Composite material wing forming mold and design method

By designing composite wing molds, using equal thickness design and reinforced rib structures, combined with M12 bolt holes and threaded connections, the existing molds have been solved in the problem of difficult and high weight, and the rapid demolding of the wings has been achieved and High-precision molding meets the lightweight and high-precision requirements of composite wings.

CN118990882APending Publication Date: 2024-11-22TAIYUAN UNIVERSITY OF TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411372480.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-29
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

When forming composite wings, existing metal molds are difficult to meet the manufacturing needs of slender, hollow, closed, and variable cross-sectional composite structural parts due to difficulties in molding and complex structural design. The mold weight and processing cost after forming are difficult. Higher.

Method used

A composite wing forming mold is designed, including upper mold, lower mold and winglet mold. It adopts equal thickness design, reinforcement structure and flow channel, and is connected through M12 bolt holes and threads to ensure rapid mold release and high precision. Forming and set rounded corners and grooves during processing to reduce processing difficulty.

Benefits of technology

It realizes rapid mold release of composite wings, high accuracy and light weight, reduces mold weight and processing costs, ensures strength and surface quality after wing molding, and is suitable for high precision and lightweight requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118990882A_ABST
    Figure CN118990882A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of mold design and manufacturing, and particularly discloses a composite wing forming mold and a design method.The composite wing forming mold comprises an upper mold and a lower mold, and a forming groove used for wing body forming is formed in the middle of the upper mold; a forming groove and a positioning pin hole which are matched with the upper mold are also formed in the middle of the lower mold, the number of the winglet molds is two, the winglet molds are symmetrically arranged on the two sides of the upper mold and the lower mold respectively, and the winglet molds are used for forming the outer surfaces of a left wingtip winglet and a right wingtip winglet of a wing body; the mold adopts an equal-thickness design mode, so that the weight of the mold is reduced, the adverse effect on the wing forming precision caused by unbalanced thermal stress in the processes of heating, curing and cooling to room temperature is greatly reduced, the strength and the precision of the formed wing are ensured, and the production cost is reduced. According to the scheme of the mold assembly, the wing can be quickly disassembled and demolded after being formed, and the surface quality of the wing is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of mold design and manufacturing, and in particular relates to a composite material wing forming mold and a design method. Background Art

[0002] Composite component forming molds are one of the important tools for manufacturing composite components. Their quality and performance directly affect the shape, size and appearance of composite components. Metal molds have high processing accuracy and good processing technology. Composite products formed by metal molds have high precision and good appearance. Metal molds are the most common mold form. However, for slender, hollow, closed, and variable-section composite structural parts, metal molds have certain limitations in application due to the difficulty of demoulding and complex structural design.

[0003] The present invention designs a molding mold for a composite wing with a specific size and shape. The wing has a large aspect ratio, and the preparation requirement is to use 100% carbon fiber prepreg, and no filling material is allowed inside. The wing after molding is required to have a low weight, high load-bearing capacity and surface quality. Considering the above-mentioned high design and production requirements, in order to better achieve rapid demoulding after molding, improve the molding quality of the wing, and reduce the mold weight and processing and manufacturing costs, a composite wing molding mold and design method are proposed. Summary of the invention

[0004] The object of the present invention is to provide a composite wing forming mold and a design method to solve the problems raised in the above background technology.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] A composite wing forming die and design method, comprising:

[0007] An upper mold, wherein a molding groove for molding the wing body is provided in the middle of the upper mold, and positioning pin holes are provided at two diagonal portions of the upper mold, and the upper mold is used to mold the entire upper surface of the wing body;

[0008] A lower mold, wherein a molding groove and a positioning pin hole matching the upper mold are also provided in the middle of the lower mold, the lower mold is positioned and connected with the positioning pin holes of the upper mold through positioning pins, and the lower mold is used to mold the lower surfaces of the left wing body and the right wing body of the wing body;

[0009] The winglet molds are two and are symmetrically arranged on both sides of the upper mold and the lower mold. The winglet molds are used to shape the outer surfaces of the left wingtip winglet and the right wingtip winglet of the wing body.

