Novel high-liquid-level glass fiber drawing furnace
By using a high-level glass fiber drawing furnace with two pairs of electrode plates arranged in a cross configuration, the problems of uneven glass melt temperature field and bubble volatilization were solved, enabling continuous and controllable production of fine fibers and improving fiber quality and furnace life.
Patent Information
- Application Number
- CN202411022232.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-15
AI Technical Summary
In existing glass fiber drawing furnaces, the temperature distribution of the molten glass is uneven during the melting process, resulting in low temperatures at the four corners of the molten glass, which affects the production of fine fibers. In addition, the glass beads have a short residence time in the refining zone, making it difficult for bubbles to evaporate, thus causing unstable operation.
A high-level glass fiber drawing furnace with two pairs of electrode plates arranged in a cross pattern improves the uniformity of the glass melt temperature field distribution, increases the glass melt clarification time, reduces bubbles, and promotes the stability of the drawing operation by forming a double-layer electric line arrangement in the center of the furnace.
It achieves a uniform distribution of the temperature field in the molten glass, improves the stability of continuous production of fine fibers, reduces the erosion of the furnace body by the molten glass, extends the service life of the furnace body, and improves fiber quality and production efficiency.
Smart Images

Figure CN118954901A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of glass fiber preparation, and in particular to a novel high-liquid-level glass fiber drawing furnace. Background Art
[0002] Glass fiber is an inorganic non-metallic material with excellent performance. It has the advantages of good insulation, strong heat resistance, good corrosion resistance and high mechanical strength. It is widely used in various fields such as reinforcement materials, insulation materials, and thermal insulation materials. In the production process of glass fiber, a crucible furnace is needed to melt and draw the glass raw materials. In the glass fiber drawing furnace, platinum-rhodium alloy is the most ideal material for the crucible furnace body. It can form a very perfect temperature field in the glass liquid when the glass is melted. However, due to its high price, platinum-substitute materials are currently commonly used as the furnace body. The drawing furnace uses electrodes to heat the glass liquid to melt the glass fiber. However, due to the limitations of the distribution of power lines in the glass liquid, the temperature of the glass liquid at the four corners during the melting process of the drawing furnace is low, and uneven chemical material is prone to affect the fiber forming, and the production of fine fibers (raw fiber diameter of 5 microns and below) cannot be well achieved.
[0003] The applicant discloses a glass fiber drawing furnace (CN 113998883 A), which uses a pair of vertical electrode plates to heat the glass liquid in the furnace, and controls the conductive area of the electrode plates to be greater than or equal to 0.5 times the conductive cross-sectional area of the glass liquid, and the volume of the glass liquid covered by the electric lines is greater than or equal to 0.45-0.8 times the volume of the glass liquid, thereby improving the uniformity of the temperature field distribution of the glass liquid. This patent can achieve the generation of fine fibers, but in the melting process, it is easy to cause problems such as unstable operation and discontinuous drawing when glass balls are added to the melt, because the glass liquid stays in the clarification area for a short time, and the bubbles generated are difficult to volatilize. Summary of the invention
[0004] In order to solve the above problems, the present invention provides a novel high liquid level glass fiber drawing furnace.
[0005] The technical solution adopted by the present invention is:
[0006] A novel high-liquid-level glass fiber drawing furnace comprises a furnace body, a furnace chamber is arranged in the furnace body, four electrode plates are arranged in the furnace chamber, the four electrode plates are respectively arranged on the four sides of the furnace body, the first electrode plate and the second electrode plate are inclinedly arranged on the lower side of the furnace body, the third electrode plate and the fourth electrode plate are arranged on the upper side of the furnace body, respectively opposite to and parallel to the first electrode plate and the second electrode plate, the first electrode plate and the third electrode plate form a pair of A electrodes; the second electrode plate and the fourth electrode plate form a pair of B electrodes.
[0007] By adopting the above technical solution, by cross-setting two pairs of electrodes, the electric lines can form a double-layer arrangement in the center of the furnace, the electric line distribution intensity in the center is large, the central hot spot temperature is high, the temperature difference between the central hot spot and the four corners is small, the glass liquid temperature field is evenly distributed, and the wire drawing quality is improved. By cross-setting two pairs of electrodes, a high liquid level of glass liquid can be formed in the furnace, which is conducive to the clarification of the glass liquid, reduces bubbles, promotes the stability of the wire drawing operation, and continuously controls it, so as to realize the continuous production of fine fibers.
[0008] Furthermore, the elevation angles of the first electrode plate and the second electrode plate are both 15-85°.
