Preparation method of quantum dot optical diffusion plate
By performing surface modification of quantum dots and reasonable mixing of polymer matrix, combined with the preparation of inorganic-organic composite protective layer, the problem of poor stability of quantum dot optical diffusion plates in the environment is solved, and the reduction of fluorescence quenching and optical performance is achieved. Long-term maintenance of performance.
Patent Information
- Application Number
- CN202411280003.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-12
- Publication Date
- 2024-11-22
AI Technical Summary
Quantum dot optical diffusion plates are prone to fluorescence quenching in the environment, and the existing preparation methods are difficult to cope with their sensitivity to temperature, water, ultraviolet light and oxygen, resulting in poor stability.
By selecting the quantum dots of the core-shell structure and performing surface modification, combining polymer matrix and additives, an inorganic-organic composite protective layer is prepared to enhance its resistance to ultraviolet light and ensure uniform dispersion and stability of the quantum dots.
It effectively improves the stability of the quantum dot optical diffusion plate, reduces the possibility of fluorescence quenching, extends the service life of the product and improves reliability, ensuring its optical performance and physical structure stability in complex environments.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of quantum dots, in particular to a method for preparing a quantum dot optical diffusion plate. Background Art
[0002] As an emerging semiconductor material, quantum dots have the characteristics of narrow emission half-width, high color purity, adjustable color and solution processability. Due to its narrow emission half-width, LCD combined with quantum dot technology can achieve high color gamut coverage, which is significantly better than traditional LCD using phosphors. The diffuser is an indispensable and important component in the backlight of liquid crystal display, which can play the role of atomizing light. Integrating quantum dots into the diffuser to prepare a quantum dot diffuser with a sandwich structure can not only homogenize the incident light, but also avoid the use of expensive water vapor barrier films. Therefore, it has great development potential in the field of liquid crystal display. In the prior art, the preparation of quantum dot optical diffuser plates faces many challenges. Due to their special physical and chemical properties, quantum dots are very sensitive to environmental factors such as temperature, water, ultraviolet light and oxygen. Traditional preparation methods often fail to fully address these sensitivity issues, resulting in the phenomenon of fluorescence quenching in quantum dots. Many preparation processes do not perform effective surface modification on quantum dots or the modification methods used are not ideal, making quantum dots easily disturbed in the environment and lose stability, resulting in fluorescence quenching. Summary of the invention
[0003] In view of the shortcomings of the prior art, the present invention provides a method for preparing a quantum dot optical diffusion plate, which solves the problem in the prior art that quantum dots are very likely to experience fluorescence quenching in the environment.
[0004] To achieve the above objectives, the present invention is implemented by the following technical solutions: A method for preparing a quantum dot optical diffusion plate comprises the following steps: S1. Surface modification of quantum dots: S1.1. Select a core-shell structure quantum dot material with a particle size range of 3-5 nm; S1.2. The quantum dots are dispersed in an organic solvent, toluene, to form a quantum dot solution having a concentration of 0.1 mol / L; S1.3. Add a surface modifier to the quantum dot solution to modify the surface of the quantum dots and improve the stability of the quantum dots; S2. Preparation of polymer matrix solution: The polymer matrix material is selected as polymethyl methacrylate, which is dissolved in an organic solvent chloroform to form a polymer matrix solution with a mass fraction of 10%-20%; S3. Mixing of quantum dots with polymer matrix: The surface-modified quantum dot solution and the polymer matrix solution are mixed in a volume ratio of 1:3, and the mixed solution is stirred at 20-30° C. for 4-6 hours at a stirring speed of 200-400 rpm to ensure that the quantum dots are evenly dispersed in the polymer matrix solution; S4. Adding light stabilizer and UV absorber: Adding a light stabilizer and a UV absorber into the mixed solution to improve the resistance of the quantum dot optical diffuser to UV light; S5. Degassing treatment: The mixed solution after adding the light stabilizer and the ultraviolet absorber is subjected to a degassing treatment by using a vacuum degassing method with a vacuum degree of -0.09 MPa and a degassing time of 2 hours to remove bubbles in the solution; S6. Molding: The degassed mixed solution is injected into a mold, and heated and cured at 60° C. for 10 hours to allow the mixed solution to be cured and formed into a quantum dot optical diffusion plate blank; S7. Preparation of surface protective layer: A protective layer is prepared on the surface of the quantum dot optical diffusion plate blank, wherein the protective layer material is an inorganic-organic composite coating, wherein the inorganic component is silicon dioxide, and the organic component is an acrylic resin modified by a silane coupling agent; S8. Post-processing: The quantum dot optical diffuser plate with the prepared protective layer is cut and polished to make its size and surface flatness meet the requirements, thereby obtaining the final quantum dot optical diffuser plate.