[0010] Preferably, the wing body further comprises a central wing box in the middle, and the upper and lower surfaces of the central wing box are both planes.

[0011] Preferably, both sides of the upper mold, the lower mold and the winglet mold are provided with wing trailing edge grooves, and the wing trailing edge grooves are provided with rounded corners.

[0012] Preferably, the upper mold and the lower mold have M12 bolt holes evenly arranged along the leading edge and trailing edge of the wing forming groove, wherein the M12 bolt holes of the upper mold are not designed with threads, and the M12 bolt holes of the lower mold are provided with threads, and the diameter of the M12 bolt holes is set according to the maximum diameter of the M12 standard bolt parts.

[0013] Preferably, the upper mold and the lower mold are provided with a plurality of reinforcing ribs along the direction of the central wing box.

[0014] Preferably, a boss is provided on the bottom surface of the lower mold at a position corresponding to the M12 bolt hole.

[0015] Preferably, a through hole is punched through the bottom surface of the lower mold corresponding to the M12 bolt hole.

[0016] Preferably, a guide groove is provided in the middle of the lower mold, and the plane between the guide groove and the leading edge of the wing body is 0.1 mm lower.

[0017] Preferably, at least two screw holes are provided on the winglet mold, and two M12 screw holes are provided on the side of the winglet mold, with a diameter enlarged by 1 mm, which are fixedly connected to the upper mold by M12 bolts; two M12 screw holes are provided at the bottom of the winglet mold, which are fixedly connected to the lower mold by M12 countersunk screws, and a groove is provided at the lower part of the winglet mold.

[0018] A method for designing a composite wing forming mold comprises the following steps:

[0019] S1. The part used for forming the wing surface should be appropriately sized. The specific sizing adjustment method is: the thickness direction is 0.5mm-0.8mm less than the theoretical thickness dimension, and the chord length is 1mm less than the theoretical chord length. When designing the upper mold and the winglet mold, the height of the winglet should be 10mm greater than the theoretical height dimension, and the top of the mold for forming the winglet part is not closed. After the wing body is prepared, the excess part is trimmed and polished;

[0020] S2. The trailing edge of the wing forms a small and sharp right angle, which will bring inconvenience to the processing of the mold. Therefore, it is necessary to set a rounded corner at the corresponding mold position to reduce the processing difficulty. After the wing is formed, the trailing edge of the wing is trimmed and polished until it meets the size requirements in the chord length direction;

[0021] S3. Positioning pin holes are set at the two diagonal positions of the upper mold and the lower mold, and the holes are punched to ensure the accuracy of the mold clamping position. Positioning pin holes are not set on the winglet mold. The positioning pins do not generate fastening force and only play a positioning role. M12 bolt holes are evenly arranged along the leading and trailing edges of the wing. The bolts use M12 standard bolts. No threads are designed in the M12 bolt holes of the upper mold. The diameter of the holes is set according to the maximum diameter of the M12 standard bolts.

[0022] S4. The upper mold is a shell of equal thickness to reduce the adverse effects of thermal stress on molding accuracy. Reinforcement ribs are set in the middle of the shell along the chord length of the wing. The side of the upper mold is grooved to facilitate the placement of the upper mold and reduce the weight of the upper mold.

[0023] S5. The lower mold needs to be provided with an M12 bolt hole at a position corresponding to the M12 bolt hole of the upper mold, and a standard internal thread is designed at the same time. A reinforcing rib is set in the middle of the shell, and a boss is set at the position corresponding to the M12 bolt hole on the bottom of the lower mold to ensure the strength of the bolt connection. The M12 bolt hole is punched through to clean the resin precipitated after the wing is formed;

[0024] S6. A guide groove is added along the leading edge of the wing of the lower mold. When the wing is heated and pressurized, the resin will precipitate through the guide groove. The plane between the guide groove and the leading edge of the wing is lowered by about 0.1 mm, which facilitates the precipitated resin to flow into the guide groove.