[0009] Furthermore, the vertical distance between the bottom ends of the first electrode plate and the second electrode plate and the bottom brick of the furnace body is 10-30 mm, and the vertical distance between the top ends of the third electrode plate and the fourth electrode plate and the surface of the glass liquid is 20-50 mm.
[0010] The above technical solution is adopted to ensure the generation of high static pressure stable laminar flow, more reasonable distribution of power lines and more uniform distribution of temperature field, further improving the stability of wire drawing operation.
[0011] Furthermore, the total volume of the glass liquid covered by the electric lines of force of the two pairs of electrode plates is 0.85-0.95 times the volume of the glass liquid, and the conductive area of any pair of electrode plates is greater than or equal to 0.5 times the conductive cross-sectional area of the glass liquid.
[0012] The adoption of the above technical solution further improves the uniformity of the glass liquid temperature field distribution, reduces the temperature difference between the central hot spot and the liquid surface and the bottom brick, thereby making the power line distribution more reasonable and the temperature field distribution more uniform.
[0013] Furthermore, the depth of the molten glass is 300-500 mm.
[0014] By adopting the above technical solution, high static pressure stable laminar flow can be generated by controlling the depth of molten glass, which can meet the flow requirements of fine-pore nozzles, further promote continuous and controllable wire drawing, and maintain operational stability.
[0015] Furthermore, the ratio of the width of any electrode plate to the depth of the glass liquid is 0.4-0.7.
[0016] By adopting the above technical solution, the conductive area of the electrode plate can be set proportionally, and the distribution of the electric lines in the furnace body can be controlled according to the required intensity, thereby controlling the gradient distribution of the temperature field, which is suitable for melting glasses with different thermal resistances.
[0017] Furthermore, the ratio of the length of the first electrode plate and the third electrode plate in the glass liquid to the width of the furnace is 0.8-0.95, and the ratio of the length of the second electrode plate and the fourth electrode plate in the glass liquid to the length of the furnace is 0.8-0.95.
[0018] By adopting the above technical solution, the conductive area of the electrode plate can be set proportionally, and the distribution of the electric lines in the furnace body can be controlled according to the required intensity, thereby controlling the gradient distribution of the temperature field, which is suitable for melting glasses with different thermal resistances.
[0019] Furthermore, at least one ball throwing hole is provided on the top of the furnace body, and a liquid flow hole is provided at the center of the bottom of the furnace body.
[0020] By adopting the above technical scheme, the wire drawing furnace of the present invention can adopt the positive ball adding method, utilize high static pressure stable laminar flow, maintain the glass in the crucible for a longer residence time, and do not need to adopt the offset furnace layout, thereby reducing the scouring of the bottom of the furnace body by the glass liquid, ensuring the wire drawing quality and increasing the service life of the furnace body.
[0021] Furthermore, when there is one ball-throwing hole, it is arranged at the center of the top of the furnace body; when there are more than two head ball holes, they are evenly distributed on the top of the wire drawing furnace.
[0022] The adoption of the technical solution can improve the uniformity of feeding.
[0023] Furthermore, the height of the liquid flow hole is 0.2-0.4 times the depth of the glass liquid.
[0024] By adopting the above technical solution, the flow rate of the molten glass can be controlled, further ensuring the formation of high-level molten glass and improving operation stability.
[0025] Furthermore, the cross section of the liquid flow hole along the length direction of the furnace is trapezoidal, and the upper aspect ratio of the trapezoidal cross section is 2-6, and the lower aspect ratio is 1-3.
[0026] By adopting the above technical solution, the design of the flow hole is more in line with the fluid mechanics distribution, the scouring of the glass liquid on the bricks of the flow hole is reduced, and the flow rate of the glass liquid is further controlled to improve the operation stability.
[0027] Beneficial effects of the present invention:
[0028] 1. By cross-setting two pairs of electrode plates, high static pressure stable laminar flow with a glass liquid depth of more than 300mm in the furnace can be achieved, meeting the flow requirements of the fine-pore nozzle, promoting continuous and controllable wire drawing, maintaining operation stability, and effectively solving the problem of unstable operation caused by the difficulty in volatilizing bubbles generated in the clarification area of the glass liquid due to the short time when the glass balls are added to the melt.
