for 2 hours. Then, 74 g of toluene was added for dilution, followed by filtration to remove insoluble matter.

[0199] The filter cake was washed with 37 g of toluene, mixed with the filtrate obtained previously, and then diluted with 74 g of ethyl acetate. Then, 130 g of hexane was added for reprecipitation. The slurry was stirred at 15 ° C for 15 minutes, and then filtered to recover the crude polyethylene glycol derivative (step (A)). The content of impurities was β-Ala-diNHS: 2819 ppm, and DCU: 3169 ppm.

[0200] A mixed organic solvent (ethyl acetate: 133 g / hexane: 55.5 g) prepared in advance was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 15° C. for 45 minutes to perform re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 6 times, and a total of 7 re-slurry washings were performed (step (B)).

[0201] After the re-slurry washing was completed, 222 g of ethyl acetate was added to the obtained polyethylene glycol derivative to dissolve at 40° C., and then 92.5 g of hexane was added for reprecipitation. After stirring at 15° C. for 15 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 148 g of hexane and then vacuum dried to obtain a compound of formula (7).

[0202] The impurity contents were β-Ala-diNHS: 8 ppm, and DCU: 13 ppm. In the repulp washing of this example, Y=0.7, T=15, and Y×T=10.5.

[0203]

[0204] (Example 2)

[0205] 5500g of α-(5-carboxypentyl)-ω-methoxypoly(ethylene oxide) (molecular weight: 10000) and 16.5kg of toluene were added to a 30L reaction tank equipped with a mechanical stirrer, a Dai condenser, a thermometer and a nitrogen inlet tube, and dissolved at 45°C while stirring under nitrogen. Then, 90.52g of N-hydroxysuccinimide and 147.53g of dicyclohexylcarbodiimide were added and reacted at 45°C for 4 hours. The mixture was filtered to remove insoluble matter, and the filter cake was washed with 11.0kg of toluene. The filtrate obtained was diluted with 11.0kg of ethyl acetate, and 16.5kg of hexane was added for reprecipitation. The mixture was stirred at 22°C for 90 minutes, and then filtered to recover the crude polyethylene glycol derivative (step (A)).

[0206] A pre-prepared mixed organic solvent (ethyl acetate: 38.5 kg / hexane: 16.5 kg / BHT: 7.7 g) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 22° C. for 30 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 4 times, and re-slurry washing was performed 5 times in total (step (B)).

[0207] To the obtained polyethylene glycol derivative, 38.5 kg of ethyl acetate and 7.7 g of BHT were added to dissolve at 40° C., and then 16.5 kg of hexane was added to reprecipitate. After stirring at 22° C. for 30 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 22.0 kg of hexane in which 4.4 g of BHT was dissolved, and then vacuum dried to obtain a compound of formula (8).

[0208] The content of impurity β-Ala-diNHS was 0.3 ppm. In the repulp washing of this example, Y = 0.7, T = 22, and Y x T = 15.4. The total time for these steps was 64 hours and 26 minutes.

[0209]

[0210] (Example 3)

[0211] 4900g of α-(5-carboxypentyl)-ω-methoxypoly(ethylene oxide) (molecular weight: 30000) and 24.5kg of toluene were added to a 50L reaction tank equipped with a mechanical stirrer, a condenser and a thermometer, and dissolved at 40°C while stirring under nitrogen. Then, 41.36g of N-hydroxysuccinimide and 67.40g of dicyclohexylcarbodiimide were added, and reacted at 45°C for 3 hours. The mixture was filtered to remove insoluble matter, and the filter cake was washed with 4.9kg of toluene. The filtrate obtained was diluted with 9.8kg of ethyl acetate and 2.5kg of acetonitrile, and 34.3kg of hexane was added for reprecipitation. The mixture was stirred at 26°C for 90 minutes, and then filtered to recover the crude polyethylene glycol derivative (step (A)).

[0212] A pre-prepared mixed organic solvent (ethyl acetate: 19.6 kg / toluene: 19.6 kg / acetonitrile: 2.5 kg / hexane: 34.3 kg / BHT: 7.84 g) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 26° C. for 30 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 3 times, and a total of 4 re-slurry washings were performed (step (B)).