[0025] S7. The connection method between the winglet mold and the lower mold is to use M12 countersunk screws. The M12 countersunk screw hole is arranged in the middle of the step. It is installed and disassembled from the bottom of the winglet mold. When designing the M12 screw hole, the diameter of the hole is enlarged by 1mm so that the winglet mold and the upper mold form a bolt connection;

[0026] S8. A groove is opened at the bottom of the winglet mold. The curvature of the groove is the same as the curvature of the connection between the wing tip and the winglet, which reduces the influence of thermal stress on wing forming and reduces the weight of the winglet mold. The reinforcing ribs at the bottom of the winglet mold are retained to increase the stability of the mold and avoid the adverse effect of the deadweight of the winglet mold on the tightening force of the bolts. The lower mold and the winglet mold are connected in a stepped form, and a 1mm chamfer is set at the protruding corners of the step to prevent difficulty in connection due to processing errors at the corners.

[0027] Compared with the prior art, the present invention has the following beneficial effects:

[0028] (1) The mold of the present invention mainly adopts a uniform thickness design method, which reduces the weight of the mold and greatly reduces the adverse effects on the wing forming accuracy caused by uneven thermal stress during heating and curing and cooling to room temperature, thereby ensuring the strength and accuracy of the wing after forming. The mold assembly scheme can achieve rapid disassembly and demolding of the wing after forming, thereby ensuring the surface quality of the wing.

[0029] (2) After the mold of the present invention is processed, protective materials can be electroplated on the outer surface to slow down the corrosion rate and extend the service life of the mold. The mold designed by the present invention is used in the molding preparation of the ultra-light composite wing. The molded wing has good demolding performance, high precision, and light weight, which meets the use requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a schematic diagram of the overall structure of a composite material wing forming mold of the present invention;

[0031] Figure 2 It is a schematic diagram of the upper mold structure of the present invention;

[0032] Figure 3 It is a schematic diagram of the wing trailing edge slot structure of the present invention;

[0033] Figure 4 For the present invention Figure 3 A magnified schematic diagram of the middle part;

[0034] Figure 5 It is a schematic diagram of the lower mold structure of the present invention;

[0035] Figure 6 It is a schematic diagram of the guide groove structure of the present invention;

[0036] Figure 7 It is a schematic diagram of the structure of the winglet mold of the present invention;

[0037] Figure 8 It is a schematic diagram of the wing body structure of the present invention;

[0038] Fig. 9 A top view of the wing body of the present invention;

[0039] Fig.10 It is a schematic diagram of the structure of the left wingtip winglet of the present invention;

[0040] Fig.11 It is a schematic diagram of the size design structure of the winglet of the present invention;

[0041] Fig.12 A structural schematic diagram of a composite wing forming mold of the present invention from another perspective

[0042] Fig.13A flow chart of a design method of a composite wing forming mold of the present invention;

[0043] In the figure: 1. wing body; 11. left wing body; 12. right wing body; 13. left wingtip winglet; 14. right wingtip winglet; 15. center wing box; 2. upper mold; 21. reinforcing rib; 22. wing trailing edge groove; 23. locating pin hole; 24. M12 bolt hole; 25. fillet; 3. lower mold; 31. boss; 32. through hole; 33. guide groove; 4. winglet mold; 41. M12 countersunk screw hole; 42. groove; 43. M12 screw hole; 5. molding groove. DETAILED DESCRIPTION

[0044] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0045] Embodiment 1:

[0046] See also Figures 1 to 12 As shown, a composite wing forming mold comprises:

[0047] An upper mold 2, wherein a molding groove 5 for molding the wing body 1 is provided in the middle of the upper mold 2, and positioning pin holes 23 are provided at two diagonal portions of the upper mold 2, and the upper mold 2 is used to mold the entire upper surface of the wing body 1;

[0048] A lower mold 3, wherein a molding groove 5 and a positioning pin hole 23 matching the upper mold 2 are also provided in the middle of the lower mold 3, and the lower mold 3 is positioned and connected with the positioning pin hole 23 of the upper mold 2 through a positioning pin, and the lower mold 3 is used to mold the lower surfaces of the left wing body 11 and the right wing body 12 of the wing body 1;

[0049] The winglet molds 4 are two and are symmetrically arranged on both sides of the upper mold 2 and the lower mold 3 . The winglet molds 4 are used to shape the outer surfaces of the left wingtip winglet 13 and the right wingtip winglet 14 of the wing body 1 .