[0029] 2. Two pairs of electrode plates form a double-layer electric line arrangement in the center of the furnace, which makes the temperature field distribution and intensity distribution of the electric lines in the glass liquid more reasonable. The electric lines are distributed in a strong intensity in the center, generating a hot spot in the center. The temperature of the central hot spot is high, which promotes the glass melting to be close to the ideal temperature field, improves thermal efficiency, reduces pool wall erosion, and thus improves glass quality, promotes wire drawing stability, and effectively solves the distribution limitations of electric lines in the glass liquid. During the melting process of the wire drawing furnace, the temperature of the glass liquid at the four corners is low, which is prone to uneven material smelting affecting fiber forming. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of the cross-sectional structure of the wire drawing furnace of the present invention along its length direction.
[0031] Figure 2 It is a schematic diagram of the cross-sectional structure of the wire drawing furnace of the present invention along its width direction.
[0032] Figure 3 It is a schematic diagram of the length direction structure of the first electrode plate and the third electrode plate of the present invention.
[0033] Figure 4 It is a schematic diagram of the structure of the flow hole in the length direction of the present invention.
[0034] In the figure: 1, furnace body; 2, furnace chamber; 3, ball adding hole; 4, liquid flow hole; 51, first electrode plate, 52, second electrode plate, 53, third electrode plate, 54, fourth electrode plate. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical solution and advantages of the present invention more clear, the technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings and a preferred implementation manner.
[0036] Figure 1 and Figure 2 In order to clearly show the installation structure size of the electrode plates, only one pair of electrode plates is shown.
[0037] like Figure 1-2 As shown, the present invention discloses a novel high liquid level glass fiber drawing furnace, comprising a furnace body 1, four evenly distributed ball adding holes 3 are arranged on the top of the furnace body, and a flow hole 4 is arranged at the center of the bottom of the furnace body; a furnace chamber 2 is arranged in the furnace body, and four electrode plates 5 are arranged in the furnace chamber 2, and the four electrode plates 5 are respectively arranged on the four sides of the furnace body 1, the first electrode plate 51 and the second electrode plate 52 are inclined at the lower side of the furnace body, and the elevation angle a1 is 15-85°, the third electrode plate 53 and the fourth electrode plate 54 are arranged on the upper side of the furnace body, respectively opposite to and parallel to the first electrode plate 51 and the second electrode plate 52, the first electrode plate 51 and the third electrode plate 53 form a pair of A electrodes; the second electrode plate 52 and the fourth electrode plate 54 form a pair of B electrodes.
[0038] like Figure 3 As shown, both pairs of electrodes are powered by Scott transformers, the plate surfaces of the first electrode plate 51 and the third electrode plate 53 extend along the width direction of the furnace body, the plate surfaces of the second electrode plate 52 and the fourth electrode plate 54 extend along the length direction of the furnace body, and the minimum distance between the four electrode plates and the inner wall of the furnace body is 10-30 mm.
[0039] The vertical distance between the bottom ends of the first electrode plate 51 and the second electrode plate 52 and the bottom brick of the furnace body is 10-30 mm, and the vertical distance between the top ends of the third electrode plate 53 and the fourth electrode plate 54 and the top brick of the furnace body is 20-50 mm.
[0040] Preferably, the elevation angles of the first electrode plate 51 and the second electrode plate 52 are equal, the vertical distances H1 between the bottom ends of the first electrode plate 51 and the second electrode plate 52 and the bottom bricks of the furnace body are equal, and the vertical distances H3 between the top ends of the third electrode plate 53 and the fourth electrode plate 54 and the top bricks of the furnace body are equal; the temperature field distribution in the furnace is more uniform, and the temperature difference between the central hot spot temperature and the liquid surface temperature and the floor tile temperature is smaller.
[0041] Preferably, the side wall, bottom brick and top brick of the furnace body in the present invention are made of at least one of corundum brick and zirconium brick. The electrode plate 5 is made of molybdenum electrode, which has the advantages of high temperature strength, good high temperature oxidation resistance and long service life.
[0042] Preferably, the cross section of the liquid flow hole 4 along the length direction of the furnace is trapezoidal, and the dimensions of the trapezoidal cross section are: the upper aspect ratio is 2-6, and the lower aspect ratio is 1-3. The height H4 of the liquid flow hole is 0.2-0.4 times the depth h of the glass liquid. The upper aspect ratio is the ratio of the upper base length B1 of the trapezoidal cross section to the trapezoidal height H4, and the lower aspect ratio is the ratio of the lower base length B2 of the trapezoidal cross section to the trapezoidal height H4.