[0213] To the obtained polyethylene glycol derivative, 19.6 kg of ethyl acetate, 19.6 kg of toluene, 2.5 kg of acetonitrile and 7.84 g of BHT were added to dissolve at 40° C., and then 16.5 kg of hexane was added to reprecipitate. After stirring at 22° C. for 30 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed twice with 29.4 kg of hexane and then vacuum dried to obtain a compound of formula (9).

[0214] The content of impurity β-Ala-diNHS was 6 ppm. In the repulp washing of this example, Y=0.5, T=26, and Y×T=13.0.

[0215]

[0216] (Example 4)

[0217] 10g of α-(2-aminoethyl)-ω-methoxypoly(ethylene oxide) (molecular weight: 20000) and 40g of toluene were added to a 100mL three-necked flask equipped with a mechanical stirrer, a Dai condenser, a thermometer and a nitrogen inlet tube, and dissolved at 45°C while stirring under nitrogen. Then, 185mg of N-succinimidyl 6-maleimidohexanoate (N-SMH) was added and reacted at 42°C for 3 hours. Filtered to remove insoluble matter, and the filter cake was washed with 10g of ethyl acetate, and the filtrate was subsequently diluted with 10g of ethyl acetate. 60g of hexane was added to the solution for reprecipitation. After stirring at 15°C for 15 minutes, the mixture was filtered to recover the crude polyethylene glycol derivative (step (A)).

[0218] A pre-prepared mixed organic solvent (ethyl acetate: 60 g / hexane: 60 g / BHT: 12 mg) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 15° C. for 15 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 3 times, and a total of 4 re-slurry washings were performed (step (B)).

[0219] To the obtained polyethylene glycol derivative, 60 g of ethyl acetate and 10 mg of BHT were added to dissolve at 40° C., and then 60 g of hexane was added to reprecipitate. After stirring at 15° C. for 15 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 40 g of hexane and then vacuum dried to obtain a compound represented by formula (10).

[0220] The impurity contents were N-SMH: 2 ppm, and NHS: 45 ppm. In the repulp washing of this example, Y=0.5, T=15, and Y×T=7.5.

[0221]

[0222] (Example 5)

[0223] 3000g of polyoxyethylene pentaerythritol ether (molecular weight: 20000), 30.0g of sodium acetate and 9.0kg of toluene were added to a 50L reaction tank equipped with a mechanical stirrer, a condenser and a thermometer, and dissolved at 45°C while stirring under nitrogen. Then, 82.15g of glutaric anhydride was added and reacted at 40°C for 1 hour. Then, 207g of N-hydroxysuccinimide and 260g of dicyclohexylcarbodiimide were added and reacted at 40°C for 3 hours. Filtered to remove insoluble matter, and the filter cake was washed with 3kg of toluene, mixed with the filtrate obtained previously, and then diluted with 12kg of ethyl acetate. Then, 12kg of hexane was added for reprecipitation. The mixture was stirred at 19°C for 1 hour, and then filtered to recover the crude polyethylene glycol derivative (step (A)).

[0224] A pre-prepared mixed organic solvent (ethyl acetate: 24 kg / acetonitrile: 1.2 kg / hexane: 12 kg / BHT: 4.8 g) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 19° C. for 30 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 4 times, and re-slurry washing was performed 5 times in total (step (B)).

[0225] To the obtained polyethylene glycol derivative, 24 kg of ethyl acetate, 1.2 kg of acetonitrile and 4.8 g of BHT were added to dissolve at 40° C. and then 12 kg of hexane was added to reprecipitate. After stirring at 19° C. for 1 hour, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 12 kg of hexane dissolved with 2.4 g of BHT, and then vacuum dried to obtain a compound of formula (11).

[0226] The impurity contents were β-Ala-diNHS: 198 ppm and Glu-diNHS: 12 ppm. In the repulp washing of this example, Y=0.7, T=19, and Y×T=13.3.