[0050] Specifically, both sides of the upper mold 2 , the lower mold 3 and the winglet mold 4 are provided with wing trailing edge grooves 22 , and the wing trailing edge grooves 22 are provided with fillets 25 .

[0051] Specifically, the upper mold 2 and the lower mold 3 evenly arrange M12 bolt holes 24 along the leading edge and trailing edge of the wing forming groove 5, wherein the M12 bolt holes 24 of the upper mold 2 are not designed with threads, and the M12 bolt holes 24 of the lower mold 3 are provided with threads, and the diameter of the M12 bolt holes 24 is set according to the maximum diameter of the M12 standard bolt.

[0052] Specifically, a boss 31 is provided on the bottom surface of the lower mold 3 at a position corresponding to the M12 bolt hole 24 .

[0053] Specifically, a through hole 32 is punched through the bottom surface of the lower mold 3 corresponding to the M12 bolt hole 24 .

[0054] Specifically, at least two screw holes are provided on the winglet mold 4, and two M12 screw holes 43 are provided on the side of the winglet mold 4, with a diameter enlarged by 1 mm, which are fixedly connected to the upper mold 2 by M12 bolts; two M12 screw holes 41 are provided at the bottom of the winglet mold 4, which are fixedly connected to the lower mold 3 by M12 countersunk screws 41, and a groove 42 is provided at the lower part of the winglet mold 4.

[0055] It can be seen from the above that when using the above-mentioned molding mold, the upper mold 2 and the lower mold 3 are first positioned by connecting the positioning pins in the positioning pin holes 23, and then the upper mold 2 and the lower mold 3 are threadedly connected to the M12 bolt holes 24 on the upper mold 2 and the lower mold 3 through the M12 standard bolts, so that the upper mold 2 and the lower mold 3 can be quickly fixed, and then the two winglet molds 4 are fixedly connected to the upper mold 2 through the M12 bolts, and fixedly connected to the lower mold 3 through the M12 countersunk screws, so as to complete the connection between the upper mold 2, the lower mold 3 and the two winglet molds 4, and then 100% carbon fiber prepreg is used to inject the molding groove 5 to obtain the wing body 1, and then the M12 countersunk screws 41 and the M12 standard bolts are removed for quick demolding.

[0056] Embodiment 2:

[0057] See also Figures 1 to 11 As shown, a composite wing forming mold comprises:

[0058] An upper mold 2, wherein a molding groove 5 for molding the wing body 1 is provided in the middle of the upper mold 2, and positioning pin holes 23 are provided at two diagonal portions of the upper mold 2, and the upper mold 2 is used to mold the entire upper surface of the wing body 1;

[0059] A lower mold 3, wherein a molding groove 5 and a positioning pin hole 23 matching the upper mold 2 are also provided in the middle of the lower mold 3, and the lower mold 3 is positioned and connected with the positioning pin hole 23 of the upper mold 2 through a positioning pin, and the lower mold 3 is used to mold the lower surfaces of the left wing body 11 and the right wing body 12 of the wing body 1;

[0060] The winglet molds 4 are two and are symmetrically arranged on both sides of the upper mold 2 and the lower mold 3 . The winglet molds 4 are used to shape the outer surfaces of the left wingtip winglet 13 and the right wingtip winglet 14 of the wing body 1 .

[0061] Specifically, the wing body 1 further includes a central wing box 15 in the middle, and the upper and lower surfaces of the central wing box 15 are both planes.

[0062] Specifically, both sides of the upper mold 2 , the lower mold 3 and the winglet mold 4 are provided with wing trailing edge grooves 22 , and the wing trailing edge grooves 22 are provided with fillets 25 .

[0063] Specifically, the upper mold 2 and the lower mold 3 evenly arrange M12 bolt holes 24 along the leading edge and trailing edge of the wing forming groove 5, wherein the M12 bolt holes 24 of the upper mold 2 are not designed with threads, and the M12 bolt holes 24 of the lower mold 3 are provided with threads, and the diameter of the M12 bolt holes 24 is set according to the maximum diameter of the M12 standard bolt.