[0043] For the convenience of explanation, the depth of the glass liquid in the furnace 2 is recorded as h, the length of the furnace is recorded as a, and the width of the furnace is recorded as b, where a is greater than or equal to b; the length of the first electrode plate 51 and the third electrode plate 53 is recorded as y1, the length of the second electrode plate 52 and the fourth electrode plate 54 is recorded as y2, and the height of the electrode plate is recorded as z. The relative distance between the first electrode plate 51 and the third electrode plate 53 is recorded as x1, and the relative distance between the second electrode plate 52 and the fourth electrode plate 54 is recorded as x2. Then the volume of the glass liquid in the furnace V = a*b*h; the conductive area S1 of the first electrode plate 51 and the third electrode plate 53 is S1 = y1*z, and the conductive area S2 of the second electrode plate 52 and the fourth electrode plate 54 is S2 = y2*z.
[0044] The conductive cross-sectional area S3 of the glass liquid between the first electrode plate 51 and the third electrode plate 53 is a*h, and the volume V1 of the glass liquid covered by the electric lines of force of the first electrode plate 51 and the third electrode plate 53 is a*z. The conductive cross-sectional area S4 of the glass liquid between the second electrode plate 52 and the fourth electrode plate 54 is b*h; the volume V2 of the glass liquid covered by the electric lines of force of the second electrode plate 52 and the fourth electrode plate 54 is a*z.
[0045] By controlling the total volume of the glass liquid covered by the electric lines of the two electrode plates to be 0.85-0.95 times the volume of the glass liquid, the conductive area of any pair of electrode plates is greater than or equal to 0.5 times the conductive cross-sectional area of the glass liquid; that is, controlling V1=0.85-0.95V, V2=0.85-0.95V, S1≧0.5S, S2≧0.5S, the uniformity of the temperature field distribution of the glass liquid can be further improved, the temperature difference between the central hot spot and the liquid surface and the bottom brick can be reduced, and the distribution of the electric lines can be more reasonable and the temperature field distribution can be more uniform.
[0046] By controlling the ratio of the width of any electrode plate to the depth of the glass liquid to be 0.4-0.7, the ratio of the length of the first electrode plate and the third electrode plate in the glass liquid to the width of the furnace is 0.8-0.95, and the ratio of the length of the second electrode plate and the fourth electrode plate in the glass liquid to the length of the furnace is 0.8-0.95; that is, by controlling z / h=0.4-0.7, y1 / a=0.8-0.95, y2 / b=0.8-0.95, the conductive area of the electrode plate can be set proportionally, and the distribution of the electric lines in the furnace body can be controlled according to the required intensity, thereby controlling the gradient distribution of the temperature field, which is suitable for melting glasses with different thermal resistances.
[0047] The effect test of using the wire drawing furnace of the present invention for melting and drawing is as follows:
[0048] The parameters of the selected drawing furnace are shown in Table 1 below. In Table 1, the length, height and elevation angle of the two pairs of electrode plates are equal, the elevation angle is 25°, the vertical distance between the bottom end of the electrode plate and the bottom brick of the furnace body is H3=10mm, the vertical distance between the top end of the electrode plate and the glass liquid surface is H1=20mm, and the distance between the electrode plate and the inner wall of the furnace body is 10mm.
[0049] Table 1
[0050]
[0051]
[0052] The total volume of the glass liquid covered by the electric lines of force of the two pairs of electrodes is 0.89 times the volume of the glass liquid, and the conductive area of the electrode plates is greater than 0.5 times the conductive cross-sectional area S1 of the glass liquid.
[0053] The drawing furnace shown in Table 1 was used for melt drawing to produce fine fibers with a diameter of 5 μm. The temperature field distribution test was as follows:
[0054] The electrode plate is energized, and a glass ball is added from the ball adding hole. When the depth of the glass liquid reaches 500 mm, a double platinum-rhodium thermocouple is used to measure the temperature at different depths from the surface of the glass liquid with a gradient of 40 mm. The central hot spot temperature is the central temperature of the flow hole, and corners 1 to 4 are the temperatures located on the floor tiles of the furnace and about 20 mm away from the side wall of the furnace body. The results are shown in Table 2
[0055] Table 2
[0056]
[0057] Comparative Example 1 is the test result of Example 1 of Chinese Patent CN 113998883 A.
[0058] It can be seen from Table 2 that the central hot spot temperature of the present invention is higher than that of the prior art, and the difference between the central hot spot temperature and the four corner temperatures is smaller, and the glass liquid temperature field distribution of the present invention is more uniform.
[0059] After continuous drawing for 24 hours, the output (kg), full barrel rate (%), raw wire finished product rate (%), raw wire qualified rate (%), raw wire passing rate (%) and mechanical strength of finished glass fiber were tested. The results are shown in Table 3. The mechanical strength was tested by a tensile strength machine, and the test method was based on GB / T 7689.5-2013 standard.
