Preparation method of high-strength and high-toughness cellulose hydrogel

By using ethanol to treat cellulose gels on the dual crosslinking strategy, the crystallinity of cellulose hydrogels is improved, and the problem of insufficient mechanical properties of cellulose hydrogels is solved, and the combination of high strength and high toughness is achieved, which expands the Its application potential in multiple fields.

CN119019714AInactive Publication Date: 2024-11-26SICHUAN UNIV

Patent Information

Application Number
CN202411329218.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing cellulose hydrogels have shortcomings in mechanical strength and toughness, which leads to their prone to rupture and fatigue fracture under external forces, and become brittle in dry or extreme environments, limiting their inability to biomedical and flexible electronics. Application in the field.

Method used

Based on the dual crosslinking strategy, the alkaline cellulose gel is treated with ethanol to control the self-assembly behavior of the cellulose chain and induce hydrophobic accumulation between the cellulose chains, thereby improving the crystallinity of the cellulose hydrogel. Prepare a high-strength, high-toughness cellulose hydrogel.

Benefits of technology

It significantly improves the compressive strength and elastic modulus of cellulose hydrogel, enhances its crystallinity and swelling resistance, realizes a combination of high strength and high toughness, is suitable for materials of various morphology and sizes, expanding Its application value in biomedicine, flexible electronics and water treatment fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

The invention relates to a preparation method of high-strength and high-toughness cellulose hydrogel, and belongs to the field of material science. The preparation method comprises the following steps: dissolving cellulose in an alkaline solution, cross-linking by using epoxy chloropropane, pouring into a mold or emulsifying, annealing and regenerating, exposing regenerated cellulose hydrogel in ethanol steam, soaking in an ethanol water solution with a certain concentration, and washing ethanol in the hydrogel by using deionized water. Results show that the cellulose hydrogel prepared by the method has high strength and high toughness, the method is simple and convenient to operate, the raw materials are cheap and easy to obtain, and the prepared cellulose hydrogel with various shapes has good mechanical properties and can be applied to the fields of flexible electronic devices, biomedical equipment and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of material science, and particularly relates to a method for preparing a high-strength and high-toughness cellulose hydrogel. Background Art

[0002] Hydrogels are high-water-content materials with a three-dimensional polymer network structure. Due to their unique physical and chemical properties, they have very wide applications in the fields of biomedicine, flexible electronics, environmental treatment, etc. Although hydrogels have many advantages, they usually have the following strength defects: (1) Low mechanical strength: The polymer network of hydrogels is relatively fragile and easily breaks when subjected to external forces; (2) Insufficient toughness: Hydrogels may suffer fatigue fracture under repeated stretching or compression; (3) Poor structural stability: In dry or extreme environments, hydrogels may lose water and become brittle. The poor mechanical properties of hydrogels have seriously hindered their practical applications. Many strategies have been used to improve the strength or toughness of hydrogels, such as macromolecular cross-linking, interpenetrating networks, composite materials, double cross-linking, etc.

[0003] Cellulose, as an abundant renewable biomass resource, has excellent biocompatibility and biodegradability, and is an ideal candidate material for hydrogel construction. In fact, the large number of hydroxyl groups present on the polysaccharide chains provide sufficient positions for the formation of non-covalent interactions (such as hydrogen bonds and hydrophobic interactions). Traditionally, the methods to improve the strength of cellulose hydrogels are mainly physical, chemical cross-linking or double cross-linking. The main limitation of current strategies is that hydrogel strengthening is usually achieved by increasing the cross-linking density, which leads to reduced ductility. Therefore, stronger hydrogels are usually brittle and lack toughness. How to overcome the conflict between strength and toughness and obtain hydrogels with both high strength and toughness is still an urgent problem to be solved.

[0004] In order to make up for the defects of mechanical properties of traditional cellulose hydrogel materials and improve their application value, the present invention proposes a new method for preparing cellulose high-strength and high-toughness hydrogel. The characteristics of this preparation method are: on the basis of the double cross-linking strategy, the alkaline cellulose gel is treated with ethanol, and the self-assembly behavior of the cellulose chain is controlled to induce the hydrophobic accumulation between the cellulose chains, thereby improving the crystallinity of the cellulose hydrogel, thereby obtaining a cellulose hydrogel with both high strength and high toughness. Summary of the invention

[0005] In view of the shortcomings of the background technology, the present invention provides a method for preparing a cellulose hydrogel having both high strength and high toughness by improving the crystallinity of the cellulose hydrogel, and the specific scheme is as follows:

[0006] A method for preparing a high-strength and high-toughness cellulose hydrogel, characterized by comprising the following steps: (1) preparation of annealed alkaline cellulose gel: dissolving cellulose in an alkaline solution, adding epichlorohydrin dropwise at -4°C while stirring, centrifuging the cellulose solution to remove bubbles, then pouring the cellulose solution into a mold or emulsifying it to prepare microspheres of different particle sizes, and annealing it at a specific temperature for 1 to 36 hours to obtain an annealed alkaline cellulose gel; (2) preparation of a high-crystallinity cellulose gel: placing the cellulose gel obtained in the previous step in an ethanol vapor environment for 8 to 48 hours, and then regenerating it in a certain concentration of ethanol aqueous solution at 5°C for 0 to 96 hours to obtain a cellulose gel with high crystallinity; (3) double-crosslinked cellulose hydrogel: washing the high-crystallinity cellulose gel obtained in the previous step with deionized water to remove ethanol and alkali to prepare a high-strength and high-toughness cellulose hydrogel.

[0007] The method for preparing a high-strength and high-toughness cellulose hydrogel as claimed in claim 1, characterized in that the cellulose used in step (1) is cotton linter pulp, microcrystalline cellulose, bacterial cellulose, bamboo fiber, ramie fiber and natural cellulose of other sizes.

[0008] A method for preparing a high-strength and high-toughness cellulose hydrogel as described in claim 1, characterized in that the cellulose solvent used in step (1) can be NaOH / urea, NaOH / alkaline urea, LiOH / urea, and the concentration of the cellulose solution is 6wt%~10wt%.

[0009] A method for preparing a high-strength and high-toughness cellulose hydrogel as claimed in claim 1, characterized in that the amount of epichlorohydrin added in step (1) is 1-2.5 mL / 50 mL of cellulose solution.

[0010] The method for preparing a high-strength and high-toughness cellulose hydrogel as described in claim 1 is characterized in that the mold used in step (1) can be any desired shape such as cylindrical, spherical, strip, lamellar, etc.

[0011] A method for preparing a high-strength and high-toughness cellulose hydrogel as described in claim 1, characterized in that the emulsion ratio used in step (1) is 40~60 mL white oil, 60~80 mL isooctane, 4.5~5.5 g Span 80 and 1.0~1.2 g Tween 80, and a mixer or homogenizer can be used for emulsification, and microspheres with a particle size ranging from a few microns to hundreds of microns can be obtained by controlling the stirring speed.

[0012] A method for preparing a high-strength and high-toughness cellulose hydrogel as described in claim 1, characterized in that the microspheres prepared in step (1) must be re-immersed in an alkaline solution after removing the oil phase by alcohol washing and water washing to ensure that the alkaline annealed gel is subjected to the next experiment.

[0013] A method for preparing a high-strength and high-toughness cellulose hydrogel as described in claim 1, characterized in that the annealing temperature used in step (1) is 5~80°C, and in order to avoid excessive evaporation of water during annealing, the mold containing the cellulose solution is placed in a sealed room with a small amount of water.

[0014] A method for preparing a high-strength and high-toughness cellulose hydrogel as described in claim 1, characterized in that the concentration of the ethanol aqueous solution used in step (2) is 75 wt%.

[0015] Compared with the prior art, the present invention has the following advantages:

[0016] The invention has simple operation, readily available raw materials and is easy for large-scale industrial production.

[0017] Compared with traditional cellulose hydrogels, the strength and toughness of the cellulose hydrogel prepared by the present invention are greatly improved, and the experimental method can be extended to other polysaccharides such as agarose, chitosan, etc.

[0018] The experimental principle of the present invention can be applied to materials of various shapes and sizes, including columns, strips, films and micron-sized microspheres. The product has a wide range of applications and can achieve high application value in the fields of biomedical bases, flexible electronics, water treatment, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 :High-strength and high-toughness cellulose hydrogel columns prepared in Example 1 and their compressive strength test, (A) SC8% is a traditional cellulose hydrogel column (directly washed with water after annealing to remove excess solvent, without subsequent steps), A / DC 8% is a high-strength and high-toughness hydrogel column; (B) Compression curves and elastic moduli of SC 8% and A / DC 8%.

[0020] Figure 2:High-strength and high-toughness cellulose hydrogel strips prepared in Example 2 and their tensile strength tests, (A) SC-DI is a traditional cellulose hydrogel strip (directly washed with water to remove excess solvent after annealing, without subsequent steps), A / DC-ET is a high-crystallinity cellulose hydrogel strip (soaked in 75% ethanol but not washed with deionized water), A / DC-DI is a high-strength and high-toughness hydrogel strip (obtained by washing A / DC-ET with water); (B) Tensile curves of SC-DI, A / DC-ET and A / DC-DI; (C) Elastic modulus, yield strength, tensile strength and strain of SC-DI, A / DC-ET and A / DC-DI.