[0064] Specifically, the upper mold 2 and the lower mold 3 are provided with a plurality of reinforcing ribs 21 along the direction of the central wing box 15 .

[0065] Specifically, a boss 31 is provided on the bottom surface of the lower mold 3 at a position corresponding to the M12 bolt hole 24 .

[0066] Specifically, a through hole 32 is punched through the bottom surface of the lower mold 3 corresponding to the M12 bolt hole 24 .

[0067] Specifically, a guide groove 33 is opened in the middle of the lower mold 3, and the plane between the guide groove 33 and the leading edge of the wing body 1 is 0.1 mm lower. Since the carbon fiber prepreg contains resin components, the resin will precipitate when the wing body 1 is heated and pressurized. In order to prevent the precipitated resin from affecting the molding of the wing body 1, a guide groove 33 is added along the leading edge of the wing of the lower mold 3, so that the precipitated resin has a place to go, and it is also convenient to clean this part of the resin.

[0068] Specifically, at least two screw holes are provided on the winglet mold 4, and two M12 screw holes 43 are provided on the side of the winglet mold 4, with a diameter enlarged by 1 mm, which are fixedly connected to the upper mold 2 by M12 bolts; two M12 screw holes 41 are provided at the bottom of the winglet mold 4, which are fixedly connected to the lower mold 3 by M12 countersunk screws, and a groove 42 is provided at the lower part of the winglet mold 4.

[0069] As can be seen from the above, when using the above-mentioned molding mold, firstly, the upper mold 2 and the lower mold 3 are positioned by connecting the positioning pins in the positioning pin holes 23, and then the upper mold 2 and the lower mold 3 are threadedly connected with the M12 bolt holes 24 on the upper mold 2 and the lower mold 3 through the M12 standard bolts, so that the upper mold 2 and the lower mold 3 can be quickly fixed, and then the two winglet molds 4 are threadedly fixedly connected with the corresponding M12 bolt holes 24 of the upper mold 2 by using the M12 countersunk screws 41, so as to complete the connection between the upper mold 2, the lower mold 3 and the two winglet molds 4, and then 100% carbon fiber prepreg is used to inject the molding groove 5 to obtain the wing body 1, and then the M12 countersunk screws 41 and the M12 standard bolts are removed to quickly demould;

[0070] In addition, the wing body 1 must be inspected for the wing outline dimensions after molding. If the mold is designed according to the specified wing body 1 outline dimensions, the actual dimensions of the wing body 1 may be slightly larger than the theoretical dimensions of the wing body 1 due to the errors that may be caused by laying prepreg and molding. Therefore, when designing the mold for the wing body 1, the part used to mold the wing surface should be appropriately adjusted in size. The specific size adjustment method is: the thickness direction is 0.5mm-0.8mm smaller than the theoretical thickness dimension, and the chord length is about 1mm smaller than the theoretical chord dimension.

[0071] In the actual molding process, the direction of the carbon fiber at the connection between the wing tip and the winglet is easily confused, which affects the strength of the winglet. Therefore, when designing the upper mold 2 and the winglet mold 4, the height of the winglet should be about 10 mm greater than the theoretical height, and the top of the mold for molding the winglet part is not closed. After the wing body 1 is prepared, the excess part can be trimmed and polished.

[0072] The trailing edge of the wing is small in size, forming a small and sharp right angle, which will bring inconvenience to the processing of the mold. Therefore, a fillet of 25 needs to be set at the corresponding mold position to reduce the difficulty of processing. After the wing is formed, the trailing edge of the wing can be trimmed and polished until it meets the size requirements in the chord length direction;

[0073] The upper mold 2 is a shell of uniform thickness to reduce the adverse effect of thermal stress on the molding accuracy, and a reinforcing rib 21 is set in the middle of the shell along the chord length direction of the wing;

[0074] The side surface of the upper mold 2 can be grooved to avoid the reinforcing ribs 21 and leave a groove of appropriate size to facilitate the placement and removal of the upper mold 2 and reduce the weight of the upper mold 2.