[0060] Among them, the output of the wire drawing furnace shift is the output of raw wire produced by a single wire drawing furnace in 24 hours, the full barrel rate is the number of full barrels produced per 12-hour shift / total number of barrels, the raw wire finished product rate = total amount of raw wire / amount of glass balls used, the raw wire qualified rate = total amount of qualified raw wire / total amount of raw wire, the raw wire pass rate = raw wire qualified rate × raw wire finished product rate, which represents the production efficiency.
[0061] Table 3
[0062]
[0063] Comparative Example 1 is the test result of Example 1 of Chinese Patent CN 113998883 A.
[0064] As can be seen from Table 3, compared with the prior art, the raw silk production per shift, full barrel rate, raw silk finished product rate, raw silk qualified rate, raw silk pass rate and glass fiber quality of the present invention are all improved, and the production per shift is increased by about 1.3 times compared with the prior art. It can be seen that the present invention effectively promotes the continuous controllable wire drawing and ensures the stability of the wire drawing operation.
[0065] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications are also within the protection scope of the present invention.
Claims
1. A new type of high liquid level glass fiber drawing furnace, comprising a furnace body, a furnace chamber is arranged in the furnace body, and is characterized in that: Four electrode plates are arranged in the furnace, and the four electrode plates are respectively arranged on the four sides of the furnace body. The first electrode plate and the second electrode plate are arranged obliquely on the lower side of the furnace body, and the third electrode plate and the fourth electrode plate are arranged on the upper side of the furnace body, respectively opposite to and parallel to the first electrode plate and the second electrode plate. The first electrode plate and the third electrode plate form a pair of A electrodes; the second electrode plate and the fourth electrode plate form a pair of B electrodes.
2. A novel high liquid level glass fiber drawing furnace according to claim 1, characterized in that: The elevation angles of the first electrode plate and the second electrode plate are both 15-85°.
3. The novel high liquid level glass fiber drawing furnace according to claim 1 is characterized in that: The vertical distance between the bottom ends of the first electrode plate and the second electrode plate and the bottom brick of the furnace body is 10-30 mm, and the vertical distance between the top ends of the third electrode plate and the fourth electrode plate and the glass liquid surface is 20-50 mm.
4. The novel high liquid level glass fiber drawing furnace according to claim 1 is characterized in that: The total volume of the glass liquid covered by the electric lines of the two pairs of electrode plates is 0.85-0.95 times the volume of the glass liquid, and the conductive area of any pair of electrode plates is greater than or equal to 0.5 times the conductive cross-sectional area of the glass liquid.
5. The novel high liquid level glass fiber drawing furnace according to claim 1 is characterized in that: The depth of the glass liquid is 300-500mm.
6. The novel high liquid level glass fiber drawing furnace according to claim 1 is characterized in that: The ratio of the width of any electrode plate to the depth of the glass liquid is 0.4-0.7; the ratio of the length of the first electrode plate and the third electrode plate in the glass liquid to the width of the furnace is 0.8-0.95, and the ratio of the length of the second electrode plate and the fourth electrode plate in the glass liquid to the length of the furnace is 0.8-0.
95.
7. The novel high liquid level glass fiber drawing furnace according to claim 1 is characterized in that: At least one ball throwing hole is arranged on the top of the furnace body, and a liquid flow hole is arranged at the center of the bottom of the furnace body.
8. The novel high liquid level glass fiber drawing furnace according to claim 7, characterized in that: When there is one ball-casting hole, it is set at the center of the top of the furnace body; when there are more than two header holes, they are evenly distributed on the top of the wire drawing furnace.
9. The novel high liquid level glass fiber drawing furnace according to claim 7, characterized in that: The height of the flow hole is 0.2-0.4 times the depth of the glass liquid.
10. The novel high liquid level glass fiber drawing furnace according to claim 9, characterized in that: The cross section of the liquid flow hole along the length direction of the furnace is trapezoidal, and the upper width-to-height ratio of the trapezoidal cross section is 2-6, and the lower height-to-width ratio is 1-3.
Citation Information
Patent Citations
Crucible pot for manufacturing ultra-fine continuous glass fiber
CN101492245A
Double-step longitudinal multi-section all-electric melting furnace
CN102092920A
Electrode boiler with electrodes unit
CN104822988A
Glass melting device and glass manufacturing method
CN117776486A
Combined leading electrode