[0021] Figure 3 :High-strength and high-toughness cellulose hydrogel microspheres prepared in Example 3 and their compressive performance test, (A) Microscope image of high-strength and high-toughness cellulose hydrogel microspheres; (B) Column pressure test curve of high-strength and high-toughness cellulose hydrogel microspheres, SC-DI is a traditional cellulose hydrogel microsphere (directly washed with water after annealing to remove excess solvent, without subsequent steps), A / DC-ET is a high-crystallinity cellulose hydrogel microsphere (soaked in 75% ethanol without washing with deionized water), A / DC-DI is a high-strength and high-toughness hydrogel microsphere (obtained by washing A / DC-ET with water). DETAILED DESCRIPTION

[0022] The following examples further illustrate the content of the present invention, but should not be construed as limiting the present invention. Without departing from the spirit and essence of the present invention, modifications or substitutions made to the methods, steps or conditions of the present invention all fall within the scope of the present invention.

[0023] Example 1: High-strength and high-toughness cellulose hydrogel column

[0024] 4 g of microcrystalline cellulose was dissolved in 46 g of LiOH / urea solution with a LiOH concentration of 8 wt% and a urea concentration of 12 wt% to obtain a cellulose solution with a concentration of 8 wt%; 2.5 mL of epichlorohydrin was added under an ice bath and stirred vigorously for 10 min; the cellulose solution was poured into a 10 mL small beaker, sealed with plastic wrap and placed in a plate filled with water, and then annealed in an oven at 60 degrees Celsius for 45 min to obtain annealed alkaline cellulose gel; the cellulose column was taken out of the beaker and steamed in an ethanol vapor environment for 8 h; the steamed cellulose column was soaked in a 75 wt% ethanol aqueous solution for 48 h, and the soaked cellulose column was washed with water to remove excess alcohol and alkali.

[0025] like Figure 1As shown in (A), the high-strength and high-toughness hydrogel A / DC 8% obtained after alkaline annealed cellulose gel was soaked in ethanol showed a smaller column diameter than the ordinary cellulose hydrogel SC 8%. This is because the higher crystallinity of A / DC 8% leads to improved anti-swelling performance. In addition, Figure 1 (B) It can be seen that the compressive strength and elastic modulus of A / DC 8% are significantly higher than those of SC 8%, which are approximately 3 times and 5 times that of SC 8%, respectively. This shows that this experimental principle can effectively improve the compressive properties of cellulose hydrogel by increasing its crystallinity.

[0026] Example 2: High-strength and high-toughness cellulose hydrogel strips

[0027] 5 g of microcrystalline cellulose was dissolved in 45 g of LiOH / urea solution with a LiOH concentration of 8 wt% and a urea concentration of 12 wt% to obtain a cellulose solution with a concentration of 10 wt%; 2.5 mL of epichlorohydrin was added under an ice bath and stirred vigorously for 10 min; the cellulose solution was poured into a long strip mold with a size of 80*40*4 mm, and then annealed in an oven at 60 degrees Celsius for 45 min to obtain annealed alkaline cellulose gel; after taking the cellulose strip out of the beaker, it was steamed in an ethanol vapor environment for 8 h; the steamed cellulose strip was soaked in a 75 wt% ethanol aqueous solution for 48 h, and the soaked cellulose strip was washed with water to remove excess alcohol and alkali.

[0028] like Figure 2 As shown in (A), the high-crystallinity cellulose gel strip A / DC-ET has a smaller swelling degree and a darker color than the traditional cellulose hydrogel strip SC-DI and the high-strength and high-toughness hydrogel strip A / DC-DI. This is because the water content of A / DC-ET is low due to immersion in ethanol, and the crystallinity is significantly higher than that of the other two strips. Therefore, the use of ethanol to steam alkaline cellulose gel can effectively improve the crystallinity and anti-swelling properties of cellulose gel; accordingly, from Figure 2 As can be seen from (B) and (C), the highly crystalline A / DC-ET has the largest modulus, yield strength and tensile strength. At the same time, the A / DC-DI obtained after further water washing still retains a higher crystallinity than SC-DI. Therefore, A / DC-DI exhibits stronger modulus, yield strength and tensile strength than SC-DI. Figure 2 As can be seen from the Strain in (C), the elongation of A / DC-ET and A / DC-DI has been significantly improved compared with that of SC-DI, indicating that this experimental scheme can effectively improve the strength and toughness of cellulose hydrogel at the same time.