[0075] Embodiment three:

[0076] This design is specifically used in the aerospace field. The composite wing forming mold can effectively cope with the challenges of large aspect ratio and high precision wing manufacturing, ensuring that the wing structure is extremely lightweight while meeting aerodynamic performance, which plays a decisive role in improving the fuel efficiency and flight performance of the aircraft. The use of carbon fiber prepreg as the main material not only greatly reduces the weight of the wing, but also significantly enhances its load-bearing capacity and durability, making it an ideal choice for advanced aircraft design.

[0077] The invention always adheres to the principle of high preparation precision, light weight and easy processing during the design process. When manufacturing the mold, cutting, milling and drilling are used, and fine processing and rough processing are combined. Alloy steel materials are selected, and the density is about 7850kg / m 3 It is estimated that the weight of the upper mold 2 is 27kg, the weight of the lower mold 3 is 23.4kg, the weight of the left and right winglet molds 4 is 6.4kg each, and the total weight of the final mold assembly is approximately 63.2kg, which effectively controls the mold weight at a low level. It not only meets the needs of modern aircraft for high performance, lightweight and complex structural design, but also greatly improves manufacturing efficiency and cost control capabilities.

[0078] For further information, see Fig.13 As shown, a design method for a composite wing forming mold comprises the following steps:

[0079] S1. The part used for forming the wing surface should be appropriately sized. The specific sizing adjustment method is: the thickness direction is 0.5mm-0.8mm less than the theoretical thickness dimension, and the chord length is 1mm less than the theoretical chord length. When designing the upper mold 2 and the winglet mold 4, the height of the winglet should be 10mm greater than the theoretical height dimension, and the top of the mold for forming the winglet part is not closed. After the wing body 1 is prepared, the excess part is trimmed and polished;

[0080] S2. The trailing edge of the wing forms a small and sharp right angle, which will bring inconvenience to the processing of the mold. Therefore, a fillet of 25 is required at the corresponding mold position to reduce the processing difficulty. After the wing is formed, the trailing edge of the wing is trimmed and polished until it meets the size requirements in the chord length direction;

[0081] S3, positioning pin holes 23 are set at two diagonal positions of the upper mold 2 and the lower mold 3, and holes 32 are punched to ensure the accuracy of the mold clamping position. The positioning pin hole 23 is not set on the winglet mold 4. The positioning pin does not generate a fastening force and only plays a positioning role. M12 bolt holes 24 are evenly arranged along the leading edge and trailing edge of the wing. The bolts use M12 standard bolts. The M12 bolt holes 24 of the upper mold 2 are not designed with threads, and the diameter of the hole is set according to the maximum diameter of the M12 standard bolt.

[0082] S4, the upper mold 2 is a shell of equal thickness to reduce the adverse effect of thermal stress on the molding accuracy. A reinforcing rib 21 is set in the middle of the shell along the chord length direction of the wing. The side of the upper mold 2 is grooved to facilitate the placement of the upper mold 2 and reduce the weight of the upper mold 2.

[0083] S5. The lower mold 3 needs to be provided with an M12 bolt hole 24 at a position corresponding to the M12 bolt hole 24 of the upper mold 2, and a standard internal thread is designed at the same time. A reinforcing rib 21 is set in the middle of the shell, and a boss 31 is set at the position corresponding to the M12 bolt hole 24 on the bottom surface of the lower mold 3 to ensure the strength of the bolt connection. The M12 bolt hole 24 is punched with a through hole 32 to clean the resin precipitated after the wing is formed;

[0084] S6. A guide groove 33 is added along the leading edge of the wing of the lower mold 3. When the wing is heated and pressurized, the resin will precipitate through the guide groove 33. The plane between the guide groove 33 and the leading edge of the wing is lowered by about 0.1 mm, which facilitates the precipitated resin to flow into the guide groove 33.