[0005] Preferably, the core of the quantum dot material of the core-shell structure is selected from one of CdSe, CdS, CdTe or InP, and the shell is one or more of ZnS, ZnSe and other inorganic semiconductor materials with matching band gaps.
[0006] Preferably, the surface modifier in S1.3 is a long-chain alkylamine, the amount added is 1.5-2.5 times the amount of the quantum dot substance, and the reaction is stirred at 30° C. for 4 hours at a reaction speed of 500 rpm.
[0007] Preferably, S2 further comprises adding an antioxidant into the polymer matrix solution, wherein the antioxidant is a hindered phenol antioxidant, and the amount added is 0.3%-0.7% of the mass of the polymer matrix to prevent the quantum dots from being oxidized.
[0008] Preferably, the light stabilizer in S4 is a hindered amine light stabilizer, and the added amount is 0.3% of the mass of the mixed solution; the ultraviolet absorber is a benzotriazole ultraviolet absorber, and the added amount is 0.2% of the mass of the mixed solution.
[0009] Preferably, S7 also includes depositing a layer of silicon dioxide on the surface of the quantum dot optical diffuser plate blank by chemical vapor deposition, the thickness of the silicon dioxide layer is adjusted between 30-80nm, the flow rate of the reaction gas silane is adjusted between 30-80sccm, the flow rate of oxygen is adjusted between 80-150sccm, and the deposition temperature is adjusted between 280-320°C.
[0010] Preferably, S7 further comprises immersing the quantum dot optical diffusion plate blank into a silane coupling agent-modified acrylic resin solution for 25-35 minutes, and drying it at 70-80° C. for 1-2 hours after taking it out, so that a protective layer is formed on the surface to block the intrusion of water and oxygen.
[0011] Preferably, the cutting operation in S8 adopts laser cutting technology with a cutting accuracy of ±0.05 mm; the grinding operation adopts precision grinding equipment to make the surface roughness reach below Ra0.1.
[0012] The present invention provides a method for preparing a quantum dot optical diffusion plate. It has the following beneficial effects: 1. The present invention improves the stability of quantum dots themselves by selecting suitable core-shell structure quantum dots and performing surface modification with long-chain alkylamines. A hindered phenol antioxidant is added during the preparation of the polymer matrix solution, and an inorganic-organic composite protective layer is prepared on the surface of the formed diffusion plate blank, which can effectively block the intrusion of water and oxygen. At the same time, hindered amine light stabilizers and benzotriazole ultraviolet absorbers are added to enhance the resistance to ultraviolet light, greatly reducing the possibility of fluorescence quenching of quantum dots in various environments, thereby ensuring the optical performance of the quantum dot optical diffusion plate in complex environments.
[0013] 2. The present invention ensures that the quantum dots are evenly dispersed in the system and avoids agglomeration through surface modification of quantum dots, reasonable mixing with a polymer matrix, and the use of various additives, which helps to maintain the stability of its optical properties for a long time. The overall preparation process enables the optical properties and physical structure of the quantum dot optical diffuser plate to remain relatively stable under different environmental conditions, thereby extending the service life of the product and improving reliability. DETAILED DESCRIPTION
[0014] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0015] Embodiment 1: An embodiment of the present invention provides a method for preparing a quantum dot optical diffuser plate, comprising the following steps: S1. Select a quantum dot material with a core-shell structure, wherein the core is CdSe with a cubic crystal structure, and the shell is ZnS with a thickness of 1 nm and a particle size of 3 nm. Disperse the quantum dots in an organic solvent, toluene. Toluene is selected as the organic solvent for quantum dots because it has good solubility for quantum dots and moderate volatility, and can maintain the dispersed state of quantum dots during the reaction. Prepare a quantum dot solution with a concentration of 0.1 mol / L, add a long-chain alkylamine as a surface modifier to the quantum dot solution, and the amount added is 1.5 times the amount of the quantum dot substance. Stir the reaction at 30°C and 500 rpm for 4 hours to modify the surface of the quantum dots with the long-chain alkylamine, thereby improving the stability of the quantum dots. S2. Select polymethyl methacrylate as the polymer matrix material, dissolve it in the organic solvent chloroform to form a polymer matrix solution with a mass fraction of 10%. At the same time, add a hindered phenol antioxidant to the polymer matrix solution in an amount of 0.3% of