Metal fiber composite material capable of being used for high-speed rail pantograph
By preparing efficient metal fiber composite materials, the problems of complex structure and low output efficiency in traditional methods are solved, and high-speed rail pantograph materials with high specific strength, fatigue resistance and low thermal expansion coefficient are achieved, which extends the service life of the equipment .
Patent Information
- Application Number
- CN202411262196.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-10
- Publication Date
- 2024-11-29
AI Technical Summary
The structure and low output efficiency of traditional metal fiber composite materials are complex in the preparation process, making it difficult to meet the durability needs of high-speed iron pantograph materials.
Through the steps of fiber product selection, cutting, dismantling, heating and kneading, rolling, drawing, annealing, sintering and hot forging, metal fiber composite materials with high specific strength, specific stiffness, fatigue resistance and low thermal expansion coefficient are prepared. .
It improves the mechanical properties and wear resistance of metal fiber composite materials, forms a good interface, and extends the service life of high-speed rail pantographs.
Smart Images

Figure CN119040614A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of pantograph metal fiber composite materials, in particular to a metal fiber composite material that can be used for high-speed railway pantographs. Background Art
[0002] During the operation of high-speed railways, pantographs are used. In order to make the pantographs last longer and be more durable, it is necessary to study the materials of the pantographs. Metal fiber composite materials need to be used. Traditional metal fiber composite materials have complex structures and low output efficiency. In view of this, this method is designed to study the above problems. Summary of the invention
[0003] The purpose of the present invention is to solve the above problems and to design a metal fiber composite material that can be used for high-speed railway pantographs.
[0004] To achieve the above-mentioned purpose, the technical solution of the present invention is a metal fiber composite material that can be used for a high-speed railway pantograph, comprising the following steps: S1, the fiber products are selected, then cut, and then the wires are unraveled to obtain metal wires; S2. The metal wire is repeatedly heated, rubbed, rolled and stirred to free the fiber monofilaments from the bond of the adhesive on the outer layer of the fiber, so that the fiber strands are separated and fluffy, and non-oriented flocculent continuous fibers are obtained. S3, drawing in a sheath, repeatedly, with an additional annealing process in the middle, cutting into segments after reaching a certain diameter, dissolving with acid, and finally obtaining the desired metal fiber, thereby obtaining a metal fiber composite material; S4, adding an annealing step to the metal fiber composite material obtained in S3, and controlling the temperature to be below 300° C.; S5, placing the metal fiber composite material dried in S3 into a vacuum atmosphere furnace at a temperature of 600° C. for sintering and keeping the temperature for 20-30 minutes; S6, cooling the sintered metal fiber composite material in S5 to 300-350°C and then hot forging and forming, and then cooling to room temperature to form mechanical parts.
[0005] The S3 uses sour nitric acid.
[0006] The S3 sheath is made of copper.
[0007] The step S1 further includes multiple soaking steps.
[0008] After S1, the method further includes the step of passivating the metal wire after the surface metallization.
[0009] A metal fiber composite material for high-speed railway pantographs made by the technical solution of the present invention has high specific strength and specific stiffness, good fatigue resistance and wear resistance, good damping, low thermal expansion coefficient, and small specific gravity. The alloy elements in the matrix are conducive to forming a good interface and improving the performance of the metal fiber composite material. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 This is a flow chart of a metal fiber composite material that can be used for a high-speed railway pantograph according to the present invention. DETAILED DESCRIPTION
[0011] The present invention will be described in detail below in conjunction with the accompanying drawings. Figure 1 As shown, a metal fiber composite material that can be used for a high-speed railway pantograph comprises the following steps: S1, the fiber products are selected, then cut, and then the wires are unraveled to obtain metal wires; S2. The metal wire is repeatedly heated, rubbed, rolled and stirred to free the fiber monofilaments from the bond of the adhesive on the outer layer of the fiber, so that the fiber strands are separated and fluffy, and non-oriented flocculent continuous fibers are obtained. S3, drawing in a sheath, repeatedly, with an additional annealing process in the middle, cutting into segments after reaching a certain diameter, dissolving with acid, and finally obtaining the desired metal fiber, thereby obtaining a metal fiber composite material; S4, adding an annealing step to the metal fiber composite material obtained in S3, and controlling the temperature to be below 300° C.; S5, placing the metal fiber composite material dried in S3 into a vacuum atmosphere furnace at a temperature of 600° C. for sintering and keeping the temperature for 20 minutes; S6, cooling the sintered metal fiber composite material in S5 to 300°C and then hot forging and forming, and then cooling to room temperature to form mechanical parts.
[0012] As a preferred technical solution, further, the S3 adopts sour nitric acid.
[0013] As a preferred technical solution, further, the S3 sheath is made of copper.
[0014] As a preferred technical solution, further, the step S1 further includes multiple soaking steps.
[0015] As a preferred technical solution, further, after S1, the step of passivating the metal wire after the surface metallization is also included.
[0016] The above technical solutions only reflect the preferred technical solutions of the technical solutions of the present invention. Some changes that may be made to certain parts thereof by technicians in this technical field all reflect the principles of the present invention and fall within the protection scope of the present invention.
Claims
1. A metal fiber composite material that can be used for high-speed railway pantographs, characterized in that: The following steps are involved: S1, the fiber products are selected, then cut, and then the wires are unraveled to obtain metal wires; S2. The metal wire is repeatedly heated, rubbed, rolled and stirred to free the fiber monofilaments from the binder of the outer layer of the fiber, so that the fiber filaments are separated and fluffy, and non-oriented flocculent continuous fibers are obtained; S3, drawing in a sheath, repeatedly, with an additional annealing process in the middle, cutting into segments after reaching a certain diameter, dissolving with acid, and finally obtaining the desired metal fiber, thereby obtaining a metal fiber composite material; S4, adding an annealing step to the metal fiber composite material obtained in S3, and controlling the temperature to be below 300° C.; S5, placing the metal fiber composite material dried in S3 into a vacuum atmosphere furnace at a temperature of 600° C. for sintering and keeping the temperature for 20-30 minutes; S6, cooling the sintered metal fiber composite material in S5 to 300-350°C and then hot forging and forming, and then cooling to room temperature to form mechanical parts.
2. The metal-based fiber reinforced sintered composite hot die forging process according to claim 1, characterized in that: The S3 uses sour nitric acid.
3. The metal-based fiber reinforced sintered composite hot die forging process according to claim 2, characterized in that: The S3 sheath is made of copper.
4. The metal-based fiber reinforced sintered composite hot die forging process according to claim 1, characterized in that: The step S1 further includes multiple soaking steps.
5. The metal-based fiber reinforced sintered composite hot die forging process according to claim 1, characterized in that: After S1, the method further includes the step of passivating the metal wire after the surface metallization.