[0085] S7, the connection mode of the winglet mold 4 and the lower mold 3 is selected to be connected by M12 countersunk screws. The M12 countersunk screw hole 41 is arranged in the middle of the step, and is installed and disassembled from the bottom of the winglet mold 4. When designing the M12 screw hole 43, the diameter of the hole is enlarged by 1mm, so that the winglet mold 4 and the upper mold 2 are bolted together;

[0086] S8. A groove 42 is opened at the lower part of the winglet mold 4. The curvature of the groove 42 is the same as the curvature of the connection between the wing tip and the winglet, which reduces the influence of thermal stress on wing forming and reduces the weight of the winglet mold 4. The reinforcing rib 21 at the bottom end of the winglet mold 4 is retained to increase the stability of the mold and avoid the adverse effect of the deadweight of the winglet mold 4 on the tightening force of the bolts. The lower mold 3 and the winglet mold 4 are connected in a stepped form, and a 1mm chamfer is set at the protruding corners of the step to prevent difficulty in connection due to processing errors at the corners.

[0087] As can be seen from the above, the mold mainly adopts the equal thickness design method, which reduces the weight of the mold and greatly reduces the adverse effects on the wing forming accuracy caused by uneven thermal stress during heating and curing and cooling to room temperature, ensuring the strength and accuracy of the wing after forming. The mold assembly solution can realize rapid disassembly and demolding of the wing after forming, ensuring the surface quality of the wing body 1.

[0088] In addition, after the mold processing is completed, protective materials can be electroplated on the outer surface to slow down the corrosion rate and extend the service life of the mold. In the molding preparation of the ultra-light composite wing prepared by the mold designed by the present invention, the molded wing body 1 has good demolding, high precision, and light weight, which meets the use requirements.

[0089] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A composite wing forming die, characterized in that: include: An upper mold (2), wherein a molding groove (5) for molding the wing body (1) is provided in the middle of the upper mold (2), positioning pin holes (23) are provided at two diagonal positions of the upper mold (2), and the upper mold (2) is used to mold the entire upper surface of the wing body (1); A lower mold (3), wherein a molding groove (5) and a positioning pin hole (23) matching the upper mold (2) are also provided in the middle of the lower mold (3), and the lower mold (3) is connected to the positioning pin hole (23) of the upper mold (2) by positioning pins, and the lower mold (3) is used to mold the lower surfaces of the left wing body (11) and the right wing body (12) of the wing body (1); The winglet molds (4) are two and are symmetrically arranged on both sides of the upper mold (2) and the lower mold (3). The winglet molds (4) are used to mold the outer surfaces of the left wingtip winglet (13) and the right wingtip winglet (14) of the wing body (1).

2. A composite wing forming mold according to claim 1, characterized in that: The wing body (1) further comprises a central wing box (15) in the middle, and the upper and lower surfaces of the central wing box (15) are both planes.

3. A composite wing forming mold according to claim 1, characterized in that: Both sides of the upper mold (2), the lower mold (3) and the winglet mold (4) are provided with wing trailing edge grooves (22), and the wing trailing edge grooves (22) are provided with rounded corners (25).

4. A composite wing forming mold according to claim 1, characterized in that: The upper mold (2) and the lower mold (3) are evenly arranged with M12 bolt holes (24) along the leading edge and trailing edge of the wing forming groove (5), wherein the M12 bolt holes (24) of the upper mold (2) are not designed with threads, and the M12 bolt holes (24) of the lower mold (3) are provided with threads, and the diameter of the M12 bolt holes (24) is set according to the maximum diameter of the M12 standard bolt.

5. A composite wing forming mold according to claim 1, characterized in that: The upper mold (2) and the lower mold (3) are provided with a plurality of reinforcing ribs (21) along the direction of the central wing box (15).

6. A composite wing forming mold according to claim 1, characterized in that: A boss (31) is provided on the bottom surface of the lower mold (3) at a position corresponding to the M12 bolt hole (24).

7. A composite wing forming mold according to claim 1, characterized in that: A through hole (32) is punched through the bottom surface of the lower mold (3) at a position corresponding to the M12 bolt hole (24).

8. The composite wing forming mold according to claim 1, characterized in that: A guide groove (33) is provided in the middle of the lower mold (3), and the plane between the guide groove (33) and the leading edge of the wing body (1) is 0.1 mm lower.