[0227]

[0228] (Example 6)

[0229] 4000g of α-methylsulfonyl-ω-methylsulfonyloxypolyoxyethylene (molecular weight: 3400), 0.94kg of thiourea and 8.0kg of 2-propanol were added to a 50L reaction tank equipped with a mechanical stirrer, a condenser and a thermometer, dissolved at 45°C while stirring under nitrogen, and then reacted at 80°C for 4 hours. Then, 16.0kg of UFW was added and the mixture was concentrated to distill off the 2-propanol. 0.726kg of dithiothreitol (DTT), 0.16kg of BHT and 4.6kg of 400g / L sodium hydroxide solution were added to the obtained residue, and a hydrolysis reaction was carried out at 70°C for 3 hours. Then, 6kg of 6N HCl was added to neutralize the mixture, and 4.0kg of common salt was added to dissolve. Then, 28.0kg of chloroform was added and stirred. After stratification, the chloroform layer was recovered and extracted. 28.0kg of chloroform was added to the remaining water layer and extracted again. The solution obtained from the two extraction processes is mixed, and 40.0 kg of 20% brine is added and stirred for washing. After stratification, the aqueous layer is discarded, and the remaining chloroform layer is washed twice with 40.0 kg of 20% brine, and a total of 3 washings are performed. The chloroform layer is concentrated under reduced pressure, and 16.0 kg of ethyl acetate is added to obtain a residue, which is then stirred and filtered to remove insoluble matter. The filter cake is washed with 4.0 kg of ethyl acetate and mixed with the previous filtrate. 24.0 kg of hexane is added to the solution for reprecipitation. After stirring at 15 ° C for 30 minutes, the mixture is filtered to recover the crude polyethylene glycol derivative (step (A)).

[0230] To the obtained crude polyethylene glycol derivative, a premixed solution (ethyl acetate: 12.0 kg / toluene: 4.0 kg / hexane: 16.0 kg) was added and stirred at 20°C for 30 minutes to perform reslurry washing, and then filtered to recover the polyethylene glycol derivative (step (B)).

[0231] To the obtained polyethylene glycol derivative, 12.0 kg of ethyl acetate and 4.0 kg of toluene were added to dissolve at 40° C., and then 16.0 kg of hexane was added to reprecipitate. After stirring at 20° C. for 30 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 16.0 kg of hexane and then vacuum dried to obtain a compound of formula (12).

[0232] The content of impurity DTT was 120 ppm. In the repulp washing of this example, Y=0.5, T=20, and Y×T=10.0.

[0233]

[0234] (Example 7)

[0235] 10g of 2,3-bis(methylpolyoxyethylene-oxy)-1-[(3-aminopropyl)polyoxyethylene-oxypropylaminocarbonyl-oxy]-propane (molecular weight: 53000), 52g of toluene and 8g of acetonitrile were added to a 200mL three-necked flask equipped with a mechanical stirrer, a Dai condenser, a thermometer and a nitrogen inlet tube, and dissolved at 40°C while stirring under nitrogen. Then, 97mg of N-methylmorpholine and 77mg of N-succinimide-3-maleimide propionic acid (SMP) were added and reacted at 25°C for 3 hours. After dilution with 40g of ethyl acetate, filtration was performed to remove insoluble matter, and the filter cake was washed with 20g of ethyl acetate. 60g of hexane was added to the solution for reprecipitation. After stirring at 25°C for 15 minutes, the mixture was filtered to recover the crude polyethylene glycol derivative (step (A)).

[0236] A pre-prepared mixed organic solvent (ethyl acetate: 120 g / hexane: 60 g / BHT: 24 mg) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 25° C. for 15 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 2 times, and re-slurry washing was performed 3 times in total (step (B)).

[0237] To the obtained polyethylene glycol derivative, 120 g of ethyl acetate and 24 mg of BHT were added to dissolve at 40° C., and then 60 g of hexane was added to reprecipitate. After stirring at 25° C. for 15 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 60 g of hexane and 12 mg of BHT and then vacuum dried to obtain a compound represented by formula (13).

[0238] The contents of impurities were SMP: 3 ppm, and NHS: 6 ppm. In the repulp washing of this example, Y=0.67, T=25, and Y×T=16.7.