the mass of the polymer matrix to prevent the quantum dots from being oxidized; S3. Mix the surface-modified quantum dot solution with the polymer matrix solution in a volume ratio of 1:3. Stir the mixed solution at 200 rpm at 20°C for 6 hours to ensure that the quantum dots are evenly dispersed in the polymer matrix solution; S4. Adding a hindered amine light stabilizer and a benzotriazole ultraviolet absorber to the mixed solution, wherein the light stabilizer is added in an amount of 0.3% by mass of the mixed solution, and the ultraviolet absorber is added in an amount of 0.2% by mass of the mixed solution to improve the resistance of the quantum dot optical diffuser to ultraviolet light; S5. The mixed solution after adding the light stabilizer and the ultraviolet absorber was degassed by vacuum degassing, and the vacuum degree was set to -0.09MPa, and the degassing time was 2 hours to remove bubbles in the solution; S6. The mixed solution after degassing is injected into the mold, and heated and cured at 60°C for 9 hours to cure the mixed solution into a quantum dot optical diffuser blank; S7. Prepare a protective layer on the surface of the quantum dot optical diffuser plate blank. First, a layer of silicon dioxide is deposited on the surface of the quantum dot optical diffuser plate blank by chemical vapor deposition, and the thickness of the silicon dioxide layer is set to 30nm, the flow rate of the reaction gas silane is 30sccm, the flow rate of the oxygen is 80sccm, and the deposition temperature is 280°C. Then, the quantum dot optical diffuser plate blank is immersed in a silane coupling agent-modified acrylic resin solution for 25 minutes. After taking it out, it is dried at 70°C for 2 hours to form a protective layer on the surface, thereby blocking the intrusion of water and oxygen; S8. The quantum dot optical diffuser plate with a prepared protective layer is cut using laser cutting technology, with the cutting accuracy controlled at ±0.05mm; then it is polished using precision polishing equipment to make the surface roughness reach below Ra0.1, and finally a quantum dot optical diffuser plate with size and surface flatness that meet the requirements is obtained.
[0016] Embodiment 2: An embodiment of the present invention provides a method for preparing a quantum dot optical diffuser plate, comprising the following steps: S1. Select core-shell structure quantum dots, the core is cubic lnP, the shell is ZnSe, the thickness is 2nm, the particle size is 5nm, disperse them in toluene to prepare a quantum dot solution with a concentration of 0.1mol / L, add long-chain alkylamine to the quantum dot solution, the amount added is 2.5 times the amount of quantum dot substance, stir and react at 30°C and 500 rpm for 4 hours to achieve surface modification of quantum dots to improve stability; S2. Take polymethyl methacrylate as the polymer matrix material and dissolve it in chloroform to form a polymer matrix solution with a mass fraction of 20%. Add a hindered phenol antioxidant to it in an amount of 0.7% of the mass of the polymer matrix to prevent the quantum dots from oxidizing; S3. Mix the surface-modified quantum dot solution and the polymer matrix solution in a volume ratio of 1:3. Stir the mixed solution at 400 rpm for 4 hours at 30°C to ensure that the quantum dots are evenly dispersed in the polymer matrix solution; S4. Adding a hindered amine light stabilizer (the amount added is 0.3% of the mass of the mixed solution) and a benzotriazole ultraviolet absorber (the amount added is 0.2% of the mass of the mixed solution) to the mixed solution to enhance the resistance to ultraviolet light; S5. The mixed solution after adding the additive was subjected to vacuum degassing treatment, the vacuum degree was -0.09MPa, and the bubbles were removed by degassing for 2 hours; S6. The mixed solution after degassing is injected into the mold, and heated and cured at 70°C for 8 hours to cure the mixed solution into a quantum dot optical diffuser blank; S7. Prepare a protective layer on the surface of the quantum dot optical diffuser blank. First, a silicon dioxide layer is deposited on the surface by chemical vapor deposition, the thickness of the silicon dioxide layer is set to 80nm, the silane flow rate is 80sccm, the oxygen flow rate is 150sccm, and the deposition temperature is 320°C. Then, the blank is immersed in a silane coupling agent-modified acrylic resin solution for 35 minutes, and then taken out and dried at 80°C for 1 hour to form a protective layer to block water and oxygen; S8. The quantum dot optical diffuser plate with a prepared protective layer is cut using laser cutting technology, with the cutting accuracy controlled at ±0.05mm; then it is polished using precision polishing equipment to make the surface roughness reach below Ra0.1, and finally a quantum dot optical diffuser plate with size and surface flatness that meet the requirements is obtained.