9. A composite wing forming mold according to claim 1, characterized in that: At least two screw holes are provided on the winglet mold (4); two M12 screw holes (43) are provided on the side of the winglet mold (4), the diameter of which is enlarged by 1 mm and fixedly connected to the upper mold (2) by M12 bolts; two M12 screw holes (41) are provided on the bottom of the winglet mold (4) and fixedly connected to the lower mold (3) by M12 countersunk screws; and a groove (42) is provided at the bottom of the winglet mold (4).

10. A method for designing a composite wing forming mold according to any one of claims 1 to 9, characterized in that: The following steps are involved: S1. The part used for forming the wing surface should be appropriately sized. The specific sized adjustment method is: the thickness direction is 0.5mm-0.8mm less than the theoretical thickness dimension, the chord length is 1mm less than the theoretical chord length, when designing the upper mold (2) and the winglet mold (4), the height of the winglet should be 10mm greater than the theoretical height dimension, and the top of the mold for forming the winglet part is not closed. After the wing body (1) is prepared, the excess part is trimmed and polished; S2. The trailing edge of the wing forms a small and sharp right angle, which will bring inconvenience to the processing of the mold. Therefore, a fillet (25) needs to be set at the corresponding mold position to reduce the processing difficulty. After the wing is formed, the trailing edge of the wing is trimmed and polished until it meets the size requirements in the chord length direction; S3, positioning pin holes (23) are arranged at two diagonal positions of the upper mold (2) and the lower mold (3), and a through hole (32) is punched to ensure the accuracy of the mold clamping position. The positioning pin hole (23) is not arranged on the winglet mold (4). The positioning pin does not generate a fastening force and only plays a positioning role. M12 bolt holes (24) are evenly arranged along the leading edge and trailing edge of the wing. The bolts use M12 standard bolts. No threads are designed in the M12 bolt holes (24) of the upper mold (2). The diameter of the hole is set according to the maximum diameter of the M12 standard bolt. S4, the upper mold (2) is a shell of uniform thickness to reduce the adverse effect of thermal stress on molding accuracy. A reinforcing rib (21) is arranged in the middle of the shell along the chord length direction of the wing. The side of the upper mold (2) is grooved to facilitate the placement of the upper mold (2) and also reduce the weight of the upper mold (2). S5. The lower mold (3) needs to be provided with an M12 bolt hole (24) at a position corresponding to the M12 bolt hole (24) of the upper mold (2), and a standard internal thread is designed at the same time. A reinforcing rib (21) is set in the middle of the shell. A boss (31) is set at a position corresponding to the M12 bolt hole (24) on the bottom surface of the lower mold (3) to ensure the strength of the bolt connection. A through hole (32) is punched through the M12 bolt hole (24) to clean the resin precipitated after the wing is formed. S6. A guide groove (33) is added along the leading edge of the wing of the lower mold (3). When the wing is heated and pressurized, the resin will precipitate through the guide groove (33). The plane between the guide groove (33) and the leading edge of the wing is lowered by about 0.1 mm, so that the precipitated resin can flow into the guide groove (33); S7. The connection method between the winglet mold (4) and the lower mold (3) is selected to be connected by M12 countersunk screws. The M12 countersunk screw hole (41) is arranged in the middle of the step, and the installation and removal are carried out from the bottom of the winglet mold (4). When designing the M12 screw hole (43), the diameter of the hole is enlarged by 1 mm, so that the winglet mold (4) and the upper mold (2) are bolted together. S8. A groove (42) is formed at the bottom of the winglet mold (4). The curvature of the groove (42) is the same as the curvature of the connection between the wing tip and the winglet, so as to reduce the influence of thermal stress on the wing molding and also reduce the weight of the winglet mold (4). The reinforcing rib (21) at the bottom of the winglet mold (4) is retained to increase the stability of the mold and avoid the adverse effect of the deadweight of the winglet mold (4) on the tightening force of the bolts. The lower mold (3) and the winglet mold (4) are connected in a stepped form, and a 1 mm chamfer is set at the protruding corners of the step to prevent difficulty in connection due to processing errors at the corners.