[0239]

[0240] (Example 8)

[0241] 2300g of polyethylene glycol (molecular weight: 20000), 11.5kg of toluene and 2g of BHT were added to a 30L reaction tank equipped with a mechanical stirrer, a Dai condenser, a thermometer and a nitrogen inlet tube, dissolved by heating, and then refluxed for dehydration for 1 hour. Then, 177g of DSC and 82g of pyridine were added, and reacted at 65°C for 8 hours. After filtering to remove insoluble matter, the filter cake was washed with 7kg of ethyl acetate and mixed with the filtrate obtained previously, and then 8kg of hexane was added to reprecipitate. After stirring at 25°C for 30 minutes, the mixture was filtered to recover the crude polyethylene glycol derivative (step (A)).

[0242] A pre-prepared mixed organic solvent (ethyl acetate: 17 kg / hexane: 7 kg / BHT: 3 g) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 25° C. for 1 hour for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 3 times, and a total of 4 re-slurry washings were performed (step (B)).

[0243] To the obtained polyethylene glycol derivative, 17 kg of ethyl acetate and 3 g of BHT were added to dissolve at 40° C., and then 7 kg of hexane was added to reprecipitate. After stirring at 25° C. for 30 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 9 kg of hexane in which 2 g of BHT was dissolved, and then vacuum dried to obtain a compound of formula (14).

[0244] The impurity contents were: DSC: not detected, NHSI: 9 ppm. In the repulp washing of this example, Y=0.7, T=25, and Y×T=17.5.

[0245]

[0246] (Example 9)

[0247] The reaction of α-(5-carboxypentyl)-ω-methoxypoly(ethylene oxide) was carried out in the same scale and manner as in Example 1. After the reaction, 74 g of ethyl acetate was added to the filtrate after filtration, and the temperature was adjusted to 35° C., and then 130 g of hexane was added to perform reprecipitation, and the mixture was stirred at 25° C. for 15 minutes, and then filtered to recover the crude polyethylene glycol derivative (step (A)).

[0248] A previously prepared mixed organic solvent (ethyl acetate: 133 g / hexane: 55.5 g) was added to the recovered crude polyethylene glycol derivative, and the reslurry washing at 35° C. was extended to 20 hours (step (B)).

[0249] That is, the dissolution time was extended assuming that the reprecipitation step was repeated, and comparison was made.

[0250] (Comparative Example 1)

[0251] The reaction of α-(5-carboxypentyl)-ω-methoxypoly(ethylene oxide) was carried out in the same scale and manner as in Example 1. After the reaction, 74 g of ethyl acetate was added to the filtrate, and the temperature was adjusted to 35° C., and then 130 g of hexane was added for reprecipitation, and the mixture was stirred at 25° C. for 15 minutes, and then filtered to recover the crude polyethylene glycol derivative (step (A)).

[0252] The recovered crude polyethylene glycol derivative was dissolved with 185 g of ethyl acetate, and the temperature was adjusted to 55° C., and the dissolution time was extended to 20 hours.

[0253] The results of Example 9 and Comparative Example 1 are shown in Table 1 below.

[0254] [Table 1]

[0255]

[0256] According to Table 1, as shown in Example 9, extending the stirring time for reslurry washing of the polyethylene glycol derivative does not lead to an increase in polydispersity, but as shown in Comparative Example 1, extending the dissolution time by heating repeated reprecipitation increases the thermal history, thereby increasing the polydispersity.

[0257] Therefore, reslurry washing proved to be a superior preparation method compared to reprecipitation because even repeated reslurry washing was less likely to result in an increase in polydispersity due to oxidative degradation of the polyethylene glycol.

[0258] In the following Example 10 and Comparative Example 2, the effect of step (C) on the homogeneity of the polyethylene glycol derivative was studied.

[0259] (Example 10)

[0260] The reaction was carried out on the same scale and in the same manner as in Example 1. After reaction and filtration, the filtrate was diluted with 74 g of ethyl acetate. Then, 130 g of hexane was added for reprecipitation. After stirring at 15° C. for 15 minutes, the mixture was filtered to recover the crude polyethylene glycol derivative (step (A)).

[0261] A pre-prepared mixed organic solvent (ethyl acetate: 133 g / hexane: 55.5 g) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 15° C. for 45 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated once, and re-slurry washing was performed twice in total (step (B)).