[0017] Through the surface modification of quantum dots, reasonable mixing with polymer matrix and the use of various additives in the above-mentioned embodiments, it is ensured that the quantum dots are evenly dispersed in the system to avoid agglomeration, which helps to maintain the stability of its optical properties for a long time. The addition of antioxidants, light stabilizers and ultraviolet absorbers enables the quantum dots to maintain a stable structure and performance when facing oxidation, ultraviolet light irradiation and the like. The preparation of the surface protective layer further ensures stability from the perspective of the external environment. Whether it is to resist external water and oxygen erosion or to cope with temperature changes, it can effectively protect the internal quantum dot structure. The overall preparation process is strictly controlled by parameters so that the optical properties and physical structure of the quantum dot optical diffuser plate can remain relatively stable under different environmental conditions, thereby extending the service life of the product and improving reliability.
[0018] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for preparing a quantum dot optical diffuser plate, characterized in that: The following steps are involved: S1. Surface modification of quantum dots: S1.
1. Select a core-shell structure quantum dot material with a particle size range of 3-5 nm; S1.
2. The quantum dots are dispersed in an organic solvent, toluene, to form a quantum dot solution having a concentration of 0.1 mol / L; S1.
3. Add a surface modifier to the quantum dot solution to modify the surface of the quantum dots and improve the stability of the quantum dots; S2. Preparation of polymer matrix solution: The polymer matrix material is selected as polymethyl methacrylate, which is dissolved in an organic solvent chloroform to form a polymer matrix solution with a mass fraction of 10%-20%; S3. Mixing of quantum dots with polymer matrix: The surface-modified quantum dot solution and the polymer matrix solution are mixed in a volume ratio of 1:3, and the mixed solution is stirred at 20-30° C. for 4-6 hours at a stirring speed of 200-400 rpm to ensure that the quantum dots are evenly dispersed in the polymer matrix solution; S4. Adding light stabilizer and UV absorber: Adding a light stabilizer and a UV absorber into the mixed solution to improve the resistance of the quantum dot optical diffuser to UV light; S5. Degassing treatment: The mixed solution after adding the light stabilizer and the ultraviolet absorber is subjected to a degassing treatment by using a vacuum degassing method with a vacuum degree of -0.09 MPa and a degassing time of 2 hours to remove bubbles in the solution; S6. Molding: The degassed mixed solution is injected into a mold, and heated and cured at 50-70° C. for 8-10 hours to cure the mixed solution into a quantum dot optical diffusion plate blank; S7. Preparation of surface protective layer: A protective layer is prepared on the surface of the quantum dot optical diffusion plate blank, wherein the protective layer material is an inorganic-organic composite coating, wherein the inorganic component is silicon dioxide, and the organic component is an acrylic resin modified by a silane coupling agent; S8. Post-processing: The quantum dot optical diffuser plate with the prepared protective layer is cut and polished to make its size and surface flatness meet the requirements, thereby obtaining the final quantum dot optical diffuser plate.
2. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The core of the quantum dot material of the core-shell structure is selected from one of CdSe, CdS, CdTe or InP, and the shell is one or more of ZnS, ZnSe and other inorganic semiconductor materials with matching band gaps.
3. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The surface modifier in S1.3 is a long-chain alkylamine, the amount of which is 1.5-2.5 times the amount of the quantum dot substance, and the reaction is stirred at 30° C. for 4 hours at a reaction speed of 500 rpm.
4. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The S2 further comprises adding an antioxidant into the polymer matrix solution, wherein the antioxidant is a hindered phenol antioxidant, and the amount of the antioxidant added is 0.3%-0.7% of the mass of the polymer matrix to prevent the quantum dots from being oxidized.
5. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The light stabilizer in S4 is a hindered amine light stabilizer, and the added amount is 0.3% of the mass of the mixed solution; the ultraviolet absorber is a benzotriazole ultraviolet absorber, and the added amount is 0.2% of the mass of the mixed solution.
6. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The S7 also includes depositing a silicon dioxide layer on the surface of the quantum dot optical diffuser blank by chemical vapor deposition, wherein the thickness of the silicon dioxide layer is adjusted between 30-80 nm, the flow rate of the reaction gas silane is adjusted between 30-80 sccm, the flow rate of the oxygen is adjusted between 80-150 sccm, and the deposition temperature is adjusted between 280-320°C.
7. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The step S7 further includes immersing the quantum dot optical diffusion plate blank into a silane coupling agent-modified acrylic resin solution for 25-35 minutes, and drying it at 70-80° C. for 1-2 hours to form a protective layer on the surface to block the intrusion of water and oxygen.
8. The method for preparing a quantum dot optical diffuser plate according to claim 1, characterized in that: The cutting operation in S8 adopts laser cutting technology with a cutting accuracy of ±0.05mm; the grinding operation adopts precision grinding equipment to make the surface roughness reach below Ra0.1.
Citation Information
Cited By
Composite particle and preparation method thereof, and LED packaging body preparation method
CN119552317A
Composite particles, method for preparing the same, and method for preparing an LED packaging body
CN119552317B