[0029] Example 3: High-strength and high-toughness cellulose hydrogel microspheres

[0030] 5 g of microcrystalline cellulose was dissolved in 45 g of NaOH / thiourea solution with a NaOH concentration of 10 wt% and a thiourea concentration of 8 wt% to obtain a cellulose solution with a concentration of 10 wt%; 2.5 mL of epichlorohydrin was added under ice bath and stirred vigorously for 10 min; the cellulose solution was slowly poured into the oil phase and emulsified for 30 min below 20°C, with the oil phase ratio of white oil 40 mL, isooctane 80 mL, Span80 5.5 g and Tween 80 1.0 g, then gradually heated to 45°C under a water bath and maintained for 45 min to obtain annealed alkaline cellulose gel microspheres; the cellulose microspheres were separated from the oil phase by centrifugation, and the excess oil phase was washed with 50% ethanol and water, then soaked in NaOH / thiourea solution for 48 h, and the soaked microspheres were steamed in an ethanol vapor environment for 8 h; the steamed cellulose microspheres were soaked in a 75 wt% ethanol aqueous solution for 48 h. h, washing the soaked cellulose microspheres with water to remove excess alcohol and alkali.

[0031] like Figure 3 As shown in (A), the high-crystallinity cellulose gel microspheres have a good spherical appearance, and the particle size distribution of the microspheres prepared by emulsification is relatively wide. After further screening or by controlling the emulsification parameters, microspheres of different particle sizes can be obtained to meet a variety of applications such as blood perfusion, drug release, bioseparation, sewage treatment, etc. Figure 3 (B) It can be seen that the column pressure of high crystallinity cellulose gel microspheres A / DC-ET is the smallest, while the traditional of The column pressure multiple of cellulose hydrogel microspheres SC-DI is the highest. The smaller the column pressure multiple, the stronger the compressive performance of the microspheres. Therefore, the compressive strength of A / DC-ET is the highest, followed by the compressive strength of A / DC-DI. This result shows that the experimental principle can be well reflected at the micron-level material scale and effectively improve the mechanical properties.

Claims

1. A method for preparing a high-strength and high-toughness cellulose hydrogel, characterized in that The method comprises the following steps: (1) preparing annealed alkaline cellulose gel: dissolving cellulose in an alkaline solution, adding epichlorohydrin dropwise at -4°C while stirring, centrifuging the cellulose solution to remove bubbles, pouring the cellulose solution into a mold or emulsifying it to prepare microspheres of different particle sizes, and annealing it at a specific temperature for 1 to 36 hours to obtain annealed alkaline cellulose gel; (2) preparing high-crystalline cellulose gel: placing the cellulose gel obtained in the previous step in an ethanol vapor environment for 8 to 48 hours, and then regenerating it in a certain concentration of ethanol aqueous solution at 5°C for 0 to 96 hours to obtain a cellulose gel with high crystallinity; (3) preparing double-crosslinked cellulose hydrogel: washing the high-crystalline cellulose gel obtained in the previous step with deionized water to remove ethanol and alkali to prepare a high-strength and high-toughness cellulose hydrogel.

2. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The cellulose used in step (1) is cotton linter pulp, microcrystalline cellulose, bacterial cellulose, bamboo fiber, ramie fiber and other natural cellulose of different sizes.

3. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The cellulose solvent used in step (1) can be NaOH / urea, NaOH / alkaline urea, LiOH / urea, and the concentration of the cellulose solution is 6 wt%~10 wt%.

4. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The amount of epichlorohydrin added in step (1) is 1-2.5 mL / 50 mL of cellulose solution.

5. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The mold used in step (1) can be in any desired shape, such as cylindrical, spherical, strip, or lamellar.

6. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The emulsion ratio used in step (1) is 40-60 mL white oil, 60-80 mL isooctane, 4.5-5.5 g Span 80 and 1.0-1.2 g Tween 80. A mixer or homogenizer can be used for emulsification. By controlling the stirring speed, microspheres with particle sizes ranging from a few microns to several hundred microns can be obtained.

7. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that After the microspheres prepared in step (1) are washed with alcohol and water to remove the oil phase, they must be re-immersed in an alkaline solution to ensure that the alkaline annealed gel is used for the next experiment.

8. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The annealing temperature used in step (1) is 5-80°C. To avoid excessive evaporation of water during annealing, the mold containing the cellulose solution is placed in a sealed room with a small amount of water.

9. The method for preparing a high-strength and high-toughness cellulose hydrogel according to claim 1, characterized in that The concentration of the ethanol aqueous solution used in step (2) is 75 wt%.

Citation Information

Patent Citations

  • Novel high-strength uniform-strength cellulose microsphere preparation method

    CN108745219A

  • Preparation method of regenerated cellulose material with low crystallinity

    CN109666188A

Cited By

  • Cellulose high-strength hydrogel material and preparation method thereof

    CN120059232A