[0262] To the obtained polyethylene glycol derivative, 222 g of ethyl acetate was added to dissolve at 40° C., and then 92.5 g of hexane was added to perform reprecipitation (step (C)). After stirring at 15° C. for 15 minutes, the mixture was filtered, and samples were taken from three randomly selected points of the filter cake to measure the content of β-Ala-diNHS.

[0263] (Comparative Example 2)

[0264] The reaction was carried out in the same scale and manner as in Example 1. After the reaction and filtration, 74 g of ethyl acetate was added to the filtrate, the temperature was adjusted to 15° C., and then 130 g of hexane was added for reprecipitation. The crude polyethylene glycol derivative was recovered by filtration (step (A)).

[0265] A pre-prepared mixed organic solvent (ethyl acetate: 133 g / hexane: 55.5 g) was added to the crude polyethylene glycol derivative, and the mixture was adjusted to 15° C. and stirred for 45 minutes for reslurry washing. The stirred solution was filtered to recover the polyethylene glycol derivative, and this operation was performed 3 times (step (B)). Step (C) was not performed.

[0266] Samples were taken from three randomly selected points of the filter cake to measure the content of β-Ala-diNHS.

[0267] The results of Example 10 and Comparative Example 2 are shown in Table 2.

[0268] [Table 2]

[0269]

[0270] According to Table 2, in Example 10, the SD value was 1, whereas in Comparative Example 2, a value as high as 26 was shown. This result shows that uniformity cannot be obtained only by reslurry washing in step (B), and step (C) is necessary to obtain a uniform polyethylene glycol derivative.

[0271] (Comparative Example 3)

[0272] In the following Comparative Example 3, in order to confirm the effect of shortening the step time, all repulp washing was replaced with reprecipitation for comparison.

[0273] The reaction was carried out on the same scale and in the same manner as in Example 2. After the reaction and filtration, the filtrate was diluted with 11.0 kg of ethyl acetate. Then, 16.5 kg of hexane was added for reprecipitation. After stirring at 25° C. for 15 minutes, the mixture was filtered to recover the crude polyethylene glycol derivative (step (A)).

[0274] The obtained crude polyethylene glycol derivative was dissolved with 38.5 kg of ethyl acetate and adjusted to 36 ° C, and then, 16.5 kg of hexane was added to reprecipitate, and the mixture was stirred at 22 ° C for 30 minutes, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 4 times, and a total of 5 reprecipitations were performed, and then 38.5 kg of ethyl acetate was added to the obtained polyethylene glycol derivative to dissolve at 40 ° C, and then 16.5 kg of hexane was added to reprecipitate. After stirring at 25 ° C for 30 minutes, filtration was performed to recover the polyethylene glycol derivative. The obtained polyethylene glycol derivative was washed with 22.0 kg of hexane, and then vacuum dried to obtain the target substance.

[0275] The total time for these steps was 73 hours and 11 minutes.

[0276] The results of Example 2 and Comparative Example 3 show that the time of the steps can be shortened by changing the reprecipitation to reslurry washing.

[0277] [Table 3]

[0278] Total time for steps Example 2 64 hours and 26 minutes Comparative Example 3 73 hours and 11 minutes

[0279] (Comparative Example 4)

[0280] In Comparative Example 4, a comparative study was conducted to see whether purification can be performed while using the same conditions as in Example 1 while setting the repulp washing conditions to Y×T=31.5.

[0281] Specifically, in Example 1, a mixed solvent of ethyl acetate: 170 g / hexane: 18.9 g (Y = 0.9) was used during reslurry washing, and the solution was adjusted to 35° C. (T = 35) and stirred for 45 minutes to perform reslurry washing. Filtration was performed to recover the polyethylene glycol derivative as a residue, and then the filtrate was concentrated to recover 4.4 g (12% of the total weight) of the polyethylene glycol derivative from the filtrate.

[0282] The results of Comparative Example 4 show that when Y×T in the repulp washing exceeds the upper limit, the polyethylene glycol derivative is dissolved in the mixed solvent.

[0283] (Comparative Example 5)

[0284] A comparative study was conducted to see whether purification could be performed while setting the repulp washing conditions to Y×T=0.1 while using the same conditions as in Example 1.

[0285] That is, the reaction was carried out in the same scale and manner as in Example 1. After the reaction and filtration, the filtrate was diluted with 74 g of ethyl acetate. Then, 130 g of hexane was added for reprecipitation. After stirring at 15° C. for 15 minutes, the mixture was filtered to recover the crude polyethylene glycol derivative (step (A)).

[0286] A pre-prepared mixed organic solvent (ethyl acetate: 18.9 g / hexane: 170 g (Y = 0.1)) was added to the obtained crude polyethylene glycol derivative, and the mixture was stirred at 1° C. (T = 1) for 45 minutes for re-slurry washing, and then filtered to recover the polyethylene glycol derivative. This operation was repeated 6 times, and a total of 7 re-slurry washings were performed (step (B)).

[0287] Next, 222 g of ethyl acetate was added to the obtained polyethylene glycol derivative to dissolve at 40° C., and then 92.5 g of hexane was added to reprecipitate. After stirring at 15° C. for 15 minutes, the mixture was filtered to recover the polyethylene glycol derivative (step (C)). The obtained polyethylene glycol derivative was washed with 148 g of hexane and then vacuum dried to obtain the target substance.

[0288] The results of Comparative Example 5 show that when Y×T in the repulp washing is below the lower limit, the impurity removal efficiency decreases.

[0289] [Table 4]

[0290]

[0291] The results of Comparative Examples 4 and 5 show that an appropriate Y×T range is necessary for repulping.

[0292] [Table 5]

[0293]

[0294] Industrial Applicability

[0295] According to the present invention, polyethylene glycol derivatives as drug raw materials or drug additives can be obtained with high efficiency, high purity and uniform quality.

[0296] Although the present invention has been described in detail and with reference to specific embodiments thereof, it will be apparent to one skilled in the art that various changes or modifications can be made to the present invention without departing from the spirit and scope of the present invention.

[0297] This application is based on the Japanese patent application filed on March 17, 2022 (Japanese Patent Application No. 2022-42041), the contents of which are incorporated herein by reference.

Claims

1. A method for preparing a polyethylene glycol derivative, the method comprising: (A) a step of preparing a crude polyethylene glycol derivative, the crude polyethylene glycol derivative comprising a polyethylene glycol derivative and impurities, the polyethylene glycol derivative having at its terminal at least one member selected from the group consisting of a functional group capable of reacting with a bio-related substance, a functional group serving as a precursor of the functional group, and a protective group for the functional group; (B) mixing the crude polyethylene glycol derivative with a mixed organic solvent comprising an organic solvent A and an organic solvent B to form a slurry, subjecting the slurry to re-slurry washing, and then recovering the polyethylene glycol derivative from the mixed organic solvent; as well as (C) dissolving the polyethylene glycol derivative obtained in step (B) in a good solvent, and then recovering the polyethylene glycol derivative from the good solvent, wherein: The organic solvent A is selected from the group consisting of xylene, toluene, benzene, methyl acetate, ethyl acetate, butyl acetate, acetonitrile, acetone, N,N-dimethylformamide (DMF), dimethyl sulfoxide (DMSO), chloroform, dichloromethane and combinations thereof, The organic solvent B is selected from the group consisting of pentane, hexane, heptane, diethyl ether, methyl tert-butyl ether (MTBE) and combinations thereof, and Assuming that the mass ratio of the organic solvent A to the total value of the mass of the organic solvent A and the mass of the organic solvent B (mass of organic solvent A / (mass of organic solvent A+mass of organic solvent B)) is Y, and the temperature during repulp washing is T (° C.), Y and T satisfy the following relationship: 0.5≤Y×T≤30.

2. The method for preparing a polyethylene glycol derivative according to claim 1, wherein: Repeat step (B) multiple times.

3. The method for preparing a polyethylene glycol derivative according to claim 1 or 2, wherein: The organic solvent A is ethyl acetate or a mixed solvent of ethyl acetate and acetonitrile, and the organic solvent B is hexane.

4. The method for preparing a polyethylene glycol derivative according to any one of claims 1 to 3, wherein The mass of the organic solvent A and the mass of the organic solvent B are each 1 to 50 times the mass of the polyethylene glycol derivative, and the temperature during the reslurry washing is 1°C to 33°C.